Laser welding method and laser welding apparatus
The laser welding method and apparatus use adjusted measurement light based on the laser's speed to accurately measure the keyhole bottom, addressing the challenge of determining penetration depth and maintaining the railway vehicle's aesthetic integrity.
Patent Information
- Application Number
- JP2023068698
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-19
- Publication Date
- 2024-10-31
AI Technical Summary
Existing laser welding methods struggle to accurately measure the penetration depth during continuous welding of railway vehicle components due to the distorted shape of the keyhole formed by the processing laser, which makes it difficult to determine if a sufficient penetration depth has been achieved without leaving visible welding marks on the outer surface.
A laser welding method and apparatus that adjusts the measurement light from optical coherence tomography based on the speed of the laser irradiation means, irradiating a predetermined scanning amount behind the processing laser to accurately measure the position of the keyhole bottom during continuous welding.
Enables precise measurement of the keyhole bottom position, ensuring adequate penetration depth without visible welding marks on the outer surface, thereby maintaining the design integrity of the railway vehicle.
Smart Images

Figure 2024154716000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a laser welding method and a laser welding apparatus for continuously welding base materials by using a processing laser irradiated by a laser irradiation means. [Background technology]
[0002] The outer plate constituting the outer surface of a railway vehicle has bone members, such as vertical bones extending along the vehicle height direction and horizontal bones extending along the track direction, joined to the inner surface (hereinafter, the back surface) of the railway vehicle. The bone members are generally joined to the outer plate by laser welding.
[0003] Specifically, for example, it is as shown in Fig. 7. Fig. 7 is a diagram showing a state in which a cross frame is joined to an outer plate. Note that Fig. 7 is a simplified diagram for the purpose of explanation, and does not represent the exact shape or size.
[0004] 7, a cross frame 52 (an example of a frame member) having a hat-shaped cross section extends on the back surface 51a of the outer plate 51, and a flange portion 52a of the cross frame 52 is joined to the back surface 51a of the outer plate 51 by laser welding. This laser welding is a continuous welding along the longitudinal direction of the cross frame 52 as shown by a welded portion 57, and is performed by irradiating a processing laser from the cross frame 52 side.
[0005] In order to ensure the strength of the welded portion 57, it is necessary to obtain a penetration depth that reaches the outer plate 51. However, if the laser irradiated from the back side of the outer plate 51 is irradiated so as to reach the surface opposite the back surface 51a of the outer plate 51, weld marks will remain on the surface of the outer plate 51. In other words, they will remain on the outer surface of the railway car. This will impair the design of the railway car, so when performing laser welding, it is necessary to perform welding so as to obtain a sufficient penetration depth while controlling so that the processing laser does not reach the surface of the outer plate 51.
[0006] However, if the processing laser is not allowed to reach the surface of the outer plate 51, it is not possible to determine from the outside whether a sufficient penetration depth has been obtained. Under such circumstances, whether a sufficient penetration depth has been obtained is determined by carrying out a non-destructive inspection or by using an optical coherence tomography method.
[0007] A method for determining whether or not a sufficient penetration depth is obtained using optical coherence tomography is disclosed in, for example, Patent Document 1. Here, the method for determining whether or not a sufficient penetration depth is obtained using the method disclosed in Patent Document 1 will be described with reference to Figs. 8 and 9. Fig. 8 is a diagram showing a state in which an outer plate 51 and a cross frame 52 (flange portion 52a) placed on the outer plate 51 are welded together by a processing laser L11 irradiated from a laser irradiation means 200 according to the conventional technology. Fig. 9 is a cross-sectional view taken along the line B-B of Fig. 8.
[0008] Both the outer plate 51 and the cross frame 52 are made of austenitic stainless steel, and the thickness of the outer plate 51 is about 2 mm, and the thickness of the cross frame 52 (flange portion 52a) is about 1.5 mm. Arrow Y in FIG. 8 indicates the direction of travel of the continuous welding, and the laser irradiation means 200 performs continuous welding by moving in the direction of arrow Y while irradiating the processing laser L11. The laser irradiation means 200 irradiates the processing laser L11 to the outer plate 51 and the cross frame 52 from the cross frame 52 side. The irradiation of the processing laser L11 melts the outer plate 51 and the cross frame 52, generating a molten material 55. The molten material 55 further evaporates to generate a keyhole 54. A weld bead 56 formed by solidifying the molten material 55 is formed on the opposite side of the keyhole 54 in the traveling direction.
[0009] Furthermore, the laser irradiation means 200 outputs the measurement light L31 by optical coherence tomography on the same axis as the processing laser L11, thereby irradiating the bottom 54a of the keyhole 54. This makes it possible to measure the position (distance d1) of the bottom 54a of the keyhole 54. Furthermore, the laser irradiation means 200 irradiates the measurement light L32 by optical coherence tomography on the surface 52b of the rib 52 (flange portion 52a). This makes it possible to measure the position (distance d2) of the surface 52b of the rib 52 (flange portion 52a). Then, the penetration depth d21 of the processing laser L11 is calculated from the difference between the position (distance d1) of the bottom 54a and the position (distance d2) of the surface 52b. Since the penetration depth d21 of this laser can be regarded as the same as the penetration depth d31 in FIG. 9, by calculating the penetration depth d21 of the processing laser L11 and checking the value, it is possible to determine whether or not a sufficient penetration depth d31 has been obtained. [Prior art documents] [Patent documents]
[0010] [Patent Document 1] Special Publication No. 2016-538134 Summary of the Invention [Problem to be solved by the invention]
[0011] As described above, the laser irradiation means 200 performs welding while moving in the direction of the arrow Y. In this case, the shape of the keyhole is not a simple cone shape as shown in Fig. 8, but is distorted into a substantially arch shape as shown in Fig. 10. Fig. 10 illustrates an example of the shape of the keyhole when the laser irradiation means 200 according to the conventional technology performs welding while moving.
[0012] When the laser irradiation means 200 performs welding while moving, the bottom 54a of the keyhole 54 is located behind the irradiation part irradiated with the processing laser L11 in the traveling direction. More specifically, the bottom 54a is located behind the axis A11 of the processing laser L11 in the traveling direction. For this reason, if the measurement light L31 is irradiated coaxially with the processing laser L11, the position of the bottom of the keyhole 54 may not be accurately measured. In other words, the penetration depth d21 and the penetration depth d31 of the processing laser L11 may not be accurately calculated.
