Wafer grinding method
The wafer grinding method uses a protective member and surfactant-containing grinding water to prevent scratches and maintain chip strength by separating abrasive grains during the grinding process.
Patent Information
- Application Number
- JP2023063577
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-10
- Publication Date
- 2024-10-23
AI Technical Summary
The formation of scratches on the surface of wafers during grinding due to abrasive grains scattered between the grinding wheel and the wafer surface leads to a decrease in the bending strength of semiconductor chips.
A wafer grinding method involving a protective member to cover the wafer, holding the wafer on a chuck table, and supplying grinding water with a surfactant to separate and remove abrasive grains during the grinding process.
Prevents scratches on the wafer surface by separating abrasive grains with surfactant-containing grinding water, maintaining the bending strength of semiconductor chips.
Smart Images

Figure 2024150253000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for grinding a wafer held on a chuck table. [Background technology]
[0002] For example, as various electronic devices such as personal computers and smartphones are required to be made smaller and thinner, the semiconductor devices used in these electronic devices also tend to be made smaller and thinner. That is, in the manufacturing process of semiconductor devices, the surface of a disk-shaped semiconductor wafer (hereinafter simply referred to as a "wafer") is divided into many rectangular areas by planned division lines called streets arranged in a grid pattern, and devices such as ICs and LSIs are formed in each rectangular area. A wafer on which many devices are formed in this way is cut along the planned division lines to form multiple semiconductor chips.
[0003] In order to reduce the size and thickness of each semiconductor chip, the back surface of the wafer (the surface opposite to the surface on which the devices are formed) is usually ground before cutting the wafer along the planned dividing lines. The wafer is ground by pressing a grinding wheel rotating at high speed against the back surface of the wafer, and during the grinding, grinding water is supplied to the contact area (grinding area) between the wafer and the grinding wheel, and the grinding water cools the contact area (grinding area) and removes grinding debris (see, for example, Patent Document 1). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2009-141176 A Summary of the Invention [Problem to be solved by the invention]
[0005] Incidentally, grinding debris generated by grinding a wafer contains abrasive grains that have fallen off the grinding wheel, and if these fallen abrasive grains get into the gap between the grinding surface (back surface) of the wafer being ground and the lower surface (grinding surface) of the grinding wheel, scratches that are deeper than the grinding marks formed by the grinding wheel may be formed on the grinding surface of the wafer. These scratches cause a decrease in the flexural strength of the chips obtained by dividing the wafer after grinding.
[0006] The present invention has been made in consideration of the above problems, and an object of the present invention is to provide a method for grinding a wafer that can suppress the formation of scratches on the grinding surface of the wafer and prevent a decrease in the flexural strength of the chips obtained by dividing the wafer. [Means for solving the problem]
[0007] In order to solve the above problems, the present invention provides a wafer grinding method for grinding the back surface of a wafer having a device formed on its front surface with a grinding wheel, the method comprising: a protective member forming step of covering the entire front surface of the wafer with a protective member; a holding step of holding the wafer on a chuck table via the protective member; and a grinding step of supplying grinding water containing a surfactant to the grinding wheel and the wafer and grinding the back surface of the wafer with the grinding wheel. Effect of the Invention
[0008] According to the present invention, when the back surface of the wafer held on the chuck table via the protective member in the holding step is ground in the grinding step, grinding water containing a surfactant is supplied to the grinding wheel and the wafer, so that the abrasive grains that fall off the grinding wheel during the grinding process are separated and removed from the grinding water by the action of the surfactant. This prevents the abrasive grains from penetrating between the lower surface (grinding surface) of the grinding wheel and the back surface (ground surface) of the wafer, suppressing the formation of scratches on the back surface of the wafer by the abrasive grains. As a result, the reduction in the flexural strength of the chips obtained by dividing the ground wafer is prevented. [Brief description of the drawings]
[0009] [Figure 1] 1 is a perspective view showing, in a partially cutaway form, a grinding apparatus for carrying out a wafer grinding method according to the present invention; [Diagram 2] FIG. [Diagram 3] 1A and 1B are diagrams showing a protective member forming step in a wafer grinding method according to the present invention, in which (a) is an exploded perspective view of a wafer and a protective tape, and (b) is a perspective view of a wafer with a protective tape attached thereto. [Figure 4] 3 is a partial cross-sectional side view showing a holding step and a grinding step (rough grinding step) of the wafer grinding method according to the present invention. FIG. [Diagram 5] 3 is a plan view showing the relationship between a wafer and a grinding wheel in a grinding step (rough grinding step) of the wafer grinding method according to the present invention. FIG. [Figure 6] FIG. 2 is a partial perspective view showing a grinding step (rough grinding step) of the wafer grinding method according to the present invention. [Figure 7] 3 is a partial cross-sectional side view showing a holding step and a grinding step (finish grinding step) of the wafer grinding method according to the present invention. FIG. [Figure 8] 3 is a plan view showing the relationship between a wafer and a grinding wheel in a grinding step (finish grinding step) of the wafer grinding method according to the present invention. FIG. [Figure 9] FIG. 2 is a partial perspective view showing a grinding step (finish grinding step) of the wafer grinding method according to the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, an embodiment of the present invention will be described with reference to the accompanying drawings.
