Semiconductor device

The controlled manufacturing process for oxide semiconductor films in transistors addresses defects and impurities, enhancing electrical performance and reliability by forming insulating films at controlled temperatures and pressures, resulting in improved semiconductor devices.

JP2024164180AActive Publication Date: 2024-11-26SEMICON ENERGY LAB CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2024143975
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2013-03-15
Filing Date
2024-08-26
Publication Date
2024-11-26
Estimated Expiration
2034-01-21

AI Technical Summary

Technical Problem

Oxide semiconductor films in transistors contain high defect levels and impurities, leading to fluctuations in electrical characteristics, increased power consumption, and reduced reliability due to oxygen vacancies and impurities like silicon, carbon, hydrogen, and nitrogen.

Method used

A manufacturing process that forms gate electrodes and insulating films at controlled temperatures (280°C to 400°C) without heat treatment, using plasma CVD to form oxide insulating films with specific gas pressures and power settings, and incorporating silicon oxide or silicon oxynitride films to reduce defects and impurities in the oxide semiconductor film.

Benefits of technology

Reduces defects and impurities in oxide semiconductor films, improving electrical characteristics, reducing power consumption, and enhancing the reliability and stability of semiconductor devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024164180000001_ABST
    Figure 2024164180000001_ABST
Patent Text Reader

Abstract

To reduce a defect of an oxide semiconductor film in a semiconductor device using the oxide semiconductor film, and also to improve electrical characteristics and reliability of the semiconductor device using the oxide semiconductor film.SOLUTION: A manufacture method for a semiconductor device comprises steps of: forming a gate electrode and a gate insulation film on a substrate; forming an oxide semiconductor film on the gate insulation film; forming a pair of electrodes making contact with the oxide semiconductor film; forming a first oxide insulation film on the oxide semiconductor film and the pair of electrodes by a plasma CVD method using a deposition condition at a temperature ranging from 280 to 400°C; and forming a second oxide insulation film on the first oxide insulation film, and then performing heat treatment at a temperature ranging from 150 to 400°C, preferably from 300 to 400°C, or more preferably from 320 to 370°C.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an article, a method, or a manufacturing method. , manufacture, or composition of matter. In particular, The present invention relates to, for example, a semiconductor device, a display device, a light-emitting device, a power storage device, a driving method thereof, or In particular, the present invention relates to a semiconductor having an oxide semiconductor, In particular, the present invention relates to a device, a display device, or a light-emitting device having a transistor, The present invention relates to a semiconductor device and a manufacturing method thereof. [Background technology]

[0002] It is used in many flat panel displays, such as liquid crystal displays and light-emitting displays. The transistors used are made of amorphous silicon and single crystal silicon formed on a glass substrate. The silicon semiconductor is made of silicon semiconductor such as polycrystalline silicon or polysilicon. Transistors using semiconductors are also used in integrated circuits (ICs).

[0003] In recent years, metal oxides that exhibit semiconducting properties have been used in transistors instead of silicon semiconductors. In this specification, the term "oxide" refers to a metal oxide that exhibits semiconductor properties. Let us call them semiconductors.

[0004] For example, a transistor using zinc oxide or an In-Ga-Zn oxide as an oxide semiconductor may be used. A transistor is manufactured and used as a switching element for pixels of a display device. Techniques have been disclosed (see Patent Documents 1 and 2). [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2007-123861 A [Patent Document 2] JP 2007-96055 A Summary of the Invention [Problem to be solved by the invention]

[0006] In a transistor including an oxide semiconductor film, the oxide semiconductor film has a large amount of defects. This leads to poor electrical characteristics of the transistor and also to deterioration over time and stress testing (e.g. For example, in a BT (Bias-Temperature) stress test, This causes an increase in the amount of variation in the electrical characteristics of the capacitor, typically the threshold voltage.

[0007] In addition to defects, impurities contained in the oxide semiconductor film, typically, constituent elements of the insulating film, If there are a lot of impurities such as silicon and carbon, the electrical characteristics of the transistor will be impaired. .

[0008] In view of the above, one embodiment of the present invention is to provide a semiconductor device including an oxide semiconductor film. Another object of the present invention is to reduce defects in a semiconductor film. In a semiconductor device using a conductor film, the impurity concentration of an oxide semiconductor film is reduced. Another object of the present invention is to provide a semiconductor device including an oxide semiconductor film. Another object of the present invention is to improve electrical characteristics of the oxide semiconductor layer. One of the objectives is to improve the reliability of a semiconductor device using a semiconductor film. Another object of one embodiment of the present invention is to provide a semiconductor device or the like having a low off-state current. Another object of one embodiment of the present invention is to provide a semiconductor device or the like with low power consumption. Another embodiment of the present invention provides a display device or the like that can reduce eye fatigue. Another object of one embodiment of the present invention is to provide a semiconductor device using a transparent semiconductor film. Another object of the present invention is to provide a novel semiconductor device, etc. Another object of one embodiment of the present invention is to provide a semiconductor device having excellent characteristics. The objective of the present invention is to provide the above. Note that the description of these objectives does not preclude the existence of other objectives. It is to be noted that one embodiment of the present invention does not necessarily solve all of these problems. Problems other than these will be obvious from the description, drawings, claims, etc. Other issues can be extracted from the description, drawings, claims, etc. It is possible to do so. [Means for solving the problem]

[0009] One aspect of the present invention is to form a gate electrode and a gate insulating film on a substrate, After the oxide semiconductor film is formed, a pair of electrodes in contact with the oxide semiconductor film is formed without performing a heat treatment process. and forming electrodes on the oxide semiconductor film and the pair of electrodes at a temperature of 280° C. or more and 400° C. or less. A first oxide insulating film is formed by a plasma CVD method under the film forming conditions, and the first oxide insulating film is A second oxide insulating film is formed on the insulating film, and the insulating film is heated at a temperature of 150° C. to 400° C., preferably 300° C. A semiconductor device that is subjected to heat treatment at a temperature of 320°C to 370°C or more is preferably used. This is a method for making the device.

[0010] The raw material gas is introduced into the processing chamber to keep the pressure in the processing chamber at 100 Pa or more and 250 Pa or less. The first oxide is formed by supplying high frequency power to an electrode provided in the processing chamber. An insulating film can be formed.

[0011] In addition, the substrate placed in the evacuated processing chamber is kept at a temperature of 180°C or higher and 280°C or lower. The raw material gas is introduced into the processing chamber to set the pressure in the processing chamber to 100 Pa or more and 250 Pa or less. The electrode in the treatment chamber is 0.17 W / cm 2 More than 0.5W / cm 2 High frequency below By supplying power, the second oxide insulating film can be formed.

[0012] The first oxide insulating film and the second oxide insulating film are formed using a deposition gas containing silicon. and forming a silicon oxide film or a silicon oxynitride film by using an oxidizing gas as a raw material gas. do. Effect of the Invention

[0013] According to one embodiment of the present invention, in a semiconductor device including an oxide semiconductor film, In another embodiment of the present invention, a semiconductor device using an oxide semiconductor film can be manufactured by using the oxide semiconductor film. In a semiconductor device or the like, impurities in an oxide semiconductor film can be reduced. According to one embodiment of the present invention, in a semiconductor device including an oxide semiconductor film, electrical characteristics can be improved. According to one embodiment of the present invention, a semiconductor device including an oxide semiconductor film can be According to one embodiment of the present invention, the off-state current can be reduced, and the reliability can be improved. According to one embodiment of the present invention, a semiconductor device or the like having low power consumption can be provided. According to one embodiment of the present invention, a semiconductor device or the like having low eye fatigue can be provided. It is possible to provide a display device or the like capable of reducing the above-mentioned problems. In this way, a semiconductor device using a transparent semiconductor film can be provided. According to one embodiment of the present invention, a novel semiconductor device or the like can be provided. According to the embodiment, a semiconductor device having excellent characteristics can be provided. [Brief description of the drawings]

[0014] [Figure 1] 1A and 1B are a top view and a cross-sectional view illustrating one embodiment of a transistor. [Diagram 2] 1A to 1C are cross-sectional views illustrating one mode of a method for manufacturing a transistor. [Diagram 3] FIG. 1 is a cross-sectional view illustrating one embodiment of a transistor. [Figure 4] FIG. 1 is a cross-sectional view illustrating one embodiment of a transistor. [Diagram 5] FIG. 1 is a cross-sectional view illustrating one embodiment of a transistor. [Figure 6] 1A and 1B are a top view and a cross-sectional view illustrating one embodiment of a transistor. [Figure 7] FIG. 1 illustrates a band structure of a transistor. [Figure 8] 1 is a cross-sectional view illustrating one embodiment of a semiconductor device. [Figure 9] 1A and 1B are a top view and a cross-sectional view illustrating one embodiment of a transistor. [Figure 10] 1A to 1C are cross-sectional views illustrating one mode of a method for manufacturing a transistor. [Figure 11] FIG. 1 is a cross-sectional view illustrating one embodiment of a transistor. [Figure 12] FIG. 1 is a cross-sectional view illustrating one embodiment of a transistor. [Figure 13] 1A and 1B are a top view and a cross-sectional view illustrating one embodiment of a transistor. [Figure 14] 1A and 1B are a top view and a cross-sectional view illustrating one embodiment of a transistor. [Figure 15]1A and 1B are a block diagram and a circuit diagram illustrating one embodiment of a semiconductor device. [Figure 16] FIG. 1 is a top view illustrating one embodiment of a semiconductor device. [Figure 17] 1 is a cross-sectional view illustrating one embodiment of a semiconductor device. [Figure 18] 1A to 1C are cross-sectional views illustrating one mode of a method for manufacturing a semiconductor device. [Figure 19] 1A to 1C are cross-sectional views illustrating one mode of a method for manufacturing a semiconductor device. [Figure 20] 1A to 1C are cross-sectional views illustrating one mode of a method for manufacturing a semiconductor device. [Figure 21] 1A to 1C are cross-sectional views illustrating one mode of a method for manufacturing a semiconductor device. [Figure 22] 1A to 1C are cross-sectional views illustrating one mode of a method for manufacturing a semiconductor device. [Figure 23] FIG. 1 is a top view illustrating one embodiment of a semiconductor device. [Figure 24] 1 is a cross-sectional view illustrating one embodiment of a semiconductor device. [Diagram 25] 1A to 1C are cross-sectional views illustrating one mode of a method for manufacturing a semiconductor device. [Figure 26] 1A to 1C are cross-sectional views illustrating one mode of a method for manufacturing a semiconductor device. [Figure 27] 1 is a cross-sectional view illustrating one embodiment of a semiconductor device. [Figure 28] 1A to 1C are cross-sectional views illustrating one mode of a method for manufacturing a semiconductor device. [Figure 29] 1A to 1C are cross-sectional views illustrating one mode of a method for manufacturing a semiconductor device. [Diagram 30] FIG. 1 is a diagram showing an electron microbeam diffraction pattern of an oxide semiconductor. [Diagram 31] FIG. 1 is a diagram showing an electron microbeam diffraction pattern of an oxide semiconductor. [Diagram 32] 1A and 1B are diagrams illustrating a touch sensor according to an embodiment. [Diagram 33] 1A to 1C are diagrams illustrating examples of configurations of a touch panel and an electronic device according to an embodiment. [Diagram 34] 1A and 1B are diagrams illustrating a pixel including a touch sensor according to an embodiment; [Diagram 35] 1A to 1C are diagrams illustrating operations of a touch sensor and a pixel according to an embodiment; [Diagram 36] FIG. 1 is a block diagram showing an example of the configuration of a liquid crystal display device. [Figure 37] 4 is a timing chart illustrating an example of a method for driving a liquid crystal display device. [Figure 38] 1A to 1C are diagrams illustrating electronic devices using a semiconductor device which is one embodiment of the present invention. [Figure 39] 1A to 1C are diagrams illustrating electronic devices using a semiconductor device which is one embodiment of the present invention. [Diagram 40] FIG. 1 is a diagram showing the Vg-Id characteristics of a transistor. [Diagram 41] 11A and 11B are diagrams showing the variation amounts of the threshold voltage and shift value of a transistor after a BT stress test and a light BT stress test. [Diagram 42] 1 is a diagram for explaining the definitions of a threshold voltage and a shift value; [Diagram 43] FIG. 13 is a diagram showing the results of a BT stress test. [Diagram 44] FIG. 1 shows the results of TDS measurement. [Diagram 45] FIG. 1 is a diagram illustrating the measurement results of ESR. [Diagram 46] FIG. 1 is a diagram for explaining the measurement results of SIMS. [Figure 47] FIG. 1 is a model diagram for the calculation of the H2O desorption process. [Figure 48] FIG. 1 is a model diagram for the calculation of the H2O desorption process. [Figure 49] Energy diagram and schematic diagram for the H2O desorption process. [Figure 50] FIG. 1 is a diagram for explaining the measurement results of SIMS. [Figure 51] FIG. 1 is a diagram for explaining the measurement results of SIMS. [Figure 52] FIG. 1 shows the results of TDS measurement. [Diagram 53] FIG. 1 is a diagram showing the Vg-Id characteristics of a transistor. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] Hereinafter, an embodiment of the present invention will be described in detail with reference to the drawings. The present invention is not limited to the following description, and the embodiments and aspects of the present invention may be modified without departing from the spirit and scope of the present invention. It will be readily understood by those skilled in the art that various modifications may be made to the embodiments and details of the present invention. However, the present invention should not be construed as being limited to the description of the following embodiments and examples. In the following embodiments and examples, the same parts or parts having similar functions are In the case of parts, the same reference numerals or the same hatch patterns are used in common among different drawings, and the repetition The explanation of the repetition will be omitted.

[0016] In each figure described in this specification, the size, thickness, or area of ​​each component is indicated by the following formula: The figures may be exaggerated for clarity and are not necessarily limited to scale. stomach.

[0017] In addition, the terms "first," "second," "third," etc., used in this specification are used interchangeably to avoid confusion of components. The number is added for convenience and is not intended to be a numerical limit. The terms can be replaced with "second" or "third" as appropriate for explanation.

[0018] The function of the "source" and "drain" is to change the direction of the current during circuit operation. For this reason, in this specification, the terms "sauce" and "dressing" are used interchangeably. The terms "in" and "in" may be used interchangeably.

[0019] Voltage is the potential difference between two points, and potential is the electrostatic field at a certain point. This refers to the electrostatic energy (electrical potential energy) possessed by a unit charge in a particle. Generally, the potential difference between a potential at a certain point and a reference potential (for example, ground potential) This is simply called potential or voltage, and potential and voltage are often used synonymously. Therefore, in this specification, unless otherwise specified, potential may be read as voltage. In this specification, voltage may be read as potential.

[0020] In this specification, when an etching process is performed after a photolithography process, The mask formed in the photolithography process is removed.

[0021] (Embodiment 1) In this embodiment, a semiconductor device according to one embodiment of the present invention and a manufacturing method thereof will be described with reference to drawings. Please refer to the following for explanation.

[0022] In a transistor including an oxide semiconductor film, An example of such defects is oxygen vacancies. The threshold voltage of a transistor using a thin film is easily shifted in the negative direction. This is because charges are generated due to oxygen vacancies in the oxide semiconductor film. When a transistor has normally-on characteristics, Various problems such as malfunctions becoming more likely or power consumption increasing when not in operation In addition, the electrical characteristics of transistors, typically There is a problem in that the amount of variation in the threshold voltage increases.

[0023] One of the causes of oxygen vacancies is damage that occurs during the manufacturing process of a transistor. For example, an insulating film or a conductive film is formed on an oxide semiconductor film by plasma CVD or sputtering. When forming an oxide semiconductor film, the oxide semiconductor film may be damaged depending on the forming conditions. There are times when this happens.

[0024] One of the causes of oxygen vacancies is oxygen desorption from an oxide semiconductor film due to heat treatment. For example, in order to remove impurities such as hydrogen and water contained in the oxide semiconductor film, However, when heat treatment is performed in a state where the oxide semiconductor film is exposed, the oxide Oxygen is released from the semiconductor film, forming oxygen vacancies.

[0025] In addition to oxygen deficiencies, impurities such as silicon and carbon, which are constituent elements of the insulating film, can also cause damage to the transistor. Therefore, the impurities may be mixed into the oxide semiconductor film, which may cause poor electrical characteristics of the transistor. As a result, the resistance of the oxide semiconductor film is reduced, and the oxide semiconductor film is easily deteriorated due to deterioration over time or in a stress test. This leads to a problem that the amount of fluctuation in the electrical characteristics of the transistor, typically the threshold voltage, increases. There is.

[0026] In view of the above, in this embodiment, a semiconductor device including a transistor having an oxide semiconductor film is In the present invention, oxygen vacancies in an oxide semiconductor film having a channel region and defects in the oxide semiconductor film are generated. One of the objectives is to reduce the concentration of impurities.

[0027] On the other hand, display devices on the market are becoming larger, with screen sizes of 60 inches or more diagonally. There is a trend toward larger screen sizes, with development also taking into account screen sizes of 120 inches or more. For this reason, the glass substrates used in display devices are large, 8th generation or higher. However, when using a large-area substrate, high-temperature processing, e.g., 450 Heating at temperatures above 30°C requires large, expensive heating equipment, which increases production costs. In addition, high temperature processing can cause warping and shrinkage of the substrate, resulting in a lower yield. is reduced.

[0028] Therefore, in this embodiment, the number of heat treatment steps is small and a large-area substrate can be used. Another object of the present invention is to manufacture a semiconductor device by using heat treatment at low temperature.

[0029] 1A to 1C are a top view and a cross-sectional view of a transistor 50 included in a semiconductor device. The transistor 50 shown in FIG. 1 is a channel-etched transistor. FIG. 1(A) is a top view of a transistor 50, and FIG. 1(B) is a top view of a transistor 50 along the dashed line A- in FIG. FIG. 1(C) is a cross-sectional view taken along dashed line CD in FIG. 1(A). In FIG. 1A, for the sake of clarity, the substrate 11 and some of the components of the transistor 50 (e.g. For example, the gate insulating film 17), the oxide insulating film 23, the oxide insulating film 24, the nitride insulating film 25, etc. etc. are omitted.

[0030] The transistor 50 shown in FIG. 1B and FIG. 1C has a gate The gate electrode 15 is formed on the substrate 11 and the gate electrode 15. an oxide semiconductor film 18 overlapping the gate electrode 15 via a gate insulating film 17; The semiconductor film 18 is in contact with a pair of electrodes 21 and 22. The gate insulating film 17 and the oxide On the semiconductor film 18 and the pair of electrodes 21 and 22, an oxide insulating film 23 and an oxide insulating film 2 4 and a protective film 26 made of a nitride insulating film 25 is formed.

[0031] The transistor 50 described in this embodiment includes the oxide semiconductor film 18. A part of the oxide semiconductor film 18 functions as a channel region. The oxide insulating film 23 is formed so as to contact the insulating film 23. A compound insulating film 24 is formed.

[0032] The oxide semiconductor film 18 is typically an In-Ga oxide film, an In-Zn oxide film, or an In -M-Zn oxide film (M is Al, Ti, Ga, Y, Zr, La, Ce, Nd, or Hf ) is available.

[0033] When the oxide semiconductor film 18 is an In-M-Zn oxide film, the sum of In and M is When the atomic percentage of In is 100 atomic %, the atomic ratio of In to M is preferably 25 atomic %. at least 75 atomic %, and more preferably In is 34 atomic % or less. ic% or more, and M less than 66 atomic%.

[0034] The oxide semiconductor film 18 has an energy gap of 2 eV or more, preferably 2.5 eV or more. More preferably, the energy gap is 3 eV or more. By using such a body, the off-state current of the transistor 50 can be reduced.

[0035] The thickness of the oxide semiconductor film 18 is 3 nm or more and 200 nm or less, preferably 3 nm or more and 10 0 nm or less, and more preferably 3 nm or more and 50 nm or less.

[0036] The oxide semiconductor film 18 is an In-M-Zn oxide film (wherein M is Al, Ti, Ga, Y, Zr, or L). a, Ce, Nd or Hf), the spa used to deposit the In-M-Zn oxide film The atomic ratio of the metal elements in the ion implantation target preferably satisfies In≧M and Zn≧M. The atomic ratio of the metal elements in such a sputtering target is In:M:Z. The preferred ranges are n=1:1:1 and In:M:Zn=3:1:2. The atomic ratio of the solid film 18 is included in the above sputtering target as an error. This includes a variation of plus or minus 20% in the atomic ratio of metal elements.

[0037] As the oxide semiconductor film 18, an oxide semiconductor film with low carrier density is used. For example, The oxide semiconductor film 18 has a carrier density of 1×10 17 pieces / cm 3 Below, preferably 1×1 0 15 pieces / cm 3 Less than 1×10, more preferably 13 pieces / cm 3 More preferably, 1×10 11 pieces / cm 3 The following oxide semiconductor film is used.

[0038] In addition, the semiconductor characteristics and electrical characteristics (field effect) of the required transistors are not limited to these. It is sufficient to use a material with an appropriate composition according to the required properties (e.g., the resultant mobility, threshold voltage, etc.). In order to obtain semiconductor characteristics of a transistor, the carrier density and impurity of the oxide semiconductor film 18 are controlled. By appropriately adjusting the concentration, defect density, atomic ratio of metal elements to oxygen, interatomic distance, density, etc. is preferred.

[0039] Note that the oxide semiconductor film 18 is an oxide semiconductor having a low impurity concentration and a low density of defect states. By using a thin film, it is possible to fabricate transistors with even better electrical properties. Here, it is preferable that the impurity concentration is low and the defect level density is low (there is little oxygen vacancy). High purity authentic or substantially high purity authentic. High purity authentic or substantially high purity authentic Some oxide semiconductors have a small number of carrier generation sources, so the carrier density can be reduced. Therefore, a transistor in which a channel region is formed in the oxide semiconductor film may In this case, the threshold voltage is rarely negative (also called normally-on). In addition, a highly purified intrinsic or substantially highly purified intrinsic oxide semiconductor film may not be formed. Since the defect level density is low, the trap level density may also be low. The oxide semiconductor film that is substantially intrinsic or highly pure has an extremely small off-state current and a large channel width. is 1×10 6 Even if the device has a channel length L of 10 μm, the source and drain electrodes When the electrode voltage (drain voltage) is in the range of 1V to 10V, the off-state current is Below the measurement limit of the meter analyzer, i.e. 1×10 -13 Obtaining a characteristic of A or lower Therefore, a transistor in which a channel region is formed in the oxide semiconductor film can be The variation in electrical characteristics is small, and the transistor can be highly reliable. The charges trapped in the trap levels of the membrane take a long time to disappear, as if they were solid. Therefore, the oxide semiconductor film with high trap state density may be A transistor in which a channel region is formed in a region containing impurities may have unstable electrical characteristics. The elements include hydrogen, nitrogen, an alkali metal, or an alkaline earth metal.

[0040] Hydrogen contained in the oxide semiconductor film reacts with oxygen that is bonded to metal atoms to form water. Oxygen vacancies are formed in the lattice from which oxygen has been removed (or in the portion from which oxygen has been removed). When hydrogen enters the gap, electrons, which act as carriers, can be generated. When it bonds with oxygen, which bonds with metal atoms, it can generate electrons, which act as carriers. Therefore, a transistor using an oxide semiconductor containing hydrogen has normally-on characteristics. It is easy to become.

[0041] For this reason, it is preferable that the amount of hydrogen in the oxide semiconductor film 18 be reduced as much as possible. Specifically, the oxide semiconductor film 18 is subjected to secondary ion mass spectrometry (SIMS). The hydrogen concentration obtained by ion mass spectrometry (DIAMS) was 5×10 19 atoms / cm 3 Less than or equal to 1×10 19 atoms / cm 3 Below, 5 x 10 18 atoms / cm 3 Less than or equal to 1×10 18 atoms / cm 3 Less than or equal to 5×10 17 atoms / cm 3 Below, more preferably 1×1 0 16 atoms / cm 3 The following applies.

[0042] When the oxide semiconductor film 18 contains silicon or carbon, which is one of the group 14 elements, As a result, oxygen vacancies increase in the oxide semiconductor film 18, and the oxide semiconductor film 18 becomes n-type. The concentration of silicon and carbon in the semiconductor film 18 (concentration obtained by secondary ion mass spectrometry) ) to 2 x 10 18 atoms / cm 3 Less than or equal to 2×10 17 atoms / cm 3 The following applies.

[0043] In addition, in the oxide semiconductor film 18, an alkali metal oxide was obtained by secondary ion mass spectrometry. The concentration of alkaline earth metals is 1×10 18 atoms / cm 3 Hereinafter, preferably 2×10 16 atoms / cm 3 The alkali metals and alkaline earth metals are When they bond with oxide semiconductors, carriers may be generated, increasing the off-state current of the transistor. For this reason, the alkali metal or alkaline earth metal of the oxide semiconductor film 18 may be It is preferable to reduce the concentration of metalloids.

[0044] In addition, when the oxide semiconductor film 18 contains nitrogen, electrons that serve as carriers are generated. The rear density increases and it becomes easier to make it n-type. As a result, A transistor having such an oxide semiconductor film tends to be normally on. It is preferable that the nitrogen content is reduced as much as possible. For example, in the secondary ion mass spectrometry, The resulting nitrogen concentration is 5×10 18 atoms / cm 3 It is preferable to do the following:

[0045] The oxide semiconductor film 18 may have a non-single crystal structure. , CAAC-OS (C Axis Aligned Crystalline Oxide Semiconductor), polycrystalline structure, microcrystalline structure (described below), or Among non-single crystal structures, the amorphous structure has the highest defect level density and CA AC-OS has the lowest defect state density.

[0046] The oxide semiconductor film 18 may have, for example, an amorphous structure. For example, the atomic arrangement is disordered and does not have crystalline components. Or, the oxide film has an amorphous structure. For example, it has a completely amorphous structure and does not have any crystalline parts.

[0047] Note that the oxide semiconductor film 18 may be divided into an amorphous region, a microcrystalline region, a polycrystalline region, and a polycrystalline region. The film may be a mixed film having two or more of the following regions: a region of a CAAC-OS structure, a region of a single crystal structure, and a region of a crystalline structure. The mixed film may have, for example, an amorphous structure region, a microcrystalline structure region, a polycrystalline structure region, a CAA In some cases, the crystal structure may have two or more regions, either a C-OS region or a single crystal structure region. The mixed film may have, for example, an amorphous structure region, a microcrystalline structure region, a polycrystalline structure region, a CAA In some cases, the material has a layered structure of two or more regions, either a C-OS region or a single crystal structure region. be.

[0048] In the transistor 50 described in this embodiment, As shown in FIG. 1, the oxide insulating film 23 is formed, and the oxide insulating film 24 is in contact with the oxide insulating film 23. is formed.

[0049] The oxide insulating film 23 is an oxygen-permeable oxide insulating film. 2. Reducing damage to the oxide semiconductor film 18 when forming the oxide insulating film 24 to be formed later. It also functions as a membrane.

[0050] The oxide insulating film 23 has a thickness of 5 nm to 150 nm, preferably 5 nm or more. A silicon oxide film, a silicon oxynitride film, or the like having a thickness of 50 nm or less can be used. In the present specification, a silicon oxynitride film is a film having a higher oxygen content than nitrogen as a composition. A silicon nitride oxide film is a film that contains more nitrogen than oxygen. Refers to a large membrane.

[0051] In addition, it is preferable that the oxide insulating film 23 has a small amount of defects. Therefore, the spin of the signal at g=2.001 originating from the silicon dangling bond Density is 3×10 17 spins / cm 3 This is because the oxide insulation If the film 23 contains a large number of defects, oxygen will be bonded to the defects, and the oxide insulating film 2 This is because the amount of oxygen permeating through 3 decreases.

[0052] In addition, the number of defects at the interface between the oxide insulating film 23 and the oxide semiconductor film 18 is small. Preferably, typically, the ESR measurement shows that the oxide semiconductor film 18 has a defect-derived g=1 The spin density of the signal appearing at .93 is 1×10 17 spins / cm 3 Further detection It is preferably equal to or lower than the lower limit.

[0053] Note that in the oxide insulating film 23, all of the oxygen that has entered the oxide insulating film 23 from the outside is Some oxygen does not move outside the oxide insulating film 23 and remains in the oxide insulating film 23. As oxygen enters the oxide insulating film 23, the oxygen contained in the oxide insulating film 23 In some cases, oxygen may move in the oxide insulating film 23 due to the movement of oxygen to the outside.

[0054] When an oxide insulating film that transmits oxygen is formed as the oxide insulating film 23, the oxide insulating film 23 The oxide insulating film 23 is formed on the upper surface of the oxide insulating film 24. The oxide insulating film 23 is formed on the upper surface of the oxide insulating film 23. The semiconductor film 18 can be made to move the

[0055] An oxide insulating film 24 is formed so as to be in contact with the oxide insulating film 23. 4 is formed using an oxide insulating film containing more oxygen than the oxygen that satisfies the stoichiometric composition. The oxide insulating film containing more oxygen than the stoichiometric composition is heated to remove the oxygen. A part of the element is released. The oxide insulating film contains more oxygen than the oxygen that satisfies the stoichiometric composition. In TDS analysis, the amount of oxygen released was 1.0 x 10 18 atoms / cm 3 More than 3.0×10 20 atoms / cm 3 The oxide insulating film It is.

[0056] The oxide insulating film 24 has a thickness of 30 nm to 500 nm, preferably 50 nm. A silicon oxide film, a silicon oxynitride film, or the like having a thickness of 400 nm or more and 400 nm or less can be used.

[0057] In addition, it is preferable that the oxide insulating film 24 has a small amount of defects. Therefore, the spin of the signal at g=2.001 originating from the silicon dangling bond Density is 1.5×10 18 spins / cm 3 Less than or even 1×10 18 spins / cm 3 Note that the oxide insulating film 24 has a thickness smaller than that of the oxide insulating film 23. Since the oxide insulating film 23 is located away from the oxide semiconductor film 18, the oxide insulating film 23 may have a higher defect density. stomach.

[0058] Other configuration details of transistor 50 are described below.

[0059] There is no particular restriction on the material of the substrate 11, but it should be at least strong enough to withstand the subsequent heat treatment. It is necessary to have heat resistance. For example, glass substrate, ceramic substrate, quartz substrate, surface treatment substrate, etc. A fiber substrate or the like may be used as the substrate 11. Also, a single material such as silicon or silicon carbide may be used. Crystalline semiconductor substrates, polycrystalline semiconductor substrates, compound semiconductor substrates such as silicon germanium, SO It is also possible to use a semiconductor substrate such as an I-substrate, and a semiconductor element is provided on the substrate. In addition, when a glass substrate is used as the substrate 11, Generation (1500mm x 1850mm), 7th generation (1870mm x 2200mm), 8th Generation (2200mm x 2400mm), 9th generation (2400mm x 2800mm), 1st By using large area substrates such as 2950mm x 3400mm, large display devices can be produced. can be produced.

