Oxygen shut-off device and casting apparatus

The oxygen cutoff device addresses turbulence issues in inert gas blowing devices by using a spiral gas flow path and multiple injection ports to maintain positive pressure, preventing molten metal oxidation and reducing defects in cast products.

JP2024157937AActive Publication Date: 2024-11-08DENSO CORP
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023072617
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-26
Publication Date
2024-11-08
Estimated Expiration
2043-04-26

AI Technical Summary

Technical Problem

In existing inert gas blowing devices for low-pressure casting machines, inert gases collide and generate turbulence, leading to air entrainment and oxidation of molten metal, resulting in oxide films or oxides that cause defects in the casting.

Method used

An oxygen cutoff device with a spiral-shaped gas flow path and multiple gas injection ports that inject inert gas in a direction crossing the molten metal flow path, maintaining positive pressure and preventing air from entering the molten metal flow path, thereby suppressing contact between molten metal and oxygen.

Benefits of technology

Prevents oxidation of molten metal, reducing defects in the cast product and minimizing tool wear during machining, while ensuring effective inert gas supply without clogging, and facilitating compact device design.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024157937000001_ABST
    Figure 2024157937000001_ABST
Patent Text Reader

Abstract

To provide an oxygen shut-off device for inhibiting melt from contacting oxygen and a casting apparatus.SOLUTION: A casting apparatus using an oxygen shut-off device 40 includes gas-ejection ports 426 communicating with a melt flow passage 420 and a gas flow passage 424. This allows the gas-ejection ports 426 to eject inert gas flowing in the gas flow passage 424 in a direction intersecting with a flow direction Df into the melt flow passage 420, whereby the gas-ejection ports 426 shut off the melt in the melt flow passage 420 from contacting oxygen. The gas-ejection ports 426 are arranged with spacing in a flow direction Df. Furthermore, the gas flow passage 424 is formed helically about an axis extending in the flow direction Df and surrounding the melt flow passage 420.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to an oxygen barrier device and a casting device. [Background technology]

[0002] Conventionally, as described in Patent Document 1, an inert gas injection device is known that is used in a low pressure casting machine and supplies an inert gas to a passage between a molten metal flow path of a mold and the molten metal. In this inert gas injection device, a cavity that communicates with the molten metal flow path and the passage is formed in the center. In addition, a supply port for supplying the inert gas is formed in the outer periphery. Furthermore, an inert gas supply path is formed in communication with the supply port and leads to the cavity, and an opening in this cavity is formed as a low-profile opening, and at least the opening is made of ceramics. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Application Publication No. 7-204824 Summary of the Invention [Problem to be solved by the invention]

[0004] In the inert gas injection device described in Patent Document 1, when inert gas is injected radially from shallow grooves on the same plane, the inert gas particles collide with each other, generating turbulence and drawing in air. This can cause the molten metal to oxidize when it comes into contact with oxygen in the air. When the molten metal oxidizes, an oxide film or oxides are formed on the surface of the molten metal. This causes the oxide film or oxides to get into the casting, resulting in defects.

[0005] An object of the present disclosure is to provide an oxygen blocking device and a casting device that prevent molten metal from coming into contact with oxygen. [Means for solving the problem]

[0006] The invention described in claim 1 is an oxygen blocking device comprising a mold (20) having a movable mold (22) that moves in an opening and closing direction and a fixed mold (24) that forms a cavity (26) corresponding to the shape of a casting (X) together with the movable mold when the movable mold is closed, a holding section (30) having a holding chamber (32) in which molten metal is held, and a connection section (42) connected to the mold (20), and the connection section is connected to a molten metal flow path (420) that communicates with the cavity and the holding chamber, a gas inlet (422) for introducing an inert gas, and the gas inlet. The oxygen blocking device has a gas flow path (424) through which an inert gas flows from a gas inlet, and a gas injection port (426) which is connected to the molten metal flow path and the gas flow path and thereby injects the inert gas flowing through the gas flow path into the molten metal flow path in a direction intersecting the flow direction (Df) of the molten metal flowing through the molten metal flow path, thereby blocking contact between the molten metal and oxygen in the molten metal flow path, wherein a plurality of gas injection ports are arranged at intervals in the flow direction, and the gas flow path is formed in a spiral shape centered on an axis extending in the flow direction and surrounds the molten metal flow path.

