Division method for wafer

By expanding grooves before cleaning, the method efficiently removes slurry, addressing inefficiencies in existing wafer dividing processes and reducing cleaning time.

JP2024156367APending Publication Date: 2024-11-06DISCO CORP

Patent Information

Application Number
JP2023070767
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-24
Publication Date
2024-11-06

AI Technical Summary

Technical Problem

Existing wafer dividing methods face inefficiencies in removing slurry from narrow cutting grooves, leading to prolonged cleaning times.

Method used

A method involving a series of steps including holding, groove formation, expansion, polishing, and cleaning, where the expansion step precedes cleaning, allowing for efficient removal of slurry from widened grooves using a cleaning fluid.

Benefits of technology

The method significantly reduces cleaning time by effectively removing slurry from expanded grooves, enabling faster wafer division.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024156367000001_ABST
    Figure 2024156367000001_ABST
Patent Text Reader

Abstract

To reduce a time required for a cleaning step.SOLUTION: A division method for a wafer W for dividing the wafer, in which each device is formed in a plurality of regions of a front surface divided by a lattice-like street, along the street contains: a holding step of holding the wafer W by a chuck table 1 via a tape T adhered to its back surface; a groove formation step of forming a plurality of grooves W1 along the street to the front surface of the wafer W held by the chuck table 1; an expansion step of expanding each groove W1 to have a predetermined width b2 by expanding the tape T in a radial direction of the wafer W; a polishing step of polishing the front surface of the wafer W by a polishing pad while supplying slurry to the wafer W; and a cleaning step of injecting a cleaning fluid to the front surface of the wafer W, and cleaning both of the front surface of the wafer W and each groove W1. The cleaning step is executed after the expansion step.SELECTED DRAWING: Figure 9
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a wafer dividing method for dividing a wafer along lattice-like streets (planned dividing lines). [Background technology]

[0002] For example, in the manufacturing process of semiconductor devices, the surface of a disk-shaped semiconductor wafer (hereinafter simply referred to as a "wafer") is divided into a number of device regions by streets (planned division lines) formed in a grid pattern, and devices such as ICs and LSIs are formed in each device region. Then, by dividing the wafer on which a large number of devices are thus formed along the streets, a number of chips are manufactured.

[0003] Here, methods for dividing a wafer along the streets include blade dicing, which involves cutting the wafer along the streets with a cutting blade to form kerfs, plasma dicing, which involves dry etching in a vacuum to form grooves in the wafer along the streets, and laser ablation, which involves irradiating the wafer surface with a laser beam to form grooves in the wafer along the streets.

[0004] Incidentally, in the wafer dividing method proposed in Patent Document 1, the surface of the wafer after cutting with a cutting blade is subjected to CMP (Chemical Mechanical Polishing) using a polishing liquid, slurry, to remove processing debris adhering to the surface of the wafer, and then a cleaning step is carried out in which cleaning water is sprayed onto the surface of the wafer to remove the slurry adhering to the surface of the wafer in the CMP polishing. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2020-170741 A Summary of the Invention [Problem to be solved by the invention]

[0006] However, in the cleaning step performed in the wafer dividing method proposed in Patent Document 1, it is not easy to remove the slurry remaining in the narrow cutting groove (kerf) formed in the surface of the wafer by cutting with the cutting blade, and the cleaning step takes a long time, making it inefficient.

[0007] The present invention has been made in consideration of the above problems, and an object of the present invention is to provide a method for dividing a wafer that can efficiently remove slurry remaining in grooves formed in a wafer by cleaning in a short period of time, thereby shortening the time required for the cleaning step. [Means for solving the problem]

[0008] In order to achieve the above object, the present invention provides a method for dividing a wafer along a plurality of areas on the surface of the wafer, the areas being partitioned by lattice-like streets, the method comprising the steps of: holding the wafer on a chuck table via a tape attached to the back surface of the wafer; forming a plurality of grooves along the streets on the surface of the wafer held on the chuck table; expanding the tape in the radial direction of the wafer to expand the grooves to a predetermined width; polishing the surface of the wafer with a polishing pad while supplying a slurry to the front side of the wafer, thereby removing deposits that have adhered to the surface of the devices during the groove forming step; and cleaning the surface of the wafer and the grooves by spraying a cleaning fluid onto the surface of the wafer, the cleaning step being performed after the expansion step. Here, the polishing step may be performed after the expansion step, and the cleaning step may be performed after the polishing step, or the expansion step may be performed after the polishing step, and the cleaning step may be performed after the expansion step. Effect of the Invention

