Electrochemical device
The electrochemical device addresses undissolved metal films and precipitation issues by using insulating films and a specific electrolyte composition, ensuring consistent mirror state performance through improved Ag solubility and reduced contamination.
Patent Information
- Application Number
- JP2023080010
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-15
- Publication Date
- 2024-11-27
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing electrochemical devices face issues with undissolved metal films and metal salt precipitation, leading to areas where no metal film can be obtained, which affects the mirror state performance.
The electrochemical device incorporates a configuration with insulating films and a specific electrolyte composition, including a solvent with a low dielectric constant and mediators like Ti, Bi, and Sn, to prevent undissolved metal films by minimizing solvent contamination and maintaining Ag ion solubility.
This configuration effectively prevents the formation of undissolved metal films and Ag precipitation, ensuring consistent mirror state performance even with repeated cycling.
Smart Images

Figure 2024164499000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to electrochemical devices. [Background technology]
[0002] There is known an electrodeposition type electrochemical device that holds an electrolyte solution between opposing electrodes and can deposit / dissolve a mirror layer (metal film) made of Ag on the electrodes by electrochemical reaction (see, for example, Japanese Patent No. 6738679). According to the study by the inventors of the present application, in this type of electrochemical device, depending on the combination of constituent materials, when the deposition and dissolution of the metal film are repeated, there are cases where the metal film remains undissolved at the timing when the metal film is dissolved to make it transparent. Furthermore, when the metal film remains undissolved, there are cases where certain constituent materials cause deposition of metal salts and the occurrence of areas where the metal film is not obtained. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Patent No. 6738679 Summary of the Invention [Problem to be solved by the invention]
[0004] One of the objects of a specific embodiment of the present disclosure is to provide a technique capable of eliminating undissolved metal film in an electrochemical device. [Means for solving the problem]
[0005] An electrochemical device according to one embodiment of the present disclosure includes: A first substrate and a second substrate arranged such that one surface of each substrate faces each other; A first electrode provided on one surface of the first substrate; A second electrode provided on one surface side of the second substrate; an electrolyte layer provided between the first electrode and the second electrode; a sealant provided between the first substrate and the second substrate so as to surround the electrolyte layer; an insulating film provided on one surface of at least one of the first electrode and the second electrode, the insulating film having a protruding portion protruding by a predetermined width toward a side closer to the electrolyte layer than an end of the sealing material on a side in contact with the electrolyte layer; Including, The electrolyte layer is an electrolyte solution containing an electrodeposition material containing Ag, a mediator containing one or more metal salts containing Ti, Bi, Cu, or Sn, a supporting salt, and a solvent. It is an electrochemical device.
[0006] According to the above configuration, a technique is provided that can eliminate the undissolved metal film in an electrochemical device. [Brief description of the drawings]
[0007] [Figure 1] Fig. 1(A) is a schematic cross-sectional view for explaining the configuration of an electrochemical device of one embodiment, and Fig. 1(B) is a schematic plan view for explaining the configuration of an electrochemical device of one embodiment. [Diagram 2] 2A and 2B are diagrams showing examples of waveforms of driving voltages. [Diagram 3] FIG. 3 is a schematic cross-sectional view for illustrating the configuration of an electrochemical device of a comparative example. [Figure 4] FIG. 4 is a graph showing the change in sheet resistance of the ITO film versus the immersion time in the electrolyte solution. [Diagram 5] 5(A) to 5(D) are diagrams showing schematic diagrams illustrating changes over time when a driving voltage is repeatedly applied to an electrochemical device of a comparative example. [Figure 6] Fig. 6(A) is a diagram for explaining the mechanism by which the solubility of Ag ions decreases in the electrochemical device of the comparative example, and Fig. 6(B) is a diagram for explaining the mechanism of operation in the electrochemical device of the embodiment. [Figure 7]FIG. 7 is a graph showing the change in reflectance when a driving voltage is repeatedly applied to the electrochemical devices of the comparative example and the example. [Figure 8] 8(A) to 8(C) are schematic cross-sectional views illustrating the configuration of an electrochemical device according to a modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] Fig. 1(A) is a schematic cross-sectional view for explaining the configuration of an electrochemical device of one embodiment. Fig. 1(B) is a schematic plan view for explaining the configuration of an electrochemical device of one embodiment. The cross-sectional view shown in Fig. 1(A) corresponds to the cross section taken along line aa shown in Fig. 1(B). The electrochemical device (electrodeposition device) of this embodiment is used, for example, as a mirror device that can be switched between a transparent state and a mirror state.