[0013] The present invention has been made to solve the above problems, and has an object to provide a laser welding method and laser welding apparatus that are capable of accurately measuring the position of the bottom of a keyhole created by irradiation with a processing laser. [Means for solving the problem]
[0014] In order to solve the above problems, the laser welding method of the present invention has the following configuration.
[0015] This laser welding method performs continuous welding of base materials by a processing laser irradiated by a laser irradiation means, and is characterized in that, while the continuous welding is being performed, measurement light using optical coherence tomography is irradiated rearward in the direction of progression of the continuous welding from the irradiation point of the processing laser with a predetermined scanning amount corresponding to the movement speed of the laser irradiation means, thereby measuring the position of the bottom of a keyhole created by the irradiation of the processing laser.
[0016] In order to solve the above problems, the laser welding apparatus of the present invention has the following configuration.
[0017] A laser welding apparatus for continuously welding a base material with a processing laser, comprising: a laser irradiation means for irradiating the processing laser; a driving means for moving the laser irradiation means; an optical interferometer for generating measurement light by optical coherence tomography; a scanning means for scanning the measurement light; and a control device having a control program for controlling the laser welding apparatus, wherein the control program irradiates the processing laser with the laser irradiation means, moves over the base material with the driving means to perform the continuous welding, generates the measurement light from the optical interferometer, and irradiates the measurement light rearward in the direction of progression of the continuous welding from the irradiation portion of the processing laser with a predetermined scanning amount according to the speed of movement of the laser irradiation means with the scanning means, and measures the position of a bottom of a keyhole created by the irradiation of the processing laser.
[0018] According to the above-mentioned laser welding method or the above-mentioned laser welding device, the measurement light by optical coherence tomography is irradiated with a predetermined scanning amount to the rear of the irradiation part of the processing laser in the traveling direction of the continuous welding, so that the measurement light can be irradiated to the bottom of the keyhole located on the rear side of the irradiation part of the processing laser in the traveling direction. Therefore, it is possible to accurately measure the position of the bottom of the keyhole while performing the continuous welding while moving the laser irradiation means.
[0019] The above-mentioned predetermined scanning amount depends on the moving speed of the laser irradiation means. Specifically, since the distance between the irradiation part of the processing laser and the position of the bottom of the keyhole increases or decreases depending on the moving speed of the laser irradiation means, it is desirable to use a value obtained by experiment in advance.
[0020] Furthermore, in the above-mentioned laser welding method or laser welding apparatus, it is preferable that a start position and an end position of the continuous welding are located on the base material, and that the scanning amount is a first predetermined amount in a steady state in which the laser irradiation means moves at a constant speed, and is a second predetermined amount smaller than the first predetermined amount in a low-speed state in which the laser irradiation means moves at a speed slower than that of the steady state.
[0021] Furthermore, in the above-mentioned laser welding method or laser welding apparatus, it is preferable that the low-speed state includes an acceleration state in which the laser irradiation means starts moving from a state in which it is stopped at the start position toward the end position and accelerates until it reaches the steady state, and a deceleration state in which the laser irradiation means decelerates from the steady state until it is stopped at the end position.
[0022] In the above-described laser welding method or laser welding apparatus, it is preferable that, in the accelerated state, the scanning amount gradually increases from the second predetermined amount to the first predetermined amount.
[0023] In the above-described laser welding method or laser welding apparatus, it is preferable that, in the decelerating state, the scanning amount gradually decreases from the first predetermined amount to the second predetermined amount.
[0024] According to the above-mentioned laser welding method or laser welding device, even if there is a fluctuation in the moving speed (e.g., acceleration or deceleration) while the laser irradiation means is moving to perform continuous welding, it is possible to accurately measure the position of the bottom of the keyhole. This will be described in detail below.
[0025] When continuous welding is performed by passing the laser irradiation means over the base material to be welded at a constant speed, the position of the bottom of the keyhole can be measured by giving a constant value that matches the passing speed as the scanning amount. This is because the distance between the irradiation part of the processing laser and the position of the bottom of the keyhole increases and decreases depending on the moving speed of the laser irradiation means, but when the laser irradiation means passes over the workpiece at a constant speed, the variation in the distance between the irradiation part of the processing laser and the bottom of the keyhole is small.
[0026] However, when the start and end positions of continuous welding exist on the base material, there is a risk that the position of the bottom of the keyhole cannot be accurately measured by giving a constant value as the scanning amount. Here, the start position of continuous welding is the point where the laser irradiation means starts moving from a stopped state while irradiating the processing laser, and the end position is the point where the movement is stopped.
[0027] If there are a start position and an end position on the base material, the laser irradiation means is stopped at the start position. When continuous welding is started from there, the laser irradiation means starts to move toward the end position. In other words, it starts to accelerate. When it reaches a predetermined speed through this acceleration, it enters a steady state where it moves at a constant speed. Then, as it approaches the end position, the laser irradiation means starts to decelerate and stops at the end position. In other words, the speed at which the laser irradiation means moves on the workpiece varies.
[0028] The shape of the keyhole depends on the speed of movement of the laser irradiation means (the speed at which welding is performed), and the distance between the irradiation point of the processing laser and the bottom of the keyhole differs between the steady state where the laser irradiation means moves at a constant speed and the accelerating and decelerating states (collectively referred to as the low-speed state).
[0029] Therefore, if a constant value is given as the scanning amount, there is a problem that the position of the bottom of the keyhole cannot be measured accurately. Specifically, for example, if a value suitable for a steady state is given as the scanning amount, the position of the bottom of the keyhole can be measured in the steady state, but accurate measurement cannot be performed in the low speed state. Also, if a value suitable for a low speed state is given as the scanning amount, the position of the bottom of the keyhole can be measured in the low speed state, but accurate measurement cannot be performed in the steady state.
