Anode thickness inspection tool and anode manufacturing method using the same
The anode thickness inspection jig simplifies and reduces costs for verifying anode ear thickness, ensuring proper anode dimensions through easy insertion checks and mold adjustments, preventing short circuits.
Patent Information
- Application Number
- JP2023069382
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-20
- Publication Date
- 2024-10-31
- Estimated Expiration
- 2043-04-20
AI Technical Summary
Existing anode thickness measurement techniques are complex, costly, and labor-intensive, making it difficult to determine if the thickness of anode ears is within an allowable range, which can lead to short circuits during electrolytic refining.
An anode thickness inspection jig with a pair of opposing sandwiching parts and a stepped connection, allowing easy insertion to verify if the ear thickness is within specified limits, using a metal rod or plate for gripping.
Enables simple and cost-effective inspection of anode ear thickness, facilitating efficient adjustment of anode molds to ensure proper thickness, thereby preventing short circuits.
Smart Images

Figure 2024155026000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an anode thickness inspection jig for inspecting whether the thickness of a specific portion of an anode produced by copper smelting is within a predetermined range, and a method for manufacturing an anode using this anode thickness inspection jig. [Background technology]
[0002] In dry copper smelting, raw materials mainly consisting of copper concentrate are subjected to a smelting process, a copper-making process, and a refining process to stepwise increase the copper grade, thereby producing electrolytic copper as a product. Specifically, in the smelting process, copper concentrate is first blown into a smelting furnace, such as a flash furnace, together with silica stone, and oxidized to produce matte with a copper content of about 60% by mass. Next, in the copper-making process, the matte is transferred from the flash furnace to a converter and further oxidized to produce blister copper with a copper content of about 98% by mass. Finally, in the refining process, the blister copper is transferred from the converter to a refining furnace to remove oxygen, producing refined blister copper with a copper content of 99% by mass or more, which is then cast to produce an anode for electrolysis (hereinafter simply referred to as an anode), which is then electrolytically refined to produce electrolytic copper with a copper content of 99.99% by mass or more.
[0003] In the above-mentioned anode casting, refined blister copper extracted from the above-mentioned refining furnace is cast through one or more troughs into a plurality of anode casting molds provided on a circular base called a turntable, thereby continuously casting a plurality of anodes. Each anode formed into a substantially rectangular plate shape by this casting is required to have a pair of ears protruding to the left and right from its upper end, each of which is required to have an appropriate thickness. The reason is that when a plurality of anodes are suspended in an electrolytic cell in the subsequent electrolytic refining step, each anode is supported by its own pair of ears. If the thickness of at least one of the pair of ears is outside the allowable range, the anode surfaces of adjacent anodes may not be parallel to each other and may approach each other at the lower end, causing a short circuit.
[0004] Therefore, various techniques have been proposed to confirm that the pair of ears of the cast anode have an appropriate thickness. For example, Patent Document 1 discloses a measuring device that measures the size of the bulge at the top of the anode and the bulge at the end of the anode during the anode casting process of copper smelting. The measuring device of Patent Document 1 includes a first air cylinder with a backing plate fixed to the rod so as to be parallel to the anode surface, a differential transformer held by a slide plate so as to move together with the backing plate in the operating direction of the air cylinder, and a second air cylinder, the rod of the air cylinder always protruding from the backing plate to the anode side and biased with a weaker pressure than the air cylinder, and the rod of the air cylinder and the core of the differential transformer are connected by a plate-shaped connector. In this way, when the rod of the first air cylinder is operated to extend the backing plate until it hits the end of the anode in order to measure the presence or absence of bulge, if there is no bulge at the anode, the tip of the rod hits the anode surface and is then pushed into the air cylinder body. On the other hand, it is described that if there is casting expansion, the depth to which the core is pressed becomes shorter, and the degree of casting expansion can be measured based on the degree of this shortening. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Japanese Utility Model Application Publication No. 4-106707 Summary of the Invention [Problem to be solved by the invention]
[0006] By adopting the technology of Patent Document 1, it would be possible to measure the size of inappropriate protruding parts during the casting of an anode or casting, but the thickness measurement in Patent Document 1 requires a measuring device with a complex mechanism, which increases the equipment costs and is also thought to require a lot of cost and effort for its maintenance. The present invention has been made in view of the above circumstances, and aims to provide a technology that can easily and inexpensively inspect whether the thickness of a specific part of an anode obtained by casting is within an allowable range. [Means for solving the problem]
