Analysis device
A protective layer in the porous substrate of analytical devices prevents plasticizer leakage, maintaining measurement sensitivity and stability, addressing performance degradation issues during long-term storage.
Patent Information
- Application Number
- JP2023078162
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-10
- Publication Date
- 2024-11-21
AI Technical Summary
Analytical devices using porous substrates face performance degradation due to plasticizer leakage during long-term storage, which affects measurement sensitivity and stability, especially in high-temperature environments.
Incorporating a protective layer within the porous substrate near the ion-selective membrane to inhibit plasticizer penetration, using materials like polyimide resin or fluororesin to seal the ion-selective membrane and base material interface.
Maintains measurement sensitivity and stability over long-term storage by preventing plasticizer diffusion, ensuring accurate ion concentration measurements even in non-temperature-controlled environments.
Smart Images

Figure 2024162555000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an analytical device having a flow path region formed inside a porous substrate. [Background technology]
[0002] In recent years, analytical devices that utilize small microchannels to efficiently perform biochemical analysis within a single chip have been attracting attention in a wide range of fields. Specifically, small analytical devices are attracting attention not only in biochemical research, but also in fields such as medicine, drug discovery, healthcare, the environment, and food.
[0003] In the early 1990s, photolithography and molds were used to form micrometer-sized fine flow channels on glass or silicon, and microanalysis chips were developed that perform sample pretreatment, stirring, mixing, reaction, and detection on a single chip. As a result, miniaturization of testing systems, rapid analysis, and reduction in specimens and waste liquids were realized.
[0004] Electrochemical analysis is a method of measuring the concentration of a target substance by measuring the potential between electrodes immersed in the sample to be analyzed, and is widely used in fields such as medicine and the environment. Conventional electrochemical analysis is performed by engineers using advanced equipment, which limits the fields and resources in which the measurement can be performed. However, there is a demand for inexpensive, easy-to-use, disposable microanalytical chips for electrochemical analysis for use in medical care in developing countries, remote areas, and disaster sites where medical facilities are insufficient, and for use in airports and other locations where it is necessary to stop the spread of infectious diseases at the border.
[0005] Patent Document 1 proposes a device including a microanalysis chip capable of measuring potential differences using a porous substrate, enabling electrochemical measurements that are low-cost, easy to handle, and easy to dispose of. This device describes a configuration for measuring potential differences between an ion-selective electrode using an ion-selective membrane as the working electrode and a reference electrode, which includes one or more working electrodes and one reference electrode on a porous substrate. In addition, the ion-selective membrane of this device typically contains a lipophilic ion receptor (ionophore) and a lipophilic ion exchanger in an optimized molar ratio, both of which are incorporated into a polymer membrane matrix such as plasticized poly(vinyl chloride) (PVC), and the potential difference can be measured using this ion-selective membrane.
[0006] In addition, Non-Patent Document 1 proposes a filter paper-based measurement device for measuring the concentrations of Na ions and K ions. This device has a dispensing section for dispensing a sample, and the dispensed sample permeates from the dispensing section into the working electrode and the reference electrode, electrically connecting the two electrodes and enabling potential difference measurement. The ion-selective membrane of this device is prepared using ionophore, anion remover, and PVC, as well as DOS and NPOE as plasticizers for Na ions and K ions, respectively, and the use of such an ion-selective membrane makes it possible to measure potential differences.
[0007] In addition, Non-Patent Document 1 describes that in order to obtain a stable potential at the reference electrode, KCl ion crystals are deposited on the reference electrode. This allows KCl to dissolve in the sample during measurement, maintaining a high concentration of Cl ions in the reference electrode region, and obtaining a stable reference electrode potential. Furthermore, Non-Patent Document 1 describes that an ion-selective membrane formed to cover the working electrode selects only the ions to be measured, enabling measurement without being affected by other ions. [Prior art documents] [Patent documents]
[0008] [Patent Document 1] US Patent Application Publication No. 2016 / 033438 [Non-patent literature]
[0009] [Non-Patent Document 1] Nipapan Ruecha, Orawon Chailapakul, Koji Suzuki and Daniel Citterio “Fully Inkjet-Printed Paper-Based Potentiometric Ion-Sensing Devices” Analytical chemistry August 29, 2017 Published, 89, pp.10608-10616 Summary of the Invention [Problem to be solved by the invention]
[0010] However, in the configuration of the analytical device using the porous substrate as described above, the performance may not be maintained during long-term storage. Specifically, in the analytical device using the porous substrate, an electrode and an ion-selective membrane are formed on the porous substrate, and the ion-selective membrane is partially in contact with the porous substrate. In addition, the ion-selective membrane contains a plasticizer, which is a lipophilic ion exchanger, and is usually liquid during measurement (above room temperature) so that it has the function of transporting ionophores during measurement, and can flow through the ion-selective membrane. Therefore, the plasticizer seeps out from the ion-selective membrane during long-term storage. When the seeped plasticizer comes into contact with the porous substrate, the seepage of the plasticizer is accelerated due to the capillary phenomenon of the porous substrate, and the plasticizer may further diffuse toward the porous substrate. This reduces the plasticizer in the ion-selective membrane, and the material ratio in the ion-selective membrane cannot be maintained in an appropriate state, resulting in a change in the responsiveness to the ion concentration of the specimen, i.e., the measurement sensitivity, and even with the same concentration of the specimen, the potential on the working electrode side may change.