[0030] The above problem is particularly prominent when welding the outer plate 51 and the cross frame 52 of a railway vehicle. This is because, in order to join the outer plate 51 and the cross frame 52 while minimizing the gap between them as much as possible, continuous welding is generally performed while pressing the cross frame 52 against the outer plate 51 with a pressing means such as a roller provided in the laser irradiation means, and therefore, in some cases, the start and end positions of the continuous welding are set on the cross frame 52.
[0031] In such a situation, according to the above-mentioned laser welding method or laser welding device, the scanning amount is a first predetermined amount in a steady state where the laser irradiation means moves at a constant speed, and is a second predetermined amount smaller than the first predetermined amount when the laser irradiation means moves at a slower speed than the steady state (for example, an accelerating or decelerating state), so that the irradiation position of the measurement light varies depending on whether the laser irradiation means is in a steady state or a slow state. Therefore, even if there is a variation in the moving speed of the laser irradiation means while performing continuous welding while moving, it is possible to accurately measure the position of the bottom of the keyhole.
[0032] In addition, if the scanning amount gradually increases from the second predetermined amount to the first predetermined amount in the accelerating state and gradually decreases from the first predetermined amount to the second predetermined amount in the decelerating state, it is possible to measure the position of the bottom of the keyhole more accurately while the laser irradiation means is accelerating or decelerating. Note that the gradual increase may be a linear increase over time or a stepwise increase. Similarly, the gradual decrease may be a linear decrease over time or a stepwise decrease. Effect of the Invention
[0033] According to the laser welding method and laser welding apparatus of the present invention, it is possible to accurately measure the position of the bottom of a keyhole created by irradiation with a processing laser. [Brief description of the drawings]
[0034] [Figure 1]FIG. 1 is a diagram showing a schematic configuration of a laser welding device. [Diagram 2] 10A to 10C are diagrams showing the process of continuous welding from a start point position on an outer plate and a cross beam to an end point position using the laser welding device according to the present embodiment over time. [Diagram 3] 11A and 11B are diagrams showing the shape of a keyhole immediately after a welding head in this embodiment starts moving from a start position or immediately before the welding head stops at an end position. [Figure 4] 11 is a diagram showing the shape of a keyhole when a welding head in this embodiment is in a steady state. FIG. [Diagram 5] Fig. 5(A) is a graph showing the relationship between the intensity of the processing laser and time. Fig. 5(B) is a graph showing the relationship between the moving speed of the welding head and time. Fig. 5(C) is a graph showing the relationship between the scanning amount of the measurement light and time. Fig. 5(D) is a graph showing the relationship between the ON and OFF of the synchronization signal and time. Fig. 5(E) is a graph showing the relationship between the ON and OFF of the measurement of the bottom position and time. [Figure 6] Fig. 6(A) is a cross-sectional photograph of a weld bead when continuous welding is performed from the start position to the end position by the laser welding device according to this embodiment. Fig. 6(B) is a graph plotting measured values when the scanning amount of the measurement light is kept constant at a second predetermined amount from the start position to the end position. Fig. 6(C) is a graph plotting measured values when the scanning amount of the measurement light is kept constant at a first predetermined amount from the start position to the end position. Fig. 6(D) is a graph plotting values measured by the measurement light in this embodiment. [Figure 7] FIG. 13 is a diagram showing the state in which a cross frame is joined to an outer panel. [Figure 8] FIG. 1 is a diagram showing a state in which an outer plate and a cross frame are welded together by a laser emitted from a laser welding device according to a conventional technology. [Figure 9] 9 is a cross-sectional view of FIG. 8 taken along line B-B. [Figure 10] 1 illustrates an example of a keyhole shape when a laser irradiation means according to a conventional technique performs welding while moving. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0035] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS An embodiment of a laser welding method and a laser welding apparatus according to the present invention will be described in detail with reference to the drawings.
[0036] (About the configuration of laser welding equipment) First, the configuration of the laser welding device 1 according to the present embodiment will be described. FIG. 1 is a diagram showing a schematic configuration of the laser welding device 1. The laser welding device 1 is used, for example, to overlap and join an outer plate 51 (an example of a base material) and a cross frame 52 (an example of a base material) of a railway vehicle as shown in FIG. 7. Specifically, the cross frame 52 is placed overlapping on the outer plate 51, and the welding head 10 performs continuous welding by moving over the cross frame 52 while irradiating the processing laser L11 from the side of the cross frame 52, thereby joining the outer plate 51 and the cross frame 52. Both the outer plate 51 and the cross frame 52 are made of austenitic stainless steel. The thickness of the outer plate 51 is not particularly limited, but is, for example, about 2 mm. The thickness of the cross frame 52 is not particularly limited, but is, for example, about 1.5 mm.
[0037] The surface of the outer plate 51 facing the inside of the railway vehicle is the back surface 51a, and a cross frame 52 having a hat-shaped cross section extends on this back surface 51a, for example, along the track direction. A flange portion 52a of this cross frame 52 is joined to the back surface 51a of the outer plate 51 by laser welding. This laser welding is continuous welding along the longitudinal direction of the cross frame 52. The continuous welding is performed, for example, by irradiating a processing laser L11 from the side of the cross frame 52 with a laser welding device 1 in a state where the cross frame 52 is placed on the outer plate 51, as shown in FIG.
[0038] The laser welding apparatus 1 includes a welding head 10 (one example of a laser irradiation means), a laser light source 2, and an optical interferometer 3. The laser welding apparatus 1 also includes a driving means (not shown) for moving the welding head 10, and the driving means can perform continuous welding while linearly moving the welding head 10, for example, along a guide or the like. Note that the arrow Y in the figure indicates the direction in which the continuous welding proceeds. The laser welding apparatus 1 is also electrically connected to a control device (not shown), and the operations of the welding head 10, the laser light source 2, the optical interferometer 3, the driving means, and the like are controlled by a control program stored in the control device.
[0039] The welding head 10 includes a laser incidence section 11. The laser light source 2 is connected to the laser incidence section 11 through an optical fiber 27. The processing laser L11 output from the laser light source 2 is incident on the welding head 10 from the laser incidence section 11 through the optical fiber 27. The incident processing laser L11 is collimated by the first collimator lens 12. The collimated processing laser L11 is reflected by the first dichroic mirror 13, and the traveling direction is changed by 90 degrees. After that, the processing laser L11 is focused by the focus lens 15 and output from the welding head 10, and is irradiated to the outer plate 51 and the cross beam 52. The focus lens 15 can be moved in the axial direction (up and down in FIG. 1). This makes it possible to change the focal position of the processing laser L11 in the axial direction (up and down in FIG. 1).
