Electrolyte and secondary battery

The electrolyte with a controlled molar ratio of lithium imide salt and ionic liquid, containing specific anion and cation species, addresses SEI film cracking in secondary batteries, thereby reducing reaction resistance and maintaining battery performance.

JP2024164737AActive Publication Date: 2024-11-27TOYOTA JIDOSHA KK
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2023080428
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-15
Publication Date
2024-11-27
Estimated Expiration
2043-05-15

AI Technical Summary

Technical Problem

The use of ionic liquid-containing electrolytes in secondary batteries leads to cracks in the SEI film at the interface between the electrolyte and the active material layer, resulting in increased reaction resistance and reduced capacity retention due to liquid decomposition and thick film formation.

Method used

An electrolyte comprising lithium imide salt and ionic liquid with a molar ratio of 1.5 or less, containing bis(fluorosulfonyl)amide ions, and optionally including 1-ethyl-3-methylimidazolium as a cation, is used, along with a separator layer, to suppress reaction resistance.

Benefits of technology

The electrolyte effectively reduces reaction resistance at the interface between the electrolyte and the active material layer, maintaining battery performance by preventing electrolyte outflow and film cracking.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024164737000001
    Figure 2024164737000001
Patent Text Reader

Abstract

To provide an electrolyte that suppresses an increase in reaction resistance at an interface between the electrolyte and an active material layer.SOLUTION: An electrolyte includes a lithium imide salt and an ionic liquid, and a molar ratio (ionic liquid / lithium imide salt) of the ionic liquid to the lithium imide salt is 1.5 or less.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to an electrolyte and a secondary battery. [Background technology]

[0002] In recent years, development of secondary batteries that use electrolytes containing flame-retardant ionic liquids has been progressing. For example, Patent Document 1 discloses a non-aqueous electrolyte lithium-ion battery that includes a positive electrode, a negative electrode, a separator, and a non-aqueous electrolyte that contains a lithium salt and an ionic liquid (claim 1, paragraph 0006). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2012-204133 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, when an electrolyte containing an ionic liquid is used in a secondary battery containing a separator, cracks occur in the SEI (Solid Electrolyte Interphase) film formed at the interface between the electrolyte and the active material layer due to charging and discharging, and a new SEI film is formed at the cracked portion. As a result, liquid decomposition of the electrolyte progresses and a thick film is formed, which tends to increase the reaction resistance at the interface between the electrolyte and the active material layer and decrease the capacity retention rate. In view of the above circumstances, the problem to be solved by the present disclosure is to provide an electrolyte that suppresses an increase in reaction resistance at the interface between the electrolyte and the active material layer, and a secondary battery including the electrolyte. [Means for solving the problem]

[0005] Means for solving the above problems include the following means. <1> A lithium imide salt and an ionic liquid are included. an electrolyte, wherein the molar ratio of the ionic liquid to the lithium imide salt (ionic liquid / lithium imide salt) is 1.5 or less. <2> Both the lithium imide salt and the ionic liquid contain bis(fluorosulfonyl)amide ion (FSA) as an anionic species; <1> The electrolyte according to claim 1. <3> The ionic liquid contains 1-ethyl-3-methylimidazolium (EMIM) as a cationic species. <1> or <2> The electrolyte according to claim 1. <4> A positive electrode layer; A negative electrode layer; The positive electrode layer and the negative electrode layer are disposed between the positive electrode layer and the negative electrode layer. <1> ~ <3> A separator layer comprising the electrolyte according to any one of the above items; A secondary battery comprising: <5> The negative electrode layer contains a Si-based active material as a negative electrode active material. <4> The secondary battery according to claim 1. Effect of the Invention

[0006] According to the present disclosure, there are provided an electrolyte that suppresses an increase in reaction resistance at the interface between the electrolyte and an active material layer, and a secondary battery including the electrolyte.

[0007] Hereinafter, an embodiment that is an example of the present disclosure will be described. These descriptions and examples are merely illustrative of the embodiment, and are not intended to limit the scope of the present invention. In the present specification, the upper or lower limit of one numerical range may be replaced with the upper or lower limit of another numerical range. In addition, in the present specification, the upper or lower limit of the numerical range may be replaced with a value shown in the examples.

[0008] Each component may contain multiple types of the corresponding substance. When referring to the amount of each component in a composition, if there are multiple substances corresponding to each component in the composition, unless otherwise specified, it means the total amount of those multiple substances present in the composition.

