Side-exposed embedded trace packaging substrate and manufacturing method thereof

The circuit-embedded packaging substrate with exposed sides addresses integration and reliability issues by increasing solder contact area and preventing packaging defects through strategic cavity design, improving welding reliability and filling.

JP2024161903AActive Publication Date: 2024-11-20ZHUHAI YUEXIN SEMICON LLC
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
JP2024075066
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-08
Filing Date
2024-05-07
Publication Date
2024-11-20
Estimated Expiration
2044-05-07

AI Technical Summary

Technical Problem

Conventional wire bonding and chip flip-chip technologies face challenges in meeting the need for higher integration and reliability in semiconductor packaging, particularly due to limited contact area and potential welding defects caused by embedded circuits.

Method used

A circuit-embedded packaging substrate with exposed sides is developed, featuring cavities in the pad regions to increase the contact area with solder and ensure proper packaging material filling, thereby enhancing welding reliability and preventing defects.

Benefits of technology

The substrate design improves welding reliability by increasing the contact area between solder and pads, ensuring stable component mounting and preventing packaging material voids, thus enhancing the overall packaging quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024161903000001_ABST
    Figure 2024161903000001_ABST
Patent Text Reader

Abstract

To provide a side-exposed embedded trace packaging substrate and a manufacturing method thereof.SOLUTION: The side-exposed embedded trace substrate includes a medium layer, a first circuit layer, and a first circuit layer embedded in the medium layer. An outer surface of the first circuit layer is not higher than a surface of the medium layer, and the first circuit layer includes a pad, where the pad has a cavity to increase a side-exposed area of the pad. An area of contact between the substrate and solder during package welding is increased so that: the welding reliability is enhanced; the problem of poor welding or poor reliability caused by embedding of circuits is avoided; and the problem of poor filling of a packaging material due to an insufficient "gap" between a component and the pad during packaging is resolved.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to the technical field of semiconductor packaging, and in particular to a packaging substrate with an exposed side and an embedded circuit and a method for fabricating the same. [Background technology]

[0002] With the trend of electronic products becoming lighter, thinner, shorter and smaller, traditional wire bonding technology is increasingly unable to meet the demand for more I / O pins, and the application of chip flip chip technology that is suitable for more I / O pins is becoming more widespread. As an advanced packaging technology, it requires the packaging substrate to have a higher degree of integration, and the circuit-embedded packaging substrate technology is well suited to this demand. Summary of the Invention [Problem to be solved by the invention]

[0003] In view of this, an object of the present disclosure is to propose a circuit-embedded packaging substrate with exposed sides and a method for manufacturing the same. [Means for solving the problem]

[0004] In accordance with the above objectives, in a first aspect, the present disclosure provides a method for producing a method for manufacturing a semiconductor device comprising: providing an exposed-side, embedded-circuit packaging substrate including a medium layer and a first circuit layer embedded in the medium layer; The height of an outer surface of the first circuit layer does not exceed the surface of the medium layer, and the first circuit layer includes a pad, the pad having a cavity to increase an exposed area of ​​a side of the pad.

[0005] In some embodiments, the cavity is located at the edge or in the center of the pad.

[0006] In some embodiments, the depth of the cavity is less than the thickness of the first circuit layer, and the pads are used to mount components.

[0007] In some embodiments, the depth of the cavity is equal to the thickness of the first circuit layer, and the pad is used for welding components.

[0008] In some embodiments, the first circuit layer includes a first sublayer and a second sublayer below the first sublayer, a top surface of the first sublayer is flush with a surface of the media layer, and the cavity is surrounded by the first sublayer and exposes the media layer surrounded by the second sublayer.

[0009] In a second aspect, an embodiment of the present disclosure includes: (a) providing a substrate, the substrate including a media layer and a first circuit layer embedded within the media layer; (b) applying a first resist layer to the substrate and forming a first window by exposure and development, the first window exposing at least a partial region of a pad of the first circuit layer; (c) etching the first circuit layer exposed by the first window to form a cavity in a portion of the pad; and (d) removing the first resist layer to obtain a circuit-embedded packaging substrate having an exposed side.

[0010] In some embodiments, the etching process is selected from an acid etch or an alkaline etch.

[0011] In some embodiments, the first window is located at the edge of the pad or in the center of the pad.

