Taro drier
The taro dryer addresses inefficiencies in conventional methods by using a conveyor and hot air system to uniformly dry taro, ensuring high quality retention during transportation.
Patent Information
- Application Number
- JP2024140681
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2042-04-20
AI Technical Summary
Conventional dry rot control methods and devices are inefficient for large-scale taro processing before shipping, requiring long processing times and leading to uneven drying and quality issues during transportation.
A taro dryer with a conveyor system and hot air generator that efficiently dries large quantities of taro by maintaining a consistent temperature within a drying chamber, using a corrugated plate to ensure even air distribution and a conveyor with steps to turn taro for uniform drying.
The dryer effectively processes large amounts of taro quickly, preventing uneven drying and maintaining high quality during transportation, with a quality retention rate of 95% or more even after three weeks.
Smart Images

Figure 2024161038000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a taro dryer used to process taro before shipping. [Background technology]
[0002] The above-mentioned pre-shipment processing method for taro is mainly carried out at taro sorting facilities where large quantities of taro are collected from taro producers such as farmers before being shipped to retailers such as supermarkets or consumers, in order to maintain the quality of the taro as good as possible during transportation and after it reaches the consumer.
[0003] Generally, taro roots dug from fields are collected at taro sorting plants. The collected taro roots are then sorted according to their shape, quality, and size at the taro sorting plants, and are then shipped after being packaged as necessary, such as in boxes. However, there have been cases where taro roots shipped from the taro sorting plants have rotted during transportation and become defective products, and these defective products are delivered to retailers and consumers. For this reason, there has been a demand for improving the rate of defective taro roots during transportation.
[0004] It has been known that taro decay occurs when dry rot is caused by Fusarium fungus in stored taro. To prevent dry rot of taro during storage, for example, Patent Document 1 discloses a method for preventing dry rot in taro by causing the taro to absorb water and then continuously irradiating the taro with far-infrared rays to keep the surface temperature of the taro at 60-70°C and maintaining that temperature for 1-5 minutes, and a device for preventing dry rot of taro comprising a conveyor equipped with a mesh belt on which the taro is placed and transported, heaters installed on both the top and bottom of the mesh belt to irradiate the taro with far-infrared rays, and a control device for controlling the output of the heaters and the speed of the conveyor based on previously obtained data so that the surface temperature of the taro is maintained at 60-70°C for 1-5 minutes. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Japanese Patent Application Publication No. 09-023812 Summary of the Invention [Problem to be solved by the invention]
[0006] However, while the conventional dry rot prevention methods and dry rot prevention devices described above may be effective for storing seed taro in a refrigerator for a long period of time, at taro sorting plants, large quantities of collected taro need to be shipped as quickly as possible, and they are not suitable for processing these large quantities of taro in a short period of time before shipping so as to maintain the quality of the taro as best as possible during transportation and after it reaches the consumer.
[0007] In other words, in the conventional dry rot prevention methods described above, not only does it take a long time, such as 24 hours, for the taro to absorb sufficient water, but it also requires the taro to be immersed in water for a predetermined period of time to absorb the water, which necessitates equipment such as a water storage tank.
[0008] In addition, in the above-mentioned device for preventing dry rot of taro, in order to make the surface temperature of the taro a required temperature, heaters installed on both the upper and lower sides of the mesh belt irradiate far-infrared rays to the taro on the mesh belt of the conveyor, so that the amount of far-infrared rays that reach the taro differs between the parts of the taro that are directly hit by the far-infrared rays and the parts in the shade. The angle of incidence of infrared rays at each part of the taro surface is also different. Therefore, the entire surface of the taro does not heat up uniformly, and a temperature difference may occur between each part of the taro surface. In particular, if the cut opening of the taro is wet, it is thought that rotting will progress from the cut opening. Even if a large amount of taro is transported by a conveyor equipped with a mesh belt and far-infrared rays are irradiated from heaters installed on both the upper and lower sides of the transport path, uneven drying is likely to occur at the cut openings of the taro between the taro, and it is not possible to improve the rate of quality taro during transportation.