[0009] The first substrate 11 and the second substrate 12 are disposed so that one surface of each substrate faces each other. Transparent substrates such as glass substrates and resin substrates are used as the first substrate 11 and the second substrate 12. Spacers (not shown) are provided between the first substrate 11 and the second substrate 12, and the space between the substrates is maintained at several μm to several hundred μm by the spacers. As the spacers, for example, spherical, columnar or partition-shaped spacers formed of resin can be used.
[0010] The first electrode 13 is provided on one surface of the first substrate 11. The second electrode 14 is provided on one surface of the second substrate 12. As the first electrode 13 and the second electrode 14, for example, a transparent conductive film such as a tin-doped indium oxide film (ITO film), a lead-doped indium oxide film (IZO film), a fluorine-doped tin oxide film (FTO film), or an antimony-doped tin oxide film (AZO film) can be used. Each electrode may be made of a conductive polymer such as polypyrrole or PEDOT (poly 3,4-ethylenedioxythiophene), or a material such as IrOx, MnOx, CrOx, NiOx, or WOx (x is any positive value in each case).
[0011] The first insulating film 15 is provided on one surface of the first electrode 13 (the surface facing the second substrate 12). The second insulating film 16 is provided on one surface of the second electrode 14 (the surface facing the first substrate 11). The first insulating film 15 and the second insulating film 16 are provided in a substantially rectangular and annular (frame-like) shape in a plan view, as shown in FIG. 1(B) by the patterns of their formation ranges. The first electrode 13 is exposed on the inner side of the first insulating film 15 in a plan view, and the second electrode 14 is exposed on the inner side of the second insulating film 16 in a plan view.
[0012] The first insulating film 15 and the second insulating film 16 each have a corner portion 20, which is a curved portion, at each of the four corners of a substantially rectangular shape in a plan view. In the illustrated example, each corner portion 20 is an arc-shaped portion. It is desirable that the radius of curvature R of each corner portion 20 is at least 3 mm. In other words, the lower limit of the radius of curvature R of each corner portion 20 is 3 mm. The upper limit of the radius of curvature R may be appropriately set depending on the size of the electrochemical device, etc.
[0013] The first insulating film 15 and the second insulating film 16 can be formed using an inorganic material or an organic material having insulating properties. Specifically, for example, SiOx or SiNx (x is any positive value in both cases) can be used as an inorganic material, and for example, acrylic resin or siloxane resin can be used as an organic material. The film thickness of the first insulating film 15 and the second insulating film 16 is preferably, for example, 10 nm or more and 1000 nm or less, and more preferably 50 nm or more and 500 nm or less.
[0014] The electrolyte layer 17 is provided between each one surface of the first electrode 13 and the second electrode 14. The electrolyte layer 17 is a liquid or gel layer containing an electrodeposition material, a supporting salt, and a mediator in a solvent.
[0015] The electrodeposition material may be a material (metal salt) containing one or more metal elements selected from the group consisting of silver (Ag), bismuth (Bi), chromium (Cr), iron (Fe), cadmium (Cd), cobalt (Co), nickel (Ni), tin (Sn), lead (Pb), and copper (Cu). The material containing silver may be, for example, AgNO3, AgCl, AgClO4, or AgBr, and the material containing bismuth may be, for example, Bi(NO3)3, BiCl3, or BiBr3. The concentration of the electrodeposition material may be, for example, 50 mM or more and 1000 mM or less, and more preferably, 200 mM or more and 800 mM or less.