[0012] In some embodiments, the depth of the cavity is less than the thickness of the first circuit layer, and the pad is used to mount a component; or The depth of the cavity is equal to the thickness of the first circuit layer, and the pad is used for welding components.

[0013] In some embodiments, step (a) comprises: (a1) providing a mounting plate; (a2) providing a first anti-coating layer on the support plate, and forming a second window by exposure and development; (a3) electroplating the second window area to form a first sub-layer of the first circuit layer; (a4) applying a second anti-coating layer to the first anti-coating layer and the first sub-layer, and forming a third window by exposure and development, the second anti-coating layer corresponding to the region where the side of the pad is exposed is maintained; (a5) electroplating the third window area to form a second sub-layer of the first circuit layer; (a6) removing the first anti-coating layer and the second anti-coating layer; (a7) forming a third anti-coating layer on the support plate and the first circuit layer, and forming a fourth window by exposure and development; (a8) electroplating the fourth window area to form a metal pillar; (a9) removing the third anti-coating layer; (a10) laminating a media layer and thinning the media layer until the metal pillars are exposed; (a11) forming a second circuit layer on the medium layer; (a12) removing the placement plate.

[0014] In some embodiments, the projections of the first window area and the third window area on the substrate do not overlap.

[0015] In some embodiments, step (a11) comprises: applying a seed layer to the medium layer; providing a fourth anti-coating layer on the seed layer, and forming a second circuit layer pattern by exposure and development; and electroplating to form the second circuit layer.

[0016] In some embodiments, the support plate includes a first metal layer and a second metal layer, and step (a12) includes: The method includes the step of separating the first metal layer and the second metal layer and etching the second metal layer that contacts the medium layer. Effect of the Invention

[0017] As can be seen from the above description, the circuit-embedded packaging substrate with exposed sides and the method for fabricating the same provided by the present disclosure provide a cavity in the pad area embedded in the first circuit layer of the medium layer to increase the exposed area of ​​the side of the pad, thereby increasing the contact area with the solder of the substrate during packaging welding, improving the reliability of welding, avoiding the problem of poor welding or unreliability due to the embedding of the circuit, and also solving the problem of poor filling of packaging material due to insufficient "gap" between the component and the pad during packaging. [Brief description of the drawings]

[0018] In the following, in order to more clearly describe the technical solutions in the present disclosure or related art, the drawings used in the description of the embodiments or related art are briefly introduced. Needless to say, the drawings described below are only the embodiments of the present disclosure, and those skilled in the art can obtain other drawings from these drawings without performing any novel work. In the drawings, the thickness and shape of some layers and regions may be exaggerated for better understanding and ease of description. [Figure 1]FIG. 1 is a structural schematic diagram of a circuit-embedded packaging substrate with exposed sides provided according to one embodiment of the present disclosure. [Diagram 2] FIG. 2 is a structural schematic diagram of a circuit-embedded packaging substrate with exposed sides provided according to another embodiment of the present disclosure. [Figure 3(a)] FIG. 3(a) is a schematic cross-sectional view of an intermediate structure in each step of a method for producing a circuit-embedded packaging substrate with an exposed side according to one embodiment of the present disclosure. [Figure 3(b)] FIG. 3(b) is a schematic cross-sectional view of an intermediate structure in each step of a method for producing a circuit-embedded packaging substrate with an exposed side according to one embodiment of the present disclosure. [Figure 3(c)] FIG. 3(c) is a schematic cross-sectional view of an intermediate structure in each step of a method for producing a circuit-embedded packaging substrate with an exposed side according to one embodiment of the present disclosure. [Figure 3(d)] FIG. 3(d) is a schematic cross-sectional view of an intermediate structure in each step of a method for producing a circuit-embedded packaging substrate with an exposed side according to one embodiment of the present disclosure. [Figure 3(e)] FIG. 3(e) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to one embodiment of the present disclosure. [Figure 3(f)] FIG. 3(f) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to one embodiment of the present disclosure. [Figure 4(a)] FIG. 4(a) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(b)] FIG. 4(b) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(c)] FIG. 4(c) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(d)]FIG. 4(d) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(e)] FIG. 4(e) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(f)] FIG. 4( f ) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(g)] FIG. 4(g) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(h)] FIG. 4(h) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(i)] FIG. 4(i) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(j)] FIG. 4(j) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(k)] FIG. 4( k ) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(l)] FIG. 4(l) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(m)] FIG. 4(m) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(n)]FIG. 4(n) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(o)] FIG. 4(o) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(p)] FIG. 4(p) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(q)] FIG. 4(q) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(r)] FIG. 4(r) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(s)] FIG. 4(s) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(t)] FIG. 4(t) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(u)] FIG. 4(u) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(v)] FIG. 4(v) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(w)] FIG. 4(w) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(x)]FIG. 4(x) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(y)] FIG. 4(y) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. [Figure 4(z)] FIG. 4(z) is a schematic cross-sectional view of an intermediate structure in each step of a method for fabricating a circuit-embedded packaging substrate with an exposed side according to another embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] Hereinafter, the present disclosure will be described in more detail using specific embodiments and with reference to the drawings, so that the objectives, technical solutions and advantages of the present disclosure can be more clearly understood.