[0011] [Grinding equipment configuration] First, the configuration of a grinding device for carrying out a grinding method according to the present invention will be described with reference to Fig. 1. In the following description, the directions of the arrows shown in Fig. 1 are the X-axis direction (left-right direction), the Y-axis direction (front-back direction), and the Z-axis direction (up-down direction), respectively.
[0012] The grinding device 1 shown in FIG. 1 is a device for grinding a disk-shaped wafer W (see FIGS. 2 and 3) which is a workpiece, and includes three chuck tables 10 arranged on a rotatable disk-shaped turntable 2, a rough grinding unit 20 and a finish grinding unit 30 which are grinding units for grinding the wafer W held on the chuck table 10, and a grinding water supply unit 40 for supplying grinding water to the grinding area of the wafer W held on the chuck table 10 as main components. Here, as shown in FIG. 2, the surface of the wafer W (the upper surface in FIG. 2) is partitioned into a number of rectangular areas by dividing lines L1 and L2 called streets which are arranged in a lattice pattern and are orthogonal to each other, and devices D such as ICs and LSIs are formed in each rectangular area. A protective tape T for protecting the devices D is attached to the surface of the wafer W on which a number of devices D are formed, and a number of semiconductor chips are obtained by cutting the wafer W along the dividing lines L1 and L2.
[0013] Other components of the grinding apparatus 1 include thickness gauges 51, 52 for measuring the thickness of the wafer W during grinding, a cleaning unit 50 for cleaning the ground wafer W, a cassette 81 for storing multiple wafers W before grinding, a cassette 82 for storing the wafers W after grinding, an alignment table 83 for aligning the wafer W removed from the cassette 81, a transfer robot 84 for loading and unloading the wafer W into and from the cassettes 81, 82 and transporting the wafer W removed from the cassette 81 to the alignment table 83, a first transport means 85 for transporting the wafer W aligned on the alignment table 83 to the chuck table 10 located in the wafer transfer area R1, and a second transport means 90 for removing the wafer W finish-ground in the finish grinding area R3 from the chuck table 10 and transporting it to the cleaning unit 50, but detailed explanations of these will be omitted.
[0014] Here, the configurations of the chuck table 10, the rough grinding unit 20, the finish grinding unit 30, and the grinding water supply unit 40, which are the main components of the grinding apparatus 1, will be described.
[0015] (Chuck table) The three chuck tables 10 are disk-shaped members, and are arranged at equal angular pitches (120° pitches) in the circumferential direction on the turntable 2, which rotates intermittently about a central axis perpendicular to the Z-axis direction. These chuck tables 10 revolve around the axis of the turntable 2 perpendicular to the Z-axis direction by an angle of 120° each time the turntable 2 intermittently rotates, and move sequentially between the wafer loading / unloading region R1, the rough grinding region R2, and the finish grinding region R3, and can rotate (spin) around the axis at a predetermined speed by a rotation mechanism (not shown).