[0060] In addition, a flexible substrate is used as the substrate 11, and the transistor 50 is directly formed on the flexible substrate. Alternatively, a release layer may be provided between the substrate 11 and the transistor 50. The layer is separated from the substrate 11 after a semiconductor device is partially or completely completed thereon, and then the layer is removed. In this case, the transistor 50 is placed on a substrate having poor heat resistance. It can also be transferred to a plate or flexible substrate.

[0061] The gate electrode 15 may be made of aluminum, chromium, copper, tantalum, titanium, molybdenum, or titanium. or an alloy containing the above-mentioned metal elements, It can be formed by using an alloy of a combination of metal elements. The metal element may be selected from one or more of the following: The electrode 15 may have a single-layer structure or a laminated structure of two or more layers. Single-layer aluminum film structure, double-layer aluminum film with titanium film laminated on top, titanium nitride Two-layer structure with a titanium film laminated on a titanium nitride film, and two-layer structure with a tungsten film laminated on a titanium nitride film. A two-layer structure in which a tungsten film is laminated on a tantalum nitride film or a tungsten nitride film. A titanium film is layered on top of an aluminum film, and then a titanium film is formed on top of that. There are also three-layer structures that use aluminum, titanium, tantalum, tungsten, and molybdenum. A combination of one or more elements selected from the group consisting of butanol, chromium, neodymium, and scandium. Alternatively, an alloy film or a nitride film may be used.

[0062] The gate electrode 15 is made of indium tin oxide or indium oxide containing tungsten oxide. oxide, indium zinc oxide with tungsten oxide, indium oxide with titanium oxide Indium tin oxide, indium zinc oxide, silicon oxide with titanium oxide A light-transmitting conductive material such as indium tin oxide can also be used. A laminate structure of the above-mentioned light-transmitting conductive material and the above-mentioned metal element may also be used.

[0063] In addition, an In-Ga-Zn-based oxynitride film is formed between the gate electrode 15 and the gate insulating film 17. , In-Sn-based oxynitride film, In-Ga-based oxynitride film, In-Zn-based oxynitride film, Sn-based oxidized nitride film, In-based oxidized nitride film, metal nitride film (InN, ZnN, etc.), etc. are provided. These films have a work function of 5 eV or more, preferably 5.5 eV or more, and are oxide films. Since the electron affinity is larger than that of a semiconductor, the The threshold voltage can be shifted to the positive side, making it a switching element with a normally-off characteristic. For example, when an In-Ga-Zn oxide / nitride film is used, at least the oxide The nitrogen concentration is higher than that of the In-Ga-Zn oxide semiconductor film 18, specifically, 7 atomic % or more. A nitride film is used.

[0064] The gate insulating film 17 is made of, for example, silicon oxide, silicon oxynitride, silicon nitride oxide, or nitride. Silicon oxide, aluminum oxide, hafnium oxide, gallium oxide or Ga-Zn metal An oxide or the like may be used, and the insulating film is provided as a laminated layer or a single layer.

[0065] The gate insulating film 17 is made of hafnium silicate (HfSiO x ), nitrogen is added Hafnium Silicate (HfSi x O y N z ), nitrogen-doped hafnium aluminium minate (HfAl x O y N z ), hafnium oxide, yttrium oxide and other high- The use of k-materials can reduce the gate leakage of transistors.

[0066] The thickness of the gate insulating film 17 is 5 nm or more and 400 nm or less, and more preferably 10 nm or more. It is preferably 300 nm or less, and more preferably 50 nm or more and 250 nm or less.

[0067] The pair of electrodes 21 and 22 are made of a conductive material such as aluminum, titanium, chromium, or nickel. , copper, yttrium, zirconium, molybdenum, silver, tantalum, or tungsten The metal or alloy mainly composed of the metal is used as a single layer or laminated structure. For example, a single layer structure of an aluminum film containing silicon, or a titanium film stacked on an aluminum film, Two-layer structure with a titanium film on a tungsten film, two-layer structure with a copper-magnesium- A two-layer structure in which a copper film is laminated on an aluminum alloy film, a titanium film or a titanium nitride film, and An aluminum film or a copper film is laminated on the titanium film or the titanium nitride film, and then the aluminum film or the copper film is laminated on the titanium film or the titanium nitride film. A three-layer structure in which a titanium film or titanium nitride film is formed on top, a molybdenum film or molybdenum nitride film A molybdenum film and an aluminum film or a copper film are laminated on the molybdenum film or the molybdenum nitride film. A three-layer structure is formed by laminating a layer of a molybdenum film or a molybdenum nitride film on top of the layer of a silicon nitride film. A transparent conductive material containing indium oxide, tin oxide, or zinc oxide may also be used. .

[0068] Further, oxygen, hydrogen, water, an alkali metal, an alkaline earth metal, etc. are deposited on the oxide insulating film 24. By providing the nitride insulating film 25 having the blocking effect, Diffusion of oxygen to the outside and intrusion of hydrogen, water, etc. into the oxide semiconductor film 18 from the outside are prevented. The nitride insulating film can be silicon nitride, silicon oxynitride, or aluminum nitride. , aluminum oxide nitride, etc. In addition, oxygen, hydrogen, water, alkali metals, alkaline earth metals, Instead of a nitride insulating film that has a blocking effect of metals, etc., a blocking material for oxygen, hydrogen, water, etc. An oxide insulating film having a blocking effect against oxygen, hydrogen, water, etc. may be provided. Examples of the oxide insulating film having such a structure include aluminum oxide, aluminum oxynitride, and gallium oxide. , gallium oxide nitride, yttrium oxide, yttrium oxide nitride, hafnium oxide, Hafnium nitride and the like.

[0069] Next, a manufacturing method of the transistor 50 shown in FIG. 1 will be described with reference to FIG.

[0070] As shown in FIG. 2A, a gate electrode 15 is formed on a substrate 11. A gate insulating film 17 is formed.

[0071] Here, a glass substrate is used as the substrate 11.

[0072] The method of forming the gate electrode 15 will be described below. First, the sputtering method, the CVD method, and the evaporation method are used. A conductive film is formed by deposition or the like, and a mask is formed on the conductive film by a photolithography process. Next, a part of the conductive film is etched using the mask to form the gate electrode 15. After this, the mask is removed.

[0073] The gate electrode 15 may be formed by electrolytic plating, printing, ink jet printing, or the like instead of the above-mentioned method. It may be formed by a jet method or the like.

[0074] Here, a tungsten film having a thickness of 100 nm is formed by sputtering. A mask is formed by a photolithography process, and a tungsten film is formed using the mask. The gate electrode 15 is formed by dry etching.

[0075] The gate insulating film 17 is formed by a sputtering method, a CVD method, a vapor deposition method or the like.

[0076] The gate insulating film 17 is a silicon oxide film, a silicon oxynitride film, or a silicon nitride oxide film. When forming a silicon film, a deposition gas containing silicon and an oxidizing gas are used as the source gas. Representative examples of deposition gases containing silicon include silane, disilane, Examples of oxidizing gases include trisilane, fluorinated silane, etc. Examples of oxidizing gases include oxygen, ozone, and nitrous oxide. , nitrogen dioxide, etc.

[0077] In addition, when a gallium oxide film is formed as the gate insulating film 17, MOCVD (Metal Organic Chemical Vapor Deposition (OCVD) method It can be formed by:

[0078] Next, as shown in FIG. 2B, an oxide semiconductor film 18 is formed on the gate insulating film 17. .

[0079] The method for forming the oxide semiconductor film 18 will be described below. Then, a photolithography is performed on the oxide semiconductor film. After a mask is formed by a lithography process, part of the oxide semiconductor film is etched using the mask. By etching, an oxide semiconductor film 18 is formed, which is isolated from the other elements, as shown in FIG. After this, the mask is removed.

[0080] The oxide semiconductor film that will later become the oxide semiconductor film 18 can be formed by sputtering, coating, pulse The layer can be formed by using a laser deposition method, a laser ablation method, or the like.

[0081] When an oxide semiconductor film is formed by a sputtering method, a power source for generating plasma The device may be an RF power supply device, an AC power supply device, a DC power supply device, or the like, as appropriate.

[0082] The sputtering gas is a rare gas (typically argon), oxygen gas, or a mixture of a rare gas and oxygen. A mixed gas is used as appropriate. In the case of a mixed gas of rare gas and oxygen, the ratio of oxygen to rare gas is It is preferable to increase the gas ratio.

[0083] The target may be appropriately selected depending on the composition of the oxide semiconductor film to be formed. .

[0084] In order to obtain a highly pure intrinsic or substantially highly pure intrinsic oxide semiconductor film, Not only is it necessary to evacuate the inside of the chamber to a high vacuum, but it is also necessary to highly purify the sputtering gas. The oxygen gas and argon gas used should have a dew point of -40°C or less, preferably -80°C or less. Gas that has been highly purified to -100℃ or less, more preferably -120℃ or less By using the above, it is possible to prevent moisture and the like from being taken into the oxide semiconductor film as much as possible. do.

[0085] Here, an In-Ga-Zn oxide target (In:Ga:Zn=1:1:1) was used. A 35-nm-thick In-Ga-Zn oxide film was deposited as an oxide semiconductor film by sputtering. Next, a mask is formed over the oxide semiconductor film, and a part of the oxide semiconductor film is By selectively etching, the oxide semiconductor film 18 is formed.

[0086] Next, as shown in FIG. 2C, after the oxide semiconductor film 18 is formed, a heat treatment is not performed. , a pair of electrodes 21 and 22 are formed.

[0087] The method for forming the pair of electrodes 21 and 22 will be described below. First, the sputtering method and the CVD method are used. Next, a conductive film is formed on the conductive film by a photolithography process. Next, the conductive film is etched using the mask to form a pair of electrodes 21 and 2 2 is formed. After this, the mask is removed.

[0088] Here, a tungsten film having a thickness of 50 nm, an aluminum film having a thickness of 400 nm, and a A titanium film having a thickness of 100 nm is then laminated on the titanium film by sputtering. A mask is formed by a photolithography process, and a tungsten film and an aluminum film are formed by using the mask. The aluminum film and the titanium film are dry etched to form a pair of electrodes 21 and 22 .

[0089] Next, as shown in FIG. 2D, on the oxide semiconductor film 18 and the pair of electrodes 21 and 22, The oxide insulating film 23 is formed. Next, the oxide insulating film 24 is formed on the oxide insulating film 23. .

[0090] After the oxide insulating film 23 is formed, the oxide insulating film 2 is successively removed without being exposed to the air. After the oxide insulating film 23 is formed, the source gas The oxide insulating film 24 is continuously formed by adjusting one or more of the flow rate, pressure, high frequency power, and substrate temperature. By forming the oxide insulating film 23 and the oxide insulating film 24 in In addition, the impurity concentration in the oxide insulating film 24 can be reduced. The amount of oxygen vacancies in the oxide semiconductor film 18 can be reduced. It is possible.

[0091] The oxide insulating film 23 is made of a silicon oxide film placed in a vacuum-evacuated processing chamber of a plasma CVD apparatus. The substrate is maintained at a temperature of 280° C. or higher and 400° C. or lower, and a source gas is introduced into the processing chamber. The pressure in the chamber is set to 20 Pa or more and 250 Pa or less, and more preferably 100 Pa or more and 250 Pa or less. Under the conditions of supplying high frequency power to an electrode provided in the processing chamber, the oxide insulating film 2 As the film 3, a silicon oxide film or a silicon oxynitride film can be formed.

[0092] As the source gas for the oxide insulating film 23, a deposition gas containing silicon and an oxidizing gas are used. Representative examples of deposition gases containing silicon include silane, disilane, Examples of oxidizing gases include trisilane, fluorinated silane, etc. Examples of oxidizing gases include oxygen, ozone, and nitrous oxide. , nitrogen dioxide, etc.

[0093] By using the above conditions, an oxide insulating film that transmits oxygen is formed as the oxide insulating film 23. In addition, by providing the oxide film 19 and the oxide insulating film 23, In the process of forming the oxide insulating film 24, damage to the oxide semiconductor film 18 can be reduced. It is.

[0094] The oxide insulating film 23 is placed in a vacuum evacuated processing chamber of a plasma CVD apparatus. The substrate is maintained at a temperature of 280° C. or higher and 400° C. or lower, and a source gas is introduced into the processing chamber. The pressure in the treatment chamber is set to 100 Pa or more and 250 Pa or less, and high-frequency power is applied to the electrode installed in the treatment chamber. Depending on the conditions for supplying oxygen, the oxide insulating film 23 may be a silicon oxide film or a silicon oxynitride film. A silicon film can be formed.

[0095] Under the film formation conditions, by setting the substrate temperature to the above temperature, the bonding strength between silicon and oxygen As a result, the oxide insulating film 23 is oxygen-permeable, dense, and hard. Oxide insulating film, typically, etching rate for 0.5% by weight hydrofluoric acid at 25°C A silicon oxide film or an oxynitride film having a crystallinity of 10 nm / min or less, preferably 8 nm / min or less. A silicon film can be formed.

[0096] In addition, since the oxide insulating film 23 is formed while heating, the oxide semiconductor Hydrogen, water, etc. contained in the oxide semiconductor film 18 can be desorbed. The hydrogen is combined with oxygen radicals generated in the plasma to become water. During the film formation process, the substrate is heated, and the water generated by the combination of oxygen and hydrogen is That is, the oxide insulating film 23 is formed by the plasma CVD method. By forming the oxide semiconductor film, the amount of water and hydrogen contained in the oxide semiconductor film can be reduced.

[0097] In addition, since heating is performed in the process of forming the oxide insulating film 23, the oxide semiconductor film 18 The heating time in an exposed state is short, and oxygen is released from the oxide semiconductor film by heat treatment. That is, the amount of oxygen vacancies in the oxide semiconductor film can be reduced. This can be done.

[0098] Furthermore, by setting the pressure in the treatment chamber to 100 Pa or more and 250 Pa or less, the oxide insulating film The water content in the 23 is reduced, which reduces the variation in the electrical characteristics of the transistor 50. It is possible to reduce the threshold voltage and suppress the fluctuation of the threshold voltage.

[0099] In addition, by setting the pressure in the treatment chamber to 100 Pa or more and 250 Pa or less, the oxide insulating film 23 When forming the oxide semiconductor film 18, damage to the oxide semiconductor film 18 can be reduced. In particular, the amount of oxygen vacancies in the oxide insulating film 23 can be reduced. Alternatively, the deposition temperature of the oxide insulating film 24 to be formed later is increased, typically to 220° C. or higher. By setting the temperature at a low level, part of oxygen contained in the oxide semiconductor film 18 is released, and oxygen vacancies are formed. In addition, in order to improve the reliability of the transistor, the oxide insulating film 2 to be formed later is By using the film formation conditions for reducing the amount of defects in 4, the amount of oxygen desorption is easily reduced. As a result, it may be difficult to reduce oxygen vacancies in the oxide semiconductor film 18. The pressure in the processing chamber is set to 100 Pa or more and 250 Pa or less during the formation of the oxide insulating film 23. By reducing damage to the oxide semiconductor film 18 caused by the oxidation of the oxide insulating film 24, the oxide semiconductor film 18 can be prevented from being damaged. The oxygen vacancies in the oxide semiconductor film 18 can be reduced by the amount of oxygen desorption.

[0100] In addition, by increasing the amount of oxidizing gas to 100 times or more the amount of deposition gas containing silicon, The hydrogen content in the oxide insulating film 23 can be reduced. Since the amount of hydrogen mixed into the semiconductor film 18 can be reduced, the threshold voltage of the transistor can be reduced. The shift can be suppressed.

[0101] Here, the oxide insulating film 23 is made of silane at a flow rate of 30 sccm and 4000 sccm. The source gas was nitrous oxide with a flow rate of 1.0 cm, the pressure in the processing chamber was 200 Pa, and the substrate temperature was 220°C. A 27.12MHz high-frequency power source was used to supply 150W of high-frequency power to the parallel plate electrodes. A silicon oxynitride film with a thickness of 50 nm is formed by the plasma CVD method under the following conditions. In this manner, a silicon oxynitride film through which oxygen is transmitted can be formed.

[0102] The oxide insulating film 24 is placed in a vacuum-evacuated processing chamber of a plasma CVD apparatus. The substrate is kept at a temperature of 180° C. or higher and 280° C. or lower, more preferably 200° C. or higher and 240° C. or lower. The raw material gas is introduced into the processing chamber to set the pressure in the processing chamber at 100 Pa or more and 250 Pa or less. More preferably, the pressure is set to 100 Pa or more and 200 Pa or less. .17W / cm2 More than 0.5W / cm 2 Less than or equal to 0.25 W / cm 2 End 0.35W / cm 2 Under the following conditions of high frequency power supply, silicon oxide film or oxide A silicon nitride film is formed.

[0103] As the source gas of the oxide insulating film 24, a deposition gas containing silicon and an oxidizing gas are used. Representative examples of deposition gases containing silicon include silane, disilane, Examples of oxidizing gases include trisilane, fluorinated silane, etc. Examples of oxidizing gases include oxygen, ozone, and nitrous oxide. , nitrogen dioxide, etc.

[0104] The oxide insulating film 24 is formed under the conditions of high frequency irradiation with the above power density in a processing chamber at the above pressure. Supplying microwave power increases the efficiency of decomposing the source gas in the plasma, and oxygen radicals are increased. As the source gas is added, the oxidation of the source gas proceeds, so that the oxygen content in the oxide insulating film 24 becomes stoichiometric. On the other hand, in the film formed at the substrate temperature, the composition of silicon and oxygen is Since the bonding strength is weak, some of the oxygen in the film is released by the heat treatment in the subsequent process. It contains more oxygen than the stoichiometric composition, and some of the oxygen is released by heating. In addition, the oxide insulating film 2 can be formed over the oxide semiconductor film 18. Therefore, in the process of forming the oxide insulating film 24, the oxide insulating film 2 3 serves as a protective film for the oxide semiconductor film 18. As a result, damage to the oxide semiconductor film 18 is prevented. Therefore, the oxide insulating film 24 can be formed by using high-frequency power with high power density while reducing the Cut.

[0105] In addition, in the deposition conditions of the oxide insulating film 24, the deposition gas containing silicon is By increasing the flow rate of the reactive gas, it is possible to reduce the number of defects in the oxide insulating film 24. Typically, ESR measurements reveal that the g value is 2.0 due to the dangling bonds of silicon. The spin density of the signal appearing in 01 is 6×10 17 spins / cm 3 Less than 3x, preferably 10 17 spins / cm 3 Less than or equal to 1.5×10 17 spins / cm 3 below As a result, the signal quality of the transistor is improved. It can increase reliability.

[0106] Here, the oxide insulating film 24 is made of silane at a flow rate of 200 sccm and SiO at a flow rate of 4000 s. The source gas was nitrous oxide (N2O) at 1.0 ccm, the pressure in the processing chamber was 200 Pa, and the substrate temperature was 220° C. A 27.12MHz high-frequency power source was used to apply 1500W of high-frequency power to the parallel plate electrodes. A silicon oxynitride film with a thickness of 400 nm is formed by the supplied plasma CVD method. The plasma CVD device has an electrode area of ​​6000 cm 2 Parallel plate plasma CVD The power supplied to the device is converted to power per unit area (power density) of 0.25W. / cm 2 It is.

[0107] Next, a heat treatment is performed. The temperature of the heat treatment is typically 150° C. or higher and 400° C. or lower. The temperature is preferably 300°C or higher and 400°C or lower, and more preferably 320°C or higher and 370°C or lower.

[0108] The heat treatment can be performed using an electric furnace, an RTA device, or the like. Therefore, heat treatment can be performed at a temperature above the distortion point of the substrate for a short period of time. The processing time can be reduced.

[0109] Heat treatment is carried out in a vacuum of nitrogen, oxygen, or ultra-dry air (water content of 20 ppm or less, preferably 1 ppm). pm or less, preferably 10 ppb or less air), or rare gases (argon, helium, etc.) In addition, the above-mentioned nitrogen, oxygen, ultra-dry air, or rare gas may be mixed with hydrogen, water, or the like. It is preferable that the above is not included.

[0110] By the heat treatment, part of oxygen contained in the oxide insulating film 24 is transferred to the oxide semiconductor film 18. By this, the amount of oxygen vacancies in the oxide semiconductor film 18 can be further reduced.

[0111] In the case where the oxide insulating film 23 and the oxide insulating film 24 contain water, hydrogen, or the like, A nitride insulating film 25 having a blocking function is then formed and heat treatment is performed, whereby the Water, hydrogen, and the like contained in the oxide insulating film 23 and the oxide insulating film 24 are transferred to the oxide semiconductor film 18. However, the heating causes the oxide semiconductor film 18 to move and generate defects. It is possible to remove water, hydrogen, etc. contained in the oxide insulating film 23 and the oxide insulating film 24. , the variation in the electrical characteristics of the transistor 50 is reduced, and the variation in the threshold voltage is suppressed. It is possible.

[0112] Note that the oxide insulating film 24 is formed over the oxide insulating film 23 while being heated. Oxygen is transferred to the oxide semiconductor film 18 to compensate for oxygen vacancies in the oxide semiconductor film 18. Therefore, the heat treatment may not be performed.

[0113] Here, heat treatment is performed in a nitrogen and oxygen atmosphere at 350° C. for 1 hour.

[0114] In addition, when the pair of electrodes 21 and 22 are formed, the conductive film is etched to form an oxide semiconductor. The oxide semiconductor film 18 is damaged, and the back channel of the oxide semiconductor film 18 (the oxide semiconductor film 18 In this case, oxygen vacancies occur on the surface opposite to the surface facing the gate electrode 15. The oxide insulating film 24 contains more oxygen than the oxygen that satisfies the stoichiometric composition. By applying this method, oxygen vacancies that occurred on the back channel side due to heat treatment can be repaired. This can reduce defects in the oxide semiconductor film 18. Therefore, the reliability of the transistor 50 can be improved.

[0115] Next, the nitride insulating film 25 is formed by sputtering, CVD or the like.

[0116] When the nitride insulating film 25 is formed by the plasma CVD method, The substrate placed in the evacuated processing chamber is heated to 300° C. or higher and 400° C. or lower, more preferably A temperature of 320° C. or higher and 370° C. or lower is preferable because it allows the formation of a dense nitride insulating film. .

[0117] When a silicon nitride film is formed as the nitride insulating film 25 by the plasma CVD method, the silicon It is preferable to use a deposition gas containing carbon, nitrogen, and ammonia as the source gas. By using a small amount of ammonia as a feed gas compared to nitrogen, the ammonia in the plasma The silicon-containing deposition gas dissociates and generates active species. This breaks the silicon-hydrogen bond and the nitrogen triple bond. Promoted bonding, fewer silicon and hydrogen bonds, fewer defects, and dense silicon nitride On the other hand, the amount of ammonia relative to nitrogen in the source gas is high. If the temperature is too low, the decomposition of the silicon-containing deposition gas and nitrogen will not proceed, and silicon and hydrogen bonds will form. As a result, defects are increased and a rough silicon nitride film is formed. For these reasons, the flow rate ratio of nitrogen to ammonia in the raw gas is preferably 5 to 50. It is preferable to set the value to 10 or more and 50 or less.

[0118] Here, silane at a flow rate of 50 sccm and 5000 The source gases were nitrogen at a flow rate of 100 sccm and ammonia at a flow rate of 100 sccm. The pressure in the processing chamber was The pressure was set at 100 Pa, the substrate temperature was set at 350°C, and a 27.12 MHz high frequency power source was used for 1000 A 50 nm thick nitride film was formed by plasma CVD using a 1000 MHz high frequency power supply to parallel plate electrodes. A silicon film is formed. The plasma CVD device has an electrode area of ​​6000 cm. 2 It is flat This is a horizontal and flat type plasma CVD device, and the supplied power is expressed as power per unit area (power density ) is converted to 1.7 × 10 -1 W / cm 2 It is.

[0119] Through the above steps, a film consisting of the oxide insulating film 23, the oxide insulating film 24, and the nitride insulating film 25 is formed. A protective film 26 can be formed by the above process.

[0120] Next, a heat treatment may be performed. The temperature of the heat treatment is typically 150° C. or higher and 40° C. or lower. 0°C or lower, preferably 300°C or higher and 400°C or lower, preferably 320°C or higher and 370°C or lower Let us assume that.

[0121] Through the above steps, the transistor 50 can be manufactured.

[0122] In this embodiment, the plasma CVD method is performed while heating the substrate to a temperature of 280° C. or higher and 400° C. or lower. In order to form the oxide insulating film using the above-mentioned method, hydrogen, water, and the like contained in the oxide semiconductor film 18 are released. In this step, the oxide semiconductor film can be heated in an exposed state. The heating time is short, and even if the temperature of the oxide semiconductor by heat treatment is 400°C or less, A transistor with the same amount of variation in threshold voltage as that of a heat-treated transistor is manufactured. As a result, the cost of the semiconductor device can be reduced.

[0123] In addition, the oxide semiconductor film having a stoichiometric composition is overlapped with the oxide semiconductor film serving as a channel region. By forming an oxide insulating film that contains more oxygen than oxygen that is As a result, oxygen contained in the oxide semiconductor film can be transferred to the oxide semiconductor film. The defect content can be reduced.

[0124] In particular, the oxide semiconductor film that functions as a channel region and the oxygen-containing oxide film that satisfies the stoichiometric composition To form an oxide insulating film that transmits oxygen between the oxide insulating film containing more oxygen than the insulating film containing the oxide insulating film. When forming an oxide insulating film containing more oxygen than the oxygen that satisfies the stoichiometric composition, Damage to the oxide semiconductor film can be suppressed. The amount of oxygen vacancies can be reduced.

[0125] From the above, it is possible to provide a semiconductor device including an oxide semiconductor film, in which the amount of defects is reduced. In addition, the electrical characteristics of a semiconductor device including an oxide semiconductor film can be improved. The above semiconductor device can be obtained.

[0126] <Reaction of hydrogen and excess oxygen contained in oxide semiconductor film> Here, we will discuss the oxygen radicals that are generated when forming an oxide insulating film by plasma CVD and the oxygen The reaction of hydrogen contained in the compound semiconductor film will be described below.

[0127] First, the source gas for generating oxygen radicals will be described.

[0128] Representative examples of atmospheres capable of generating oxygen radicals include nitrous oxide atmosphere and There is an oxygen atmosphere.

[0129] A reaction in which oxygen radicals are generated in a plasma generated in a nitrous oxide atmosphere. The reaction enthalpy was calculated using Gaussian 09. The calculation method was Moller-Plesset quadratic perturbation (MP2) is used, and the basis functions are The calculation results are shown in Equation 1.

[0130]

number

[0131] In addition, the reaction in which oxygen radicals are generated in the plasma generated in an oxygen atmosphere The reaction enthalpy was calculated. The calculation was performed using Gaussian 09. The calculation method was as follows: Moller-Plesset quadratic perturbation (MP2) is used, and the basis functions are The calculation results are shown in Equation 2.

[0132]

number

[0133] From the calculation results shown in Equation 1 and Equation 2, it can be seen that the amount of nitrogen oxide generated in a nitrous oxide atmosphere is greater than that in an oxygen atmosphere. It can be seen that oxygen radicals are easily generated in the plasma.

[0134] Next, InGaZnO4 was used as the oxide semiconductor film, and the surface of the oxide semiconductor film was The excess oxygen (hereinafter referred to as exO) that bonds with the Ga atom or oxygen atom that is The separation process was investigated.

[0135] Here, the basic unit cell of the InGaZnO4 crystal is doubled in the a-axis and b-axis. The (Ga,Zn)O layer is the outermost layer of the structure, and the (Ga,Zn)O layer and the InO2 layer The crystal structure was adjusted to have three layers, a (001) layer, and a (Ga,Zn)O layer. A surface model (number of atoms: 112) with a vacuum region in the c-axis direction was used to measure H2 A calculation was performed on the O desorption process. The model used for the calculation is shown in Figure 47(A). In A), the excess oxygen bonded to the surface of InGaZnO4 is indicated as exO. Two H atoms were placed at positions separated from O. As shown in FIG. 4. The exO on the surface is energetically stable when it forms Ga-exO-O. For this reason, the structure shown in Figure 47(A) was used as the initial structure for the reaction path. The calculation conditions are shown in Table 1. As shown in.

[0136] [Table 1]

[0137] FIG. 48 shows the structure of InGaZnO4 from step (0) to step (8). The two H atoms are represented as H1 and H2 in the order of their proximity to the exO.

[0138] From step (0) to step (1), H1 diffuses near exO.

[0139] In steps (1) and (2), H1 is bonded to exO (O1 )

[0140] From step (2) to step (3), H1 moves outside O1.

[0141] In steps (3) and (4), H1 binds to exO to form Ga-exO - Form H1.

[0142] In steps (4) and (5), H2 binds to O1.

[0143] In steps (5) and (6), H2 moves outside O1.

[0144] In steps (6) and (7), H2 binds to exO.

[0145] In steps (7) and (8), H1, exO, and H2 are mixed. 2O is eliminated.

[0146] Next, the structure at step (0) is set as the energy standard (0.00 eV) for the reaction path. The energy diagram showing the calculated energy changes from step (1) to step (8) and each A schematic diagram of the reactions of Ga, O, and H in the steps is shown in FIG.

[0147] As shown in FIG. 49, when exO is bonded to the InGaZnO4 surface, the exO and InGaZn The reaction of H in O4 to produce H2O and the reaction of H2O desorption produce large amounts of energy. That is, it is found that the reaction is an exothermic reaction.

[0148] This indicates that oxygen radicals contained in the plasma are bound to the In-Ga-Zn oxide surface. When the In-Ga-Zn oxide is combined with the In-Ga-Zn oxide and exists as exO, oxygen vacancies are not formed in the In-Ga-Zn oxide. It is possible that H in the n-Ga-Zn oxide reacts with exO to produce HO. In addition, the H2O can be released. As a result, the hydrogen contained in the oxide semiconductor film can be The concentration is reduced.

[0149] <Modification 1, Regarding the Undercoat Insulating Film> In the transistor 50 of this embodiment, the substrate 11 and the gate electrode A base insulating film can be provided between the electrodes 15. The base insulating film can be made of silicon oxide. Silicon oxide nitride, silicon nitride, silicon oxide nitride, gallium oxide, hafnium oxide Examples of the oxides include aluminum oxide, yttrium oxide, aluminum oxide nitride, etc. The insulating film materials are silicon nitride, gallium oxide, hafnium oxide, and yttrium oxide. By using aluminum oxide or the like, impurities, typically alkali metals, The diffusion of water, hydrogen, and the like into the oxide semiconductor film 18 can be suppressed.

[0150] The base insulating film can be formed by a sputtering method, a CVD method, or the like.

[0151] <Modification 2: Gate insulating film> In the transistor 50 according to this embodiment, a gate insulating film 17 may be stacked as necessary. The gate insulating film 17 may have a layer structure. explain.