[0020] Unless otherwise defined, technical or scientific terms used in the embodiments of the present disclosure have the common meanings understood by those skilled in the art. The terms "first", "second" and similar terms used in the embodiments of the present disclosure do not denote any order, quantity or importance, but are used to distinguish different components. The term "comprises" or similar terms means that the element or object appearing before the term covers the element or object listed after the term and its equivalents, but does not exclude other elements or objects. The terms "upper", "lower", "left", "right", etc. are used to express only relative positional relationships, and if the absolute position of the described object changes, the relative positional relationships may change accordingly.

[0021] Embedded trace substrate (ETS) is a packaging substrate with embedded circuit patterns that is manufactured based on coreless substrate technology.

[0022] By using Coreless technology, the circuitry on either side of the outermost circuitry (front or back) is embedded in the media layer, which can avoid etching the sidewalls of the circuitry when etching the seed layer later, improving the performance of the circuitry. In addition, the circuitry has better flatness than the conventional MSAP and SAP processes, and since the circuitry is embedded in the media layer, it helps reduce the thickness of the substrate.

[0023] However, in the case of a conventional embedded circuit board, all five sides except the front side of the circuit on a specific side are embedded in the medium layer. In the packaging welding process, the five sides of the conventional non-embedded circuit are in contact with the welding material, while only one side of the embedded circuit is in contact with the welding material, which makes it unreliable and prone to welding failure due to the influence of shear stress when contacting one side. In addition, when passive components need to be mounted on pads using surface mounted technology (SMT), the lack of "gap" between the components and pads often means that the packaging material cannot flow through the small gap, resulting in packaging voids.

[0024] In view of this, an exemplary embodiment of the present disclosure provides a circuit-embedded packaging substrate with exposed sides, which combines the advantages of traditional non-embedded circuit substrates and the advantages of embedded circuit substrates, and the traditional coreless embedded circuit packaging technology can solve the problem of poor welding or unreliability caused by embedding the circuit during packaging welding, and also solve the problem of poor filling of packaging material due to lack of "gap" between components and pads during packaging.

[0025] Specifically, as shown in FIG. 1 and FIG. 2, the circuit-embedded packaging substrate with exposed sides is: The substrate includes a media layer 301, 412 and a first circuit layer 302, 406 embedded in the media layer 301, 412, the first circuit layer 302, 406 including a pad (not shown in the figure) that includes a cavity 305, 420 to increase the exposed area of ​​a side of the pad.

[0026] In the embodiments of the present disclosure, the side of the pad refers to the side perpendicular to the surface direction of the substrate, and does not refer to the outer periphery of the pad.

[0027] In this technical solution, the cavity is used to expose the side of the pad, increasing the contact area between the solder 306 and the pad, thereby avoiding the problem of poor welding or unreliability; the cavity also widens the gap between the pad and the component 307, 421, which allows the packaging material to be filled sufficiently, improving the packaging quality.

[0028] In some embodiments, the cavity is located at the edge (left side in FIG. 1) or center (right side in FIG. 1, FIG. 2) of the pad, although the cavity may be located on one side of the pad or on multiple sides of the pad (see FIG. 3(d)), and the disclosure is not limited in this respect.

[0029] In addition, the width and depth of the cavity may be set based on design requirements. In the present disclosure, an exemplary description is given as follows.

