Piezoelectric actuator and liquid discharge head

A multi-layer protective structure for piezoelectric actuators in liquid ejection heads addresses insulation resistance and failure issues by using aluminum oxide, silicon oxide, and silicon nitride layers to maintain performance in humid conditions.

JP2024154875APending Publication Date: 2024-10-31CANON KK
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023069080
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-20
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Piezoelectric actuators in liquid ejection heads suffer from insulation resistance reduction and failure due to moisture exposure, especially when aluminum oxide insulating layers are altered at high temperatures, leading to decreased displacement characteristics.

Method used

A piezoelectric actuator design with multiple protective layers, including a first protective layer of aluminum oxide, a second protective layer of silicon oxide, and a third protective layer of silicon nitride, to prevent moisture intrusion and maintain insulation resistance, while ensuring sufficient displacement characteristics.

Benefits of technology

The design effectively suppresses dielectric breakdown and failure caused by increased leakage current, maintaining both good piezoelectric characteristics and high reliability in high humidity environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154875000001_ABST
    Figure 2024154875000001_ABST
Patent Text Reader

Abstract

To provide a piezoelectric actuator which has both of an excellent piezoelectric characteristic and high reliability obtained by suppressing lowering of insulation resistance and a failure.SOLUTION: A piezoelectric actuator includes a piezoelectric element having a first electrode, a piezoelectric layer, and a second electrode in order from a substrate, and further includes: first wiring which is electrically connected to the first electrode and second wiring which is electrically connected to the second electrode. The piezoelectric actuator includes: a first layer which covers the piezoelectric element; a second layer which is arranged between the piezoelectric element and the first wiring and between the piezoelectric element and the second wiring; and a third layer which is arranged to cover the first wiring, the second wiring and a circumference in plan view of the piezoelectric layer in this order from the substrate.SELECTED DRAWING: Figure 6
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a piezoelectric actuator and a liquid ejection head. [Background technology]

[0002] Piezoelectric bodies, whose shape changes when an electric field is applied, are used in various industrial products as a means of moving or vibrating objects minutely and precisely. For example, they are used in small speakers, hard disk drives, printers (liquid ejection devices), etc. Among them, some printers use a piezoelectric layer in the liquid ejection head that ejects droplets. In such liquid ejection heads, an electric field is applied by electrodes (upper electrode, lower electrode) formed to sandwich the piezoelectric layer from above and below, driving the piezoelectric layer to eject droplets. At this time, the voltage required to sufficiently displace the piezoelectric layer is several tens of volts, and a relatively high voltage must be applied for a semiconductor device. In addition, in order to perform high-definition recording, wiring and electrodes with different potentials are densely arranged in the liquid ejection head.

[0003] In such a liquid ejection head equipped with a piezoelectric actuator having a piezoelectric layer, moisture in a high humidity environment can cause a deterioration in the characteristics of the piezoelectric layer, and an increase in leakage current can cause insulation breakdown or failure.

[0004] Patent Document 1 shows a liquid ejection head capable of maintaining the electromechanical conversion characteristics of the piezoelectric layer even in a high humidity environment. In Patent Document 1, a pair of electrodes (upper electrode, lower electrode) sandwich the piezoelectric layer from above and below, and an insulating layer is provided between the upper wiring connected to the upper electrode and the piezoelectric body, between the lower electrode and the upper wiring, and between the lower wiring connected to the lower electrode and the lower electrode. In addition, the leakage current is controlled by adjusting the amount of excess lead in the piezoelectric layer, which is the source of leakage. With this configuration, the leakage current density of the piezoelectric layer is reduced to 4.2×10 -6 A / cm 2 The following discloses a liquid ejection head capable of suppressing the above-mentioned problems. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2020-25082 A Summary of the Invention [Problem to be solved by the invention]

[0006] The aluminum oxide used as the insulating layer in the configuration disclosed in Patent Document 1 is subject to surface deterioration when exposed to moisture at high temperatures. When etching is performed to form contact holes and wiring while the aluminum oxide film is on the outermost surface of the piezoelectric actuator, the surface of the aluminum oxide film may be exposed to moisture during a cleaning process or the like. In this case, there is a risk that the moisture remaining on the film surface will be heated to high temperatures during etching and ashing, causing the aluminum oxide surface to deteriorate. If an altered insulating layer exists on the piezoelectric layer, this may cause a decrease in insulation resistance and lead to failure.

[0007] Furthermore, if the insulating layer in the piezoelectric actuator is only an aluminum oxide layer, the thickness of the aluminum oxide layer must be increased in order to obtain sufficient insulation resistance, which may lead to a deterioration in the displacement characteristics of the piezoelectric actuator.

