Glass plate laminate and glass plate package
The glass plate laminate's specific interleaving paper arrangement addresses gripping issues, enabling efficient and protective removal of interleaving papers, ensuring smooth unpacking and glass plate protection.
Patent Information
- Application Number
- JP2024079392
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-17
- Filing Date
- 2024-05-15
- Publication Date
- 2024-11-28
AI Technical Summary
Existing glass plate packaging systems face challenges in efficiently removing interleaving papers due to issues with gripping failure by robots, as the interleaving paper may not be properly grasped or aligned, leading to incomplete removal and potential damage to glass plates.
The glass plate laminate is designed with interleaving paper arranged to cover the glass plates, ensuring a difference in protrusion length of 110 mm or less at both ends and a deviation of 1 mm or more in 60% or more of the total length, with fiber orientation parallel or perpendicular to the sides, facilitating smooth removal by robots.
This design allows for seamless extraction of interleaving papers, preventing gripping failures and ensuring complete removal while protecting the glass plates, enhancing unpacking efficiency and preventing direct contact between glass plates.
Smart Images

Figure 2024166151000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a glass sheet laminate and a glass sheet package. [Background technology]
[0002] Patent Document 1 discloses a glass plate package in which a plurality of glass plates are stacked together with interleaving paper between adjacent glass plates to form a glass plate laminate, and the glass plate laminate is loaded on a pallet in a flat position, as a packaging form for transporting and storing glass plates. In this glass plate package, the interleaving paper interposed between the glass plates is, for example, a rectangular interleaving paper having an area slightly larger than the glass plates, and the interleaving paper protrudes from at least three of the four sides of the glass plates. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] International Publication No. 2021 / 106451 Summary of the Invention [Problem to be solved by the invention]
[0004] When opening the glass plate package and removing the glass plates from the glass plate laminate, for example, a robot that sucks and removes the uppermost glass plate from the glass plate laminate, and a robot that picks up and removes the end of the uppermost interleaf paper from the glass plate laminate are operated. The robot that removes the interleaf paper has a plurality of gripping parts arranged in a straight line, and picks up and holds one side of the interleaf paper protruding from the glass plate with a pair of claws of these gripping parts so as to pinch and hold it, and pulls it up in that state to remove the interleaf paper.
[0005] However, when a robot removes interleaf sheets from a glass plate laminate, there are cases where one of the claws of the robot's gripping parts cannot be inserted under the interleaf sheets to be removed. Even if one of the claws of the robot's gripping parts can be inserted under the interleaf sheets, there are cases where all of the gripping parts arranged along the entire side of the interleaf sheets to be removed cannot grip the interleaf sheets.
[0006] The present invention has been made in consideration of the above-mentioned circumstances, and an object of the present invention is to provide a glass plate laminate and a glass plate package that enable the interleaf paper to be easily removed when the glass plate and the interleaf paper are removed in order. [Means for solving the problem]
[0007] The above object of the present invention can be achieved by the following configuration. (1) A glass plate laminate in which interleaf paper is placed on the front and back of glass plates and laminated, the interleaf paper is disposed so as to cover the glass plate, A first side, which is one side of the interleaf paper adjacent to the upper side of the glass plate in the stacking direction, The difference in the protrusion length from the glass plate at both ends of the first side is 110 mm or less, a section of one side of the interleaf paper adjacent to the glass plate on the lower side in the stacking direction, the section being shifted by an amount of shift of 1 mm or more from a second side that is the side located on the lower side of the first side, as viewed in the stacking direction, the section occupying 60% or more of a total length of the first side.
[0008] According to the glass plate laminate having the above configuration (1), in the interleaf paper arranged to cover the glass plates, the difference in overhang length at both ends of one side of the interleaf paper is set to 110 mm or less, and furthermore, a shift of 1 mm or more is provided in a section of 60% or more of the total length relative to the interleaf paper below in the stacking direction. This makes it easier for the claws of the gripping parts to be inserted between the interleaf papers above and below in the stacking direction when the interleaf paper is removed by a interleaf paper removal robot having multiple gripping parts arranged in a straight line, and allows one side of the interleaf paper to be gripped by all of the gripping parts of the interleaf paper removal robot. Thus, according to this glass plate laminate, the interleaf paper can be smoothly removed by the interleaf paper removal robot, suppressing poor gripping of the interleaf paper.
[0009] (2) The glass plate laminate according to (1), wherein the length of the interleaf paper protruding from the glass plate at the first side is 10 mm or more and 110 mm or less.
