Method for reducing volume of contaminated concrete

The method of crushing, heating, and trapping gases in an alkaline solution efficiently reduces the volume of contaminated concrete, addressing inefficiencies in existing methods by minimizing labor and time while containing radioactive gases.

JP2024162022APending Publication Date: 2024-11-21SHIMIZU CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023077164
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-09
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

Existing methods for reducing the volume of contaminated concrete contaminated with radioactive carbon dioxide are inefficient, requiring significant energy, time, and labor due to high-temperature heating and crushing processes, which can scatter radioactive gases and are impractical for large concrete volumes.

Method used

A method involving crushing contaminated concrete to a size 1 to 2 times the maximum aggregate size, heating it to 300 to 400°C, and using an alkaline solution to trap generated gases, followed by a grinding process to separate aggregate and mortar.

Benefits of technology

Reduces the volume of contaminated concrete efficiently without extensive labor or time, effectively containing radioactive gases and improving separation efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024162022000001_ABST
    Figure 2024162022000001_ABST
Patent Text Reader

Abstract

To provide a method for reducing a volume of contaminated concrete capable of reducing the volume of contaminated concrete without requiring much labor and time.SOLUTION: A method for reducing a volume of contaminated concrete according to the present invention is a method for reducing the volume of contaminated concrete that contains aggregate and mortar and is contaminated by radioactive carbon dioxide, and comprises a crushing process of crushing the contaminated concrete into pieces 1 to 2 times the maximum dimension of the aggregate, a heating process of heating the crushed contaminated concrete to a temperature of 300 to 400°C, and a grinding process of separating the aggregate from the heated contaminated concrete by grinding processing.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] The present invention relates to a method for reducing the volume of contaminated concrete that contains aggregate and mortar and is contaminated with radioactive carbon dioxide. [Background technology]

[0002] Generally, operating nuclear reactors are radioactive carbon ( 14 C) is produced, and the radiocarbon produced is converted into radiocarbon dioxide ( 14 Radioactive carbon dioxide exists as CO2. Radioactive carbon dioxide is absorbed by concrete, but because gaseous substances are free to move, the contamination range is wide. In fact, widespread contamination by radioactive carbon dioxide has been found in the concrete of nuclear power plant reactor buildings, resulting in a large amount of radioactive waste. Against this background, methods for reducing the volume of radioactive waste have been proposed. Specifically, radioactive gases and liquids penetrate the mortar portion of concrete, resulting in contamination of the mortar but not the coarse aggregate. Therefore, if concrete is separated into coarse aggregate and mortar, the coarse aggregate can be disposed of as non-radioactive waste, and the mortar can be disposed of as radioactive waste. For this reason, Patent Document 1 proposes a method for reducing the volume of radioactive waste by separating aggregate from contaminated concrete by grinding. Patent Document 2 also describes that heating contaminated concrete to a temperature of 300-500°C before grinding improves the separation of aggregate and mortar. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Application Laid-Open No. 2017-227493 [Patent Document 2] Japanese Patent Application Publication No. 11-292602 Summary of the Invention [Problem to be solved by the invention]

[0004] However, if contaminated concrete is heated to temperatures between 300 and 500°C before grinding, the radioactive carbon dioxide absorbed in the contaminated concrete dissipates, and the amount of dissipation increases with increasing temperature. If the contaminated concrete is heated at even higher temperatures, the entire amount of absorbed radioactive carbon dioxide will volatilize, allowing the contaminated concrete to be disposed of as non-radioactive waste. However, heating at high temperatures requires a large amount of energy and requires the disposal of high concentrations of radioactive carbon dioxide, making this impractical. Furthermore, when heating large pieces of contaminated concrete, it takes a long time for the heat to reach the interior of the contaminated concrete. In this case, crushing the contaminated concrete into smaller pieces makes it easier for the heat to reach the interior of the contaminated concrete, but the crushing process takes time.

[0005] The present invention has been made to solve the above-mentioned problems, and its object is to provide a method for reducing the volume of contaminated concrete that can reduce the volume of contaminated concrete without requiring much effort and time. [Means for solving the problem]

[0006] The method for reducing the volume of contaminated concrete of the present invention is a method for reducing the volume of contaminated concrete that contains aggregate and mortar and is contaminated with radioactive carbon dioxide, and includes a crushing step of crushing the contaminated concrete into pieces that are 1 to 2 times the maximum size of the aggregate, a heating step of heating the crushed contaminated concrete to a temperature of 300 to 400°C, and a grinding step of separating the aggregate from the heated contaminated concrete by a grinding process.

[0007] The heating step may include a step of supplying gas generated during heating to the alkaline solution. [Effects of the Invention]

[0008] According to the method for reducing the volume of contaminated concrete of the present invention, the volume of contaminated concrete can be reduced without requiring much labor and time. [Brief explanation of the drawings]

[0009] [Figure 1] FIG. 1 is a flowchart showing the flow of a process for reducing the volume of contaminated concrete according to one embodiment of the present invention. [Figure 2] FIG. 2 shows the change in the removal rate of radioactive carbon dioxide with the change in heating temperature. [Figure 3] FIG. 3 is a schematic diagram showing the configuration of an electric furnace. DETAILED DESCRIPTION OF THE INVENTION

[0010] Hereinafter, a method for reducing the volume of contaminated concrete according to one embodiment of the present invention will be described with reference to the drawings.