[0008] SUMMARY OF THE PRESENT EMBODIMENTS An object of the present invention is to provide a piezoelectric actuator that combines good piezoelectric characteristics with high reliability in which deterioration of insulation resistance and failures are suppressed. [Means for solving the problem]

[0009] The present invention, which solves the above problems, is a piezoelectric actuator having a piezoelectric element having a first electrode, a piezoelectric layer, and a second electrode, in that order from a substrate, and further having a first wiring electrically connected to the first electrode and a second wiring electrically connected to the second electrode, wherein the piezoelectric actuator has, in this order from the substrate, a first layer covering the piezoelectric element, a second layer arranged between the piezoelectric element and the first wiring, and between the piezoelectric element and the second wiring, and a third layer arranged so as to cover the first wiring, the second wiring, and the periphery of the piezoelectric layer when viewed in a planar view. Effect of the Invention

[0010] According to the present invention, it is possible to provide a piezoelectric actuator that combines good piezoelectric characteristics with high reliability in which deterioration of insulation resistance and failures are suppressed. [Brief description of the drawings]

[0011] [Figure 1] 1 is a diagram illustrating an example of a liquid ejection apparatus according to the present invention. [Diagram 2] 1 is a diagram illustrating an example of a liquid ejection apparatus according to the present invention. [Diagram 3] 1 is a diagram illustrating an example of a liquid ejection head of the present invention. [Figure 4] FIG. 2 is a diagram showing an example of a liquid ejection unit of the present invention. [Diagram 5] FIG. 2 is a diagram showing an example of a liquid ejection unit of the present invention. [Figure 6] 1 is a diagram showing an example of a piezoelectric actuator of the present invention. [Figure 7] FIG. 13 is a diagram showing the results of evaluating moisture penetration into a silicon oxide single layer film. [Figure 8] 3A to 3C are diagrams illustrating a part of a manufacturing process for the piezoelectric actuator of the present invention. [Figure 9] 1 is a diagram showing an example of a piezoelectric actuator of the present invention. [Figure 10] 1 is a diagram showing an example of a piezoelectric actuator of the present invention. [Figure 11] 1 is a diagram showing an example of a piezoelectric actuator of the present invention. [Figure 12] 1 is a diagram showing an example of a piezoelectric actuator of the present invention. [Figure 13] 1 is a diagram showing an example of a piezoelectric actuator of the present invention. [Figure 14] 1 is a diagram showing an example of a piezoelectric actuator of the present invention. [Figure 15] 1 is a diagram showing an example of a piezoelectric actuator of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] An embodiment of the present invention will be described with reference to the drawings. The same reference numerals are given to components having the same functions, and repeated description may be omitted. In the following, an example in which the present invention is applied to a piezoelectric actuator used in a liquid ejection head provided in a liquid ejection device such as an inkjet printer will be described. However, the present invention is not limited to the embodiment shown below, and other modifications, additions, corrections, deletions, and other changes can be made within the scope of what a person skilled in the art can conceive. In any aspect, as long as the action and effect of the present invention are achieved, it is included in the scope of the present invention.

[0013] (First embodiment) <Liquid discharge device> Fig. 1 is a diagram showing an example of the configuration of a liquid ejection device. A recording medium 1, such as recording paper, is transported in the direction of the arrow by transport means 2, such as a paper feed roller, and recorded on a platen 3. The device is equipped with four liquid ejection heads 4, which perform recording by ejecting cyan, magenta, yellow, and black ink, respectively. Each liquid ejection head 4 is connected to a driving means 5 that electrically drives the pressure generating means of the liquid ejection head. The driving means 5 generates a driving signal based on an image signal sent from a controller 6.

[0014] FIG. 2 is another diagram showing an example of the configuration of a liquid ejection device. The liquid ejection device shown in FIG. 2 is a one-pass type that records an image by moving the recording medium 1 once. This is an example of a liquid ejection device (hereinafter also referred to as the device body) equipped with a liquid ejection head as a full-line head in which an element substrate having an ejection port from which liquid is ejected is arranged over the side corresponding to the full width of the recording medium 1. The recording medium 1 is transported in the direction of the arrow by a transport means 2, and recording is performed by a liquid ejection head 4. The liquid ejection head according to the present invention can be embodied in any form including the examples of FIG. 1 and FIG. 2, and is not limited to other forms. In FIG. 2, a liquid ejection device equipped with eight liquid ejection heads 4 (4Ka, 4Kb, 4Ya, 4Yb, 4Ma, 4Mb, 4Ca, 4Cb) is shown. These eight liquid ejection heads 4 are positioned within the liquid ejection device by a reference member.

[0015] As described above, the liquid ejection head of this embodiment is a one-pass type so-called page-wide head having a length corresponding to the width of the recording medium (the size in the direction perpendicular to the conveying direction of the recording medium). However, the present invention can also be applied to a so-called serial type liquid ejection head that performs printing while scanning the liquid ejection head over the recording medium. An example of a serial type liquid ejection head is a configuration in which one element substrate for black ink and one element substrate for color ink are mounted. Another example is a liquid ejection head having a width shorter than the recording medium, in which several element substrates are arranged so that the ejection openings overlap in the ejection opening row direction.