[0040] The processing laser L11 output from the welding head 10 melts and vaporizes the outer plate 51 and the cross frame 52 around the processing laser L11, forming a keyhole 54 (see FIG. 2) in the outer plate 51 and the cross frame 52. The keyhole 54 is surrounded by a molten material 55 (see FIG. 2) formed by melting the outer plate 51 and the cross frame 52, and the molten material 55 solidifies as the distance from the focus of the processing laser L11 increases. Therefore, a weld bead 56 (see FIG. 2) formed by solidifying the molten material 55 is formed on the opposite side to the progression direction of the continuous welding (the direction of the arrow Y).
[0041] The welding head 10 also includes a measurement light incident section 19. The optical interferometer 3 is connected to the measurement light incident section 19 via an optical fiber 29. The measurement light L21 output from the optical interferometer 3 is incident on the welding head 10 from the measurement light incident section 19 through the optical fiber 29. The incident measurement light L21 is collimated by the second collimator lens 21. The collimated measurement light L21 is reflected by the second dichroic mirror 23, and its traveling direction is changed by approximately 90 degrees. Thereafter, the measurement light L21 passes through the first dichroic mirror 13, is focused by the focus lens 15, and is output from the welding head 10. As a result, the measurement light L21 is irradiated onto the portions of the outer plate 51 and the cross beam 52 to be measured. The portions to be measured are at least the bottom 54a of the keyhole 54 (see FIGS. 2 to 4). The irradiated measurement light L21 is reflected by the area to be measured, returns to the measurement light incident section 19 via the first dichroic mirror 13 and the second dichroic mirror 23, and enters the optical interferometer 3 through the optical fiber 29.
[0042] The optical interferometer 3 uses, for example, a technique called swept source optical coherence tomography (SS-OCT), which is one of the optical coherence tomography techniques, and can measure the optical path length of the measurement light L21 and measure the position of the part to be measured based on the measured optical path length. Note that the optical interferometer 3 is not limited to one that uses the SS-OCT technique, and may use a technique called Spectral domain optical coherence tomography (SD-OCT) or Time domain optical coherence tomography (TD-OCT).
[0043] The welding head 10 also includes a scanning means 25 for swinging the second dichroic mirror 23. The scanning means 25 swings the second dichroic mirror 23 to scan the measurement light L21 and vary the irradiation position. As a result, the measurement light L21 is irradiated backward in the advancing direction of the continuous welding from the irradiation portion of the processing laser L11 with a predetermined scanning amount set according to the amount of positional deviation (details will be described later).
[0044] In addition, a protective lens 17 is attached to the welding head 10 in order to protect the inside of the welding head 10 from spatters and fumes that are generated when the outer plate 51 and the cross frame 52 are laser-welded.
[0045] (About continuous welding) The continuous welding performed using the above-described laser welding apparatus 1 will be described with reference to Fig. 2. Fig. 2 is a diagram showing the state over time of continuous welding from a start position P11 on an outer plate 51 and a cross frame 52 to an end position P12 using the laser welding apparatus 1 according to this embodiment.
[0046] In this embodiment, continuous welding is performed by moving the welding head 10 over the outer plate 51 and the cross frame 52 from a start position P11 to an end position P12 while irradiating the cross frame 52 with a processing laser L11.
[0047] When performing continuous welding from start position P11 to end position P12, welding head 10 starts moving from a state stopped at start position P11 toward end position P12. When welding head 10 starts moving, it enters an acceleration state in which it accelerates to a predetermined speed V11 (see FIG. 5(B)). Then, when welding head 10 reaches the predetermined speed V11, it enters a steady state in which it moves at a constant speed V11. Then, as welding head 10 approaches end position P12, it enters a deceleration state in which the moving speed is decelerated, and it is stopped at end position P12. Note that the acceleration state and deceleration state are states in which the moving speed of welding head 10 is slower than the steady state, so hereinafter, the acceleration state and deceleration state may be collectively referred to as a low-speed state.
[0048] The speed V11 is not particularly limited, but is, for example, 6 m / min. The time during which the accelerated state continues is appropriately set according to the value of the speed V11, but in this embodiment, the accelerated state continues for 0.5 seconds. That is, it is set so that the moving speed reaches 6 m / min 0.5 seconds after the welding head 10 starts moving. The time during which the decelerated state continues is also appropriately set according to the value of the speed V11, but in this embodiment, the decelerated state continues for 0.5 seconds. That is, the welding head 10 enters a decelerated state 0.5 seconds before reaching the end position P12, and the moving speed of the welding head 10 changes from 6 m / min to a stopped state in 0.5 seconds. The distance from the start position P11 to the end position P12 is not particularly limited, but is, for example, about 6 m.
[0049] As described above, when welding is performed while the welding head 10 moves in the direction of the arrow Y, the shape of the keyhole 54 becomes distorted into a substantially arched shape, and the position of the bottom 54a of the keyhole 54 is located behind the irradiation part of the processing laser L11 in the traveling direction of the continuous welding. Specifically, the position of the bottom 54a is located behind the axis A11 of the processing laser L11 in the traveling direction of the continuous welding. Hereinafter, the distance of the bottom 54a from the axis A11 in the traveling direction of the continuous welding is referred to as the positional deviation amount.
[0050] The amount of positional deviation varies depending on the moving speed of the welding head 10. Specifically, please refer to the shape of the keyhole 54 shown in Figures 3 and 4. Note that the shape of the keyhole 54 shown in Figures 3 and 4 is a schematic representation of the results obtained experimentally. Specifically, the measurement light was scanned forward and backward in the direction of travel of the continuous welding while performing the continuous welding as shown in Figure 2, and the measurement light was obtained.
[0051] 3 is a diagram showing the shape of the keyhole 54 immediately after the welding head 10 in this embodiment starts moving from the starting position P11 or immediately before stopping at the ending position P12. The bottom 54a is located behind the axis A11 of the processing laser L11, and the positional deviation D11 at this time varies depending on the speed of the welding head 10 in the steady state, the duration of the acceleration state and the deceleration state, etc., but is about 0.05 mm in this embodiment.