[0030] In some embodiments, the depth of the cavity 420 is smaller than the thickness of the first circuit layer 406, and the pads are used to mount the components 421. The provision of the cavity 420 in this manner not only ensures the mounting stability of the mounted components 421, but also meets the need for filling the packaging material and avoids the waste of the packaging material.

[0031] In some embodiments, the depth of the cavity 305 is equal to the thickness of the first circuit layer 302, as shown in FIG. 1, and the pads are used to weld the components.

[0032] In some embodiments, the first circuit layer 406 includes a first sublayer 4061 and a second sublayer 4062, the surface of the first sublayer 4061 is flush with the surface of the media layer 412, and the cavity 420 is located in the first sublayer 4061 and has a bottom in the media layer 412.

[0033] An exemplary embodiment of the present disclosure also provides a method for fabricating a circuit-embedded packaging substrate having an exposed side edge. Figures 3(a) to 3(e) are schematic cross-sectional views of intermediate structures in each step of the method for fabricating a circuit-embedded packaging substrate having an exposed side edge according to an embodiment of the present disclosure.

[0034] The fabrication method includes the following steps: As shown in Fig. 3(a), a substrate 300 is provided (step (a)), where the substrate 300 includes a medium layer 301 and a first circuit layer 302, whose surfaces are flush with each other.

[0035] The number of medium layers included in the substrate 300 is not limited to one, but in the following process, only a substrate including one medium layer is shown. In this disclosure, the number of layers of the substrate, the thickness of each layer, and the type of material of each layer are not limited.

[0036] In addition, the substrate 300 may be fabricated using a coreless technique or a normal CCL build-up technique to fabricate multiple media layers, and the interlayer conductivity method may be, but is not limited to, conductivity through copper pillars, conductivity through laser drilling, or conductivity through machine drilling.

[0037] Next, as shown in Figures 3(b) and 3(c), a first resist layer 303 is applied to the substrate, and a first window 304 is formed by exposure and development (step (b)). The first window 304 at least partially overlaps the pad region of the first circuit layer 302. Setting the position of the first window 304 helps to ensure that a cavity formed later by etching is located in the pad region, increasing the exposed area of ​​the side of the pad.

[0038] Optionally, the first window 304 is located at the edge of the pad or in the center of the pad.

[0039] Optionally, the process of applying the first resist layer 303 may be laminating a dry resist film or applying a resist material, for example a photoresist material.

[0040] Generally, a resist film layer is applied to both sides of a substrate, and only the circuit-embedded side is shown in the figures. A resist film layer is applied to the non-embedded side only to protect the circuit from etching, and no special etching process is performed. This is not shown in the examples of this disclosure, as it is not the focus of the disclosure.

[0041] Then, as shown in Fig. 3(d), the first circuit layer in the first window region is etched to form a cavity 305 (step (c)), where the location of the cavity 305 is the location to be etched. Optionally, the etching process is selected from acid etching or alkaline etching.

[0042] In Fig. 3(d), the structure in the upper right is a plan view of the pad area. Note that the location of the cavity is merely exemplary, and the cavity 305 may be provided on one, two, three or four horizontal sides of the pad according to design requirements. Of course, the cavity 305 may be provided in the center of the pad.

[0043] Finally, as shown in FIG. 3(e), the first resist layer 303 is removed to obtain a circuit-embedded packaging substrate with exposed sides (step (d)). Those skilled in the art can understand that if resist film layers are applied to both sides of the substrate, the resist film layers on both sides are removed at the same time here. Those skilled in the art may select a suitable film peeling process according to their needs, and the present disclosure is not limited thereto.

[0044] In some embodiments, the depth of the cavity 305 is equal to the thickness of the first circuit layer 302, and the pad is used to weld the component. As shown in FIG. 3(f), the cavity can expose the sides of the pad, and welding at the exposed sides of the pad increases the contact area between the solder 306 and the substrate, while at the same time improving the ability of the solder to vertically encapsulate the substrate circuitry and withstand shear stress in the horizontal direction without fracturing, i.e. improving the reliability of the weld.