[0016] Fig. 3 shows a perspective view of the liquid ejection head 4, and Fig. 4 shows a perspective view of the liquid ejection unit 7. In the liquid ejection head 4 according to this embodiment, a plurality of liquid ejection units 7, each of which includes an element substrate 11 having an ejection port 19 for ejecting liquid, are fixed onto a support member 40. Note that the present invention can also be suitably used in a liquid ejection head having a configuration in which only one liquid ejection unit 7 is fixed onto one support member.

[0017] 3, the liquid ejection head 4 has a plurality of liquid ejection units 7 arranged in a staggered pattern. Each liquid ejection unit 7 has approximately 1000 ejection ports 19, enabling recording at 1200 dpi. An electric wiring board 20 such as a flexible wiring board is connected to the element substrate 11. The electric wiring board 20 is configured to supply energy and electric signals for ejecting liquid to the ejection ports.

[0018] <Flow path configuration of liquid ejection unit> 5 is a cross-sectional view showing the flow path configuration of the liquid discharge unit according to this embodiment. The liquid discharge unit has a flow path substrate 11, an actuator substrate 12, a pressure chamber substrate 13, and a discharge port substrate .

[0019] The flow path substrate 11 has a supply port 15 for supplying the liquid to be discharged from the discharge port 19 to the pressure chamber 17 described later, and an outlet port 16 for causing the liquid to flow out from the pressure chamber 17. Therefore, the liquid is configured to be able to circulate inside and outside the pressure chamber. The piezoelectric actuator of the present invention can be suitably used even in a liquid discharge head having a structure in which the flow path substrate does not have the outlet port 16. In addition, the liquid discharge head may be configured to supply the liquid to the pressure chamber from both the supply port 15 and the outlet port 16 in FIG. 5. The flow path substrate 11 in this embodiment is formed by etching a silicon substrate, as an example, but any material and manufacturing method may be used.

[0020] An actuator substrate 12 is bonded to the flow path substrate 11. The actuator substrate 12 has a substrate (substrate 101, see FIG. 6) and a piezoelectric element 110. A detailed configuration of the actuator substrate 12 will be described later, and the actuator substrate and a piezoelectric actuator described later are simply shown in FIG.

[0021] A pressure chamber substrate 13 is bonded to the surface of the actuator substrate 12 opposite to the surface to which the flow path substrate 11 is bonded. The pressure chamber substrate 13 is provided with pressure chambers 17 corresponding to the piezoelectric elements 110. The pressure chamber substrate 13 in this embodiment may be formed, like the flow path substrate 11, by etching a silicon substrate, for example, using any material and manufacturing method.

[0022] An ejection port substrate 14 is bonded to the surface of the pressure chamber substrate 13 opposite to the actuator substrate 12. The ejection port substrate 14 is provided with an ejection port 19. In the liquid ejection unit 7, liquid is supplied from a supply port 15 to a pressure chamber 17, and is ejected from the ejection port 19 by driving a piezoelectric element 110 to deform the actuator substrate 12.

[0023] A protective layer may be provided so as to cover the inner walls of the liquid flow paths that communicate from the supply port 15 to the pressure chamber 17, the discharge port 19, and the recovery port 16. By forming a protective layer made of a material that is more resistant to the discharged liquid than the silicon that constitutes the flow path substrate 11 and the pressure chamber substrate 13 on the walls of the flow path, it is possible to obtain an effect of improving the long-term reliability of the liquid discharge unit 7. When the flow path substrate 11 and the pressure chamber substrate 13 are made of a silicon substrate, for example, SiO2, SiC, Al2O3, HfO2, TaO, DLC (diamond-like carbon), etc. can be used for the protective layer.

[0024] <Configuration of Piezoelectric Actuator> Next, a detailed description will be given of the actuator substrate 12. Note that the components described in the following embodiments are merely examples, and are not intended to limit the scope of the present invention to only those components.

[0025] FIG. 6 shows a cross-sectional view of the piezoelectric actuator in this embodiment. As shown in FIG. 6, the actuator substrate 12 has a piezoelectric element 110 in which a lower electrode 111, a piezoelectric layer 112, and an upper electrode 113 are formed in this order on a substrate 101. The substrate 100 and the piezoelectric element 110 are combined to form a piezoelectric actuator 100 (hereinafter also referred to as an actuator). As shown in FIG. 5, in the liquid ejection unit 7, a pressure chamber 17 is disposed on the side of the substrate 101 opposite to the side on which the actuator is disposed, and the piezoelectric layer 112 is disposed so as to overlap with the pressure chamber 17 when viewed from the liquid ejection direction. The thickness of the piezoelectric layer 112 is determined by the applied voltage and piezoelectric characteristics required to obtain a desired amount of displacement of the actuator substrate 12, and is about 1 to 2 μm, for example, in this embodiment.

