Foam lightweight structure of light diffusion plate and method for manufacturing the same
A multi-layered foamed structure with varying cell sizes and thicknesses addresses the limitations of existing light diffusing plates, enhancing transmittance and haze while reducing weight and cost.
Patent Information
- Application Number
- JP2024068420
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-09
- Filing Date
- 2024-04-19
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2044-04-19
AI Technical Summary
Existing foamed light diffusing plates face challenges in achieving both high light transmittance and haze levels due to limitations in thickness, density, and bubble size, which affect brightness and diffusion efficiency, failing to meet industry standards of 90-94% diffusion rate.
A multi-layer coextrusion molding technology is employed to create a foamed lightweight structure with varying cell sizes and thicknesses in multiple layers, combining a thin first layer with small cells for diffusion and a thicker second layer with larger cells for transmittance, reducing density while maintaining performance.
The solution achieves light transmittance between 40-60% and haze between 92-96%, significantly reducing weight by over 50% compared to conventional methods, while maintaining competitive performance.
Smart Images

Figure 2024163033000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a light diffusion plate, and more particularly to a lightweight foam structure for a light diffusion plate and a method for producing the same. [Background technology]
[0002] Light diffusers are chemically or physically used to detect the physical phenomena of refraction, reflection, and scattering when light encounters two media with different refractive indices (densities) during its travel. By adding inorganic or organic light diffusing agents to the substrate such as PMMA, PC, PS, PP, HIPS, or by artificially adjusting the light through the array arrangement of micro-feature structures on the substrate surface, the light is refracted, reflected, and scattered in different directions, thus changing the light travel path and achieving the effect of sufficient color dispersion and optical diffusion of the incident light. Light diffusers are widely used in LCD displays, LED lighting, and imaging display systems, and their main function is to sufficiently scatter the incident light and achieve a softer and more uniform illumination effect. Summary of the Invention [Problem to be solved by the invention]
[0003] In the currently disclosed patents and technologies for foam light diffusion plates, air bubbles are used as a medium for light diffusion, and the haze is increased to improve the light diffusion efficiency, but the size of the pores of one type of air bubble and the thickness of the plate material are limited, which affects the light transmittance and haze. When the thickness remains unchanged, two types of situations occur when the density is reduced. 1. The number of bubbles increases and the bubbles become smaller. 2. The number of bubbles remains the same, but the bubbles become larger. As is well known, as the number of bubbles increases and the bubbles become smaller, the light undergoes more refraction when passing through these bubbles, reducing the light transmittance and ultimately the brightness of the display. If the thickness remains the same and the bubbles become larger and the weight becomes lighter, the light transmittance increases, but the light haze decreases, and the diffusion rate also does not meet the requirement (90-94%). The density of these light diffusion foam boards that are currently being mass-produced is 0.8-0.85g / cm. 3 The density was only in the range of 0.8g / cm3, and the light transmittance was only in the range of 40-50%. 3 Anything lower would result in a light transmittance of less than 40% or a haze of less than 90%, which is not up to the standards currently required in the industry.
[0004] As rising raw material prices put pressure on product profit margins, there was a pressing need to find a solution to the problem of how to reduce product costs while still ensuring light transmittance and light diffusion performance.
[0005] Moving beyond the conventional known technology, in order to further solve the foam lightweight structure of the light diffusion plate, a different technology of multi-layer co-extrusion molding technology and bubble structure layer is adopted to realize a new technical method that can control the light transmittance and light diffusion haze.
[0006] Therefore, the present inventors believed that the above-mentioned drawbacks could be improved, and as a result of extensive research, they came to propose the present invention, which effectively improves the above-mentioned problems through rational design.