[0016] The supporting salt is not particularly limited as long as it promotes the oxidation-reduction reaction of the electrodeposition material, and for example, lithium salts (LiCl, LiBr, LiI, LiBF4, LiClO4, etc.), potassium salts (KCl, KBr, KI, etc.), and sodium salts (NaCl, NaBr, NaI, etc.) can be used. When using lithium salts as the supporting salt, the concentration ratio of Li to the metal element of the electrodeposition material is preferably 1:1 or more, and more preferably 1:2 or more and 1:8 or less.
[0017] As the mediator, for example, a material containing copper can be used. A mediator containing copper causes the electrolyte layer to become colored. By using a material containing tantalum (Ta) as the mediator, the electrolyte layer can be made almost colorless. Note that the transparency of the electrolyte layer can be increased by using a mediator containing molybdenum (Mo), niobium (Nb), or the like other than tantalum. Specifically, TaCl5, MoCl5, NbCl5, or the like can be used.
[0018] The solvent is not particularly limited as long as it can stably hold the electrodeposition material, etc., and for example, N,N-dimethylacetamide, 4-butyrolactone, dimethylsulfoxide, tetrahydrofuran, propylene carbonate, acetonitrile, etc. can be used. The gelling agent is not necessarily used. When gelling the electrolyte layer, there is no particular limitation as long as the polymer is stable in the solvent, and for example, polyvinyl alcohol resin, polyvinyl butyral resin, polyvinylidene fluoride resin, etc. can be used.
[0019] The sealant 18 is provided between each surface of the first substrate 11 and the second substrate 12 so as to surround the electrolyte layer 17. The sealant 18 is for sealing the electrolyte layer 17, and is not particularly limited as long as it is a material that can stably hold the electrolyte layer 17, but for example, a photocurable resin, a thermosetting resin, glass frit, etc. can be used. As an example, in this embodiment, the sealant 18 is made of an ultraviolet-curable resin.
[0020] 1(A), the sealant 18 has a portion in contact with each of the first insulating film 15 and the second insulating film 16, and is provided so as not to have a portion in direct contact with each of the first substrate 11 and the second substrate 12. As shown in the figure, the sealant 18 is not provided within a range of width L1 from the end of the inner side (the side closer to the electrolyte layer 17) of the first insulating film 15, but is provided outside the range of width L1 (the side farther from the electrolyte layer 17).
[0021] In other words, the first insulating film 15 has a protruding portion 15a that protrudes by a width L1 toward the side closer to the electrolyte layer 17 than the end of the sealing material 18 that contacts the electrolyte layer 17. The protruding portion 15a is provided in a substantially rectangular shape (frame shape) in a plan view as shown in FIG.
[0022] Similarly, the sealing material 18 is not provided within a certain width L2 from the inner end (the side closer to the electrolyte layer 17) of the second insulating film 16, but is provided outside the range of width L2 (the side farther from the electrolyte layer 17).
[0023] In other words, the second insulating film 16 has a protruding portion 16a that protrudes by a width L2 toward the side closer to the electrolyte layer 17 than the end of the sealing material 18 that contacts the electrolyte layer 17. The protruding portion 16a is provided in a substantially rectangular shape (frame shape) in a plan view as shown in FIG.
[0024] The widths L1 and L2 of the protruding portions 15a and 16a are preferably at least 3 mm, and more preferably about 10 mm. Note that the widths L1 and L2 may be different lengths.