[0052] As the moving speed increases, the distortion of the keyhole 54 increases, and the amount of misalignment also increases. Fig. 4 is a diagram showing the shape of the keyhole 54 when the welding head 10 in this embodiment is in a steady state. The steady state is a state in which the amount of misalignment is the largest during the continuous welding shown in Fig. 2, and the amount of misalignment D12 at this time varies depending on the speed of the welding head 10 in the steady state, but is about 0.25 mm in this embodiment.
[0053] The continuous welding shown in FIG. 2 is performed by the control program controlling the laser welding device 1 as shown in FIG. 5. FIG. 5(A) is a graph showing the relationship between the intensity of the processing laser L11 and time. FIG. 5(B) is a graph showing the relationship between the moving speed of the welding head 10 and time. FIG. 5(C) is a graph showing the relationship between the scanning amount of the measurement light L21 and time. FIG. 5(D) is a graph showing the relationship between the ON and OFF of the synchronization signal and time. The synchronization signal is a signal for instructing the timing to start gradually increasing and gradually decreasing the scanning amount of the measurement light L21 (the gradual increase and gradual decrease will be described later). FIG. 5(E) is a graph showing the relationship between the ON and OFF of the measurement of the position of the bottom 54a and time. In FIG. 5, the continuous welding starts at time t1 and is completed at time t4, and the period from time t1 to time t2 corresponds to the acceleration state, the period from time t2 to time t3 corresponds to the steady state, and the period from time t3 to time t4 corresponds to the deceleration state.
[0054] First, from time t0, which is before time t1 when continuous welding starts, measurement of the position of the bottom 54a is turned ON as shown in Fig. 5(E). This causes the optical interferometer 3 to generate measurement light L21, and irradiation of the measurement light L21 from the welding head 10 begins. However, at this point, irradiation of the processing laser L11 has not started and the keyhole 54 has not been formed, so that the measurement of the position of the bottom 54a being ON at this point does not mean that measurement is currently being performed, but rather means that the laser welding device 1 is in a state where it can measure the position of the bottom 54a.
[0055] 5(C), at time t0, the scanning amount of the measurement light L21 is set to a value S11 (an example of a second predetermined amount). That is, the measurement light L21 is irradiated rearward in the advancing direction of the continuous welding from the irradiation portion of the processing laser L11 by the amount of this value S11. Note that, since the irradiation of the processing laser L11 has not started at time t0, the measurement light L21 is irradiated rearward by the amount of the value S11 from the position of the axis A11 when the processing laser L11 is irradiated.
[0056] The value of the scanning amount S11 corresponds to the positional deviation amount D11 (see FIG. 3) experimentally obtained in advance, and is set before the start of continuous welding. In this embodiment, the value S11 is set to 0.05 mm, which corresponds to the positional deviation amount D11 being about 0.05 mm. The interval from time t0 to time t1 is not particularly limited, but is, for example, about 0.1 seconds.
[0057] Next, from time t1, the synchronization signal is turned ON (see FIG. 5(D)). This starts continuous welding. That is, the welding head 10 starts emitting the processing laser L11, starts moving from the start position P11 in the direction of the arrow Y, and enters an accelerating state.
[0058] Specifically, the processing laser L11 is generated from the laser light source 2, and the processing laser L11 is irradiated onto the outer plate 51 and the cross frame 52 from the cross frame 52 side. At this time, the focus position of the processing laser L11 is adjusted by the focus lens 15 according to the target value of the penetration depth of the processing laser L11 into the outer plate 51 and the cross frame 52. Then, as shown in FIG. 5(A), the intensity of the processing laser L11 is linearly increased with time, and as shown in FIG. 5(B), the moving speed of the welding head 10 is accelerated toward the speed V11. The reason for gradually increasing the intensity of the processing laser L11 is that if the intensity of the processing laser L11 is increased while the moving speed of the welding head 10 is slow, excessive penetration into the outer plate 51 and the cross frame 52 may occur.
[0059] Furthermore, the synchronous signal is turned ON, and the gradual increase of the scanning amount is started. Specifically, as shown in FIG. 5(C), the scanning amount is gradually increased linearly from the value S11 to the value S12 (one example of the first predetermined amount). That is, as the moving speed of the welding head 10 increases, the position where the measuring light L21 is irradiated moves away from the axis A11 of the processing laser L11 to the opposite side of the traveling direction. Here, the value S12 of the scanning amount is a value corresponding to the positional deviation amount D12 (see FIG. 4) experimentally obtained in advance, and is a value set before the start of continuous welding. In this embodiment, the value S12 is set to 0.25 mm corresponding to the positional deviation amount D12 being about 0.25 mm.
[0060] As the moving speed of the welding head 10 increases, the amount of positional deviation gradually increases, but by gradually increasing the scanning amount linearly, it is possible to irradiate the bottom 54a with the measurement light L21 so as to follow the bottom 54a where the amount of positional deviation increases, even when the welding head 10 is in an accelerating state. Therefore, it is possible to accurately measure the position of the bottom 54a, even when the welding head 10 is in an accelerating state.
[0061] Next, at time t2, as shown in FIG. 5(A), the intensity of the processing laser L11 reaches a maximum intensity W11, and as shown in FIG. 5(B), the moving speed of the welding head 10 reaches a speed V11 and enters a steady state. The value of the maximum intensity W11 is appropriately set based on the target value of the penetration depth of the processing laser L11 into the outer plate 51 and the cross frame 52. As the welding head 10 enters the steady state, the scanning amount reaches a value S12, as shown in FIG. 5(C). While the steady state continues, the scanning amount is constant at the value S12. In the steady state, the fluctuation of the positional deviation amount is small, so that the position of the bottom 54a can be sufficiently measured even if the scanning amount is constant at the value S12.
[0062] Next, at time t3, the synchronization signal is turned OFF (see FIG. 5(D)). This causes the welding head 10 to enter a deceleration state. Specifically, the welding head 10, which had been moving at a speed V11, slows down over time in order to stop at the end position P12, as shown in FIG. 5(B). In conjunction with this, the intensity of the processing laser L11 is reduced over time, as shown in FIG. 5(A).