[0007] The present invention has been made by the inventors through intensive research in view of the above problems, and its purpose is to provide a foamed lightweight structure of a light diffusion plate and a manufacturing method thereof. That is, in order to reduce the cost of the light diffusion sheet, it is necessary to increase the number of bubbles through which light passes and reduce light scattering and loss. It has been proved through testing that, in a situation where the thickness does not change, when the density decreases and the bubbles become larger, the number of bubbles decreases, the light transmittance increases, but the haze decreases. In a situation where the thickness does not change, the density decreases and the bubbles become smaller, the number of bubbles increases, the light transmittance decreases, but the haze increases. In these two situations, the change in light diffusion or haze is disadvantageous to meet the requirements of the light diffusion plate industry, but is advantageous to reduce the weight of the foamed light diffusion plate that has already been industrialized. Therefore, the present invention combines one or more thin layers of fine bubble foaming on the above basis to form excellent light diffusion and suitable light transmittance, and effectively reduce the weight of the light diffusion plate. [Means for solving the problem]
[0008] In order to solve the above problems, the foamed lightweight structure of the light diffusion plate according to one embodiment of the present invention includes an upper surface layer, a first foam layer, a second foam layer, and a lower surface layer, which are successively connected to each other, and the thickness of the first foam layer is thinner than that of the second foam layer, and the average diameter of the bubbles in the first foam layer is smaller than that of the second foam layer. The upper surface layer and the lower surface layer together act to protect the first and second foam layers from the protective layer. The first foam layer is used to increase the diffusion of light, and the second foam layer is used to increase the transmittance of light and to reduce the average density of the light diffusion plate.
[0009] In the light-weight foamed structure of the light-diffusing plate according to the present invention, the total thickness of the light-diffusing plate is in the range of 1 to 5 mm, and the average density is 0.3 to 0.85 g / cm. 3 The range is between .
[0010] In addition, the lightweight foam structure of the light diffusion plate according to the present invention further comprises the first foam layer between the second foam layer and the lower surface layer.
[0011] In addition, the lightweight foam structure of the light diffusion plate according to the present invention further comprises the second foam layer between the upper surface layer and the first foam layer.
[0012] In the lightweight foamed structure of the light diffusion plate according to the present invention, the upper surface layer and the lower surface layer each have a thickness ranging from 0.01 to 0.05 mm. The first foamed layer has a thickness ranging from 0.2 to 1 mm, and the average diameter of the bubbles in the first foamed layer is between 0.03 and 0.08 mm. The second foamed layer has a thickness ranging from 0.78 to 3.9 mm, and the average diameter of the bubbles in the second foamed layer is between 0.3 and 0.8 mm.
[0013] In the lightweight foam structure of the light diffusion plate according to the present invention, the upper surface layer and the lower surface layer each have a thickness ranging from 0.01 to 0.05 mm. The first foam layer has a thickness ranging from 0.1 to 0.5 mm, and the average diameter of the bubbles in the first foam layer is between 0.03 and 0.08 mm. The second foam layer has a thickness ranging from 0.78 to 3.9 mm, and the average diameter of the bubbles in the second foam layer is between 0.3 and 0.8 mm.
[0014] In the lightweight foam structure of the light diffusion plate according to the present invention, the upper surface layer and the lower surface layer each have a thickness ranging from 0.01 to 0.05 mm. The first foam layer has a thickness ranging from 0.2 to 1 mm, and the average diameter of the bubbles in the first foam layer is between 0.03 and 0.08 mm. The second foam layer has a thickness ranging from 0.39 to 1.95 mm, and the average diameter of the bubbles in the second foam layer is between 0.3 and 0.8 mm.
[0015] In addition, in the foamed lightweight structure of the light diffusion plate according to the present invention, the first foamed layer can be replaced with a light diffusion agent. The light diffusion agent is an inorganic light diffusion agent and / or an organic light diffusion agent, and the inorganic light diffusion agent includes nano-barium sulfate, calcium carbonate, silicon dioxide, etc., and the organic light diffusion agent includes acrylic type, styrene monomer type, acrylic resin type, organosilicon particles, etc.
