Semiconductor light emission device

The semiconductor light emitting device addresses heat and optical damage issues by applying compressive strain through higher Ni concentration at electrode ends, enhancing the bandgap and enabling efficient heat dissipation without material or structural limitations.

JP2024153458AActive Publication Date: 2024-10-29DENSO CORP +2
View PDF 17 Cites 0 Cited by

Patent Information

Application Number
JP2023067361
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-17
Publication Date
2024-10-29
Estimated Expiration
2043-04-17

AI Technical Summary

Technical Problem

Existing semiconductor lasers face issues with non-radiative recombination causing temperature rise and optical damage due to light absorption, which are not effectively addressed by current structures that either limit material choices or fail to dissipate heat near the end face.

Method used

A semiconductor light emitting device with a structure that applies compressive strain to the active layer by increasing the Ni concentration at the ends of the conductivity type electrodes, enhancing the bandgap and preventing light absorption while allowing for effective heat dissipation without notches or material restrictions.

Benefits of technology

The device suppresses catastrophic optical damage and provides efficient heat dissipation by maintaining a flat end face and avoiding impurity diffusion, applicable to various semiconductor materials and structures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024153458000001_ABST
    Figure 2024153458000001_ABST
Patent Text Reader

Abstract

To provide a semiconductor light emission device which does not receive restriction of a semiconductor material and a structure and can obtain a good heat dissipation characteristic with a structure not using diffusion of an impurity.SOLUTION: A semiconductor light emission device includes: an element unit 4 configured on one surface side of a light emission element substrate 11 while forming each layer; an n-type electrode 10 formed on the light emission element substrate 11; a p-type electrode 18 arranged at an opposite side of the n-type electrode 10 while sandwiching the element unit 4; a light emission element 2 which has one direction as a resonance direction, and emits light at least one of both end faces in the resonance direction; and a substrate 3 connected with the p-type electrode 18. The p-type electrode 18 has a junction structure between a first electrode arranged at the light emission element 2 side and a second electrode arranged at the substrate side. The junction layers 18d to 18f between the first electrode and the second electrode include at least Au, Sn, and Ni. An Ni concentration being a concentration of the Ni at both ends of in the resonance direction is larger than the Ni concentration at center section being inside of both ends.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a semiconductor light emitting device having a semiconductor laser. [Background technology]

[0002] In semiconductor lasers, there are many interface states at both end faces. For this reason, it is known that non-radiative recombination causes a rise in temperature, narrowing the band gap, absorbing light, and the temperature rise due to light absorption is repeated, resulting in catastrophic optical damage (COD). In response to this, a structure called a window structure has been proposed, which enlarges the band gap at both end faces and makes it less likely for light absorption to occur.

[0003] For example, there is a structure in which the semiconductor active layer that generates light is formed as a quantum well, and impurities are diffused to disorder the quantum well, i.e., to make it a mixed crystal, thereby increasing the band gap. However, since GaAs or InP-based materials are required to diffuse the impurities, there are limitations on the material of the active layer, and there are also limitations on the well layer thickness as an active layer structure.

[0004] On the other hand, a similar effect can be obtained by including impurities with high electronegativity in the GaN-based active layer. This structure has the advantage of being free from the effects of heat, as it can be formed by plasma processing. However, this structure can only be applied when the active layer is made of GaN-based materials that generate polarization. Therefore, there are limitations on the semiconductor materials and element structures.

[0005] In response to this, Patent Document 1 proposes a structure in which a notch is provided near the end face to prevent the lower end of the resonator end face from coming into contact with the semiconductor substrate, thereby reducing distortion, as a technology for suppressing COD in nitride-based materials. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] JP 2011-228570 A Summary of the Invention [Problem to be solved by the invention]

[0007] However, although the structure proposed in Patent Document 1 suppresses light absorption, it is not possible to dissipate heat generated near the end faces that are cut out, and it is only applicable when the active layer is tensile strained.