[0025] The electrochemical device of this embodiment has such a configuration, and can be operated, for example, by using the first electrode 13 as a working electrode and the second electrode 14 as a counter electrode, connecting a bipolar DC power supply to both electrodes, and applying a driving voltage. The driving voltage at this time is equal to the potential difference between the first electrode 13 and the second electrode 14. When a driving voltage having a waveform as exemplified in FIG. 2(A) or FIG. 2(B) is used and a driving voltage equal to or greater than the potential difference at which metal precipitates is applied during the first period, a current flows between the first electrode 13 and the second electrode 14, and metal ions (e.g., Ag) contained in the electrolyte are precipitated at the first electrode 13, which is the working electrode. + ) passes through the electrode and electrons (e - ), and is reduced as a simple metal (for example, Ag) and precipitates on one surface of the first electrode 13. At this time, if the surface of the first electrode 13 is flat, a mirror state is obtained. Note that if the surface of the first electrode 13 has fine irregularities, a black state (low reflection state) is obtained.
[0026] The inventors of the present application have conducted detailed studies on the above-mentioned electrochemical device to determine in what cases parts of the device are not formed with a metal film, thereby causing the phenomenon of a poor mirror surface. The details of the study are described below. In the study, an electrochemical device having a configuration as shown in FIG. 3 was used as a comparative example. The electrochemical device of this comparative example differs from the electrochemical device of the above-mentioned embodiment in that the first insulating film 15 and the second insulating film 16 are not provided. Components common to both devices are given the same reference numerals, and detailed descriptions of these components will be omitted.
[0027] In the electrochemical device of the comparative example, the inventors of the present application conducted an investigation using materials containing Cu, Ge, Ta, Mo, Sn, Nb, Sb, Ti, and Bi as mediators contained in the electrolyte layer 17, and found that the mediators that did not dissolve the first electrode 13 and the second electrode 14 or the sealant 18 were materials containing Ti, Bi, Cu, and Sn. In detail, the inventors of the present application investigated the solubility of an ITO film, which is an example of a transparent conductive film used as the first electrode 13 and the second electrode 14, in an electrolyte solution as follows.
[0028] Figure 4 is a graph showing the change in sheet resistance of the ITO film with respect to the immersion time in the electrolyte solution. Here, a soda lime glass substrate with a thickness of 0.7 mm was used, on whose upper surface an ITO film was formed by sputtering. The ITO film was a polycrystalline film with a thickness of about 365 nm and a sheet resistance of 5 Ω / sq. before immersion. The electrolyte solution to be immersed was prepared using N,N-dimethylacetamide as a solvent, LiBr as a supporting salt, AgBr as an electrodeposition material, and materials containing Ta, Mo, Nb, Ti, Bi, Cu, and Sn as mediators, as well as a blank without a mediator. The electrolyte solution was kept at 70°C, and the substrate with the ITO film described above was immersed in it to evaluate the change in sheet resistance with respect to the immersion time, which is the elapsed time. The sheet resistance was measured using a four-terminal method.
[0029] As shown in the figure, almost no change in sheet resistance over time was observed for mediator materials containing Ti, Bi, Cu, and Sn, as well as for the blank. On the other hand, a change in sheet resistance over time was observed for mediator materials containing Ta, Mo, and Nb. This change over time is thought to be due to the dissolution of the ITO film. From these results, it is inferred that mediators that do not dissolve the ITO film are materials containing Ti, Bi, Cu, and Sn.
[0030] Here, the relative dielectric constant of the solvent is a parameter that indicates the polarity of the solvent, and generally, the higher the relative dielectric constant, the higher the solubility. On the other hand, Ag ions are affected by solvation by the solvent, and the reflectance of the mirror state changes depending on the solvent. For example, in the case of a combination of ITO films as the first and second electrodes and Sn as the mediator, a relatively high reflectance is obtained with a solvent having a low relative dielectric constant. Therefore, in this combination of an ITO film and a material containing a mediator that does not dissolve the ITO film, it is preferable to use a solvent with a low relative dielectric constant in order to improve the reflectance. Specifically, according to the study by the present inventors, it is preferable to use a solvent with a relative dielectric constant of 8 or less.