[0026] As shown in FIG. 5, the substrate 101 constitutes one of the walls of the pressure chamber 17, and preferably has a flat surface. The material can be appropriately selected, and for example, materials such as silicon (Si), silicon carbide (SiC), quartz, gallium nitride (GaN), gallium arsenide (GaAs), indium phosphide (InP), and sapphire can be suitably used. In order to easily form the pressure chamber 17, the substrate 101 and the pressure chamber substrate 13 may be formed from an SOI (Silicon On Insulator) substrate. The SOI substrate has a silicon oxide layer (BOX layer) on a silicon substrate, and further has a silicon layer thereon. The BOX layer can be formed to a thickness of several tens of nm to several hundreds of μm, and the film thickness of the silicon layer thereon can be relatively freely selected. By appropriately combining these film thicknesses and performing selective etching on the silicon substrate using the BOX layer as an etching stop layer, the pressure chamber 17 can be formed by removing only the silicon. The bottom of the recess obtained by such selective etching becomes the surface of the BOX layer, and an extremely flat surface can be obtained as the wall surface of the substrate 101 constituting the pressure chamber 17. In this case, the substrate 101 has at least a silicon oxide layer derived from the BOX layer and a silicon layer in contact with the surface of the silicon oxide layer opposite to the pressure chamber. In this manner, the substrate 101 in the piezoelectric actuator 100 may have a laminated structure.

[0027] The lower electrode 111 may be exposed to a high temperature of several hundred degrees Celsius in a subsequent firing process of the piezoelectric layer, and is therefore preferably made of a material with a high melting temperature. Examples of such materials include copper, platinum, gold, chromium, cobalt, titanium, and alloys thereof. In addition, when the piezoelectric layer 112 is formed so as to contact the surface of the lower electrode 111, the lower electrode 111 may also serve as a film for controlling the crystal orientation of the piezoelectric layer 112. In this case, a material having an appropriate crystal structure may be appropriately selected for the lower electrode 111. For example, when lead zirconate titanate (PZT) is used as the piezoelectric layer 112, platinum can be used as the lower electrode that also serves as a crystal orientation control film. A general film formation method such as magnetron sputtering can be used to form the platinum film, and the film thickness is appropriately adjusted so as to obtain the desired orientation.

[0028] In order to improve adhesion between the lower electrode 111 and the substrate 101 serving as the base film, a thin film of titanium, chromium, or the like may be further provided as an adhesion layer.

[0029] The upper electrode 113 is formed on the piezoelectric layer 112 and is made of, for example, platinum, titanium, tungsten, or an alloy thereof. As with the lower electrode 111, a thin film of titanium, chromium, or the like may be further provided as an adhesion layer between the piezoelectric layer 112 and the upper electrode 113 in order to improve adhesion to the undercoat film.

[0030] When the substrate 101 is conductive, it is preferable to have an insulating layer 102 between the lower electrode 111 and the substrate 101. For the insulating layer 102, a general insulating material such as a silicon oxide film, a silicon nitride film, a silicon oxynitride film, or an aluminum oxide film can be used.

[0031] In order to apply a desired voltage between the lower electrode 111 and the upper electrode 113 and displace the piezoelectric layer 112, a lower wiring 150 is electrically connected to the lower electrode 111 and an upper wiring 140 is electrically connected to the upper electrode 113.

[0032] Materials commonly used for electrical wiring, such as aluminum, copper, gold, or alloys thereof, can be used for the lower wiring 150 and the upper wiring 140. In order to improve the adhesion of the wiring, a titanium or chromium film may be provided between the lower wiring 150 or the upper wiring 140 and the film in contact therewith.

[0033] <Protective layer for piezoelectric actuator> 6, the piezoelectric actuator of the present invention includes, in a plan view, a first protective layer 120 formed so as to cover the lower electrode 111, the piezoelectric layer 112, and the upper electrode 113, a second protective layer 130 formed thereon and covering the first protective layer 120 at least at a position overlapping with the lower wiring 150 or the upper wiring 140, and a third protective layer 160 formed thereon. In this embodiment shown in FIG. 6, the first protective layer 120 and the second protective layer 130 have contact holes 131 and 132 for connecting the lower electrode 111 and the lower wiring 150, and the upper electrode 113 and the upper wiring 140.

[0034] Between the piezoelectric element 110 and the lower wiring 111, and between the piezoelectric element 110 and the upper wiring, there is a silicon oxide film which is a second protective layer 130 as an insulating layer. As with the insulating layer 102, the second protective layer 130 can be appropriately selected from among general insulating materials such as silicon nitride, silicon oxynitride, and aluminum oxide. It may also be a laminated film in which two or more different types of films are laminated. The second protective layer 130 can be formed by a general film formation method such as a chemical vapor deposition method (CVD method) or a sputtering method. In this embodiment, a silicon oxide film is formed as the second protective layer 130 by the CVD method because of its excellent production rate.