[0008] In view of the above, an object of the present disclosure is to provide a semiconductor light-emitting device that has a structure that does not involve impurity diffusion into a semiconductor layer, is not restricted by semiconductor materials or structures, and has good heat dissipation properties. [Means for solving the problem]

[0009] In order to achieve the above object, the invention described in claim 1 comprises: A semiconductor light emitting device, a light emitting element (2) having a light emitting element substrate (11) made of a semiconductor material of a first conductivity type, including an element section (4) in which a first clad layer (12) of the first conductivity type, a first guide layer (13) of the first conductivity type, an active layer (14), a second guide layer (15) of a second conductivity type, and a second clad layer (16) of the second conductivity type are arranged in this order on one surface side of the light emitting element substrate, a first conductivity type electrode (10) formed on the side of the light emitting element substrate opposite the first clad layer, and a second conductivity type electrode (18) arranged on the opposite side of the first conductivity type electrode with the element section in between, and emitting light from at least one of both end faces in the resonance direction with one direction as a resonance direction; A substrate (3) connected to the second conductivity type electrode, The second conductivity type electrode has a junction structure between a first electrode arranged on the light emitting element side and a second electrode arranged on the substrate side, and the junction layer (18d to 18f) between the first electrode and the second electrode contains at least Au, Sn and Ni, and has a higher Ni concentration at both ends in the resonance direction than in the central portion located further inward.

[0010] In this way, the second conductive type electrode is designed so that the Ni concentration is higher at both ends in the light resonance direction than at the center, making it possible to apply compressive strain to the active layer. This makes the band gap larger at both ends in the light resonance direction, making it difficult for light absorption to occur and making it possible to suppress COD. In addition, it is not necessary to provide notches or the like on both end faces in the light resonance direction, and the end faces can be simply flat. Therefore, a semiconductor light emitting device can be made that has good heat dissipation properties without being limited by semiconductor materials or structures, with a structure that does not involve the diffusion of impurities into the semiconductor layer.

[0011] The reference symbols in parentheses attached to each component indicate an example of the correspondence between the component and specific components described in the embodiments described below. [Brief description of the drawings]

[0012] [Figure 1] 1 is a cross-sectional view of a semiconductor light emitting device according to a first embodiment of the present disclosure. [Figure 2A] 2A to 2C are cross-sectional views illustrating a manufacturing process for the semiconductor light emitting device shown in FIG. [Figure 2B] 2B is a cross-sectional view showing a manufacturing process of the semiconductor light emitting device subsequent to FIG. 2A. [Figure 2C] 2C is a cross-sectional view showing a manufacturing process of the semiconductor light emitting device subsequent to FIG. 2B. [Figure 2D] 2D is a cross-sectional view showing a manufacturing process of the semiconductor light emitting device subsequent to FIG. 2C. [Figure 2E] 2E is a cross-sectional view showing a manufacturing process of the semiconductor light emitting device subsequent to FIG. 2D. [Figure 3A] 5A to 5C are cross-sectional views illustrating a manufacturing process of a semiconductor light-emitting device according to a second embodiment of the present disclosure. [Figure 3B] 3B is a cross-sectional view showing a manufacturing process of the semiconductor light emitting device subsequent to FIG. 3A. [Figure 4] 11 is a cross-sectional view of a semiconductor light emitting device according to a third embodiment of the present disclosure. [Figure 5A] 5A to 5C are cross-sectional views illustrating a manufacturing process for the semiconductor light emitting device illustrated in FIG. [Figure 5B] 5B is a cross-sectional view showing a manufacturing process of the semiconductor light emitting device subsequent to FIG. 5A. [Figure 5C] 5C is a cross-sectional view showing a manufacturing process of the semiconductor light emitting device subsequent to FIG. 5B. [Figure 5D] 5D is a cross-sectional view showing a manufacturing process of the semiconductor light emitting device subsequent to FIG. 5C. [Figure 5E] 5B is a cross-sectional view showing a manufacturing process of the semiconductor light emitting device subsequent to FIG. 5D. [Figure 6A] 10A to 10C are cross-sectional views illustrating a manufacturing process of a semiconductor light-emitting device according to a fourth embodiment of the present disclosure. [Figure 6B] 6B is a cross-sectional view showing a manufacturing process of the semiconductor light emitting device subsequent to FIG. 6A. [Figure 7] 11 is a cross-sectional view of a semiconductor light emitting device according to a fifth embodiment of the present disclosure. [Figure 8] 8A to 8C are cross-sectional views illustrating a manufacturing process for the semiconductor light emitting device illustrated in FIG. [Figure 9] 13 is a cross-sectional view of a semiconductor light-emitting device according to a sixth embodiment of the present disclosure. [Figure 10] 10A to 10C are cross-sectional views illustrating a manufacturing process for the semiconductor light emitting device illustrated in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] Hereinafter, embodiments of the present invention will be described with reference to the drawings. In the following embodiments, parts that are the same or equivalent to each other will be denoted by the same reference numerals.