[0009] According to the present invention, the widening step is carried out before the cleaning step, and the cleaning step is carried out in a state in which the width of the groove formed in the wafer in the groove forming step is widened by the widening step, so that the slurry remaining in the widened groove is efficiently removed in a short time by the sprayed cleaning fluid, thereby shortening the time required for the cleaning step and enabling the wafer to be divided efficiently in a short time. [Brief description of the drawings]

[0010] [Figure 1] 1 is a flowchart showing the process steps of a wafer dividing method according to a first embodiment of the present invention. [Diagram 2] FIG. [Diagram 3] FIG. [Figure 4] 3 is a side cross-sectional view showing a holding step in the wafer dividing method according to the first embodiment of the present invention. FIG. [Diagram 5] 5(a) to 5(c) are side cross-sectional views showing a groove forming step in the wafer dividing method according to the first embodiment of the present invention in the order of steps. [Figure 6] 10 is a side cross-sectional view showing another mode of a groove forming step in the wafer dividing method according to the first embodiment of the present invention. FIG. [Figure 7] 5(a) to 5(c) are side cross-sectional views showing, in order of steps, expansion steps in the wafer dividing method according to the first embodiment of the present invention. [Figure 8] FIG. 2 is a cutaway side view showing a polishing step in the wafer dividing method according to the first embodiment of the present invention. [Figure 9] 3 is a side cross-sectional view showing a cleaning step in the wafer dividing method according to the first embodiment of the present invention. FIG. [Figure 10] 10 is a flowchart showing the process steps of a wafer dividing method according to a second embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, an embodiment of the present invention will be described with reference to the accompanying drawings.

[0012] First Embodiment First, a wafer dividing method according to a first embodiment of the present invention will be described. As shown in FIG. 1, the wafer dividing method includes the following steps: 1) Holding process 2) Groove formation process 3) Expansion process 4) Polishing process 5) Cleaning process The above steps are carried out in this order to divide a wafer W (see FIGS. 2 and 3) into a plurality of chips C (see FIGS. 5(c) and 6).

[0013] Here, the wafer W to be divided is, for example, a thin disk-shaped member made of single crystal silicon (Si) as shown in Fig. 2, and its surface (the upper surface in Fig. 2) is partitioned into a plurality of rectangular regions by mutually orthogonal streets (planned division lines) L1, L2 arranged in a lattice pattern, and devices D such as ICs and LSIs are formed in each rectangular region. The wafer W having a large number of devices D formed on its surface is then incorporated into a work set WS shown in Fig. 3, and the above-mentioned processes are carried out on the wafer W. Note that, as the material of the wafer W, silicon carbide (SiC), glass, ceramics, sapphire, etc., can be used in addition to silicon (Si).

[0014] As shown in Fig. 3, the work set WS is configured by bonding the back surface (lower surface in Fig. 3) of a disk-shaped wafer W to a heat-shrinkable tape T that is attached to cover a circular opening of a ring-shaped ring frame F, thereby supporting the wafer W on the ring frame F via the tape T and integrating the wafer W, the ring frame F, and the tape T. The material of the tape T is not particularly limited as long as it has both elasticity and heat shrinkability, but for example, a two-layer structure in which a glue layer is laminated on a base layer made of polyolefin, polyvinyl chloride, polypropylene, etc. is used. This tape T has an outer diameter at least larger than the diameter of the wafer W, and the tape T1, which is a ring-shaped exposed portion between the outer circumference of the wafer W and the inner circumference of the ring frame F, is a portion that is likely to become loose after the tape T is expanded in the expansion process described below (see Fig. 7(c)).

[0015] Next, each of the steps in the method for dividing the wafer W according to the first embodiment of the present invention will be described (see FIG. 1).

[0016] 1) Holding process: 4, the holding step is a step of suction-holding the work set WS on the holding surface 2a of the chuck table 1, and the wafer W is suction-held on the holding surface 2a of the chuck table 1 via a tape T attached to the back surface (the lower surface in FIG. 4). Here, a disk-shaped porous member 2 made of a porous material such as porous ceramic is incorporated in the upper center of the chuck table 1, and the upper surface of this porous member 2 constitutes the holding surface 2a.