[0016] 4, a disk-shaped porous member 10A made of porous ceramic or the like is incorporated in the center of each chuck table 10, and the upper surface of each porous member 10A forms a holding surface 10a that suction-holds a disk-shaped wafer W. The porous member 10A of each chuck table 10 is selectively connected to a suction source 11 (see FIG. 4) such as a vacuum pump, as will be described later.
[0017] (Rough grinding unit and finish grinding unit) The grinding device 1 according to this embodiment includes a rough grinding unit 20 and a finish grinding unit 30, which are vertically arranged in a state of being arranged side by side in the X-axis direction (left and right direction) at the +Y-axis direction end (rear end) of a rectangular box-shaped base 200 that is long in the Y-axis direction (front and back direction) as shown in Fig. 1. Here, the rough grinding unit 20 is a unit that roughly grinds the back surface (upper surface in Fig. 4) of the wafer W held on the holding surface 10a of the chuck table 10 located in the rough grinding region R2, and the finish grinding unit 30 is a unit that finish grinds the back surface (upper surface in Fig. 7) of the wafer W held on the holding surface 10a of the chuck table 10 located in the finish grinding region R3, and the basic configurations of both are the same.
[0018] That is, the rough grinding unit 20 includes a spindle motor 22 fixed to a holder 21, a spindle 23 rotated by the spindle motor 22, a disk-shaped mount 24 attached to the lower end of the spindle 23, and a grinding wheel 25 detachably mounted on the lower surface of the mount 24. Here, the grinding wheel 25 is composed of a disk-shaped base 25a and a plurality of grinding stones 25b attached in an annular shape to the lower surface of the base 25a.
[0019] Similarly to the rough grinding unit 20, the finish grinding unit 30 also includes a spindle motor 32 fixed to a holder 31, a spindle 33 rotated by the spindle motor 32, a disk-shaped mount 34 attached to the lower end of the spindle 33, and a grinding wheel 35 detachably attached to the lower surface of the mount 34. Here, the grinding wheel 35 is composed of a disk-shaped base 35a and a plurality of grinding wheels 35b attached in an annular shape to the lower surface of the base 35a, and these grinding wheels 35b are composed of finer abrasive grains than the grinding wheels 25b of the rough grinding unit 20.
[0020] The rough grinding unit 20 and the finish grinding unit 30 are supported so as to be able to rise and fall by lifting mechanisms 3 provided on the -Y axis direction end faces (front faces) of a pair of block-shaped columns 101 that are erected vertically along the X axis direction (left and right direction) at the +Y axis direction end (rear end) of the base 200. Here, since both lifting mechanisms 3 have the same configuration, corresponding components will be described below with the same reference numerals.
[0021] Each lifting mechanism 3 lifts and lowers the rough grinding unit 20 and the finish grinding unit 30 independently along the Z-axis direction (up and down direction), and includes a rectangular plate-shaped lifting plate 4 and a guide rail 5 for guiding the lifting and lowering movement of the lifting plate 4. Here, the rough grinding unit 20 and the finish grinding unit 30 are respectively attached to each lifting plate 4. The guide rail 5 is disposed vertically on the front surface of the column 101.
[0022] A rotatable ball screw 6 is provided vertically along the Z-axis direction (up and down direction) beside each guide rail 5, and the upper end of the ball screw 6 is connected to a servo motor 7, which serves as a drive source and can rotate forward and backward. The lower end of the ball screw 6 is rotatably supported on a column 101 by a bearing (not shown), and a nut member (not shown) that is provided on the back surface of the lift plate 4 and protrudes horizontally toward the rear (+Y-axis direction) is screwed into the ball screw 6.
[0023] Therefore, when the servo motor 7 of each lifting mechanism 3 configured as described above is started to rotate each ball screw 6 forward and backward, each lifting plate 4, on which a nut member (not shown) that screws into each ball screw 6 is protruding, moves up and down along the guide rail 5, and the rough grinding unit 20 and the finish grinding unit 30 attached to the lifting plate 4 also move up and down independently of each other along the Z-axis direction (up and down direction).