[0063] Furthermore, the synchronous signal is turned OFF, and the gradual decrease in the scanning amount starts. Specifically, as shown in Fig. 5(C), the scanning amount is gradually decreased linearly from value S12 to value S11. In other words, as the moving speed of the welding head 10 becomes slower, the position irradiated with the measuring light L21 approaches the axis A11 of the processing laser L11 from the opposite side of the traveling direction.
[0064] As the moving speed of the welding head 10 slows down, the amount of positional deviation gradually decreases, but by gradually decreasing the scanning amount linearly, it is possible to irradiate the bottom 54a with the measurement light L21 so as to follow the bottom 54a where the amount of positional deviation becomes smaller. Therefore, even if the welding head 10 is in a decelerating state, it is possible to accurately measure the position of the bottom 54a.
[0065] Next, at time t4, the moving speed of the welding head 10 becomes zero and the welding head 10 stops at the end position P12, and the intensity of the processing laser L11 becomes zero and the irradiation is stopped. This completes the continuous welding. At this point, the measurement of the position of the bottom 54a is ON as shown in FIG. 5(E), and the welding head 10 is in a state of irradiating the measurement light L21 with the scanning amount set to value S11. Then, at time t5, the measurement of the position of the bottom 54a is turned OFF. In other words, the irradiation of the measurement light L21 is stopped. The interval from time t4 to time t5 is not particularly limited, but is, for example, about 0.1 seconds.
[0066] The result of measuring the position of the bottom 54a by the measuring light L21 while performing continuous welding as described above will be described with reference to FIG. 6. FIG. 6(A) is a cross-sectional photograph of a weld bead 56 when continuous welding is performed from the start position P11 to the end position P12 by the laser welding device 1 according to this embodiment. The "acceleration region" shown in FIG. 6(A) means the region where continuous welding is performed when the welding head 10 is in an accelerating state, the "steady region" means the region where continuous welding is performed when the welding head 10 is in a steady state, and the "deceleration region" means the region where continuous welding is performed when the welding head 10 is in a deceleration state. FIG. 6(B) is a graph plotting the measured values when the scanning amount of the measuring light L21 is constant at a value S11 from the start position P11 to the end position P12. FIG. 6(C) is a graph plotting the measured values when the scanning amount of the measuring light L21 is constant at a value S12 from the start position P11 to the end position P12. 6(D) is a graph plotting values measured by the measurement light L21 in this embodiment. That is, in the acceleration state, the scanning amount of the measurement light L21 is gradually increased from value S11 to value S12, in the steady state, the scanning amount of the measurement light L21 is set to value S12, and in the deceleration state, the scanning amount of the measurement light L21 is gradually decreased from value S12 to value S11, and the graph plots the measured values.
[0067] The continuous welding described above has been explained assuming that there is a start position P11 and an end position P12 of the continuous welding on the outer plate 51 and the cross frame 52. However, if there is no start position P11 and end position P12 of the continuous welding on the outer plate 51 and the cross frame 52, and continuous welding is performed by the welding head 10 passing over the outer plate 51 and the cross frame 52 at a constant speed (i.e., if continuous welding is performed while passing over the outer plate 51 and the cross frame 52 in a steady state), the position of the bottom 54a of the keyhole 54 can be measured by setting a constant value that matches the passing speed as the scanning amount. For example, if passing at 6 m / min, the scanning amount can be set to 0.25 mm, and the position of the bottom 54a can be measured during continuous welding.
[0068] However, if there is a start position P11 and an end position P12 on the outer plate 51 and the cross frame 52, the amount of positional deviation of the bottom 54a varies as the moving speed of the welding head 10 varies from an accelerating state to a steady state to a decelerating state, as already explained in Figures 2 and 3. Therefore, in this case, if a constant value is given as the scanning amount, the position of the bottom 54a of the keyhole 54 cannot be accurately measured. Specifically, this is as shown in Figures 6(B) and 6(C).
[0069] As shown in FIG. 6B, when the scanning amount of the measurement light L21 is constant at value S11 from the start position P11 to the end position P12, in the region where the speed of the welding head 10 is relatively slow at the beginning of the acceleration region and the end of the deceleration region (hereinafter referred to as the start and end region of the low speed state), the measured values are plotted in a form that follows the shape of the lower end of the weld bead 56 shown in FIG. 6A, so that it can be said that the position of the bottom 54a of the keyhole 54 can be accurately measured. This is because when the welding head 10 is in a relatively slow state at the start and end region of the low speed state (the start of the acceleration state or the end of the deceleration state), the positional deviation amount of the bottom 54a of the keyhole 54 matches the value S11 of the scanning amount, and the measurement light L21 can be irradiated to the bottom 54a. On the other hand, it can be said that accurate measurement cannot be performed in the region other than the start and end region of the low speed state and in the steady region. This is thought to be because when the welding head 10 is in a relatively fast state in areas other than the start and end areas of the low speed state and in the steady area, the amount of positional deviation of the bottom 54a of the keyhole 54 is greater than when the welding head 10 is in the start and end areas of the low speed state, so the scanning amount S11 is not sufficient and the measurement light L21 cannot be irradiated to the bottom 54a.
[0070] Also, as shown in Fig. 6C, when the scanning amount of the measurement light L21 is constant at value S12 from the start position P11 to the end position P12, in the region other than the start and end region of the low speed state and in the steady state region, the measured values are plotted in a form that follows the shape of the lower end of the weld bead 56 shown in Fig. 6A, so it can be said that the position of the bottom 54a of the keyhole 54 can be accurately measured. This is because when the welding head 10 is in the region other than the start and end region of the low speed state and in the steady state, the positional deviation amount of the bottom 54a of the keyhole 54 matches the scanning amount value S12, and the measurement light L21 can be irradiated to the bottom 54a. On the other hand, it can be said that the measurement cannot be accurately measured in the start and end region of the low speed state (the beginning of the acceleration region and the end of the deceleration region). This is thought to be because when the welding head 10 is in a region where the speed of the welding head 10 is relatively slow in the start and end region of the low speed state (the beginning of the acceleration state or the end of the deceleration state), the amount of positional deviation of the bottom 54a of the keyhole 54 is smaller than when the welding head 10 is in a region other than the start and end region of the low speed state or in a steady region where the speed of the welding head 10 is relatively fast, so the scanning amount S12 is too large and the measurement light L21 cannot be irradiated to the bottom 54a.