[0007] The invention recited in claim 8 is a casting apparatus comprising: a mold (20) having a movable mold (22) that moves in an opening / closing direction and a fixed mold (24) that, together with the movable mold, forms a cavity (26) corresponding to the shape of a casting (X) when the movable mold is closed; a holding section (30) having a holding chamber (32) in which molten metal is held; and an oxygen blocking device (40) having a connection section (42) connected to the mold and the holding section, the connection section having a molten metal flow path (420) communicating with the cavity and the holding chamber, a gas inlet (422) for introducing an inert gas, and a gas introducing section (423) for introducing an inert gas. The casting apparatus has a gas flow path (424) that is connected to the inlet and through which an inert gas flows from the gas inlet, and a gas injection port (426) that is connected to the molten metal flow path and the gas flow path and thereby injects the inert gas flowing through the gas flow path into the molten metal flow path in a direction intersecting the flow direction (Df) of the molten metal flowing through the molten metal flow path, thereby blocking contact between the molten metal and oxygen in the molten metal flow path, wherein the gas injection ports are arranged at intervals in the flow direction, and the gas flow path is formed in a spiral shape centered on an axis extending in the flow direction and surrounds the molten metal flow path.

[0008] As a result, the inert gas is ejected from the gas ejection port in a spiral pattern in multiple directions. As a result, a positive pressure is maintained in the entire area of ​​the molten metal flow path, and a flow of inert gas due to the pressure difference is created from the molten metal flow path toward the space of the fixed mold corresponding to the cavity. As a result, air that has entered the space of the fixed mold cannot enter the molten metal flow path. As a result, contact between the air that has entered the space of the fixed mold and the molten metal held in the holding chamber is suppressed. As a result, contact between the oxygen in the air and the molten metal held in the holding chamber is suppressed. As a result, exposure of the molten metal to oxygen is suppressed.

[0009] Note that the reference symbols in parentheses attached to each component indicate an example of the correspondence between the component and specific components described in the embodiments described below. [Brief description of the drawings]

[0010] [Figure 1] 1 is a cross-sectional view of a casting machine in which an oxygen blocking device according to a first embodiment is used. [Diagram 2] FIG. [Diagram 3] FIG. [Figure 4] Cross-sectional view taken along line IV-IV in Figure 3. [Diagram 5] Enlarged view of part V in Figure 4. [Figure 6] FIG. 2 is a cross-sectional view of the casting apparatus as molten metal flows into the cavity. [Figure 7] FIG. 2 is a cross-sectional view of the casting apparatus as the molten metal solidifies in the cavity. [Figure 8] FIG. 2 is a cross-sectional view of the casting apparatus when the casting is completed. [Figure 9] FIG. 1 is a cross-sectional view of a casting device when reproducing a casting. [Figure 10] FIG. 5 is a cross-sectional view of an oxygen blocking device according to a second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, embodiments will be described with reference to the drawings. In the following embodiments, the same or equivalent parts are denoted by the same reference numerals, and the description thereof will be omitted.

[0012] (First embodiment) The oxygen blocking device of the present embodiment prevents the molten metal from coming into contact with oxygen. Specifically, the oxygen blocking device is used in a casting apparatus that performs low pressure casting or high pressure casting. First, the casting apparatus will be described.

[0013] As shown in FIG. 1, the casting apparatus 10 includes a mold 20, a holder 30, an intermediate stalk 35, and an oxygen blocking device 40.

[0014] The mold 20 has a movable mold 22 and a fixed mold 24. The movable mold 22 is driven by a driving device of the facility (not shown). The movable mold 22 moves in an opening and closing direction. Here, the opening direction Do coincides with the top direction. The closing direction Dc coincides with the bottom direction. The fixed mold 24 forms a cavity 26 together with the movable mold 22 when the movable mold 22 closes. The cavity 26 is a space corresponding to the shape of the casting X.

[0015] The holding unit 30 has a holding chamber 32. The holding chamber 32 is a space in which the molten metal is held. Furthermore, the holding chamber 32 is connected to a holding furnace (not shown) that holds the molten metal. The molten metal is metal containing aluminum and the like that has been melted for casting.