[0010] According to the glass plate laminate having the configuration (2) above, the protruding length of one side of the interleaf paper adjacent to the glass plate on the upper side in the stacking direction is set to 10 mm or more and 110 mm or less. By setting the protruding length of the interleaf paper from the glass plate to 10 mm or more and 110 mm or less in this way, the one side of the interleaf paper hangs down appropriately, sufficiently protecting the end face of the glass plate, and further preventing poor gripping due to alignment with the one side of the interleaf paper on the lower side in the stacking direction.
[0011] (3) The glass sheet laminate according to (2), wherein the interleaf paper is arranged such that a grain direction, which is a fiber orientation direction, is approximately parallel to the first side, and the protruding length is 20 mm or more and 80 mm or less.
[0012] According to the glass sheet laminate having the configuration of (3) above, in the case of horizontal streaks in which the streaks of aligned fibers are arranged approximately parallel to one side, the length of the interleaf that protrudes from the glass sheet is set to 20 mm or more and 80 mm or less. In this way, in the case of horizontal streaks, by setting the protruding length to 20 mm or more and 80 mm or less, one side is allowed to hang down appropriately, and gripping problems caused by lining up with one side of the interleaf paper on the lower side in the stacking direction can be further prevented.
[0013] (4) The glass sheet laminate according to (2), wherein the interleaf paper is arranged such that a grain direction, which is a fiber orientation direction, is approximately perpendicular to the first side, and the protruding length is 20 mm or more and 110 mm or less.
[0014] According to the glass sheet laminate having the configuration of (4) above, in the case of vertical streaks in which the streaks of aligned fibers are oriented substantially perpendicular to one side, the length of the interleaf protruding from the glass sheet is set to 20 mm or more and 110 mm or less. In this way, in the case of vertical streaks, by setting the protruding length to 20 mm or more and 110 mm or less, one side is allowed to hang down appropriately, and poor gripping caused by lining up with one side of the interleaf paper on the lower side in the stacking direction can be further prevented.
[0015] (5) A glass sheet laminate comprising: the glass sheet laminate according to any one of (1) to (4); and a base; The glass plate package is a glass plate package in which the glass plate laminate is placed on the base and packaged.
[0016] According to the glass plate package having the above configuration (5), the package contains a glass plate stack from which the interleaf paper can be smoothly removed by a paper removal robot, and therefore the ease of unpacking can be improved. Effect of the Invention
[0017] According to the present invention, it is possible to provide a glass sheet laminate and a glass sheet package from which the interleaf paper can be easily removed when the glass sheets and the interleaf paper are removed in order.
[0018] The present invention has been briefly described above. Furthermore, the details of the present invention will be further clarified by reading the following description of the embodiment of the present invention (hereinafter, referred to as "embodiment") with reference to the accompanying drawings. [Brief description of the drawings]
[0019] [Figure 1] FIG. 1 is a schematic cross-sectional view of a glass plate package in which a glass plate laminate according to this embodiment is packaged. [Diagram 2]FIG. 2 is a schematic plan view of a glass plate package provided with a mounting table. [Diagram 3] FIG. 3 is a schematic plan view of a glass plate package not provided with a mounting table. [Figure 4] FIG. 4 is a schematic cross-sectional view of a glass plate package in which a glass plate laminate is placed vertically. [Diagram 5] FIG. 5 is a schematic cross-sectional view of a glass plate package illustrating a process of removing a glass plate from a glass plate laminate. [Figure 6] FIG. 6 is a schematic cross-sectional view of a glass plate package illustrating a step of removing the interleaf paper from the glass plate laminate. [Figure 7] FIG. 7 is a schematic plan view of a glass plate package illustrating a step of removing the interleaf paper from the glass plate laminate. [Figure 8] FIG. 8 is a schematic plan view of a glass plate package illustrating poor gripping during the step of removing the interleaf paper. [Figure 9] FIG. 9 is a schematic cross-sectional view of an edge portion of a glass plate laminate, illustrating poor gripping during the step of removing the interleaf paper. [Figure 10] FIG. 10 is a schematic plan view showing the arrangement of interleaf papers in a glass plate laminate. [Figure 11] FIG. 11 is a schematic cross-sectional view of an edge portion of a glass plate laminate in a state in which one side of an interleaf sheet on an upper side in the stacking direction is shifted inward with respect to one side of an interleaf sheet on a lower side in the stacking direction. [Figure 12] FIG. 12 is a schematic cross-sectional view of an edge portion of a glass plate laminate in a state in which one side of an interleaf sheet on an upper side in the stacking direction is shifted outward with respect to one side of an interleaf sheet on a lower side in the stacking direction. [Figure 13] FIG. 13 is a graph showing the test results for horizontal streaks. [Figure 14] FIG. 14 is a graph showing the test results for vertical streaks. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0020] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, an embodiment of the present invention will be described with reference to the drawings. FIG. 1 is a schematic cross-sectional view of a glass sheet package 17 in which a glass sheet laminate 10 according to this embodiment is packaged.