[0011] FIG. 1 is a flowchart showing the flow of a process for reducing the volume of contaminated concrete according to one embodiment of the present invention.

[0012] As shown in FIG. 1, a process for reducing the volume of contaminated concrete according to one embodiment of the present invention includes a crushing step S1, a heating step S2, and a grinding step S3.

[0013] First, in the crushing step S1, the contaminated concrete is crushed to a predetermined size. Specifically, the maximum size of coarse aggregate used in concrete is generally 25 mm. Crushing the contaminated concrete smaller than the size of the aggregate would also crush the aggregate, resulting in an inappropriate size. Crushing the contaminated concrete to a size 1 to 2 times the maximum size of the aggregate results in clumps with mortar adsorbed to each aggregate, making it an appropriate size for grinding. Crushing the contaminated concrete to a size larger than 1 to 2 times the maximum size of the aggregate results in the crushed debris containing several aggregate particles, reducing the efficiency of separating the aggregate and mortar in the initial stage of the grinding step S3. For this reason, the crushed size of the contaminated concrete is set to be within the range of 1 to 2 times the maximum size of the aggregate.

[0014] Next, in the heating step S2, the contaminated concrete crushed in the crushing step S1 is heated in an electric furnace for a predetermined time. Specifically, the removal rate of radioactive carbon dioxide when the contaminated concrete collected from the reactor building is heated at 250 to 600°C for 2 hours is shown in Figure 2 (ICONE16-48602, Proceedings of the 16 th (Excerpt from the International Conference on Nuclear Engineering) As shown in Figure 2, if contaminated concrete is heated to a temperature of 300-400°C, the removal rate (volatilization rate) of radioactive carbon dioxide can be reduced to a few percent. For this reason, the heating temperature for contaminated concrete should be set within the range of 300-400°C.

[0015] In addition, if the contaminated concrete A is heated using an electric furnace 1 as shown in Figure 3 and the gas generated during heating is supplied to the alkaline solution 2, the radioactive carbon dioxide ( 14 Since the CO2 gas is trapped in the alkaline solution 2, it is possible to prevent the dispersion of radioactive carbon dioxide gas. In this case, it is preferable to connect two or three traps for the alkaline solution 2 in series. It is also preferable to use a sodium hydroxide solution as the alkaline solution 2. The pH of the alkaline solution 2 is monitored using a pH meter 3, and when the pH becomes more acidic than 12, the alkaline solution 2 is replaced and the used alkaline solution 2 is disposed of as radioactive waste. Since radioactive carbon dioxide gas is not absorbed when the pH becomes more acidic than neutral, the pH at which the alkaline solution 2 is replaced is set to 12 as a safety margin.

[0016] Finally, in the grinding step S3, the contaminated concrete is reduced in volume by separating aggregate from the contaminated concrete by grinding, for example, using the method described in Patent Document 1. This completes the series of processes for reducing the volume of contaminated concrete.

[0017] As is clear from the above explanation, the process for reducing the volume of contaminated concrete, which is one embodiment of the present invention, includes a crushing step S1 in which the contaminated concrete is crushed into pieces one to two times the maximum size of the aggregate, a heating step S2 in which the crushed contaminated concrete is heated to a temperature of 300 to 400°C, and a grinding step S3 in which the aggregate is separated from the heated contaminated concrete by a grinding process. This makes it possible to reduce the volume of contaminated concrete without requiring much labor or time.

[0018] Although the present invention has been described above as an embodiment, the present invention is not limited to the descriptions and drawings that form part of the disclosure of the present invention. In other words, other embodiments, examples, and operational techniques that can be made by those skilled in the art based on the present invention are all included in the scope of the present invention. [Explanation of symbols]

[0019] 1 electric furnace 2. Alkaline solution 3 pH meter

Claims

1. A method for reducing the volume of contaminated concrete that contains aggregate and mortar and is contaminated by radioactive carbon dioxide, comprising the steps of: A crushing step of crushing the contaminated concrete into pieces having a size 1 to 2 times the maximum dimension of the aggregate; a heating step of heating the crushed contaminated concrete to a temperature of 300-400°C; a grinding step of separating the aggregate from the heated contaminated concrete by a grinding process; A method for reducing the volume of contaminated concrete, comprising:

2. The method for reducing the volume of contaminated concrete according to claim 1 , wherein the heating step includes a step of supplying gas generated during heating to an alkaline solution.

Citation Information

Patent Citations

  • Cement-based composition

    JP1999292602A

  • Contaminated concrete mass decontamination method and contaminated concrete mass decontamination device

    JP2017227493A