[0016] Here, the oxygen blocking device 40 is attached to the intermediate stalk 35 arranged between the mold 20 and the holding part 30, and blocks contact between oxygen and the molten metal. Specifically, the oxygen blocking device 40 has a connection part 42. The connection part 42 is connected to the fixed mold 24 and the holding part 30. The connection part 42 is formed into a rectangular prism shape from metal or the like by, for example, a 3D printer or the like. Furthermore, the length of the connection part 42 in the opening and closing direction is, for example, 10 to 500 mm. The shape of the connection part 42 is not limited to a rectangular prism shape, and may be, for example, a polygonal prism shape or a cylindrical shape.

[0017] As shown in FIGS. 1 to 5, the connection portion 42 includes a molten metal flow path 420, a gas inlet 422, a gas flow path 424, and a gas ejection port 426.

[0018] 1, the molten metal passage 420 communicates with the cavity 26 and the holding chamber 32. When the molten metal held in the holding furnace is pressurized by a pressurizing device (not shown), the molten metal flows from the holding furnace through the holding chamber 32 and the molten metal passage 420 into the cavity 26. Here, the flow direction Df of the molten metal flowing through the molten metal passage 420 coincides with the opening direction Do and the upward direction. The molten metal passage 420 is, for example, a truncated cone-shaped space extending in the opening / closing direction.

[0019] As shown in FIG. 4, the length of the boundary between the molten metal flow passage 420 and the cavity 26 in the direction perpendicular to the flow direction Df is defined as a first boundary length L1. The length of the boundary between the molten metal flow passage 420 and the holding chamber 32 in the direction perpendicular to the flow direction Df is defined as a second boundary length L2. The first boundary length L1 and the second boundary length L2 are, for example, 0.05 to 200 mm. Furthermore, the first boundary length L1 and the second boundary length L2 are different. Here, the first boundary length L1 is smaller than the second boundary length L2. This makes it easier for the molten metal flow passage 420 to return the molten metal to the holding chamber 32.

[0020] The gas inlet 422 is provided with a valve and a cylinder (not shown) to introduce an inert gas such as argon or nitrogen. The amount of the inert gas introduced is, for example, 0.1 to 50 L / min. As shown in Figs. 2 to 4, the gas inlet 422 is, for example, a cylindrical space extending in a direction perpendicular to the flow direction Df. The diameter of the gas inlet 422 is, for example, 0.05 to 50 mm. The shape of the gas inlet 422 is not limited to a cylindrical shape, and may be, for example, a screw hole shape. In this case, the size of the pipe taper thread of the gas inlet 422 is, for example, Rc1 / 16 to Rc1. The shape of the gas inlet 422 may be, for example, a polygonal column shape.

[0021] 4, the gas inlet 422 is disposed closer to the holder 30 than the center plane So. The center plane So is a plane that is perpendicular to the flow direction Df and passes through the center of the molten metal flow path 420.

[0022] The gas flow passage 424 communicates with the gas inlet 422. In this way, the inert gas from the gas inlet 422 flows through the gas flow passage 424. As shown in FIG. 2 and FIG. 3, the gas flow passage 424 is a spiral space centered on an axis extending in the flow direction Df, and surrounds the molten metal flow passage 420. As shown in FIG. 4, the partial cross-sectional shape of the gas flow passage 424 when cut in the flow direction Df while passing through the center of the connection part 42 is circular. The diameter of the circular part in the cross section of the gas flow passage 424 when cut in the flow direction Df while passing through the center of the connection part 42 is the same as the diameter of the gas inlet 42, and is, for example, 0.05 to 50 mm. The diameter of the gas flow passage 424 in the direction perpendicular to the flow direction Df is, for example, 3 to 200 mm. The length of the interval between the gas flow passages 424 in the flow direction Df is, for example, 0.55 to 50.5 mm. The partial cross-sectional shape of the gas flow passage 424 when cut in the flow direction Df while passing through the center of the connection portion 42 is not limited to a circular shape, and may be, for example, a rectangular shape, a polygonal shape, an elliptical shape, or the like. In addition, in Fig. 4, the diameter of the gas flow passage 424 in the direction perpendicular to the flow direction Df is indicated by Lh. Furthermore, the interval length of the gas flow passage 424 in the flow direction Df is indicated by Lj.