[0021] As shown in Fig. 1, a glass plate laminate 10 according to this embodiment is a laminate in which glass plates 11 and interleaf papers 13 are alternately laminated. That is, the vertical direction in Fig. 1 is the stacking direction. The interleaf papers 13 are arranged on the front and back sides so as to cover the glass plates 11. This glass plate laminate 10 is placed on a base 15 of a pallet 19 and packaged to form a glass plate package 17, and is transported or stored in the state of this glass plate package 17.
[0022] The interleaf paper 13 is formed in a rectangular shape having an area larger than that of the glass plate 11. Therefore, the interleaf paper 13 is interposed between the glass plates 11 such that at least three of the four sides of the interleaf paper 13 extend beyond the glass plate 11. As shown in FIG. 2, when the pallet 19 is provided with a mounting table 16 that abuts against one side of the glass plate 11 and supports the glass plate 11, the interleaf paper 13 is arranged so as to extend beyond the three sides of the four sides of the glass plate 11 other than the side that abuts against the mounting table 16, and is arranged so as to cover at least 90% of each of the two sides extending from both ends of the side that abuts against the mounting table 16. In this case, the interleaf paper 13 may cover 100% of each of the two sides. On the other hand, when the pallet 19 is not provided with a mounting table as shown in FIG. 3, the interleaf paper 13 is arranged so as to cover the entire surface of the glass plate 11 and the interleaf paper on all sides extends beyond the glass plate 11. Regarding the flat pallet on which the glass plate laminate 10 is laid flat, a mounting table may or may not be provided, so the interleaf paper 13 is arranged as described above depending on the presence or absence of the mounting table. In the case of a vertical pallet on which the glass plate laminate 10 is laid vertically as shown in FIG. 4, the glass plate laminate 10 is placed on the pallet 19 so that the main surface of the interleaf paper 13 contacts the inclined surface of the inclined table 18, and the lower side of the glass plate laminate 10 is supported by the mounting table 16. Therefore, the interleaf paper 13 is arranged so as to protrude from three sides of the four sides of the glass plate 11 other than the lower side. In the case of a vertical pallet, the glass plate laminate 10 viewed from the lamination direction of the glass plate 11 is the same as that shown in FIG. 2, and the interleaf paper 13 is arranged so as to cover at least 90% of each of the two sides extending from both ends of the one side abutting against the mounting table 16. In this case, the interleaf paper 13 may cover 100% of each of the two sides. In other words, when the glass plate laminate 10 placed on a flat pallet or a vertical pallet provided with a mounting table 16 is viewed from the stacking direction of the glass plates 11, a portion of the glass plate will not be covered by the interleaf paper 13 as shown in Figure 2, except when the interleaf paper 13 covers 100% of each of the two sides.
[0023] The glass plate 11 is used for, for example, a flat panel display (FPD) such as a liquid crystal display (LCD) or an organic light-emitting diode (OLED).
[0024] The slip sheet 13 has, for example, a smoothness of 5 to 30 seconds (JIS P 8119, 1998) and a density of 0.4 to 1.0 g / cm 3 The resin content is 0.5 mass% or less (JIS P 8224, 2002), has excellent cushioning properties, and has little transfer of the resin content. More specifically, the smoothness is 20 seconds or less (JIS P 8119, 1998), the density is 0.8 g / cm 3 The resin content of the interleaf paper 13 is preferably 0.05% by mass or less (JIS P 8224, 2002), has excellent cushioning properties, and exhibits minimal transfer of the resin content. The resin content of the interleaf paper 13 is preferably 0.05% by mass or less (JIS P 8224, 2002), and is particularly preferably about 0.01% by mass (JIS P 8224, 2002). A paper quality that does not adversely affect the quality of the glass plate 11 itself due to the combined effect of the above-mentioned paper surface roughness is selected. Although each side of the interleaf paper 13 is generally straight, depending on the manufacturing conditions (such as the cutting device for the base paper), the sides may be slightly curved or jagged.