[0009] The present invention has been made in consideration of the above-mentioned problems of the conventional art. The main object of the present invention is to provide a taro dryer that can process a large amount of taro in a relatively short time before shipping so as to improve the rate of quality of the taro during transportation.
[0010] A taro dryer according to a first aspect of the present invention comprises a unit drying chamber, a hot air generator arranged above the unit drying chamber and capable of adjusting the temperature of the hot air supplied, and a plurality of drying units arranged in a row, each having an exhaust duct arranged below the unit drying chamber for discharging the hot air generated by the hot air generator, and a conveyor having a transport path that passes through the drying chamber formed by connecting the unit drying chambers arranged in a row in the front-to-rear direction, and is configured such that the hot air generated by the hot air generator is supplied to the drying chamber and passes through the drying chamber while maintaining the temperature within the drying chamber at 50 degrees Celsius or higher, and a large number of taro are transported along the transport path by the conveyor and passed through the drying chamber, thereby drying the notched openings of the taro and forming a dried layer at the notched openings.
[0011] With this configuration, it is possible to process taro in a relatively short time before shipping a large amount of taro, so as to improve the rate of non-defective taro during transportation.
[0012] According to a second aspect of the taro dryer of the present invention, the conveyor is provided with a mesh belt as an endless transport belt on which the taro is placed, and the endless transport belt circulates to return to the transport path via a return path that passes below the drying chamber, and the drying chamber can be configured to have a hot air supply inlet on the upper side of the drying chamber and a hot air exhaust outlet on the lower side of the drying chamber, and to have a plate arranged directly below the transport path that obstructs the downward flow of the hot air.
[0013] With this configuration, the hot air passing through the mesh belt is received by the plate, and sufficient hot air can be applied to the underside of the taro on the mesh belt, so that the entire surfaces of a large amount of taro can be efficiently dried, and uneven drying at the cut openings of the taro can be suppressed.
[0014] According to the taro dryer according to the third aspect of the present invention, the plate can be configured to be a corrugated plate curved in a wave shape in the transport direction of the taro.
[0015] With this configuration, the hot air that hits the corrugated plate is less likely to escape in the conveying direction of the conveyor, making it possible to more effectively dry the entire surface of the taro, including the notch.
[0016] According to the taro dryer according to the fourth aspect of the present invention, the conveying path can be configured to have a step at least at one location in the conveying direction.
[0017] With this configuration, the taro rolls over the step during transportation and is turned upside down, so that the entire taro including the cut end can be dried more evenly. [Brief description of the drawings]
[0018] [Figure 1] FIG. 2 is a front view of the taro dryer of the present invention. [Diagram 2] FIG. 2 is a left side view of the dryer shown in FIG. [Diagram 3] 1 is an enlarged photograph of the vicinity of the surface layer of a vertical cross section of a notch of a taro according to Comparative Example 1. [Figure 4] 1 is an enlarged photograph of the vicinity of the surface layer of a vertical cross section of a notch of a taro according to Example 4. [Diagram 5] 13 is an enlarged photograph of the surface layer of a vertical cross section of a cut opening of a taro according to Example 6. [Figure 6] 1 is a graph showing the relationship between the number of days elapsed since processing and the number of commercially valuable taro and the rate of non-defective products. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] Hereinafter, an embodiment of the present invention will be described based on the drawings. However, the embodiment shown below is an example of a taro dryer for embodying the technical idea of the present invention, and the present invention does not specify them as follows. In addition, this specification never specifies the members shown in the claims to the members of the embodiment. In particular, the dimensions, materials, shapes, and relative positions of the components described in the embodiment are not intended to limit the scope of the present invention to those, and are merely explanatory examples, unless otherwise specified. Note that the size and positional relationship of the members shown in each drawing may be exaggerated to clarify the explanation. Furthermore, in the following explanation, the same name and symbol indicate the same or similar members, and detailed explanation will be omitted as appropriate. Furthermore, each element constituting the present invention may be configured as a form in which multiple elements are composed of the same member and multiple elements are shared by one member, or conversely, the function of one member can be shared by multiple members. (dryer)
[0020] 1 and 2 show an example of a taro dryer of the present invention, and this dryer 1 is equipped with a drying chamber 2 and a conveyor 3 having a transport path 3A for the taro T, and the transport path 3A for the taro T passes through the drying chamber 2. The left side of the paper in Fig. 1 is the front side of the drying chamber 2, and the right side of the paper in Fig. 1 is the rear side of the drying chamber 2. The conveyor 3 transports the taro T from the front side to the rear side of the drying chamber 2 along the transport path 3A.