[0031] For example, triethylene glycol dimethyl ether (molecular weight 178.23 g / mol, relative dielectric constant 7.5), diethylene glycol dimethyl ether (molecular weight 134.17 g / mol, relative dielectric constant 7.3), ethylene glycol dimethyl ether (molecular weight 90.12 g / mol, relative dielectric constant 7.2), etc. can be suitably used as the solvent. On the other hand, solvents with relatively high relative dielectric constants such as N,N-dimethylacetamide (molecular weight 87.1 g / mol, relative dielectric constant 37.8), γ-butyrolactone (molecular weight 86.1 g / mol, relative dielectric constant 39.1), dimethyl sulfoxide (molecular weight 78.13 g / mol, relative dielectric constant 46.68), and n-methyl 2-pyrrolidone (molecular weight 99.13 g / mol, relative dielectric constant 32) are not so suitable as solvents from the viewpoint of improving reflectance.
[0032] On the other hand, it was found that when a solvent with a relatively low relative dielectric constant ε was used, the solubility of Ag ions in the electrolyte layer 17 decreased.
[0033] 5(A) to 5(D) are diagrams for explaining the change over time when a test was conducted in which a driving voltage was repeatedly applied to the electrochemical device of the comparative example. The electrochemical device was tested in an upright position, as in normal use. In this system, even if Ag was initially dissolved, when a test was conducted in which the driving voltage was repeatedly turned on and off, a residual component 30, which is an undissolved portion of Ag, is generated near the seal material 18, as shown diagrammatically in FIG. 5(A). When the driving voltage is further repeatedly turned on and off, the residual component 30 moves to the lower region of the electrolyte layer 17 due to its own weight (see FIG. 5(B)).
[0034] Furthermore, when the driving voltage is repeatedly turned on and off, a concentration gradient occurs in the electrolyte layer 17 in the vertical direction in the figure, where the Ag concentration is low on the upper side and high on the lower side (see FIG. 5(C)). The precipitated Ag is converted to Ag by the mediator. + When the Br concentration in the mediator is high enough, [AgBr x ] - However, when the amount of Ag on the lower side of the electrolyte layer 17 increases due to precipitation, and the Br concentration becomes relatively low, it precipitates as AgBr crystals 31 (see FIG. 5(D)). This results in some areas that do not have a mirror finish. This is because the precipitation of crystals 31 prevents electrochemical reactions from occurring in the crystals 31, and the Ag ion concentration becomes low in the upper part of the electrochemical device, so that a reduction reaction sufficient to obtain a mirror finish does not occur.
[0035] 6(A) is a diagram for explaining the mechanism by which the solubility of Ag ions decreases in the electrochemical device of the comparative example. In this figure, a schematic enlarged view of the vicinity of the sealant 18 is shown. When the sealant 18 is cured during the manufacture of the electrochemical device, a contaminated portion 32 due to organic components such as outgassing from the sealant 18 occurs near the sealant 18. It is presumed that this organic component is a monomolecular component that did not polymerize when the sealant 18 was cured. Therefore, it can be said that the organic component basically occurs only during the manufacture, and does not continue to occur over time.
[0036] Thereafter, application of the driving voltage causes the Ag film 22 to be deposited on the first electrode 13 (working electrode), at which time Ag particles 33 are also deposited inside the contaminated portion 32. After the driving voltage is turned off, the Ag film 22 that exists in the portion other than the contaminated portion 32 dissolves, but some of the Ag particles 33 that exist inside the contaminated portion 33 do not dissolve and remain. It is presumed that the above-mentioned residual component 30 is generated by such a mechanism.
[0037] Here, the following factors are considered to be the cause of the residual components 30 being generated in the contaminated portion 32. (1) Decrease in the rate of electrode oxidation (part 1) The generation of the contaminated portion 32 causes a voltage drop in the region including the contaminated portion 32, leading to a decrease in the dissolution rate due to the electrode oxidation of Ag. (2) Decrease in electrode oxidation rate (part 2) Bonds form between the organic components of the contaminated portion 32 and Ag, increasing the voltage required for dissolution, thereby slowing down the dissolution rate. (3) Decrease in dissolution rate by mediator The distance between the Ag that has penetrated into the contaminated portion 32 and the mediator increases, resulting in a decrease in the dissolution rate.