[0014] (First embodiment) A first embodiment will be described. As shown in Fig. 1, a semiconductor light emitting device 1 of this embodiment includes a light emitting element 2 and a substrate 3. The semiconductor light emitting device 1 is applied to, for example, a laser radar or LiDAR. LiDAR is an abbreviation for Light Detection And Ranging.

[0015] The light emitting element 2 is a part that constitutes a semiconductor laser, and is a light source that generates laser light. As shown in Fig. 1, the light emitting element 2 has an n-type electrode 10, a light emitting element substrate 11, a first cladding layer 12, a first guide layer 13, an active layer 14, a second guide layer 15, a second cladding layer 16, a contact layer 17, and a p-type electrode 18. The light emitting element 2 emits light from at least one of both end faces in one direction, which is the left-right direction of the paper surface of Fig. 1 in this case, as the resonance direction.

[0016] The n-type electrode 10 is formed on the light emitting element substrate 11. The light emitting element substrate 11 is a base material on which each layer constituting the light emitting element 2 is formed, and is of n-type. In this embodiment, an InP (indium phosphide) substrate is used as the light emitting element substrate 11. The first cladding layer 12 is made of n-InP and is disposed on one side of the light emitting element substrate 11. The first guide layer 13 is made of n-InGaAsP (indium gallium arsenide phosphide) and is disposed on the opposite side of the light emitting element substrate 11 with the first cladding layer 12 sandwiched therebetween. The active layer 14 is made of InGaAsP or the like and is disposed on the opposite side of the first cladding layer 12 with the first guide layer 13 sandwiched therebetween. The second guide layer 15 is made of p-InGaAsP and is disposed on the opposite side of the first guide layer 13 with the active layer 14 sandwiched therebetween. The second cladding layer 16 is made of p-InGaAsP and is disposed on the opposite side of the active layer 14 with the second guide layer 15 sandwiched therebetween. The contact layer 17 is made of p-InGaAs, and is disposed on the opposite side to the second guide layer 15, sandwiched between the second cladding layers 16. In this manner, the light-emitting element substrate 11 has a structure in which the first cladding layer 12, the first guide layer 13, the active layer 14, the second guide layer 15, the second cladding layer 16, and the contact layer 17 are laminated in this order on one surface side of the light-emitting element substrate 11 on the lower side of the drawing.

[0017] The first cladding layer 12 and the second cladding layer 16 increase the electron density and hole density in the junction region of the active layer 14 and, together with the first guide layer 13 , the second guide layer 15 and the contact layer 17 , serve to confine light within the active layer 14 .

[0018] The first guide layer 13 and the second guide layer 15 serve to confine the light emitted from the active layer 14 within the active layer 14 .

[0019] The contact layer 17 is formed as necessary for low contact. Since the band gap becomes wider from the active layer 14 to the p-type electrode 18 through the second guide layer 15 and the second cladding layer 16, and the contact resistance becomes larger, the contact layer 17 is formed to narrow the band gap and reduce the contact resistance.

[0020] The active layer 14 resonates and emits light at a wavelength according to the band gap as the injected carriers recombine. Although a detailed structure of the active layer 14 is omitted, the active layer 14 has a multi-quantum well structure in which a plurality of quantum dot layers each having granular quantum dots formed by, for example, crystal growth or microfabrication are repeatedly stacked in layers.

[0021] The first cladding layer 12 , the first guide layer 13 , the active layer 14 , the second guide layer 15 , the second cladding layer 16 and the contact layer 17 form an element section 4 of the light emitting element 2 .

[0022] The p-type electrode 18 is a metal layer for making contact with the element portion 4, and is disposed on the opposite side of the n-type electrode 10 across the element portion 4. In this embodiment, the p-type electrode 18 is formed by laminating, in order from the element portion 4 side, a Ti (titanium) layer 18a, a Pt (platinum) layer 18b, a Ni layer 18c, an AuNiSn (gold-nickel-tin) layer 18d, an Au5Sn layer 18e, an AuSn (gold-tin) layer 18f, a Pt layer 18g, and a Ti layer 18h.