[0025] Next, the case where the glass plates 11 and the interleaving paper 13 are removed from the glass plate stack 10 of the glass plate package 17 will be described. Fig. 5 is a schematic cross-sectional view of the glass plate package 17 illustrating a process of removing the glass plate 11 from the glass plate laminate 10. Fig. 6 is a schematic cross-sectional view of the glass plate package 17 illustrating a process of removing the interleaf paper 13 from the glass plate laminate 10. Fig. 7 is a schematic plan view of the glass plate package 17 illustrating a process of removing the interleaf paper 13 from the glass plate laminate 10.
[0026] 5, the uppermost glass plate 11 is sucked by the suction part 23 of the glass plate suction robot 21 and pulled upward, and the uppermost glass plate 11 is removed from the glass plate stack 10. At this time, the side of the glass plate stack 10 is pressed down by the pressing member 25. As a result, the interleaf paper 13 adjacent to the lower side of the uppermost glass plate 11 is peeled off from the uppermost glass plate 11, and the uppermost glass plate 11 is smoothly removed.
[0027] 6 and 7, after the uppermost glass plate 11 is removed, the uppermost interleaf paper 13 is then removed by an interleaf paper removal robot 27. This interleaf paper removal robot 27 has a plurality of gripping parts 29 arranged in a straight line, and these gripping parts 29 pinch and grip one side 13a of the uppermost interleaf paper 13 to be removed.
[0028] Each of the gripping portions 29 has an upper claw portion 31 and a lower claw portion 33, and the rear ends of the upper claw portion 31 and the lower claw portion 33 are rotatably connected by a hinge portion 35. When gripping one side 13a of the interleaf paper 13 with the gripping portions 29, the lower claw portion 33 is inserted below the interleaf paper 13 in the stacking direction, and the upper claw portion 31 is positioned above the interleaf paper 13 in the stacking direction. This causes the one side 13a of the interleaf paper 13 to be positioned between the upper claw portion 31 and the lower claw portion 33 of the gripping portion 29. In this state, the upper claw portion 31 and the lower claw portion 33 are rotated in a direction approaching each other, whereby the one side 13a of the interleaf paper 13 is pinched and gripped by the upper claw portion 31 and the lower claw portion 33. Thereafter, the gripping portion 29 is moved, and the interleaf paper 13 is removed from the glass sheet laminate 10.
[0029] Then, the process of taking out the glass plates 11 by the glass plate suction robot 21 and the process of taking out the interleaf paper 13 by the interleaf paper taking out robot 27 are repeated, so that the glass plates 11 and the interleaf papers 13 are taken out one by one from the glass plate stack 10.
[0030] To laminate the glass plates 11 to form the glass plate laminate 10, the glass plates 11 and the interleaf paper 13 are laminated in that order, in the reverse order to the above-mentioned operation of removing the glass plates 11. At this time, an image is taken with a camera, and the glass plates 11 and the interleaf paper 13 are laminated while being positioned based on the image.
[0031] Incidentally, in the process of removing the interleaf sheets 13 by the interleaf sheet removing robot 27, there are cases where the uppermost interleaf sheet 13 to be removed is poorly gripped.
[0032] Fig. 8 is a schematic plan view of the glass plate package 17, illustrating poor gripping during the step of removing the interleaf paper 13. Fig. 9 is a schematic cross-sectional view of an edge of the glass plate laminate 10, illustrating poor gripping during the step of removing the interleaf paper 13.
[0033] 8, for example, the length of protrusion of one side 13a of the interleaf paper 13 from the glass plate 11 may vary significantly at both ends. If the difference in the protrusion length at both ends of one side 13a of the interleaf paper 13 is too large in this way, there will be areas that cannot be grasped by the multiple gripping parts 29 of the interleaf paper removal robot 27, and the interleaf paper 13 may not be properly gripped.
[0034] Furthermore, if there is a large difference in the overhang length at both ends of one side 13a of the interleaf paper 13, the interleaf paper 13 will not cover the entire surface of the glass sheets 11, and there is a risk that the laminated glass sheets 11 will come into direct contact with each other.
[0035] Also, as shown in Fig. 9, one side 13a of the uppermost interleaf paper 13 and one side 13a of the adjacent interleaf paper 13 on the lower side in the stacking direction may be aligned. That is, in the example shown in Fig. 9, one side 13a (first side) of the interleaf paper 13 adjacent to the upper side in the stacking direction relative to the glass plate 11 is not misaligned with one side 13a (second side) of the interleaf paper 13 adjacent to the lower side in the stacking direction relative to the glass plate 11. When one side 13a of the upper and lower interleaf papers 13 is aligned in this way, it becomes difficult for the lower claw portion 33 of the gripping portion 29 to be inserted between these interleaf papers 13, which may result in poor gripping.
