Block manufacturing method using blast furnace slag fine powder

The method addresses bleeding and separation issues in block manufacturing by using pulverized blast furnace slag as a binder without cement, achieving efficient block production with reduced CO2 emissions through sequential curing and additives.

JP2024154830AInactive Publication Date: 2024-10-31ECO BLOCKS CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023068942
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-20
Publication Date
2024-10-31
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing block manufacturing methods using pulverized blast furnace slag as a binder face issues like bleeding and material separation, and there is a demand to reduce CO2 emissions associated with cement production.

Method used

A method for manufacturing blocks using a kneaded material that consists of pulverized blast furnace slag as a binder without cement, utilizing a vibrating mold for immediate demolding and sequential curing processes to achieve desired bending strength, with optional additives like gypsum and alkaline ionized water to enhance strength and facilitate demolding.

Benefits of technology

This method enables efficient production of blocks with improved strength and reduced CO2 emissions by leveraging pulverized blast furnace slag, allowing for immediate demolding and effective curing stages.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154830000001_ABST
    Figure 2024154830000001_ABST
Patent Text Reader

Abstract

To provide a method for efficiently manufacturing blocks using a mixture that does not contain cement which emits a large discharge amount of CO2.SOLUTION: A mixture of a binder, an aggregate, an admixture and water is supplied into an oscillation mold, the mixture is molded by the oscillation mold, and then immediately demolded onto a pallet to form a molded body, the molded body is subjected to a first curing while being placed on the pallet until a bending strength of 2 N / mm2 or more is achieved, and then to a second curing until a bending strength of 3 N / mm2 or more is achieved.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for producing a block from a mixture containing at least ground granulated blast furnace slag as a binder and not containing cement. [Background technology]

[0002] Conventionally, blocks have been proposed that use ground granulated blast furnace slag having latent hydraulic properties as a binder (see, for example, Patent Documents 1 and 2). However, when the ratio of ground granulated blast furnace slag is high, problems such as bleeding and material separation can occur easily. Therefore, this problem has been addressed by replacing part of the cement used as the binder with ground granulated blast furnace slag.

[0003] Meanwhile, in recent years, there has been a demand to reduce the use of cement, which has high CO2 emissions (it is said that approximately 758 kg of CO2 is emitted to produce 1 ton of cement, while ground granulated blast furnace slag emits approximately 27 kg of CO2) in order to curb CO2 emissions. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2018-154542 A [Patent Document 2] JP 2014-152073 A DISCLOSURE OF THEINVENTION [Problem to be solved by the invention]

[0005] An object of the present invention is to provide a method for efficiently producing blocks using a mixture that does not contain cement, which has a high CO2 emission rate. [Means for solving the problem]

[0006] In order to achieve the above object, the method for producing a block using ground granulated blast furnace slag of the present invention is a method for producing a block from a mixture containing at least ground granulated blast furnace slag as a binder and not containing cement, the method comprising: supplying a mixture of a binder, aggregate, admixture and water into a vibration mold; molding the mixture with the vibration mold, and immediately demolding the molded body onto a pallet; and subjecting the molded body to a compression force of 2 N / mm 2 The first curing is carried out while placed on a pallet until the bending strength of the above is achieved, and then the bending strength is increased to 3N / mm 2 The second curing is carried out until the bending strength described above is attained.

[0007] In this case, the binder may include gypsum.

[0008] The water may be alkaline ionized water.

[0009] The water / binder ratio of the kneaded product may be 30% or less.

[0010] In addition, the kneaded material is 1 m 3 Each unit can contain more than 250 kg of ground granulated blast furnace slag.

[0011] In addition, the block is 1m 3 A base layer made of a mixture containing 250kg to 300kg of ground granulated blast furnace slag per 1m 3 The surface layer may be made of a mixture containing 400 kg or more of ground granulated blast furnace slag per unit area. Effect of the Invention

[0012] According to the method for producing blocks using ground granulated blast furnace slag of the present invention, blocks can be produced efficiently using a kneaded material that does not contain cement, which emits a large amount of CO2. [Brief description of the drawings]

[0013] [Figure 1]FIG. 1 is a flow chart showing one embodiment of a method for producing a block using ground granulated blast furnace slag according to the present invention. [Diagram 2] This is a graph showing the relationship between the age of a block (thickness: 60 mm) and its bending strength. [Diagram 3] This is a photograph showing the state of a block that was broken 35 days after production and the cross section treated with a phenolphthalein solution. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] Hereinafter, an embodiment of the method for producing a block using ground granulated blast furnace slag according to the present invention will be described.