[0152] As shown in FIG. 3A, the gate insulating film 17 is made of a nitride insulating film 17a and an oxide insulating film. The gate electrode 15 may have a laminated structure in which the gate electrodes 17b and 17b are laminated in order from the gate electrode 15 side. By providing the nitride insulating film 17a on the electrode 15 side, impurities from the gate electrode 15, typically Hydrogen, nitrogen, an alkali metal, an alkaline earth metal, or the like moves to the oxide semiconductor film 18. This can prevent the following from happening:

[0153] In addition, by providing the oxide insulating film 17b on the oxide semiconductor film 18 side, the gate insulating film 17 In addition, the defect state density at the interface with the oxide semiconductor film 18 can be reduced. As a result, a transistor with little deterioration in electrical characteristics can be obtained. As the oxide insulating film 24, more oxygen than that satisfying the stoichiometric composition is used as the oxide insulating film b. When the oxide insulating film 17 is formed using an oxide insulating film containing This is more preferable since it is possible to further reduce the defect state density in the semiconductor layer.

[0154] As shown in FIG. 3B, the gate insulating film 17 is made of a nitride insulating film 17c having few defects and The nitride insulating film 17d having high hydrogen blocking properties and the oxide insulating film 17b are formed on the gate electrode. The gate insulating film 17 may have a laminated structure in which the layers are laminated in order from the side of the gate insulating film 15. By providing the nitride insulating film 17c with a small amount of oxide, the dielectric strength of the gate insulating film 17 is improved. In addition, by providing the nitride insulating film 17d having high hydrogen blocking properties, Hydrogen from the gate electrode 15 and the nitride insulating film 17c moves to the oxide semiconductor film 18. It can be prevented.

[0155] An example of a method for forming the nitride insulating films 17c and 17d shown in FIG. The plasma CVD method uses a mixture of silane, nitrogen, and ammonia as the source gas. As a result, a silicon nitride film with few defects is formed as the nitride insulating film 17c. The gas was switched to a mixture of silane and nitrogen to reduce the hydrogen concentration and block hydrogen. A silicon nitride film capable of being etched is formed as the nitride insulating film 17d. By using this method, a nitride insulating film having few defects and a blocking property against hydrogen can be deposited. A layered gate insulating film 17 can be formed.

[0156] As shown in FIG. 3C, the gate insulating film 17 is made of a nitride having a high impurity blocking property. The insulating film 17e, the nitride insulating film 17c having few defects, and the nitride insulating film 17c having high hydrogen blocking properties A laminated structure in which an insulating film 17d and an oxide insulating film 17b are laminated in this order from the gate electrode 15 side. The gate insulating film 17 may be made of a nitride having a high impurity blocking property. By providing the insulating film 17e, impurities from the gate electrode 15, typically hydrogen, nitrogen, The alkali metal, the alkaline earth metal, or the like is prevented from migrating to the oxide semiconductor film 18. This can be done.

[0157] An example of a method for forming the nitride insulating films 17e, 17c, and 17d shown in FIG. 3(C) will be described below. First, a plasma was generated using a mixture of silane, nitrogen, and ammonia as the source gas. A silicon nitride film with high impurity blocking properties is formed by the CVD method as the nitride insulating film 17e. Next, the flow rate of ammonia is increased to form silicon nitride with fewer defects. The resulting film is formed as a nitride insulating film 17c. Next, the source gas is a mixed gas of silane and nitrogen. By switching to silicon nitride, which has a low hydrogen concentration and can block hydrogen, The nitride insulating film 17d is formed by using a silicon film. Also, a gate insulating film 17 is formed by laminating a nitride insulating film having an impurity blocking property. It is possible.

[0158] <Modification 3: Pair of Electrodes> The pair of electrodes 21 and 22 in the transistor 50 shown in this embodiment are elemental or non-elementary metals such as tantalum, titanium, aluminum, copper, molybdenum, chromium, or tantalum It is preferable to use a conductive material that easily bonds with oxygen, such as an alloy. The oxygen contained in the membrane 18 is bonded to the conductive material contained in the pair of electrodes 21 and 22 to form an oxide. An oxygen vacancy region is formed in the oxide semiconductor film 18. In some cases, some of the constituent elements of the conductive material that forms the electrodes 21 and 22 may be mixed in. As a result, as shown in FIG. 4, in the oxide semiconductor film 18, the area in contact with the pair of electrodes 21 and 22 The low resistance regions 20a and 20b are formed in the vicinity of the low resistance region. The gate insulating film 17 is formed between the pair of electrodes 21 and 22 and the gate insulating film 17. The low resistance regions 20a and 20b have high electrical conductivity and therefore form a pair of electrodes with the oxide semiconductor film 18. It is possible to reduce the contact resistance with the electrodes 21 and 22, thereby increasing the on-current of the transistor. It is possible to do so.

[0159] The pair of electrodes 21 and 22 are made of the conductive material that easily bonds with oxygen, titanium nitride, and nitrogen. Alternatively, the layer structure may be a laminate structure with a conductive material that is difficult to bond with oxygen, such as tantalum chloride or ruthenium. By using such a layered structure, the oxide insulating film 23 is In this way, it is possible to prevent the pair of electrodes 21 and 22 from being oxidized, and the pair of electrodes 21 and 22 can be highly It is possible to suppress the development of resistance.

[0160] <Modification 4: Oxide Semiconductor Film> In the method for manufacturing the transistor 50 described in this embodiment, In this embodiment, a compound produced by a reaction of the oxide semiconductor film 18 can be provided. 5 is an enlarged view of the oxide semiconductor film 18 and its surroundings in the transistor 50 in FIG. do.

[0161] For example, as shown in FIG. 5A, an oxide semiconductor film 18 is formed on the back channel side thereof. A compound 18c can be provided by reacting the semiconductor film 18. The compound 18c is After forming a pair of electrodes 21 and 22, TMAH (Tetramethylammonium hydroxide) Alkaline solutions such as phosphoric acid, nitric acid, hydrofluoric acid, The oxide semiconductor film 18 is exposed to an acidic solution such as hydrochloric acid, sulfuric acid, acetic acid, or oxalic acid. It is possible.

[0162] In this process, a part of the oxide semiconductor film 18 is etched and the upper The oxide semiconductor film 18 reacts with the alkaline solution and the acidic solution, and a reaction product remains. In-Ga oxide, In-M-Zn oxide (M is Al, Ti, Ga, Y, Zr, La, C In the case where the oxide semiconductor film 18 is formed of In (indium oxide) contained in the SiO2 is preferentially removed, so Ga or In this case, a compound 18c is formed in which the proportion of M is higher than that in the oxide semiconductor film 18.

[0163] Compound 18c, which has a high ratio of Ga or M compared to In, is characterized by Al, Ti, and Ga. , Y, Zr, La, Ce, Nd or Hf in a higher atomic ratio than In. Since it is possible to block impurities from the outside, the impurities can be prevented from moving from the outside to the oxide semiconductor film 18. As a result, it is possible to reduce the amount of impurities that are introduced into the transistor with less fluctuation in threshold voltage. It is possible to fabricate a transistor.

[0164] In addition, the etching residue between the pair of electrodes 21 and 22 is removed by this treatment. As a result, the occurrence of leakage current flowing between the pair of electrodes 21 and 22 can be suppressed. It is possible.

[0165] In addition, as shown in FIG. 5B, a compound 18d is provided on the side surface of the oxide semiconductor film 18. The compound 18d can be obtained by dissolving the compound 18d in a TMAH solution or the like when forming the oxide semiconductor film 18. Alkaline solutions, acids such as phosphoric acid, nitric acid, hydrofluoric acid, hydrochloric acid, sulfuric acid, acetic acid, and oxalic acid The insulating layer can be formed by wet etching using a solution having a high molecular weight. A dry etching process is performed using boron trichloride gas and chlorine gas as etching gas. Alternatively, the oxide semiconductor film 18 can be formed by Then, the oxide semiconductor film 18 is exposed to the above solution to form a compound 18d. do.

[0166] Compound 18d, like compound 18c, has a higher ratio of Ga or M compared to In. Therefore, compound 18d is capable of shielding impurities from the outside, and thus is It is possible to reduce the amount of impurities that move from the oxide semiconductor film 18 to the oxide semiconductor film 18. Therefore, it is possible to manufacture a transistor with a small fluctuation in voltage.

[0167] <Modification 5: Regarding Oxide Semiconductor Film> In the method for manufacturing the transistor 50 described in this embodiment, After the formation of the oxide semiconductor film 18, the oxide semiconductor film 18 is exposed to plasma generated in an oxygen atmosphere to form an oxide semiconductor Oxygen can be supplied to the film 18. The oxidizing atmosphere can be oxygen, ozone, dinitrogen monoxide, etc. In the plasma treatment, the atmosphere is oxygen, nitrogen dioxide, etc. It is preferable to expose the oxide semiconductor film 18 to plasma generated without applying a bias. As a result, oxygen can be supplied to the oxide semiconductor film 18 without damaging it. As a result, the amount of oxygen vacancies in the oxide semiconductor film 18 can be reduced. The etching process removes impurities, such as fluorine and chlorine, remaining on the surface of the oxide semiconductor film 18. It is possible to remove halogens, etc. Also, the plasma treatment is not heated to 300°C or higher. It is preferable to perform the treatment while keeping the oxygen in the plasma and the hydrogen contained in the oxide semiconductor film 18 bonded to each other. Since the substrate is heated, the water is released from the oxide semiconductor film 18. As a result, the amount of hydrogen and water contained in the oxide semiconductor film 18 can be reduced.

[0168] The structures and methods described in this embodiment may be used in conjunction with structures and methods described in other embodiments and examples. and the like.

[0169] (Embodiment 2) In this embodiment, the number of defects in the oxide semiconductor film is further reduced compared to that in the first embodiment. A semiconductor device having a transistor capable of implementing the above-mentioned method will be described with reference to the drawings. The transistor described in this embodiment has a structure similar to that of the transistor in Embodiment 1, in which an oxide semiconductor film and an oxide The difference is that it has a multilayer film having an oxide in contact with a nitride semiconductor film.

[0170] FIG. 6A and FIG. 6B are a top view and a cross-sectional view of a transistor 60 included in the semiconductor device. 6(B) is a cross-sectional view of the transistor 60 taken along dashed line AB in FIG. 6(A). In FIG. 6A, the configuration of the substrate 11 and the transistor 60 is shown in FIG. A part of the element (for example, the gate insulating film 17), the oxide insulating film 23, the oxide insulating film 24, the nitride The insulating film 25 and other parts are omitted.

[0171] The transistor 60 shown in FIG. 6A and FIG. 6B has a gate The multilayer film 2 overlaps the gate electrode 15 via the gate insulating film 17. 0 and a pair of electrodes 21 and 22 in contact with the multilayer film 20. On the multilayer film 20 and the pair of electrodes 21 and 22, an oxide insulating film 23, an oxide insulating film 24, A protective film 26 made of a nitride insulating film 25 is formed.

[0172] In the transistor 60 described in this embodiment, the multilayer film 20 includes the oxide semiconductor film 18 and The multilayer film 20 has a two-layer structure including the oxide semiconductor film 1 and the oxide film 19. A part of the multilayer film 20 functions as a channel region. A film 23 is formed, and an oxide insulating film 24 is formed so as to contact the oxide insulating film 23. That is, the oxide film 19 is provided between the oxide semiconductor film 18 and the oxide insulating film 23. It is being done.

[0173] The oxide film 19 is an oxide film composed of one or more elements that constitute the oxide semiconductor film 18. The oxide film 19 is composed of one or more elements that constitute the oxide semiconductor film 18. Therefore, interface scattering occurs at the interface between the oxide semiconductor film 18 and the oxide film 19. Therefore, the movement of carriers is not hindered at the interface, and the transistor The field effect mobility is increased.

[0174] The oxide film 19 is typically made of In-Ga oxide, In-Zn oxide, In-M-Zn oxide (M is Al, Ti, Ga, Y, Zr, La, Ce, Nd or Hf), and The energy of the bottom of the conduction band is closer to the vacuum level than that of the oxide semiconductor film 18. The energy of the lower end of the conduction band of the oxide semiconductor film 18 is The difference between the energy and the potential is 0.05 eV or more, 0.07 eV or more, 0.1 eV or more, or 0.15 eV or more and 2 eV or less, 1 eV or less, 0.5 eV or less, or 0.4 eV or less That is, the difference between the electron affinity of the oxide film 19 and the electron affinity of the oxide semiconductor film 18 is 0. 05 eV or more, 0.07 eV or more, 0.1 eV or more, or 0.15 eV or more and 2 e V or less, 1 eV or less, 0.5 eV or less, or 0.4 eV or less.

[0175] As the oxide film 19, Al, Ti, Ga, Y, Zr, La, Ce, Nd or Hf is added to the By having a higher atomic ratio than n, the following effects may be obtained: (1) Oxide film 19 (2) To decrease the electron affinity of the oxide film 19. (3) (4) Blocking impurities from the outside. (5) Higher insulating properties compared to the oxide semiconductor film 18. 5) Al, Ti, Ga, Y, Zr, La, Ce, Nd, and Hf have strong bonding strength with oxygen. Because they are metallic elements, Al, Ti, Ga, Y, Zr, La, Ce, Nd or Hf are added to In By having a higher atomic ratio, oxygen deficiency is less likely to occur.

[0176] When the oxide film 19 is an In-M-Zn oxide film, the sum of In and M is 100 atom. When expressed as mic%, the atomic ratio of In and M is preferably 50 atomic % In. less than 50 atomic %, M is 50 atomic % or more, and more preferably In is less than 25 atomic %. , M is 75 atomic% or more.

[0177] The oxide semiconductor film 18 and the oxide film 19 are In-M-Zn oxide films (M is Al, In the case of Ti, Ga, Y, Zr, La, Ce, Nd or Hf, compared with the oxide semiconductor film 18 In comparison, M (Al, Ti, Ga, Y, Zr, La, Ce, Nd, or Hf) is large, and typically, the atomic ratio of the above atoms contained in the oxide semiconductor film 18 is The number of atoms is at least 1.5 times, preferably at least 2 times, and more preferably at least 3 times higher than that of It is a ratio.

[0178] The oxide semiconductor film 18 and the oxide film 19 are In-M-Zn oxide films (M is Al, In the case of Ti, Ga, Y, Zr, La, Ce, Nd or Hf, the oxide film 19 is In:M Zn=x1:y1:z1 [atomic ratio], and the oxide semiconductor film 18 is In:M:Zn=x2: When y2:z2 is the atomic ratio, y1 / x1 is greater than y2 / x2, and preferably, y1 / x1 is 1.5 times or more larger than y2 / x2. More preferably, y1 / x1 is y 2 / x2, and more preferably, y1 / x1 is 3 times larger than y2 / x2. In this case, when y2 is equal to or larger than x2 in the oxide semiconductor film, This is preferable because it can provide stable electrical characteristics to a transistor using a conductor film. When 2 is three times or more of x2, the field-effect mobility of the transistor including the oxide semiconductor film is Therefore, it is preferable that y2 is less than three times x2.

[0179] The oxide semiconductor film 18 is an In-M-Zn oxide film (wherein M is Al, Ti, Ga, Y, Zr, or L). a, Ce, Nd or Hf), the sintering agent used to deposit the In-M-Zn oxide film The atomic ratio of the metal elements in the sputtering target preferably satisfies In≧M and Zn≧M. The atomic ratio of the metal elements in such a sputtering target is preferably In:M: Preferred are Zn=1:1:1 and In:M:Zn=3:1:2.

[0180] The oxide film 19 is an In-M-Zn oxide film (where M is Al, Ti, Ga, Y, Zr, La, C e, Nd or Hf), the sputtering method used to deposit the In-M-Zn oxide film The atomic ratio of the metal elements in the target is M>In, Zn>0.5×M, and further Zn>M. It is preferable that the atomic ratio of the metal elements in such a sputtering target and Then, In:Ga:Zn=1:3:2, In:Ga:Zn=1:3:4, In:Ga:Z n=1:3:5, In:Ga:Zn=1:3:6, In:Ga:Zn=1:3:7, In :Ga:Zn=1:3:8, In:Ga:Zn=1:3:9, In:Ga:Zn=1:3 :10, In:Ga:Zn=1:6:4, In:Ga:Zn=1:6:5, In:Ga: Zn=1:6:6, In:Ga:Zn=1:6:7, In:Ga:Zn=1:6:8, I Preferred are n:Ga:Zn=1:6:9 and In:Ga:Zn=1:6:10.

[0181] The atomic ratios of the oxide semiconductor film 18 and the oxide film 19 are each calculated by subtracting the above error from the atomic ratios. This includes a variation of ±20% in the atomic ratio.

[0182] The oxide film 19 is formed on the oxide semiconductor film 18 when the oxide insulating film 24 is formed later. It also functions as a membrane to mitigate damage to the skin.

[0183] The thickness of the oxide film 19 is 3 nm or more and 100 nm or less, preferably 3 nm or more and 50 nm or less. Below.

[0184] Similarly to the oxide semiconductor film 18, the oxide film 19 may have, for example, a non-single crystal structure. The non-single crystal structure is, for example, CAAC-OS (C Axis Aligned C crystalline oxide semiconductor), polycrystalline structure, see below The crystal structure may be microcrystalline or amorphous.

[0185] The oxide film 19 may have, for example, an amorphous structure. The oxide semiconductor film having an amorphous structure is, for example, The atomic arrangement is disordered and does not have any crystalline components. Alternatively, an oxide film having an amorphous structure is, for example, For example, it has a completely amorphous structure and does not have any crystalline parts.

[0186] Note that the oxide semiconductor film 18 and the oxide film 19 form an amorphous structure region and a microcrystalline structure region. A mixture of two or more of the following structures: The mixed film may have an amorphous structure, a microcrystalline structure, a polycrystalline structure, or a mixture of the amorphous and microcrystalline structures. The structure has two or more regions, either a region of CAAC-OS structure or a region of single crystal structure. In addition, the mixed film may have regions with an amorphous structure, a microcrystalline structure, a polycrystalline structure, etc. A stack of two or more regions of the following structure: a region of a crystalline structure, a region of a CAAC-OS structure, and a region of a single crystal structure It may have a structure.

[0187] Here, the oxide film 19 is provided between the oxide semiconductor film 18 and the oxide insulating film 23. Therefore, between the oxide film 19 and the oxide insulating film 23, the oxide film 19 is not oxidized due to impurities and defects. Even if a trap state is formed by the oxide semiconductor film 18, there is no distance between the trap state and the oxide semiconductor film 18. As a result, electrons flowing through the oxide semiconductor film 18 are less likely to be captured by the trap states. It is possible to increase the on-current of the transistor and also to improve the field effect mobility. In addition, when an electron is captured in the trap level, the electron is transferred to a negative fixed charge. As a result, the threshold voltage of the transistor changes. However, since there is a gap between the oxide semiconductor film 18 and the trap states, It is possible to reduce the trapping of electrons in the semiconductor device, and thus the variation in the threshold voltage can be reduced. do.

[0188] In addition, the oxide film 19 can block impurities from the outside. It is possible to reduce the amount of impurities that move to the oxide semiconductor film 18. For these reasons, the impurity concentration in the oxide semiconductor film 18 is In addition, the amount of oxygen vacancy can be reduced.

[0189] The oxide semiconductor film 18 and the oxide film 19 are not simply laminated but are continuously connected to each other. In this case, the energy of the bottom of the conduction band changes continuously between the layers. In other words, defects such as trap centers and recombination centers are created at the interfaces of each film. The stacked structure is designed so that there are no impurities that would create a level. When impurities are present between the compound semiconductor film 18 and the oxide film 19, the energy bands are disjointed. Continuity is lost, and carriers are trapped or recombined at the interface and disappear.

[0190] To form continuous junctions, a multi-chamber deposition system equipped with a load lock chamber is required. Each film is laminated in succession using a sputtering device without exposing it to the air. Each chamber in the sputtering apparatus is required for the oxide semiconductor film. In order to remove impurities such as water as much as possible, an adsorption type vacuum pump such as a cryopump is used. High vacuum pump (5×10 -7 Pa~1×10 -4 It is preferable to use a temperature of up to about 10 Pa. Alternatively, a turbo molecular pump and cold trap can be combined to separate the chamber from the exhaust system. It is preferable to prevent the backflow of gases into the bar, especially gases containing carbon or hydrogen. stomach.

[0191] As shown in FIG. 6C and FIG. 6D, a transistor 65 is formed with a gate insulating film 17 interposed therebetween. The multilayer film 34 overlaps the gate electrode 15, and the pair of electrodes 21 and 22 contact the multilayer film 34. may have the following structure:

[0192] The multilayer film 34 includes an oxide film 31, an oxide semiconductor film 18, and an oxide film 19. That is, The multilayer film 34 has a three-layer structure. The oxide semiconductor film 18 functions as a channel region. do.

[0193] In addition, the gate insulating film 17 and the oxide film 31 are in contact with each other. An oxide film 31 is provided between the semiconductor film 18 .

[0194] The multilayer film 34 and the oxide insulating film 23 are in contact with each other. That is, the oxide semiconductor film 18 and the oxide insulating film 23 are in contact with each other. 19 are provided.

[0195] The oxide film 31 may be formed by using a material and a method similar to those of the oxide film 19 shown in the first embodiment. There can be.

[0196] The oxide film 31 is preferably thinner than the oxide semiconductor film 18. By making the thickness of the transistor 1 nm or more and 5 nm or less, and preferably 1 nm or more and 3 nm or less, It is possible to reduce the amount of variation in the threshold voltage of the transistor.

[0197] When the oxide film 19 is an In-M-Zn oxide, the sum of In and M is 100a. When the atomic percentage of In and M is 50 atomic %, the atomic ratio of In and M is preferably 50 atomic %. c%, M is 50 atomic % or more, and more preferably In is 25 atomic % and M is 75 atomic% or more.

[0198] In the transistor described in this embodiment, Therefore, the oxide film 19 is provided between the oxide film 19 and the oxide insulating film 23. In this case, even if a trap level is formed by impurities and defects, the trap level and the oxide semiconductor There is a gap between the oxide semiconductor film 18 and the conductive film 18. As a result, the electrons flowing through the oxide semiconductor film 18 This makes it possible to increase the on-state current of the transistor. In addition, when an electron is captured in the trap level, The electrons become negative fixed charges. As a result, the threshold voltage of the transistor However, there is a gap between the oxide semiconductor film 18 and the trap level. Therefore, it is possible to reduce the capture of electrons at the trap level, and the threshold voltage Fluctuations can be reduced.

[0199] In addition, the oxide film 19 can block impurities from the outside. It is possible to reduce the amount of impurities that move to the oxide semiconductor film 18. For these reasons, the impurity concentration in the oxide semiconductor film 18 is In addition, the amount of oxygen vacancy can be reduced.

[0200] In addition, an oxide film 31 is provided between the gate insulating film 17 and the oxide semiconductor film 18. In other words, the oxide film 19 is provided between the oxide semiconductor film 18 and the oxide insulating film 23. Therefore, the concentration of silicon and carbon in the vicinity of the interface between the oxide film 31 and the oxide semiconductor film 18, and the concentration of oxygen The concentration of silicon or carbon in the oxide semiconductor film 18, or the concentration of the oxide film 19 and the oxide semiconductor film As a result, the concentration of silicon and carbon in the vicinity of the interface with 18 can be reduced. In the multilayer film 34, the absorption coefficient derived by the constant photocurrent measurement method is 1×10 -3 / cm Less than 1 x 10 -4 / cm, and the localized levels are extremely low.

[0201] The transistor 65 having such a structure is formed by a multilayer film 34 including an oxide semiconductor film 32. Since there are very few defects in the Typically, it is possible to increase the on-current and improve the field effect mobility. Threshold voltage fluctuations during BT stress testing and optical BT stress testing, which are examples of testing Small quantity and high reliability.

[0202] <Band structure of transistor> Next, the band structure of the multilayer film 20 provided in the transistor 60 shown in FIG. This will be explained with reference to FIG.

[0203] Here, as an example, the oxide semiconductor film 18 has an energy gap of 3.15 eV. The oxide film 19 is made of In-Ga-Zn oxide with an energy gap of 3.5e The energy gap is measured using a spectroscopic ellipsometer. (HORIBA JOBIN YVON UT-300) can be used for measurement. do.

[0204] The energy difference between the vacuum level and the top of the valence band of the oxide semiconductor film 18 and the oxide film 19 (ion The electron potentials (also called electron-electron potentials) are 8 eV and 8.2 eV, respectively. The energy difference between the potential and the top of the valence band was determined by ultraviolet photoelectron spectroscopy (UPS). Photoelectron Spectroscopy (PHI) equipment It can be measured using ersaProbe.

[0205] Therefore, the vacuum level and the energy of the conduction band minimum of the oxide semiconductor film 18 and the oxide film 19 are The electron affinity difference (also called electron affinity) is 4.85 eV and 4.7 eV, respectively.

[0206] FIG. 7A shows a schematic diagram of a part of the band structure of the multilayer film 20. The case where a silicon oxide film is provided in contact with the film 20 will be described. EcI1 indicates the energy of the conduction band minimum of the silicon oxide film, and EcS1 indicates the energy of the oxide semiconductor film. EcS2 is the energy of the conduction band minimum of the oxide film 19. EcI2 indicates the energy of the bottom of the conduction band of the silicon oxide film. corresponds to the gate insulating film 17 in FIG. 1B, and EcI2 corresponds to , which corresponds to the oxide insulating film 23.

[0207] As shown in FIG. 7A, in the oxide semiconductor film 18 and the oxide film 19, The energy of changes smoothly without any barriers. In other words, it changes continuously. This is because the multilayer film 20 contains elements common to the oxide semiconductor film 18 and is an oxide A mixed layer is formed between the semiconductor film 18 and the oxide film 19 by the mutual transfer of oxygen. It can be said that this is for the purpose.

[0208] As shown in FIG. 7A, the oxide semiconductor film 18 of the multilayer film 20 serves as a well. In the transistor using 0, a channel region is formed in the oxide semiconductor film 18. In addition, since the energy of the conduction band minimum of the multilayer film 20 changes continuously, It can also be said that the oxide semiconductor film 18 and the oxide film 19 are in continuous junction.

[0209] As shown in FIG. 7A, in the vicinity of the interface between the oxide film 19 and the oxide insulating film 23, Although a trap level due to impurities or defects may be formed, the oxide film 19 is provided. This can keep the oxide semiconductor film 18 away from the trap levels. When the energy difference between EcS1 and EcS2 is small, the electrons in the oxide semiconductor film 18 The electron can exceed the energy difference and reach the trap level. The electron is captured in the trap level. This generates a negative charge at the interface of the insulating film, and the threshold voltage of the transistor increases in the positive direction. Therefore, the energy difference between EcS1 and EcS2 is 0.1 eV If the value is set to 0.15 eV or more, preferably 0.15 eV or more, the fluctuation in the threshold voltage of the transistor is reduced. This is preferable since it results in stable electrical characteristics.

[0210] FIG. 7B is a schematic diagram showing a part of the band structure of the multilayer film 20. In this example, a silicon oxide film is provided in contact with the multilayer film 20. In addition, EcI1 shown in FIG. 7B is the minimum conduction band of the silicon oxide film. EcS1 represents the energy of the bottom of the conduction band of the oxide semiconductor film 18, and E cI2 indicates the energy of the bottom of the conduction band of the silicon oxide film. 1B), corresponds to the gate insulating film 17, and EcI2 corresponds to the oxide insulating film It corresponds to the membrane 23 .

[0211] In the transistor shown in FIG. 6B, the multilayer film 20 is formed when the pair of electrodes 21 and 22 are formed. On the other hand, the upper part of the oxide semiconductor film 1, i.e., the oxide film 19, may be etched. On the upper surface of the substrate 8, a mixed layer of the oxide semiconductor film 18 and the oxide film 19 is formed during the formation of the oxide film 19. This may be the case.

[0212] For example, the oxide semiconductor film 18 is an In- Ga-Zn oxide, or In-Ga-Z with In:Ga:Zn=3:1:2 [atomic ratio] n oxide as a sputtering target, and The film 19 is an In-Ga-Zn oxide having an atomic ratio of In:Ga:Zn=1:3:2. In-Ga-Zn oxide with an atomic ratio of In:Ga:Zn=1:6:4 was sputtered. In the case of an oxide film formed using a fluorine-containing target, the oxide semiconductor film 18 is more likely to have a high oxide content than the oxide semiconductor film 18. Since the Ga content of the film 19 is high, a GaOx layer or an oxide layer is formed on the upper surface of the oxide semiconductor film 18. A mixed layer containing more Ga than the compound semiconductor film 18 can be formed.

[0213] Therefore, even when the oxide film 19 is etched, the EcS1 side of the EcI2 The energy of the conduction band edge of the GaN- ... be.

[0214] When the band structure shown in FIG. 7B is obtained, when observing the cross section of the channel region, The multilayer film 20 may appear to be composed of only the oxide semiconductor film 18. In reality, a mixture containing more Ga than the oxide semiconductor film 18 is formed on the oxide semiconductor film 18. Since a mixed layer is formed, the mixed layer can be regarded as a 1.5 layer. When the elements contained in the multilayer film 20 are measured by, for example, EDX analysis, the mixed layer is This can be confirmed by analyzing the composition above the oxide semiconductor film 18. For example, The composition in the upper portion of the oxide semiconductor film 18 has a higher Ga content than the composition in the oxide semiconductor film 18. This can be confirmed by the configuration.

[0215] (Embodiment 3) In this embodiment, compared with Embodiments 1 and 2, defects in an oxide semiconductor film are The present invention provides a transistor that can further reduce the amount of semiconductor material and increase the on-state current of the transistor. A semiconductor device according to the present invention will be described with reference to the drawings. In comparison with the first embodiment, an oxide insulating film 23 is formed between the pair of electrodes 21 and 22. The difference is that the present embodiment uses the first embodiment for explanation, but This is preferably applicable to the second embodiment.

[0216] FIG. 9 shows a top view and a cross-sectional view of a transistor 70 included in the semiconductor device. A top view of the rotor 70 is shown in FIG. 9(A). In FIG. 9(A), a cross-sectional view between the dashed line AB is shown. FIG. 9(B) shows the cross section between dashed lines CD and FIG. 9(C) shows the cross section between dashed lines CD and CD in FIG. For clarity, the substrate 11 and some of the components of the transistor 70 (e.g., the gate insulator The insulating film 17), the oxide insulating film 23, the oxide insulating film 24, the nitride insulating film 25, etc. are omitted. .

[0217] The transistor 70 is different from the transistor 50 in that the pair of electrodes 21 and 22 are made of oxide semiconductor. The difference is that the transistor is surrounded by a conductor film 18a and an oxide film 19a. 70 is a film formed by stacking an oxide semiconductor film 18a on the gate insulating film 17 and an oxide semiconductor film 18 a pair of electrodes 21 and 22 provided on the oxide semiconductor film 18a and the pair of electrodes 21; 22 and an oxide film 19a provided on the substrate 22.