[0009] [Electrolytes] The electrolyte according to the present disclosure is an electrolyte that contains a lithium imide salt and an ionic liquid, and the molar ratio of the ionic liquid to the lithium imide salt (ionic liquid / lithium imide salt) is 1.5 or less. The electrolyte according to the present disclosure, having the above-mentioned configuration, can suppress an increase in reaction resistance at the interface between the electrolyte and the active material layer. The mechanism of this action is not entirely clear, but is presumed to be as follows. By setting the molar ratio of the ionic liquid to the lithium imide salt in the electrolyte within the above range, the viscosity of the electrolyte is increased, and an increase in the resistance value caused by the outflow of the ionic liquid from the electrode can be suppressed. In addition, by increasing the concentration of the ionic liquid, which has conventionally been considered to have low ionic conductivity, it is believed that an increase in the reaction resistance at the interface between the electrolyte and the active material layer can be suppressed.

[0010] The electrolyte according to the present disclosure can be used for both positive and negative electrodes. In particular, since the electrolyte contains an ionic liquid, it is softer than an electrolyte that does not contain an ionic liquid, and is useful for a solid-state battery having an electrode (e.g., a negative electrode, more specifically, a silicon-containing negative electrode) that contains an active material that is prone to expansion and contraction.

[0011] [Lithium imide salt] The electrolyte according to the present disclosure includes a lithium imide salt. Examples of the lithium imide salt include lithium bis(trifluoromethanesulfonyl)imide (LiTFSA), lithium bis(fluorosulfonyl)imide (LiFSA), lithium difluoro(oxalato)borate (LiDFOB), and lithium bis(oxalato)borate (LiBOB). The lithium imide salt may be used alone or in combination of two or more.

[0012] Among the above, from the viewpoint of further suppressing an increase in reaction resistance at the interface between the electrolyte and the active material layer, it is preferable that the lithium imide salt contains a bis(fluorosulfonyl)amide ion (FSA) as an anion species, and it is more preferable that the lithium imide salt contains lithium bis(fluorosulfonyl)imide (LiFSA).

[0013] [Ionic liquid] The electrolyte according to the present disclosure includes an ionic liquid. Examples of the ionic liquid include 1-ethyl-3-methylimidazolium bis(fluorosulfonyl)imide [EMIM-FSA], N-methyl-N-propylpyrrolidinium bis(fluorosulfonyl)imide [PP13-FSA], N-methyl-N-propylpyrrolidinium bis(fluorosulfonyl)imide [PP13-FSA], cesium bis(fluorosulfonyl)imide [CsFSA], N,N-diethyl-N-methyl-N-(2-methoxyethyl)ammonium bis(fluorosulfonyl)imide [DEMEFSA], N-methyl-N-propylpyrrolidinium bis(trifluoromethanesulfonyl)amide [PP13TFSA], cesium bis(trifluoromethylsulfonyl)amide [CsTFSA], and N,N-diethyl-N-methyl-N-(2-methoxyethyl)ammonium bis(trifluoromethanesulfonyl)amide [DEMETFSA]. The ionic liquid may be used alone or in combination of two or more kinds.

[0014] Among the above, the ionic liquid preferably contains 1-ethyl-3-methylimidazolium (EMIM) as a cationic species, and more preferably contains 1-ethyl-3-methylimidazolium bis(fluorosulfonyl)imide [EMIM-FSA]. EMIM-FSA is preferred from the viewpoint of further suppressing an increase in reaction resistance at the interface between the electrolyte and the active material layer by making the viscosity of the ionic liquid appropriate, and from the viewpoint of battery performance.

[0015] As described above, in the electrolyte of the present disclosure, from the viewpoint of further suppressing an increase in reaction resistance at the interface between the electrolyte and the active material layer, it is preferable that both the lithium imide salt and the ionic liquid contain a bis(fluorosulfonyl)amide ion (FSA) as an anion species.

[0016] [Other ingredients] The electrolyte according to the present disclosure may further contain other components as necessary within the range in which the effects of the present disclosure are achieved. Examples of the other components include fillers, binder resins, sulfide solid electrolytes, oxide solid electrolytes, halide solid electrolytes, polymers or rubbers other than the binder resins, and conductive assistants (e.g., fibrous carbon materials).