[0045] In addition, by welding the passive component 307 on such a pad, after the component is welded, a "void" will be formed at the bottom of the component, which is helpful for the packaging resin material to flow and fill in the later packaging process of the substrate, and avoids the technical problem that the "void" is too small, resulting in poor flow of adhesive at the bottom of the component.

[0046] 4(a) to 4(y) show schematic cross-sectional views of intermediate structures at each step of a method for fabricating a circuit-embedded packaging substrate with exposed sides according to another embodiment of the present disclosure, the illustrative embodiment including a specific method for fabricating the substrate (see FIG. 4(a) to FIG. 4(u)).

[0047] The manufacturing method includes the following steps: As shown in Fig. 4(a), a support plate is provided (step (a1)). Note that the support plate may have a symmetrical structure on both sides, and Fig. 4(a) shows only the structure on one side.

[0048] The mounting plate includes a mounting plate 401, a first metal layer 402, and a second metal layer 403, where the first metal layer 402 is attached to the mounting plate 401. Optionally, both the first metal layer 402 and the second metal layer 403 can be separated in a physical manner.

[0049] Optionally, the first metal layer 402 is a copper foil having a thickness of 16-20 μm, for example 18 μm, and the second metal layer 403 is a copper foil having a thickness of 2-3 μm.

[0050] Next, as shown in Figure 4(b) and Figure 4(c), a first anti-coating layer 404 is applied to the support substrate, and a second window 405 is formed by exposure and development (step (a2)). Here, the second window 405 exposes the area of ​​the circuit to be electroplated.

[0051] 4(d), the area of ​​the second window 405 is electroplated to form a first sub-layer 4061 of the first circuit layer (step (a3)). Exemplarily, the thickness of the first sub-layer 4061 may be half the thickness of the first circuit layer, or the thickness of the electroplating may be specifically set according to actual needs, and the present disclosure is not limited thereto.

[0052] Next, as shown in Figures 4(e) and 4(f), a second anti-coating layer 407 is applied to the first anti-coating layer 404 and the first sub-layer 4061, and a third window 408 is formed by exposure and development (step (a4)).

[0053] The second anti-coating layer 407 corresponding to the region where the side of the pad is exposed is maintained. By setting in this way, the second anti-coating layer at the corresponding position can be an etching barrier layer, thereby accurately controlling the etching depth of the cavity.

[0054] As one skilled in the art will appreciate, the third window 408 exposes locations to be subsequently electroplated such that the third window area is smaller than the second window area.

[0055] Next, as shown in FIG. 4(g), the third window area is electroplated to form the second sub-layer 4062 of the first circuit layer (step (a5)).

[0056] Subsequently, as shown in FIG. 4(h), the first anti-coating layer 404 and the second anti-coating layer 407 are removed (step (a6)).

[0057] Next, as shown in FIG. 4(i) and FIG. 4(j), a third anti-coating layer 409 is formed on the support plate and the first circuit layer, and a fourth window 410 is formed by exposure and development (step (a7)).

[0058] Then, as shown in FIG. 4(k), the fourth window area is electroplated to form metal pillars 411 (step (a8)).

[0059] Next, as shown in FIG. 4(l), the third anti-coating layer 409 is removed (step (a9)).

[0060] Next, as shown in FIG. 4(m) and FIG. 4(n), medium layer 412 is laminated and thinned until metal pillars 411 are exposed (step (a10)).

[0061] The material of the medium layer 412 may be resin coated copper foil (RCC), resin coated film (RCF), or a resin material not containing glass fiber, for example, one selected from the group consisting of liquid crystal polymer, bismaleimide triazine (BT) resin, prepreg, Ajinomoto Build-up (ABF) film, epoxy resin, and polyimide resin, but the present invention is not limited thereto.

[0062] Optionally, the process for thinning the media layer 412 is selected from grinding, plasma etching, or sandblasting.

[0063] Next, as shown in FIG. 4(o) to FIG. 4(r), a second circuit layer 416 is formed on the medium layer 412 (step (a11)).

[0064] The surface mounting process has limitations on the thickness of the circuit layer, and if the cavity is too deep or large, it is easy to cause uneven filling. In the embodiment of two-layer electroplating, which provides two anti-coating layers and electroplates in two steps, the medium layer that later replaces the second anti-coating layer can be an etching stop layer, so that the depth of the cavity can be adjusted by active control according to the fluidity requirements of the packaging material.