[0218] The transistor 70 has a pair of electrodes 21 and 22 in contact with the oxide semiconductor film 18a. Therefore, compared with the transistor 60, the oxide semiconductor film 18a and the pair of electrodes 21 and 22 This transistor has a low contact resistance and an improved on-current compared to the transistor 60.

[0219] In addition, the transistor 70 has a pair of electrodes 21 and 22 in contact with the oxide semiconductor film 18a. Therefore, the contact resistance between the oxide semiconductor film 18a and the pair of electrodes 21 and 22 is not increased. In this way, the oxide film 19a can be made thicker. The trap level is generated due to plasma damage during the deposition or contamination of the constituent elements of the protective film 26. Therefore, it is possible to prevent the oxide semiconductor film 18a from being formed in the vicinity of the interface between the oxide semiconductor film 18a and the oxide film 19a. In other words, the transistor 70 achieves both an improvement in on-state current and a reduction in the amount of variation in the threshold voltage. It is possible.

[0220] A method for manufacturing the transistor 70 will be described with reference to FIG. Then, a gate electrode and a gate insulating film 17 are formed on the substrate 11 .

[0221] Next, an oxide semiconductor film 28 that will later become the oxide semiconductor film 18a is formed. The electrodes 21 and 22 are formed. Next, the oxide film 29 that will later become the oxide film 19a is formed ( See Figure 10(A).

[0222] The oxide semiconductor film 28 is formed using a material similar to that of the oxide semiconductor film 18 described in Embodiment 1. The pair of electrodes 21 and 22 may be formed in the same manner as in FIG. The pair of electrodes 21 and 22 are formed on the oxide semiconductor film 28. The oxide film 29 is formed using the same material and method as the oxide film 19 in Embodiment 1. It can be used appropriately.

[0223] Next, the oxide semiconductor film 28 and the oxide film 29 are each partially etched to form oxide semiconductor films. A multilayer film 20 having an oxide semiconductor film 18a and an oxide film 19a is formed (see FIG. 10(B)). (See FIG. 13.) The etching is performed by photolithography on the oxide film that will become the oxide film 29. This can be achieved by forming a mask in a process and then performing etching using the mask. In addition, since the oxide semiconductor film 28 and the oxide film 29 are simultaneously etched, The ends of the solid film 18a and the oxide film 19a are substantially aligned.

[0224] Next, a protective film is formed so as to cover the gate insulating film 17, the multilayer film 20, and the pair of electrodes 21 and 22. A protective film 26 is formed (see FIG. 10(C)). The protective film 26 is formed in the same manner as in the first embodiment. In addition, in the method for manufacturing the transistor 70, Heat treatment can be carried out by referring to the above appropriately.

[0225] In addition, the oxide semiconductor film 18a is formed by etching to form the pair of electrodes 21 and 22. Defects such as oxygen vacancies may occur, increasing the carrier density, so an oxide film29 is formed. Before the formation of the oxide semiconductor film 18a, the oxide semiconductor film 18a is exposed to plasma generated in an oxygen atmosphere. It is preferable to supply oxygen to the oxide semiconductor film 18a. In the transistor 70, a trap quasi-electrode is formed in the vicinity of the interface between the oxide semiconductor film 18a and the oxide film 19a. It is possible to suppress the formation of potentials, and thus to reduce the amount of variation in the threshold voltage. In the transistor 70, the multilayer film 20 is formed by flowing in the vicinity of the side surface of the oxide semiconductor film 18a. This can reduce the leakage current and suppress an increase in the off-state current.

[0226] In addition, the multilayer film 20 is damaged by the etching for forming the pair of electrodes 21 and 22. As a result, oxygen vacancies occur on the back channel side of the multilayer film 20, but the oxide insulating film 24 A part of the oxygen contained in the oxide semiconductor film 18a is moved to the oxide semiconductor film 18a. This makes it possible to compensate for the defect, thereby improving the reliability of the transistor 70. It is possible.

[0227] <Variation 1> In the transistor 70 shown in this embodiment, the multilayer film 20 and the pair of electrodes 21 and 22 The laminated structure can be appropriately changed. For example, a modified example shown in FIG. The transistor can be used.

[0228] The transistor illustrated in FIG. 11 has a structure similar to that of the transistor 60 in that the oxide semiconductor film 18b and the The difference is that the oxide semiconductor film 18b and the oxide film 19b are formed in different steps. The difference is that the portion is covered with a pair of electrodes 21 and 22 and is not in contact with the oxide film 19b.

[0229] The transistor shown in FIG. 11 has a pair of electrodes 21 and 22 and Since the oxide semiconductor film 18b is in direct contact with the multilayer film 20, the multilayer film 20 and the pair of electrodes 21 and 22 This transistor has low contact resistance and an improved on-state current compared to the transistor 50.

[0230] In addition, in the transistor illustrated in FIG. 11, a pair of electrodes 21 and 22 are formed of an oxide semiconductor film 18b. Since the multilayer film 20 is in direct contact with the pair of electrodes 21 and 22, the contact resistance between the multilayer film 20 and the pair of electrodes 21 and 22 is not increased. In addition, the oxide film 19b can be thickened. Traps that occur due to plasma damage during the etching process or due to the inclusion of constituent elements of the protective film 26. The formation of a level near the interface between the oxide semiconductor film 18b and the oxide film 19b can be suppressed. In other words, it is possible to improve the on-current and reduce the fluctuation in the threshold voltage at the same time.

[0231] The structures and methods described in this embodiment may be used in conjunction with structures and methods described in other embodiments and examples. and the like.

[0232] (Embodiment 4) In this embodiment, a transistor having a structure different from those in Embodiments 1 to 3 will be described. 12. A transistor 80 described in this embodiment includes an oxide semiconductor film The semiconductor device is characterized in that it has a plurality of gate electrodes opposed to each other via a gate electrode.

[0233] A transistor 80 shown in FIG. 12 has a gate electrode 15 provided on a substrate 11 . In addition, a gate insulating film 17 formed on the substrate 11 and the gate electrode 15 and a gate insulating film 1 The oxide semiconductor film 18 overlapping the gate electrode 15 through the gate electrode 7 and the oxide semiconductor film 18 contacting the gate electrode 15 through the gate electrode 7 are The gate insulating film 17, the oxide semiconductor film 18, and the pair of electrodes 21 and 22 are connected to each other. On the pair of electrodes 21 and 22, an oxide insulating film 23, an oxide insulating film 24, and a nitride insulating film are formed. A protective film 26 is formed by the insulating film 25. In addition, the oxide semiconductor It has a gate electrode 61 overlapping the film 18 .

[0234] The gate electrode 61 can be formed in the same manner as the gate electrode 15 .

[0235] In the transistor 80 of this embodiment, a gate electrode 81 faces a gate electrode 82 with an oxide semiconductor film 18 interposed therebetween. The gate electrode 15 and the gate electrode 61 are applied with different potentials. By applying this voltage, the threshold voltage of the transistor 80 can be controlled.

[0236] In addition, by using the oxide semiconductor film 18 in which the amount of oxygen vacancies is reduced, In addition, the variation in threshold voltage is small, and the reliability is high. This results in a high-performance transistor.

[0237] In addition, the configuration and method described in this embodiment may be applied to configurations and methods described in other embodiments and examples. and the like.

[0238] (Embodiment 5) In this embodiment, a transistor having a structure different from those in Embodiments 1 to 4 will be described. This will be explained with reference to FIG.

[0239] In this embodiment, compared with Embodiments 1 to 4, defects in an oxide semiconductor film can be reduced. A semiconductor device having a transistor capable of further reducing the amount of The transistor described in this embodiment will be described in the following. In contrast, the back channel side of the oxide semiconductor film 18 is covered with a protective film, and The difference is that the substrate is not exposed to plasma generated in the etching process for forming the substrate.

[0240] FIG. 13 illustrates a top view and a cross-sectional view of a transistor 90 included in the semiconductor device. FIG. 13(A) is a top view of a transistor 90, and FIG. 13(B) is a top view of a transistor 90 along the dashed line A- 13(C) is a cross-sectional view taken along dashed line CD in FIG. 13(A). In FIG. 13A, for the sake of clarity, the substrate 11 and some of the components of the transistor 90 are shown. portion (for example, gate insulating film 17), oxide insulating film 23, oxide insulating film 24, nitride insulating film 25 etc. are omitted.

[0241] A transistor 90 shown in FIG. 13 has a gate electrode 15 provided on a substrate 11 . In addition, a gate insulating film 17 formed on the substrate 11 and the gate electrode 15 and a gate insulating film 1 The gate electrode 15 is overlapped with the oxide semiconductor film 18 via the gate insulating film 7. An oxide insulating film 23, an oxide insulating film 24, and a nitride insulating film 25 are formed on the oxide semiconductor film 17 and the oxide semiconductor film 18. A protective film 26 is formed by an insulating film 25, and a film is formed on the protective film 26. The second electrode 21b and the second electrode 22b are connected to the oxide semiconductor film 18.

[0242] Next, a method for manufacturing the transistor 90 will be described.

[0243] As in the first embodiment, a gate electrode 15 is formed on a substrate 11. A gate insulating film 17 is formed on the electrode 15. Next, an oxide semiconductor film 1 is formed on the gate insulating film 17. Form 8.

[0244] Next, in the same manner as in the first embodiment, 280 After forming the oxide insulating film 23 while heating at a temperature of 0.5 to 400° C., the oxide insulating film 24 and After the oxide insulating film 24 is formed, a heat treatment is performed. Part of the oxygen contained in the oxide insulating film 24 is supplied to the oxide semiconductor film 18.

[0245] Next, a part of each of the oxide insulating film 23, the oxide insulating film 24, and the nitride insulating film 25 is An opening is formed by etching to expose a part of the oxide semiconductor film 18. A pair of electrodes 21b, 22b in contact with the organic semiconductor film 18 are formed in the same manner as in the first embodiment.

[0246] In this embodiment, when the pair of electrodes 21b and 22b are etched, the oxide semiconductor Since the membrane 18 is covered with the protective film 26, the etching for forming the pair of electrodes 21b, 22b is As a result of this, the oxide semiconductor film 18, particularly the back channel region of the oxide semiconductor film 18, is damaged. Furthermore, the oxide insulating film 24 contains more oxygen than the stoichiometric composition. The oxide insulating film 24 is formed of an oxide insulating film containing a large amount of oxygen. A part of the oxygen vacancies in the oxide semiconductor film 18 is transferred to the oxide semiconductor film 18. As a result, the amount of oxygen vacancies in the oxide semiconductor film 18 can be reduced. It is possible.

[0247] Through the above steps, defects contained in the oxide semiconductor film 18 can be reduced. The reliability of the transistor 90 can be improved.

[0248] (Embodiment 6) In this embodiment, a transistor having a structure different from those in Embodiments 1 to 5 will be described. This will be explained with reference to FIG.

[0249] In this embodiment, compared with Embodiments 1 to 4, defects in an oxide semiconductor film can be reduced. A semiconductor device having a transistor capable of further reducing the amount of The transistor described in this embodiment is a transistor including an oxide semiconductor The back channel side of the conductive film 18 is covered with a protective film, and an electrode for forming a pair of electrodes is provided. The difference between the first to fourth embodiments is that the semiconductor device is not exposed to plasma generated during the etching process. different.

[0250] FIG. 14 illustrates a top view and a cross-sectional view of a transistor 100 included in the semiconductor device. The transistor 100 shown in FIG. 14 is a channel protection transistor. 14(B) is a top view of the transistor 100, and FIG. 14(B) is a diagram showing the structure between the dashed line AB in FIG. 14(A). 14(C) is a cross-sectional view taken along dashed line CD in FIG. 14A, for the sake of clarity, the substrate 11 and some of the components of the transistor 100 ( For example, the gate insulating film 17 and the like are omitted.

[0251] The transistor 100 shown in FIG. 14 has a gate electrode 15 provided on a substrate 11. In addition, a gate insulating film 17 formed on the substrate 11 and the gate electrode 15, and a gate insulating film The gate electrode 15 is overlapped with an oxide semiconductor film 18 via a gate insulating film 17. On the insulating film 17 and the oxide semiconductor film 18, an oxide insulating film 23a, an oxide insulating film 24a, and The protective film 26a is made of a nitride insulating film 25a, and the gate insulating film 17 and the oxide semiconductor film 1 8, and a pair of electrodes 21c, 22c formed on the protective film 26a.

[0252] Next, a method for manufacturing the transistor 100 will be described.

[0253] As in the first embodiment, a gate electrode 15 is formed on a substrate 11. A gate insulating film 17 is formed on the electrode 15. Next, an oxide semiconductor film 1 is formed on the gate insulating film 17. Form 8.

[0254] Next, in the same manner as in the first embodiment, 280 After forming the oxide insulating film 23 while heating at a temperature of 0.5 to 400° C., the oxide insulating film 24 and After the oxide insulating film 24 is formed, a heat treatment is performed. Part of the oxygen contained in the oxide insulating film 24 is supplied to the oxide semiconductor film 18.

[0255] Next, a part of each of the oxide insulating film 23, the oxide insulating film 24, and the nitride insulating film 25 is The oxide insulating film 23a, the oxide insulating film 24a, and the nitride insulating film 25a are formed by etching. A protective film 26a is formed.

[0256] Next, the pair of electrodes 21c and 22c in contact with the oxide semiconductor film 18 are is formed.

[0257] In this embodiment, when the pair of electrodes 21c and 22c are etched, the oxide semiconductor Since the body membrane 18 is covered with the protective film 26a, the edges forming the pair of electrodes 21c and 22c are The oxide semiconductor film 18 is not damaged by the etching. The region a is formed using an oxide insulating film containing more oxygen than the amount of oxygen required for the stoichiometric composition. As a result, part of the oxygen contained in the oxide insulating film 24a is moved to the oxide semiconductor film 18, It is possible to compensate for oxygen vacancies in the oxide semiconductor film 18. The amount of oxygen vacancies in the oxide semiconductor film 18 can be reduced.

[0258] In FIG. 14, a nitride insulating film 25a is formed as the protective film 26a. The oxide insulating film 23a and the oxide insulating film 24a may have a stacked structure. After forming the electrodes 21c and 22c, it is preferable to form the nitride insulating film 25a. As a result, it is possible to prevent hydrogen, water, and the like from entering the oxide semiconductor film 18 from the outside.

[0259] Through the above steps, defects contained in the oxide semiconductor film 18 can be reduced. The reliability of the transistor 100 can be improved.

[0260] (Embodiment 7) Various films such as the metal film, the oxide semiconductor film, and the inorganic insulating film disclosed in the above embodiments are For the CVD (Plasma Chemical Vapor Deposition) method However, it may be formed by other methods, for example, a thermal CVD method. As an example of the CVD method, MOCVD (Metal Organic Chemical Vapor Deposition) por Deposition method and ALD (Atomic Layer Deposition) method. tion) method may also be used.

[0261] Thermal CVD is a film formation method that does not use plasma, so defects can occur due to plasma damage. This has the advantage that no additional steps are required.

[0262] In the thermal CVD method, the source gas and the oxidizing agent are fed into the chamber at the same time, and the chamber is heated to atmospheric pressure. Alternatively, a film is formed by reacting the reactants near or on the substrate under reduced pressure and depositing the reactants on the substrate. You may go.

[0263] In addition, in the ALD method, the pressure inside the chamber is set at atmospheric pressure or reduced pressure, and the source gas for the reaction is The gases may be introduced into the chamber in sequence, and the film may be formed by repeating the gas introduction sequence. For example, by switching each switching valve (also called high-speed valve), two or more types of The above source gases are supplied to the chamber in order, and the first source gas is supplied to the chamber in order to prevent the mixture of the source gases. An inert gas (such as argon or nitrogen) is introduced simultaneously with or after the raw material gas. The second source gas is introduced. When an inert gas is introduced at the same time, the inert gas is It acts as a carrier gas, and even if an inert gas is introduced at the same time as the second source gas is introduced, In addition, the first source gas is discharged by evacuation instead of introducing an inert gas. After that, a second source gas may be introduced. The first source gas is adsorbed on the surface of the substrate to form a first layer. The first layer is deposited on the second layer by reacting with the second source gas introduced later. This process is repeated several times while controlling the gas introduction sequence until the desired thickness is reached. By doing so, a thin film with excellent step coverage can be formed. The thickness of the thin film is determined by the gas introduction. The thickness can be precisely adjusted by changing the number of times the sequence is repeated. This is suitable for producing miniature FETs.

[0264] Thermal CVD methods such as MOCVD and ALD have been disclosed in the embodiments described above. It is possible to form various films such as metal films, oxide semiconductor films, and inorganic insulating films. In the case of forming an nGaZnO film, trimethylindium, trimethylgallium, and Dimethyl zinc is used. The chemical formula for trimethyl indium is In(CH3)3. The chemical formula for trimethylgallium is Ga(CH3)3. The chemical formula for lead is Zn(CH3)2. Using triethylgallium (chemical formula Ga(C2H5)3) instead of methylgallium It is also possible to use diethylzinc (chemical formula Zn(C2H5)2) instead of dimethylzinc. It is also possible.

[0265] For example, when forming a hafnium oxide film using a film forming apparatus that uses ALD, the solvent and a liquid containing a hafnium precursor compound (hafnium alkoxide solution, typically tetra The raw material gas is vaporized with tetramethyl tert-butyl amide hafnium (TDMAH) as an oxidizing agent. Two types of gases are used: tetrakisdimethylamidohafnium (TDA) and ozone (O3). The chemical formula is Hf[N(CH3)2]4. Other material liquids include tetrakis(ethoxycarbonyl) (ethylmethylamido) hafnium.

[0266] For example, when forming an aluminum oxide film using an ALD deposition system, A liquid containing a catalyst and an aluminum precursor compound (e.g., trimethylaluminum (TMA)) is added. Two types of gases are used: vaporized source gas and H2O as an oxidizing agent. The chemical formula for aluminum is Al(CH3)3. Other liquid materials include Tris( Dimethylamido)aluminum, triisobutylaluminum, aluminum tris(2 ,2,6,6-tetramethyl-3,5-heptanedionate).

[0267] For example, when forming a silicon oxide film using a deposition system that uses ALD, Chlorodisilane is adsorbed onto the surface to be coated, the chlorine contained in the adsorbed matter is removed, and the oxidizing gas (O 2. Nitrous oxide (NO) radicals are supplied to react with the adsorbed material.

[0268] For example, when forming a tungsten film using an ALD deposition system, WF6 The initial tungsten film was formed by repeatedly introducing B2H6 gas and WF 6 gas and H2 gas are introduced simultaneously to form a tungsten film. Alternatively, SiH4 gas may be used.

[0269] For example, an oxide semiconductor film, such as In-Ga-Zn- When forming an O film, In(CH3)3 gas and O3 gas are introduced in sequence. Then, Ga(CH3)3 gas and O3 gas are introduced simultaneously to form a GaO layer. Then, Zn(CH3)2 and O3 gases are introduced simultaneously to form a ZnO layer. The order of these layers is not limited to this example. A mixed compound layer such as an O layer, an In-Zn-O layer, or a Ga-Zn-O layer may be formed. Instead of O3 gas, H2O gas obtained by bubbling with an inert gas such as Ar can be used. However, it is preferable to use O3 gas that does not contain H. In(CH3)3 gas is also used. Alternatively, In(C2H5)3 gas may be used. Ga(C2H5)3 gas may be used. Also, instead of In(CH3)3 gas, In( C2H5)3 gas may be used. Also, Zn(CH3)2 gas may be used.

[0270] (Embodiment 8) In this embodiment, a semiconductor device which is one embodiment of the present invention will be described with reference to drawings. Note that in this embodiment, a semiconductor device which is one embodiment of the present invention will be described using a display device as an example. do.

[0271] FIG. 15A shows an example of a semiconductor device. The semiconductor device shown in FIG. 101, a scanning line driving circuit 104, and a signal line driving circuit 106 are parallel or approximately parallel to each other. m scanning lines 107, the potentials of which are controlled by a scanning line driving circuit 104; , each are arranged in parallel or approximately in parallel, and the potentials are controlled by a signal line driving circuit 106. The pixel section 101 is arranged in a matrix. The pixel 301 is arranged parallel or approximately parallel to the scanning line 107. The capacitance lines 115 are arranged along the signal lines 109. The scanning line driver circuit 104 and the signal line driver circuit 105 may be arranged in parallel or approximately in parallel. The drive circuits 106 may be collectively referred to as a drive circuit section.

[0272] Each scanning line 107 corresponds to one of the pixels 301 arranged in m rows and n columns in the pixel section 101. The signal lines 109 are electrically connected to the n pixels 301 arranged in any one row. is m pixels 301 arranged in m rows and n columns, and m pixels 301 arranged in any one of the columns. 1. m and n are both integers of 1 or more. is n pixels 301 arranged in any one of the rows among the pixels 301 arranged in m rows and n columns. 1. Capacitor lines 115 are arranged parallel to each other along the signal line 109. In the case where the pixels 301 are arranged in m rows and n columns, any one of the pixels 301 may be arranged in a matrix of m rows and n columns. The pixel array 301 is electrically connected to m pixels 301 arranged in a column.

[0273] 15B and 15C show the structure of the pixel 301 of the display device shown in FIG. 4 shows a circuit configuration that can

[0274] The pixel 301 shown in FIG. 15B includes a liquid crystal element 132, a transistor 131_1, and a capacitor. The capacitance element 133_1 is a capacitance element.

[0275] The potential of one of the pair of electrodes of the liquid crystal element 132 is appropriately set according to the specifications of the pixel 301. The alignment state of the liquid crystal element 132 is set by the written data. A common potential (common potential) is applied to one of a pair of electrodes of the liquid crystal element 132 in each pixel 301. In addition, one of the pair of electrodes of the liquid crystal element 132 for each row of pixels 301 may be applied. may be given different potentials.

[0276] For example, the display device including the liquid crystal element 132 can be driven in a TN mode, an STN mode, or the like. Mode, VA mode, ASM (Axially Symmetric Aligned M icro-cell mode, OCB (Optically Compensated Birefringence mode, FLC (Ferroelectric Liquid id Crystal) mode, AFLC (AntiFerroelectric Li quid Crystal) mode, MVA mode, PVA (Patterned Ve Vertical Alignment) mode, IPS mode, FFS mode, or TB A (Transverse Bend Alignment) mode may be used. In addition to the above-mentioned driving method, the display device can be driven by ECB (Electro cally Controlled Birefringence) mode, PDLC( Polymer Dispersed Liquid Crystal) mode, PNL C (Polymer Network Liquid Crystal) mode, guest However, the liquid crystal element and its driving method are not limited to these. A variety of different ones can be used.

[0277] Also, a liquid crystal composition containing a liquid crystal exhibiting a blue phase and a chiral agent. The liquid crystal element may be configured by the liquid crystal that exhibits the blue phase. Since it is short and optically isotropic, alignment treatment is not required and viewing angle dependency is small.

[0278] In the pixel 301 in the mth row and the nth column, One of the electrodes is electrically connected to the signal line DL_n, and the other is a pair of electrodes of the liquid crystal element 132. The gate electrode of the transistor 131_1 is electrically connected to the other of the scan lines G L_m. The transistor 131_1 is in an on state or an off state. By this, the write control circuit 100 has a function of controlling the writing of data of the data signal.

[0279] One of a pair of electrodes of the capacitor 133_1 is connected to a wiring to which a potential is supplied (hereinafter, a capacitor line CL ) and the other is electrically connected to the other of the pair of electrodes of the liquid crystal element 132. The value of the potential of the capacitance line CL is appropriately set according to the specifications of the pixel 301. The child 133_1 has a function as a storage capacity for storing written data.

[0280] For example, in a display device having a pixel 301 shown in FIG. 15B, The pixels 301 in each row are selected in sequence, and the transistors 131_1 are turned on to supply data signals Write the data.

[0281] The pixel 301 to which the data has been written is turned off by turning off the transistor 131_1. By repeating this process row by row, an image can be displayed.

[0282] In addition, the pixel 301 shown in FIG. 15C includes a transistor 131_2 and a capacitor 133. _2, a transistor 134, and a light-emitting element 135.

[0283] One of the source electrode and the drain electrode of the transistor 131_2 is supplied with a data signal. Further, the transistor The gate electrode of 131_2 is a wiring to which a gate signal is applied (hereinafter, referred to as a scanning line GL_m). ) is electrically connected to

[0284] The transistor 131_2 is turned on or off to output the data signal. It has a function to control writing of data.

[0285] One of a pair of electrodes of the capacitor 133_2 is connected to a wiring to which a potential is applied (hereinafter, a potential supply line VL_a), and the other is electrically connected to the source electrode of the transistor 131_2 and The gate electrode is electrically connected to the other of the drain electrodes.

[0286] The capacitor 133_2 has a function as a storage capacitor for storing written data. .

[0287] One of the source electrode and the drain electrode of the transistor 134 is connected to the potential supply line VL_a. Furthermore, the gate electrode of the transistor 134 is electrically connected to the gate of the transistor 131_ The second source electrode and the second drain electrode are electrically connected to each other.

[0288] One of the anode and the cathode of the light-emitting element 135 is electrically connected to the potential supply line VL_b. The other is electrically connected to the other of the source electrode and drain electrode of the transistor 134. will be done.

[0289] The light-emitting element 135 may be, for example, an organic electroluminescence element (also called an organic EL element). However, the light emitting element 135 is not limited to this. Alternatively, an inorganic EL element made of an inorganic material may be used.

[0290] A high power supply potential VDD is applied to one of the potential supply lines VL_a and VL_b. and the other is supplied with a low power supply potential VSS.

[0291] In a display device having the pixel 301 of FIG. 15C, the scanning line driving circuit 104 The pixels 301 are sequentially selected, the transistors 131_2 are turned on, and the data of the data signal is input. Write.

[0292] The pixel 301 to which the data has been written is turned off by turning off the transistor 131_2. Furthermore, the state of the transistor 134 is changed according to the potential of the written data signal. The amount of current flowing between the source electrode and the drain electrode is controlled, and the light emitting element 135 The light is emitted with a brightness that corresponds to the flow rate. By performing this process row by row, an image can be displayed.

[0293] In this specification and the like, the term "display element," "display device having a display element," "light-emitting element," A light-emitting device, which is a device having a light-emitting element, can be used in various forms or in various Examples of a display element, a display device, a light-emitting element, or a light-emitting device include For example, EL (electroluminescence) elements (EL elements including organic and inorganic materials, organic EL elements, inorganic EL elements), LEDs (white LEDs, red LEDs, green LEDs, blue LEDs) etc.), transistors (transistors that emit light according to electric current), electron-emitting devices, liquid crystal devices , electronic ink, electrophoretic element, grating light valve (GLV), plasma display Display (PDP), MEMS (Micro Electro Mechanical Systems), Digital Micromirror Device (DMD), DMS (Digital Micro Shutter), M IRASOL (trademark), IMOD (Interference Modulation) element , piezoelectric ceramic displays, carbon nanotubes, etc., due to electromagnetic effects. Some have display media that change contrast, brightness, reflectance, transmittance, etc. An example of a display device using an electron-emitting device is an EL display. An example of a display device that has been used is a field emission display (FED) or S ED type flat panel display (SED: Surface-conduction Electrodes) Display devices using liquid crystal elements. One example is a liquid crystal display (transmissive liquid crystal display, semi-transmissive liquid crystal display, etc.). (a) Reflective LCD, Direct-view LCD, Projection LCD, etc. An example of a display device using electronic ink or electrophoretic elements is electronic paper. There are some.

[0294] An example of an EL element is a device that includes an anode, a cathode, and an EL layer sandwiched between the anode and the cathode. One example of an EL layer is a device that uses light emission (fluorescence) from singlet excitons. Those that utilize emission from triplet excitons (phosphorescence), and those that utilize emission from singlet excitons ( those that utilize fluorescence and those that utilize emission from triplet excitons (phosphorescence), Those formed by organic matter, those formed by inorganic matter, those formed by organic matter Materials made of polymeric materials, including materials made of inorganic materials and materials made of inorganic materials. , those containing low molecular weight materials, or those containing high molecular weight materials and low molecular weight materials, etc. However, there is no limitation to these, and various types of EL elements can be used. .

[0295] An example of a liquid crystal element is a device that controls the transmission or non-transmission of light by the optical modulation action of liquid crystals. The element can be constructed with a pair of electrodes and a liquid crystal layer. The optical modulation effect of liquid crystals is due to the electric field applied to the liquid crystal (horizontal electric field, vertical electric field or oblique electric field). Specifically, the liquid crystal element is controlled by an electric field in the forward direction. , nematic liquid crystal, cholesteric liquid crystal, smectic liquid crystal, discotic liquid crystal, Motropic liquid crystal, lyotropic liquid crystal, low molecular weight liquid crystal, polymer liquid crystal, polymer dispersed liquid crystal ( PDLC), ferroelectric liquid crystal, antiferroelectric liquid crystal, main chain liquid crystal, side chain polymer liquid crystal, banana-shaped liquid crystal Some examples include:

[0296] Next, a specific example of a liquid crystal display device using liquid crystal elements in the pixels 301 will be described. Here, a top view of the pixel 301 shown in FIG. 15(B) is shown in FIG. 16. In this case, the counter electrode and the liquid crystal element are omitted.

[0297] In FIG. 16, the conductive film 304c functioning as the scanning line is oriented in a direction substantially perpendicular to the signal line ( The conductive film 310d that functions as a signal line is provided so as to extend in a direction perpendicular to the plane of the drawing. The capacitor line extends in a direction substantially perpendicular to the scan line (vertical direction in the figure). The conductive film 310f extends in a direction parallel to the signal lines. The conductive film 304c that functions is electrically connected to the scanning line driver circuit 104 (see FIG. 15A). The conductive film 310d that functions as a signal line and the conductive film 310b that functions as a capacitance line are connected. 310f is electrically connected to the signal line driver circuit 106 (see FIG. 15(A)). .

[0298] The transistor 103 is provided in a region where the scanning line and the signal line intersect. The gate electrode 304c functions as a conductive film, and the gate insulating film (shown in FIG. 16) functions as a gate electrode. The oxide semiconductor film 308 in which the channel region is formed is formed on the gate insulating film. b, the conductive film 310d, 310e functioning as a source electrode and a drain electrode; Note that the conductive film 304c also functions as a scan line and overlaps with the oxide semiconductor film 308b. The conductive film 310d serves as a gate electrode of the transistor 103. The oxide semiconductor film 308b also functions as a signal line. It functions as a source electrode or a drain electrode. In terms of shape, the end portion is located outside the end portion of the oxide semiconductor film 308b. The lines function as a light-shielding film that blocks light from a light source such as a backlight. The oxide semiconductor film 308b included in the transistor is not irradiated with light, and the electrical characteristics of the transistor are not changed. This can suppress movement.