[0017] The porous member 2 is connected to a suction source 4 such as a vacuum pump or an ejector by a pipe 3, and an electromagnetic opening / closing valve V1 is provided on the pipe 3. Therefore, as shown in Fig. 4, when the work set WS is placed on the holding surface 2a of the chuck table 1 with the tape T facing down and the suction source 4 is driven to open the opening / closing valve V1, the porous member 2 of the chuck table 1 is evacuated by the suction source 4, generating a negative pressure on the holding surface 2a, and the work set WS together with the wafer W is sucked and held on the holding surface 2a of the chuck table 1 by this negative pressure.

[0018] 2) Groove formation process: The groove forming step is a step of forming lattice-shaped grooves W1 (see FIG. 5(c)) along the streets L1 and L2 (see FIG. 2) on the surface of the wafer W held by suction together with the work set WS on the holding surface 2a of the chuck table 1. In this embodiment, plasma dicing is used as a method for forming the grooves W1 on the wafer W. This plasma dicing is as follows: 2-1) Protective film formation process 2-2) Protective film groove formation process 2-3) Plasma etching process Through these steps, a grid-like groove W1 is formed in the wafer W. Each step will be described below.

[0019] 2-1) Protective film formation process: In the protective film forming process, as shown in FIG. 5(a), the surface of the wafer W (device D) is covered with a water-soluble resin film (hereinafter referred to as a "protective film") P, which is a mask material, and when forming this protective film P, a water-soluble liquid resin is dropped from above the center of the wafer W by a nozzle 5. Here, the nozzle 5 is supported by a holder 7 that can be moved horizontally in the radial direction of the wafer W by a horizontal movement mechanism 6, and a liquid resin supply source 8 is connected to this nozzle 5. Note that polyvinyl alcohol (PVA), polyvinylpyrrolidone (PVP), etc. are used as the water-soluble liquid resin.

[0020] Thus, when the liquid resin supplied from the liquid resin supply source 8 to the nozzle 5 is dropped from the nozzle 5 toward the center of the upper surface of the wafer W, the chuck table 1 is rotated around its axis together with the work set WS in the direction of the arrow in the figure (counterclockwise direction) by a rotation mechanism (not shown). Then, the wafer W also rotates in the same direction, and the liquid resin dropped onto the center of the upper surface of the wafer W spreads around due to centrifugal force, forming a protective film P of a certain thickness as a mask layer on the upper surface of the wafer W. Thereafter, when the protective film P dries and hardens, the upper surface of the wafer W is covered with the protective film P that functions as a mask layer.

[0021] 2-2) Protective film groove forming process: In the protective film groove forming process, a protective film groove P1 is formed by removing a portion of the protective film P formed on the surface of the wafer W in the protective film forming process that is along the streets L1, L2 (see FIG. 2) of the wafer W. In this protective film groove forming process, as shown in FIG. 5(b), a laser beam emitted from a laser head LH is irradiated onto the streets L1, L2 (see FIG. 2) of the wafer W in the portion where the protective film groove P1 of the protective film P is to be formed, and the streets L1, L2 of the wafer W are melted by the irradiation of the laser beam, and the protective film P evaporates due to the heat generated by melting the wafer W, forming the protective film groove P1 in the protective film P. Note that a laser beam having a wavelength that is absorbent by the wafer W is emitted from the laser head LH.

[0022] Specifically, when the chuck table 1 is indexed in the horizontal direction (left and right direction in FIG. 5(b)) by the horizontal movement mechanism 9 and the position on the protective film P where the laser beam is irradiated is positioned relative to the laser head LH, the laser head LH moves in the vertical direction of the paper in FIG. 5(b) while irradiating the laser beam, thereby forming protective film grooves P1 along one direction (up and down direction on the paper in FIG. 5(b)). Then, when the formation of all the protective film grooves P1 along this one direction is completed, the chuck table 1 is rotated by an angle of 90° around the axis center by a rotation mechanism (not shown), and protective film grooves P1 along the other direction are similarly formed. Then, a lattice-like protective film grooves P1 that are perpendicular to each other are formed in the protective film P.