[0016] In order to achieve the above object, the method for manufacturing a foamed light diffusion plate according to another embodiment of the present invention manufactures a four-layer or five-layer light diffusion plate by combining a distributor with a screw extruder or by an in-mold composite method, and the light diffusion plate has an upper surface layer, a first foam layer, a second foam layer, and a lower surface layer, which are connected in sequence. The raw material composition of the first foam layer and the second foam layer includes a high polymer transparent material and a foaming agent. The high polymer transparent material is any one selected from polystyrene, polypropylene, polycarbonate, and polyethylene terephthalate, and when the high polymer transparent material is polystyrene, the raw material composition further includes a reinforcing agent or a transparent thermoplastic elastomer. When the high polymer transparent material is polycarbonate, the raw material composition further includes a reinforcing agent, and the addition ratio of the reinforcing agent is in the range of 1 to 20 wt% of the raw material composition.
[0017] In addition, in the manufacturing method of the foamed lightweight structure of the light diffusion plate according to the present invention, the first foamed layer adopts expandable microspheres or a foaming agent, and the foaming agent is an endothermic or / and heat-dissipating foaming agent having a pore size after foaming in the range of 0.003-0.005 mm, and the amount of the foaming agent is in the range of 0.5-2 wt% of the raw material composition of the first foamed layer. The second foamed layer adopts an endothermic or / and heat-dissipating foaming agent having a particle size in the range of 0.050-0.090 mm, and the amount of the foaming agent is in the range of 0.7-6 wt% of the raw material composition of the second foamed layer. The back pressure of the mold of the in-mold composite method is in the range of 2-25 MPa, and the temperature of the mold is in the range of 160-230°C. [Brief description of the drawings]
[0018] [Figure 1] 1 is a schematic diagram showing a lightweight foam structure of a light diffusion plate according to a first embodiment of the present invention. [Diagram 2] FIG. 5 is a schematic diagram showing the configuration of a lightweight foam structure of a light diffusion plate according to a second embodiment of the present invention. [Diagram 3] FIG. 11 is a schematic diagram showing the configuration of a lightweight foam structure of a light diffusion plate according to a third embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] Hereinafter, the embodiments of the present invention will be described in detail. However, the present invention is not limited to these, and various modifications are possible within the scope of the description. The technical scope of the present invention also includes embodiments obtained by appropriately combining the technical means disclosed in the different embodiments.
[0020] (First embodiment) FIG. 1 is a schematic diagram showing a foamed lightweight structure of a light diffusion plate according to a first embodiment of the present invention. The structure includes an upper surface layer 1, a first foamed layer 2, a second foamed layer 3, and a lower surface layer 4, which are successively connected to each other. The thickness of the first foamed layer 2 is thinner than that of the second foamed layer 3, and the diameter of the bubbles in the first foamed layer 2 is smaller than that of the second foamed layer 3. Both the upper surface layer and the lower surface layer generate a protective effect from the protective layer to the core layer (the core layer is a structural layer between the upper surface layer 1 and the lower surface layer 4, which is the first foamed layer 2 and the second foamed layer 3 in the first embodiment). The bubbles in the first foamed layer 2 are used to increase the diffusion of light, and the bubbles in the second foamed layer 3 are used to increase the light transmittance and to reduce the average density of the foamed light diffusion plate.
[0021] In the first embodiment, the light diffusion plate has one first foam layer 2 between two upper and lower surface layers, and one second foam layer 3 is added to form a four-layer structure plate material of the core layer. More specifically, the total thickness of the foam light diffusion plate of the first embodiment is in the range of 1 to 5 mm, and the thicknesses of the upper surface layer 1 and the lower surface layer 4 are both in the range of 0.01 to 0.05 mm. The thickness of the first foam layer 2 is in the range of 0.2 to 1 mm, and the average diameter of the bubbles is in the range of 0.03 to 0.08 mm. The thickness of the second foam layer 3 is in the range of 0.78 to 3.9 mm, and the average diameter of the bubbles is in the range of 0.3 to 0.8 mm.