[0007] In order to achieve the above-mentioned object, the anode thickness inspection jig of the present invention is an anode thickness inspection jig comprising a metallic inspection part consisting of a pair of opposing clamping portions spaced apart by a width equal to the upper limit of the allowable thickness of a specific portion of the anode and a connection portion connecting one ends of the pair of clamping portions, and a rod-shaped metallic gripping portion attached to the connection portion, wherein the inspection part has a step portion on its rear side which makes it one step narrower, and the width of the one step narrower is equal to the lower limit of the allowable thickness of the specific portion of the anode. Effect of the Invention
[0008] According to the present invention, it is possible to easily and at low cost inspect whether the thickness of a specific portion of an anode is within an allowable range. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1 is a schematic plan view of an electrolytic anode casting apparatus for casting an anode that is to be inspected by the anode thickness inspection jig of the present invention. [Diagram 2] 1 is a perspective view of an anode to be inspected by the anode thickness inspection jig of the present invention. FIG. [Diagram 3] FIG. 2 is a perspective view of an anode thickness inspection jig according to an embodiment of the present invention. [Figure 4] 4A is a front view, (b) a side view, (c) a plan view, and (d) a bottom view of the anode thickness inspection jig in FIG. [Diagram 5] FIG. 11 is a perspective view of another embodiment of the anode thickness inspection jig of the present invention. [Figure 6] FIG. 11 is a perspective view of still another embodiment of the anode thickness inspection jig of the present invention. [Figure 7] 4A is a perspective view showing a state in which the lug of an anode suspended on a suspension stand is being inspected using the anode thickness inspection jig of FIG. 3, and FIG. 4B is a perspective view showing a state in which the lug of an anode suspended in a cooling tank is being inspected using the anode thickness inspection jig of FIG. [Figure 8] 4 is a front view showing how the lug of the anode is judged as pass or fail using the anode thickness inspection jig of FIG. 3. [Figure 9] 1 is a perspective view showing a state in which a liner is inserted under an anode mold based on the inspection results of the anode thickness inspection jig of an embodiment of the present invention. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] 1. Electrochemical anode casting equipment First, a specific example of an electrolytic anode casting facility in which the anodes to be inspected by the anode thickness inspection jig of the present invention are cast will be described with reference to Fig. 1. The electrolytic anode casting facility shown in Fig. 1 is a so-called twin-wheel type anode casting facility consisting of two turntables, and is capable of continuously casting a plurality of anodes from refined blister copper consisting of a molten mass.
[0011] Specifically, the electrolytic anode casting equipment shown in FIG. 1 comprises two circular turntables 1 that rotate intermittently in the direction of the white arrow, a number of anode molds 2 mounted on each turntable 1 at equal intervals in the circumferential direction, a trough section 3 for sequentially pouring a fixed amount of refined crude copper (also called molten metal) made of a molten metal refined in a batchwise manner in a pre-stage refining furnace (not shown) into the anode molds 2, and a cooling device for spraying cooling water onto the molten metal sequentially poured into the anode molds 2 to cool and solidify it. The cooling system is mainly composed of a cooling device 4, a stripping machine 5 that strips the anode A solidified in the cooling device 4 from the anode mold 2, a release agent sprayer 6 that sprays a slurry release agent into the anode mold 2 to improve the releasability during stripping, a cooling tank 7 that cools the anode A stripped by the stripping machine 5, a suspension stand 8 that temporarily holds the anodes A cooled in the cooling tank 7 in a suspended state so that they can be transported by a forklift in groups of multiple anodes A, and a transfer machine 9 that lifts the anodes A from the cooling tank 7 and transfers them to the suspension stand. Note that, although an example in which 18 anode molds 2 are provided on the turntable 1 is shown in FIG. 1, the number of anode molds is not limited to this.
[0012] The anode A cast in the above-mentioned electrolysis anode casting equipment is immersed in the electrolytic solution while being suspended by the opposing side walls of the electrolytic cell as described above. Therefore, as shown in FIG. 2, the anode A has a pair of tabs A protruding to the left and right of the drawing at the upper corners of a substantially rectangular plate-shaped portion having a length and width of about 1000 to 1500 mm. L , A R The anode A has a pair of ears A L , A R In addition, the pair of chain conveyors and the suspension stand 8 in the cooling tank 7 described later are supported by the pair of lugs A L , A R It is supported by.