[0023] The Ti layer 18a is a layer for making contact with the element part 4. The Pt layer 18b is a layer formed as necessary, and is a barrier layer that suppresses the arrival of AuSn to the Ti layer 18a side. The Ni layer 18c is a layer that is partially alloyed with the Au layer 181 and the AuSn layer 182 described later during bonding, but only a part of the surface layer is alloyed, and is composed of the remaining part that is not alloyed. The AuNiSn layer 18d, the Au5Sn layer 18e, and the AuSn layer 18f are bonding layers for bonding the element part 4, the Ti layer 18a, and the Pt layer 18b to the base material 3. The AuNiSn layer 18d, the Au5Sn layer 18e, and the AuSn layer 18f are the Au layer 181, the AuSn layer 182, and the Au layer 183 described later before bonding, but are alloyed by melting to become these layers. The Pt layer 18g is also a layer formed as necessary, and is a barrier layer that prevents AuSn from reaching the Ti layer 18h side. The Ti layer 18h is an adhesion auxiliary layer that facilitates adhesion to the base material 3. As described later, the base material 3 is made of Si, so the Ti layer 18h is used as an adhesion auxiliary layer. However, if the base material 3 is made of a material other than Si, a metal that has good adhesion to that material may be selected. Of course, even if the base material 3 is made of Si, the adhesion auxiliary layer may be made of a metal other than Ti.

[0024] The light emitting element 2 is mounted on the substrate 3 via the p-type electrode 18, and in this example, the substrate 3 is a semiconductor substrate made of Si. A wiring pattern electrically connected to the p-type electrode 18 is formed on the substrate 3, and a desired voltage can be applied to the p-type electrode 18. The substrate 3 may also be made of a material other than Si.

[0025] In the semiconductor light emitting device 1 thus configured, the light is resonated in the left-right direction of the paper and emitted to the outside from at least one end face. The Ni concentration is higher at both ends of the resonance direction than at the center, which is located inside the resonance direction. In the case of this embodiment, the thickness of the Ni layer 18c is made thicker at both ends of the resonance direction than at the center, so that the Ni concentration at the corresponding locations is higher than at the center. In addition, the AuNiSn layer 18d formed on the Ni layer 18c is also formed on the Ni layer 18c, so that both ends in the left-right direction of the paper protrude toward the base material 3 from the center, which is located inside the both ends.

[0026] In this way, by making the Ni concentration larger at both ends in the light resonance direction in the semiconductor light emitting device 1 than at the center, for example, by making the Ni layer 18c thick as in this embodiment, it is possible to apply compressive strain to the active layer 14 as described later. As a result, the band gap becomes larger at both ends in the light resonance direction, making it difficult for light absorption to occur, and it is possible to suppress COD. And, by making the Ni concentration larger at both ends in the light resonance direction than at the center, for example, by making the thickness of a part of the electrode material, the Ni layer 18c, thicker at both ends in the light resonance direction than at the center, the COD suppression effect can be obtained. Therefore, since it is not necessary to provide a notch or the like on the end face, the end face can be simply a flat surface. Therefore, the semiconductor light emitting device 1 can be structured not by diffusing impurities into the semiconductor layer, and can also obtain good heat dissipation without being restricted by the semiconductor material or structure.

[0027] Next, a method for manufacturing the semiconductor light emitting device 1 according to this embodiment will be described with reference to FIGS. 2A to 2E.

[0028] First, as a step shown in FIG. 2A, a light emitting element substrate 11 is prepared, and each layer constituting the element section 4 and a part of a metal layer for constituting the p-type electrode 18 are formed on the light emitting element substrate 11. Specifically, the first clad layer 12, the first guide layer 13, the active layer 14, the second guide layer 15, the second clad layer 16, and the contact layer 17 are formed in this order on the light emitting element substrate 11 to form the element section 4. Then, a Ti layer 18a and a Pt layer 18b are formed on the contact layer 17, and then a Ni layer 18c is formed thereon. The Ni layer 18c is formed so that both ends in one direction, that is, both ends in the resonance direction when the semiconductor light emitting device 1 is formed, are thicker than the central part on the inside, and in this embodiment, the Ni layer 18c is formed using a lift-off method.

[0029] More specifically, as shown in FIG. 2A, the first layer 18ca of the Ni layer 18c is formed, and then the resist 30 is formed thereon, and exposed so that the resist 30 remains in the central portion of the first layer 18ca and does not remain in the portions located at both ends. Then, the second layer 18cb, which is the remaining portion of the Ni layer 18c, is formed on the resist 30. As a result, the second layer 18cb is piled up at both ends of the first layer 18ca, and the second layer 18cb is formed on the resist 30 except for the both ends. After that, as shown in FIG. 2B, when the resist 30 is removed by a stripping solution or the like, the portion of the second layer 18cb formed on the resist 30 is also removed. As a result, the Ni layer 18c having a thicker thickness at both ends in one direction can be formed.

[0030] 2C, an Au layer 181 is formed on the Ni layer 18c. This Au layer 181 is an optional layer, and is formed to prevent oxidation because the Ni layer 18c may be oxidized by the surrounding oxygen if it is on the outermost surface.