[0023] 2-3) Plasma etching process: In the plasma etching process, a lattice-shaped groove W1 (see FIG. 5(c)) is formed by plasma etching in a portion of the wafer W corresponding to the protective film groove P1 formed in the protective film P in the protective film groove formation process (the portion along the lattice-shaped streets L1, L2 (see FIG. 2)).

[0024] 5(c), the work set WS is placed, with the tape T facing down, on the holding surface of an electrostatic chuck table 11 housed in a reduced pressure chamber S of a plasma etching apparatus 10. When a DC voltage is applied from a DC power supply 14 to a pair of electrodes 12, 13 for electrostatic attraction provided on the electrostatic chuck table 11, an electrostatic attraction force is generated on the holding surface of the electrostatic chuck table 11, and the work set WS is attracted and held on the holding surface of the electrostatic chuck table 11 by this electrostatic attraction force.

[0025] In the above state, the pressure in the decompression chamber S is reduced, and while the electrostatic chuck table 11 is cooled by a cooling unit (not shown), a plasma gas 15 is generated by a gas supply mechanism and a plasma generation mechanism (not shown) and the plasma gas 15 is supplied to the decompression chamber S. Then, the part of the wafer W that is not covered by the protective film P (the lattice-shaped part in which the protective film grooves P1 of the protective film P are formed) is exposed to highly reactive particles in the plasma gas 15, and this part is etched to form a lattice-shaped groove W1 along the streets L1, L2 (see FIG. 2) in the wafer W. In this way, the lattice-shaped grooves W1 are formed in the wafer W, and the wafer W is divided along the grooves W1, and a plurality of chips C each having a device D mounted thereon are obtained. For example, SF6 (fluorine-based gas) is used as the plasma gas 15.

[0026] Incidentally, a protective film (water-soluble resin film) P remains on the surface of the wafer W on which the lattice-shaped grooves W1 are formed by the above-mentioned plasma dicing, so when cleaning water is sprayed onto the surface of the wafer W, the protective film P is dissolved and removed by the cleaning water.

[0027] In the groove forming step, blade dicing shown in Fig. 6 can be used as a method for forming lattice-shaped grooves W1 along the streets L1, L2 (see Fig. 2) in the wafer W. That is, as shown in Fig. 6, the wafer W held by suction together with the work set WS on the holding surface 2a of the chuck table 1 is cut (full cut) by a disk-shaped cutting blade 16 rotating in the direction of the arrow in the figure, thereby forming lattice-shaped grooves W1 in the wafer W. In Fig. 6, the same elements as those shown in Fig. 4 are denoted by the same reference numerals.

[0028] Specifically, the chuck table 1 can be moved in the left-right direction and the direction perpendicular to the paper surface of FIG. 6 by a horizontal movement mechanism (not shown). When a groove W1 along one direction (the direction perpendicular to the paper surface of FIG. 6) is formed, the horizontal movement mechanism indexes the chuck table 1 and the wafer W in the left-right direction of FIG. 6 to determine the position to cut the wafer W relative to the cutting blade 16, and the cutting blade 16 cuts the wafer W along the one direction (the direction perpendicular to the paper surface of FIG. 6) while moving the chuck table 1 and the wafer W in the direction perpendicular to the paper surface of FIG. 6, forming the groove W1 along the one direction (the direction perpendicular to the paper surface of FIG. 6) in the wafer W. When the formation of all the grooves W1 along one direction is completed in this way, the chuck table 1 rotates by an angle of 90°, and the grooves W1 along the other direction are formed in the same way. Then, the wafer W is formed with lattice-like grooves W1 that are orthogonal to each other. In this way, the wafer W is divided along the grooves W1 by forming the lattice-like grooves W1 on the wafer W, and a plurality of chips C on each of which a device D is mounted are obtained.

[0029] 3) Expansion process: In the above groove forming process, lattice-shaped grooves W1 are formed in the wafer W along the streets L1, L2 (see Figure 2) and the wafer W is divided into multiple chips C. In the expansion process, which is carried out through the steps shown in Figures 7(a) to 7(c), the tape T is expanded radially outward in the radial direction of the wafer W, thereby widening the width of the lattice-shaped grooves W1 formed in the wafer W.