[0013] 2. Anode thickness inspection jig The anode thickness inspection jig according to the embodiment of the present invention is a jig for inspecting the thickness of an anode produced in the electrolytic anode casting facility. L , A R 3 and 4, an anode thickness inspection jig 10 according to an embodiment of the present invention is configured with a metallic gate-shaped inspection section 13 including a pair of mutually opposing, substantially rectangular plate-shaped clamping sections 11a, 11b and a substantially rectangular plate-shaped connecting section 12 connecting one ends of the pair of clamping sections 11a, 11b, and a metallic rod-shaped gripping section 14 erected in the center of the connecting section 12 on the side opposite to the side from which the pair of clamping sections 11a, 11b extend.
[0014] The gate-shaped inspection section 13 preferably has a thickness of 3 mm or more and 10 mm or less. If the thickness is less than 3 mm, the strength may decrease and the inspection section 13 may deform during use. Conversely, if the thickness exceeds 10 mm, it becomes difficult to insert the inspection section 13 into the gaps between the ears of adjacent anodes that are arranged in a row while suspended in the cooling tank 7. In addition, the inspection section 13 preferably has a width W of 10 mm or more and 30 mm or less and a height H of 40 mm or more and 100 mm or less when viewed from the direction in which the pair of clamping sections 11a, 11b move away from each other (i.e., the opposing direction) with the gripping section 14 extended directly upward. If the width W is less than 10 mm, the strength may decrease and the inspection section 13 may deform during use. Conversely, if the width W exceeds 30 mm, the inspection section 13 may not be able to insert the inspection section 13 into the gaps between the ears of the anodes to be inspected. L , A R When inspecting the thickness of the L , A R There is a risk that a thickness other than the intended thickness will be inspected.
[0015] The pair of clamping parts 11a and 11b in the inspection part 13 clamps the ear part A of the anode A to be inspected for thickness. L , A R The anodes 11a and 11b are spaced apart by a first width D1 that is equal to the upper limit of the allowable thickness of the anode 1. Furthermore, at least one of the pair of clamping portions 11a and 11b is provided with a step 15 at the connection point with the connection portion 12, and this makes the portion behind the step 15 narrower by one step. The second width D2 at the portion that is one step narrower behind the step 15 is equal to the second width D2 at the portion that is one step narrower behind the step 15. L , A R This corresponds to the lower limit of the allowable thickness.
[0016] The first width D1 is preferably in the range of 35 mm to 55 mm. On the other hand, the second width D2 narrower than the first width D1 is preferably in the range of 20 mm to 40 mm. This allows the width of the ear A of the anode A, which is generally handled in copper smelting and has a mass of about 300 kg to 500 kg per sheet, to be reduced. L , A RIn FIG. 3, the step 15 is provided perpendicular to the clamping portion 11a, but the present invention is not limited to this, and a step that is gradually narrower may be provided. L , A R This makes it easier to guide the liquid to the back side of the step portion 15.
[0017] Furthermore, the shape of the inspection part 13 is not limited to the structure in which a bent part having a substantially L-shaped cross section is provided at the corner where one of the pair of clamping parts 11a, 11b and the connection part 12 are joined as shown in FIG. 3, as long as the inspection part 13 has a front part having a first width D1 and a part having a second width D2 narrower than the first width D1, the bent part is located on the rear side of the step part 15. For example, as shown in FIG. 5(a) as an anode thickness inspection jig 20 of another embodiment, one of the pair of clamping parts 21a, 21b may be bent at two places to provide a step part 25, or as shown in FIG. 5(b) as an anode thickness inspection jig 30 of another embodiment, both of the pair of clamping parts 31a, 31b may be bent at two places to provide step parts 35a, 35b. Note that providing a step only in one of the pair of clamping parts 21a, 21b in the former embodiment is advantageous in that the ear part A of the anode A is located on the rear side of the step. L , A R This is preferable because it is easy to derive the above.