[0021] In this embodiment, the dryer 1 is provided with six drying units 4 arranged in a row in the conveying direction of the conveyor 3 in order to effectively dry the taro T, and each drying unit 4 is provided with a unit drying chamber 5, a hot air generator 6 arranged above the unit drying chamber 5, and an exhaust duct 7 arranged below the unit drying chamber 5. The drying chamber 2 is formed by connecting the unit drying chambers 5 of each drying unit 4 in the front-to-rear direction. Note that FIG. 1 shows a cross-sectional view of the unit drying chambers 5 and the exhaust duct 7 as if they were cut by a vertical plane extending in the front-to-rear direction of the drying chamber 2.
[0022] The unit drying chamber 5 is formed in a rectangular parallelepiped shape by being surrounded by plates on the front, back, left, right, top and bottom, and has openings 8a, 8b formed in the front and rear plates for passing the conveyor 3 and the taro T, a supply port 9 formed in the upper plate for introducing hot air generated by the hot air generator 6, and a plurality of exhaust ports 10 formed in the lower plate for discharging the hot air to the exhaust duct 7.
[0023] 2, the hot air generator 6 is configured to generate hot air by injecting LPG gas into a combustion duct 11 having an air intake 11a with a burner 12 and burning the gas in the combustion duct 11, and to send the hot air to the drying chamber 2 with a blower 13. Furthermore, the hot air generator 6 is provided with a temperature sensor 14 disposed near the hot air supply port 9 for detecting the temperature of the hot air supplied to the unit drying chamber 5, and a temperature regulator (not shown) for automatically operating the burner 12 so that the temperature of the hot air detected by the temperature sensor 14 becomes a preset temperature.
[0024] 1, the upper surface of the exhaust duct 7 is open to receive hot air discharged from the exhaust port 10 of each unit drying chamber 5, and the exhaust ducts 7 of the six drying units 4 are connected to adjacent ones to form one exhaust path 15. The rearmost exhaust duct 7 has an opening 16 that communicates with an exhaust duct (not shown) provided outside the dryer 1. This opening 16 may be provided, for example, for each drying unit 4 as necessary.
[0025] The conveyor 3 is provided with a wire mesh belt that can pass hot air from the front side to the back side as a conveying endless belt 17 on which the taro T is placed. The conveying endless belt 17 has a predetermined width in the left-right direction of the drying chamber 2 as shown by the two-dot chain line in FIG. 2, and is hung on roller parts 18a, 18b, 18c, 18d, 18e, 18f, 18g, 18h, and 18i as shown by the one-dot chain line in FIG. 1. By rotating the roller part 18h by the motor 19, the taro T circulates back to the conveying path 3A via the return path 3B that passes under the exhaust duct 7 on the lower side of the drying chamber 2. The conveying path 3A is formed by the roller parts 18a to 18d, and the return path 3B is formed by the roller parts 18d, 18e to 18i, and 18a. Further, the transport path 3A has a step 20 that is inclined downward in the transport direction, and this step 20 is formed by roller portions 18b and 18c.
[0026] Taro T is constantly supplied to the front end of the conveyor 3 from outside the dryer 1 by a conveyor not shown, and the taro T that has passed through the drying chamber 2 is transported from the rear end of the conveyor 3 to a predetermined position outside the dryer 1 by another conveyor not shown.