[0024] (Grinding water supply unit) 1, the grinding water supply unit 40 supplies grinding water containing a surfactant to the contact area (grinding area) between the grinding wheel 25b of the rough grinding unit 20 and the wafer W during grinding, and includes a grinding water supply source 41. A pure water supply source 43 and a surfactant supply source 44 are connected to the grinding water supply source 41, and the pure water supplied from the pure water supply source 43 to the grinding water supply source 41 is mixed with the surfactant supplied from the surfactant supply source 44 to the grinding water supply source 41, thereby generating grinding water containing a surfactant in the grinding water supply source 41. In this embodiment, the concentration of the surfactant contained in the grinding water is set to about 0.1%.
[0025] A pipe 42 extends from the grinding water supply source 41, and two branch pipes 42a, 42b branch out from this pipe 42. Each of the branch pipes 42a, 42b is connected to a supply path (not shown) formed in the axial center of each of the spindle motors 22, 32 of the rough grinding unit 20 and the finish grinding unit 30, and opening / closing valves V1, V2 are provided midway along these branch pipes 42a, 42b, respectively. Although not shown, a supply passage (not shown) formed in the center of the shaft of each spindle motor 22, 32 of the rough grinding unit 20 and the finish grinding unit 30 is connected to a supply passage (not shown) formed in each spindle 23, 33, mount 24, 34 and grinding wheel 25, 35 of the rough grinding unit 20 and the finish grinding unit 30, and by switching the opening and closing of the opening / closing valves V1, V2, grinding water containing a surfactant is selectively supplied to the contact area (grinding area) between the grinding wheels 25b, 35b of the rough grinding unit 20 or the finish grinding unit 30 and the wafer W during grinding processing.
[0026] [Wafer grinding method] Next, a method for grinding the wafer W according to the present invention, which is carried out in the grinding apparatus 1 configured as above, will be described.
[0027] The method for grinding a wafer (W) according to the present invention comprises the steps of: 1) Protective material forming process 2) Holding process 3) Grinding process This is a method for grinding the back surface of the wafer W through the steps. Each step will be explained below.
[0028] 1) Protective member formation process: 3(a) and (b), the protective member forming step is a step of adhering a protective tape T, which is a protective member, to the surface (the lower surface in FIG. 3) of a wafer W. That is, as shown in FIG. 3(a), by adhering a thin circular protective tape T to the surface (the upper surface in FIG. 3(a)) of a wafer W on which a plurality of devices D are formed, the plurality of devices D (see FIG. 3(a)) formed on the surface (the lower surface in FIG. 3(b)) of the wafer W is protected by the protective tape T, as shown in FIG. 3(b).
[0029] 2) Holding process: The holding step is a step of holding the wafer W, on whose surface the protective tape T has been attached by the protective member forming step, with the protective tape T facing down on the holding surface 10a of the chuck table 10, as shown in Fig. 4. In this holding step, the porous member 10A of the chuck table 10 is connected to a suction source 11 shown in Fig. 4. Then, the suction source 11 draws a vacuum on the porous member 10A, generating a negative pressure in the porous member 10A, and the wafer W is sucked and held together with the protective tape T on the holding surface 10a of the chuck table 10 by this negative pressure, as shown in Fig. 4.
[0030] 3) Grinding process: The grinding process includes a rough grinding process for roughly grinding the back surface (top surface in FIG. 4) of the wafer W held on the holding surface 10a of the chuck table 10, as shown in FIGS. 4 to 6, and a finish grinding process for finish grinding the back surface (top surface in FIG. 7) of the wafer W held on the holding surface 10a of the chuck table 10, as shown in FIGS. 7 to 9. These rough grinding process and finish grinding process will be described below.