[0030] Here, we will explain the equipment used in the expansion process.The equipment has as its main components a table 20 that holds the portion (central portion) of the work set WS corresponding to the wafer W, a frame holding section 30 that holds the ring frame F of the work set WS, a lifting mechanism 40 that raises and lowers the table 20 and the frame holding section 30 relative to one another, and a thermal shrinkage means 50 that heats the ring-shaped tape T1 between the outer periphery of the wafer W and the inner periphery of the ring frame F to thermally shrink the tape T1.

[0031] The table 20 is a disk-shaped member, and a first suction section 21 is provided in the center of the upper surface thereof to suction and hold the center of the tape T of the work set WS. A ring-shaped second suction section 22 is formed on the radial outside of the first suction section 21 so as to surround the first suction section 21. The first suction section 21 is connected to a first suction source 24 via a pipe 23, and the second suction section 22 is connected to a second suction source 26 via a pipe 25. The pipes 23 and 25 are provided with electromagnetic opening and closing valves V2 and V3, respectively. The table 20 is also provided with elongated round rod-shaped rollers 27 rotatably disposed along its outer periphery. These rollers 27 rotate in contact with the tape T when the tape T is expanded as described later, thereby reducing friction with the tape T generated at the outer periphery of the table 20.

[0032] The frame holding section 30 includes a mounting plate 31 on which the lower surface of the ring frame F is placed, and a cover plate 32 that holds down the upper surface of the ring frame F. Circular holes 31a, 32a having an inner diameter larger than the outer diameter of the table 20 are respectively opened in the centers of the mounting plate 31 and the cover plate 32. The mounting plate 31 and the cover plate 32 can be raised and lowered by a lifting mechanism 40 described later while holding the ring frame F of the work set WS therebetween.

[0033] The lifting mechanism 40 lifts and lowers the frame holding part 30, and is composed of a plurality of cylinder mechanisms 41 (only two are shown in FIG. 7) that support the mounting plate 31 so that it can be lifted and lowered. Here, each cylinder mechanism 41 is composed of a vertically erected cylinder 42, a piston (not shown) fitted in the cylinder 42 so as to be able to slide up and down, and a piston rod 43 that extends upward from the piston through the cylinder 42, and the mounting plate 31 is attached to the upper end of each piston rod 43. Although not shown, the interior of each cylinder 42 is divided into an upper chamber and a lower chamber by the piston.

[0034] Therefore, in each cylinder mechanism 41, if compressed air, for example, is supplied to the lower chamber of the cylinder 42 while the air in the upper chamber is exhausted, the piston rod 43 rises and the mounting plate 31 also rises, and conversely, if compressed air is supplied to the upper chamber while the air in the lower chamber is exhausted, the piston rod 43 descends and the mounting plate 31 also descends.

[0035] 7(c), the heat shrinking means 50 is disposed above the table 20, and includes a pair of heaters 52 attached to both ends of a horizontal arm 51 sandwiching the center of the wafer W, a lifting section 53 provided in the center of the arm 51, and a rotating means 54 for rotating the pair of heaters 52 about the center of the wafer W. Here, each heater 52 is composed of a far-infrared heater or the like, and can irradiate a spot with far-infrared rays having a predetermined peak waveform.

[0036] Thus, the tape T is expanded by the device configured as above in the following manner.

[0037] 7(a), the work set WS is held horizontally by the frame holding part 30 and placed on the upper surface of the table 20. At this time, the opening and closing valves V2 and V3 are both closed, so that the first suction part 21 and the second suction part 22 of the table 20 are not sucked by the first suction source 24 and the second suction source 26. Note that the second suction part 22 and the opening and closing valve V3 are not essential and do not necessarily have to be provided.

[0038] From the above state, as shown in FIG. 7(b), when the lifting mechanism 40 is driven and the piston rods 43 of the cylinder mechanisms 41 are lowered, the frame holding portion 30 holding the ring frame F of the work set WS is lowered together with the piston rods 43. Then, since the ring frame F of the work set WS is positioned lower than the table 20, the tape T is radially expanded by this ring frame F. At this time, since both opening and closing valves V2 and V3 remain closed, the first suction source 24 and the second suction source 26 do not suck the first suction portion 21 and the second suction portion 22 of the table 20 (suction holding of the work set WS), and the width of the lattice-like grooves W2 formed on the wafer W is expanded. Specifically, compared to the width b1 of the groove W1 of the wafer W shown in FIG. 7(a) before the tape T is expanded, the width b2 of the groove W2 of the wafer W shown in FIG. 7(b) after the tape T is expanded becomes larger (b2>b1). During expansion of the tape T, the tape T is not sucked by the first suction portion 21 and the second suction portion 22 of the table 20, so that the tape T can be expanded smoothly. In addition, friction between the tape T and the table 20 when expanding the tape T is reduced by the rotation of the multiple rollers 27, so that the tape T can be expanded smoothly.