[0015] FIG. 1 shows a flow diagram of one embodiment of the method for producing blocks using ground granulated blast furnace slag according to the present invention. The method for manufacturing blocks using this ground granulated blast furnace slag is a method for manufacturing blocks from a mixture that contains at least ground granulated blast furnace slag as a binder and does not contain cement, and comprises the following steps (1) to (5).

[0016] (1) Mixing process The binder, aggregate, admixture and water are charged into a kneader to prepare a kneaded mixture. The binder used is mainly ground granulated blast furnace slag and does not contain cement. The ground granulated blast furnace slag may be ground granulated blast furnace slag equivalent to ground granulated blast furnace slag 4000 (JIS A 6206) (density: 2.8 or more, specific surface area: 3500 or more and less than 5000), for example, ground granulated blast furnace slag with added gypsum. The kneaded material is 1m 3 Each unit can contain more than 250 kg of ground granulated blast furnace slag. In addition, if the blocks are paving blocks, the mixture is 3 A base layer (for example, thickness: about 50 mm) using a mixture containing 250 kg to 300 kg of ground granulated blast furnace slag per 1 m 3The surface layer (for example, thickness: about 10 mm) made of a mixture containing 400 kg or more of ground granulated blast furnace slag per unit area can be laminated, thereby improving the strength of the surface layer. The binder can also contain gypsum, and ground granulated blast furnace slag with added gypsum can be used preferably. Gypsum reacts with the aluminum trioxide contained in the ground granulated blast furnace slag to produce ettringite (3CaO·Al2O3·3CaOSO4·32H2O), which can improve the initial strength of the block immediately after molding. As the aggregate, general-purpose aggregates such as crushed stone, crushed sand, fine blast furnace slag aggregate, and crushed lime sand can be used. Water should be added so that the water-binder ratio of the mixture is 30% or less (25-30%). By making the water-binder ratio of the mixture 30% or less, the amount of water contained in the mixture is reduced, and the frictional heat generated by the aggregate during mixing increases, so the temperature of the concrete after mixing increases and the initial hydration reaction of the binder (fine powdered slag) contained in the mixture tends to be accelerated, and as described below, the concrete will reach a specified strength (3N / mm 2 60-70% of the bending strength (2N / mm 2 or more) is obtained, making it possible to handle the molded product. As for the water, in addition to ordinary water, alkaline ionized water (alkaline ionized water having a pH of 11.0 to 13.5, preferably a pH of 12.0 to 13.3, more preferably a pH of 12.5 to 13.1, which is produced by electrolyzing filtered water) can be used. By applying alkaline stimulation to the ground granulated blast furnace slag contained as a binder, it is possible to develop an initial strength that allows for immediate demolding. Admixtures are added to increase strength while compensating for the loss of workability caused by setting the water-binder ratio of the mixture to 30% or less. High-performance water reducers and air-entraining agents, such as the high-performance water reducer "Mighty HS" (product name) manufactured by Kao Chemical Corporation, can be used.

[0017] (2) Molding process The kneaded material prepared in the kneading step is fed into a vibration mold of a molding machine, and the kneaded material is molded into a predetermined shape by the vibration mold. The vibration mold of the molding machine can be a general-purpose type used for molding concrete blocks, equipped with a vibrator with a rotation speed of approximately 2500 to 4000 rpm and configured to vibrate the mold with an amplitude of approximately 1 to 5 mm.

[0018] (3) Demolding process After the kneaded mixture is molded by the vibration mold, it is immediately demolded onto a pallet; that is, the kneaded mixture is molded by the vibration mold to a substantially zero slump state, and a molded body can be obtained. Here, the time from when the kneaded material is fed into the vibration mold of the molding machine until it is removed from the mold is less than one minute (usually, about 20 to 30 seconds).