[0011] This problem is influenced by the fluidity of the plasticizer in the ion-selective membrane, and is particularly likely to occur during long-term storage in a high-temperature environment. Therefore, the degree of occurrence of the problem can be reduced by setting the storage environment of the analytical device at a low temperature, such as below 10°C. On the other hand, storing the analytical device at a low temperature requires storage equipment and power supply facilities, which may not be usable in some medical settings, such as POCT. Therefore, there is a demand for chips that can perform more stable analysis even after long-term storage, even if they are not stored at low temperatures.
[0012] In view of the above, an object of the present invention is to provide an analytical device for measuring the concentration of an electrolyte that maintains good measurement sensitivity even after long-term storage and that can obtain an appropriate potential for a selected ion. [Means for solving the problem]
[0013] According to one aspect of the present invention, porous substrate, an electrode formed within, on, or from within and onto the surface of the porous substrate; an ion-selective membrane covering the electrode; and protective layer, the ion selective membrane comprises a plasticizer; The protective layer is formed inside the porous substrate in close proximity to at least a portion of the ion selective membrane and contains a component that inhibits the penetration of the plasticizer. Analytical Devices is provided. Effect of the Invention
[0014] According to the present invention, it is possible to provide an analytical device for measuring the concentration of an electrolyte, which maintains good measurement sensitivity even during long-term storage and can obtain an appropriate potential for a selected ion. [Brief description of the drawings]
[0015] [Figure 1A] FIG. 1 is a schematic diagram illustrating an analytical device according to a first embodiment. [Figure 1B]FIG. 1B is a cross-sectional view taken along the dotted line in FIG. 1A. [Figure 2A] FIG. 2 is a schematic diagram showing an analytical device according to a modified example of the first embodiment. [Figure 2B] FIG. 2B is a cross-sectional view taken along the dotted line in FIG. 2A. [Diagram 3] FIG. 1 is a schematic diagram illustrating an analytical device according to a first embodiment. [Figure 4A] FIG. 13 is a schematic diagram showing an example of a potentiometric measurement of an analytical device. [Figure 4B] FIG. 2 is a schematic diagram illustrating a state when a sample is dispensed into an analytical device. [Figure 5A] FIG. 2 is a schematic diagram illustrating an analytical device according to a comparative example of the present invention. [Figure 5B] FIG. 5B is a cross-sectional view taken along the dotted line in FIG. 5A. [Figure 6A] FIG. 2 is a schematic diagram showing the analytical devices of Examples 2 and 4. [Figure 6B] FIG. 6B is a cross-sectional view taken along the dotted line in FIG. 6A. [Figure 7A] FIG. 13 is a schematic diagram showing an analytical device according to a modified example of Example 3. [Figure 7B] FIG. 7B is a cross-sectional view taken along the dotted line in FIG. 7A. [Figure 8A] FIG. 13 is a schematic diagram showing the analytical device of Example 5. [Figure 8B] FIG. 8B is a cross-sectional view taken along the dotted line in FIG. 8A. [Figure 9A] FIG. 11 is a schematic diagram showing how a sample is measured using the analytical device of Example 5. [Figure 9B] 9B is a cross-sectional view taken along the dotted line in FIG. 9A. [Figure 10] FIG. 13 is a schematic diagram showing a modified example of the analysis device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0016] One embodiment of the present invention provides an analytical device having a porous substrate, an electrode formed inside, on a surface, or from inside to a surface of the porous substrate, an ion selective membrane covering the electrode, and a protective layer, wherein the ion selective membrane contains a plasticizer, and the protective layer is formed inside the porous substrate in close proximity to at least a portion of the ion selective membrane and contains a component that inhibits penetration of the plasticizer.
[0017] The analytical device may have a flow path region (sometimes simply referred to as a flow path) surrounded by a flow path wall formed inside the porous substrate. In this case, the electrodes, the ion selective membrane, and the protective layer are formed in the flow path region. The flow path region includes a first flow path chamber, a second flow path chamber, and a flow path connecting them, and the electrodes, the ion selective membrane, and the protective layer are formed in the first flow path chamber, and the second flow path chamber may include a reference electrode.