[0039] As described above, when the tape T is expanded and the width of the groove W1 of the wafer W is expanded from b1 to b2, as shown in Fig. 7(c), both opening and closing valves V1 and V2 are opened, and the first suction source 24 and the second suction source 26 respectively evacuate the first suction portion 21 and the second suction portion 22 of the table 20, generating negative pressure in the first suction portion 21 and the second suction portion 22, and the tape T is sucked and held on the upper surface of the table 20 by this negative pressure. Therefore, the width of the groove W1 of the wafer W is maintained at the expanded width b2.

[0040] Then, the work set WS is subsequently removed from the table 20 and transported to a polishing device 60 shown in FIG. 8 to carry out a polishing process described later. For handling at that time, the ring frame F is raised by the lifting mechanism 40 to a height position where the tape T is horizontal, as shown in FIG. 7(c). At this time, slack is generated in the tape T1 expanded in the expanding process, as shown in the figure. If slack is generated in the tape T1 in this way, as described above, the width of the groove W1 of the wafer W will become narrow when handling the work set WS. For this reason, the slack generated in the tape T1 is removed by heating the tape T1 by the thermal shrinking means 50.

[0041] That is, as shown in Fig. 7(c), the heat shrinking means 50 is positioned above the work set WS, and the arm 51 and a pair of heaters 52 attached to both ends of the arm 51 are rotated by the rotating means 54 at a predetermined speed around the center of the wafer W as an axis, while each heater 52 irradiates far infrared rays toward the ring-shaped tape T1, thereby uniformly heating the tape T1. Then, the tape T1, which has heat shrinkability, shrinks due to the heating, and the slack that has occurred in the tape T1 is removed. When the slack is removed from the tape T1 in this way, the tape T1 returns to a taut state without slack, so that when the work set WS is handled, the width of the groove W1 of the wafer W is maintained at the expanded value b2 due to the slack in the tape T1.

[0042] 4) Polishing process: In the polishing step, the upper surface of the wafer W, in which the width of the groove W1 has been expanded from b1 to b2 (>b1) in the expanding step, is polished by CMP using the polishing pad 63b of the polishing apparatus 60 shown in FIG.

[0043] 8, when the work set WS is placed on the holding surface 2a of the chuck table 1 with the tape T facing down, the porous member 2 of the chuck table 1 is suctioned by a suction source (not shown). Then, a negative pressure is generated in the porous member 2, and the work set WS is sucked and held by the holding surface 2a of the chuck table 1 due to the negative pressure.

[0044] A polishing wheel 63 of a polishing device 60 is disposed above the chuck table 1, and this polishing wheel 63 is detachably attached to the underside of a disk-shaped mount 62 attached to the lower end of a vertical spindle 61. This polishing wheel 63 is composed of a disk-shaped base 63a and a disk-shaped polishing pad 63b attached to the underside of the base 63a. The polishing pad 63b is composed of a pad material such as nonwoven fabric containing abrasive grains or urethane.

[0045] Here, the spindle 61 is rotated in the direction of the arrow (counterclockwise) by a spindle motor (not shown), and a supply path 64 for passing the slurry is vertically provided through the center of the spindle 61, the mount 62, and the grinding wheel 63. A pipe 66 extending from a slurry supply source 65 is connected to this supply path 64, and an electromagnetic opening and closing valve V4 is provided on this pipe 66. The polishing device 60 including the spindle 61, the mount 62, the grinding wheel 63, etc. can be raised and lowered by a lifting mechanism 67.