[0019] (4) First curing process The compact is placed on a pallet and moved by a conveyor while being steam cured to a strength of 2N / mm 2 The bending strength above this level (strength that allows handling (holding and transporting by a conveying machine)) is to be exhibited. At this time, the molded body maintains its shape while placed on the pallet, but since it is not strong enough to be held and transported by a conveying machine, a non-contact state is maintained. Here, the duration of the first curing step is about one day (usually, about 20 to 24 hours).

[0020] (5)Second curing process After that, the strength is 2N / mm, which is the strength at which handling (holding and transporting with a conveying machine) is possible. 2 Molded products that have achieved a bending strength of 3N / mm can be re-shipped, etc., as necessary. 2 Curing should be continued until the above bending strength is achieved. Here, the period of the second curing step is about one week (usually about 5 to 7 days).

[0021] Table 1 shows the nominal mix for building blocks, and Table 2 shows the nominal mix for paving blocks. Here, the water used was normal water or alkaline ionized water (alkaline ionized water with a pH of 12.5 to 13.1 produced by electrolyzing filtered water). By using alkaline ionized water, an alkaline stimulus is applied to the ground granulated blast furnace slag contained in the mixture as a binder. It was confirmed that, for example, even when crushed limestone sand is not used as aggregate, the alkaline ionized water functions as an alkaline stimulant, contributing to the development of initial strength that allows for immediate demolding.

[0022] [Table 1]

[0023] [Table 2]

[0024] It was confirmed that the bending strength of the blocks manufactured in this manner increased with the passage of time, as shown in FIG.

[0025] It was also confirmed that, as the blocks aged, they neutralized the CO2 by absorbing it from the surface as the days passed, as shown in Figure 3 (the uncolored areas in Figure 3 are the neutralized areas).

[0026] The method for manufacturing a block using ground granulated blast furnace slag according to the present invention has been described above based on the examples. However, the present invention is not limited to the configurations described in the above examples. The configuration can be modified as appropriate without departing from the spirit of the present invention. [Industrial Applicability]

[0027] The method for producing blocks using ground granulated blast furnace slag of the present invention can efficiently produce blocks using a mixture that does not contain cement, which has high CO2 emissions, and can therefore be widely applied to blocks for various purposes, including paving blocks with reduced CO2 emissions.

Claims

1. A method for producing a block from a kneaded material containing at least ground granulated blast furnace slag as a binder and not containing cement, the method comprising: supplying a kneaded material of binder, aggregate, admixture, and water into a vibration mold; molding the kneaded material with the vibration mold; immediately demolding the molded material onto a pallet; and subjecting the molded material to a compression force of 2 N / mm 2 The first curing is carried out while the product is placed on a pallet until the bending strength of 3 N / mm is achieved. 2 A method for manufacturing blocks using ground granulated blast furnace slag, characterized in that a second curing is carried out until the above bending strength is achieved.

2. 2. The method for manufacturing a block using ground granulated blast furnace slag according to claim 1, wherein the binder contains gypsum.

3. 2. The method for manufacturing a block using ground granulated blast furnace slag according to claim 1, wherein the water is alkaline ionized water.

4. 4. The method for manufacturing a block using ground granulated blast furnace slag according to claim 1, 2 or 3, wherein the water-binder ratio of the kneaded product is 30% or less.

5. The kneaded material is 1 m 3 4. The method for producing a block using ground granulated blast furnace slag according to claim 1, 2 or 3, characterized in that the block contains 250 kg or more of ground granulated blast furnace slag per block.

6. The block is 1 m 3 a base layer made of a mixture containing 250 kg to 300 kg of ground granulated blast furnace slag per 1 m 3 4. The method for manufacturing a block using ground granulated blast furnace slag according to claim 1, 2 or 3, characterized in that the block is laminated with a surface layer made of a kneaded material containing 400 kg or more of ground granulated blast furnace slag per unit area.

Citation Information

Patent Citations

  • Block having high water retentivity, and method for producing the same

    JP2014152073A

  • Concrete block for decoration

    JP2018154542A