[0023] The gas jet port 426 is in communication with the molten metal flow path 420 and the gas flow path 424. As a result, the gas jet port 426 jets the inert gas flowing through the gas flow path 424 into the molten metal flow path 420 in a direction intersecting with the flow direction Df. As a result, the gas jet port 426 blocks contact between the molten metal and oxygen in the molten metal flow path 420. Note that the direction intersecting with the flow direction Df here is a direction perpendicular to the flow direction Df.

[0024] Moreover, the gas ejection ports 426 are arranged at intervals in the flow direction Df. Furthermore, since the gas flow passage 424 is spiral, the gas ejection ports 426 are arranged on a spiral. Therefore, the gas ejection ports 426 that are different from each other in the flow direction Df are arranged at intervals in the circumferential direction around an axis extending in the flow direction Df. As a result, the gas ejection ports 426 that are different from each other in the flow direction Df are arranged with a circumferential shift while maintaining a circumferential interval along the spiral shape of the gas flow passage 424. Moreover, the circumferential angle between the gas ejection ports 426 adjacent to each other in the circumferential direction is, for example, 5° or more and less than 90°. In FIG. 3, the circumferential angle between the gas ejection ports 426 adjacent to each other in the circumferential direction is indicated by θk.

[0025] Furthermore, the gas ejection port 426 includes a plurality of slits 428 as shown in FIG. 5. The slits 428 are arranged at intervals in the flow direction Df. The slits 428 are formed, for example, in a rectangular shape. The slits 428 are inclined with respect to the flow direction Df. The length of the slits 428 in one direction is, for example, 0.05 to 50 mm. The length of the slits 428 in a direction perpendicular to the one direction is, for example, 0.05 to 50 mm. The interval length in the direction in which the slits 428 are arranged is, for example, 0.05 to 50 mm. In FIG. 5, the length of the slits 428 in one direction is indicated by Lm. The length of the slits 428 in a direction perpendicular to the one direction is indicated by Ln. The interval length in the direction in which the slits 428 are arranged is indicated by Lp. The inclination angle of the slits 428 with respect to the flow direction Df is indicated by θg. Moreover, the slit 428 is not limited to being inclined with respect to the flow direction Df, and may not be inclined with respect to the flow direction Df. Furthermore, the corners of the slit 428 may be rounded with R chamfers of, for example, R0 to R25. Furthermore, the corners of the slit 428 may be rounded with C chamfers of, for example, C0 to C25. Furthermore, the shape of the slit 428 is not limited to being rectangular, and may be polygonal, circular, elliptical, or the like. Furthermore, in FIG. 5, the corners of the slit 428 are indicated by Cs.

[0026] As described above, the casting apparatus 10 using the oxygen blocking device 40 is configured. Next, the production of the casting X using this casting apparatus 10 will be described with reference to Figs. 1 and 6 to 9.

[0027] 1, the movable mold 22 is moved in a closing direction Dc by the driving device to close the fixed mold 24. As a result, a cavity 26 corresponding to the shape of the casting X is formed.

[0028] Next, the pressurizing device pressurizes the molten metal held in the holding furnace. As a result, as shown in FIG. 6, the molten metal flows from the holding furnace through the holding chamber 32 and the molten metal flow path 420 into the cavity 26. In the figure, the molten metal is shown with a dot pattern. At this time, the valve is closed. Therefore, the gas inlet 422 does not introduce the inert gas. Therefore, the inert gas is not injected from the gas injection port 426 into the molten metal flow path 420. Furthermore, at this time, the molten metal that does not enter the cavity 26 is held in the molten metal flow path 420 and the holding chamber 32.

[0029] Next, when the molten metal in the cavity 26 solidifies, the valve is opened at the timing when the pressurization of the molten metal stops. As a result, the gas inlet 422 introduces an inert gas. The introduced inert gas flows through the gas flow path 424. The inert gas that flows through the gas flow path 424 is injected from the gas injection port 426 into the molten metal flow path 420 as shown in FIG. 7. Therefore, at this time, contact between the oxygen in the air that enters from outside the casting apparatus 10 through gaps or the like and the molten metal in the molten metal flow path 420 is blocked. Note that in FIG. 7, the flow of the inert gas from the gas injection port 426 is diagrammatically indicated by arrows.