[0031] In this manner, the light emitting element 2 and a portion of the metal layer for constituting the p-type electrode 18 can be formed on the light emitting element substrate 11. Note that the portion of the metal layer for constituting the p-type electrode 18 formed at this time corresponds to the first electrode.

[0032] 2A to 2C, a step shown in FIG. 2D is performed to deposit a Ti layer 18h, a Pt layer 18g, an Au layer 183, and an AuSn layer 182 in this order on the base material 3. This forms a remaining portion of the metal layers for forming the p-type electrode 18. The remaining portion of the metal for forming the p-type electrode 18 formed at this time corresponds to the second electrode.

[0033] Thereafter, in the step shown in Fig. 2E, the light emitting element substrate 11 on which the light emitting element 2 and some of the metal layers for constituting the p-type electrode 18 have been formed through the step shown in Fig. 2C are bonded to the base material 3 on which the remaining metal layers for constituting the p-type electrode 18 have been formed through the step shown in Fig. 2D. They are arranged so that the metal layers for constituting the p-type electrode 18 face each other, and are bonded by heating at, for example, 280°C or higher.

[0034] At this time, the AuSn layer 182 and the AuSn and Ni contained in the Ni layer 18c cause a reaction according to the following chemical formula. In addition, Au constituting the Au layer 181 and the Au layer 183 is appropriately used in the reaction. As a result, the Au layer 181, the AuSn layer 182, and the Au layer 183 become the Au5Sn layer 18e and the AuSn layer 18f. In addition, Ni in the Ni layer 18c diffuses to the AuSn layer 182 and reacts with AuSn to form the AuNiSn layer 18d. Then, the AuNiSn layer 18d, the Au5Sn layer 18e, and the AuSn layer 18f function as bonding layers to bond the first electrode and the second electrode. Although Ni3Sn2 is not shown in FIG. 1, it is formed at the interface between the AuNiSn layer 18d and the Ni layer 18c.

[0035] [C1] 7Au 0.71 Sn 0.29 +1.53Ni → 0.51Ni3Sn2+Au5Sn It is known that when the reaction described in the above chemical formula occurs, 22 mol% of Ni reacts, resulting in a volumetric shrinkage of 3.2% (see Materials Science & Engineering A 773 (2020) 138738). In one axial direction, shrinkage of 1% occurs.

[0036] Therefore, by increasing the Ni content in the AuNiSn layer 18d, which becomes a bonding layer near the end face in the resonance direction, the compressive strain on the active layer 14 can be increased. That is, as in this embodiment, by increasing the thickness of both ends of the Ni layer 18c, the amount of Ni diffusion and the Ni concentration at those locations increase, and the volume shrinkage rate increases, so that the compressive strain can be increased. When compressive strain is applied, the band gap of the light emitting layer of the optical device can be increased (Phys, Rev.B (43) 12 pp9649-9661). Therefore, it is possible to suppress the COD suppression due to light absorption at the end face.

[0037] Moreover, the energy spread of the emitted light from the semiconductor laser is 10 meV or less. By generating a band shift of 10 meV or more, a better COD suppression effect can be expected. In that case, it is preferable to add a compressive strain of 0.25%, and by incorporating 5 mol% or more of Ni into the bonding layer, that is, by making the Ni concentration difference between both ends and the center of the bonding layer in the resonance direction 5 mol% or more, it is possible to further suppress COD.

[0038] Although the subsequent steps are not shown, the n-type electrode 10 is formed on the light emitting element substrate 11, and the semiconductor light emitting device 1 is completed.

[0039] As described above, in the semiconductor light emitting device 1 of this embodiment, by making the Ni concentration larger than that of the center, for example, by making the Ni layer 18c thick as in this embodiment, it is possible to apply compressive strain to the active layer 14 as described later. As a result, the band gap becomes larger at both ends in the resonance direction of light, making it difficult for light absorption to occur, and it is possible to suppress COD. Then, by making the Ni concentration larger at both ends in the resonance direction of light than that of the center, for example, by making the thickness of a part of the electrode material, the Ni layer 18c, thicker at both ends in the resonance direction of light than that of the center, the COD suppression effect can be obtained. Therefore, since it is not necessary to provide a notch or the like on the end face, the end face can be simply a flat surface. Therefore, the semiconductor light emitting device 1 can be structured not by diffusing impurities into the semiconductor layer, and can also obtain good heat dissipation without being restricted by the semiconductor material or structure.