[0046] In the polishing process, the chuck table 1 and the work set WS held by it by suction are rotated at a predetermined speed in the direction of the arrow (counterclockwise) by a rotation mechanism (not shown), and the polishing wheel 63, which is rotated at a predetermined speed in the direction of the arrow (counterclockwise) by a spindle motor (not shown), is lowered by the lifting mechanism 67, so that the polishing pad 63b of the polishing wheel 63 comes into contact with the surface of the wafer W as shown. At the same time, the opening and closing valve V4 is opened and slurry is supplied from the slurry supply source 65 through the piping 66 and the supply path 64 to the contact portion between the polishing pad 63b and the wafer W.

[0047] Then, the surface of the wafer W is polished by the polishing pad 63b, and processing waste generated in the groove forming process and attached to the surface of the wafer W is removed. In addition, the polishing pad 63b comes into contact with the side of the groove W1, which is the gap between adjacent chips C of the wafer W whose width has been expanded from b1 to b2 in the expanding process, and the side and corners of the groove W1 are polished by the polishing pad 63b, thereby increasing the flexural strength of each chip C. In addition, the protective film formed on the upper surface of the chip C may be removed in the polishing process. The protective film may be removed between the groove forming process and the expanding process, or between the expanding process and the polishing process.

[0048] 5) Washing process: The cleaning process is a process in which the slurry adhering to the surface of the wafer W in the previous polishing process and the slurry remaining in the grooves W1 are removed by cleaning with a mixed fluid (two-fluid) of water and air sprayed from the spray nozzle 71 of the cleaning device 70 shown in Figure 9.

[0049] The cleaning device 70 is disposed above the chuck table 1, and the spray nozzle 71 is attached to a holder 73 that can be moved horizontally along the radial direction of the wafer W by a horizontal movement mechanism 72, and a cleaning water supply source 74 and an air supply source 75 are connected to the spray nozzle 71.

[0050] Thus, while the chuck table 1 holding the work set WS is rotated at a predetermined speed around the axis center in the illustrated arrow (counterclockwise direction) by a rotating mechanism (not shown), a spray nozzle 71 of the cleaning device 70 is moved horizontally above the wafer W along the radial direction of the wafer W, and a mixed fluid (two fluids) of cleaning water (pure water) and air supplied from a cleaning water supply source 74 and an air supply source 75 is sprayed from the spray nozzle 71 toward the wafer W. Then, the entire upper surface of the wafer W is cleaned by the mixed fluid (two fluids), and the slurry attached to the upper surface of the wafer W in the polishing process, which is the previous process, and the slurry remaining in the grooves W1 formed in the wafer W are removed. In this embodiment, a mixed fluid (two fluids) of cleaning water and air is used as the cleaning fluid, but only cleaning water (pure water) may be used. Also, cleaning water to which ultrasonic vibration is propagated may be used as the cleaning fluid.

[0051] In particular, in this embodiment, the widening step is carried out before the cleaning step is carried out, and the cleaning step is carried out in a state in which the width of the groove W1 formed on the surface of the wafer W in the groove forming step is widened from b1 (see FIG. 7(a)) to b2 (see FIG. 7(b)) by the widening step, so that the slurry remaining in the widened groove W1 is efficiently removed in a short time by the mixed fluid (two-fluid) sprayed from the spray nozzle 71. This reduces the time required for the cleaning step, and the wafer W can be divided efficiently in a short time.

[0052] <Second embodiment> Next, a second embodiment of the method for dividing the wafer W according to the present invention will be described.

[0053] The method for dividing the wafer W according to this embodiment is as follows: 1) Holding process 2) Groove formation process 3) Polishing process 4) Expansion process 5) Cleaning process This is a method of dividing the wafer W by sequentially going through the above steps, but unlike the first embodiment, a polishing step is carried out before expanding the tape T by the expansion step to polish the upper surface of the wafer W and remove processing debris, and a cleaning step is carried out immediately after the expansion step to remove the slurry adhering to the upper surface of the wafer W in the polishing step and the slurry remaining in the groove W1 by cleaning. Each step, i.e., the holding step, groove forming step, polishing step, expansion step and cleaning step, is carried out in the same manner as the corresponding steps in the first embodiment.