[0022] The average density of the light diffusion plate according to the first embodiment is 0.3 to 0.85 g / cm 3The thickness can be controlled within a range between 100% and 40%, the light transmittance can be controlled within a range between 40% and 60%, and the haze can be controlled within a range between 92% and 96%. To be more specific, the average density, light transmittance, and haze of the light diffusion plate can be adjusted by adjusting the thickness or the diameter of the bubbles of the first foamed layer 2 and the second foamed layer 3, respectively, to obtain a required light diffusion plate. Table 1 shows the relationship between different thicknesses, average density, haze, and light transmittance of the light diffusion plate according to the first embodiment.
[0023] TIFF2024163033000002.tif93146
[0024] (Second Example) FIG. 2 is a schematic diagram showing a foamed lightweight structure of a light diffusion plate according to a second embodiment of the present invention. In the second embodiment, the light diffusion plate has a four-layer structure modified to a five-layer structure, with three foam layers between the upper surface layer 1 and the lower surface layer 4, and the core layer has a two-layer structure in which one second foam layer 3 is laminated on one original first foam layer 2, forming a three-layer structure of the first foam layer 2-second foam layer 3-first foam layer 2. More specifically, the total thickness of the light diffusion plate according to the second embodiment is in the range of 1 to 5 mm, and the thicknesses of both the upper surface layer 1 and the lower surface layer 4 are in the range of 0.01 to 0.05 mm. The thickness of the first foam layer 2 is in the range of 0.1 to 0.5 mm, and the average diameter of the bubbles is in the range of 0.03 to 0.08 mm. The thickness of the second foam layer 3 is in the range of 0.78 to 3.9 mm, and the average diameter of the bubbles is in the range of 0.3 to 0.8 mm.
[0025] The average density of the light diffusion plate according to the second embodiment is 0.3 to 0.85 g / cm 3The thickness can be controlled within a range between 40% and 60%, the light transmittance can be controlled within a range between 40% and 60%, and the haze can be controlled within a range between 92% and 96%. To be more specific, the average density, light transmittance, and haze of the light diffusion plate can be adjusted by adjusting the thickness or the diameter of the bubbles of the first foamed layer 2 and the second foamed layer 3, respectively, to obtain a desired diffusion plate. Table 2 shows the relationship between different thicknesses, average density, haze, and light transmittance of the light diffusion plate according to the second embodiment.
[0026] <Table 2: Haze and light transmittance of light diffusion plates having different total thicknesses and average densities according to Example 2> TIFF2024163033000003.tif88138
[0027] (Third Example) FIG. 3 is a schematic diagram showing a foamed lightweight structure of a light diffusion plate according to a second embodiment of the present invention. In the third embodiment, the light diffusion plate has a four-layer structure modified to a five-layer structure, with three foam layers between two upper and lower surface layers, and the core layer has a two-layer structure in which one second foam layer 3 is laminated on one original first foam layer 2, and a three-layer structure of the second foam layer 3-first foam layer 2-second foam layer 3 is formed. More specifically, the total thickness of the light diffusion plate according to the third embodiment is in the range of 1 to 5 mm, and the thicknesses of both the upper surface layer 1 and the lower surface layer 4 are in the range of 0.01 to 0.05 mm. The thickness of the first foam layer 2 is in the range of 0.2 to 1 mm, and the average diameter of the bubbles is in the range of 0.03 to 0.08 mm. The thickness of the second foam layer 3 is in the range of 0.39 to 1.95 mm, and the average diameter of the bubbles is in the range of 0.3 to 0.8 mm.
[0028] The average density of the light diffusion plate according to the third embodiment is 0.3 to 0.85 g / cm 3The thickness can be controlled within a range between 40% and 60%, the light transmittance can be controlled within a range between 40% and 60%, and the haze can be controlled within a range between 92% and 96%. To be more specific, the average density, light transmittance, and haze of the light diffusion plate can be adjusted by adjusting the thickness or the diameter of the bubbles of the first foamed layer 2 and the second foamed layer 3, respectively, to obtain a required foamed light diffusion plate. Table 3 shows the relationship between different thicknesses, average density, haze, and light transmittance of the light diffusion plate according to the third embodiment.