[0031] 3-1) Rough grinding process: As described above, the rough grinding step is a step of roughly grinding the back surface of the wafer W held on the holding surface 10a of the chuck table 10, but as shown in Fig. 4, the holding surface 10a of the chuck table 10 is configured as a conical surface that is inclined downward radially outward with the center as the apex, and the chuck table 10 is rotated in the direction of the arrow shown around a vertical axis passing through the center. Meanwhile, the inclination of the spindle 23 and grinding wheel 25 of the rough grinding unit 20 is adjusted by an inclination adjustment mechanism (not shown) so that they are parallel to the holding surface 10a (radial area) of the chuck table 10, and they are rotated in the direction of the arrow shown by the spindle motor 22 shown in Fig. 1.
[0032] In order to roughly grind the back surface (top surface in FIG. 4) of the wafer W by the rough grinding unit 20, the grinding wheel 25b is positioned so that the circumscribing circle passes through the center of the wafer W held on the holding surface 10a of the chuck table 10.
[0033] When the grinding wheel 25b is lowered in the -Z-axis direction by the lifting mechanism 3 shown in Fig. 1 from the above state, the lower surface (grinding surface) of the grinding wheel 25b rotates while contacting the back surface (upper surface) of the wafer W, so that the back surface (upper surface) of the wafer W is roughly ground. Here, the rotation trajectory of the grinding wheel 25b is shown by C1 in Fig. 5, and the grinding wheel 25b contacts the back surface of the wafer W in the arc-shaped region S1 shown in Fig. 5 to roughly grind the entire back surface (upper surface) of the wafer W. Then, when the back surface (upper surface) of the wafer W is roughly ground by the grinding wheel 25b, a plurality of arc-shaped grinding marks r1 are formed radially on the back surface (upper surface) of the wafer W from the center of the wafer W toward the periphery, as shown in Fig. 6.
[0034] Thus, during rough grinding of the wafer W, grinding water containing a surfactant is supplied from the grinding water supply source 41 of the grinding water supply unit 40 shown in Fig. 1 to the contact area (grinding area) S1 (see Fig. 5) between the grinding wheel 25b of the rough grinding unit 20 and the wafer W. That is, when one of the on-off valves V2 is closed and the other on-off valve V1 is opened, the grinding water containing a surfactant is supplied from the grinding water supply source 41 to the contact area (grinding area) S1 between the grinding wheel 25b and the wafer W through the piping 42, the branch pipe 42a, and a supply path (not shown) formed at the center of the axis of the spindle motor 22 and the spindle 23 of the rough grinding unit 20, and is used for cooling and cleaning the contact area (grinding area) S1. The concentration of the surfactant contained in the grinding water is not limited to 0.1% and may be any concentration within the range of 0.01% to 0.2%. In the case of rough grinding, the grinding debris discharged is large in proportion to the size of the abrasive grains of the grinding wheel 25b and is unlikely to adhere to the wafer W, so the concentration of the surfactant may be 0.01%.
[0035] During the rough grinding process of the wafer W by the grinding wheel 25b of the rough grinding unit 20, the thickness of the wafer W is measured by a thickness measuring device 51 shown in FIG. 1, and the rough grinding of the wafer W is continued until the thickness of the wafer W measured by the thickness measuring device 51 reaches a target thickness. When the rough grinding is completed because the amount of the wafer W ground reaches a predetermined value, the turntable 2 shown in FIG. 1 rotates by an angle of 120° in the direction of the arrow, so that the chuck table 10 also revolves by the same angle and moves from the rough grinding region R2 to the finish grinding region R3. Then, the back surface (upper surface) of the wafer W held by the chuck table 10 that has moved to the finish grinding region R3 is ground by the finish grinding unit 30 in the same manner as the rough grinding.
[0036] 3-2) Finish grinding process: As described above, the finish grinding process is a process for finish-grinding the back surface of the wafer W held on the holding surface 10a of the chuck table 10, and as shown in Fig. 7, the holding surface 10a of the chuck table 10 is rotated in the direction of the arrow in the figure around a vertical axis passing through the center. Meanwhile, the inclination of the spindle 23 and grinding wheel 35 of the rough grinding unit 20 is adjusted by an inclination adjustment mechanism (not shown) so that they are parallel to the holding surface 10a (radial area) of the chuck table 10, and they are rotated in the direction of the arrow in the figure by the spindle motor 32 shown in Fig. 1.