[0038] Therefore, in the electrochemical device of this embodiment, the influence of the contaminated portion 32 is suppressed by providing the first insulating film 15 and the like. Specifically, as shown in FIG. 6B, even if the contaminated portion 32 occurs near the seal material 18, the contaminated portion 32 remains at a position overlapping the first insulating film 15. The same applies to the second insulating film 16, although not shown. The inventors of the present application have found that the range in which the contaminated portion 32 spreads is within a range of about 3 mm from the seal material 18. For this reason, it is preferable that the distances L1 and L2 of the protruding portions 15a and 16a of the first insulating film 15 and the second insulating film 16 protruding toward the electrolyte layer 17 side are at least 3 mm or more, as described above. The effect of keeping the contaminated portion 32 is more reliably obtained by setting the distances L1 and L2 to about 10 mm.
[0039] When the Ag film 22 is deposited on the first electrode 13 (working electrode) by application of the driving voltage, the presence of the first insulating film 15 between the contaminated portion 32 and the first electrode 13 makes it possible to prevent deposition of Ag particles 33 in the contaminated portion 32. Therefore, even after the driving voltage is turned off, no residual components 30 are generated because no Ag particles 33 were originally deposited inside the contaminated portion 32. Due to the above-mentioned mechanism, the electrochemical device of this embodiment can eliminate the inconvenience of not being able to obtain a mirror surface.
[0040] 7 is a graph showing the change in reflectance when a driving voltage is repeatedly applied to each of the electrochemical devices of the Comparative Example and the Example. Here, samples of electrochemical devices having the configurations of the above-mentioned embodiments were prepared as Examples, and samples of electrochemical devices of the Comparative Example were also prepared, and the change in reflectance of each was measured.
[0041] In both the embodiment and the comparative example, the first electrode 13 and the second electrode 14 were formed by sputtering to a thickness of 365 nm, and the electrolyte solution constituting the electrolyte layer 17 was formed by an electrolyte solution consisting of 200 mM AgBr, 800 mM LiBr, 30 mM SnCl4, and diethylene glycol dimethyl ether. An on-off test was performed by repeatedly applying a driving voltage under a room temperature environment. The first insulating film 15 and the second insulating film 16 were formed by sputtering to a thickness of 200 nm SiO2, and the distances L1 and L2 protruding from each of the insulating films to the electrolyte layer 17 side were both 10 mm. As for the driving voltage (see FIG. 1(B)), the length of the on period (first period) was 10 seconds, the voltage (potential difference) at that time was 2.5 V, the length of the off period (second period) was 30 seconds, and the voltage (potential difference) at that time was -0.5 V, and the total of these was 40 seconds, which was one cycle (one on-off count).
[0042] As shown in the figure, in the electrochemical device of the embodiment, no crystals (AgBr crystals 31) were precipitated even after 10,000 on-off cycles, and the decrease in reflectance was suppressed. On the other hand, in the electrochemical device of the comparative example, crystals were precipitated after 200 on-off cycles, and the reflectance also tended to decrease gradually.
[0043] As described above, according to the present embodiment, the occurrence of undissolved metal film in the electrochemical device when the device is turned off can be eliminated, and the occurrence of areas where the metal film cannot be obtained due to the undissolved metal film can be eliminated.
[0044] The present disclosure is not limited to the above-described embodiment, and various modifications can be made within the scope of the present disclosure. For example, the structures of the first insulating film 15 and the second insulating film 16 are not limited to the above-described embodiment, and various modifications can be made as described below.
[0045] 8(A), the sealant 18 may be provided so as to have a portion overlapping and in contact with the first insulating film 15, and a portion in contact with one surface of the first substrate 11 at a position farther from the electrolyte layer 17 than the position where the sealant 18 overlaps with the first insulating film 15. Similarly, the sealant 18 may be provided so as to have a portion overlapping and in contact with the second insulating film 16, and a portion in contact with one surface of the second substrate 12 at a position farther from the electrolyte layer 17 than the position where the sealant 18 overlaps with the second insulating film 16.