[0018] Furthermore, the inspection part may be formed of the same metal rod as the grip part, instead of the metal plate. That is, as in the anode thickness inspection jig 40 of another embodiment shown in FIG. 6(a), one of the pair of clamping parts 41a, 41b made of a metal rod may be bent at two places to provide a step part 45, or as in the anode thickness inspection jig 50 of another embodiment shown in FIG. 6(b), both of the pair of clamping parts 51a, 51b made of a metal rod may be bent at two places to provide step parts 55a, 55b. When the inspection part is formed of a metal rod in this way, although the strength is slightly lower than that of the anode thickness inspection jig of FIG. 3 or FIG. 5 formed of the above-mentioned metal plate, it can be made lighter and at a lower cost.
[0019] Using the anode thickness inspection jig 10 according to the embodiment of the present invention, the ear A of the anode A is L , A R When inspecting, anode A must be connected to ear A. L , A R For example, as shown in FIG. 7(a), in a suspension base 8 used for lifting by hooking with the claws F of a forklift, lugs A are provided on the upper ends of both side walls. L , A R It is preferable to carry out the inspection on the anode A in a suspended state with the respective electrodes mounted thereon.
[0020] Alternatively, as shown in FIG. 7(b), in the cooling tank 7, a chain conveyor 7b driven by a motor 7a is provided in the tank, and the lugs A of the anode A are attached to the upper surface of the endless tracks on both sides of the chain conveyor 7b. L , A R By placing the lug A on the endless track, the anode A is transported in the longitudinal direction of the cooling tank 7 while being immersed in the cooling water in the tank and cooled. L , A R When the ear A is placed L , A R In this case, the anode thickness inspection tool 10 can be simply moved up and down relative to the automatically transported anode A, making it possible to perform the inspection extremely simply and efficiently.
[0021] The above-mentioned anode thickness inspection jig 10 is used to inspect the ear A. L , A R In the inspection of the ear A L , A R The pass / fail can be easily judged by whether the inspection part 13 can be sandwiched between the anode A and the left ear A. L When inspecting, as shown in FIG. 8(a), the front side of the inspection unit 13 is clamped by a pair of clamping parts 11a and 11b. L However, the ear A is located on the back side of the step 15. L If it is not possible to pinch the ear A LSince the thickness satisfies both the upper and lower limit requirements of the allowable range, it can be judged as being acceptable. On the other hand, as shown in FIG. 8(b), the ear A of the anode A L If it is possible to sandwich the ear A behind the step portion 15, L Since the thickness of the ear A of the anode A is below the lower limit of the allowable range, it can be judged as a failure. L If the left ear A cannot be clamped by the pair of clamping parts 11a, 11b at the front side of the inspection part 13, L Since the thickness of exceeds the upper limit of the tolerance, it can be judged as a failure.
[0022] As described above, by using the anode thickness inspection jig according to the embodiment of the present invention, L , A R Thus, simply by checking whether the inspection portion of the anode thickness inspection tool can be clamped against a specific portion of anode A, it is possible to easily determine whether the thickness of that specific portion exceeds the upper limit of the allowable range or is below the lower limit of the allowable range.
[0023] 3. Anode manufacturing method Next, a method for producing an anode for copper electrolysis using the anode thickness inspection jig according to the embodiment of the present invention will be described. The method for manufacturing this anode includes a casting process in which refined breeze copper with a copper content of 99% or more produced in a previous smelting furnace is transported using one or more troughs, and then sequentially cast into a plurality of anode molds placed at equal intervals circumferentially on an intermittently rotating turntable; a solidification process in which cooling water is sprayed onto the refined breeze copper cast into the anode mold to cool and solidify the anode; a stripping process in which the solidified anode is peeled off from the anode mold; a cooling process in which the peeled off anode is supported by its ears on both sides and suspended, and immersed in cooling water in a cooling tank to cool it; and a suspension process in which the anodes A cooled in the cooling tank are temporarily held in a suspended state on a suspension stand for transport by a forklift in groups of several, and an inspection is performed to see whether the ears of the anodes suspended in the cooling tank can be clamped between the front and back sides of the inspection portion 13 of the anode thickness inspection jig 10.
[0024] As a result of the above inspection, the ear A of anode A L , A R If at least one of the thicknesses is outside the allowable range, a wedge-shaped or plate-shaped liner L is used under the corresponding anode mold 2 on the turntable 1 on which the anode A was cast, as shown in FIG. 9, to adjust the height of the four corners of the anode mold 2 in a plan view. For example, L If the thickness of the left ear A exceeds the upper limit of the tolerance, L This means that there is too much refined blister copper in the part where the ear A is cast. L As shown in Figure 9, a liner L is inserted under the part to be cast, or if a liner is already inserted in this part, its thickness is increased. L This allows the height of the casting area to be relatively increased, thereby reducing the amount of refined blister copper that enters this area.