[0030] Next, the movable die 22 is moved in the opening direction Do by the driving device to open the fixed die 24, as shown in Fig. 8. At this time, the solidified casting X in the cavity 26 that has solidified and shrunk and clung to the movable die 22 moves in the opening direction Do. The casting X that has solidified and shrunk and clung to the movable die 22 is removed from the movable die 22. This completes the casting X.

[0031] In addition, at this time, by opening the fixed die 24, air enters the space of the fixed die 24 corresponding to the cavity 26. Furthermore, the space of the fixed die 24 communicates with the molten metal passage 420. Therefore, the air that has entered the space of the fixed die 24 tries to come into contact with the molten metal in the molten metal passage 420. However, the inert gas is injected from the gas injection port 426 into the molten metal passage 420. Furthermore, the inert gas from the gas injection port 426 is injected in a spiral manner in multiple directions. As a result, a positive pressure is maintained in the entire area of ​​the molten metal passage 420, and a flow of the inert gas due to the pressure difference is generated from the molten metal passage 420 toward the space of the fixed die 24 corresponding to the cavity 26. Therefore, the air that has entered the space of the fixed die 24 cannot enter the molten metal passage 420. Therefore, contact between the air that has entered the space of the fixed die 24 and the molten metal held in the holding chamber 32 is suppressed. Therefore, contact between the oxygen in the air and the molten metal held in the holding chamber 32 is suppressed. 8, the flow of the inert gas from the gas ejection port 426 is shown typically by arrows. Also, air entering the space of the fixed mold 24 corresponding to the cavity 26 is shown typically by Air and an arrow.

[0032] Next, in order to manufacture the casting X again, as shown in FIG. 9, the movable die 22 is moved in the closing direction Dc by the driving device to close the fixed die 24. As a result, the cavity 26 corresponding to the shape of the casting X is formed. At this time, the inert gas is injected from the gas injection port 426 into the molten metal passage 420. The inert gas from the gas injection port 426 is injected in a spiral manner in multiple directions. As a result, a positive pressure is maintained in the entire area of ​​the molten metal passage 420, and a flow of the inert gas due to the pressure difference is generated from the molten metal passage 420 toward the space of the fixed die 24 corresponding to the cavity 26. As a result, the contact between the oxygen in the air that enters the space of the fixed die 24 corresponding to the cavity 26 and the molten metal is blocked before the movable die 22 is closed. In FIG. 9, the flow of the inert gas from the gas injection port 426 is shown typically by arrows.

[0033] Next, after the cavity 26 is formed, the valve is closed. Therefore, the gas inlet 422 does not introduce the inert gas. Therefore, the inert gas is not injected from the gas injection port 426 into the molten metal flow path 420. In addition, after the valve is closed, the molten metal held in the holding furnace is pressurized by the pressurizing device. As a result, the molten metal held in the holding chamber 32 and the molten metal flow path 420 flows into the cavity 26, as shown in FIG. 6.

[0034] Next, when the molten metal in cavity 26 solidifies, the valve is opened in the same manner as described above at the timing when the pressurization of the molten metal is stopped. As a result, gas inlet 422 introduces inert gas. The introduced inert gas flows through gas flow path 424. The inert gas that has flowed through gas flow path 424 is injected from gas injection port 426 into molten metal flow path 420, as shown in FIG. 7. Therefore, at this time, contact between oxygen in the air that enters from outside of casting apparatus 10 through gaps or the like and the molten metal in molten metal flow path 420 is blocked.

[0035] Next, as shown in FIG. 8, the movable die 22 is moved in the opening direction Do by the driving device to open the fixed die 24. At this time, the solidified casting X in the cavity 26 that has solidified and shrunk and clung to the movable die 22 moves in the opening direction Do. The casting X that has solidified and shrunk and clung to the movable die 22 is removed from the movable die 22. This completes the next casting X. At this time, as described above, air enters the space of the fixed die 24 corresponding to the cavity 26 by opening the fixed die 24. Furthermore, since the space of the fixed die 24 is connected to the molten metal flow path 420, the entered air is about to come into contact with the molten metal in the molten metal flow path 420. However, the inert gas is injected from the gas injection port 426 into the molten metal flow path 420. Moreover, the inert gas from the gas injection port 426 is injected in a spiral multiple manner. As a result, a positive pressure is maintained in the entire area of ​​the molten metal flow path 420, and a flow of inert gas due to the pressure difference is created from the molten metal flow path 420 toward the space of the fixed mold 24 corresponding to the cavity 26. Therefore, air that has entered the space of the fixed mold 24 cannot enter the molten metal flow path 420. This prevents the air that has entered the space of the fixed mold 24 from coming into contact with the molten metal held in the holding chamber 32. This prevents the oxygen in the air from coming into contact with the molten metal held in the holding chamber 32.