[0035] In the piezoelectric actuator 100 used in the liquid ejection head, a relatively large potential difference is applied between the upper electrode 113 or upper wiring 140 and the lower electrode 111 or lower wiring 150 in order to displace the piezoelectric layer 112, which is a semiconductor device. To obtain a sufficient amount of displacement, a potential difference of approximately 30 V or more is applied to the piezoelectric layer 112 in the film thickness direction. When the second protective layer 130 is a silicon oxide film formed by a CVD method, the dielectric breakdown strength is about 7 MV / cm. Therefore, in order to obtain a dielectric strength voltage of, for example, 50 V, the film thickness of the second protective layer is set to 72 nm or more, thereby reducing the probability of failure. Furthermore, the second protective layer 130 also serves as a moisture-proof film for the layer below it (the first protective layer 120 described later). FIG. 7 is a diagram showing the results of moisture penetration evaluation of a silicon oxide film with a thickness of 410 nm formed on a silicon substrate. Figure 7 shows time-of-flight secondary ion mass spectrometry (TOF-SIMS) D-SIMS depth profiles before and after humidification using heavy water (DO) as a marker. These results show that in order to ensure moisture resistance of the silicon oxide film underlying the film, it is preferable for the film thickness to be 200 nm or more. On the other hand, if the film thickness is too thick, the displacement characteristics of the piezoelectric actuator will decrease, so it is preferable for the film thickness of the second protective layer (silicon oxide film) to be 1.5 μm or less. In other words, it is preferable for the thickness of the second protective layer to be 200 nm or more and 1.5 μm or less.

[0036] When forming the silicon oxide film 130 as the second protective layer, the piezoelectric layer 112 may be damaged and the piezoelectric characteristics may deteriorate. Therefore, the piezoelectric layer 112 has an aluminum oxide film as the first protective layer 120 on the surface of the piezoelectric layer 112 as a protective layer to prevent damage to the piezoelectric layer 112. On the other hand, the surface of aluminum oxide is altered when exposed to moisture at high temperature. During the manufacturing process, when the contact holes 131 and 132 and the upper wiring 140 and the lower wiring 150 are formed in a state where the aluminum oxide is exposed on the outermost surface of the piezoelectric actuator 100, the surface of the aluminum oxide film may be exposed to moisture during cleaning. The moisture remaining on the surface of the aluminum oxide film may become hot during etching or ashing, causing the aluminum oxide surface to be altered. If the altered aluminum oxide film exists on the piezoelectric layer, it may lead to a decrease in insulation resistance and cause a failure. Therefore, it is preferable that the silicon oxide film as the second protective layer 130 is formed in contact with the aluminum oxide film as the first protective layer 120 so as to cover it.

[0037] The thickness of the first protective layer 120 is preferably the minimum thickness necessary from the viewpoint of reducing the influence on the displacement characteristics of the piezoelectric body and the formation of contact holes. Specifically, it is preferably 50 nm or less, more preferably 25 nm or less. In addition, in order to obtain a dielectric strength voltage of, for example, 50 V or more, it is preferable to set the thickness of the aluminum oxide film 120 to 5 nm or more, taking into consideration the step coverage to the piezoelectric layer 112 having a thickness of the order of μm. That is, the thickness of the first layer 120 is preferably 5 nm or more and 50 nm or less, more preferably 5 nm or more and 25 nm or less. As described above, in a piezoelectric actuator used in a liquid ejection head, a relatively high voltage is applied to obtain a sufficient amount of displacement to eject liquid, and when ejection ports are arranged at a high density, the surface density of the piezoelectric elements on the element substrate 11 is high. Under such conditions, in a humid environment in which ink is ejected, a current may flow through the surface of the piezoelectric actuator, leading to a breakdown. In a piezoelectric actuator used in a liquid ejection head for ejecting liquid such as ink, the presence of liquid has a particularly large effect on the piezoelectric actuator. For this reason, the upper wiring 140 and the lower wiring 150 are covered with the third protective layer 160 as a passivation film having high moisture resistance and insulation. The third protective layer 160 can be made of a silicon oxide film, a silicon nitride film, a silicon oxynitride film, or the like. In particular, a passivation film including a silicon nitride film as a part of the film has high moisture resistance compared to a silicon oxide film, and can obtain sufficient moisture resistance and insulation even if the film thickness is thin compared to a case where the film is made of a silicon oxide film, so that it is preferable because it is less likely to adversely affect the displacement characteristics of the piezoelectric actuator. That is, it is preferable that the third protective layer 160 has a higher moisture resistance than the second layer 130. The moisture resistance of the two layers may be compared using a commonly used moisture resistance evaluation method such as the moisture intrusion evaluation described above. In addition, from the viewpoint of insulation, it is preferable that the third protective layer is arranged so as to cover at least the lower wiring, the upper wiring, and the periphery when the piezoelectric layer is viewed in a plan view. It is preferable that the film thickness of the third protective layer 160 is the minimum necessary thickness from the viewpoint of reducing the influence on the displacement characteristics of the piezoelectric body and from the viewpoint of contact hole formation.On the other hand, in the piezoelectric actuator of the present invention, in order to prevent the displacement characteristics from being impaired, the piezoelectric layer is backfilled with an insulating layer or the like, and the upper and lower wirings formed thereon cannot be planarized by a chemical mechanical polishing method (CMP method) or the like. Therefore, the shapes of the upper wiring 140 and the lower wiring 150 inherit the step shape caused by the piezoelectric element 110, so the film thickness of the third protective layer needs to be set to a thickness that takes into consideration the step coverage to the piezoelectric layer 112 and the upper and lower wirings. In this embodiment, as an example, the second protective layer 160 has a silicon nitride film with a thickness of 200 nm so as to sufficiently cover the piezoelectric layer 112 with a thickness of 2 μm and the lower wiring 150 and upper wiring 140 with a thickness of 700 nm.