[0027] The hot air generated by the hot air generator 6 is supplied to the unit drying chamber 5 from the supply port 9, blown onto the taro T transported along the transport path 3A, passes through the transport endless belt 17 from top to bottom, and is further discharged from the exhaust port 10 to the exhaust duct 7. In order to ensure that the hot air that has passed through the transport endless belt 17 from top to bottom can be fully utilized for drying the lower part of the taro T, the unit drying chamber 5 has a plate 21 disposed immediately below the transport path 3A. This plate 21 is intended to prevent the hot air that has passed through the transport endless belt 17 from flowing directly downward, and is made of a corrugated plate curved in a wave shape in the transport direction of the taro T of the transport endless belt 17. (How taro is processed before shipping)
[0028] To process taro before shipping using the taro dryer of the present invention, the above-mentioned taro dryer 1 is installed, and hot air generated by the hot air generator 6 is supplied to the drying chamber 2 and passed through the drying chamber 2 while adjusting the temperature in the drying chamber 2, i.e., the temperature of the hot air passing through the drying chamber 2, to maintain it at a predetermined value. Then, a large number of taro T are conveyed along the conveying path 3A by the conveyor 3 and passed through the drying chamber 2, and while the taro T passes through the drying chamber 2, the cut opening of the taro T is dried to form a dry layer at the cut opening, which will be described later. The cut opening of the taro T is the separation surface formed when the parent taro and the child taro or the child taro and the grandchild taro are separated, or the cut surface formed when the taro is cut. At this time, even if moisture is attached to the surface of the taro T, the moisture evaporates while the taro T passes through the drying chamber 2, and the surface of the taro T is also dried. When the pre-shipment processing of the taro T is completed, the supply of hot air from the hot air generator 6 to the drying chamber 2 is stopped and the operation of the conveyor 3 is stopped. EXAMPLES
[0029] In order to grasp the change in quality of taro treated by the pre-shipment processing method of the present invention, 300 taro were divided into six groups of 50 taro, and the pre-shipment processing method of taro was carried out on each of the six groups using a dryer 1 and maintaining a different temperature in the drying chamber 2 for each group.
[0030] In this dryer 1, the maximum conveying weight of the conveyor 3 is 60 kilograms per minute, and the conveying speed of the conveyor 3 is 6 meters per minute. The burner 12 is an LPG gas burner, and the amount of air supplied to the drying chamber 2 is 480 cubic meters per minute, which is the total amount of air sent out by the blower 13 for each drying unit 4, and the passage time through the drying chamber 2 is 135 seconds. The temperature in the drying chamber 2 was measured for each example by a thermometer 22 installed near the conveying path 3A in the drying chamber 2, and the temperature in the drying chamber 2 was adjusted so that the measured temperature was 30 degrees Celsius in Example 1, 50 degrees Celsius in Example 2, 60 degrees Celsius in Example 3, 64 degrees Celsius in Example 4, 68 degrees Celsius in Example 5, and 72 degrees Celsius in Example 6, and 50 taro were supplied to the conveyor 3 for each adjusted temperature and passed through the drying chamber 2.
[0031] Furthermore, as Comparative Example 1, 50 taro pieces were supplied to the conveyor 3 and passed through the drying chamber 2 without supplying hot air into the drying chamber 2. The temperature inside the drying chamber 2 at this time was 8 degrees Celsius.
[0032] The 50 taro roots used in Examples 1 to 6 and Comparative Example 1 were shipped to a taro sorting facility by the same producer one day before the above-mentioned processing was carried out, and from the shipped taro roots, those with rotting or rotten taro roots were removed. (Condition of the notch after processing)
[0033] For each of Examples 1 to 6 and Comparative Example 1, the drying state of the notched end of the taro was observed immediately after it was carried out from the drying chamber 2.
[0034] For the taro in Comparative Example 1, no change was observed in the state of the notch of the taro before being carried into the drying chamber 2 and after passing through the drying chamber 2, and the notch of the taro carried out from the drying chamber 2 was glossy with liquid and looked wet from the liquid seeping out. In addition, when touching the notch with a fingertip and removing the fingertip from the notch, a slight adhesive force was felt.