[0065] In some embodiments, step (a11) includes: As shown in Fig. 4(o), a seed layer 413 is applied to the medium layer 412, where the seed layer 413 can be fabricated by sputtering, chemical vapor deposition process. Optionally, the material of the seed layer 413 can be copper, copper+titanium. As shown in Fig. 4(p), a fourth anti-coating layer 414 is then applied to the seed layer 413, and a second circuit layer pattern 415 is formed by exposure and development, and finally, a second circuit layer 416 is formed by electroplating, as shown in Fig. 4(r).

[0066] As can be understood by those skilled in the art, the formation process of each anti-coating layer can be dry film lamination or coating, and the present disclosure is not limited thereto. The material of each anti-coating layer can be photoresist material or other organic material, and is not limited thereto.

[0067] Illustratively, the material of the first circuit layer, the second circuit layer and the metal pillar in the embodiment of the present disclosure may be copper.

[0068] Finally, as shown in Figures 4(s) to 4(u), the support plate is removed (step (a12)). Now, referring to Figure 4(s), the first metal layer 40 and the second metal layer 403 are separated, and as shown in Figure 4(u), the second metal layer 403 in contact with the medium layer 412 is etched.

[0069] Optionally, the method further includes removing the fourth anti-coating layer 414 before etching the second metal layer 403 in contact with the medium layer 412 (FIG. 4(t)). As can be understood by those skilled in the art, the step may be completed before the first metal layer 40 and the second metal layer 403 are separated, or after the first metal layer 40 and the second metal layer 403 are separated, and the present disclosure is not limited thereto.

[0070] Note that the seed layer 413 is etched at the same time as the second metal layer 403 is etched. Note that the second metal layer 403 is also used as a seed layer for forming the first circuit layer.

[0071] Thus, after removing the mounting plate, a substrate 400 is obtained, which may be used to fabricate a circuit-embedded packaging substrate with exposed sides.

[0072] Next, referring to the above-mentioned steps (b) to (d), a circuit-embedded packaging substrate with exposed sides is fabricated.

[0073] First, as shown in FIG. 4(v) and FIG. 4(w), a first resist layer 417, 418 is applied to a substrate 400, and a first window 419 is formed by exposure and development. The first resist layer 418 is used to protect a second circuit layer. Here, the projections of the first window area and the third window area on the substrate do not overlap. By setting in this way, the medium layer replacing the second anti-coating layer can be used as an etching barrier layer to control the etching depth of the first window area, thereby realizing effective control over the cavity depth.

[0074] Then, the first circuit layer in the first window area is etched to form a cavity 420, as shown in FIG. 4(x).

[0075] Finally, as shown in FIG. 4(y), the first resist layers 417 and 418 are removed to obtain a circuit-embedded packaging substrate with exposed sides.

[0076] Here, as shown in FIG. 4(z), the depth of the cavity is smaller than the thickness of the first circuit layer, and the pad may be used to mount the component 421, and a “void” is formed at the bottom of the component, which is helpful for the packaging resin material to flow and fill in the later packaging process of the substrate, and avoids the technical problem that the “void” is too small, resulting in poor adhesive flow at the bottom of the component.

[0077] Those skilled in the art will understand that the description of any of the above embodiments is merely illustrative and does not suggest that the scope of the present disclosure (including claims) is limited to these examples. Under the spirit of the present disclosure, the technical features of the above embodiments or different embodiments may be combined with each other, steps may be performed in any order, and there may be many other variations of different aspects of the above embodiments of the present disclosure, which are not provided in the detailed description for the sake of simplicity.

[0078] The embodiments of the present disclosure are intended to include all such replacements, amendments, and modifications that fall within the broad scope of the claims, and therefore any omissions, amendments, equivalent replacements, improvements, etc. that fall within the spirit and principles of the embodiments of the present disclosure are intended to be included within the scope of the claims of the present disclosure. [Explanation of symbols]