[0038] As described above, the piezoelectric actuator of the present invention has the first protective layer, second protective layer, and third protective layer as described above, which has the effect of suppressing deterioration of the piezoelectric layer's properties due to moisture, and insulation breakdown and failure due to increased leakage current.

[0039] <Manufacturing method of piezoelectric actuator> The method for manufacturing the piezoelectric actuator of the present invention will be described with reference to the drawings. First, as shown in Fig. 8(a), a silicon substrate 101 is prepared, and a silicon thermal oxide film with a thickness of about 500 nm is formed as an insulating layer 102 by wet oxidation using oxygen and hydrogen gas.

[0040] Next, as shown in FIG. 8(b), a lower electrode 111, a piezoelectric layer 112, and an upper electrode 113 are formed in this order on the insulating layer .

[0041] The lower electrode 111 can be formed by, for example, a sputtering method. When the material of the piezoelectric layer 112 is lead zirconate titanate (PZT), it is preferable to use platinum for the lower electrode 111, which also serves as a crystal orientation control film. In this embodiment, as an example, platinum is formed to a thickness of about 100 nm. A thin film of titanium, chromium, or the like may be formed as an adhesion layer to improve adhesion between the lower electrode 111 and the insulating layer 102.

[0042] The piezoelectric layer 112 is formed by applying a starting material such as a sol-gel liquid onto the lower electrode 111 and firing it to obtain a desired crystal orientation. In this embodiment, as an example, a PZT film having a thickness of 2 μm is formed.

[0043] Then, the upper electrode 113 is formed by sputtering etc. In this embodiment, as an example, an alloy film of titanium and tungsten having a thickness of about 100 nm is formed.

[0044] Next, a resist pattern (not shown) is formed by photolithography so that the upper electrode 113 and the piezoelectric layer 112 have a desired pattern, and then the upper electrode 113 and the piezoelectric layer 112 are patterned by etching as shown in FIG. 8(c).

[0045] Next, a resist pattern (not shown) is formed by photolithography so that the lower electrode 111 has a desired pattern, and then the lower electrode 111 is patterned by etching as shown in Fig. 8(d) By the above steps, a piezoelectric element 110 having the lower electrode 111, the piezoelectric layer 112, and the upper electrode 113 is formed.

[0046] 8(e), an aluminum oxide film is formed as the first protective layer 120 so as to cover at least the upper surface 110a and the side surface 110b of the piezoelectric element 110, the lower electrode 111, and the upper electrode 113. An atomic layer deposition method (ALD method) is used, and in this embodiment, the film thickness is, for example, 23 nm.

[0047] 8(f), a silicon oxide film is formed as a second protective layer 130 so as to cover the aluminum oxide film 120. In this embodiment, the film thickness is, for example, 400 nm.

[0048] 8(g), the upper through-hole 132 and the lower through-hole 131 are formed by photolithography. After a resist pattern (not shown) for forming through-holes to serve as contact holes in the first protective layer 120 and the second protective layer 130 is formed on the second protective layer 130, the upper through-hole 132 and the lower through-hole 131 are formed by etching.

[0049] 8(h), a wiring material that will become the upper wiring 140 and the lower wiring 150 is formed on the second protective layer 130 by a sputtering method. After that, the wiring material is patterned by a photolithography method using a resist pattern to form the upper wiring 140 and the lower wiring 150. In this embodiment, as an example, an aluminum alloy is used as the wiring material, and the film thickness is 600 nm.

[0050] 8(i), a silicon nitride film is formed as a third protective layer 160 having higher moisture resistance than the second protective layer 130 (silicon oxide film) so as to cover the upper wiring 140 and the lower wiring 150. The silicon nitride film is formed by a CVD method, and in this embodiment, the film has a thickness of 200 nm, for example. The third protective layer 160 is etched into a desired pattern by a photolithography method using a resist pattern, thereby forming the piezoelectric actuator 100.

[0051] Thereafter, a pressure chamber substrate and an ejection port substrate having pressure chambers and ejection ports, and a flow path substrate having a flow path for supplying liquid to the pressure chambers are prepared, and then bonded to the piezoelectric actuator 100 to create a liquid ejection head (see FIG. 5).

[0052] In this way, by using the piezoelectric actuator of the present invention, it is possible to provide a liquid ejection head 4 in which deterioration of the piezoelectric layer properties due to moisture and insulation breakdown and failure due to an increase in leakage current are suppressed.