[0035] The taro of Example 1 did not appear to be sufficiently dried, and the taro of Example 2, the taro of Example 3, the taro of Example 4, the taro of Example 5, and the taro of Example 6 did not show any liquid seeping out or liquid gloss on the surface of the cutout, and appeared to be smooth and dry. In addition, when touching the cutout with a fingertip and removing the fingertip, no adhesive force was felt like the cutout of the taro of Comparative Example 1. The color of the cutout of each of the taro of Examples 1 to 6 appeared to be closer to white the higher the temperature in the drying chamber 2.
[0036] Furthermore, for the taro according to Comparative Example 1, the taro according to Example 4, and the taro according to Example 6, the cut opening was cut in a direction approximately perpendicular to the surface, and the vicinity of the surface of the cut surface of the cut opening (i.e., the vertical section of the cut opening) was photographed using a microscope. FIG. 3 is an enlarged photograph according to Comparative Example 1, FIG. 4 is an enlarged photograph according to Example 4, and FIG. 5 is an enlarged photograph according to Example 6. The taro is shown in the right-hand part of the photographs in FIG. 3 to FIG. 5, and the background is shown in the left-hand part. In FIG. 3, the surface layer of the cut opening of the taro seen near the center of the photograph and the part deeper than the surface layer seen near the right edge of the photograph are both approximately uniform in texture. In FIG. 4 and FIG. 5, the texture of the surface layer of the taro seen near the center of the photograph is different from the texture of the part deeper than the surface layer seen near the right side of the photograph. And a hollow part is generated at the location indicated by the arrow in the photograph, that is, at the boundary between the surface layer of the cut opening and the part deeper than it. The hollow areas near the surface of the notch and the surface layer of the notch are thought to have been created by the drying of the notch, and it is believed that the appearance of such surface layers at the notch inhibits the taro from rotting at the notch. Here, the surface layer of the notch as seen in Figures 4 and 5 will be called the dry layer. In Figures 4 and 5, the dark areas near the center of the photographs are thought to be soil that was attached to the surface of the notch. (Verification of the Effects of the Example)
[0037] Fifty taro roots of each of Examples 1 to 6 and Comparative Example 1 that had passed through the drying chamber 2 were placed in separate nylon bags for each Example, and stored in separate boxes at room temperature in a state where they were easily damaged. The deterioration of the quality of the taro roots was observed every day for a certain period of time. When a taro root was found that had a slimy texture at the cut end, was soft, and had melted tissue, the taro root was taken out of the box as being damaged, that is, having lost its commercial value. The observation results are shown in Table 1 and FIG. 6. [Table 1]
[0038] Table 1 shows the relationship between the number of days after processing and the number of taro that have been damaged or moldy. The numbers in the "damaged" column in Table 1 indicate the number of taro that have been damaged and lost their commercial value, and the numbers in the "mold, etc." column indicate the number of taro that have been moldy and lost their commercial value. In addition, "A" to "F" in the "mold, etc." column in Table 1 indicate that some taro have signs of quality deterioration even though they still have commercial value, with "A" indicating that red spots have appeared at the cut edge, "B" indicating that the cut edge has become soft, "C" indicating that an odor has appeared inside the nylon bag, "D" indicating that the cut edge has become slimy, "E" indicating that the bottom of the taro has become soft, and "F" indicating that the taro has shriveled.
[0039] As shown in Table 1, in Examples 1 to 6, the taro showed signs of quality deterioration later than in Comparative Example 1. Furthermore, in Example 3, which passed through a drying chamber 2 at 60 degrees Celsius, and Example 4, which passed through a drying chamber 2 at 64 degrees Celsius, the taro showed signs of quality deterioration later than in the other Examples.