[0040] Second embodiment The second embodiment will be described. This embodiment is similar to the first embodiment except that the configuration of the Au layer 183 is changed, and therefore only the differences from the first embodiment will be described.

[0041] In the first embodiment, when the Ni layer 18c is formed by the lift-off method, the first layer 18ca of the Ni layer 18c is exposed when the first layer 18ca is formed. For this reason, as the process shown in FIG. 3A, a part of the Au layer 181 may be formed on the first layer 18ca, and then the resist 30 and the second layer 18cb may be formed, and then the remaining part of the Au layer 181 may be formed on the second layer 18cb. In this case, as the process shown in FIG. 3B after that, when the resist 30 is removed, the second layer 18cb and the remaining part of the Au layer 181 on the resist 30 may also be removed. In this way, the Au layer 181 may be formed on each of the first layer 18ca and the second layer 18cb.

[0042] Third embodiment The second embodiment will be described. This embodiment is similar to the first embodiment except that the configuration of the Au layer 183 is changed, and therefore only the differences from the first embodiment will be described.

[0043] As shown in Figure 4, the semiconductor light-emitting device 1 of this embodiment also includes a light-emitting element 2 and a substrate 3, but the stacking order of the metal layers that make up the p-type electrode 18 is different from that of the first embodiment.

[0044] Specifically, in this embodiment, the p-type electrode 18 is configured by a laminated structure of a Ti layer 18a, a Pt layer 18b, an AuSn layer 18f, an Au5Sn layer 18e, an AuNiSn layer 18d, a Ni layer 18c, and a Ti layer 18h in this order from the element unit 4. The Ni layer 18c, which is thickened at both ends, is formed on the substrate 3 side and then bonded to a part of the metal layer for forming the p-type electrode 18 on the element unit 4 side. Note that the laminated order of the metal layers constituting the p-type electrode 18 is different from that of the first embodiment, but the role of each metal layer is the same as that of the first embodiment. In this embodiment, the Pt-lined 18g is not formed on the surface of the Ti layer 18h formed on the substrate 3, but it may be formed.

[0045] The semiconductor light emitting device 1 having such a structure can be manufactured through the steps shown in FIGS. 5A to 5E.

[0046] First, in the process shown in Figures 5A to 5C, a base material 3 on which a wiring pattern or the like is formed is prepared, and a part of a metal layer for forming a p-type electrode 18 is formed on the base material 3. Specifically, in the process shown in Figures 5A and 5B, a Ti layer 18h is formed on the base material 3, and then a Ni layer 18c is formed thereon. The Ni layer 18c is designed so that both ends in one direction, that is, both ends in the resonance direction when the semiconductor light emitting device 1 is formed, are thicker than the central part on the inside, and in this embodiment, the Ni layer 18c is formed by using a lift-off method.

[0047] More specifically, as shown in FIG. 5A, the first layer 18ca of the Ni layer 18c is formed, and then the resist 30 is formed thereon, and exposed so that the resist 30 remains in the central portion of the first layer 18ca and does not remain in the portions located at both ends. Then, the second layer 18cb, which is the remaining portion of the Ni layer 18c, is formed on the resist 30. As a result, the second layer 18cb is piled up at both ends of the first layer 18ca, and the second layer 18cb is formed on the resist 30 except at both ends. After that, as shown in FIG. 5B, when the resist 30 is removed by a stripping solution or the like, the portion of the second layer 18cb formed on the resist 30 is also removed. As a result, the Ni layer 18c having a thicker thickness at both ends in one direction can be formed.

[0048] Furthermore, as a step shown in FIG. 5C, an Au layer 181 is formed on the Ni layer 18c to prevent oxidation of the Ni layer 18c, if necessary.

[0049] In this manner, a portion of the metal layer for constituting the p-type electrode 18 can be formed on the base material 3. Note that the portion of the metal layer for constituting the p-type electrode 18 formed on the base material 3 at this time corresponds to the second electrode.

[0050] Meanwhile, by performing a step shown in FIG. 5D in addition to the steps shown in FIGS. 5A to 5C, the light emitting element 2 is formed and the remaining metal layers for constituting the p-type electrode 18 are also formed. Specifically, the layers constituting the element section 4 are formed on the light emitting element substrate 11. Then, the Ti layer 18a, the Pt layer 18b, the Au layer 183, and the AuSn layer 182 are formed on the contact layer 17 to form the remaining metal layers for constituting the p-type electrode 18. The remaining metal for constituting the p-type electrode 18 formed at this time corresponds to the first electrode.