[0053] In the following embodiment, the differences from the above-mentioned first embodiment will be mainly described, and the description of the same parts as those in the above-mentioned configuration will be omitted.

[0054] Second embodiment A second embodiment of the present invention will be described with reference to FIG. 9. In this embodiment, the upper surface 110a of the piezoelectric element 110 has a recess 170 where the silicon oxide film, which is the second protective layer 130, is interrupted. That is, the second layer has an opening in an area overlapping the piezoelectric layer 112 in a plan view. The second protective layer 130 is partially removed on the upper surface 110a of the piezoelectric element 110, so that the rigidity of the piezoelectric actuator can be reduced. This makes it possible to drive the piezoelectric actuator at a lower voltage than in the first embodiment, and the effect of improving the driving efficiency of the piezoelectric actuator can be obtained. On the other hand, the second protective layer 130 is disposed at a position where leakage is likely to occur, specifically, between the lower electrode and the lower wiring, between the lower electrode or the upper electrode and the upper wiring, and at a position where it overlaps with the periphery of the piezoelectric layer 112 in a plan view. Therefore, even with the configuration of this embodiment, the effect of the present invention that the deterioration of the characteristics of the piezoelectric layer due to moisture and the insulation breakdown due to the increase in leakage current are unlikely to occur can be sufficiently obtained. Note that the second protective layer 130 may have a configuration in which the recess 170 is formed by being recessed in a direction perpendicular to the substrate in plan view, rather than being opened.

[0055] In manufacturing the piezoelectric actuator of this embodiment, in the step of forming the upper through-hole 132 and the lower through-hole 131 by etching shown in Fig. 8(g), the recess 170 can be formed by simultaneously etching at least a part of the center of the second protective layer 130 on the upper surface 110a of the piezoelectric element 110. The formation of the recess 170 may be performed after the step of forming the upper wiring 140 and the lower wiring 150 shown in Fig. 8(h).

[0056] The recess 170 may be formed by recessing or opening the third protective layer 160, instead of the second protective layer 130, in a region overlapping with the piezoelectric layer 112 in a plan view. However, in terms of ensuring moisture resistance of the piezoelectric layer, it is preferable to reduce the rigidity of the piezoelectric actuator by partially removing the second protective layer 130, rather than using the third protective layer 160, which has better moisture resistance than the second protective film.

[0057] (Third embodiment) A third embodiment of the present invention will be described with reference to FIG. 10. In this embodiment, the fourth protective layer (fourth layer) 180 is further formed so as to cover the first protective layer 120. The fourth protective layer 180 is preferably more moisture resistant than the first protective layer 120, and this can further prevent the deterioration of the characteristics of the piezoelectric layer 112 due to moisture. In this embodiment, as an example, the fourth protective layer 180 has a hafnium oxide film that is more moisture resistant than the aluminum oxide film of the first protective layer 120. The fourth protective layer 180 is not limited to hafnium oxide, and may be any film that is more moisture resistant than the aluminum oxide film. In FIG. 10, the first protective layer 120 and the fourth protective layer 180 are each formed as a single layer, but may be a laminate of two types of layers. For example, a laminate film in which an aluminum oxide film having a thickness of 5 nm as the first protective layer and a hafnium oxide film having a thickness of 5 nm as the fourth protective layer 180 are alternately laminated is considered. In the case of such a laminated structure, moisture resistance of the piezoelectric layer 112 can be more securely ensured than in the case of a single layer film, even if pinholes or the like are present in one layer.

[0058] (Fourth embodiment) A fourth embodiment of the present invention will be described with reference to Fig. 11. In this embodiment, a recess 170 is formed on an upper surface 110a of a piezoelectric element 110, where the silicon oxide film 130 serving as the second protective layer is interrupted, and a fourth protective layer 180 is further formed so as to cover the first protective layer 120. That is, this embodiment is a combination of the second and third embodiments described above.

[0059] By providing the fourth protective layer 180, which has higher moisture resistance than the first protective layer 120, it is possible to sufficiently prevent the deterioration of the characteristics of the piezoelectric layer 112 due to moisture, even if a recess 170 for improving the drive characteristics of the piezoelectric actuator is formed. In Fig. 11, the first protective layer 120 and the fourth protective layer 180 are each formed as a single layer, but they may be laminated bodies as described in the third embodiment.

[0060] Fifth embodiment A fifth embodiment of the present invention will be described with reference to FIG. 12. In this embodiment, the lower electrode 111 is formed so as to also serve as the lower wiring. In this case, the effect of being able to reduce the process of forming a contact hole for connecting the lower electrode and the lower wiring and the process of forming the lower wiring can be obtained. On the portion 111a of the lower electrode 111 that serves as the lower wiring, an aluminum oxide film as the first protective layer 120, a silicon oxide film as the second protective layer 130, and a silicon nitride film as the third protective layer 160 are formed. The film thicknesses of each are the same as those of the first embodiment. Even in a piezoelectric actuator having a structure in which the lower electrode 111 also serves as the lower wiring and the lower electrode is integrally formed with the lower wiring as in this embodiment, it is possible to provide a liquid ejection head that does not cause deterioration of the characteristics of the piezoelectric layer due to moisture or insulation breakdown or failure due to an increase in leakage current by suitably using the present invention.