[0299] In addition, the conductive film 310e has a light-transmitting property that functions as a pixel electrode in the opening 362c. The conductive film 316b is electrically connected to the conductive film 316b.

[0300] The capacitor 105 is connected to a conductive film 310f that functions as a capacitor line in the opening 362. The capacitor 105 is formed of a light-transmitting conductive film formed on a gate insulating film. a dielectric film formed of a nitride insulating film provided on the transistor 103; The pixel electrode 316a is made of a light-transmitting conductive film 316b that functions as a pixel electrode. The element 105 has light-transmitting properties.

[0301] In this way, since the capacitor 105 has a light-transmitting property, the capacitor 105 is large and can be placed in the pixel 301. Therefore, it is possible to form the aperture ratio in a large area, preferably 50% or more. or 55% or more, preferably 60% or more, and the charge capacity can be increased. For example, a semiconductor device with high resolution, such as a liquid crystal display, can be obtained. In a display device, the area of ​​a pixel is reduced, and the area of ​​a capacitance element is also reduced. In a semiconductor device with high resolution, the charge capacity stored in the capacitive element is small. However, since the capacitor 105 shown in this embodiment has a light-transmitting property, the capacitor By providing the element, it is possible to obtain a sufficient charge capacity in each pixel while increasing the aperture ratio. Typically, high resolution displays have a pixel density of 200 ppi or more, or even 300 ppi or more. The present invention can be suitably used for semiconductor devices having a large number of semiconductor devices.

[0302] 16, the pixel 301 has a side parallel to the conductive film 310d that functions as a signal line. In comparison, the side parallel to the conductive film 304c functioning as the scanning line is longer, and The conductive film 310f functioning as a quantity line is parallel to the conductive film 310d functioning as a signal line. As a result, the area of ​​the conductive film 310f in the pixel 301 is reduced. It is possible to reduce the number of layers, which increases the aperture ratio. Since the conductive film 310f is in direct contact with the conductive film 308c having light-transmitting properties without using a connection electrode, , the aperture ratio can be further increased.

[0303] In addition, according to one embodiment of the present invention, the aperture ratio can be increased even in a high-resolution display device. This allows the light from light sources such as backlights to be used efficiently, and reduces the power consumption of the display device. The force can be reduced.

[0304] Next, a cross-sectional view taken along the dashed line CD in FIG. 16 is shown in FIG. 17. In the embodiment, a driving circuit section including a scanning line driving circuit 104 and a signal line driving circuit 106 (top view omitted) A cross-sectional view of the liquid crystal display device according to the present embodiment is shown in FIG. This article explains:

[0305] The liquid crystal display device shown in this embodiment has a liquid crystal display device between a pair of substrates (a substrate 302 and a substrate 342). The element 322 is sandwiched.

[0306] The liquid crystal element 322 is connected to a light-transmitting conductive film 316b above the substrate 302 to control the alignment. A liquid crystal layer 320 and a conductive film 350 are arranged in a liquid crystal display device. Note that the light-transmitting conductive film 316b is used as one electrode of the liquid crystal element 322. The conductive film 350 functions as the other electrode of the liquid crystal element 322 .

[0307] Thus, a liquid crystal display device is a device that has liquid crystal elements. The liquid crystal display device includes a driving circuit for driving a plurality of pixels. A control circuit, a power supply circuit, a signal generating circuit, a backlight module, etc., are arranged in It is also called a liquid crystal module.

[0308] In the driver circuit portion, a conductive film 304a functions as a gate electrode, and a gate insulating film The insulating film 305 and the insulating film 306 functioning as a channel region are formed in the oxide semiconductor film 30. 8a, the conductive films 310a and 310b functioning as a source electrode and a drain electrode The oxide semiconductor film 308a constitutes the transistor 102. The oxide semiconductor film 308a is provided over the gate insulating film.

[0309] In the pixel portion, a conductive film 304c functions as a gate electrode, and a gate insulating film The insulating film 305 and the insulating film 306 are formed on the gate insulating film. a conductive film 310 serving as a source electrode and a drain electrode; The oxide semiconductor film 308b is a gate The insulating film 312 and the insulating film 313 are provided on the conductive films 310d and 310e. 314 is provided as a protective film.

[0310] In addition, a light-transmitting conductive film 316b functioning as a pixel electrode is formed between the insulating film 312 and the insulating film 316b. The insulating film 314 is connected to the conductive film 310e through an opening provided therein.

[0311] In addition, a light-transmitting conductive film 308c functioning as one electrode and a dielectric film The insulating film 314 serving as the other electrode and the light-transmitting conductive film 316b serving as the other electrode form a capacitor. The light-transmitting conductive film 308c is provided over the gate insulating film. .

[0312] In the driving circuit section, the conductive film 304a and the conductive film 304c are formed at the same time. 4b and the conductive film 31 The light-transmitting conductive film 310c is formed at the same time as the light-transmitting conductive film 316b. Connected via 6a.

[0313] The conductive film 304b and the light-transmitting conductive film 316a are The conductive film 310c and the light-transmitting conductive film 310b are connected to each other through an opening provided in the conductive film 310c. The insulating film 312 and the insulating film 314 are connected to each other through an opening provided therein.

[0314] Here, the components of the display device shown in FIG. 17 will be described below.

[0315] Conductive films 304a, 304b, and 304c are formed on the substrate 302. The conductive film 04a functions as a gate electrode of a transistor in the driver circuit portion. 304c is formed in the pixel portion 101 and functions as a gate electrode of a transistor in the pixel portion. The conductive film 304b is formed in the scanning line driver circuit 104 and is connected to the conductive film 310c. do.

[0316] For the substrate 302, the material of the substrate 11 shown in Embodiment 1 can be used as appropriate.

[0317] The conductive films 304a, 304b, and 304c may be the same as those of the gate electrode 15 shown in the first embodiment. Materials and manufacturing methods can be used as appropriate.

[0318] An insulating film 305, an insulating film 306, and an insulating film 307 are formed on the substrate 302 and the conductive films 304a, 304c, and 304b. The insulating film 305 and the insulating film 306 are formed on the transistor of the driving circuit section. The insulating film functions as a gate insulating film and a gate insulating film of a transistor in the pixel portion 101 .

[0319] The insulating film 305 is the nitride insulating film described in the gate insulating film 17 in the first embodiment. The insulating film 306 is preferably formed using the gate insulating film shown in Embodiment 1. It is preferable to form the insulating film by using the oxide insulating film described above with respect to the insulating film 17 .

[0320] Over the insulating film 306, oxide semiconductor films 308a and 308b and a light-transmitting conductive film 30 The oxide semiconductor film 308a is formed in a position overlapping with the conductive film 304a. The oxide semiconductor layer is formed on the insulating film and functions as a channel region of the transistor in the driver circuit portion. The film 308b is formed in a position overlapping with the conductive film 304c, and is a channel of the transistor in the pixel portion. The light-transmitting conductive film 308c functions as a panel region. It functions as a pole.

[0321] The oxide semiconductor films 308a and 308b and the light-transmitting conductive film 308c are The material and the formation method of the oxide semiconductor film 18 shown in Embodiment 1 can be used as appropriate.

[0322] The light-transmitting conductive film 308c is an oxide semiconductor film similar to the oxide semiconductor films 308a and 308b. The film is a semiconductor film containing impurities. In addition, impurities such as boron, phosphorus, tin, antimony, and rare gases can be used instead of hydrogen. It may contain elements, alkali metals, alkaline earth metals, etc.

[0323] The oxide semiconductor films 308a and 308b and the light-transmitting conductive film 308c are all gate electrodes. The oxide semiconductor film 308a is formed over the oxide semiconductor insulating film 308b, but has a different impurity concentration. The impurity concentration of the light-transmitting conductive film 308c is higher than that of the light-transmitting conductive film 308b. The hydrogen concentration in the nitride semiconductor films 308a and 308b is 5×10 19 atoms / cm 3 Less than 5 x 10 18 atoms / cm 3 less than 1×10 18 atoms / cm 3 Less than or equal to 5×10 17 atoms / cm 3 Further details are below. Preferably 1 x 10 16 atoms / cm 3 The light-transmitting conductive film 308c is as follows: The hydrogen concentration in 19 atoms / cm 3 More than 1×10 20 atoms / cm 3 More preferably, 5×10 20 atoms / cm 3 That's all. In addition, compared with the oxide semiconductor films 308a and 308b, the conductive film 308c having a light-transmitting property The hydrogen concentration is twice as high, preferably 10 times or more.

[0324] In addition, the light-transmitting conductive film 308c has a lower resistance than the oxide semiconductor films 308a and 308b. The resistivity of the light-transmitting conductive film 308c is low compared to that of the oxide semiconductor films 308a and 308b. b resistivity 1×10 -8 1×10 times more -1 It is preferable that the ratio is less than 1 / 2. 1×10 -3 Ωcm or more 1×10 4 Ωcm, and more preferably a resistivity of 1×10 - 3 Ωcm or more 1×10 -1 It is preferable that the resistivity is less than Ωcm.

[0325] The oxide semiconductor films 308a and 308b are formed by forming the oxide semiconductor film 308a and the oxide semiconductor film 308b on the insulating film 306 and the insulating film 312. Since it is in contact with a film made of a material that can improve the interface characteristics with the conductor film, it is acid-resistant. The oxide semiconductor films 308a and 308b function as semiconductors. The transistor having 08b has excellent electrical characteristics.

[0326] On the other hand, the light-transmitting conductive film 308c is formed in the opening 362 (see FIG. 6A). The insulating film 314 is in contact with the insulating film 314. The insulating film 314 is used to prevent impurities from the outside, such as water and alkali metals. The film is formed of a material that prevents an alkaline earth metal or the like from diffusing into the oxide semiconductor film. Therefore, hydrogen in the insulating film 314 is absorbed in the oxide semiconductor films 308a and 308b. When hydrogen diffuses into the oxide semiconductor film formed at the same time as b, hydrogen is converted into oxygen in the oxide semiconductor film. The insulating film 314 is formed by the plasma CVD method. Alternatively, when the oxide semiconductor film is formed by a sputtering method, the oxide semiconductor film is exposed to plasma, and oxygen vacancies are generated. Hydrogen contained in the insulating film 314 enters the oxygen vacancy, and the carrier As a result, the oxide semiconductor film becomes more conductive and functions as a conductor. In other words, the oxide semiconductor film 308 can be regarded as a highly conductive oxide semiconductor film. The oxide semiconductor films 308a and 308b are mainly made of the same material as the oxide semiconductor films 308a and 308b, and the hydrogen concentration is The metal oxide having a higher electrical conductivity than that of the conductive film 30 having light transmitting properties is It's called 8c.

[0327] However, one aspect of the embodiment of the present invention is not limited to this. In some cases, it is possible that 8c is not in contact with the insulating film 314.

[0328] In addition, one aspect of the embodiment of the present invention is not limited to this. In some cases, the oxide semiconductor films 308a and 308b may be formed in separate steps. In that case, the light-transmitting conductive film 308c may be formed by removing the oxide semiconductor films 308a and 308b. For example, the light-transmitting conductive film 308c may be made of a material different from that of the light-transmitting conductive film 308b. It is made of indium tin oxide (hereinafter referred to as ITO) or indium zinc oxide. It may be possible to do so.

[0329] The semiconductor device described in this embodiment includes a capacitor and an oxide semiconductor film. In addition, a light-transmitting conductive film that functions as a pixel electrode is formed. The other electrode of the capacitor element is used. Since the step of forming a conductive film is not required, the manufacturing steps of the semiconductor device can be reduced. Since the pair of electrodes is formed of a conductive film having a light-transmitting property, the light-transmitting property is obtained. As a result, the area occupied by the capacitive element can be increased while increasing the aperture ratio of the pixel.

[0330] The conductive films 310a, 310b, 310c, 310d, and 310e are the same as those shown in the first embodiment. The material and manufacturing method for the pair of electrodes 21 and 22 can be appropriately used.

[0331] An insulating film 306, oxide semiconductor films 308a and 308b, a light-transmitting conductive film 308c, An insulating film 312 is formed on the conductive films 310a, 310b, 310c, 310d, and 310e. An insulating film 314 is formed. The insulating film 312 is made of an oxide semiconductor, similar to the insulating film 306. It is preferable to use a material capable of improving the interface characteristics with the film. The same materials and formation methods as those of the oxide insulating film 24 in Embodiment 1 can be used as appropriate. As shown in Embodiment 1, the oxide insulating film 23 and the oxide insulating film are stacked. This is also fine.

[0332] The insulating film 314, like the insulating film 305, is resistant to external impurities such as water and alkaline metals. It is preferable to use a material that prevents metals, alkaline earth metals, and the like from diffusing into the oxide semiconductor film. The material and the formation method of the nitride insulating film 25 shown in Embodiment 1 can be used as appropriate. do.

[0333] In addition, conductive films 316a and 316b having light-transmitting properties are formed over the insulating film 314. The light-transmitting conductive film 316a is conductive in the opening 364a (see FIG. 20C). The conductive film 304b is electrically connected to the conductive film 304b, and the conductive film 304b is electrically connected to the conductive film 304b at the opening 364b (see FIG. 20(C)). That is, the conductive film 304b and the conductive film 310c are electrically connected to each other. The conductive film 316b having light-transmitting properties functions as a connection electrode. C). In the above, the conductive film 310e is electrically connected to the conductive film 310c, and functions as a pixel electrode of the pixel. The light-transmitting conductive film 316b is used as one of a pair of electrodes of a capacitor. It can function.

[0334] In order to form a connection structure in which the conductive film 304b and the conductive film 310c are in direct contact with each other, the conductive film 3 Before forming 10c, a patterning process is performed to form openings in the insulating film 305 and the insulating film 306. It is necessary to perform photolithography and form a mask, but the connection structure of FIG. However, as shown in FIG. 17, the conductive film 316a having a light-transmitting property is used. The conductive film 304b and the conductive film 310c are connected to each other. This eliminates the need to create a connection part where c is in direct contact, and reduces the number of photomasks by one. That is, the number of manufacturing steps of the semiconductor device can be reduced.

[0335] The light-transmitting conductive films 316a and 316b are made of indium oxide containing tungsten oxide. Indium Zinc Oxide with Tungsten Oxide, Indium Zinc Oxide with Titanium Oxide Oxide, indium tin oxide with titanium oxide, ITO, indium zinc oxide, oxide ketone A light-transmitting conductive material such as indium-tin oxide doped with indium can be used. do.

[0336] In addition, a film having color (hereinafter, referred to as a color film 346) is formed on the substrate 342. The colored film 346 functions as a color filter. A light-shielding film 344 is formed on the substrate 342 and is adjacent to the light-shielding film 344. The colored film 346 does not necessarily have to be provided. For example, In some cases, such as when the device is black and white, the color film 346 may not be provided.

[0337] The colored film 346 may be any colored film that transmits light in a specific wavelength range. For example, A red (R) color filter that transmits light in the red wavelength range, and a green (G) color filter that transmits light in the green wavelength range. A green (G) color filter transmits light in the blue wavelength range, and a blue (B) color filter transmits light in the blue wavelength range. A filter or the like can be used.

[0338] The light-shielding film 344 may be made of a metal or other material as long as it has a function of blocking light in a specific wavelength range. Alternatively, an organic insulating film containing a black pigment or the like can be used.

[0339] In addition, an insulating film 348 is formed on the colored film 346. The insulating film 348 is planarized. The function of the colored film 346 is to prevent impurities contained therein from diffusing toward the liquid crystal element. It has the function of controlling

[0340] In addition, a conductive film 350 is formed on the insulating film 348. The conductive film 350 is The liquid crystal element has a function as the other of the pair of electrodes. An insulating film having a function as an alignment film is formed on the films 316a and 316b and the conductive film 350. It may be formed separately.

[0341] In addition, the liquid crystal layer 3 is provided between the conductive films 316a and 316b having light transmitting properties and the conductive film 350. The liquid crystal layer 320 is formed on the substrate 3 using a sealing material (not shown). The sealing material is used to prevent moisture from entering the device. In order to suppress oxidation, it is preferable to have a structure in which the inorganic material is in contact with the inorganic material.

[0342] In addition, a liquid crystal layer 320 is provided between the conductive films 316a and 316b having light-transmitting properties and the conductive film 350. A spacer may be provided to maintain the thickness (also called the cell gap) of the pixel.

[0343] Regarding a method for manufacturing an element portion provided on a substrate 302 shown in the semiconductor device shown in FIG. This will be explained with reference to FIG. 18 to FIG.

[0344] First, prepare a substrate 302. Here, a glass substrate is used as the substrate 302.

[0345] Next, a conductive film is formed on the substrate 302, and the conductive film is processed into a desired region. The conductive films 304a, 304b, and 304c are formed. The formation of c is performed by forming a mask by a first patterning in a desired region, and then covering the mask. It can be formed by etching the uncut areas (see FIG. 18(A)).

[0346] The conductive films 304a, 304b, and 304c are typically formed by deposition or CVD. The insulating film can be formed by a method such as sputtering or spin coating.

[0347] Next, an insulating film 305 is formed on the substrate 302 and the conductive films 304a, 304b, and 304c. Then, an insulating film 306 is formed over the insulating film 305 (see FIG. 18A).

[0348] The insulating film 305 and the insulating film 306 are formed by a sputtering method, a CVD method, or the like. When the insulating film 305 and the insulating film 306 are successively formed in a vacuum, impurities are easily removed. This is preferable because it suppresses the inclusion of

[0349] Next, an oxide semiconductor film 307 is formed over the insulating film 306 (see FIG. 18B).

[0350] The oxide semiconductor film 307 can be formed by a sputtering method, a coating method, a pulsed laser deposition method, a laser deposition method, or the like. The thin film can be formed by using a method such as ablation.

[0351] Next, the oxide semiconductor film 307 is processed into a desired region to form an island-shaped oxide semiconductor film 3 The oxide semiconductor films 308a, 308b, and 308d are formed. The formation of 08d involves forming a mask by second patterning in a desired area, and then forming the mask The etching can be performed by etching the area not covered by the The etching process can be dry, wet, or a combination of both. (See FIG. 18(C)).

[0352] Next, a conductive film 3 is formed over the insulating film 306 and the oxide semiconductor films 308a, 308b, and 308d. 09 (see Figure 19(A)).

[0353] The conductive film 309 can be formed by, for example, a sputtering method.

[0354] Next, the conductive film 309 is processed into a desired region to form conductive films 310a, 310b, and 311. In addition, the conductive films 310a, 310b, 310c, 310d, and 310e are formed. The formation of 10d and 310e involves forming a mask by third patterning in a desired area. The regions not covered by the mask can be etched to form the etched region (FIG. 1). 9(B)).

[0355] Next, the insulating film 306, the oxide semiconductor films 308a, 308b, and 308d, and the conductive film 31 An insulating film 311 is formed so as to cover the layers 310a, 310b, 310c, 310d, and 310e. (See FIG. 19(C)).

[0356] The insulating film 311 can be formed by the same method as the oxide insulating film 23 and the oxide insulating film 24 described in Embodiment 1. The oxide layer can be formed by stacking under the same conditions. The insulating film 23 is formed while being heated, so that the oxide semiconductor films 308a, 308b, and 308 By removing hydrogen, water, and the like contained in the oxide semiconductor film, a highly purified oxide semiconductor film can be formed. Cut.

[0357] Next, the insulating film 311 is processed into a desired region to form an insulating film 312 and an opening 362. The insulating film 311 and the opening 362 are formed in a desired region by forming a fourth pattern. A mask is formed by etching, and the area not covered by the mask is etched. It can be formed by the above (see FIG. 20(A)).

[0358] Note that the opening 362 is formed so that the surface of the oxide semiconductor film 308d is exposed. The opening 362 can be formed by, for example, dry etching. However, the method for forming the opening 362 is not limited to this, and may be a wet etching method or the like. Alternatively, a combination of dry etching and wet etching may be used.

[0359] Thereafter, in the same manner as in the first embodiment, a heat treatment is performed to remove oxygen contained in the insulating film 311. Part of the oxygen is transferred to the oxide semiconductor films 308a and 308b. As a result, the oxygen vacancies in the oxide semiconductor film 308b can be compensated for. The amount of oxygen vacancies contained in 08a and 308b can be reduced.

[0360] Next, the insulating film 313 is formed over the insulating film 312 and the oxide semiconductor film 308d (FIG. 20 (See (B)).

[0361] The insulating film 313 is made of a material that is free of impurities from the outside, such as oxygen, hydrogen, water, alkali metals, It is preferable to use a material that prevents an alkaline earth metal or the like from diffusing into the oxide semiconductor film. , and preferably contains hydrogen, typically an inorganic insulating material containing nitrogen, such as a nitride The insulating film 313 may be formed by using, for example, a CVD method. It is possible.

[0362] The insulating film 314 is resistant to external impurities such as water, alkali metals, alkaline earth metals, etc. The film is formed of a material that prevents diffusion of hydrogen into the oxide semiconductor film and further contains hydrogen. Therefore, when hydrogen in the insulating film 314 diffuses into the oxide semiconductor film 308d, the oxide semiconductor In the film 308d, hydrogen combines with oxygen to generate electrons, which are carriers. The oxide semiconductor film 308d has high conductivity and becomes the light-transmitting conductive film 308c.

[0363] In addition, the silicon nitride film is preferably formed at a high temperature in order to enhance blocking properties. The substrate temperature is preferably 100° C. or higher and 400° C. or lower, more preferably 300° C. or higher and 400° C. or lower. It is preferable to form the film by heating at a temperature of 0.1 °C or less. Oxygen is released from the oxide semiconductor used as the conductive films 308a and 308b, and the carrier concentration Since a phenomenon in which the temperature rises may occur, the temperature should be set at a level at which such a phenomenon does not occur.

[0364] Next, the insulating film 313 is processed into a desired region to form an insulating film 314 and an opening 364. The insulating film 314 and the openings 364a, 364b, and 364c are formed. b, 364c form a mask by fifth patterning in a desired area, and the mask The area not covered by the etchant can be etched away (see FIG. 20(C)). ).

[0365] The opening 364a is formed so that the surface of the conductive film 304b is exposed. The opening 364b is formed so as to expose the conductive film 310c. The conductive film 310e is formed so as to be exposed.

[0366] The openings 364a, 364b, and 364c can be formed, for example, by dry etching. However, the method for forming the openings 364a, 364b, and 364c may be different. The etching method is not limited to this, and may be a wet etching method or a dry etching method. A formation method in which wet etching is combined may also be used.

[0367] Next, a conductive film 31 is formed on the insulating film 314 so as to cover the openings 364a, 364b, and 364c. 5 (see FIG. 21(A)).

[0368] The conductive film 315 can be formed by, for example, a sputtering method.

[0369] Next, the conductive film 315 is processed into a desired region to form a light-transmitting conductive film 316a, The light-transmitting conductive films 316a and 316b are formed. A mask is formed on the region by a sixth patterning, and the region not covered by the mask is It can be formed by etching (see FIG. 21(B)).

[0370] Through the above steps, a pixel portion having a transistor and a driver circuit portion are formed on the substrate 302. In the manufacturing process shown in this embodiment, the first to sixth patterned This means that transistors and capacitors can be formed simultaneously using six masks. do.

[0371] Note that in this embodiment, hydrogen contained in the insulating film 314 is diffused into the oxide semiconductor film 308d. The oxide semiconductor film 308d was dispersed to increase the conductivity. The oxide semiconductor film 308d is covered with a mask, and impurities, typically hydrogen, boron, or lithium, are introduced into the oxide semiconductor film 308d. Addition of tin, antimony, rare gas elements, alkali metals, alkaline earth metals, etc. The oxide semiconductor film 308d may be doped with hydrogen or boron to increase the conductivity. The method of adding elements such as phosphorus, tin, antimony, and rare gas elements is ion doping. On the other hand, when an alkali metal or an alkaline earth metal is added to the oxide semiconductor film 308d, As a method for adding a metal or the like, a method of exposing a solution containing the impurity to the oxide semiconductor film 308d is used. There is a law.

[0372] Next, the structure formed on the substrate 342 provided opposite the substrate 302 will be described below. Provide an explanation.

[0373] First, a substrate 342 is prepared. The substrate 342 is made of the same material as that of the substrate 302. Next, a light-shielding film 344 and a colored film 346 are formed on the substrate 342 (FIG. 22( See A).

[0374] The light-shielding film 344 and the colored film 346 are formed of various materials by a printing method, an ink-jet method, They are formed at desired positions by an etching method using photolithography technology.

[0375] Next, an insulating film 348 is formed on the light-shielding film 344 and the colored film 346 (see FIG. 22(B)). see).

[0376] The insulating film 348 is made of an organic insulating material such as an acrylic resin, an epoxy resin, or a polyimide. By forming the insulating film 348, for example, the colored film 34 It is possible to prevent impurities contained in the liquid crystal layer 6 from diffusing to the liquid crystal layer 320 side. However, the insulating film 348 is not necessarily required, and a structure in which the insulating film 348 is not formed may be used. Good too.

[0377] Next, a conductive film 350 is formed over the insulating film 348 (see FIG. 22C). As the conductive film 315, the materials shown in the conductive film 315 can be used.

[0378] Through the above steps, the structure formed on the substrate 342 can be formed.

[0379] Next, the insulating film 31 formed on the substrate 302 and the substrate 342, more specifically, on the substrate 302, 4. The conductive films 316a and 316b having light transmitting properties and the conductive film 35 formed on the substrate 342 0, an alignment film 318 and an alignment film 352 are formed. The film can be formed by using a rubbing method, a photo-alignment method, or the like. A liquid crystal layer 320 is formed between the substrate 342 and the liquid crystal layer 320. or by bonding the substrate 302 and the substrate 342 together and then using the capillary phenomenon. An injection method for injecting liquid crystal can be used.

[0380] Through the above steps, the display device shown in FIG. 17 can be manufactured.

[0381] Note that this embodiment mode can be appropriately combined with other embodiment modes shown in this specification. do.

[0382] <Variation 1> A modified example of a liquid crystal display device using a liquid crystal element in the pixel 301 will be described. A top view of the pixel 301 shown in FIG. 15(B) is shown in FIG. The electrodes and liquid crystal elements are omitted. Note that the description of the same configuration as in the eighth embodiment is omitted. do.

[0383] <Configuration of Semiconductor Device> In FIG. 23, the opening 374c is provided inside the opening 372c, which is the same as that shown in FIG. Also, the pixel 301 is different from the pixel 301 shown in FIG. The conductive film 310e is formed in the opening 372c and the opening 374c. The conductive film 316b is electrically connected to a light-transmitting conductive film 316b which functions as a pixel electrode.

[0384] Next, a cross-sectional view taken along the dashed line CD in FIG. 23 is shown in FIG. 24. A cross-sectional view of the drive circuit portion (a top view is omitted) is shown at AB.

[0385] As shown in FIG. 24, the insulating film 306 and the insulating film 312 are provided on the conductive film 304a. 25A ) and an opening 374 provided in the insulating film 314. The opening 374a (see FIG. 25(C)) is an opening The opening 374a (see FIG. 25(C)) is located inside the opening 372a (see FIG. 25(A)). In the illustrated example, the conductive film 304a and the light-transmitting conductive film 316a are connected to each other.

[0386] In addition, an opening 372b (FIG. 25(A)) provided in the insulating film 312 is formed on the conductive film 310c. 25(C) ) and an opening 374b (see FIG. 25(C) ) provided in the insulating film 314. The opening 374b (see FIG. 25(C)) is formed in a space between the opening 372b (see FIG. 25(A)). In the opening 374b (see FIG. 25(C)), the conductive film 310c and a light-transmitting conductive film 316a are connected thereto.

[0387] In addition, an opening 372c (FIG. 25(A)) provided in the insulating film 312 is formed on the conductive film 310e. 25(C) ) and an opening 374c (see FIG. 25(C) ) provided in the insulating film 314. The opening 374c (see FIG. 25(C)) is formed in a substantially rectangular shape similar to the opening 372c (see FIG. 25(A)). In the opening 374c (see FIG. 25C), the conductive film 310e and a light-transmitting conductive film 316b are connected thereto.

[0388] In addition, an opening 372 provided in the insulating film 312 is formed on the light-transmitting conductive film 308c. (See FIG. 25A.) In the opening 372, the conductive film 308 having light-transmitting properties is The portion c is in contact with the insulating film 314 .

[0389] A connection portion between the conductive film 304b and the light-transmitting conductive film 316a, the conductive film 310c, and the light-transmitting conductive film 316b are The conductive film 310e and the light-transmitting conductive film 316b are connected to each other. The connection parts are covered with an insulating film 305 and / or an insulating film 314. The insulating film 314 and the insulating film 315 are resistant to impurities from the outside, such as water, alkali metals, alkaline earth metals, etc. The insulating film is made of a material that prevents metals and the like from diffusing into the oxide semiconductor film. In addition, the side surfaces of the openings 372a, 372b, 372c, and 372 (see FIG. 25(A)) are insulated. The insulating film 305 and / or the insulating film 314 are covered with the insulating film 305 and / or the insulating film 314. Since an oxide semiconductor film is provided on the side of the gate electrode, impurities from the outside, such as water and alkaline metals, can be prevented. The conductive film 304b, the conductive films 310c and 310e, and the light-transmitting The oxide film included in the transistor is formed from the connection portion of the conductive films 308c, 316a, and 316b. This prevents the diffusion of the ions into the semiconductor film, which reduces the change in the electrical properties of the transistor. It is possible to prevent such a malfunction, and the reliability of the semiconductor device can be improved.

[0390] Regarding a method for manufacturing an element portion provided on a substrate 302 shown in the semiconductor device shown in FIG. This will be explained with reference to Figures 19, 25, and 26.

[0391] As in the eighth embodiment, a gate electrode is formed on a substrate 302 through the steps shown in FIGS. the conductive films 304a, 304b, and 304c functioning as gate insulating films; The insulating film 305, the insulating film 306, the oxide semiconductor films 308a, 308b, and 308d, and the conductive film 31 0a, 310b, 310c, 310d, 310e, and an insulating film 311 are formed. In the process, first to third patterning are performed to form the conductive film 30 4a, 304b, 304c, oxide semiconductor film 308a, 308b, 308d, conductive film 31 0a, 310b, 310c, 310d, and 310e.

[0392] Thereafter, in the same manner as in the eighth embodiment, a heat treatment is performed to remove some of the oxygen contained in the insulating film 311. Oxygen is transferred from the oxide semiconductor film 308a to the oxide semiconductor film 308b. The oxygen vacancies in the oxide semiconductor film included in 08b can be filled. The amount of oxygen vacancies in the oxide semiconductor films 308a and 308b can be reduced.

[0393] Next, as shown in FIG. 25(A), the insulating film 311 is processed into a desired region to form an insulating The film 312 and the openings 372, 372b, and 372c are formed. The insulating film 306, which is a part of the insulating film, is processed into a desired region to form an opening 372a. The insulating film 305, the insulating film 312, and the openings 372, 372a, 372b, and 372c The formation is performed by forming a mask by the fourth patterning in a desired region, and covering the mask. The openings 372, 372a can be formed by etching the areas that are not covered by the insulating film. , 372b, and 372c may be formed by appropriately using the method for forming the opening 362 shown in the eighth embodiment. The method can be used.