[0029] <Table 3: Haze and light transmittance of light diffusion plates having different total thicknesses and average densities according to the present embodiment> TIFF2024163033000004.tif88138
[0030] The present invention further provides a method for manufacturing a foamed lightweight structure for a light diffusion plate, which manufactures a light diffusion plate with a four-layer or five-layer structure by combining a distributor with a screw extruder or by an in-mold compounding method. The four-layer light diffusion plate is successively connected to an upper surface layer 1, a first foam layer 2, a second foam layer 3, and a lower surface layer 4. The five-layer light diffusion plate is successively connected to an upper surface layer 1, a first foam layer 2, a second foam layer 3, a first foam layer 2, and a lower surface layer 4, or successively connected to an upper surface layer 1, a second foam layer 3, a first foam layer 2, a second foam layer 3, and a lower surface layer 4.
[0031] The surface layer of the light diffusion plate adopts materials and techniques common in this field, and the raw material composition of the foam layer includes a high polymer transparent material and a foaming agent. The high polymer transparent material is any one of polystyrene (PS), polypropylene (PP), polycarbonate (PC), or polyethylene terephthalate (PET). When the high polymer transparent material is polystyrene, the raw material composition further includes a reinforcing agent SEBS, transparent TPE, or TPR. When the high polymer transparent material is polycarbonate, the raw material composition further includes a reinforcing agent MBS. When the high polymer transparent material is polypropylene or polyethylene terephthalate, it is not necessary to add a reinforcing agent. When the raw material composition of the first foam layer 2 and the second foam layer 3 includes a reinforcing agent, the addition ratio of the reinforcing agent is in the range of 1 to 20 wt% of the raw material composition.
[0032] When the first foam layer 2 employs an expandable microsphere foaming agent or an endothermic and / or exothermic foaming agent with a particle size ranging from 0.003 to 0.005 mm, the dosage of the foaming agent ranges from 0.5 to 2 wt% of the raw material of the first foam layer 2. When the first foam layer 2 employs an expandable microsphere foaming agent, it is not necessary to combine it with a nucleating agent separately. When the first foam layer 2 employs an endothermic and / or exothermic foaming agent, a nucleating agent is further combined to induce the formation of a micropore structure with a pore size of less than 0.08 mm and control the pore size of the bubbles. The aforementioned nucleating agent is calcium carbonate or silicon dioxide, and the dosage of the nucleating agent ranges from 0.1 to 3 wt% of the raw material of the first foam layer 2.
[0033] The second foam layer 3 adopts endothermic and / or exothermic foaming agents with particle sizes ranging from 0.05 to 0.09 mm, and the dosage of the foaming agent ranges from 0.7 to 6 wt% of the raw materials of the second foam layer 3. The pore size reaches a range of 0.3 to 0.8 mm, and no nucleating agent can be used in the second foam layer 3 to prevent the pore size from becoming small.
[0034] The endothermic blowing agent is sodium bicarbonate, and the exothermic blowing agent is azodicarbonamide.
[0035] The back pressure of the in-mold composite die is in the range of 2-25 MPa, and the temperature of the die is in the range of 160-230°C. Different pressures cause different speeds of pressure drop, and the higher the pressure, the faster the pressure drop, resulting in smaller bubble size, so that the difference in pressure can be used to adjust the bubble size. When the die temperature is in the range of 160-230°C, suitable viscoelasticity is formed during processing of the material, and the desired bubble pore size can be obtained by combining the die pressure drop.