[0071] As described above, in the case where the scanning amount is set constant, in the acceleration state, the scanning amount of the measurement light L21 is gradually increased from value S11 to value S12, in the steady state, the scanning amount of the measurement light L21 is set to value S12, and in the deceleration state, the scanning amount of the measurement light L21 is gradually decreased from value S12 to value S11, it can be seen that the measured values are plotted in a manner that follows the shape of the lower end portion of the weld bead 56 shown in Fig. 6(A) in all regions, the acceleration region, the steady region, and the deceleration region, as shown in Fig. 6(D). Therefore, it can be said that the position of the bottom 54a of the keyhole 54 can be accurately measured from the start position P11 to the end position P12.
[0072] In this way, by varying the scanning amount, i.e., the irradiation position of the measurement light L21, depending on whether the welding head 10 is in a steady state or a low-speed state, it is possible to accurately measure the position of the bottom 54a of the keyhole 54.
[0073] As described above, the laser welding method of this embodiment is a laser welding method for continuously welding base materials (e.g., outer plate 51 and cross beams 52) using a processing laser L11 irradiated by a laser irradiation means (e.g., welding head 10), and is characterized in that, while the continuous welding is being performed, measurement light L21 using optical coherence tomography is irradiated rearward in the direction of progression of the continuous welding from the irradiation point of the processing laser L11 with a predetermined scanning amount (e.g., value S11 or value S12) corresponding to the speed of movement of the laser irradiation means (welding head 10), thereby measuring the position of the bottom 54a of the keyhole 54 created by the irradiation of the processing laser L11.
[0074] As described above, the laser welding apparatus 1 according to this embodiment, which performs continuous welding of base materials (e.g., an outer plate 51 and a cross beam 52) by a processing laser L11, includes a laser irradiation means (e.g., a welding head 10) for irradiating the processing laser L11, a driving means for moving the laser irradiation means (welding head 10), an optical interferometer 3 for generating measurement light L21 by optical coherence tomography, a scanning means 25 for scanning the measurement light L21, and a control device having a control program for controlling the laser welding apparatus 1, and the control program The present invention is characterized in that while the laser irradiation means (welding head 10) irradiates the processing laser L11, the driving means moves over the base material (outer plate 51 and cross frame 52) to perform continuous welding, the optical interferometer 3 generates measurement light L21, and the scanning means 25 irradiates the measurement light L21 with a predetermined scanning amount (e.g., value S11 or value S12) according to the speed of movement of the laser irradiation means (welding head 10) rearward of the irradiation point of the processing laser L11 in the direction of progression of the continuous welding, thereby measuring the position of the bottom 54a of the keyhole 54 created by the irradiation of the processing laser L11.
[0075] According to the above-mentioned laser welding method or the above-mentioned laser welding device 1, the measurement light L21 by optical coherence tomography is irradiated with a predetermined scanning amount (value S11 or value S12) rearward in the advancing direction of the continuous welding from the irradiation part of the processing laser L11, so that the measurement light L21 can be irradiated to the bottom 54a of the keyhole 54 located rearward in the advancing direction from the irradiation part of the processing laser L11. Therefore, while the laser irradiation means (welding head 10) is moving and performing the continuous welding, it is possible to accurately measure the position of the bottom 54a of the keyhole 54.
[0076] The above-mentioned predetermined scanning amount (value S11 or value S12) corresponds to the moving speed of the laser irradiation means. Specifically, the shape of the keyhole 54 changes depending on the moving speed (welding speed) of the laser irradiation means (welding head 10), and the distance between the irradiation part of the processing laser L11 and the position of the bottom 54a of the keyhole 54 (for example, the positional deviation amount D11 or the positional deviation amount D12) increases or decreases depending on the moving speed of the laser irradiation means (welding head 10), so it is desirable to use a value obtained in advance by experiment.
[0077] Furthermore, in the above-mentioned laser welding method or laser welding apparatus 1, when there is a start position P11 and an end position P12 of continuous welding on the base material (outer plate 51 and cross frame 52), it is preferable that the scanning amount is a first predetermined amount (value S12) in a steady state in which the laser irradiation means (welding head 10) moves at a constant speed V11, and is a second predetermined amount (value S11) smaller than the first predetermined amount (value S12) in a low-speed state in which the laser irradiation means (welding head 10) moves at a speed slower than the steady state.
[0078] In the above-mentioned laser welding method or laser welding apparatus 1, it is preferable that the low-speed state includes an acceleration state in which the laser irradiation means (welding head 10) starts moving from a state stopped at the start position P11 toward the end position P12 and accelerates until it reaches a steady state, and a deceleration state in which the laser irradiation means (welding head 10) decelerates from the steady state until it is stopped at the end position P12.
[0079] In the above-described laser welding method or laser welding apparatus 1, it is preferable that in the accelerated state, the scanning amount gradually increases from the second predetermined amount (value S11) to the first predetermined amount (value S12).
[0080] In the above-described laser welding method or laser welding apparatus 1, it is preferable that in the deceleration state, the scanning amount gradually decreases from the first predetermined amount (value S12) to the second predetermined amount (value S11).
[0081] According to the above-described laser welding method or laser welding device 1, the scanning amount is a first predetermined amount (value S12) in a steady state where the laser irradiation means (welding head 10) moves at a constant speed, and is a second predetermined amount (value S11) smaller than the first predetermined amount (value S12) in a slow speed state (e.g., an accelerating state or a decelerating state) where the laser irradiation means (welding head 10) moves slower than the steady state, so that the irradiation position of the measurement light L21 varies depending on whether the laser irradiation means (welding head 10) is in a steady state or a slow speed state. Therefore, even if there is a variation in the moving speed of the laser irradiation means (welding head 10) while performing continuous welding while moving, it becomes possible to accurately measure the position of the bottom 54a of the keyhole 54.