[0037] In order to finish grind the back surface (top surface in FIG. 7) of the wafer W by the finish grinding unit 30, the grinding wheel 35b is positioned so that the circumscribing circle passes through the center of the wafer W held on the holding surface 10a of the chuck table 10.
[0038] When the grinding wheel 35b is lowered in the -Z-axis direction by the lifting mechanism 3 shown in FIG. 1 from the above state, the lower surface (grinding surface) of the grinding wheel 35b rotates while contacting the back surface (upper surface) of the wafer W, so that the back surface (upper surface) of the wafer W is finish-ground. Here, the rotation trajectory of the grinding wheel 35b is shown by C2 in FIG. 8, and the grinding wheel 35b contacts the back surface of the wafer W in the arc-shaped region S2 shown in FIG. 8 to finish-grind the back surface (upper surface) of the wafer W over the entire surface. Then, when the back surface (upper surface) of the wafer W is finish-ground by the grinding wheel 35b, a plurality of arc-shaped grinding marks r2 are formed on the back surface (upper surface) of the wafer W in the rough grinding process, as shown in FIG. 9. In other words, when the grinding mark r1 formed by the rough grinding is intersected, finish grinding is started, forming a grinding mark r2 that intersects with the grinding mark r1, and the finish grinding is completed when the back surface (top surface) of the wafer W has only the grinding mark r2 formed thereon.
[0039] Thus, during the finish grinding of the wafer W, the grinding water containing the surfactant is supplied from the grinding water supply source 41 of the grinding water supply unit 40 shown in FIG. 1 to the contact area (grinding area) S2 (see FIG. 8) between the grinding wheel 35b of the finish grinding unit 30 and the wafer W. That is, when one of the on-off valves V1 is closed and the other on-off valve V2 is opened, the grinding water containing the surfactant is supplied from the grinding water supply source 41 to the contact area (grinding area) S2 between the grinding wheel 35b and the wafer W through the piping 42, the branch pipe 42b, and a supply path (not shown) formed at the center of the axis of the spindle motor 32 and the spindle 33 of the finish grinding unit 30, and is used for cooling and cleaning the contact area (grinding area) S2. Note that, even during the finish grinding, the concentration of the surfactant contained in the grinding water is set to 0.1%, but the concentration of the surfactant contained in the grinding water is not limited to 0.1% and may be any concentration within the range of 0.01% to 0.2%. In the case of finish grinding, the size of the abrasive grains of the grinding wheel 35b is smaller than the abrasive grains of the grinding wheel 25b used for rough grinding, and therefore the grinding debris discharged is small in proportion to the size of the abrasive grains of the grinding wheel 35b and easily adheres to the wafer W, so the concentration of the surfactant may be 0.2%.
[0040] During the finish grinding process of the wafer W by the grinding wheel 35b of the finish grinding unit 30, the thickness of the wafer W is measured by the thickness gauge 52 shown in Fig. 1, and the finish grinding of the wafer W is continued until the thickness of the wafer W measured by the thickness gauge 52 reaches a target thickness. When the finish grinding is completed because the amount of the wafer W ground reaches a predetermined value, the turntable 2 shown in Fig. 1 rotates by an angle of 120° in the direction of the arrow, and the chuck table 10 also revolves by the same angle and moves from the finish grinding region R3 to the wafer loading / unloading region R1. The wafer W held by the chuck table 10 moved to the wafer loading / unloading region R1 is held by the second transport means 90 and transported to the cleaning unit 50 shown in Fig. 1.
[0041] The wafer W transported to the cleaning unit 50 is held on the spinner table 53 of the cleaning unit 50 and rotates together with the spinner table 53, and the grinding surface (upper surface) is cleaned by the injection of cleaning water from the cleaning water injection nozzles 54. Then, the wafer W whose grinding surface has been cleaned is held by the carry-in / out robot 84 and transported to the cassette 82, and is stored in the cassette 82, completing the series of grinding processes for the wafer W.