[0036] Three screw extruders are used as hosts, with No. 3 corresponding to the second foamed layer 3, No. 1 corresponding to the upper surface layer 1 and the lower surface layer 4, and No. 2 corresponding to the first foamed layer 2. The layers are compounded by one distributor, and the materials with different pore sizes extruded by the three screw extruders and the non-foamed surface layer obtain three types of structure layers, which are pressed by a flat die to form light diffusion plate layers with three types of structures as shown in Figures 1, 2, and 3. Each of the three screw extruders includes seven heating areas, namely, a first area, a second area, a third area, a fourth area, a fifth area, a sixth area, and a seventh area, from the feed end to the discharge end, in which the heating temperature of the first area is in the range of 150 to 160°C, the heating temperature of the second area is in the range of 160 to 170°C, the heating temperature of the third area is in the range of 180 to 190°C, the heating temperature of the fourth area is in the range of 190 to 205°C, the heating temperature of the fifth area is in the range of 190 to 170°C, the heating temperature of the sixth area is in the range of 160 to 170°C, and the heating temperature of the seventh area is in the range of 150 to 160°C. The heating temperature of the filter area ranges between 150-160°C, the heating temperature of the distributor ranges between 150-160°C, and the heating temperature of the die head device ranges between 150-200°C (PC material is heated an additional 30°C on this basis).
[0037] In the embodiment of the present invention, the raw material of the foam layer is polystyrene and a reinforcing agent SEBS, and the adding ratio of the reinforcing agent is in the range of 1-20 wt% of the raw material. The first foam layer 2 is made of an endothermic foaming agent sodium bicarbonate with a particle size of 0.003-0.005 mm, and the amount of the foaming agent is in the range of 0.5-2 wt% of the raw material of this layer, and a nucleating agent of silicon dioxide is used to induce the formation of a micropore structure with a pore size of less than 0.080 mm and control the pore size of the air bubbles, and the amount of the nucleating agent is in the range of 0.1-3 wt% of the raw material of the first foam layer. The second foam layer 3 is made of a heat-dissipating foaming agent azodicarbonamide with a particle size of 0.05-0.09 mm, and the amount of the foaming agent is in the range of 0.7-6 wt% of the raw material of the second foam layer 3. The pore diameter reaches 0.3 to 0.8 mm, and in order to prevent the pore diameter from becoming small, the second foam layer 3 cannot use a nucleating agent.
[0038] A method for manufacturing a light diffusion plate according to an embodiment of the present invention includes the following steps. 1. Mix the raw materials for each layer based on the mixing ratio, mix evenly in a mixer, and then store. 2. Select a mold that is compatible with the 5-layer extrusion molding method, install the extrusion head, and check whether the extrusion equipment and each rotating part are complete. 3. Adjust the temperature control table to the operating temperature, heat the cylindrical mold, and maintain the temperature constant for 30 minutes after the temperature reaches the set value. 4. Of the three screw extruders, one corresponds to the upper surface layer 1 and the lower surface layer 4, one corresponds to the first foamed layer 2 connected to the upper surface layer 1 and the lower surface layer 4, and one corresponds to the second foamed layer 3. The mixed materials of each layer after being uniformly mixed are fed into the corresponding feed port. The filters of each extruder are replaced, the metering pumps are started in sequence, the screw motors are rotated, and parameters such as the metering pump pressure, feed speed, and host rotation speed are set. The plastic material is plasticized as it passes through the cylinder and is extruded by the extruder. The die lip is cleaned. The metering pump, main line speed, pressure, and other parameters are adjusted to start extrusion. 5. The materials in the three screw extruders are melted and then extruded into a mold to compound, and the composite plate is extruded from the outlet of the mold to produce a five-layer light diffusion plate sheet material.
[0039] In this embodiment, the upper and lower surface layers are manufactured using materials and means commonly used in the art.