[0025] Conversely, the left ear A of anode A LIf the thickness of the left ear A is below the lower limit of the allowable range, L Therefore, the amount of refined blister copper that can be cast into the anode mold 2 is insufficient. L If a liner is already inserted under the part to be cast, remove it or replace it with a thinner one, or insert liner L in another part. This will L Since the height of the part where the copper is cast can be relatively lowered, a large amount of refined blister copper can be introduced into this part.
[0026] The above describes an anode thickness inspection jig according to an embodiment of the present invention and a method for manufacturing an anode using the inspection jig, but the present invention is not limited to the above embodiment and can include various modifications and alternatives within the scope of the present invention. For example, the anode thickness inspection jig according to the above embodiment of the present invention inspects the thicknesses of the left and right ears of the anode, but is not limited to this and may inspect the thickness of, for example, the upper, side, or lower part of a substantially rectangular plate-shaped portion of the anode. EXAMPLES
[0027] Anodes to be electrolytically refined in copper smelting were manufactured using an anode casting facility as shown in Fig. 1. Specifically, refined blister copper with a copper content of 99% or more produced in a smelting furnace was discharged from the smelting furnace and transported using three troughs 3, and the refined blister copper was cast in sequence into 18 anode molds placed on two turntables 1 while they were intermittently rotating, and the refined blister copper was solidified by spraying cooling water with a cooling device 4. Thereafter, the anode A was stripped from the anode mold by a stripping machine 5, and its ears A were removed. L , A R The anodes A were suspended by being supported by a chain conveyor 7b in the cooling tank 7 and immersed in the cooling water. After this, the anodes A cooled in the cooling tank were temporarily held in a suspended state on a suspension stand 8 in order to be transported by a forklift in groups of several anodes A. The anodes A were suspended on the suspension stand 8. L , A RThe thickness of each anode was inspected using an anode thickness inspection jig 10 having a shape shown in FIG.
[0028] In this anode thickness inspection jig 10, a gate-shaped inspection section 13 consisting of a pair of clamping sections 11a, 11b and their connection section 12 is formed from a metal plate with a thickness of 5 mm, a width W of 30 mm, and a height H of 50 mm, and a single iron round bar with a length of 500 mm and a diameter of 10 mm is erected as a gripping section 14 at the center of the outer side of the connection section 12. Furthermore, an L-shaped step section 15 is provided on the inside of the inspection section 13 at the corner where the right side 11a of the pair of clamping sections 11a, 11b and the connection section 12 are joined. This allows the pair of clamping sections 11a, 11b to be positioned at the ear A of the anode A. L , A R The anodes are spaced apart from each other by a first width D1 equal to the upper limit of the allowable thickness of the anodes. L , A R The second width D2 is equal to the lower limit of the allowable thickness of the first step.
[0029] The gripping portion 14 of the anode thickness inspection jig 10 is gripped, and the lug A of the anode A supported by the chain conveyor 7b in the cooling tank as shown in FIG. L , A R It was checked whether the test piece 13 could be sandwiched between the front and rear sides of the test piece 13. That is, as shown in FIG. L , A R In contrast, if the anode can be sandwiched in front of the inspection section 13 separated by a first width D1, but cannot be sandwiched behind the step section 15 separated by a second width D2 (FIG. 8(a)), it is judged as passing, whereas if the anode can be sandwiched behind the step section 15 (FIG. 8(b)) or cannot be sandwiched in front of the inspection section 13 (FIG. 8(c)), it is judged as failing. Then, for the anode mold 2 from which the anode was cast that was judged to be failing as a result of the above judgment, the thickness of the liner L was adjusted as shown in FIG. 9 to reduce the width of the ear section A in the anode mold 2. L , A R The height of the part where it is cast has been adjusted.
[0030] Anodes were produced from 72 batches of refined crude copper in the refining furnace by the above-mentioned method. Then, for each batch, 36 anodes A were inspected for their thickness using the above-mentioned anode thickness inspection jig 10 at 1 hour, 3 hours, and 5 hours after the start of casting. L , A R As a result, it was possible to adjust the height of 0.5 anode molds 2 per batch on average.