[0036] As described above, a series of operations of the casting apparatus 10 produces the casting product X. Next, it will be described how the casting apparatus 10 using the oxygen blocking device 40 prevents the molten metal from coming into contact with oxygen.

[0037] Here, in the inert gas injection device described in Patent Document 1, when the inert gas is injected radially from shallow grooves on the same plane, the inert gases collide with each other, generating turbulence and drawing in air. For this reason, the molten metal may be oxidized by contacting with oxygen in the air. When the molten metal is oxidized, an oxide film or oxide is generated on the surface of the molten metal. In addition, since the opening for supplying the inert gas is made of ceramics, solidification of the molten metal at the opening is unlikely to occur. However, even if the molten metal is not yet solidified, the molten metal may clog the opening, preventing the inert gas from being supplied. If the inert gas is not supplied, the molten metal will come into contact with oxygen in the air and oxidize. As a result, the oxide film or oxide will enter the casting X, causing defects.

[0038] Furthermore, when the molten metal comes into contact with oxygen, it oxidizes, and an oxide film or oxides are formed on the surface of the molten metal. The molten metal is pressurized and enters the cavity 26, where it solidifies, producing a casting X having an oxide film or oxide inclusions. The hardness of the generated oxide film and oxides is higher than the hardness of a portion of the casting X that does not have an oxide film or oxide inclusions. For this reason, if an oxide film or oxide inclusions is present in the casting X, tools are likely to wear and break when the casting X is machined, such as by cutting.

[0039] Furthermore, by joining the casting X to a member such as an extrusion material or a plate material by friction stir welding or the like, a flow path for fluids such as water, oil, and gas may be formed. In addition, since oxide films and oxides are not easily plastically flowed, it is not easy to friction stir the oxide films and oxides. For this reason, if the oxide films and oxides get into the casting X, defects are likely to occur in the joined product.

[0040] In contrast to these, in the casting apparatus 10 in which the oxygen blocking device 40 of this embodiment is used, the gas jet port 426 communicates with the molten metal flow path 420 and the gas flow path 424. As a result, the gas jet port 426 jets the inert gas flowing through the gas flow path 424 into the molten metal flow path 420 in a direction intersecting the flow direction Df, thereby blocking contact between the molten metal in the molten metal flow path 420 and oxygen. Furthermore, a plurality of gas jet ports 426 are arranged at intervals in the flow direction Df. Furthermore, as shown in FIGS. 2 to 4, the gas flow path 424 is formed in a spiral shape centered on an axis extending in the flow direction Df, and surrounds the molten metal flow path 420.

[0041] As a result, the inert gas from the gas injection port 426 is ejected in a spiral manner in multiple directions. As a result, a positive pressure is maintained in the entire area of ​​the molten metal passage 420, and a flow of the inert gas due to the pressure difference is generated from the molten metal passage 420 toward the space of the fixed die 24 corresponding to the cavity 26. Therefore, the air that has entered the space of the fixed die 24 cannot enter the molten metal passage 420. Therefore, contact between the air that has entered the space of the fixed die 24 and the molten metal held in the holding chamber 32 is suppressed. Therefore, contact between the oxygen in the air and the molten metal held in the holding chamber 32 is suppressed. Therefore, contact of the molten metal with oxygen is suppressed. This suppresses the intrusion of oxide films and oxides into the casting X. Therefore, when machining the casting X by cutting or other machining, wear and damage of tools are suppressed. Furthermore, when joining the casting X to a member such as an extruded material or a plate material by friction stir welding or other methods, defects in the joined product are suppressed. Furthermore, since the gas flow path 424 is formed in a spiral shape, the flow direction of the inert gas introduced from the gas inlet 422 is limited. Therefore, it is easy to form a flow path through which the inert gas injected from the gas injection port 426 flows toward the mold 20. Also, since the size of the gas flow path 424 can be minimized, the connection part 42 is prevented from becoming large. Therefore, the oxygen blocking device 40 can be made compact.