[0018] The ion selective membrane may be formed within, on, or both within and on the surface of the porous substrate and includes a plasticizer.
[0019] The protective layer is formed in close proximity to at least a part of the back surface or periphery of the ion selective membrane. The back surface refers to the surface facing the front surface. In this specification, "close" and "close to" mean either adjacent or nearby. The protective layer is formed in close proximity to at least a part of the ion selective membrane, such as the electrode or the bottom surface and periphery of the ion selective membrane. The protective layer inhibits the penetration of the plasticizer contained in the ion selective membrane, and suppresses the plasticizer in the ion selective membrane from seeping out and diffusing into the porous substrate through the voids in the porous substrate or the fibers constituting the porous substrate. Therefore, the protective layer is preferably made of a material with which the plasticizer is incompatible. The protective layer preferably contains a resin, and examples of such resins include polyimide resins and fluorine resins. The polyimide resin is preferably a resin made of a polymer compound containing an imide bond (-CO-NR-CO-). The fluorine resin is preferably a resin containing a fluoroalkylene structure, and preferably contains a repeating structure of -(CF)- or -(CF2)-. Alternatively, the protective layer can be formed by printing and further heating resin particles, in which case a preferred example of the resin particles is toner particles.
[0020] Examples and comparative examples of the present invention will be described below with reference to the drawings. Note that the following examples are illustrative and do not limit the present invention to the contents of the embodiments. In addition, in the following drawings, components that are not necessary for the description of the embodiments are omitted from the drawings.
[0021] [Example 1] The configuration of the analytical device of this embodiment will be described with reference to the drawings. 1A and 1B show an analytical device 100 of Example 1. The analytical device 100 has a flow path region 3 surrounded by a flow path wall 2 provided inside a porous substrate 1. The analytical device 100 has a horizontal width L1 of 22 mm and a vertical width H1 of 17 mm. The flow path region 3 has a first flow path chamber 3a, a second flow path chamber 3b, each 6 mm square, a third flow path chamber 3c and a fourth flow path chamber 3d, each 6 mm square, each 6 mm wide and 3 mm high, as contact portions of the base electrode, a flow path 6 mm wide and 4 mm high connecting the first flow path chamber 3a and the second flow path chamber 3b, and a flow path 2 mm wide and 3 mm high connecting the first flow path chamber 3a and the third flow path chamber 3c, and the second flow path chamber 3b and the fourth flow path chamber 3d. The third flow path chamber 3c and the fourth flow path chamber 3d can be provided from the viewpoint of adhesion between the substrate and the electrodes, but they may not be provided. A working electrode 4 is disposed in the first flow channel chamber 3a, and the working electrode 4 is composed of a 2 mm square base electrode 5 connected to the third flow channel chamber and a 4 mm square ion selective membrane 6 provided to cover it. A plasticizer 7 is contained in the ion selective membrane 6. A protective layer 8 is disposed on the back surface of the working electrode 4 in the analytical device 100, at the portion where the ion selective membrane 6 is present. In this embodiment, the protective layer 8 is actually located on the back surface of the ion selective membrane 6 and cannot be seen from above, but for convenience, the protective layer 8 is shown in FIG. 1A. FIG. 1B is a cross-sectional view of the analytical device 100 taken along the dotted line in FIG. 1A.
[0022] The specific configuration and manufacturing method of the analytical device of this embodiment will be described. In this embodiment, filter paper with a thickness of 100 μm and a porosity of 50% was used as the porous substrate 1. By using filter paper as the porous substrate, capillary action can be generated in the liquid, and the sample to be measured can flow through the flow path even in an electroless environment.
[0023] In this embodiment, filter paper is used as the porous substrate, but the present invention is not limited to this, and any substrate that generates capillary action in liquid may be used. For example, the porous substrate may have open cells and nanofibers or other porous structures such as a mesh structure, and may be resin, glass, an inorganic substrate, fabric, metal paper, or the like.
[0024] In addition, the thickness of the porous substrate 1 is 100 μm, but it is not limited to this and can be appropriately selected depending on the purpose, and about 20 μm to 300 μm is often used. If it is less than 20 μm, the strength as a substrate may not be maintained. If it is more than 300 μm, the materials such as the ion selective membrane 6 and the protective layer 8 may easily diffuse into the analytical device, which may deteriorate the dimensional accuracy, but depending on the application, the arrangement in the analytical device may be adjusted and a thick porous substrate 1 with a thickness of about 600 μm may be used.
[0025] The flow channel region 3 was formed by the method described in JP 2021-37612 A. Specifically, a desired flow channel pattern was formed in an unfixed state on a porous substrate by electrophotography using flow channel wall forming particles T1 (toner) having melting properties, and then the substrate was heated in an oven or heater to cause the flow channel pattern to penetrate into the porous substrate, thereby forming the flow channel wall 2 and the flow channel region 3.