[0054] Thus, in this embodiment as well, the expansion step is carried out before the cleaning step and is carried out immediately after the expansion step, so that the cleaning step is carried out in a state in which the width of the groove W1 formed in the surface of the wafer W in the groove forming step has been expanded from b1 (see FIG. 7(a)) to b2 (see FIG. 7(b)) by the expansion step. Therefore, the slurry remaining in the expanded groove W1 is efficiently removed in a short time by the cleaning fluid sprayed from the spray nozzle 71 (see FIG. 9). As a result, the time required for the cleaning step is shortened, and the wafer W can be divided efficiently in a short time, which is the same effect as that obtained in the first embodiment.

[0055] In the above embodiment, plasma dicing (see FIG. 5) and blade dicing (see FIG. 6) have been described as examples of methods for forming the grooves W1 in the wafer W in the groove forming step, but other methods such as laser ablation can be used, in which a laser beam is irradiated onto the wafer W to form the grooves W1 in the wafer W. As another method, in the first embodiment in which the expansion step is always performed before the polishing step, a laser beam having a wavelength that is transparent to the wafer W may be irradiated to form a modified layer inside the wafer W, and the wafer W may be divided starting from the modified layer by the expansion step.

[0056] In addition, the present invention is not limited to the application of the embodiments described above, and various modifications are possible within the scope of the claims and the technical ideas described in the specification and drawings. [Explanation of symbols]

[0057] 1: chuck table, 2: porous member, 2a: holding surface, 3: piping, 4: suction source, 5: nozzle, 6: horizontal movement mechanism, 7: holder, 8: liquid resin supply source, 9: horizontal movement mechanism, 10: plasma etching device, 11: electrostatic chuck table, 12, 13: electrodes, 14: DC power supply, 15: plasma gas, 16: cutting blade, 20: table, 21: First suction part, 22: Second suction part, 23: Piping, 24: First suction source, 25: Piping, 26: second suction source, 27: roller, 30: frame holding portion, 31: mounting plate, 31a: circular hole, 32: cover plate, 32a: circular hole, 40: lifting mechanism, 41: cylinder mechanism, 42: cylinder, 43: piston rod, 50: heat shrink means, 51: arm, 52: heater, 53: lifting section, 54: rotating means, 60: polishing device, 61: spindle, 62: mount, 63: grinding wheel, 63a: base, 63b: polishing pad; 64: supply channel; 65: slurry supply source; 66: piping; 67: lifting mechanism, 70: cleaning device, 71: spray nozzle, 72: horizontal movement mechanism, 73: holder, 74: cleaning water supply source, 75: air supply source, b1, b2: groove width, C: Chip, D: Device, F: Ring frame, L1, L2: Street, LH: Laser head, P: Protective film, P1: Protective film groove, S: Decompression chamber, T: Tape, T1: exposed part of tape, V1-V4: open / close valves, W: wafer, W1: Wafer groove, WS: Work set

Claims

1. A wafer dividing method for dividing a wafer having devices formed in a plurality of regions on a surface partitioned by lattice-like streets along the streets, the method comprising the steps of: a holding step of holding the wafer on a chuck table via a tape attached to the back surface of the wafer; a groove forming step of forming a plurality of grooves along the streets on the surface of the wafer held on the chuck table; an expanding step of expanding the tape in a radial direction of the wafer to expand the groove to a predetermined width; a polishing step of polishing the surface of the wafer with a polishing pad while supplying a slurry to the surface side of the wafer, thereby removing deposits that have adhered to the surface of the device during the groove forming step; a cleaning step of spraying a cleaning fluid onto the surface of the wafer to clean the surface and the grooves of the wafer; Including, The method for dividing a wafer is characterized in that the widening step is carried out and then the cleaning step is carried out.

2. 2. The method for dividing a wafer according to claim 1, wherein after said groove forming step, said widening step, said polishing step and said cleaning step are carried out in this order.

3. 2. The method for dividing a wafer according to claim 1, wherein after said groove forming step, said polishing step, said widening step and said cleaning step are carried out in this order.

Citation Information

Patent Citations

  • Cleaning method and apparatus for wafer

    JP1996031785A

  • Dicing device and its method

    JP1997266182A

  • Wafer processing method

    JP2015230964A

  • Method for processing wafer

    JP2015233077A

  • Semiconductor chip bonding method and semiconductor chip bonding device

    JP2018160687A

Cited By

  • Wastewater treatment apparatus, processing apparatus, and workpiece processing method

    JP2026089127A