[0031] As a comparative example, without using the above-described anode thickness inspection jig 10, an anode was removed from the cooling tank 7 and moved to an anode storage area using a forklift. In the anode storage area, a worker measured the thickness of the ear A using a vernier caliper. L , A R Other than that, anodes were produced from 22 batches of refined crude copper in the refining furnace in the same manner as in the above-mentioned Example. In this Comparative Example, the same amount of work time as in the Example was spent on the process, and the thickness of the ears A of 18 anodes A was measured once every 11 batches. L , A R Therefore, on average, the height of only two anode molds 2 per 11 batches could be adjusted.
[0032] As described above, by using the anode thickness inspection jig 10 that satisfies the requirements of the present invention, the thickness of the ear portion of the anode can be easily inspected. As a result, in the embodiment, it was possible to inspect, on average, more than 60 times as many anodes per batch compared to the comparative example. Based on the inspection results, the height of the anode mold could be finely adjusted in the embodiment. [Explanation of symbols]
[0033] 1 Turntable 2 Anode mold 3 Hibe 4 Cooling device 5 Peeling machine 6 Release agent sprayer 7 Cooling tank 7a Drive motor 7b Means of transport 8 Suspension platform 9 Transfer machine 10, 20, 30, 40, 50 Anode thickness inspection jig 11a, 21a, 31a, 41a, 51a Right side of clamping part 11b, 21b, 31b, 41b, 51b Left side of clamping part 12, 22, 32, 42, 52 Connections 13, 23, 33, 43, 53 Inspection Department 14, 24, 34, 44, 54 Grip part 15, 25, 35a, 35b, 45, 55a, 55b Step A Anode F Forklift claw L Liner
Claims
1. An anode thickness inspection jig comprising a metallic inspection part consisting of a pair of opposing clamping portions spaced apart by a width equal to the upper limit of the allowable thickness of a specific portion of an anode and a connection portion connecting one ends of the pair of clamping portions, and a metallic rod-shaped gripping portion attached to the connection portion, wherein the inspection part has a step portion on its rear side which makes it one step narrower, and the width of the one step narrower is equal to the lower limit of the allowable thickness of the specific portion of the anode.
2. 2. The anode thickness inspection jig according to claim 1, wherein the inspection portion consisting of the pair of clamping portions and the connection portion has a thickness of 3 mm or more and 10 mm or less, a width of 10 mm or more and 30 mm or less, and a height of 40 mm or more and 100 mm or less, when the inspection portion is viewed from a direction in which the pair of clamping portions separate with the gripping portion directly above.
3. 3. The anode thickness inspection jig according to claim 2, wherein the upper limit of the allowable thickness is 35 mm or more and 55 mm or less, and the lower limit of the allowable thickness is 20 mm or more and 40 mm or less.
4. 2. The anode thickness inspection jig according to claim 1, wherein the step portion is a bent portion having a substantially L-shaped cross section provided at a corner where one of the pair of clamping portions and the connecting portion are joined.
5. 2. A method for manufacturing an anode for copper electrolysis, comprising the steps of: transporting refined blister copper having a copper content of 99% or more produced in a smelting furnace using one or more troughs, and sequentially casting the refined blister copper cast into a plurality of anode molds placed at equal intervals in the circumferential direction on an intermittently rotating turntable; cooling and solidifying the refined blister copper cast into the plurality of anode molds; peeling the anodes cast from the plurality of anode molds; cooling the peeled anodes by immersing them in cooling water while suspended by lugs on both sides; and holding a plurality of the cooled anodes together in a suspended state on a suspension stand, wherein the method for manufacturing an anode comprises the steps of: inspecting whether the thickness of a specific portion of the anode in the suspended state is within an allowable range by determining whether the inspection portion of the anode thickness inspection jig according to claim 1 can be clamped into the specific portion of the anode in the suspended state.
6. 6. The method for manufacturing an anode according to claim 5, wherein, if the result of the inspection indicates that the thickness of the specific portion of the anode is not within the allowable range, the height of the anode mold placed on the turntable is adjusted by a liner.
Citation Information
Patent Citations
The gate of the di -
JP1983187702U
Deciding method for thickness propriety of anode plate for electrolysis
JP1988052007A
Formation of anode and method for measuring anode thickness
JP2000096280A
A copper anode to cast measuring device
JP1992106707U