[0026] In this example, particles T1 having a number-average particle size of 6.5 μm, which were produced by the following production method, were used as the flow path wall forming particles. The production method of particles T1 will be described below.
[0027] <Production of Particle T1> [Preparation of polymerizable monomer composition] The following composition was mixed and dispersed in a ball mill for 3 hours. Styrene 70.0 parts n-Butyl acrylate 30.0 parts Divinylbenzene 0.1 parts Polyester resin 5.0 parts (Polycondensation product of propylene oxide modified bisphenol A and isophthalic acid (glass transition point 65°C, weight average molecular weight (Mw) 10,000, number average molecular weight (Mn) 6,000)) The obtained dispersion was transferred to a reactor equipped with a propeller stirring blade and heated to 60°C while stirring at a rotation speed of 300 rpm, after which 3.0 parts of 2,2'-azobis(2,4-dimethylvaleronitrile) was added and dissolved to obtain a polymerizable monomer composition.
[0028] [Preparation of aqueous dispersion medium] 710 parts of ion-exchanged water and 450 parts of 0.1 mol / L-sodium phosphate aqueous solution were added to a 2 L four-neck flask equipped with a high-speed stirring device TK Homomixer (manufactured by Primix Corporation), and heated to 60° C. while stirring at a rotation speed of 12,000 rpm. 68.0 parts of 1.0 mol / L-calcium chloride aqueous solution were added thereto to prepare an aqueous dispersion medium containing calcium phosphate (a poorly water-soluble dispersion stabilizer).
[0029] [Granulation / Polymerization] The polymerizable monomer composition was put into the aqueous dispersion medium, and the rotation speed was maintained at 12000 rpm. 10 parts of t-butyl peroxypivalate, a polymerization initiator, was spread and granulated for 15 minutes. After that, the high-speed agitator was replaced with a propeller agitator, and the polymerization reaction was continued for 5 hours while maintaining the internal temperature at 60°C. The internal temperature was then raised to and maintained at 80°C, and the polymerization reaction was continued for another 3 hours. After the polymerization reaction was completed, the remaining monomer was distilled off at 80°C under reduced pressure, and the mixture was cooled to 30°C to obtain a polymer microparticle dispersion.
[0030] [Cleaning] The polymer microparticle dispersion was transferred to a washing container, and diluted hydrochloric acid was added while stirring to adjust the pH to 1.5. The dispersion was stirred for 2 hours, and then subjected to solid-liquid separation with a filter to obtain polymer microparticles. This was added to 1200 parts of ion-exchanged water and stirred, and the dispersion was made again, and then subjected to solid-liquid separation with a filter. This operation was repeated three times to obtain mother particles of particles T1.
[0031] [External attachment] Furthermore, 1.0 part of a flowability improver (silica having a number average particle diameter of 7 nm) surface-treated with hexamethyldisilazane was dry-mixed with 100.0 parts of the obtained base particles for 5 minutes in a Henschel mixer to obtain particles T1 for forming a flow path pattern image having a number average particle diameter D1 of 6.5 μm.
[0032] The method of forming the flow paths is not limited to the method of this embodiment. As long as the flow paths can be formed in a flow path pattern, other methods such as cutting the porous substrate 1 and leaving only the flow path shape, or forming the flow path walls 2 with a wax printer may be used.
[0033] Next, the protective layer, which is a feature of the present invention, will be described. In this embodiment, the protective layer 8 was made of flow path wall forming particles T1 (toner). As a manufacturing method, the flow path wall 2 was patterned on the ion selective membrane 5 formed portion on the porous substrate 1 by electrophotography, as in the above-mentioned flow path wall forming process. Here, it is preferable that the protective layer portion has as many flow path wall forming particles as possible permeate into the porous substrate from the viewpoint of sealing the porous substrate. Therefore, the flow path wall pattern drawing formation process by electrophotography and the permeation process into the inside of the porous substrate by an oven or heater were repeatedly performed four times so that the amount of the flow path wall 2 pattern drawn in the protective layer 8 portion was greater than the amount of the flow path wall 2 drawn in the flow path wall forming process. That is, the protective layer contained about four times as many flow path wall forming particles as the flow path wall. The formed protective layer pattern is as shown in FIG. 1A and FIG. 1B.
[0034] In this embodiment, the protective layer forming step was performed after the flow path wall forming step, but the pattern formation in the flow path wall forming step and the pattern formation in the protective layer forming step may be performed simultaneously. In this case, since there is a limit to the amount of the flow path wall forming particles transferred to the porous substrate, the protective layer forming step may be additionally performed as necessary, as in this embodiment, to increase the amount of drawing in the protective layer portion.