[0082] Furthermore, if, in the accelerating state, the scanning amount gradually increases from the second predetermined amount (value S11) to the first predetermined amount (value S12), and, in the decelerating state, the scanning amount gradually decreases from the first predetermined amount (value S12) to the second predetermined amount (value S11), it is possible to more accurately measure the position of the bottom 54a of the keyhole 54 while the laser irradiation means (welding head 10) is accelerating or decelerating.
[0083] The above embodiment is merely an example and does not limit the present invention in any way. Therefore, the present invention can be improved and modified in various ways without departing from the scope of the present invention. For example, in the present embodiment, the gradual increase in the scanning amount is a linear increase over time, but it may be a stepwise increase. Similarly, in the present embodiment, the gradual decrease in the scanning amount is a linear decrease over time, but it may be a stepwise decrease.
[0084] Also, while it is most desirable to gradually increase or decrease the scanning amount when the welding head 10 is in a low speed state, it is considered possible to measure the position of the bottom 54a even if the scanning amount is kept constant at value S11 while the welding head 10 is in a low speed state.
[0085] Furthermore, as disclosed in Patent Document 1, the penetration depth of the processing laser L11 into the outer plate 51 and the cross bone 52 may be calculated based on the position of the bottom 54a of the keyhole 54 and the position of the surface of the cross bone 52. Specifically, by scanning the measurement light L21, the position of the bottom 54a of the keyhole 54 is measured, and the position of the surface of the cross bone 52 is measured, and the penetration depth of the processing laser L11 is calculated from the difference between the position of the bottom 54a and the position of the surface of the cross bone 52.
[0086] Alternatively, as disclosed in Japanese Patent Application No. 2021-204981 filed by the present applicant, the height of the weld bead 56 may be measured by scanning the measurement light L21, the gap between the outer plate 51 and the cross frame 52 may be calculated based on the height of the weld bead 56, and the penetration depth of the processing laser L11 may be calculated based on the gap, the position of the bottom 54a, and the position of the surface of the cross frame 52. In addition, in this embodiment, a lap joint in which the first base material (outer plate 51) and the second base material (cross frame 52) are welded in an overlapping state is described as an example, but a fillet joint or a butt joint may also be used. [Explanation of symbols]
[0087] 1 Laser welding equipment 10 Welding head (an example of a laser irradiation means) 51 Exterior plate (example of base material) 52 Cross bone (example of base material) 54 Keyhole 54a bottom L11 Processing Laser L21 measurement light
Claims
1. A laser welding method for continuously welding a base material by a processing laser irradiated by a laser irradiation means, comprising: While the continuous welding is being performed, a measurement light by optical coherence tomography is irradiated backward in the direction of progression of the continuous welding from the irradiation portion of the processing laser with a predetermined scanning amount corresponding to the speed of movement of the laser irradiation means, thereby measuring the position of a bottom of a keyhole generated by irradiation of the processing laser; A laser welding method comprising the steps of:
2. 2. The laser welding method according to claim 1, The start and end positions of the continuous welding are located on the base material; The scanning amount is In a steady state where the laser irradiation means moves at a constant speed, the first predetermined amount is a second predetermined amount smaller than the first predetermined amount when the laser irradiation means is in a low speed state slower than the steady state; A laser welding method comprising the steps of:
3. The laser welding method according to claim 2, The low speed state includes: an acceleration state in which the laser irradiation means starts moving from a state in which the laser irradiation means is stopped at the start position toward the end position and accelerates until the laser irradiation means reaches the steady state; a deceleration state in which the laser irradiation means decelerates from the steady state until it is stopped at the end point position; Include: A laser welding method comprising the steps of:
4. The laser welding method according to claim 3, In the accelerated state, the scanning amount gradually increases from the second predetermined amount to the first predetermined amount; A laser welding method comprising the steps of:
5. 5. The laser welding method according to claim 3, In the deceleration state, the scanning amount gradually decreases from the first predetermined amount to the second predetermined amount; A laser welding method comprising the steps of:
6. In a laser welding device that performs continuous welding of base materials using a processing laser, A laser irradiation means for irradiating the processing laser; A driving means for moving the laser irradiation means; an optical interferometer that generates measurement light using optical coherence tomography; a scanning means for scanning the measurement light; a control device having a control program for controlling the laser welding device; To have the control program causes the laser irradiation means to irradiate the processing laser while moving over the base material using the drive means to perform the continuous welding, generates the measurement light from the optical interferometer, and irradiates the measurement light rearward in a direction of progression of the continuous welding beyond the irradiation portion of the processing laser by the scanning means with a predetermined scanning amount corresponding to a speed of movement of the laser irradiation means, thereby measuring a position of a bottom of a keyhole created by irradiation of the processing laser; A laser welding device characterized by:
7. 7. The laser welding apparatus according to claim 6, The start and end positions of the continuous welding are located on the base material; The scanning amount is In a steady state where the laser irradiation means moves at a constant speed, the first predetermined amount is a second predetermined amount smaller than the first predetermined amount when the laser irradiation means is in a low speed state slower than the steady state; A laser welding device characterized by:
8. 8. The laser welding apparatus according to claim 7, The low speed state includes: an acceleration state in which the laser irradiation means starts moving from a state in which the laser irradiation means is stopped at the start position toward the end position and accelerates until the laser irradiation means reaches the steady state; a deceleration state in which the laser irradiation means decelerates from the steady state until it is stopped at the end point position; Include: A laser welding device characterized by:
9. 9. The laser welding apparatus according to claim 8, In the accelerated state, the scanning amount gradually increases from the second predetermined amount to the first predetermined amount; A laser welding device characterized by:
10. 10. The laser welding apparatus according to claim 8, In the deceleration state, the scanning amount gradually decreases from the first predetermined amount to the second predetermined amount; A laser welding device characterized by:
Citation Information
Patent Citations
Laser welding method and laser welding system
JP2007118078A
Measuring device and laser welding device
JP2018153842A
Manufacturing method of metallic component
JP2022133532A
Methods and Systems for Characterizing Laser Machining Properties by Measuring Keyhole Dynamics Using Interferometry
US20160039045A1
Method for measuring penetration depth of laser beam into workpiece, and laser processing apparatus