[0040] Usually, when taro is shipped from a taro sorting facility to a retailer such as a supermarket, it takes about one week to transport the taro, and it takes about one week for the retailer to package the taro that arrived and put it on display at the storefront, and it is expected that it takes about one week for the taro to be purchased by the consumer, and it takes about one week for the consumer to consume the taro. In addition, retailers acknowledge that some taro will be damaged during the transportation period, and if the quality rate of the taro that arrived is 95% or more, they will not make a complaint against the taro sorting facility. Therefore, it is sufficient if the quality rate of taro shipped from the taro sorting facility after being subjected to the pre-shipment treatment method of the present invention is 95% or more three weeks later, and it can be evaluated that the taro can maintain its quality well during transportation and after it reaches the consumer.
[0041] Fig. 6 is a graph showing the relationship between the number of days after processing and the number and quality rate of marketable taro remaining in the box. Looking at the quality rate of taro after one week (7 days) in Fig. 6, one out of 50 taros of Example 1 that passed through a drying chamber 2 at 30 degrees Celsius was damaged, giving a quality rate of 98%, while none of the 50 taros of Example 2 that passed through a drying chamber 2 at 50 degrees Celsius were damaged, giving a quality rate of 100%, none of the 50 taros of Example 3 that passed through a drying chamber 2 at 60 degrees Celsius were damaged, giving a quality rate of 100%, and none of the 50 taros of Example 4 that passed through a drying chamber 2 at 64 degrees Celsius were damaged, giving a quality rate of 100%. The taro of Example 4, which passed through the drying chamber 2 at 68 degrees Celsius, had no damaged taro out of 50, and the quality rate was 100%. The taro of Example 5, which passed through the drying chamber 2 at 68 degrees Celsius, had one damaged taro out of 50, and the quality rate was 98%. The taro of Example 6, which passed through the drying chamber 2 at 72 degrees Celsius, had three damaged taro out of 50, and the quality rate was 94%. The taro of Comparative Example 1, which passed through the drying chamber 2 in a windless and unheated state, had three damaged taro out of 50, and the quality rate was 94%. Therefore, while the quality rate of the taro of Comparative Example 1 after one week has passed is 94%, the taro of Examples 1 to 5 maintains a quality rate of 95% or more even after one week has passed, and it can be seen that the treatment of the taro in Examples 1 to 5 was effective. It is considered that the taro of Example 6, which passed through the drying chamber 2 at 72 degrees Celsius, became easily damaged due to the cell tissue of the surface layer such as the notch being destroyed by heat.
[0042] In addition, in FIG. 6, when attention is paid to the quality rates of the taro according to Examples 1 to 6 and Comparative Example 1 three weeks after shipping, 7 out of 50 taro according to Example 1 that passed through the drying chamber 2 at 30 degrees Celsius were damaged, and the quality rate was 86%, 1 out of 50 taro according to Example 2 that passed through the drying chamber 2 at 50 degrees Celsius was damaged, and the quality rate was 98%, 4 out of 50 taro according to Example 3 that passed through the drying chamber 2 at 60 degrees Celsius was damaged, and the quality rate was 92%, and 1 out of 50 taro according to Example 4 that passed through the drying chamber 2 at 64 degrees Celsius was damaged, and the quality rate was 94%. In the case of the taro of Example 4 which passed through the drying chamber 2 at 68 degrees Celsius, not one of the 50 taro was damaged, and the quality rate was 100%. In the case of the taro of Example 5 which passed through the drying chamber 2 at 68 degrees Celsius, 3 of the 50 taro were damaged, and the quality rate was 94%. In the case of the taro of Example 5 which passed through the drying chamber 2 at 72 degrees Celsius, 10 of the 50 taro were damaged, and the quality rate was 80%. In the case of the taro of Comparative Example 1 which passed through the drying chamber 2 in a windless and unheated state, 12 of the 50 taro were damaged, and the quality rate was 76%. Therefore, the taro of Example 2 which passed through the drying chamber 2 at 50 degrees Celsius and the taro of Example 4 which passed through the drying chamber 2 at 64 degrees Celsius each maintained a quality rate of 95% or more even after three weeks had passed after the treatment, so it can be seen that the treatment of the taro in Example 2 and Example 4 was effective.