[0017] The conductive assistant is not particularly limited as long as it is a normal conductive assistant that can be used in lithium ion batteries. Examples of the conductive assistant include carbon black such as acetylene black and ketjen black, and carbon materials such as vapor grown carbon fiber.

[0018] The conductive assistant is not particularly limited as long as it is a material having conductivity. For example, it may be a metal such as aluminum, stainless steel (SUS), silver, gold, copper, titanium, etc. Or it may be carbon such as graphite and carbon black (acetylene black, ketjen black, furnace black, channel black, thermal lamp black, etc.) Or it may be an alloy or metal acid thereof. The conductive assistant may be used alone or in combination of two or more kinds. Furthermore, the conductive assistant is not limited to particles, and may be a so-called filler-based conductive assistant such as carbon nanofibers and carbon nanotubes.

[0019] [Content] The molar ratio of the ionic liquid to the lithium imide salt (ionic liquid / lithium imide salt) is 1.5 or less, and from the viewpoint of further suppressing an increase in the reaction resistance at the interface between the electrolyte and the active material layer, it is preferably 1.55 or less, and more preferably 1.56 or less. The lower limit of the molar ratio (ionic liquid / lithium imide salt) is not particularly limited, but may be, for example, the amount of lithium imide salt added until it reaches a saturated state.

[0020] The electrolyte of the present disclosure may contain an organic electrolyte (i.e., an organic solvent containing carrier ions according to the purpose and having ion-conducting ability to transport the ions between electrodes) within the range in which the effects of the present application are achieved. For example, the proportion of the organic electrolyte is preferably 10 mass% or less, more preferably 5 mass% or less, even more preferably 3 mass% or less, and most preferably 0 mass%, i.e., not contained, relative to the total amount of the electrolyte.

[0021] [Secondary battery] The secondary battery of the present disclosure includes the electrolyte of the present disclosure. The method for manufacturing the secondary battery is not particularly limited, and a known method for manufacturing a secondary battery can be applied. For example, the method described in the examples can be mentioned. The secondary battery of the present disclosure includes, for example, a positive electrode layer, a negative electrode layer, and a separator layer containing the electrolyte of the present disclosure disposed between the positive electrode layer and the negative electrode layer. Known materials can be used for the separator layer, the positive electrode layer, and the negative electrode layer.

[0022] In the secondary battery of the present disclosure, the negative electrode layer may contain a Si-based active material as a negative electrode active material. The Si-based active material is not particularly limited as long as it contains silicon and can act as an active material, and examples thereof include silicon simple particles, silicon alloy particles (e.g., alloys of Si and one or more metals selected from the group consisting of Sn, Ti, Fe, Ni, Cu, Co, and Al), porous silicon, silicon clathrate compounds, silicon oxides, and mixtures thereof. The Si-based active material may be one type alone or two or more types in combination. A secondary battery having a negative electrode layer containing a Si-based active material has advantages such as a high capacity and a relatively low operating potential, but the expansion and contraction caused by charging and discharging is larger than that of other active materials. Therefore, cracks occur in the SEI coating formed at the interface between the electrolyte and the active material layer due to charging and discharging due to the expansion and contraction, and a new SEI coating is formed at the cracked portion. As a result, the reaction resistance at the interface between the electrolyte and the active material layer is likely to increase. In contrast, in the secondary battery according to the present disclosure, the separator layer contains the electrolyte according to the present disclosure, so that the increase in the reaction resistance at the interface between the electrolyte and the active material layer is suppressed.

[0023] The secondary battery of the present disclosure may be a lithium-ion secondary battery. Applications of the secondary battery include power sources for vehicles, electronic devices, and electrical storage. EXAMPLES

[0024] Examples will be described below, but the present invention is not limited to these examples in any way.

[0025] <Example 1> The ionic liquid (EMIM-FSA) was mixed with lithium imide salt (LiFSA) at a molar ratio (ionic liquid / lithium imide salt) of 1.5:1, and the mixture was stirred at room temperature (23±1° C.) to obtain the electrolyte of Example 1.

[0026] <Comparative Example 1> The ionic liquid (EMIM-FSA) was mixed with lithium imide salt (LiFSA) at a molar ratio (ionic liquid / lithium imide salt) of 6:1, and the mixture was stirred at room temperature (23±1° C.) to obtain the electrolyte of Example 1.