[0061] Sixth embodiment The sixth embodiment of the present invention will be described with reference to Fig. 13. In this embodiment, as in the fifth embodiment, the lower electrode 111 is formed to also serve as the lower wiring. Furthermore, as in the second embodiment, the upper surface 110a of the piezoelectric element 110 has a recess 170 at the end of the silicon oxide film 130, which is the second protective layer. That is, this embodiment is a combination of the fifth and second embodiments described above.

[0062] Seventh embodiment A seventh embodiment of the present invention will be described with reference to Fig. 14. In this embodiment, as in the fifth embodiment, the lower electrode 111 is formed so as to also serve as the lower wiring. In addition, a fourth protective layer 180 is further formed so as to cover the first protective layer 120. That is, this is a configuration that combines the fifth and third embodiments described above.

[0063] Eighth embodiment The eighth embodiment of the present invention will be described with reference to FIG. 15. In this embodiment, as in the fifth embodiment, the lower electrode 111 is formed to also serve as the lower wiring. Furthermore, as in the second embodiment, the upper surface 110a of the piezoelectric element 110 has a recess 170 at which the silicon oxide film 130, which is the second protective layer, is interrupted. In addition, a fourth protective layer 180 is further formed to cover the first protective layer 120. That is, this is a configuration that combines the fifth, second, and third embodiments described above.

[0064] (Other embodiments) The effects of the present invention can be obtained even with a configuration in which the above-described embodiments of the present invention are appropriately combined. [Explanation of symbols]

[0065] 4. Liquid ejection head 10 Liquid dispensing device 100 Piezoelectric actuator 101 Substrate 102 Insulating layer 110 Piezoelectric element 111 Lower electrode 112 Piezoelectric layer 113 Upper electrode 120 First protective layer 130 Second protective layer 140 upper wiring 150 Bottom wiring 160 Third Layer of Protection 180 The Fourth Layer of Protection

Claims

1. A piezoelectric actuator having a piezoelectric element including a first electrode, a piezoelectric layer, and a second electrode in this order from a substrate, and further having a first wiring electrically connected to the first electrode and a second wiring electrically connected to the second electrode, a first layer covering the piezoelectric element; a second layer disposed between the piezoelectric element and the first wiring and between the piezoelectric element and the second wiring; a third layer disposed so as to cover the first wiring, the second wiring, and a periphery of the piezoelectric layer in a plan view; A piezoelectric actuator having the above in this order from the substrate.

2. The piezoelectric actuator of claim 1 , wherein the third layer is more moisture resistant than the second layer.

3. The piezoelectric actuator according to claim 1 , wherein the second layer has a recess or an opening in a region overlapping with the piezoelectric layer in a plan view.

4. The piezoelectric actuator according to claim 1 , wherein the second layer is disposed so as to cover the piezoelectric layer in a plan view.

5. The piezoelectric actuator according to claim 1 , wherein the first layer has a thickness of 5 nm or more and 50 nm or less.

6. The piezoelectric actuator according to claim 1 , wherein the first layer has a thickness of 5 nm or more and 25 nm or less.

7. The piezoelectric actuator according to claim 1 , wherein the second layer has a thickness of not less than 200 nm and not more than 1.5 μm.

8. The piezoelectric actuator of claim 1 , wherein the third layer comprises silicon nitride.

9. 7. A piezoelectric actuator as claimed in claim 1, 5 or 6, wherein the first layer is made of aluminium oxide.

10. 7. The piezoelectric actuator according to claim 1, wherein the first layer is made of aluminum oxide and the second layer is made of silicon oxide.

11. The piezoelectric actuator according to claim 1 , further comprising a fourth layer disposed in contact with the first layer so as to cover the first layer in a plan view.

12. The piezoelectric actuator according to claim 11 , wherein the first layers and the fourth layers are alternately stacked in a plurality of layers.

13. The piezoelectric actuator according to claim 1 , wherein the first electrode and the first wiring are integrally formed as a same layer.

14. A liquid ejection head comprising the piezoelectric actuator according to claim 1 .

15. 2. A liquid ejection head comprising: an ejection port for ejecting liquid; a pressure chamber for supplying liquid to the ejection port; and the piezoelectric actuator according to claim 1, The liquid ejection head, wherein the substrate constitutes one of the walls of the pressure chamber.

16. 16. The liquid ejection head according to claim 14, for ejecting ink as the liquid.

Citation Information

Patent Citations

  • Electromechanical transducer, liquid discharge head, liquid discharge unit, device for discharging liquid, and piezoelectric device

    JP2020025082A