[0035] In this embodiment, toner, which is a particle for forming the flow path wall, is used as the material of the protective layer 8, but the present invention is not limited thereto. It is sufficient that the protective layer 8 seals the area where the ion selective membrane 6 and the porous substrate 1 are close to each other. An analytical device according to a modified example of the first embodiment is shown in FIG. 2A and FIG. 2B. For example, as shown in the cross-sectional view of FIG. 2B, a known toner that is less likely to penetrate into the porous substrate 1 can be placed as a protective layer in advance at the area where the ion selective membrane 6 and the porous substrate 1 are in contact with each other. If the porous substrate 1 on which the protective layer is formed is turned upside down and a base electrode 5 and an ion selective membrane 6 are formed thereon, a configuration shown in FIG. 8B can be obtained. In addition, by drawing the toner locally, a protective layer can be formed around the ion selective membrane as shown in FIG. 7B. In addition, by locally increasing or decreasing the amount of drawing, a protective layer can be formed on the back side and around the ion selective membrane as shown in FIG. 6B. The thickness of the protective layer (thickness perpendicular to the surface of the device) is preferably 10 μm or more when the protective layer is disposed on the back surface of the ion selective membrane, and there is no particular upper limit. If it is 10 μm or less, there is a possibility that the penetration of the plasticizer cannot be sufficiently inhibited. When the protective layer is disposed around the ion selective membrane, it is desirable to adjust the width of the protective layer so that the specimen dropped on the ion selective membrane can move to the porous substrate. As shown in FIG. 10, when the ion selective membrane is formed inside the porous substrate, the width of the protective layer (thickness in the surface direction of the device) is preferably 1 mm or less. When the ion selective membrane is located on the substrate surface, as shown in FIG. 4B, the specimen moves by utilizing the height difference between the ion selective membrane and the porous substrate, so the upper limit of the width of the protective layer can be 2 mm.
[0036] In this embodiment, as shown in Figure 1B, a protective layer was placed inside the porous substrate in the ion selective membrane forming portion, but this is not limited to this. As in the embodiments described later, by filling the area where the ion selective membrane 6 and the porous substrate 1 are in contact with each other with a protective layer, it is possible to reduce the diffusion of the plasticizer 7 contained in the ion selective membrane 6 into the porous substrate 1.
[0037] Next, a working electrode 4 was formed on the flow path pattern 3 formed above by screen printing, an inkjet device, a dispenser, or the like.
[0038] 1A, an Ag / AgCl electrode was printed by screen printing on the flow path pattern 3 as the base electrode 5 of the working electrode. Next, an intermediate layer of NaCl (not shown) was formed on the base electrode 5 by an inkjet method, and then an ion selective membrane 6 having selectivity for the target ion was laminated thereon to form a solid contact type ion selective electrode as the working electrode 4. In this example, the ion selective electrode was formed using Na ions as the target ion.
[0039] The base electrode 5 may be an electrode using known materials such as Ag / AgCl, carbon, and PEDOT / PSS, without any particular limitation. For the preparation of an electrode using Ag / AgCl or carbon, refer to, for example, Patent Document 1. For the preparation of an electrode using PEDOT / PSS, refer to, for example, Non-Patent Document 1. For the base electrode, an electrode suited to the required characteristics of the device, such as cost and performance, may be selected. In this embodiment, an Ag / AgCl electrode was used as the base electrode 5.
[0040] The intermediate layer may be made of any commonly used electrolyte, such as NaCl or KCl, and in this embodiment, was made by applying an aqueous NaCl solution by the inkjet method.
[0041] The ion selective membrane 6 may be any commonly used membrane, as long as it has sensitivity to the target ions and sufficient selectivity to interfering ions.
[0042] The material used for the ion-selective membrane may be any commonly used material. The ion-selective membrane preferably contains an ionophore and an anion remover that exhibit ion selectivity. An example of the ionophore is 12-crown 4-ether having a crown ether structure, and an example of the anion remover is sodium tetraphenylborate (NaTPB). The above materials were used in this embodiment. Any known material can be used for the ion-selective membrane, and for such materials, see pages 138 to 140 of "I want to measure ion concentration with an electrode" by Dojindo Laboratories, Ltd.
[0043] In addition, in order to maintain the structure of the ion selective membrane, a polymeric agent is included in the ion selective membrane. Examples of the polymeric agent include polyvinyl chloride (abbreviated as PVC) and a copolymer of vinyl chloride and vinyl acetate. In this embodiment, polyvinyl chloride is used.