[0042] Furthermore, the casting apparatus 10 in which the oxygen blocking device 40 is used also provides the following effects.

[0043] [1] As shown in FIGS. 2 to 4, the gas ejection ports 426 located at different positions in the flow direction Df are arranged at intervals in the circumferential direction about an axis extending in the flow direction Df, and are therefore arranged in a shifted manner.

[0044] This makes it easier for the inert gas from the gas injection port 426 to be ejected in a spiral pattern in multiple directions. As a result, a positive pressure is maintained in the entire area of ​​the molten metal passage 420, and a flow of inert gas due to the pressure difference is generated from the molten metal passage 420 toward the space of the fixed mold 24 corresponding to the cavity 26. Therefore, air that has entered the space of the fixed mold 24 cannot enter the molten metal passage 420. This prevents the air that has entered the space of the fixed mold 24 from coming into contact with the molten metal held in the holding chamber 32. This prevents the oxygen in the air from coming into contact with the molten metal held in the holding chamber 32.

[0045] [2] As shown in FIG. 4, the gas inlet 422 is disposed perpendicular to the flow direction Df and closer to the holder 30 than the center plane So.

[0046] As a result, in the same manner as above, the inert gas from the gas ejection port 426 is easily ejected in a spiral manner in multiple directions. Therefore, a positive pressure is maintained in the entire area of ​​the molten metal passage 420, and a flow of inert gas due to the pressure difference is generated from the molten metal passage 420 toward the space of the fixed mold 24 corresponding to the cavity 26. Therefore, the air that has entered the space of the fixed mold 24 cannot enter the molten metal passage 420. Therefore, contact between the air that has entered the space of the fixed mold 24 and the molten metal held in the holding chamber 32 is suppressed. Therefore, contact between the oxygen in the air and the molten metal held in the holding chamber 32 is suppressed.

[0047] [3] As shown in FIG. 7, when the molten metal in the cavity 26 solidifies, the gas jet port 426 jets out the inert gas flowing through the gas passage 424 when the pressurization of the molten metal stops.

[0048] As a result, when the molten metal in cavity 26 solidifies, contact between the oxygen in the air that enters from outside casting apparatus 10 through gaps or the like and the molten metal in molten metal flow path 420 is blocked.

[0049] [4] As shown in FIG. 8, when the molten metal in the cavity 26 solidifies and the movable mold 22 opens, the gas jet 426 jets out the inert gas that flows through the gas passage 424.

[0050] This prevents oxygen in the air that enters the space of the fixed mold 24 corresponding to the cavity 26 from coming into contact with the molten metal when the movable mold 22 opens.

[0051] [5] As shown in FIG. 9 , when the movable die 22 is closed while the molten metal is held in the holding chamber 32 and the molten metal flow path 420, the gas jet orifice 426 jets out the inert gas flowing through the gas flow path 424.

[0052] This prevents the molten metal from coming into contact with oxygen in the air that may enter the space of the fixed mold 24 corresponding to the cavity 26 until the movable mold 22 is closed.

[0053] [6] As shown in FIG. 6, the gas jet 426 stops jetting the inert gas when the molten metal flows from the holding chamber 32 through the molten metal passage 420 to the cavity 26.

[0054] This prevents the inert gas from entering the molten metal in the cavity 26. This prevents defects such as cavities from occurring in the casting X.

[0055] Second embodiment In the second embodiment, instead of the first boundary length L1 being smaller than the second boundary length L2, the first boundary length L1 is equal to or larger than the second boundary length L2 as shown in Fig. 10. Even in such a second embodiment, the same effects as those of the first embodiment are achieved.

[0056] (Other embodiments) The present disclosure is not limited to the above-described embodiments, and appropriate modifications can be made to the above-described embodiments. Furthermore, in each of the above-described embodiments, it goes without saying that the elements constituting the embodiments are not necessarily essential, except in cases where they are particularly clearly stated as essential or where they are clearly considered essential in principle.

[0057] In each of the above-described embodiments, the opening and closing direction coincides with the vertical direction. However, the opening and closing direction is not limited to the vertical direction and may be, for example, a direction perpendicular to the vertical direction.