[0394] In this etching step, at least the opening 372a is formed, so that the subsequent In the etching step using the mask formed in the fifth patterning, etching It is possible to reduce the amount of

[0395] Next, the insulating film 305, the conductive films 310c and 310e, the insulating film 312, and the oxide semiconductor film An insulating film 313 is formed on 308d (see FIG. 25(B)).

[0396] Next, in the same manner as in the eighth embodiment, the insulating film 313 is processed into a desired region, so that the insulating film 3 14, and openings 374a, 374b, and 374c are formed. The openings 374a, 374b, and 374c are formed by forming a fifth patterning mask in a desired area. The mask can be formed by forming a mask and then etching the area not covered by the mask. (See Figure 25(C)).

[0397] Next, in the same manner as in the eighth embodiment, an insulating A conductive film 315 is formed over the film 314 (see FIG. 26A).

[0398] Next, the conductive film 315 is processed into a desired region to form a light-transmitting conductive film 316a, The light-transmitting conductive films 316a and 316b are formed. A mask is formed on the region by a sixth patterning, and the region not covered by the mask is It can be formed by etching (see FIG. 26(B)).

[0399] Through the above steps, a pixel portion having a transistor and a driver circuit portion are formed on the substrate 302. In the manufacturing process shown in this embodiment, the first to sixth patterned This means that transistors and capacitors can be formed simultaneously using six masks. do.

[0400] In the case of a process in which the opening 372a is not formed in FIG. 25(A), In the etching process, the insulating film 305, the insulating film 306, the insulating film 312, and the insulating film 31 4 must be etched, which means the amount of etching is greater than for other openings. Therefore, there is variation in the etching process, and in some areas, The opening 374a is not formed, and the conductive film 316a and the conductive film 317b having a light-transmitting property are formed later. However, in this embodiment, the contact failure occurs twice. In order to form the openings 372a and 374a by the etching process, As a result, the yield of semiconductor devices is improved. In this embodiment, the opening 372a is used for the explanation. The portion 374b and the opening 374c have the same effect.

[0401] <Variation 2> A modified example of a liquid crystal display device using a liquid crystal element in the pixel 301 will be described. In the liquid crystal display device shown in FIG. 24, the light-transmitting conductive film 308 is in contact with the insulating film 314. However, it may be structured so that it is in contact with the insulating film 305. In this case, as shown in FIG. Since there is no need to provide an opening 362, the surfaces of the conductive films 316a and 316b having light transmitting properties are Therefore, the alignment of the liquid crystal material contained in the liquid crystal layer 320 can be improved. It is possible to reduce the disturbance. In addition, it is possible to manufacture a semiconductor device with high contrast. can be done.

[0402] In such a structure, in FIG. 18B, before the oxide semiconductor film 307 is formed, The insulating film 306 may be selectively etched to expose a portion of the insulating film 305 .

[0403] <Variation 3> Here, a modification of the semiconductor device shown in the first embodiment will be described with reference to FIGS. In FIG. 27, AB shows a cross-sectional view of the driving circuit section, and CD shows a cross-sectional view of the pixel section. The surface view is shown.

[0404] The semiconductor device shown in FIG. 27 has a channel protection The difference is that a transistor of the same type is used.

[0405] In the driver circuit portion, a conductive film 304a functions as a gate electrode, and a gate insulating film The insulating film 305 and the insulating film 306 functioning as a channel region are formed in the oxide semiconductor film 30. 8a, the conductive films 310a and 310b functioning as a source electrode and a drain electrode The transistor 102 is formed between the oxide semiconductor film 308a and the conductive films 310a and 310b. An insulating film 312 that functions as a channel protective film is provided. An insulating film 314 is provided as a protective film on the layers 10b and 310c.

[0406] In the pixel portion, a conductive film 304c functions as a gate electrode, and a gate insulating film The insulating film 305 and the insulating film 306 are formed on the gate insulating film. a conductive film 310 serving as a source electrode and a drain electrode; The oxide semiconductor film 308b and the conductive film 310e constitute the transistor 103. Between 10d and 310e, an insulating film 312 that functions as a channel protective film is provided. In addition, an insulating film 314 is formed over the conductive films 310d and 310e and the light-transmitting conductive film 308c. It is provided as a protective film.

[0407] In addition, a light-transmitting conductive film 316b functioning as a pixel electrode is provided on the insulating film 314. In the opening, the conductive film 310e is connected.

[0408] In addition, a light-transmitting conductive film 308c functioning as one electrode and a dielectric film The insulating film 314 serving as the other electrode and the light-transmitting conductive film 316b serving as the other electrode form a capacitor. The element 105 is formed.

[0409] In the driving circuit section, the conductive film 304a and the conductive film 304c are formed at the same time. 4b and the conductive film 31 The light-transmitting conductive film 310c is formed at the same time as the light-transmitting conductive film 316b. Connected via 6a.

[0410] In this modification, the conductive films 310a, 310b, 310d, and 310e are etched. At that time, since the oxide semiconductor films 308a and 308b are covered with the insulating film 312, the conductive film 3 The oxide semiconductor films 10a, 310b, 310d, and 310e are formed by etching. The insulating film 312 has a stoichiometric composition. The insulating film 312 is formed of an oxide insulating film containing more oxygen than the insulating film 312. Part of the oxygen contained in the oxide semiconductor film 308a and 308b is transferred to the oxide semiconductor film 308a and 308b. The amount of oxygen vacancies contained in 308a and 308b can be reduced.

[0411] Regarding a method for manufacturing an element portion provided on a substrate 302 shown in the semiconductor device shown in FIG. This will be explained with reference to Figures 19, 28, and 29.

[0412] As in the eighth embodiment, a gate electrode is formed on the substrate 302 through the process shown in FIG. the insulating film 305 which functions as a gate insulating film; Then, an insulating film 306 and oxide semiconductor films 308a, 308b, and 308d are formed. In the process, a first patterning and a second patterning are performed to form a conductive film 30 4a, 304b, and 304c, and oxide semiconductor films 308a, 308b, and 308d are formed. do.

[0413] Next, as shown in FIG. 28(A), an insulating film 311 is formed in the same manner as in the eighth embodiment.

[0414] Thereafter, in the same manner as in the eighth embodiment, a heat treatment is performed to remove some of the oxygen contained in the insulating film 311. Oxygen is transferred from the oxide semiconductor film 308a to the oxide semiconductor film 308b. The oxygen vacancies in the oxide semiconductor film included in 08b can be filled. The amount of oxygen vacancies in the oxide semiconductor films 308a and 308b can be reduced.

[0415] Next, as shown in FIG. 28(B), the insulating film 311 is processed into a desired region, and then oxidized. An insulating film 312 is formed on the semiconductor films 308a and 308b. When the insulating film 306 is formed of the same material as the insulating film 312, a part of the insulating film 306 is etched. Only the regions covered with the oxide semiconductor films 308a and 308b remain. The film 306 and the insulating film 312 are formed by forming a mask in a desired area by a third patterning. The mask can be formed by depositing a layer of silicon dioxide on the silicon substrate and then etching the areas not covered by the mask. do.

[0416] Next, a conductive film is formed over the insulating film 305, the insulating film 306, and the oxide semiconductor films 308a and 308b. After the formation, the conductive films 310a, 310b, 310c, and 310d are formed through the same process as in the eighth embodiment. 10d and 310e are formed (see FIG. 28(C)). , 310c, 310d, and 310e are formed in desired areas by a fourth patterning. The mask is then formed and the area not covered by the mask is etched to form the can be done.

[0417] Next, the insulating film 305, the insulating film 312, the oxide semiconductor film 308d, the conductive films 310a and 31 An insulating film 313 is formed on the layers 310b, 310c, 310d, and 310e (see FIG. 29(A)). .

[0418] Next, in the same manner as in the eighth embodiment, the insulating film 313 is processed into a desired region, so that the insulating film 3 14, and openings 384a, 384b, and 384c are formed. The openings 384a, 384b, and 384c are formed by applying a fifth patterning mask to desired areas. The mask can be formed by forming a mask and then etching the area not covered by the mask. (See Figure 29(B)).

[0419] Next, in the same manner as in the eighth embodiment, an insulating After a conductive film is formed on the film 314, the conductive film is processed into a desired region to form a light-transmitting film. Conductive films 316a and 316b are formed through the insulating film 316a (see FIG. 29C). The formation of the conductive films 316a and 316b is performed by forming a mask by a sixth patterning in a desired area. and then etching the areas not covered by the mask.

[0420] Through the above steps, a pixel portion having a transistor and a driver circuit portion are formed on the substrate 302. In the manufacturing process shown in this embodiment, the first to sixth patterned This means that transistors and capacitors can be formed simultaneously using six masks. do.

[0421] <Variation 4> In this embodiment and the modified example, a pair of electrodes constituting the capacitor element 105 is made of a light-transmitting material. The conductive film 308c having a light-transmitting property and the conductive film 316b having a light-transmitting property are used. As shown in FIG. 8, a light-transmitting conductive film 31 is provided between the insulating film 312 and the insulating film 314. 7, a light-transmitting conductive film 316c is formed over the insulating film 314, and a light-transmitting conductive film The conductive film 317 and the light-transmitting conductive film 316c are disposed in a pair of electrodes forming the capacitor 105. It can be used as a pole.

[0422] Furthermore, on the insulating film 312, an organic insulating film such as an acrylic resin, an epoxy resin, or a polyimide is applied. Since an organic insulating film made of an acrylic resin or the like has high flatness, it is possible to provide a light-transmitting film. It is possible to reduce the step on the surface of the conductive film 316a. It is possible to reduce the alignment disorder of the liquid crystal material that is generated by the liquid crystal display. A device can be fabricated.

[0423] <Variation 5> In this embodiment and the modified example, a pair of electrodes constituting a capacitor element is made of a light-transmitting material. The conductive film 308c and the light-transmitting conductive film 316b are used. Conductive films 310a, 310b, 310c ... The conductive film 308c having a light-transmitting property and the conductive film 308b having a light-transmitting property are formed at the same time as the conductive film 308d and the conductive film 310e. It is possible to appropriately select two or more of the conductive films 316b having the above structure.

[0424] (Embodiment 9) In this embodiment, a transistor included in the semiconductor device described in the above embodiment is In the above, one embodiment applicable to the oxide semiconductor film 18, the multilayer film 20, and the multilayer film 34 is as follows: Note that, in this example, an oxide semiconductor film included in a multilayer film will be used as an example. The oxide film can also have a similar structure.

[0425] The oxide semiconductor film is an oxide semiconductor having a single crystal structure (hereinafter referred to as a single crystal oxide semiconductor). , a polycrystalline oxide semiconductor (hereinafter referred to as a polycrystalline oxide semiconductor), oxide semiconductors having an amorphous structure (hereinafter referred to as microcrystalline oxide semiconductors) and amorphous oxide semiconductors having an amorphous structure (hereinafter referred to as The oxide semiconductor film may be formed of one or more of the following: The oxide semiconductor film may be made of an amorphous oxide semiconductor. The oxide semiconductor may be composed of a single crystal oxide semiconductor having a crystal grain. oxide semiconductor, CAAC-OS, polycrystalline oxide semiconductor, microcrystalline oxide semiconductor, and amorphous oxide semiconductor We will explain about this.

[0426] <Single crystal oxide semiconductor> For example, a single crystal oxide semiconductor has a low impurity concentration and a low density of defect states (oxygen vacancies). Therefore, the carrier density can be reduced. The transistors used in the channel region rarely have normally-on electrical characteristics. In addition, since the density of defect states in a single crystal oxide semiconductor is low, the density of trap states is also low. Therefore, a transistor using a single crystal oxide semiconductor for a channel region may In this case, the change in electrical characteristics may be small, resulting in a highly reliable transistor.

[0427] <caac-os> The CAAC-OS film is one of the oxide semiconductor films that has multiple crystal parts. The crystal part is small enough to fit inside a cube with one side less than 100 nm. The crystal parts contained in the OS film are in the form of cubes with one side less than 10 nm, 5 nm, or 3 nm. The CAAC-OS film has a smaller defect density than a microcrystalline oxide semiconductor film. The CAAC-OS film has a low density of recessed states. .

[0428] CAAC-OS is, for example, a method for analyzing the The crystals were confirmed by the observation image using a TEM. The crystal parts in the CAAC-OS can be seen, for example, in TEM images. In most cases, the size of the CAAC-OS is within a cube with a side length of 100 nm. In TEM images, the boundaries between crystalline regions may not be clearly visible. CAAC-OS is a TEM image showing the grain boundary. In some cases, it is not possible to clearly confirm the grain boundaries of CAAC-OS. Therefore, impurities are less likely to segregate. Therefore, the defect density is unlikely to increase. Since there are no clear grain boundaries, the decrease in electron mobility is small.

[0429] For example, the CAAC-OS has a plurality of crystal parts, and the c-axes of the crystal parts are aligned in the crystal parts. They may be aligned in a direction parallel to the normal vector of the forming plane or the normal vector of the surface. Therefore, CAAC-OS can be characterized by, for example, X-ray diffraction (XRD). When the out-of-plane analysis was performed using a fusion apparatus, two In some cases, a peak appears around 31°. In some cases, spots (bright points) are observed in the diffraction pattern. The electron diffraction patterns obtained using an electron beam of 0 nmφ or less or 5 nmφ or less are called The electron microbeam diffraction pattern is called the electron microbeam diffraction pattern. In some cases, the a-axis and b-axis of each of the three crystals may not be aligned. For example, the c-axis of the CAAC-OS may not be aligned. The a-axis and / or b-axis may not be aligned macroscopically.

[0430] FIG. 30 shows an example of an electron microbeam diffraction pattern of a sample having a CAAC-OS. The sample was cut in a direction perpendicular to the CAAC-OS surface to obtain a thickness of about 40 nm. In this case, the electron beam with a beam diameter of 1 nmφ is applied to the cut surface of the sample. From Figure 30, the electron micro diffraction pattern of CAAC-OS is , it can be seen that spots are observed.

[0431] The crystal part included in the CAAC-OS has a c-axis that is normal to the surface on which the CAAC-OS is formed. The vectors are aligned parallel to the surface normal vector and perpendicular to the ab plane. When viewed from the direction, the metal atoms are arranged in a triangular or hexagonal shape, and when viewed from the direction perpendicular to the c-axis, the metal atoms are arranged in a triangular or hexagonal shape. Metal atoms are arranged in layers, or metal atoms and oxygen atoms are arranged in layers. In this specification, the a-axis and the b-axis may be oriented in different directions. When described, the range includes 80° to 100°, preferably 85° to 95°. In addition, when simply describing it as parallel, it is -10° or more and 10° or less, preferably The range from -5° to 5° is also included.

[0432] The c-axis of the crystalline part in the CAAC-OS is the normal vector of the surface on which the CAAC-OS is formed. Or, the shape of CAAC-OS ( Depending on the cross-sectional shape of the surface to be formed or the cross-sectional shape of the surface, the directions may differ from each other. In addition, the crystallization process such as heat treatment was performed when or after the film was formed. Therefore, the c-axis of the crystal part is the same as that of the unformed part when CAAC-OS is formed. Aligns to be parallel to the face normal vector or surface normal vector.

[0433] CAAC-OS can be formed, for example, by reducing the impurity concentration. Here, the impurities are the main impurities of oxide semiconductors, such as hydrogen, carbon, silicon, and transition metal elements. In particular, elements such as silicon are metal elements that make up oxide semiconductors. Therefore, when the element removes oxygen from the oxide semiconductor, the oxygen In addition, iron, nickel, and other elements can disrupt the atomic arrangement of semiconductors and reduce their crystallinity. Heavy metals, argon, carbon dioxide, etc. have large atomic (or molecular) radii, so they are acidic. This can disrupt the atomic arrangement of the oxide semiconductor and reduce the crystallinity of the oxide semiconductor. CAAC-OS is an oxide semiconductor with a low impurity concentration. Impurities present in the semiconductor layer may act as a carrier generation source.

[0434] In the CAAC-OS, the distribution of the crystal parts may not be uniform. In the process of forming C-OS, when crystal growth is performed from the surface side of the oxide semiconductor, The proportion of crystalline parts may be higher near the surface than near the bottom. -When impurities are mixed into the OS, the crystallinity of the crystal part in the region where the impurities are mixed is reduced. It may go down.

[0435] In addition, the CAAC-OS can be formed by, for example, reducing the density of defect states. In an oxide semiconductor, for example, when there is oxygen vacancy, the density of defect states increases. The loss acts as a carrier trap or a carrier generation source by capturing hydrogen. To form a CAAC-OS, for example, oxygen vacancies are introduced into an oxide semiconductor. Therefore, CAAC-OS is an oxide with a low density of defect states. Alternatively, the CAAC-OS is an oxide semiconductor with few oxygen vacancies.

[0436] In CAAC-OS, the constant photocurrent measurement method (CPM) The absorption coefficient derived by the current method is 1×10 -3 / cm or less, good Preferably 1×10 -4 / cm, more preferably less than 5×10 -5 / cm. The absorption coefficient is the energy (depending on the wavelength) corresponding to the localized level caused by oxygen vacancies and impurity contamination. Since the CAAC-OS has a positive correlation with the lattice constant (r / s), the number of defect levels in the CAAC-OS is extremely small.

[0437] In addition, the absorption coefficient curve obtained by CPM measurement shows that the arbor due to the tail of the band is By excluding the absorption coefficient called Urbach tail, the absorption coefficient due to defect levels can be calculated by the following formula. Note that the Urbach tail refers to a region having a constant slope in the curve of the absorption coefficient obtained by CPM measurement, and the slope is called Urbach energy. It can be calculated from the following formula. The Urbach tail refers to a region having a constant slope in the curve of the absorption coefficient obtained by CPM measurement, and the slope is called Urbach energy. In the curve of the absorption coefficient obtained by CPM measurement, the region having a constant slope is referred to as the Urbach tail, and the slope is called the Urbach energy. Here, α(E) represents the absorption coefficient at each energy, and α represents the absorption coefficient due to the Urbach tail.

[0438]

Equation

[0439] Here, α(E) represents the absorption coefficient at each energy, and α represents the absorption coefficient due to the Urbach tail. u The Urbach tail represents the absorption coefficient due to the Urbach tail. Here, α(E) represents the absorption coefficient at each energy, and α represents the absorption coefficient due to the Urbach tail.

[0440] In addition, a transistor using CAAC-OS that is highly pure intrinsic or substantially highly pure intrinsic has little variation in electrical characteristics due to irradiation with visible light or ultraviolet light. In addition, a transistor using CAAC-OS that is highly pure intrinsic or substantially highly pure intrinsic has little variation in electrical characteristics due to irradiation with visible light or ultraviolet light.

[0441] <Method for manufacturing CAAC-OS> Since the c-axis of the crystal part included in CAAC-OS is aligned in a direction parallel to the normal vector of the surface to be formed of CAAC-OS or the normal vector of the surface, depending on the shape of CAAC-OS (the cross-sectional shape of the surface to be formed or the cross-sectional shape of the surface), they may face different directions. Note that the direction of the c-axis of the crystal part is parallel to the normal vector of the surface to be formed or the normal vector of the surface when CAAC-OS is formed. The crystal part is formed by film formation or by performing a crystallization treatment such as heat treatment after film formation. Since the c-axis of the crystal part included in CAAC-OS is aligned in a direction parallel to the normal vector of the surface to be formed of CAAC-OS or the normal vector of the surface, depending on the shape of CAAC-OS (the cross-sectional shape of the surface to be formed or the cross-sectional shape of the surface), they may face different directions. Note that the direction of the c-axis of the crystal part is parallel to the normal vector of the surface to be formed or the normal vector of the surface when CAAC-OS is formed. The crystal part is formed by film formation or by performing a crystallization treatment such as heat treatment after film formation. Since the c-axis of the crystal part included in CAAC-OS is aligned in a direction parallel to the normal vector of the surface to be formed of CAAC-OS or the normal vector of the surface, depending on the shape of CAAC-OS (the cross-sectional shape of the surface to be formed or the cross-sectional shape of the surface), they may face different directions. Note that the direction of the c-axis of the crystal part is parallel to the normal vector of the surface to be formed or the normal vector of the surface when CAAC-OS is formed. The crystal part is formed by film formation or by performing a crystallization treatment such as heat treatment after film formation. The direction of the c-axis of the crystal part is parallel to the normal vector of the surface to be formed or the normal vector of the surface when CAAC-OS is formed. The crystal part is formed by film formation or by performing a crystallization treatment such as heat treatment after film formation. The direction of the c-axis of the crystal part is parallel to the normal vector of the surface to be formed or the normal vector of the surface when CAAC-OS is formed. The crystal part is formed by film formation or by performing a crystallization treatment such as heat treatment after film formation. The crystal part is formed by film formation or by performing a crystallization treatment such as heat treatment after film formation.

[0442] There are three methods for forming CAAC-OS.

[0443] The first method is to form an oxide semiconductor film with a film formation temperature of 100°C or higher and 450°C or lower. In this way, the c-axis of the crystal part included in the oxide semiconductor film is aligned with the normal vector of the formation surface or the surface This method forms crystals aligned in a direction parallel to the normal vector of the crystal. In this case, the film formation temperature is preferably set to 100° C. or higher and 400° C. or lower.

[0444] The second method is to form an oxide semiconductor film to a small thickness, and then heat the film at a temperature of 200° C. to 700° C. By performing heat treatment, the c-axis of a crystal part included in the oxide semiconductor film is aligned along the normal vector of the formation surface. This is a method for forming crystals aligned in a direction parallel to the normal vector of the crystal or surface. In this specification, the heating temperature is preferably 200° C. or higher and 400° C. or lower.

[0445] The third method is to form a thin oxide semiconductor film as a first layer, and then heat the film at 200° C. or higher for 700 Heat treatment at 0.4 °C or less is performed, and then a second oxide semiconductor film is formed. The c-axis of the crystal part contained in the conductive film is aligned with the normal vector of the surface on which it is formed or the normal vector of the surface. This is a method for forming crystals aligned in parallel directions. It is preferable to set the temperature to 200° C. or higher and 400° C. or lower.

[0446] Here, a method for forming a CAAC-OS using the first method will be described.

[0447] <Target and target preparation method> In addition, the CAAC-OS can be used as a sputtering target for a polycrystalline oxide semiconductor. The sputtering target is used to deposit a thin film. When the ions collide, the crystalline regions in the sputtering target cleave from the ab plane. The sputtered particles are either flat or pellet-shaped with a surface parallel to the ab plane. In this case, the plate-like or pellet-like sputtered particles may become crystalline. By reaching the target surface while maintaining this state, a CAAC-OS film can be formed. .

[0448] In addition, in order to form a CAAC-OS film, the following conditions are preferably applied.

[0449] By reducing the amount of impurities mixed in during film formation, it is possible to prevent the crystal state from being destroyed by impurities. For example, the concentration of impurities (hydrogen, water, carbon dioxide, nitrogen, etc.) present in the film formation chamber can be In addition, the impurity concentration in the deposition gas may be reduced. A deposition gas having a temperature of -80°C or lower, preferably -100°C or lower, is used.

[0450] In addition, by increasing the heating temperature (for example, the substrate heating temperature) of the surface to be formed during film formation, After the sputtering particles reach the target surface, they migrate. The temperature is set to 100° C. or higher and 740° C. or lower, preferably 200° C. or higher and 500° C. or lower. By increasing the temperature of the surface during film formation, the plate-shaped sputtering particles reach the surface. When the sputtered particles are mixed with the surface, migration occurs on the surface to be formed, and the flat surface of the sputtered particles The sputtering particles adhere to the surface on which the oxide is formed, although this varies depending on the type of oxide. , the diameter (equivalent circle diameter) of the plane parallel to the ab plane is 1 nm or more and 30 nm or less, or 1 nm or more The diameter of the plate-shaped sputtered particles is about 10 nm or less. The hexagonal faces of the plate-shaped sputtered particles are in the ab plane. In this case, the direction perpendicular to the hexagonal surface is the c-axis direction. It is in the direction.

[0451] In addition, the sputtering target is sputtered using oxygen cations. Therefore, the plasma damage during film formation can be reduced. When it hits the surface of the ring target, the crystallinity of the sputtering target decreases. It is possible to suppress the crystallization or amorphization.

[0452] In addition, the sputtering target is sputtered using oxygen or argon cations. By ringing, when a flat sputtering particle has a hexagonal column shape, the hexagonal surface is The corners of the hexagonal faces can be positively charged. As a result, the positive charges in each sputtering particle repel each other, maintaining the flat shape. It can be held.

[0453] In order for the corners of the surface of a flat sputtered particle to have a positive charge, a direct current ( It is preferable to use a DC power supply. Note that a radio frequency (RF) power supply or an alternating current (AC) power supply may also be used. However, the RF power source is a sputtering device capable of depositing a film on a large-area substrate. In addition, DC power is preferable to AC power for the following reasons: It is possible.

[0454] When an AC power source is used, adjacent targets alternate between cathode and anode potentials. When flat sputtering particles are positively charged, they repel each other. However, when using an AC power source, the plate shape can be maintained. Since there is a period of time when no electric field is applied to the plate-shaped sputtering particle, the charge on the plate-shaped sputtering particle The structure of the sputtered particles may be destroyed due to the loss of the AC current. It has been found that using a DC power supply is preferable to using a DC power supply.

[0455] In addition, by increasing the oxygen ratio in the deposition gas and optimizing the power, plasma damage during deposition is reduced. The oxygen ratio in the deposition gas is preferably 30% by volume or more, and more preferably 100% by volume or more. Expressed as volume percent.

[0456] As an example of a sputtering target, an In-Ga-Zn compound target is The details are shown below.

[0457] InO X powder, GaO Y Powder, and ZnO Z The powders are mixed in a specified number of moles and pressurized. Then, it is heated at a temperature between 1000℃ and 1500℃ to produce polycrystalline In-G The target is a Zn-based compound. The pressure treatment is performed while cooling (or cooling naturally). The reaction may be performed while heating or while heating. In addition, X, Y and Z are any positive numbers. Here, the predetermined molar ratio is, for example, InO X powder, GaO Y Powder and ZnO Z powder However, 2:2:1, 8:4:3, 3:1:1, 1:1:1, 4:2:3, 3:1:2, 1: The ratio is 3:2, 1:6:4, or 1:9:6. The powder type and the mixture ratio are The ol ratio may be appropriately changed depending on the sputtering target to be produced.

[0458] By using a sputtering target in the above manner, the thickness is uniform and In this way, an oxide semiconductor film with uniform crystal orientation can be formed.

[0459] <Polycrystalline oxide semiconductor> An oxide semiconductor having polycrystals is called a polycrystalline oxide semiconductor. Contains a number of crystal grains.

[0460] In the case of polycrystalline oxide semiconductors, for example, crystal grains can be confirmed in TEM images. Crystal grains contained in a polycrystalline oxide semiconductor may be, for example, , 2nm to 300nm, 3nm to 100nm, or 5nm to 50nm In addition, polycrystalline oxide semiconductors are often observed with a grain size of 100 nm or less in a TEM image. In some cases, the boundaries between crystal grains can be confirmed. For example, grain boundaries may be visible in TEM images.

[0461] The polycrystalline oxide semiconductor has, for example, a plurality of crystal grains, and the crystal grains have different orientations. In addition, the polycrystalline oxide semiconductor may be analyzed by, for example, an XRD apparatus. When the out-of-plane analysis was performed, a peak was observed near 31° 2θ, which indicates orientation. In addition, a peak showing a plurality of types of orientation may appear. For example, spots may be observed in an electron diffraction pattern.

[0462] A polycrystalline oxide semiconductor has high crystallinity and therefore high electron mobility. Therefore, a transistor using a polycrystalline oxide semiconductor for a channel region has a high current. However, in polycrystalline oxide semiconductors, impurities may segregate at grain boundaries. In addition, the grain boundaries of a polycrystalline oxide semiconductor become defect states. Since the channel region of a polycrystalline oxide semiconductor may be a carrier generation source or a trap state, The transistor using CAAC-OS for the channel region is In all cases, the electrical characteristics may vary significantly, resulting in a transistor with low reliability.

[0463] The polycrystalline oxide semiconductor is formed by a heat treatment at a high temperature or a laser light treatment. can be done.

[0464] <Microcrystalline oxide semiconductor> In the TEM image of the microcrystalline oxide semiconductor film, crystal parts can be clearly seen. The crystal parts contained in the microcrystalline oxide semiconductor film may have a size of 1 nm or more and 100 nm or more. In particular, the size of the particles is between 1 nm and 10 nm. Nanocrystals (nc) are microcrystals with a diameter of 1 to 3 nm or less. The oxide semiconductor film having nc-OS (nanocrystalline O The nc-OS film is called a T In EM images, grain boundaries may not be clearly visible.

[0465] The nc-OS film is a microscopic region (e.g., a region of 1 nm to 10 nm, especially a region of 1 nm or less). The nc-OS film has a periodic atomic arrangement in the region of 3 nm or less. There is no regularity in the crystal orientation between the crystal parts, and therefore no orientation is observed throughout the film. Therefore, the nc-OS film cannot be distinguished from an amorphous oxide semiconductor film depending on the analysis method. For example, XRD, which uses X-rays with a diameter larger than that of the crystal part, is used for nc-OS films. When structural analysis is performed using the out-of-plane method, the crystal planes are In addition, the peaks shown in the figure are not detected in the nc-OS film because the probe diameter is larger than that in the crystalline region. Electron beam diffraction (also called selected area electron beam diffraction) using an electron beam of 50 nm or more (for example) When the diffraction pattern is changed to nc-OS film, a halo-like diffraction pattern is observed. The probe diameter is close to or smaller than the size of the crystal part (for example, 1 nm to 30 nm). When electron beam diffraction (also called nanobeam electron beam diffraction) is performed using the electron beam shown below, In addition, when the nc-OS film was subjected to nanobeam electron diffraction, a circular pattern was observed. In addition, for the nc-OS film, a bright area (ring-shaped) may be observed. When performing nanobeam electron diffraction, multiple spots may be observed within a ring-shaped region. be.

[0466] Figure 31 shows the nanobeam electron diffraction patterns of the sample with the nc-OS film at different measurement points. In this example, the sample was cut in a direction perpendicular to the surface on which the nc-OS film was formed. The thickness of the slice is reduced to 10 nm or less. The sagittal beam is incident from a direction perpendicular to the cut surface of the sample. When nanobeam electron diffraction is performed on a sample, a diffraction pattern showing the crystal planes is obtained. It was found that no orientation to a specific crystal plane was observed.

[0467] The nc-OS film is an oxide semiconductor film that has higher order than an amorphous oxide semiconductor film. Therefore, the nc-OS film has a lower density of defect states than the amorphous oxide semiconductor film. In the nc-OS film, the crystal orientation is not regular between different crystal parts. The OS film has a higher density of defect states than the CAAC-OS film.