[0044] The ion selective membrane also contains a plasticizer 7 to make the ionophore operable. Although known plasticizers can be used as the plasticizer 7, lipophilic ion exchange materials that act as lipophilic ion exchangers in the ion selective membrane are more preferable. Examples of known materials include 2-nitrophenyl octyl ether (abbreviation: NPOE), bis(2-ethylhexyl) sebacate (abbreviation: DOS), bis(2-ethylhexyl) adipate (abbreviation: DOA), and di-n-octylphenylphosphonate (abbreviation: DOPP). In this embodiment, DOS was used as the plasticizer 7.
[0045] The above-mentioned components are mixed in appropriate amounts, dissolved or dispersed in a solvent such as THF or cyclohexanone, and the resulting liquid is applied by an inkjet method onto a base electrode (Ag / AgCl electrode) having an intermediate layer of NaCl or the like laminated thereon, thereby producing the ion-selective membrane 6.
[0046] The method for applying the ion selective membrane 6 is not limited to the inkjet method, and a dispenser, screen printing, etc. may be used as appropriate. The ion selective membrane 6 may be laminated on the base electrode 5 after adjusting the viscosity of the solution according to each application method.
[0047] In this embodiment, the configuration and manufacturing method of the working electrode according to the present invention have been described, but in order to measure the electrolyte of a sample, a reference electrode 9 may be provided in addition to the working electrode 4, as shown in Fig. 3, and a configuration in which the measurement is performed using the potential difference between the two electrodes may be used. In this figure, the reference electrode is shown as being composed of only an electrode. The configuration and manufacturing method of the reference electrode are not described here because they can be publicly known.
[0048] Next, a method for measuring the electrolyte concentration of a sample using the analytical device of the present invention will be described. In this example, in order to focus only on the performance of the working electrode, as shown in FIG. 4A, a commercially available reference electrode 10 was placed on one side of the main analytical device where the reference electrode was formed, and the reference electrode 10 and the working electrode 4 were connected with a sample, and the potential difference between the two electrodes was measured.
[0049] In this embodiment, a sample was dispensed onto the surface of the working electrode 4, and measurement was performed. As shown in Figures 4A and 4B, the sample 11 is dispensed onto the surface of the ion selective membrane 6 in the first flow channel chamber 3a, and then flows by capillary action, passes through a flow channel connecting the first flow channel chamber 3a and the second flow channel chamber 3b, and reaches the reference electrode portion of the second flow channel chamber 3b. As a result, the reference electrode 10 and the working electrode 4 are electrically connected by the sample 11, and the potential difference is measured.
[0050] In this embodiment, the Na concentration of the sample 11 to be dispensed is set to 10 -5 Measurements were carried out while varying the concentration from 0.5 mol / L to 1 mol / L, and the potential difference between the reference electrode 10 and the working electrode 4 was plotted, and the slope was calculated as the sensitivity.
[0051] Next, a method for evaluating the long-term storage performance of an analytical device will be described. In this example, as an accelerated test for long-term storage, the analytical device was stored in a thermo-hygrostat at 55° C. and 30% for three months, and the change in sensitivity to Na ions before and after storage was evaluated.
[0052] The evaluation results of the accelerated test are as follows: When the absolute value of the rate of change in sensitivity before and after storage was less than 1%, it was rated as "good", when it was 1% or more but less than 2%, it was rated as "passable", and when it was 2% or less, it was rated as "unacceptable". The absolute value of the rate of change in sensitivity was calculated using the following formula (1). 100 × |Sensitivity after storage - Sensitivity before storage| / Sensitivity before storage Formula (1)
[0053] Moreover, as a comparative example for comparing the effects of this embodiment, a similar evaluation was performed using the analysis device 200 having the configuration shown in Figs. 5A and 5B. The structure of the analytical device 200 of the comparative example is the same as that of Example 1, except that it does not have the protective layer 8. The evaluation results are shown in Table 1.
[0054] When the analytical device 200 of the comparative example was used, the sensitivity increased significantly after storage, but when the analytical device 100 of the first example was used, it was found that the change in sensitivity was suppressed.
[0055] In the analytical device of Example 1, the protective layer 8 is disposed inside the porous substrate 1 on the back surface of the portion where the ion selective membrane 6 is formed, so that it is possible to reduce the portion where the ion selective membrane 6 and the porous substrate 1 are in direct contact with each other. In addition, since the inside of the porous substrate 1 is filled and sealed with the protective layer 8, it acts to suppress the plasticizer 7 in the ion selective membrane 6 from seeping out and diffusing into the porous substrate 1 through the voids in the porous substrate 1 or the fibers that constitute the porous substrate 1.
[0056] The contact angle of the protective layer of this example with water was measured using a contact angle meter (DropMaster, manufactured by Kyowa Interface Science Co., Ltd.). The results are shown in Table 1.