[0040] In this embodiment, the screw extruder for producing the first foam layer 2 includes seven heating areas, namely, the first area, the second area, the third area, the fourth area, the fifth area, the sixth area, and the seventh area, from the feed end to the discharge end, and the heating temperature of the first area is in the range of 150-160°C, the heating temperature of the second area is in the range of 160-170°C, the heating temperature of the third area is in the range of 180-190°C, the heating temperature of the fourth area is in the range of 190-205°C, the heating temperature of the fifth area is in the range of 190-170°C, the heating temperature of the sixth area is in the range of 160-170°C, and the heating temperature of the seventh area is in the range of 150-160°C. The heating temperature of the filter area is in the range of 150-160°C, the heating temperature of the distributor is in the range of 150-160°C, and the heating temperature of the die head device is in the range of 150-200°C. The screw extruder for producing the second foam layer 3 includes seven heating areas, namely, the first area, the second area, the third area, the fourth area, the fifth area, the sixth area, and the seventh area, from the feed end to the discharge end, and the heating temperature of the first area is in the range of 150 to 160 ° C., the heating temperature of the second area is in the range of 160 to 170 ° C., the heating temperature of the third area is in the range of 180 to 190 ° C., the heating temperature of the fourth area is in the range of 190 to 205 ° C., the heating temperature of the fifth area is in the range of 190 to 170 ° C., the heating temperature of the sixth area is in the range of 160 to 170 ° C., and the heating temperature of the seventh area is in the range of 150 to 160 ° C. The heating temperature of the filter area is in the range of 150 to 160 ° C., the heating temperature of the distributor is in the range of 150 to 160 ° C., and the heating temperature of the die head device is in the range of 150 to 200 ° C. The back pressure of the in-mold composite die is in the range of 2-25 MPa, and the temperature of the die is in the range of 160-230° C. When the temperature of the die is in the range of 160-230° C., the material forms suitable viscoelasticity during processing, and the desired pore size of the bubbles can be obtained in combination with the pressure drop of the die.
[0041] In an embodiment of the present invention, the first foam layer 2 can be replaced with a light diffusing agent. The light diffusing agent can be an inorganic light diffusing agent and / or an organic light diffusing agent. The inorganic light diffusing agent includes nano barium sulfate, calcium carbonate, silicon dioxide, etc., and the organic light diffusing agent includes acrylic type, styrene monomer type, acrylic resin type, organosilicon particles, etc.
[0042] Compared with the prior art, the present invention has the following advantages: 1. The present invention improves the structure of the light diffusion plate by combining two types of foam layers, one with a small average bubble diameter and a thin foam layer, and the other with a large average bubble diameter and a thick foam layer, ensuring that the performance of the light diffusion plate reaches the level of the prior art while reducing its density to 0.3g / cm. 3 The conventional technology reduces the density to 0.85 g / cm 3 Compared with the previous year, the reduction is more than 50%, which means a clear reduction in costs and a clear advantage in market competition. 2. The present invention adjusts the average density, light transmittance, and haze of the light diffusion plate by adjusting the thickness of each of the first foamed layer 2 and the second foamed layer 3 or the average diameter of the bubbles thereof, and adjusts the average density of the light diffusion plate to 0.3 to 0.85 g / cm. 3 the light transmittance can be in the range of 40-60%, and the haze can be in the range of 92-96%.
[0043] Although the present invention has been described above using the embodiments, the technical scope of the present invention is not limited to the scope described in the above embodiments. It is clear to those skilled in the art that various modifications and improvements can be made to the above embodiments. It is clear from the description of the claims that such modifications and improvements can also be included in the technical scope of the present invention. [Explanation of symbols]
[0044] 1 Upper surface layer 2 First foam layer 3 Second foam layer 4 Lower surface layer
Claims
1. A foamed lightweight structure of a light diffusion plate, The light diffusion plate includes an upper surface layer, a first foam layer, a second foam layer, and a lower surface layer, which are successively connected to each other; The thickness of the first foam layer is smaller than the thickness of the second foam layer, The average diameter of the bubbles in the first foam layer is smaller than the average diameter of the bubbles in the second foam layer. Lightweight foam structure for light diffusion panels.
2. The total thickness of the light diffusion plate is in the range of 1 to 5 mm, and the average density is 0.3 to 0.85 g / cm 3 2. The light diffusing plate according to claim 1, wherein the foamed lightweight structure is in the range of 0.1 to 1.
0.
3. 3. The foamed lightweight structure of a light diffusion plate according to claim 2, further comprising one layer of the first foamed layer between the second foamed layer and the lower surface layer.