[0046] Also, as in the electrochemical device of the modified example shown in Fig. 8(B), the insulating film may be provided on at least one of the substrates. In the illustrated example, it is assumed that the first electrode 13 is used as a working electrode and the second electrode 14 is used as a counter electrode, so the first insulating film 15 is provided on the first electrode 13 side, which is the working electrode side, and the second insulating film 16 is omitted. Similarly, in the modified example shown in Fig. 8(A) described above, either one of the insulating films (for example, the second insulating film 16) may be omitted.
[0047] 8(C), the seal material 18 may be provided so as to have a portion in contact with each of one surface of the first substrate 11 and one surface of the second substrate 12, and a portion in contact with the outer edge of the insulating film in a plan view. In the illustrated example, it is assumed that the first electrode 13 is used as a working electrode and the second electrode 14 is used as a counter electrode, so that the first insulating film 15 is provided on the first electrode 13 side, which is the working electrode side, and the second insulating film 16 is omitted. The first insulating film 15 is in contact with the seal material 18 at its outer edge, i.e., the end farther from the electrolyte layer 17. The second insulating film 16 may also be provided on the second substrate 12 side in the same configuration as the illustrated first insulating film 15.
[0048] In the above-described embodiment and each modified example, the first insulating film 15 and the second insulating film 16 may be composed of a single layer or may be composed of multiple layers. When composed of multiple layers, each layer may be an insulating layer of a different material. In the above-described embodiment, the electrode is an ITO film, the solvent of the electrolyte layer is a solvent having a relative dielectric constant of 8 or less, and the mediator is each material including Ti, Bi, Cu, and Sn. However, the present disclosure is not limited to these combinations of materials.
[0049] The solvent for the electrolyte layer is not limited to a solvent having a relative dielectric constant of 8 or less, and may be a carbonate-based organic solvent such as dimethyl carbonate, diethyl carbonate, or ethyl methyl carbonate. Even in this case, it is possible to eliminate the undissolved metal film in an electrochemical device configured by combining a solvent having a relative dielectric constant of more than 8 with an appropriate mediator.
[0050] The present disclosure has the following features. (Appendix 1) A first substrate and a second substrate arranged such that one surface of each substrate faces each other; A first electrode provided on one surface of the first substrate; A second electrode provided on one surface side of the second substrate; an electrolyte layer provided between the first electrode and the second electrode; a sealant provided between the first substrate and the second substrate so as to surround the electrolyte layer; an insulating film provided on one surface of at least one of the first electrode and the second electrode, the insulating film having a protruding portion protruding by a predetermined width toward a side closer to the electrolyte layer than an end of the sealing material on a side in contact with the electrolyte layer; Including, The electrolyte layer is an electrolyte solution containing an electrodeposition material containing Ag, a mediator containing one or more materials containing Ti, Bi, Cu or Sn, a supporting salt and a solvent. Electrochemical equipment. (Appendix 2) The solvent of the electrolyte layer has a relative dielectric constant of 8 or less. 2. The electrochemical device of claim 1. (Appendix 3) The solvent of the electrolyte layer includes at least one of an ether-based organic solvent and a carbonate-based organic solvent. 2. The electrochemical device of claim 1. (Appendix 4) The ether-based organic solvent is any one of triethylene glycol dimethyl ether, diethylene glycol dimethyl ether, and ethylene glycol dimethyl ether. 4. The electrochemical device of claim 3. (Appendix 5) The carbonate-based organic solvent is any one of dimethyl carbonate, diethyl carbonate, and ethyl methyl carbonate. 