[0079] 40 First metal layer, 300 Substrate, 301 Medium layer, 302 First circuit layer, 303 First resist layer, 304 First window, 305 Cavity, 306 Solder, 307 Passive components, 400 Substrate, 401 Support plate, 402 First metal layer, 403 Second metal layer, 404 First anti-coating layer, 405 Second window, 406 First circuit layer, 407 Second anti-coating layer, 408 Third window, 409 Third anti-coating layer, 410 Fourth window, 411 Metal pillar, 412 Medium layer, 413 Seed layer, 414 Fourth anti-coating layer, 415 Second circuit layer pattern, 416 Second circuit layer, 417 First resist layer, 418 First resist layer, 419 First window, 420 Cavity, 421 Mounting components, 4061 1st sublayer, 4062 2nd sublayer

Claims

1. a media layer and a first circuit layer embedded within the media layer; A packaging substrate with an exposed side, characterized in that the height of an outer surface of the first circuit layer does not exceed the surface of the medium layer, the first circuit layer includes a pad, and the pad has a cavity to increase the exposed area of ​​the side of the pad.

2. The circuit-embedded packaging substrate according to claim 1 , wherein the cavity is located at an edge or a center of the pad.

3. 2. The circuit-embedded packaging substrate according to claim 1, wherein the depth of the cavity is smaller than the thickness of the first circuit layer, and the pads are used for mounting components.

4. 2. The circuit-embedded packaging substrate according to claim 1, wherein the depth of the cavity is equal to the thickness of the first circuit layer, and the pad is used for welding a component.

5. 2. The circuit-embedded packaging substrate of claim 1, wherein the first circuit layer includes a first sublayer and a second sublayer below the first sublayer, the top surface of the first sublayer is flush with the surface of the media layer, and the cavity exposes the media layer surrounded by the first sublayer and surrounded by the second sublayer.

6. (a) providing a substrate, the substrate including a media layer and a first circuit layer embedded within the media layer; (b) applying a first resist layer to the substrate and forming a first window by exposure and development, the first window exposing at least a portion of a pad of the first circuit layer; (c) etching the first circuit layer exposed by the first window to form a cavity in a portion of the pad; and (d) removing the first resist layer to obtain a circuit-embedded packaging substrate having an exposed side.

7. 7. The method of claim 6, wherein the etching process is selected from acid etching and alkaline etching.

8. 7. The method of claim 6, wherein the first window is located at an edge of the pad or at the center of the pad.

9. the depth of the cavity is less than the thickness of the first circuit layer; or 7. The method of claim 6, wherein the depth of the cavity is equal to the thickness of the first circuit layer.

10. Step (a) (a1) providing a mounting plate; (a2) providing a first anti-coating layer on the support plate, and forming a second window by exposure and development; (a3) electroplating the second window area to form a first sub-layer of the first circuit layer; (a4) applying a second anti-coating layer to the first anti-coating layer and the first sub-layer, and forming a third window by exposure and development, the second anti-coating layer corresponding to the region where the side of the pad is exposed is maintained; (a5) electroplating the third window area to form a second sub-layer of the first circuit layer; (a6) removing the first anti-coating layer and the second anti-coating layer; (a7) forming a third anti-coating layer on the support plate and the first circuit layer, and forming a fourth window by exposure and development; (a8) electroplating the fourth window area to form a metal pillar; (a9) removing the third anti-coating layer; (a10) laminating a media layer and thinning the media layer until the metal pillars are exposed; (a11) forming a second circuit layer on the medium layer; The method of claim 6, further comprising the step of: (a12) removing the support plate.

11. 11. The method of claim 10, wherein the projections of the first window area and the third window area on the substrate do not overlap.

12. Step (a11) is applying a seed layer to the medium layer; applying a fourth anti-coating layer to the seed layer, and forming a second circuit layer pattern by exposure and development; 11. The method of claim 10, further comprising the step of electroplating to form the second circuit layer.

13. The support plate includes a first metal layer and a second metal layer, and step (a12) includes:

11. The method of claim 10, further comprising the step of: separating the first metal layer and the second metal layer and etching the second metal layer in contact with the medium layer.

Citation Information

Patent Citations

  • Substrate for loading semiconductor chip, manufacturing method therefor, semiconductor device and manufacturing method therefor

    JP2003229512A

  • Module for mounting electrical component and method for manufacturing the same

    JP2005051204A

  • Method for manufacturing wiring board

    JP2009253118A

  • Circuit module, electronic component mounting board and circuit module manufacturing method

    JP2012164934A

  • Wiring board and method of manufacturing the same

    JP2014132673A