4. 3. The foamed lightweight structure of a light diffusion plate according to claim 2, further comprising one second foamed layer between the upper surface layer and the first foamed layer.
5. The thickness of each of the upper surface layer and the lower surface layer is in the range of 0.01 to 0.05 mm; The thickness of the first foam layer is in the range of 0.2 to 1 mm, and the average diameter of the bubbles in the first foam layer is in the range of 0.03 to 0.08 mm; The foamed lightweight structure of the light diffusion plate according to claim 2, wherein the thickness of the second foamed layer is in the range of 0.78 to 3.9 mm, and the average diameter of the bubbles in the second foamed layer is in the range of 0.3 to 0.8 mm.
6. The thickness of each of the upper surface layer and the lower surface layer is in the range of 0.01 to 0.05 mm; The thickness of the first foam layer is in the range of 0.1 to 0.5 mm, and the average diameter of the bubbles in the first foam layer is in the range of 0.03 to 0.08 mm; The foamed lightweight structure of the light diffusion plate according to claim 3, characterized in that the thickness of the second foamed layer is in the range of 0.78 to 3.9 mm, and the average diameter of the bubbles in the second foamed layer is in the range of 0.3 to 0.8 mm.
7. The thickness of each of the upper surface layer and the lower surface layer is in the range of 0.01 to 0.05 mm; The thickness of the first foam layer is in the range of 0.2 to 1 mm, and the average diameter of the bubbles in the first foam layer is in the range of 0.03 to 0.08 mm; The foamed lightweight structure of the light diffusion plate according to claim 4, characterized in that the thickness of the second foamed layer is in the range of 0.39 to 1.95 mm, and the average diameter of the bubbles in the second foamed layer is in the range of 0.3 to 0.8 mm.
8. 8. The foamed lightweight structure of a light diffusion plate according to claim 1, wherein the first foamed layer is replaceable with a light diffusing agent.
9. A four-layer or five-layer light diffusion plate is manufactured by combining a distributor with a screw extruder or by an in-mold compounding method, and the light diffusion plate includes an upper surface layer, a first foam layer, a second foam layer, and a lower surface layer, which are connected in sequence, The raw material composition of the first foam layer and the second foam layer includes a high polymer transparent material and a foaming agent, The high polymer transparent material is selected from the group consisting of polystyrene, polypropylene, polycarbonate, and polyethylene terephthalate. When the high polymer transparent material is polystyrene, the raw material composition further includes a reinforcing agent or a transparent thermoplastic elastomer; When the high polymer transparent material is polycarbonate, the raw material composition further includes a reinforcing agent, and the addition ratio of the reinforcing agent is in the range of 1 to 20 wt% of the raw material composition; A method for manufacturing a lightweight foam structure for a light diffusion plate.
10. The first foam layer adopts expandable microspheres or foaming agents, and the foaming agents are endothermic and / or exothermic foaming agents with a pore size of 0.003-0.005 mm after foaming, and the amount of the foaming agent is in the range of 0.5-2 wt % of the raw material composition of the first foam layer; The second foam layer employs an endothermic or / and exothermic foaming agent having a particle size ranging from 0.050 to 0.090 mm, and the amount of the foaming agent is in the range of 0.7 to 6 wt % of the raw material composition of the second foam layer; The method for manufacturing a foamed lightweight structure of a light diffusion plate according to claim 9, wherein the back pressure of the in-mold composite mold is in the range of 2 to 25 MPa, and the temperature of the mold is in the range of 160 to 230°C.
Citation Information
Patent Citations
Compound and preparation method thereof, and light conversion device and display device comprising same
CN113980400A
Production process of micro-foaming diffusion plate
CN115061228A
Light-weight foaming structure of light diffusion plate and preparation method of light-weight foaming structure
CN116577856A
Light modulating plate, and backlight assembly and display device having the plate
JP2006128060A
Optical diffusion board
JP2006276838A
Cited By
Display apparatus and method for manufacturing optical member for display apparatus
WO2026225735A1