[0468] Therefore, the nc-OS film may have a higher carrier density than the CAAC-OS film. An oxide semiconductor film having a high carrier density may have high electron mobility. In some cases, a transistor using an nc-OS film has high field-effect mobility. The nc-OS film has a higher defect density than the CAAC-OS film, which leads to carrier transport. Therefore, the transistor using the nc-OS film is Compared to transistors using OS films, the electrical characteristics fluctuate greatly and the reliability is low. However, the nc-OS film can be formed even if it contains a relatively large amount of impurities. Therefore, it is easier to form than the CAAC-OS film, and is preferably used depending on the application. Therefore, a semiconductor having a transistor using an nc-OS film can be The devices may be capable of being manufactured productively.

[0469] <Method for manufacturing microcrystalline oxide semiconductor film> Next, a method for forming a microcrystalline oxide semiconductor film will be described below. The film is heated to a temperature of from room temperature to 75° C., preferably from room temperature to 50° C., in an atmosphere containing oxygen. The film is formed by sputtering under an oxygen-containing atmosphere. As a result, oxygen vacancies in the microcrystalline oxide semiconductor film are reduced, and the film includes a microcrystalline region. This can be done.

[0470] By reducing oxygen vacancies in a microcrystalline oxide semiconductor film, the film has stable physical properties. In particular, when a semiconductor device is manufactured by using a microcrystalline oxide semiconductor film, The oxygen vacancies in the microcrystalline oxide semiconductor film act as donors, and carriers are introduced into the microcrystalline oxide semiconductor film. This generates electrons that are the cause of fluctuations in the electrical characteristics of the semiconductor device. By manufacturing a semiconductor device using a microcrystalline oxide semiconductor film in which defects are reduced, Therefore, a high-performance semiconductor device can be obtained.

[0471] In the microcrystalline oxide semiconductor film, oxygen vacancies occur when the oxygen partial pressure in the film formation atmosphere is increased. More specifically, the oxygen partial pressure in the film formation atmosphere is preferably reduced to 33%. It is preferable that the amount is equal to or more than that.

[0472] Note that a target used in forming the microcrystalline oxide semiconductor film by a sputtering method is The CAAC-OS can use the same target and its preparation method as those of the CAAC-OS.

[0473] In addition, nc-OS can be formed even if it contains a relatively large amount of impurities. It is easier to form than CAAC-OS and can be used preferably for some applications. For example, nc-OS can be formed by a deposition method such as sputtering using an AC power source. The sputtering method using an AC power source is capable of depositing a film on a large substrate with high uniformity. Therefore, it is possible to develop a semiconductor device having a transistor with nc-OS in the channel region. The device can be produced productively.

[0474] <Amorphous oxide semiconductor> For example, an amorphous oxide semiconductor has a disordered atomic arrangement and does not have a crystal part. An amorphous oxide semiconductor has an amorphous state like quartz, for example, and has regular atomic arrangement. Not seen.

[0475] In the amorphous oxide semiconductor, for example, crystal parts can be confirmed in the observation image by TEM. There may not be.

[0476] Amorphous oxide semiconductors are analyzed by the out-of-plane method using an XRD device. In addition, when the amorphous oxide semiconductor is used, the peak indicating the orientation may not be detected. For example, a halo pattern may be observed in the electron diffraction pattern. For example, no spots can be observed in the ultrafine electron diffraction pattern of a halo semiconductor. -patterns may be observed.

[0477] Amorphous oxide semiconductors are formed by, for example, containing a high concentration of impurities such as hydrogen. Therefore, the amorphous oxide semiconductor may be formed by, for example, It is an oxide semiconductor containing

[0478] When an oxide semiconductor contains a high concentration of impurities, defects such as oxygen vacancies occur in the oxide semiconductor. Therefore, an amorphous oxide semiconductor with a high impurity concentration has a high density of defect states. In addition, amorphous oxide semiconductors have low crystallinity, so The defect level density is higher than that of

[0479] Therefore, the amorphous oxide semiconductor has a higher carrier density than the nc-OS. Therefore, a transistor using an amorphous oxide semiconductor for a channel region has a Therefore, normally-on electrical characteristics are required. In some cases, an amorphous oxide semiconductor can be suitably used for a transistor in which defects are formed. Since the density of states is high, the density of trap states may also be high. Transistors using conductors for the channel region use CAAC-OS or nc-OS for the channel region. Compared to transistors used in the field, these transistors have large fluctuations in electrical characteristics and are less reliable. However, amorphous oxide semiconductors tend to contain a relatively large amount of impurities. Since it can be formed by a film forming method, it is easy to form and is suitable for some applications. For example, spin coating, sol-gel, immersion, and spinning Plating, screen printing, contact printing, inkjet printing, roll-coating The amorphous oxide semiconductor may be formed by a film formation method such as a vapor deposition method or a mist CVD method. Therefore, a semiconductor device having a transistor using an amorphous oxide semiconductor for a channel region It can be produced with high productivity.

[0480] In addition, for example, the density of an oxide semiconductor is high when the number of defects is small. For example, when the crystallinity of hydrogen or the like is high, the density of the oxide semiconductor is high. For example, single-crystal oxide semiconductors have a high density when the concentration of impurities such as hydrogen is low. It may be denser than AC-OS. For example, CAAC-OS is a microcrystalline oxide. In addition, polycrystalline oxide semiconductors, for example, can have a higher density than microcrystalline oxide semiconductors. In addition, for example, a microcrystalline oxide semiconductor may have a higher density than an amorphous oxide semiconductor. The density may be higher than that of an oxide semiconductor.

[0481] (Embodiment 10) In this embodiment, a human body to which the semiconductor device of one embodiment of the present invention can be applied is The interface will be explained. In particular, the sensor that can detect the proximity or contact of the object to be detected will be described. A configuration example of a touch sensor will be described below.

[0482] Touch sensors include capacitive, resistive, surface elastic, infrared, and optical. Various methods can be used, such as the method.

[0483] Representative examples of capacitive touch sensors include surface capacitive touch sensors and projected capacitive touch sensors. In addition, the projected capacitive type has a self-driving function, which is mainly due to the difference in the driving method. There are capacitance type, mutual capacitance type, etc. Here, when using the mutual capacitance type, multiple points can be detected simultaneously. This is preferable because it enables multiple points to be detected (also called multi-touch).

[0484] Here, we will explain the touch sensor in detail, but in addition to this, cameras (infrared cameras The system detects the movement (gesture) of the object to be detected (e.g., finger or hand) and the user's gaze. Sensors that can detect point movements are used as a human interface. It is also possible.

[0485] <Example of sensor detection method> 32(A) and (B) are schematic diagrams showing the configuration of a mutual capacitance type touch sensor and input / output A touch sensor includes a pair of electrodes, and a capacitance is formed between the electrodes. An input voltage is input to one of the pair of electrodes. It is equipped with a detection circuit that detects the current (or the potential of the other electrode).

[0486] For example, as shown in FIG. 32(A), when a square wave is used as the input voltage waveform, the output voltage A waveform having a sharp peak is detected as a flow waveform.

[0487] As shown in FIG. 32(B), when a conductive object to be detected approaches or comes into contact with the capacitance, In this case, the capacitance between the electrodes decreases, and the output current value decreases accordingly.

[0488] In this way, the change in capacitance can be calculated using the change in output current (or potential) relative to the input voltage. By detecting the object, the proximity or contact of the object to be detected can be detected.

[0489] <Example of touch sensor configuration> FIG. 32C shows a configuration example of a touch sensor having a plurality of capacitors arranged in a matrix. Shows.

[0490] The touch sensor is made up of a number of wirings extending in the X direction (horizontal direction of the paper) and The wiring has a plurality of wirings that intersect and extend in the Y direction (the vertical direction of the paper). A capacitance is formed in the

[0491] In addition, the wiring extending in the X direction is used to carry the input voltage or common potential (including the ground potential and reference potential). In addition, a detection circuit (for example , source meter, sense amplifier, etc.) are electrically connected, and the current (or is the electric potential).

[0492] The touch sensor is designed so that the input voltage is input in sequence to multiple wirings extending in the X direction. By scanning in the Y direction and detecting changes in the current (or potential) flowing through the wiring extending in the Y direction, This enables two-dimensional sensing of the object to be detected.

[0493] <Touch panel configuration example> Below, a configuration example of a touch panel including a display unit having a plurality of pixels and a touch sensor will be described. An example in which the touch panel is incorporated into an electronic device will be described.

[0494] FIG. 33(A) is a schematic cross-sectional view of an electronic device equipped with a touch panel.

[0495] The electronic device 3530 includes a housing 3531 and at least a touch panel 3532 disposed in the housing 3531. 532, a battery 3533, and a control unit 3534. The touch panel 3532 is The display unit 3534 is electrically connected to the control unit 3534 via wiring 3535. The display of images on the touch sensor and the sensing operation of the touch sensor are controlled. 3 is electrically connected to the control unit 3534 via wiring 3536 and supplies power to the control unit 3534. can be supplied.

[0496] The touch panel 3532 is provided so that its display surface side is exposed outside the housing 3531. An image is displayed on the exposed surface of the touch panel 3532, and a touch panel 3533 is displayed on the exposed surface of the touch panel 3532. It is possible to detect a detection target.

[0497] 33B to 33E show configuration examples of a touch panel.

[0498] The touch panel 3532 shown in FIG. 33B includes a first substrate 3541 and a second substrate 354. A display panel 3540 having a display unit 3542 and a touch sensor 3544 are provided between the display panel 3540 and the touch sensor 3544. It includes a third substrate 3545 and a protection substrate 3546 .

[0499] The display panel 3540 may be a liquid crystal element, an organic EL (Electro Luminescence) It can be used in a variety of display devices, such as display devices using a Cence element and electronic paper. The touch panel 3532 may be configured with a backlight or polarizer depending on the configuration of the display panel 3540. A light plate or the like may be provided separately.

[0500] Since the object to be detected comes into contact with or is close to one surface of the protective substrate 3546, at least that surface It is preferable that the mechanical strength of the surface is increased. For example, the surface is strengthened by ion exchange or air cooling. The glass is physically or chemically treated to apply compressive stress to its surface. It can be used for a protective substrate 3546. Or, it can be used for a plastic substrate with a coated surface. A flexible substrate such as a plastic film may be used. A film may also be provided.

[0501] The touch sensor 3544 is provided on at least one surface of the third substrate 3545. Alternatively, a pair of electrodes constituting the touch sensor 3544 is formed on both sides of the third substrate 3545. In order to make the touch panel thinner, a flexible film may be used as the third substrate 3545. The touch sensor 3544 may be formed on a pair of substrates (including a film). A clamped configuration may also be used.

[0502] In FIG. 33B, a protection substrate 3546 and a third substrate having a touch sensor 3544 are Although the configuration shown is bonded with adhesive layer 3547, these are not necessarily bonded. In addition, the third substrate 3545 and the display panel 3540 may be bonded together by an adhesive layer. This may also be configured.

[0503] The touch panel 3532 shown in FIG. 33B is a display panel and a substrate having a touch sensor. The touch panel having such a configuration is called an external touch panel. This type of configuration allows the display panel and touch sensor to be By stacking these, the touch sensor function is realized on the display panel. This allows touch panels to be easily manufactured without any special manufacturing process. It can be manufactured.

[0504] The touch panel 3532 shown in FIG. 33C has a touch sensor 3544 on the second substrate 35. The touch panel having such a configuration is provided on the surface of the protection substrate 3546 of the touch panel 43. This can also be called an on-cell type touch panel. Since the number of sheets can be reduced, the touch panel can be made thinner and lighter.

[0505] In the touch panel 3532 shown in FIG. 33(D), a touch sensor 3544 is disposed on a protection substrate 354. With this configuration, the display panel and the touch panel are Since the sensors can be made separately, touch panels can be easily made. Furthermore, the number of substrates required can be reduced, making the touch panel thinner and lighter. This can be achieved.

[0506] The touch panel 3532 shown in FIG. 33(E) includes a touch sensor 3544. The touch panel having such a configuration is provided on the inner side of the pair of substrates of 40. This can also be called a cell-type touch panel. With this type of configuration, the number of substrates required is reduced. Since the number of touch panels can be reduced, the touch panel can be made thinner and lighter. The panel is a first substrate, for example, formed by transistors, wiring, electrodes, etc., provided in the display unit 3542. A circuit that functions as a touch sensor is fabricated on the plate 3541 or the second substrate 3543. In addition, when an optical touch sensor is used, a photoelectric conversion element is It may be configured to include the above.

[0507] <Example of in-cell touch panel configuration> The following describes the configuration of a touch panel in which a touch sensor is incorporated in a display unit having multiple pixels. Here, a liquid crystal element is used as a display element provided in a pixel. Here is an example.

[0508] FIG. 34(A) shows one of the pixel circuits provided in the display unit of the touch panel exemplified in this configuration example. FIG. 1 is an equivalent circuit diagram of a portion

[0509] One pixel has at least a transistor 3503 and a liquid crystal element 3504. A wiring 3501 is connected to the gate of the transistor 3503, and a wiring 3502 is connected to either the source or drain. 02 are electrically connected to each other.

[0510] The pixel circuit includes a plurality of wirings extending in the X direction (for example, wiring 3510_1, wiring 3510_2, _2) and a plurality of wirings (for example, wiring 3511) extending in the Y direction, which are mutually The electrodes are disposed so as to intersect with each other, and a capacitance is formed therebetween.

[0511] In addition, among the pixels provided in the pixel circuit, some adjacent pixels are The electrodes of the liquid crystal elements are electrically connected to each other to form one block. The lock is divided into island blocks (e.g., block 3515_1, block 3515_2) and , a linear block extending in the Y direction (e.g., block 3516) In addition, although FIG. 34 shows only a part of the pixel circuit, these two types of The blocks are arranged repeatedly in the X and Y directions.

[0512] The wiring 3510_1 (or 3510_2) extending in the X direction is arranged in an island-shaped block 351 5_1 (or block 3515_2). The wiring 3510_1 extending in the X direction is discontinuous along the X direction via a line-shaped block. The island-shaped blocks 3515_1 arranged in the Y direction are electrically connected to each other. The existing wiring 3511 is electrically connected to the line-shaped block 3516 .

[0513] FIG. 34B shows a plurality of wirings 3510 extending in the X direction and a plurality of wirings 3510 extending in the Y direction. FIG. 3 is an equivalent circuit diagram showing a connection configuration of the wiring 3511. An input voltage or a common potential can be input to the wiring 3 extending in the Y direction. A ground potential is input to each of the wirings 3511, or the wiring 3511 is electrically connected to the detection circuit. It is possible.

[0514] <Touch panel operation example> Hereinafter, the operation of the above-mentioned touch panel will be described with reference to FIG.

[0515] As shown in FIG. 35(A), one frame period is divided into a writing period and a sensing period. The write period is a period during which image data is written to the pixels, and the wiring 3510 (gate line On the other hand, during the detection period, sensing is performed by the touch sensor. During this period, the wirings 3510 extending in the X direction are selected in sequence and an input voltage is input.

[0516] FIG. 35B is an equivalent circuit diagram during the writing period. A common potential is input to both the wiring 3510 extending in the Y direction and the wiring 3511 extending in the Y direction. can be.

[0517] FIG. 35(C) is an equivalent circuit diagram at a certain point in the detection period. Each of the wirings 3511 extending in the X direction is electrically connected to a detection circuit. Of the wiring 3510, the input voltage is input to the selected one, and the other A common potential is input.

[0518] In this way, the image writing period and the period for sensing by the touch sensor are separated. This prevents touch noise caused by pixel writing noise. The decrease in sensitivity of the sensor can be suppressed.

[0519] (Embodiment 11) In this embodiment mode, a driving method for reducing power consumption of a display device will be described. A display device in which an oxide semiconductor transistor is used in a pixel is driven by the driving method of this embodiment. Further reduction in power consumption can be achieved. An example of reducing power consumption in a liquid crystal display device will now be described.

[0520] FIG. 36 is a block diagram showing an example of the configuration of a liquid crystal display device according to the present embodiment. As shown, the liquid crystal display device 500 has a liquid crystal panel 501 as a display module, and further , a control circuit 510 and a counter circuit.

[0521] The liquid crystal display device 500 receives an image signal (Video) which is digital data, and a liquid crystal panel. A synchronization signal (SYNC) is input to control rewriting of the screen of the panel 501. The signals include, for example, a horizontal synchronization signal (Hsync), a vertical synchronization signal (Vsync), and There are reference clock signals (CLK), etc.

[0522] The liquid crystal panel 501 includes a display unit 530, a scanning line driving circuit 540, and a data line driving circuit 550. The display unit 530 has a plurality of pixels 531. The pixels 531 in the same row are shared. The pixels 531 in the same column are connected to a common scanning line 541 to a scanning line driving circuit 540. The data line 551 is connected to a data line driving circuit 550 .

[0523] The liquid crystal panel 501 is supplied with a common voltage (Vcom) and a high power supply voltage ( The common voltage (Vcom) is supplied to the display unit 5. 30 pixels 531.

[0524] The data line driving circuit 550 processes the input image signal, generates a data signal, and The scanning line driving circuit 540 outputs a data signal to the data line 551. A scanning signal for selecting a pixel 531 to be scanned is output to a scanning line 541.

[0525] The pixel 531 is a switch whose electrical connection with the data line 551 is controlled by a scanning signal. When the switching element is turned on, a signal is sent from the data line 551 to the pixel 531. The data signal is written.

[0526] The electrode to which Vcom is applied corresponds to the common electrode.

[0527] The control circuit 510 is a circuit for controlling the entire liquid crystal display device 500. It is equipped with a circuit that generates a control signal for the circuit that constitutes 0.

[0528] The control circuit 510 controls the scanning line driver 540 and the data line driver 540 in response to a synchronization signal (SYNC). The scanning line driving circuit 540 has a control signal generating circuit that generates a control signal for the scanning line driving circuit 550. The control signals include a start pulse (GSP) and a clock signal (GCLK). A start pulse (SSP), a clock signal (SC For example, the control circuit 510 may generate clock signals (GCLK, SCLK) and This generates multiple clock signals with the same period but shifted phases.

[0529] The control circuit 510 also receives an image signal (Vide The output of the data line driver circuit 550 is controlled by the data line driver circuit 550.

[0530] The data line driving circuit 550 is a digital / analog conversion circuit (hereinafter, a DA conversion circuit 55 The DA conversion circuit 552 converts the image signal into an analog signal, and outputs a data signal. Generate a number.

[0531] When the image signal input to the liquid crystal display device 500 is an analog signal, the control circuit The signal is converted into a digital signal by a line 510 and output to a liquid crystal panel 501 .

[0532] The image signal is composed of image data for each frame. The control circuit 510 processes the image signal. Based on the information obtained by this processing, the output of the image signal to the data line driving circuit 550 is controlled. Therefore, the control circuit 510 detects the movement from the image data for each frame. When the motion detection unit 511 determines that there is no motion, Then, the control circuit 510 stops outputting the image signal to the data line driving circuit 550 and the motion is disabled. If it is determined that the image signal is not output, the output of the image signal is resumed.

[0533] There are no particular restrictions on the image processing for motion detection performed by the motion detection unit 511. For example, a motion detection method may be to extract differential data from image data between two consecutive frames. The difference data obtained can be used to determine whether there is movement or not. There are also methods for detecting motion vectors.

[0534] The liquid crystal display device 500 is also provided with an image signal correction circuit that corrects the input image signal. For example, a voltage higher than the voltage corresponding to the gray level of the image signal can be applied to the pixel 531. The image signal is corrected so that the image can be written in the correct manner. In this way, the image signal is corrected and processed to drive the control circuit 510. The method of changing the frame frequency of the image signal is called overdrive. When performing double-speed driving to drive the liquid crystal display device 500 at an integer multiple, the control circuit 510 Create image data that interpolates between two frames, or display black between two frames It is only necessary to generate image data for this purpose.

[0535] Below, using the timing chart shown in FIG. 37, we will explain how to deal with moving images such as video images, The operation of the liquid crystal display device 500 for displaying a motionless image such as a still image will now be described. FIG. 37 shows a vertical synchronization signal (Vsync) and a data line 550 from the data line driving circuit 550. The signal waveform of the data signal (Vdata) outputted to 51 is shown.

[0536] FIG. 37 is a timing chart of the liquid crystal display device 500 during a 3m frame period. So, there is motion in the image data for the first k frame period and the last j frame period. In other frame periods, there is no motion in the image data. Note that k and j are each 1 An integer greater than or equal to m-2 inclusive.

[0537] During the first k frame period, the motion detector 511 detects motion in the image data of each frame. Based on the result of the determination by the motion detector 511, the control circuit 510 The data signal (Vdata) is output to the data line 551 .

[0538] Then, the motion detection unit 511 performs image processing for motion detection, and the k+1th frame If it is determined that there is no motion in the image data, the control circuit 510 determines whether the motion detector 511 detects the motion. Based on the result, in the k+1-th frame period, the image signal (Vid eo) is stopped. Furthermore, in order to stop rewriting of the display unit 530, Therefore, a control signal (start pulse signal) to the scanning line driving circuit 540 and the data line driving circuit 550 is The control circuit 510 stops the supply of the signal (the signal, the clock signal, etc.). 1, the data line driving circuit 550 is turned on until a determination result that there is motion in the image data is obtained. output of the image signal, output of control signals to the scanning line driving circuit 540 and the data line driving circuit 550 The force is stopped and rewriting of the display unit 530 stops.

[0539] In this specification, "not supplying" a signal to the liquid crystal panel means that the signal is not supplied. Applying a voltage to the wiring that is different from the voltage specified for operating the circuit, or This refers to putting wiring into an electrically floating state.

[0540] When rewriting of the display unit 530 is stopped, the electric field in the same direction continues to be applied to the liquid crystal element. This may cause the liquid crystal in the liquid crystal element to deteriorate. Regardless of the result of the motion detection unit 511, the control circuit 510 outputs a scan signal at a predetermined timing. A signal is supplied to the line driving circuit 540 and the data line driving circuit 550, and a data A signal is written to the data line 551 to invert the direction of the electric field applied to the liquid crystal element. .

[0541] The polarity of the data signal input to the data line 551 is determined based on Vcom. The polarity is positive when the data signal voltage is higher than Vcom, and negative when it is lower. is the polarity.

[0542] Specifically, as shown in FIG. 37, in the (m+1)th frame period, the control circuit 510 , and outputs control signals to the scanning line driving circuit 540 and the data line driving circuit 550. The data line driving circuit 550 outputs an image signal Video to the data line driving circuit 550. During this period, the polarity of the data signal (Vdata) output to the data line 551 is inverted. The data signal (Vdata) is output to the data line 551. In the (m+1)th frame period and the (2m+1)th frame period in which the polarity is not detected, The inverted data signal (Vdata) is written to the data line 551. During the period when there is no change, the display unit 530 is rewritten intermittently, so that the power consumption due to the rewriting is This makes it possible to reduce costs and prevent deterioration of the liquid crystal element.

[0543] Then, the motion detection unit 511 detects whether there is any motion in the image data of the (2m+1)th frame and thereafter. When it is determined that the scanning line driving circuit 540 and the data line driving circuit 550 are to be driven, the control circuit 510 and rewrites the display unit 530.

[0544] As described above, according to the driving method of FIG. 37, the effectiveness of the motion of the image data (Video) is improved. Regardless of whether or not the data signal (Vdata) is inverted in polarity every m frame periods. On the other hand, the rewriting of the display unit 530 is performed for each frame during the display period of an image including a motion. The display unit 530 is rewritten, and the period during which a still image is displayed is every m frames. As a result, the power consumption associated with rewriting the display can be reduced. This makes it possible to suppress the increase in power consumption caused by an increase in the driving frequency and the number of pixels. Cut.

[0545] As described above, the liquid crystal display device 500 has a mode for displaying moving images and a mode for displaying still images. By changing the driving method of the LCD device in each mode, deterioration of the LCD can be suppressed and the display quality can be improved. It is therefore possible to provide a power-saving liquid crystal display device while maintaining a high level of image quality.

[0546] In addition, when displaying a still image, if the pixels are rewritten every frame, the human eye cannot read the rewritten pixels. In some cases, the image may appear as flickering, which can cause eye fatigue. Since the pixels of a display device are rewritten less frequently during the display period of a still image, this is effective in reducing eye fatigue. It is.

[0547] Therefore, it is possible to use a liquid crystal panel in which a backplane is formed using oxide semiconductor transistors. This provides a small- to medium-sized LCD display device with high resolution and low power consumption that is highly suitable for portable electronic devices. It is possible to do so.

[0548] In order to prevent deterioration of the liquid crystal, the interval between polarity inversions of the data signal (here, m frame periods) is The time between the start and end of the pulse should be 2 seconds or less, and preferably 1 second or less.

[0549] In addition, the motion detection of the image data was performed by the motion detection unit 511 of the control circuit 510. The motion detection unit 511 does not need to output the motion data. Alternatively, the signal may be input to the control circuit 510 from outside.

[0550] The condition for determining that there is no motion in the image data is the image data between two consecutive frames. The number of frames required for the determination does not depend on the data, but on the usage pattern of the liquid crystal display device 500. For example, if there is no motion in the image data of consecutive m frames, In this case, rewriting of the display unit 530 may be stopped.

[0551] In the present embodiment, a liquid crystal display device is used as the display device. The driving method of the above embodiment can be used for other display devices, for example, light-emitting display devices.

[0552] The structures and methods described in this embodiment may be used in conjunction with structures and methods described in other embodiments and examples. and the like.

[0553] (Embodiment 12) The semiconductor device according to one embodiment of the present invention can be applied to various electronic devices (including game machines). The electronic equipment includes a television set (television or television receiver) (also called a receiver.) Computer monitors, digital cameras, digital video cameras digital photo frames, mobile phones, portable game consoles, personal digital assistants, audio playback equipment These electronic devices include gaming machines (pachinko machines, slot machines, etc.) and game cabinets. An example of the device is shown in FIG.

[0554] FIG. 38(A) shows a table 9000 having a display section. A display unit 9003 is built into the housing 9001, and an image is displayed on the display unit 9003. It is possible to support the housing 9001 with four legs 9002. The housing 9001 also includes a power cord 9005 for supplying power.

[0555] The semiconductor device described in any of the above embodiments can be used for the display portion 9003. Therefore, the display quality of the display portion 9003 can be improved.

[0556] The display unit 9003 has a touch input function. By touching the display button 9004 displayed on the screen with a finger or the like, the screen can be operated or information can be input. It also allows communication with and control of other home appliances, It may also be used as a control device to control other home appliances by operating the screen. If a semiconductor device having a touch sensor function is used, the display portion 9003 can have a touch input function. It is possible.

[0557] In addition, the screen of the display unit 9003 can be fixed to the floor by a hinge provided in the housing 9001. It can also be placed vertically and used as a television set. A large-screen television set will take up a lot of free space, but it can be placed on a table. If the display unit is built into the device, the space in the room can be used more effectively.

[0558] FIG. 38(B) shows a television device 9100. A display unit 9103 is incorporated in a housing 9101, and an image is displayed on the display unit 9103. In this example, the housing 9101 is supported by a stand 9105. The configuration shown is as follows.

[0559] The television device 9100 can be operated using an operation switch provided on the housing 9101 or a separate remote control. This can be done by using a remote control operation device 9110. The channel and volume can be controlled by the 9109, and the display 9103 shows The remote control device 9110 can control the video. A display unit 9107 for displaying information output from the device 9110 may be provided.

[0560] A television device 9100 shown in FIG. 38(B) includes a receiver, a modem, and the like. The television device 9100 can receive general television broadcasts using a receiver. Furthermore, by connecting to a wired or wireless communication network via a modem, Either directional (from sender to receiver) or bidirectional (between sender and receiver, or between receivers, etc.) ) information communication is also possible.

[0561] The semiconductor device described in any of the above embodiments can be used for the display portions 9103 and 9107. This makes it possible to improve the display quality of the television device.

[0562] FIG. 38C shows a computer 9200, which includes a main body 9201, a housing 9202, a display unit 9 203, keyboard 9204, external connection port 9205, pointing device 920 6, etc.

[0563] The semiconductor device described in any of the above embodiments can be used for the display portion 9203. Therefore, the display quality of the computer 9200 can be improved.

[0564] The display unit 9203 has a touch input function. 03 Touch the display buttons with your finger to operate the screen or input information. It can also communicate with other home appliances or control them, making the screen It may also be a control device that controls other home appliances by operation.

[0565] FIG. 39(A) and FIG. 39(B) show a tablet terminal that can be folded in two. 9631a, the tablet terminal is in an open state. 9631b, a display mode changeover switch 9034, a power switch 9035, a power saving mode It has a mode changeover switch 9036, a fastener 9033, and an operation switch 9038.

[0566] The semiconductor device described in any of the above embodiments includes a display portion 9631a and a display portion 9631b. Therefore, it is possible to improve the display quality of tablet devices. Cut.

[0567] A part of the display unit 9631a can be used as a touch panel area 9632a. By touching the operation keys 9638 displayed on the display unit 96, data can be input. In 31a, as an example, half of the area has a display function only, and the other half The display unit 96 has a touch panel function, but is not limited to this. The entire area of ​​the display unit 931a may have a touch panel function. The entire surface of 631a is made to display keyboard buttons to serve as a touch panel, and the display section 9631b is made to display It can be used as a display screen.

[0568] In addition, in the display unit 9631b, as in the display unit 9631a, The part of the touch panel can be the area 9632b of the touch panel. Touch the area where the mode display switch button 9639 is displayed with your finger or a stylus. A keyboard button can be displayed on the display portion 9631b.

[0569] In addition, the touch panel area 9632a and the touch panel area 9632b are simultaneously You can also use touch input.

[0570] A display mode changeover switch 9034 is used to change the display orientation, such as portrait or landscape. You can switch between black and white and color display. The switch 9036 is a switch that turns on and off when the tablet terminal is in use and is detected by a light sensor built into the tablet terminal. The brightness of the display can be optimized according to the amount of light. In addition to sensors, other detection devices such as gyros, acceleration sensors, etc. that detect tilt may be incorporated.

[0571] FIG. 39A shows an example in which the display area of ​​the display portion 9631b is the same as that of the display portion 9631a. However, there is no particular limitation, and one size may be different from the other size. The quality of the display may also be different. For example, one display panel may provide a higher resolution display than the other. It may also be used as a rule.

[0572] FIG. 39(B) shows the tablet terminal in a closed state. The tablet terminal includes a housing 9630 and a solar cell 9 39B, the charge / discharge control circuit 96 As an example of the 34, a configuration having a battery 9635 and a DC-DC converter 9636 is described below. This is shown.

[0573] In addition, since the tablet device can be folded in half, the case 9630 can be folded when not in use. Therefore, the display portions 9631a and 9631b can be protected. This makes it possible to provide a tablet device that is highly durable and reliable even when used for a long period of time.