[0051] Thereafter, in the step shown in Fig. 5E, the base material 3 on which a part of the metal layer for forming the p-type electrode 18 has been formed through the step shown in Fig. 5C is bonded to the light emitting element 2 and the remaining part of the metal layer for forming the p-type electrode 18 on which a part of the metal layer for forming the p-type electrode 18 has been formed through the step shown in Fig. 5D. The metal layers for forming the p-type electrode 18 are arranged to face each other, and they are bonded by heating at, for example, 280°C or higher. This completes the semiconductor light emitting device 1 of this embodiment shown in Fig. 4.

[0052] In this way, even if the Ni layer 18c with thickened thickness at both ends is formed on the substrate 3 side and then bonded to a part of the metal layer for forming the p-type electrode 18 on the element section 4 side, the compressive strain on the active layer 14 can be increased near the end face in the resonance direction. This increases the amount of Ni diffusion at that location and increases the volumetric shrinkage rate, thereby increasing the compressive strain and increasing the band gap of the light emitting layer of the optical device. Therefore, it is possible to suppress COD suppression due to light absorption at the end face, and the same effect as in the first embodiment can be obtained.

[0053] (Modifications of the first and third embodiments) In the first and third embodiments, a structure in which both ends of the Ni layer 18c are thicker than the center is realized by using the lift-off method. This structure may be realized by other methods. For example, although not shown, after the Ni layer 18c is formed thick on the entire surface, a mask is placed to cover both ends of the Ni layer 18c while leaving the center of the Ni layer 18c open, and the Ni layer 18c is etched to the middle of its thickness while being covered with the mask. In this manner, a structure in which both ends of the Ni layer 18c are thicker than the center can also be realized.

[0054] (Fourth embodiment) The fourth embodiment will be described. This embodiment is similar to the third embodiment except for the configuration of the Au layer 181, and therefore only the differences from the third embodiment will be described.

[0055] In the third embodiment, when the Ni layer 18c is formed by the lift-off method, the first layer 18ca of the Ni layer 18c is exposed when the first layer 18ca is formed. For this reason, as the process shown in FIG. 6A, a part of the Au layer 181 may be formed on the first layer 18ca, and then the resist 30 and the second layer 18cb may be formed, and then the remaining part of the Au layer 181 may be formed on the second layer 18cb. In this case, as the process shown in FIG. 6B after that, when the resist 30 is removed, the second layer 18cb and the remaining part of the Au layer 181 on the resist 30 may also be removed. In this way, the Au layer 181 may be formed on each of the first layer 18ca and the second layer 18cb.

[0056] Fifth embodiment A fifth embodiment will be described. This embodiment is similar to the first embodiment except that the configuration of the Ni layer 18c is changed, and therefore only the differences from the first embodiment will be described.

[0057] 7, in this embodiment, the Ni layer 18c has a substantially uniform thickness, is divided into a plurality of stripes in the resonance direction, and the width of the Ni layer 18c is wider at both ends than at the center. That is, the amount of the Ni layer 18c is greater at both ends than at the center.

[0058] Such a structure can be obtained by dividing the Ni layer 18c into multiple stripes in the resonance direction when forming the Ni layer 18c, as shown in FIG. 8, and then depositing an Au layer 181 on the Ni layer 18c to bond the element portion 4 side and the substrate 3 side.

[0059] Here, the Ni layer 18c is divided into multiple pieces in the resonance direction to form stripes. However, the shape is not limited to stripes and may be any shape. It is sufficient to provide an in-plane distribution in the Ni layer 18c so that the amount of Ni layer 18c distributed at both ends in the resonance direction is greater than that at the center.

[0060] Sixth embodiment The sixth embodiment will be described. This embodiment is the same as the fourth embodiment except that the configuration of the Ni layer 18c is changed as in the fifth embodiment, and other points are the same as in the fourth embodiment, so only the points different from the fourth embodiment will be described.

[0061] 9, in this embodiment, the Ni layer 18c has a substantially uniform thickness, is divided into a plurality of stripes in the resonance direction, and the width of the Ni layer 18c is wider at both ends than at the center. That is, the amount of the Ni layer 18c is greater at both ends than at the center.

[0062] Such a structure can be obtained by dividing the Ni layer 18c into multiple stripes in the resonance direction when forming the Ni layer 18c, as shown in FIG. 10, and then depositing an Au layer 181 on the Ni layer 18c to bond the element portion 4 side and the substrate 3 side.

[0063] Here, the Ni layer 18c is divided into multiple pieces in the resonance direction to form stripes. However, the shape is not limited to stripes and may be any shape. It is sufficient to provide an in-plane distribution in the Ni layer 18c so that the amount of Ni layer 18c distributed at both ends in the resonance direction is greater than that at the center.