[0042] As described above, in the grinding method of the wafer W according to the present invention, when the back surface of the wafer W held on the chuck table 10 via the protective tape T in the holding step is ground in the grinding step (rough grinding step and finish grinding step), grinding water containing a surfactant is supplied to the contact area (grinding area) S1, S2 (see Figs. 5 and 8) between the grinding wheels 25b, 35b and the wafer W, so that the abrasive grains that have fallen off the grinding wheels 25b, 35b during the grinding process are separated and removed from the grinding water by the action of the surfactant. This prevents the abrasive grains from penetrating between the lower surface (grinding surface) of the grinding wheels 25b, 35b and the back surface (ground surface) of the wafer W, and suppresses the formation of scratches on the back surface of the wafer W by the abrasive grains. As a result, the effect of preventing the reduction in the bending strength of the chips obtained by dividing the ground wafer W is obtained. In addition, it is possible to reduce adhesion of grinding debris (particles) to the back surface (ground surface) of the ground wafer W. This makes it possible to complete cleaning of the wafer W in a short time while it is held on the chuck table 10.
[0043] In the grinding apparatus 1 according to the above embodiment, a method is adopted in which grinding water is supplied from the center of each axis of the rough grinding unit 20 and the finish grinding unit 30 toward the wafer W, but a method can also be adopted in which grinding water is supplied from the side toward the wafer W from a cleaning water jet nozzle arranged on the side of the chuck table 10. Here, the cleaning water jet nozzle is an internal nozzle arranged inside the grinding wheel to jet grinding water onto the inner surface of the grinding stone, or an external nozzle arranged outside the grinding wheel to jet grinding water onto the outer surface of the grinding stone, and either one or both may be provided.
[0044] Moreover, the grinding apparatus 1 may be configured to include only one of the rough grinding unit 20 and the finish grinding unit 30. Furthermore, the grinding apparatus 1 may be configured to include one grinding unit and one chuck table.
[0045] In addition, the present invention is not limited to the application of the embodiments described above, and various modifications are possible within the scope of the claims and the technical ideas described in the specification and drawings. [Explanation of symbols]
[0046] 1: grinding device, 2: turntable, 3: lifting mechanism, 4: lifting plate, 5: guide rail, 6: ball screw, 7: servo motor, 10: chuck table, 10A: porous member, 10a: holding surface, 11: suction source, 20: rough grinding unit, 21: holder, 22: spindle motor, 23: spindle, 24: mount, 25: grinding wheel, 25a: base, 25b: grinding wheel, 30: finish grinding unit, 31: holder, 32: spindle motor, 33: spindle, 34: mount, 35: grinding wheel, 35a: base, 35b: grinding wheel, 40: grinding water supply unit, 41: grinding water supply source, 42: piping; 42a, 42b: branch pipes; 43: pure water supply source; 44: surfactant supply source; 50: cleaning unit, 51, 52: thickness measuring device, 53: spinner table, 54: cleaning water injection nozzle, 60: tape mounter, 61: 81, 82: cassette, 83: alignment table, 84: loading / unloading robot, 85: first conveying means, 90: second conveying means, 100: base, 101: column, C1: Rotational trajectory of the grinding wheel during rough grinding, C2: Rotational trajectory of the grinding wheel during finish grinding, D: device, L1, L2: division line, R1: wafer loading / unloading area, R2: Rough grinding area, R3: Finish grinding area, r1: Grinding marks from rough grinding, r2: grinding marks during finish grinding, S1: contact area of the grinding wheel during rough grinding, S2: contact area of the grinding wheel during finish grinding, T: protective tape (protective material), V1, V2: On-off valve, W: Wafer
Claims
[Claim 1] A wafer grinding method for grinding a back surface of a wafer having a device formed on a front surface thereof with a grinding wheel, comprising the steps of: a protective member forming step of covering the entire surface of the wafer with a protective member; a holding step of holding the wafer on a chuck table via the protective member; a grinding step of supplying a grinding water containing a surfactant to the grinding wheel and the wafer and grinding the back surface of the wafer with the grinding wheel; A method for grinding a wafer comprising the steps of:
Citation Information
Patent Citations
Method of grinding wafer
JP2009141176A