[0057] The contact angle of water of the protective layer 8 of the analytical device 100 of Example 1 was increased compared to the analytical device 200 without a protective layer of the comparative example. The surface free energy of the protective layer 8 portion was reduced, which acted to reduce the wettability of the plasticizer 7 to the porous substrate 1, and therefore the penetration of the plasticizer 7 into the porous substrate 1 in the protective layer 8 portion was reduced.
[0058] [Example 2] In this embodiment, instead of the flow path wall forming particles used in Example 1, a polyimide resin was filled inside and around the ion selective membrane of the porous substrate to form a protective layer.
[0059] In this embodiment, as shown in Figures 6A and 6B, a flow path pattern 3 was formed on a porous substrate 1 in the same manner as in Example 1, and then a base electrode 5, an intermediate layer, and an ion selective membrane 6 were formed. Then, a polyimide varnish (KPI-MX300F manufactured by Kawamura Sangyo Co., Ltd. dissolved in methyl ethyl ketone) was drawn by an inkjet method on the back surface (position indicated by diagonal lines in Figure 6B) of the porous substrate 1 on which the ion selective membrane 6 was arranged, and dried at 150 ° C. to form a polyimide film inside the porous substrate 1 on which the porous ion selective membrane 6 was arranged and in the vicinity thereof, which was used as a protective layer 8. The evaluation results of this embodiment are shown in Table 1.
[0060] [Example 3] In this example, instead of the polyimide used in Example 2, a fluororesin was filled in the vicinity of the ion selective membrane of the porous substrate to form a protective layer.
[0061] In this example, as shown in Figures 7A and 7B, a flow path pattern 3, a base electrode 5, an intermediate layer, and an ion selective membrane 6 were formed on a porous substrate 1 in the same manner as in Example 2. Thereafter, a fluororesin (SF Coat: SFE-B002H manufactured by AGC Seimi Chemical Co., Ltd.) was drawn by an inkjet method at the position of the porous substrate on which the ion selective membrane 6 was arranged, that is, the vicinity of the ion selective membrane 6 of the porous substrate 1, and naturally dried at room temperature to form a fluoropolymer membrane, which was used as a protective layer 8. The evaluation results of this example are shown in Table 1.
[0062] [Example 4] In this example, instead of the polyimide used in Example 2, a fluororesin was filled into the inside of the porous substrate where the ion selective membrane was disposed and in the vicinity thereof to form a protective layer.
[0063] In this example, as shown in Figures 6A and 6B, a flow path pattern 3, a base electrode 5, an intermediate layer, and an ion selective membrane 6 were formed on a porous substrate 1 in the same manner as in Example 2. Thereafter, a fluororesin (Somaflon AF manufactured by Somar) was drawn by an inkjet method at the position indicated by the hatched lines in Figure 6B of the porous substrate 1 on which the ion selective membrane 6 was arranged, and the resulting material was naturally dried at room temperature to form a fluoropolymer membrane, which was used as a protective layer. The evaluation results of this example are shown in Table 1.
[0064] [Example 5] This embodiment differs from Example 4 in the arrangement of the protective layer, in that the protective layer is formed by filling a fluorine-based resin inside the porous substrate where the ion selective membrane is arranged.
[0065] In this example, as shown in Figures 8A and 8B, a flow path pattern 3, a base electrode 5, an intermediate layer, and an ion selective membrane 6 were formed on a porous substrate 1 in the same manner as in Example 2. Thereafter, a fluororesin (Somaflon AF manufactured by Somar) was drawn by an inkjet method at the position of the porous substrate 1 where the ion selective membrane 6 was arranged, which is indicated by hatching in Figure 8B, and naturally dried at room temperature to form a fluoropolymer membrane as a protective layer, which was used as the protective layer.
[0066] In this example, as shown in Figures 9A and 9B, a sample was dispensed onto the surface of the flow path between the working electrode and the reference electrode, and measurements were performed. After the sample 11 was dispensed into the flow path connecting the first flow path chamber 3a and the second flow path chamber 3b, it flowed due to capillary action and reached the side of the working electrode 4 in the first flow path chamber 3a and the reference electrode in the second flow path chamber 3b. As a result, the commercially available reference electrode 10 and the working electrode 4 were connected by the sample 11, and the potential difference was measured. The evaluation results of this example are shown in Table 1.
[0067] [Table 1]
[0068] Each embodiment will be explained with reference to Table 1. In comparison with the comparative example in which there was no protective layer in the vicinity of the ion selective membrane, the contact angle of the protective layer was higher than the contact angle of the porous substrate in all the examples, which shows that the contact angle of the protective layer increased and the surface free energy decreased.