[0574] In addition, the tablet terminals shown in Figs. 39(A) and 39(B) can be used in various Functions that display information (still images, videos, text images, etc.), calendars, dates or times A function to display the information on the display, and a function to operate the information displayed on the display by touch input or editing. It has touch input function, function to control processing by various software (programs), etc. It is possible.

[0575] The solar cell 9633 attached to the surface of the tablet device supplies power to the touch panel. The solar cell 9633 can supply the light to a display unit, a video signal processor, or the like. , which can be provided on one or both sides of the housing 9630, and can efficiently charge the battery 9635. This is preferable because it can be configured to perform the operation efficiently. The use of lithium ion batteries has the advantage of enabling miniaturization.

[0576] The configuration and operation of the charge / discharge control circuit 9634 shown in FIG. A block diagram is shown in FIG. 39(C) and will be explained. In FIG. 39(C), a solar cell 9633 and a battery 9 635, DC-DC converter 9636, converter 9637, switches SW1 to SW3 , a display unit 9631, a battery 9635, a DC-DC converter 963 6. The converter 9637 and the switches SW1 to SW3 are configured to perform the charge / discharge control shown in FIG. This corresponds to the circuit 9634 .

[0577] First, an example of operation when power is generated by the solar cell 9633 due to external light will be described. The power generated by the solar cell is converted to a voltage to charge the Battery 9635. The CDC converter 9636 steps up or steps down the voltage. When power is supplied from the solar cell 9633, switch SW1 is turned on and the converter The voltage is increased or decreased by a voltage converter 9637 to a voltage required for the display unit 9631. When no display is to be made on the display unit 9631, the switch SW1 is turned off and the switch SW2 is turned on. It is sufficient to configure it so that the power is turned on and the battery 9635 is charged.

[0578] The solar cell 9633 is shown as an example of a power generating means, but is not limited thereto. , and other power generation methods such as piezoelectric elements and thermoelectric conversion elements (Peltier elements) For example, the battery 9635 may be charged. A non-contact power transmission module that transmits and receives power and charges, or a combination of other charging methods This may also be configured.

[0579] Note that the structure described in this embodiment mode may be appropriately combined with structures described in other embodiments. It can be used. EXAMPLES

[0580] In this example, the Vg-Id characteristics of the transistor and the measurement results of the optical BT stress test We will explain about this.

[0581] First, a manufacturing process of a transistor included in Sample 1 will be described. The following description will be given with reference to FIG.

[0582] First, as shown in FIG. 2(A), a glass substrate is used as the substrate 11, and a gate electrode is formed on the substrate 11. A contact electrode 15 was formed.

[0583] A tungsten film with a thickness of 100 nm was formed by sputtering, and then photolithography was performed. A mask is formed on the tungsten film by the process, and a part of the tungsten film is removed by using the mask. The portion was etched to form a gate electrode 15.

[0584] Next, a gate insulating film 17 (corresponding to GI in FIG. 40) was formed on the gate electrode 15.

[0585] The gate insulating film 17 is made of a first silicon nitride film having a thickness of 50 nm, a second oxide film having a thickness of 200 nm, and a third oxide film having a thickness of 200 nm. The silicon nitride film was formed by laminating a silicon nitride film.

[0586] The silicon nitride film was formed using silane at a flow rate of 50 sccm and nitrogen at a flow rate of 5000 sccm. The gas is supplied to the processing chamber of the plasma CVD device, and the pressure in the processing chamber is controlled to 60 Pa. The formation was performed by supplying 150 W of power using a 27.12 MHz high frequency power source.

[0587] Next, silane at a flow rate of 20 sccm and dinitrogen monoxide at a flow rate of 3000 sccm were used as the source gas. The pressure in the processing chamber is controlled to 40 Pa, and 27. A silicon oxynitride film is formed by supplying 100 W of power using a 12 MHz high frequency power supply. did.

[0588] In the process of forming the silicon nitride film and the silicon oxynitride film, the substrate temperature was set to 350 The temperature was set to °C.

[0589] Next, an oxide semiconductor film 18 is formed so as to overlap the gate electrode 15 via the gate insulating film 17. Ta.

[0590] Here, an oxide semiconductor film having a thickness of 35 nm is formed on the gate insulating film 17 by a sputtering method. Next, a mask was formed over the oxide semiconductor film by a photolithography process. A part of the oxide semiconductor film is etched using a mask to form an oxide semiconductor film 18 (S in FIG. 40 ). 1).

[0591] The oxide semiconductor film (S1) was formed by sputtering a sputtering target of In:Ga:Zn=1:1: The target was 1 (atomic ratio), and the flow rate was 100 sccm of argon and 100 sccm of m of oxygen is supplied as a sputtering gas into a processing chamber of a sputtering device, The pressure was controlled to 0.6 Pa, and a direct current of 5 kW was supplied to form the oxide semiconductor. The substrate temperature was set to 170° C. when the solid film was formed.

[0592] The structure obtained through the steps up to this point can be seen in FIG.

[0593] Next, a part of the gate insulating film 17 is etched to expose the gate electrode (not shown). 2C, a pair of electrodes 21 and 22 are formed in contact with the oxide semiconductor film 18. Successful.

[0594] Here, a conductive film was formed over the gate insulating film 17 and the oxide semiconductor film 18. As a result, an aluminum film having a thickness of 400 nm is formed on a tungsten film having a thickness of 50 nm. A titanium film having a thickness of 100 nm was formed on the aluminum film. A mask is formed on the conductive film by a process, and a part of the conductive film is wet-etched using the mask. A pair of electrodes 21 and 22 was formed by etching.

[0595] Next, the substrate is moved to a reduced pressure processing chamber, heated to 350° C., and then placed in the processing chamber. A high-frequency power of 150 W was supplied to the upper electrode using a 27.12 MHz high-frequency power source. The oxide semiconductor film 18 was exposed to oxygen plasma generated in a dinitrogen oxide atmosphere.

[0596] Next, a protective film 26 was formed on the oxide semiconductor film 18 and the pair of electrodes 21 and 22 (FIG. 2 Here, the protective film 26 is an oxide insulating film 23 (corresponding to P1 in FIG. 40). An oxide insulating film 24 (corresponding to P2 in FIG. 40) was formed.

[0597] First, after the above plasma treatment, the oxide insulating film 23 and the oxide film 24 are successively formed without being exposed to the air. As the oxide insulating film 23, a silicon oxynitride film having a thickness of 10 nm was formed. A silicon oxynitride film was formed as the oxide insulating film 24 to a thickness of 390 nm.

[0598] The oxide insulating film 23 is formed by silane at a flow rate of 20 sccm and dioxygen at a flow rate of 3000 sccm. Nitrogen was used as the source gas, the pressure in the processing chamber was 200 Pa, the substrate temperature was 350°C, and the The film was formed by the plasma CVD method in which high frequency power was supplied to parallel plate electrodes.

[0599] The oxide insulating film 24 is formed by using silane at a flow rate of 160 sccm and monoxide at a flow rate of 4000 sccm. Dinitrogen was used as the source gas, the pressure in the processing chamber was 200 Pa, the substrate temperature was 220°C, and The film was formed by the plasma CVD method in which a high-frequency power of 1000 MW was supplied to parallel plate electrodes. As a result, the mixture contains more oxygen than the stoichiometric composition, and some of the oxygen is removed by heating. A silicon oxynitride film can be formed to separate the insulating film.

[0600] Next, heat treatment is performed to remove water, nitrogen, hydrogen, and the like from the oxide insulating film 23 and the oxide insulating film 24. At the same time, part of oxygen contained in the oxide insulating film 24 is supplied to the oxide semiconductor film 18. Here, the heat treatment was carried out at 350° C. for 1 hour in a nitrogen and oxygen atmosphere.

[0601] Next, although not shown, a part of the protective film 26 is etched to expose one of the pair of electrodes 21 and 22. An opening was formed to expose the portion.

[0602] Next, a planarizing film was formed on the protective film 26 (not shown). After being coated on the substrate 26, the substrate 26 is exposed to light and developed to form a film having openings that expose a portion of the pair of electrodes. A planarizing film was formed by applying a 1.5 μm thick acrylic resin. After that, a heat treatment was carried out. The heat treatment was carried out at a temperature of 250° C. in a nitrogen-containing atmosphere. I went there for an hour.

[0603] Next, a conductive film was formed to connect to a part of the pair of electrodes (not shown). A 100 nm thick ITO film containing silicon oxide was formed by the ion beam deposition method. Heat treatment was carried out in a nitrogen atmosphere at 250° C. for 1 hour.

[0604] Through the above steps, Sample 1 having a transistor was manufactured.

[0605] In the transistor of Sample 1, the gate insulating film 17 is a first insulating film having a thickness of 50 nm. a silicon nitride film having a thickness of 100 nm, a second silicon nitride film having a thickness of 300 nm, and a third silicon nitride film having a thickness of 50 nm. The silicon film and the silicon oxynitride film having a thickness of 50 nm were laminated. Instead of the semiconductor film 18, a 35 nm thick oxide semiconductor film (corresponding to S1 in FIG. 40) and A multilayer film was formed by laminating an oxide film (corresponding to S2 in FIG. 40) having a thickness of 10 nm. After forming the pair of electrodes, the surface of the multilayer film was immersed in a phosphoric acid solution that was 100 times diluted with 85% phosphoric acid. The surface was cleaned. In addition, a 10 nm thick oxide insulating film 23 and a 10 nm thick The nitride insulating film 24 is formed of a 400 nm thick oxide insulating film and a 100 nm thick silicon nitride film. A nitride insulating film 25 (corresponding to P3 in FIG. 40) was laminated to form a sample having such a structure. The fee shall be 2.

[0606] In the sample 2, the first silicon nitride film to the third silicon nitride film constituting the gate insulating film 17 The conditions for forming the silicon film are as follows.

[0607] The first silicon nitride film was formed using a mixture of silane at a flow rate of 200 sccm and nitrogen at a flow rate of 2000 sccm. and ammonia at a flow rate of 100 sccm was used as the source gas in the processing chamber of the plasma CVD device. The pressure in the processing chamber was controlled to 100 Pa, and a high frequency power source of 27.12 MHz was used. It was formed by supplying 2000W of power.

[0608] Next, under the conditions of the source gas for the first silicon nitride film, the flow rate of ammonia was set to 2000 The flow rate was changed to sccm to form a second silicon nitride film.

[0609] Next, silane at a flow rate of 200 sccm and nitrogen at a flow rate of 5000 sccm were used as source gases. The gas was supplied to the processing chamber of the plasma CVD device, and the pressure in the processing chamber was controlled to 100 Pa. A third silicon nitride film was formed by supplying 2000 W of power using a 2 MHz high frequency power source. Successful.

[0610] In the sample 2, the oxide film (S2) in contact with the oxide semiconductor film 18 was formed under the following conditions: The oxide film (S2) was formed by sputtering a sputtering target of In:Ga:Zn=1:3:2 ( The sputtering gas was 180 sccm Ar and 20 s ccm of oxygen was supplied to the processing chamber of the sputtering device, and the pressure in the processing chamber was set to 0.6 Pa. The oxide film was formed by controlling the temperature of the substrate and supplying 5 kW of DC power. The temperature was set to 170°C.

[0611] In sample 2, the deposition conditions for nitride insulating film 25 (corresponding to P3 in FIG. 40) are as follows. The nitride insulating film 25 is formed by mixing silane at a flow rate of 50 sccm, nitrogen at a flow rate of 5000 sccm, and The source gas was ammonia at a rate of 100 sccm, the pressure in the processing chamber was 100 Pa, and the substrate temperature was The plasma CVD method was performed at 350°C and with 1000 W of high-frequency power supplied to parallel plate electrodes. It was formed.

[0612] In addition, in the transistor of Sample 1, the gate insulating film 17 has the same structure as that of Sample 2. After the oxide semiconductor film 18 was formed, a heat treatment was performed at 450° C. In addition, after forming a pair of electrodes, the sample was treated with 85% phosphoric acid at 100 times the concentration. The surface of the oxide semiconductor film 18 was washed with a phosphoric acid solution diluted to 100%. The thickness of the insulating film 23 was set to 50 nm. The oxide insulating film 23 (corresponding to P1 in FIG. 40) The film formation temperature was set to 220° C. As the protective film, the same as in Sample 2, The oxide insulating film 23, the oxide insulating film 24, and the nitride insulating film 25 (corresponding to P3 in FIG. 40) were stacked and formed. A sample having such a structure is designated as Comparative Sample 1.

[0613] Further, in Comparative Sample 1, a sample in which the heat treatment temperature after forming the oxide semiconductor film 18 was set to 350 °C is designated as Comparative Sample 2.

[0614] Further, in Comparative Sample 1, instead of the oxide semiconductor film 18, a sample provided with a multilayer film of the oxide semiconductor film 18 and the oxide film was prepared using the same structure and conditions as in Sample 2, and this sample is designated as Comparative Sample 3.

[0615] Note that the transistors included in each sample have a channel length (L) of 6 μm and a channel width (W ) of 50 μm.

[0616] <Vg-Id characteristics> Next, the Vg-Id characteristics of the transistors included in Sample 1 and Sample 2, and Comparative Sample 1 and Comparative Sample 2 were measured as initial characteristics. Here, the substrate temperature was set to 25 °C, the potential difference between the source and drain (hereinafter referred to as drain voltage) was set to 1 V and 10 V, and the potential difference between the source-gate electrodes (hereinafter referred to as gate voltage) was changed from -15 V to +15 V, and the change characteristics of the current flowing between the source and drain (hereinafter referred to as drain current), that is, the Vg-Id characteristics were measured.

[0617] FIG. 40 shows the Vg-Id characteristics of the transistors included in each sample. In each graph shown in FIG. 40, the horizontal axis represents the gate voltage Vg, the vertical axis represents the drain current Id, and the right vertical axis represents the field effect mobility. Note that the horizontal axis is shown from -15 V to 15 V. Also, the solid line ​​​​The dashed lines indicate the Vg-Id characteristics when the drain voltage Vd is 1 V and 10 V, respectively. The field effect mobility is shown as a function of gate voltage when the drain voltage Vd is set to 10 V. The field effect mobility is the result in the saturation region for each sample.

[0618] In addition, for each sample, 20 transistors with the same structure were fabricated within the substrate.

[0619] As shown in FIG. 40, in each of Sample 1 and Sample 2, and Comparative Sample 1 and Comparative Sample 2, It is clear that good switching characteristics are obtained.

[0620] Next, the BT stress test and the light test of Sample 1 and Sample 2, and Comparative Sample 1 and Comparative Sample 2 were performed. A BT stress test was conducted. The BT stress test is a type of accelerated test, and is suitable for long-term use. This allows the change in transistor characteristics (i.e., change over time) to be evaluated in a short period of time. It is important to check the amount of change in transistor characteristics before and after the BT stress test in order to improve reliability. This is an important indicator for investigating the following:

[0621] <Gate BT stress test and optical gate BT stress test> First, a gate BT stress test and an optical gate BT stress test were performed.

[0622] Here, the measurement method of the gate BT stress test will be explained. The Vg-Id characteristics of the transistor at its initial stage are measured.

[0623] Next, the substrate temperature is kept constant at a given temperature (hereinafter referred to as the stress temperature). A pair of electrodes that function as the source and drain of the transistor are set to the same potential, and the source and drain electrodes A potential different from that of the pair of electrodes that function as drain electrodes is applied to the gate electrode for a certain period of time (hereafter, Next, the substrate temperature is appropriately set and the electrical characteristics of the transistor are As a result, the threshold voltage and the shunt current in the electrical characteristics before and after the gate BT stress test were measured. The difference in the soft values ​​can be obtained as the amount of fluctuation.

[0624] The stress test in which a negative voltage is applied to the gate electrode is called the negative gate BT stress test. A stress test in which a positive voltage is applied is called a Dark GBT. This is called a stress test (Dark +GBT). In addition, a negative voltage is applied to the gate electrode while irradiating light. The stress test in which a voltage is applied is called a photo-negative gate BT stress test (Photo -GBT ), and the stress test in which a positive voltage is applied is called the optical positive gate BT stress test (Pho to +GBT).

[0625] Here, the gate BT stress conditions are a stress temperature of 60°C and a stress time of 3 The gate electrode was applied with -30 V or +30 V, and the source and drain electrodes were applied with 0 V for 600 seconds. At this time, the electric field strength applied to the gate insulating film was set to 0.66 MV / cm. .

[0626] In addition, using the same conditions as the BT stress test, 10,000 lx white LED light was used. The transistor was irradiated with light and a light gate BT stress test was performed. After the BT stress test, The measurement temperature for the Vg-Id characteristics of the transistor was set to 60°C.

[0627] The initial characteristics of the transistors included in Sample 1 and Sample 2, and Comparative Sample 1 and Comparative Sample 2 The difference between the threshold voltage after the BT stress test and the threshold voltage after the BT stress test (i.e., the variation of the threshold voltage) The difference between the shift values ​​(i.e., the amount of change in the shift value (ΔShift)) is shown in FIG. In FIG. 41(A), a positive gate BT stress test (Dark +G BT), negative gate BT stress test (Dark -GBT), light positive gate BT Stress test (Photo +GBT), Photo negative gate BT stress test (Phot o -GBT) are shown.

[0628] Next, a stress test was carried out by changing the stress temperature. Under the conditions of the stress test, the gate BT stress test was performed at a stress temperature of 125°C. The measurement temperature for the Vg-Id characteristics of the transistor after the gate BT stress test was 4 The temperature was set to 0°C.

[0629] Variation in threshold voltages in Sample 1 and Sample 2, and Comparative Sample 1 and Comparative Sample 2 (ΔVth) and the amount of change in the shift value (ΔShift) are shown in FIG. 41(B). In the positive gate BT stress test (Dark +GBT), negative gate BT The amount of variation for each stress test (Dark-GBT) is shown.

[0630] Here, the threshold voltage and the shift value in this specification will be described with reference to FIG. .

[0631] In this specification, the threshold voltage (Vth) is expressed as the gate voltage (Vg [V]) on the horizontal axis, Square root of drain current (Id 1 / 2 In the curve 612 plotted with [A] as the vertical axis, The maximum slope is Id 1 / 2 When the tangent 614 of the tangent 614 is extrapolated, the tangent 614 and the Vg axis (i.e. Id 1 / 2 This is defined as the gate voltage at the intersection with 0A (see FIG. 42(A)). In this specification, the threshold voltage is calculated assuming that the drain voltage Vd is 10 V. In this specification, the threshold voltage (Vth) is the threshold voltage of 20 transistors included in each sample. This is the average Vth of each tester.

[0632] In this specification, the shift value (Shift) is the gate voltage (Vg [V]). In the curve 616, which is a plot of the logarithm of the drain current (Id [A]) on the vertical axis, When the tangent 618 of the large slope Id is extrapolated, the straight line Id = 1.0 × 10 -12 [A] and The gate voltage at the intersection of the gate electrodes is defined as the gate voltage at the intersection of the gate electrodes (see FIG. 42(B)). The shift value is calculated with the rain voltage Vd set to 10 V. The value is the average shift value of each of the 20 transistors included in each sample.

[0633] From FIG. 41(A), when the stress temperature is 60°C, the Samples 1 and 2 were subjected to a positive gate BT stress test (Dark +GBT) and It can be seen that the amount of variation in the Inasgate BT stress test (Dark-GBT) is small.

[0634] From FIG. 41(B), when the stress temperature is 120° C., the results are compared with those of Comparative Sample 1 and Comparative Sample 2. Samples 1 and 2 were subjected to a positive gate BT stress test (Dark +GBT) and It can be seen that the amount of variation in the negative gate BT stress test (Dark -GBT) is small.

[0635] From the above, after the oxide semiconductor film or the multilayer film is formed, no special heat treatment is required. In either case, the deposition temperature of the oxide insulating film formed on the oxide semiconductor film or the multilayer film is set to 280° C. or higher. By setting the temperature at 400° C. or lower, impurities can be eliminated from the oxide semiconductor film or the multilayer film. It is clear that this is possible and that the amount of variation in transistor characteristics can be reduced.

[0636] In addition, in Samples 1 and 2, and Comparative Samples 1 and 3, the positive gate B A T stress test (Dark +GBT) was performed. Here, the stress temperature was increased to 60°C. or 125°C, and the stress time was 100 seconds, 500 seconds, 1500 seconds, The amount of change in the threshold voltage was measured for 2000 seconds and 3600 seconds. The graph shows the variation of the threshold voltage over time and the approximate curve obtained from each variation. The vertical axis indicates the time required for switching, and the vertical axis indicates the amount of change in threshold voltage (ΔVth). 43(B) shows the measurement results when the stress temperature is 125°C. The measurement results are shown at ℃.

[0637] As shown in FIG. 43A, the amount of change in threshold voltage of Samples 1 and 2 compared to Comparative Sample 1 is This shows that the oxide semiconductor film or multilayer film is formed and then heated. The oxide insulating film formed on the oxide semiconductor film or the multilayer film can be formed at a low temperature without heat treatment. By setting the temperature at 280°C or higher and 400°C or lower, the amount of variation in transistor characteristics can be reduced. I realized that...

[0638] In addition, from FIG. 43(A) and FIG. 43(B), the change in the transistor characteristics of Sample 1 and Sample 2 The amount of variation is larger than that of Comparative Sample 3, but it is found that the amount of variation is the same as that of Comparative Sample 3. do. EXAMPLES

[0639] In this example, the water and oxygen from the oxide insulating film 23 and the oxide insulating film 24 described in Embodiment 1 were The amount of oxygen released and the amount of defects in the film will be described below.

[0640] First, the amount of water and oxygen desorbed was measured by TDS measurement of a sample having an oxide insulating film. An evaluation was performed.

[0641] First, the sample preparation process will be described.

[0642] A silicon wafer was subjected to plasma etching under the conditions for the oxide insulating film 23 described in the first embodiment. A silicon oxynitride film was formed by a CVD method. This sample was designated as Sample 3. The silicon oxynitride film contained therein had a thickness of 100 nm.

[0643] The silicon oxynitride film included in sample 3 was formed by silane with a flow rate of 20 sccm and a flow rate of 3000 s ccm of dinitrogen monoxide was supplied as a source gas to the processing chamber of the plasma CVD device. The pressure was controlled at 200 Pa, the substrate temperature was set at 350°C, and the high frequency power supply was set at 27.12 MHz. The formation was carried out by supplying 100 W of power using the .

[0644] In addition, a silicon wafer was subjected to a process for forming the oxide insulating film 24 under the conditions described in the first embodiment. A silicon oxynitride film was formed by plasma CVD. This sample was designated as Sample 4. The silicon oxynitride film contained in Sample 4 had a thickness of 400 nm.

[0645] The silicon oxynitride film included in Sample 4 was formed by silane with a flow rate of 160 sccm and The source gas was dinitrogen monoxide at 0 sccm, the pressure in the processing chamber was 200 Pa, and the substrate temperature was 22 It was formed by the plasma CVD method in which the temperature was set to 0°C and high-frequency power of 1500 W was supplied to the parallel plate electrodes. Under these conditions, a silicon oxynitride film can be formed that contains more oxygen than stoichiometric oxygen and from which a part of the oxygen desorbs upon heating.

[0646] Also, a silicon oxynitride film was formed on a silicon wafer by the plasma CVD method under conditions of lower film formation pressure and film formation temperature compared to Sample 3. This sample was used as Comparative Sample 4. Note that the film thickness of the silicon oxynitride film contained in Comparative Sample 4 was 400 nm.

[0647] The silicon oxynitride film contained in Comparative Sample 4 was formed by supplying silane with a flow rate of 30 sccm and dinitrogen monoxide with a flow rate of 400 sccm as source gases to the processing chamber of a plasma CVD apparatus, controlling the pressure in the processing chamber to 40 Pa, setting the substrate temperature to 220°C, and supplying power of 150 W using a 27.12 MHz high-frequency power source.

[0648] <TDS Measurement> The results of TDS measurements for Sample 3, Sample 4, and Comparative Sample 4 are shown in Fig. 44. The upper part of Fig. 44 shows the measurement results representing the desorption amount of water molecules, and the lower part of Fig. 44 shows the measurement results representing the desorption amount of oxygen molecules.

[0649] As shown in the upper part of Fig. 44, in Comparative Sample 4, a peak of M / z = 18 corresponding to the mass number of water molecules was confirmed. On the other hand, it was confirmed that for Sample 3 and Sample 4, the peak intensity in the vicinity of a substrate temperature of 50°C to 150°C was smaller compared to Comparative Sample 4. From this, it can be seen that the films formed using the conditions of the oxide insulating film 23 and the oxide insulating film 24 of Embodiment 1 have a low water content. ​

[0650] As shown in the lower part of FIG. 44, in Sample 4, M / z = 3 corresponding to the mass number of oxygen molecules A peak of 2 was confirmed. On the other hand, in Samples 3 and Comparative Sample 4, compared with Sample 4, the substrate temperature It was confirmed that the peak intensity at 300°C to 400°C was small. From this, it can be seen that the film formed using the conditions of the oxide insulating film 24 in Embodiment 1 has a high oxygen content.

[0651] Next, the amount of defects in the oxide insulating films contained in Sample 3, Sample 4, and Comparative Sample 4 will be described using the ESR (electron spin resonance) measurement results.

[0652] First, the structure of the evaluated samples will be described.

[0653] A sample in which a silicon oxynitride film contained in Sample 3 is formed on a quartz substrate is designated as Sample 5. The thickness of the silicon oxynitride film contained in Sample 5 was 100 nm.

[0654] A sample in which a silicon oxynitride film contained in Sample 4 is formed on a quartz substrate is designated as Sample 6. The thickness of the silicon oxynitride film contained in Sample 6 was 400 nm.

[0655] A sample in which a silicon oxynitride film contained in Comparative Sample 4 is formed on a quartz substrate is designated as Comparative Sample 5. The thickness of the silicon oxynitride film contained in Comparative Sample 5 was 400 nm.

[0656] <ESR Measurement> Next, ESR measurements were performed on Sample 5, Sample 6, and Comparative Sample 5. The ESR measurement is based on the equation g = hν / βH from the value (H0) of the magnetic field at which microwave absorption occurs at a predetermined temperature. ​​0, a parameter called g value is obtained by using ν, where ν is the microwave frequency. h is the Planck constant and β is the Bohr magneton, both of which are constants.

[0657] Here, the ESR measurements were performed under the following conditions: the measurement temperature was -170°C, and the applied current was 8.92G. The microwave power was set at 1 mW at 100 Hz, and the magnetic field was oriented along the film surface of the sample. The surface was parallel to the plane. Note that the g value, which is derived from the dangling bond of silicon, appears at 2. The detection limit for the spin density of the signal is 1.1×10 11 The number of spins was small. The smaller the thickness, the fewer defects, which are dangling bonds of silicon.

[0658] The first derivative curves obtained by ESR measurement for each sample are shown in the upper part of Figure 45. In each sample, the g value of 2, which is due to the dangling bond of silicon, appears. The spin density of the signal is shown in the lower part of Figure 45. Note that the measured spin number is expressed in units of The spin density per unit area is shown.

[0659] In this case, in order to measure the change in the amount of defects caused by the heat treatment, The ESR measurement was performed for each sample. In Fig. 45, the measurement results before heat treatment are shown as The measurement results after heat treatment at 350°C are indicated as -depo and the measurement results after heat treatment at 350°C are indicated as 350°C.

[0660] As shown in the upper part of FIG. 45, the silicon oxynitride film included in Sample 5 has the following characteristics before and after the heat treatment: In the present study, no signal with symmetry was detected at a g value of 2. The silicon oxynitride film contained in the semiconductor device has very few defects or no defects. It becomes clear that...

[0661] On the other hand, the silicon oxynitride films included in Sample 6 and Comparative Sample 5 had the following properties before the heat treatment: A signal with symmetry at a g value of 2 was detected, indicating that a defect was included. In sample 6, a signal having symmetry at a g value of 2 was detected after heat treatment. However, in the case of comparative sample 5, the g value after heat treatment is symmetric at 2. No signal was detected. This indicates that the heat treatment of the comparative sample 5 It can be seen that the amount of defects is reduced or no defects are present.

[0662] From the above, it can be seen that the defect amount can be reduced by using the conditions for the oxide insulating film 23 described in Embodiment 1. It was found that an oxide insulating film with little damage could be formed. EXAMPLES

[0663] In this example, the deposition temperature of the oxide insulating film 23 and the oxide semiconductor film and the oxide In this embodiment, the relationship between the concentration of hydrogen contained in the oxide semiconductor insulating film and the concentration of hydrogen contained in the oxide semiconductor insulating film will be described. The hydrogen concentration was measured by SIMS on a sample with a laminated body and oxide insulating film. .

[0664] First, the sample preparation process will be described.

[0665] A 100 nm-thick oxide semiconductor film (corresponding to OS in Figure 46) was sputtered onto a quartz substrate. Next, a heat treatment was performed.

[0666] Here, the oxide semiconductor film was formed under the same conditions as those of the oxide semiconductor film included in Sample 1 described in Example 1. A nitride semiconductor film was formed. The film was then heat-treated at 350°C for 1 hour in a nitrogen atmosphere. Subsequently, heat treatment was performed at 350 °C for 1 hour in an atmosphere containing nitrogen and oxygen.

[0667] Next, using the conditions of the oxide insulating film 23 sho...

Claims

1. a gate electrode on a substrate; A gate insulating film on the gate electrode, an oxide semiconductor film on the gate insulating film; an oxide film over the oxide semiconductor film, A pair of electrodes on the oxide film, the oxide semiconductor film contains In, Ga, and Zn; The oxide film contains In, Ga, and Zn, The pair of electrodes includes Ti, the oxide semiconductor film has a region that functions as a channel formation region, The oxide film has a non-single crystal structure and contains c-axis oriented crystals, an atomic ratio of Ga contained in the oxide film is greater than an atomic ratio of Ga contained in the oxide semiconductor film; The atomic ratio of the oxide film satisfies Ga>In and Zn>Ga.

2. In claim 1, An oxide insulating film is provided. A nitride insulating film is provided on the oxide insulating film, The oxide film is disposed between the oxide semiconductor film and the oxide insulating film.

3. In claim 1 or 2, the nitride insulating film comprises silicon or aluminum; The oxide insulating film is a semiconductor device having silicon.

4. In any one of claims 1 to 3, The gate electrode comprises an element selected from the group consisting of aluminum, chromium, copper, tantalum, titanium, molybdenum, and tungsten.

Citation Information

Patent Citations

  • Amorphous oxide and field effect transistor

    JP2006165529A

  • Thin film transistor and method of manufacturing the same, and device with thin film transistor

    JP2012059860A

  • Semiconductor integrated circuit

    JP2012257187A

  • Semiconductor device and method for manufacturing the same

    JP2007096055A

  • Semiconductor device and its manufacturing method

    JP2007123861A