4. The electrochemical device of claim 3. (Appendix 6) The width of the protruding portion of the insulating film is 3 mm or more. 6. The electrochemical device according to any one of claims 1 to 5. (Appendix 7) The insulating film is provided in a frame shape in a plan view. 7. The electrochemical device according to any one of claims 1 to 6. (Appendix 8) The insulating film has arc-shaped portions at four corners in a plan view. 8. The electrochemical device of claim 7. (Appendix 9) the sealing material is provided so as to have a portion overlapping the insulating film without having a portion in contact with the first electrode or the second electrode; An electrochemical device according to any one of claims 1 to 8. (Appendix 10) the sealing material is provided so as to have a portion in contact with one surface of the first electrode or the second electrode and a portion overlapping the insulating film. An electrochemical device according to any one of claims 1 to 8. (Appendix 11) the sealing material is provided so as to have a portion in contact with one surface of the first electrode or the second electrode and a portion in contact with an outer edge portion of the insulating film in a plan view. An electrochemical device according to any one of claims 1 to 8. (Appendix 12) The first electrode and the second electrode are each formed using an ITO film. 12. The electrochemical device according to any one of claims 1 to 11. (Appendix 13) The sealing material is made of a photocurable resin, a thermosetting resin, or a glass frit. 13. The electrochemical device according to any one of claims 1 to 12. [Explanation of symbols]
[0051] 11: first substrate, 12: second substrate, 13: first electrode, 14: second electrode, 15: first insulating film, 16: second insulating film, 17: electrolyte layer, 18: sealing material
Claims
1. A first substrate and a second substrate arranged such that one surface of each substrate faces each other; A first electrode provided on one surface side of the first substrate; A second electrode provided on one surface side of the second substrate; an electrolyte layer provided between the first electrode and the second electrode; a sealant provided between the first substrate and the second substrate so as to surround the electrolyte layer; an insulating film provided on one surface of at least one of the first electrode and the second electrode, the insulating film having a protruding portion protruding by a predetermined width toward a side closer to the electrolyte layer than an end of the sealing material on a side in contact with the electrolyte layer; Including, The electrolyte layer is an electrolyte solution containing an electrodeposition material containing Ag, a mediator containing one or more materials containing Ti, Bi, Cu, or Sn, a supporting salt, and a solvent. Electrochemical equipment.
2. the solvent of the electrolyte layer has a relative dielectric constant of 8 or less; 2. The electrochemical device of claim 1.
3. The solvent of the electrolyte layer includes at least one of an ether-based organic solvent and a carbonate-based organic solvent.
2. The electrochemical device of claim 1.
4. The ether-based organic solvent is any one of triethylene glycol dimethyl ether, diethylene glycol dimethyl ether, and ethylene glycol dimethyl ether.
4. The electrochemical device of claim 3.
5. The carbonate-based organic solvent is any one of dimethyl carbonate, diethyl carbonate, and ethyl methyl carbonate.
4. The electrochemical device of claim 3.
6. The width of the protruding portion of the insulating film is 3 mm or more.
2. The electrochemical device of claim 1.
7. The insulating film is provided in a frame shape in a plan view.
2. The electrochemical device of claim 1.
8. The insulating film has arc-shaped portions at four corners in a plan view.
8. The electrochemical device of claim 7.
9. the sealing material is provided so as to have a portion overlapping the insulating film without having a portion in contact with the first electrode or the second electrode; 2. The electrochemical device of claim 1.
10. the sealing material is provided so as to have a portion in contact with one surface of the first electrode or the second electrode and a portion overlapping the insulating film; 2. The electrochemical device of claim 1.
11. the sealing material is provided so as to have a portion in contact with one surface of the first electrode or the second electrode and a portion in contact with an outer edge portion of the insulating film in a plan view; 2. The electrochemical device of claim 1.
12. The first electrode and the second electrode are each formed using an ITO film.
2. The electrochemical device of claim 1.
13. The sealing material is composed of a photocurable resin, a thermosetting resin, or a glass frit.
2. The electrochemical device of claim 1.
Citation Information
Patent Citations
Electrochemical Equipment
JP6738679B2