[0064] (Other embodiments) Although the present disclosure has been described based on the above-described embodiment, it is not limited to the embodiment, and includes various modifications and modifications within the equivalent range. In addition, various combinations and forms, and other combinations and forms including only one element, more than one element, or less than one element, are also within the scope and concept of the present disclosure.

[0065] For example, in the above embodiment, not all of the metal layers constituting the p-type electrode 18 are necessary, and they may be provided as necessary, and the materials may be changed as appropriate. Similarly, the semiconductor materials constituting the element portion 4 and the base material 3 of the light-emitting element 2 are merely examples, and other semiconductor materials may be used. In particular, the active layer does not have to be made of GaAs or InP-based materials, and nitride-based semiconductor materials may also be used.

[0066] In addition, in each of the above embodiments, the first conductivity type is n-type, the second conductivity type is p-type, and the light emitting element substrate 11 side is n-type, but it may be p-type. That is, it is sufficient that the first clad layer 12 and the first guide layer 13 of the first conductivity type, the active layer 14, the second guide layer 15 and the second clad layer 16 of the second conductivity type, and the first electrode are formed in this order on the light emitting element substrate 11 of the first conductivity type, and joined to the second electrode formed on the base material 3 side. [Explanation of symbols]

[0067] 1...semiconductor light emitting device, 2...light emitting element, 3...substrate, 4...element portion, 10...n-type electrode 11...light emitting element substrate, 12...first cladding layer, 13...first guide layer 14...active layer, 15...second guide layer, 16...second cladding layer 17...contact layer, 18...p-type electrode, 18a...Ti layer, 18b...Pt layer 18c...Ni layer, 18ca...1st layer, 18cb...2nd layer, 18d...AuNiSn layer 18e...Au5Sn layer, 18f...AuSn layer, 18g...Pt layer, 18h...Ti layer, 30...resist, 181...Au layer, 182...AuSn layer, 183...Au layer

Claims

1. A semiconductor light emitting device, a light-emitting element (2) having a light-emitting element substrate (11) made of a semiconductor material of a first conductivity type, an element section (4) in which a first clad layer (12) of a first conductivity type, a first guide layer (13) of a first conductivity type, an active layer (14), a second guide layer (15) of a second conductivity type, and a second clad layer (16) of a second conductivity type are arranged in this order on one surface side of the light-emitting element substrate, a first conductivity type electrode (10) formed on the side of the light-emitting element substrate opposite the first clad layer, and a second conductivity type electrode (18) arranged on the side opposite the first conductivity type electrode with the element section in between, the light-emitting element (2) having one direction as a resonance direction and emitting light from at least one of both end faces in the resonance direction; A substrate (3) connected to the second conductivity type electrode, The second conductive type electrode has a junction structure between a first electrode arranged on the light-emitting element side and a second electrode arranged on the substrate side, and a junction layer (18d to 18f) between the first electrode and the second electrode contains at least Au, Sn and Ni, and the Ni concentration is higher at both ends in the resonance direction than in a central portion located further inward.

2. 2 . The semiconductor light emitting device according to claim 1 , wherein the bonding layer has a Ni concentration difference of 5 mol % or more between both ends and a center portion in the resonance direction.

3. The semiconductor light emitting device of claim 2 , wherein the first electrode comprises a Ni layer (18c).

4. The semiconductor light emitting device according to claim 3 , wherein the Ni layer is thicker at both ends in the resonance direction than at a central portion.

5. The semiconductor light emitting device according to claim 3 , wherein the Ni layer has a distribution amount greater at both ends in the resonance direction than at a central portion.

6. The semiconductor light emitting device of claim 2 , wherein the second electrode comprises a Ni layer (18c).

7. The semiconductor light emitting device according to claim 6 , wherein the Ni layer is thicker at both ends in the resonance direction than at a central portion.

8. The semiconductor light emitting device according to claim 6 , wherein the Ni layer has a distribution amount greater at both ends in the resonance direction than at a central portion.

9. 9. The semiconductor light emitting device according to claim 1, wherein said active layer is made of a nitride-based semiconductor material.

Citation Information

Patent Citations

  • Bonding method of semiconductor component

    JP1994177135A

  • Semiconductor laser element

    JP1994232502A

  • Bonding material and bonding method of electric element

    JP1996181392A

  • Semiconductor light emitting device

    JP2001244562A

  • Semiconductor laser device

    JP2004055938A