[0043] The taro of Example 3, which passed through a drying chamber 2 at 60 degrees Celsius, and the taro of Example 5, which passed through a drying chamber 2 at 68 degrees Celsius, had passability rates of 94% and 92% after three weeks, both of which exceeded 90%.Compared to the taro of Comparative Example 1, which passed through a drying chamber 2 in a windless and unheated state, the passability rate of 76% after three weeks, these maintain a significantly higher passability rate.
[0044] The taro according to Examples 1 to 6 and Comparative Example 1 are stored at room temperature in a state where they are easily damaged after passing through the drying chamber 2, but in reality, at taro sorting centers and retail stores, large quantities of taro that arrive are stored in refrigerators or other conditions to minimize damage. Therefore, if the taro according to Examples 3 and 5 are stored appropriately as usual in the actual distribution process, it can be expected that the non-defective product rate will be 95% or more even three weeks after shipping from the taro sorting center.
[0045] As described above, even when the pre-shipment processing method of taro of the present invention is carried out under worse conditions than the actual management conditions, the taro of Examples 2 and 4 achieve the set condition of a quality rate of 95% or more three weeks after processing, and the taro of Examples 3 and 5 also achieve a quality rate of 90% or more three weeks after processing, and it can be fully expected that the quality rate will be 95% or more even three weeks after shipping. Therefore, if the operating conditions of the dryer 1 are optimized according to the environment, it can be said that this method can be fully practical as a pre-shipment processing method of taro that processes a large amount of taro in a short period of time. [Explanation of symbols]
[0046] 1...Dryer 2…Drying room 3...Conveyor, 3A...Transport path, 3B...Return path 4. Drying unit 5...Unit drying room 6…Hot air generator 7…Exhaust duct 8a, 8b…Aperture 9…Supply port 10…Discharge port 11...combustion duct, 11a...air intake 12…Burner 13...Blower 14...Temperature sensor 15…Exhaust duct 16...Aperture 17...Endless conveyor belt 18a~18i...Roller section 19…Motor 20...Step 21…Plate 22...Thermometer T…Taro
Claims
1. A plurality of drying units arranged in a line, each of which has a unit drying chamber, a hot air generating device arranged above the unit drying chamber and capable of adjusting the temperature of hot air to be supplied, and an exhaust duct arranged below the unit drying chamber for discharging the hot air generated by the hot air generating device; a conveyor having a transport path passing through the drying chambers formed by connecting the unit drying chambers arranged in a row in the front-rear direction, The hot air generated by the hot air generator is supplied to the drying chamber and passed through the drying chamber while maintaining a temperature within the drying chamber at 50 degrees Celsius or higher; A large number of taros are transported along the transport path by the conveyor and passed through the drying chamber, The taro dryer is characterized in that the cut opening of the taro is dried to form a dry layer at the cut opening.
2. The taro dryer according to claim 1, The conveyor includes a mesh belt as an endless belt for conveying the taro, the endless conveying belt circulates so as to return to the conveying path via a return path passing under the drying chamber, The drying chamber has a hot air supply port on the upper side of the drying chamber and a hot air exhaust port on the lower side of the drying chamber, and has a plate arranged directly below the conveying path to prevent the hot air from flowing downward. A taro dryer.
3. The taro dryer according to claim 2, The plate is a corrugated plate curved in a wave shape in the conveying direction of the taro.
4. The taro dryer according to claim 3, The taro dryer is characterized in that the conveying path has a step at at least one location in the conveying direction.
Citation Information
Patent Citations
A method for drying and conditioning taro using a three-in-one combination of hot air, far-infrared radiation, and microwave.
CN105509416B
A taro peeling machine with a drying device
CN106418584B
Method for producing shochu (japanese distilled spirit)
JP2011139664A
Food drying device
JP2014119142A
Conveying dryer
JP2022100025A