[0027] <Comparative Example 2: High-concentration organic electrolyte (4M LiFSI / DME+120vol% TTE)> LiFSA was mixed with DME (1,2-dimethoxyethane) to give a molar concentration of 4.0 M, and stirred at room temperature (23±1° C.). Then, TTE (1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether) was added to the solution at a volume ratio of 120% by volume, and the mixture was stirred at room temperature (23±1° C.) to obtain the electrolyte of Comparative Example 1.

[0028] <Comparative Example 3: Dilute organic electrolyte (1.2M LiPF6 / FEC-EC-DMC-EMC)> As a solvent, FEC (fluoroethylene carbonate), EC (ethylene carbonate), DMC (dimethyl carbonate) and EMC (ethyl methyl carbonate) were mixed in a volume ratio (FEC:EC:DMC:EMC) of 1:2:3:4. Then, LiPF was added to the solution to make the concentration 1.2M. 6 The mixture was stirred at room temperature (23±1° C.) to obtain an electrolyte of Comparative Example 2.

[0029] <Measurement and evaluation of reaction resistance 1: In the case of porous Si> A coin cell (subject cell) was produced by laminating SUS foil, porous Si, an aramid-based separator containing the electrolyte of each example, Li metal as the counter electrode, and SUS foil in that order, with an aluminum laminate exterior material. The secondary battery of each example was placed in a thermostatic chamber at 25° C. After charging until the battery voltage reached 2.2 V, the AC impedance of the battery was measured, and the battery was discharged until the SOC (State Of Charge) reached 50%. The battery was charged at a constant current of 1 / 3C rate until the battery voltage reached 2.7V, and then at a constant voltage, and charging was terminated when the charging current reached the equivalent of 0.01C. The AC impedance measurement was performed at an AC amplitude of 10 mV and in the frequency range of 1 MHz to 10 mHz. A curve was obtained by fitting the waveform of the circular arc portion appearing in the Nyquist diagram obtained from the AC impedance measurement. The difference between the x-axis intercepts on the high frequency side and the low frequency side of the obtained curve was taken as the initial resistance. The results are shown in Table 1.

[0030] <Measurement and evaluation of reaction resistance 2: In the case of crystalline Si> Except for changing the porous Si to crystalline Si, the coin cells of each example were fabricated in the same manner as in "Measurement and Evaluation of Reaction Resistance 1". Then, impedance measurements were performed. The reaction resistance value originating from the interface between the porous Si and the electrolyte in the Nyquist diagram obtained by the same method as in "Measurement and evaluation of reaction resistance 1" was calculated by circle fitting, and the increase rate of the reaction resistance value was calculated as (reaction resistance value when using porous Si) / (reaction resistance value when using crystalline Si)×100(%). The results are shown in Table 1.

[0031] [Table 1]

[0032] As shown in Table 1, the electrolytes of the examples had low reaction resistance values ​​compared to the electrolytes of the comparative examples, even in the case of porous Si with a large specific surface area, and it was found that they suppressed an increase in reaction resistance at the interface between the electrolyte and the active material layer.

Claims

1. A lithium imide salt and an ionic liquid are included. an electrolyte, wherein the molar ratio of the ionic liquid to the lithium imide salt (ionic liquid / lithium imide salt) is 1.5 or less.

2. 2. The electrolyte of claim 1, wherein the lithium imide salt and the ionic liquid both contain bis(fluorosulfonyl)amide ions (FSA) as an anionic species.

3. The electrolyte of claim 1 , wherein the ionic liquid comprises 1-ethyl-3-methylimidazolium (EMIM) as a cationic species.

4. A positive electrode layer; A negative electrode layer; A separator layer comprising the electrolyte according to any one of claims 1 to 3 and disposed between the positive electrode layer and the negative electrode layer; A secondary battery comprising:

5. The secondary battery according to claim 4 , wherein the negative electrode layer contains a Si-based active material as a negative electrode active material.

Citation Information

Patent Citations

  • Electrolyte solution for lithium ion secondary battery, and lithium ion secondary battery

    JP2018170272A

  • Gel electrolyte, hard gel electrolyte, and electrochemical device

    JP2019057425A

  • Nonaqueous electrolyte

    JP2019197649A

  • Lithium secondary battery and electrolyte solution

    JP2021125416A

  • Lithium metal secondary battery

    JP2022106553A