[0069] In addition, in Example 3, since no protective layer is provided on the back surface of the ion selective membrane, which is the contact portion between the ion selective membrane and the porous substrate, the degree of diffusion of the plasticizer into the porous substrate increases, and the rate of change in sensitivity is larger than in Examples 2 and 4. However, it can be seen that the effect of suppressing the outflow of the plasticizer from the ion selective membrane can be obtained if a protective layer is provided at least in the vicinity thereof. Therefore, the arrangement of the protective layer is not limited to the position shown in this example, and it may be in a nearby area such as the periphery or back surface of the ion selective membrane.
[0070] With regard to the adjacent region, it is more preferable to place a protective layer at the contact area between the ion selective membrane and the porous substrate, since by placing the protective layer so as to further reduce the contact area between the ion selective membrane and the porous substrate, it is possible to prevent the plasticizer that has flowed out from the ion selective membrane from penetrating and diffusing into the porous substrate due to capillary action.
[0071] In addition, the material of the protective layer is not limited to the material shown in this embodiment, and known materials can be used. By disposing the protective layer, the pores in the porous substrate are sealed, and the contact angle of the porous substrate is increased, and the surface free energy is reduced, so that the penetration of the plasticizer can be further suppressed, which is preferable. The contact angle of the protective layer is preferably higher than the contact angle of the porous substrate 1, and more specifically, from the viewpoint of reducing the surface free energy, it is preferably 80° or more, and more preferably 100° or more.
[0072] In addition, there is no particular regulation regarding the thickness of the protective layer, but when the protective layer is disposed around the ion selective membrane in the vicinity thereof as in Example 4, it is more preferable to set the thickness of the protective layer so that the height of the protective layer is lower than the height of the ion selective membrane in order to facilitate connection of the measurement sample between the ion selective membrane and the flow path during measurement. However, the ion selective membrane does not necessarily have to be on the surface of the porous substrate, and may be disposed inside the porous substrate as shown in FIG. 10, with the protective layer disposed around it. In such a case, the width of the surrounding protective layer is preferably 1 mm or less in order to facilitate connection of the measurement sample between the ion selective membrane and the flow path.
[0073] The embodiments of the present invention include the following configurations. [Configuration 1] porous substrate, an electrode formed within, on, or from within and onto the surface of the porous substrate; an ion-selective membrane covering the electrode; and protective layer, the ion selective membrane comprises a plasticizer; The protective layer is formed inside the porous substrate in close proximity to at least a portion of the ion selective membrane and contains a component that inhibits the penetration of the plasticizer. Analysis devices. [Configuration 2] A flow path region surrounded by a flow path wall formed inside the porous substrate. 2. The analytical device according to configuration 1. [Configuration 3] The electrodes, the ion selective membrane, and the protective layer are formed in the flow path region. An analytical device according to configuration 1 or 2. [Configuration 4] The plasticizer is a lipophilic ion exchange material. An analytical device according to any one of configurations 1 to 3. [Configuration 5] The protective layer contains at least a resin. An analytical device according to any one of configurations 1 to 4. [Configuration 6] The protective layer is made of a material with which the plasticizer is incompatible. An analytical device according to any one of configurations 1 to 5. [Configuration 7] The protective layer contains at least a fluorine-based resin. 7. An analytical device according to any one of configurations 1 to 6. [Configuration 8] The contact angle of the protective layer is higher than the contact angle of the porous substrate. 10. An analytical device according to any one of configurations 1 to 9. [Explanation of symbols]
[0074] 1 Porous base material 2 Channel Wall 3 Flow path area (flow path pattern) 4 Working electrode 5 Base Electrode 6. Ion-selective membranes 7 Plasticizers 8 Protective layer 9 Reference electrode 10. Commercially available reference electrodes 11 Samples 100 Analytical Devices
Claims
1. porous substrate, an electrode formed within, on, or from within and onto the surface of the porous substrate; an ion-selective membrane covering the electrode; and protective layer, the ion selective membrane comprises a plasticizer; The protective layer is formed inside the porous substrate in close proximity to at least a portion of the ion selective membrane and contains a component that inhibits the penetration of the plasticizer. Analysis devices.
2. A flow path region surrounded by a flow path wall formed inside the porous substrate. The analytical device according to claim 1 .
3. The electrodes, the ion selective membrane, and the protective layer are formed in the flow path region. The analytical device according to claim 2 .
4. The plasticizer is a lipophilic ion exchange material. The analytical device according to claim 1 or 2.
5. The protective layer contains at least a resin. The analytical device according to claim 1 or 2.
6. The protective layer is made of a material with which the plasticizer is incompatible. The analytical device according to claim 1 or 2.
7. The protective layer contains at least a fluorine-based resin. The analytical device according to claim 1 or 2.
8. The contact angle of the protective layer is higher than the contact angle of the porous substrate. The analytical device according to claim 1 or 2.
Citation Information
Patent Citations
Paper-Based Reference Electrode And Potentiometric Ion Sensing
US20160033438A1