[0058] In each of the above embodiments, the oxygen blocking device 40 is attached to the intermediate stalk 35. However, the oxygen blocking device 40 is not limited to being attached to the intermediate stalk 35, and may be attached to the mold 20, for example.

[0059] The above embodiments may be combined as appropriate. [Explanation of symbols]

[0060] 10 Casting Equipment 22 Movable mold 24 Fixed mold 30 Holding part 40 Oxygen cutoff device 42 Connection 420 Molten metal flow path 422 Gas inlet 424 Gas flow path 426 Gas nozzle

Claims

1. An oxygen blocking device, comprising: The mold (20) has a movable mold (22) that moves in an opening / closing direction and a fixed mold (24) that forms a cavity (26) corresponding to the shape of a casting (X) together with the movable mold when the movable mold is closed, and a holding part (30) that has a holding chamber (32) in which molten metal is held, and a connection part (42) that is connected to the mold (20), The connection portion is a molten metal passage (420) communicating with the cavity and the holding chamber; A gas inlet (422) for introducing an inert gas; a gas flow path (424) communicating with the gas inlet, through which an inert gas flows from the gas inlet; a gas injection port (426) that is in communication with the molten metal flow path and the gas flow path, and that injects an inert gas flowing through the gas flow path into the molten metal flow path in a direction that intersects with a flow direction (Df) of the molten metal flowing through the molten metal flow path, thereby blocking contact between the molten metal in the molten metal flow path and oxygen; having The gas ejection ports are arranged at intervals in the flow direction, The gas flow passage is formed in a spiral shape centered on an axis extending in the flow direction, and is an oxygen blocking device surrounding the molten metal flow passage.

2. The oxygen blocking device according to claim 1 , wherein the gas injection ports located at different positions in the flow direction are arranged at intervals in a circumferential direction about an axis extending in the flow direction.

3. 3. The oxygen blocking device according to claim 1, wherein the gas inlet is disposed on the side of the retaining portion relative to a plane (So) that is perpendicular to the flow direction and passes through a center of the molten metal flow path.

4. 3. The oxygen blocking device according to claim 1, wherein the gas ejection port ejects the inert gas flowing through the gas flow passage when the pressurization of the molten metal in the cavity is stopped in the case where the molten metal in the cavity is solidified.

5. 3. The oxygen blocking device according to claim 1, wherein the gas ejection port ejects the inert gas flowing through the gas flow passage when the molten metal in the cavity solidifies and the movable die opens.

6. 3. The oxygen blocking device according to claim 1, wherein the gas injection port injects an inert gas flowing through the gas flow passage when the movable die is closed with the molten metal held in the holding chamber and the molten metal flow passage.

7. 3. The oxygen blocking device according to claim 1, wherein the gas jetting port stops jetting the inert gas when the molten metal flows from the holding chamber through the molten metal flow path into the cavity.

8. 1. A casting apparatus comprising: a mold (20) having a movable mold (22) that moves in an opening / closing direction and a fixed mold (24) that, together with the movable mold, forms a cavity (26) corresponding to the shape of a casting (X) when the movable mold is closed; A holding section (30) having a holding chamber (32) in which molten metal is held; an oxygen blocking device (40) having a connection part (42) connected to the mold and the holding part; Equipped with The connection portion is a molten metal passage (420) communicating with the cavity and the holding chamber; A gas inlet (422) for introducing an inert gas; a gas flow path (424) communicating with the gas inlet, through which an inert gas flows from the gas inlet; a gas injection port (426) that is in communication with the molten metal flow path and the gas flow path, and that injects an inert gas flowing through the gas flow path into the molten metal flow path in a direction that intersects with a flow direction (Df) of the molten metal flowing through the molten metal flow path, thereby blocking contact between the molten metal in the molten metal flow path and oxygen; having The gas ejection ports are arranged at intervals in the flow direction, The gas flow passage is formed in a spiral shape centered on an axis extending in the flow direction and surrounds the molten metal flow passage.

Citation Information

Patent Citations

  • JP1988101156U

  • Low pressure casting device and rare gas supply method to low pressure casting device

    JP1991254352A

  • Device for blowing inert gas

    JP1995051833A

  • Stroke for low pressure casting, low pressure casting method using it and low pressure casting machine

    JP1996090203A

  • Device for blowing inert gas into low pressure casting machine

    JP1997216045A