[0036] Thus, in order for the interleaf paper removal robot 27 having a plurality of gripping portions 29 to smoothly remove the interleaf paper 13, the positional relationship of the upper and lower interleaf papers 13 with respect to the glass plates 11 in the glass plate laminate 10 is important.
[0037] For this reason, in the glass plate laminate 10 according to this embodiment, in order to prevent poor gripping and the like as described above and to smoothly remove the interleaf paper 13, the positions of the interleaf paper 13 on the front and back of the glass plate 11 are specified as follows.
[0038] Fig. 10 is a schematic plan view showing the arrangement of the interleaving paper 13 in the glass plate laminate 10. Fig. 11 is a schematic cross-sectional view of an edge of the glass plate laminate 10 in a state where one side 13a of the interleaving paper 13 on the upper side in the stacking direction is shifted inward relative to one side 13a of the interleaving paper 13 on the lower side in the stacking direction. Fig. 12 is a schematic cross-sectional view of an edge of the glass plate laminate 10 in a state where one side 13a of the interleaving paper 13 on the upper side in the stacking direction is shifted outward relative to one side 13a of the interleaving paper 13 on the lower side in the stacking direction.
[0039] In the glass plate laminate 10 according to this embodiment, as shown in FIG. 10, one side 13a of the interleaving paper 13 on the upper side of the glass plate 11 in the stacking direction has a difference (|P1-P2|) between the protruding lengths P1, P2 from the glass plate 11 at both ends of 110 mm or less.
[0040] In this manner, if the difference between the overhang lengths P1, P2 at both ends of one side 13a of the interleaf paper 13 is 110 mm or less, one side 13a of the interleaf paper 13 can be gripped by all of the grippers 29 of the interleaf paper take-out robot 27.
[0041] In the glass sheet laminate 10 according to the present embodiment, as shown in Figs. 11 and 12, one side 13a of the uppermost interleaf paper 13 (hereinafter also referred to as the upper interleaf paper 13) and one side 13a of the interleaf paper 13 adjacent to the upper interleaf paper 13 on the lower side in the stacking direction (hereinafter also referred to as the lower interleaf paper 13) are arranged so as to be misaligned with each other. The upper and lower interleaf papers 13 in the stacking direction have a section in which the amount of misalignment is 1 mm or more in the total length of the one side 13a of the interleaf paper 13 of the interleaf paper 13 of 60% or more, preferably 70% or more, and more preferably 80% or more. The amount of misalignment is the distance between the ends 13a, 13a of the upper and lower interleaf papers 13 when viewed from a direction perpendicular to the main surface of the interleaf paper 13, without taking into consideration the sagging of the upper interleaf paper 13 and the lower interleaf paper 13. That is, it corresponds to the difference in the protruding length of the upper interleaf paper 13 and the lower interleaf paper 13. More specifically, in the example shown in FIGS. 11 and 12, since the interleaf paper 13 is hanging down, the upper and lower interleaf papers 13 are brought into a horizontal state, and then the amount of misalignment is measured by viewing from a direction perpendicular to the main surface of the upper interleaf paper 13.
[0042] In addition, one side 13a of the interleaf paper 13 may be shifted to a position pulled inward relative to the side 13a of the interleaf paper 13 on the lower side in the stacking direction (see FIG. 11), or may be shifted to a position protruding outward relative to the side 13a of the interleaf paper 13 on the lower side in the stacking direction (see FIG. 12).
[0043] In this way, by providing a misalignment of 1 mm or more in a section of 60% or more of the total length of the sides 13a of the upper and lower interleaf sheets 13 in the stacking direction, it becomes easier to insert the lower claw portion 33 of the gripping portion 29 between the interleaf sheets 13 compared to when the sides 13a are aligned. This allows the gripping portion 29 to grip the sides 13a of the interleaf sheets 13 smoothly.
[0044] As described above, in the glass sheet laminate 10 according to this embodiment, the difference between the overhang lengths P1, P2 at both ends of one side 13a of the interleaf paper 13, which is arranged to cover the entire surface of the glass sheet 11 and protect the entire surface of the glass sheet 11, is set to 110 mm or less. Furthermore, in this glass sheet laminate 10, a shift of 1 mm or more is provided for the interleaf paper 13 on the lower side in the stacking direction in a section of 60% or more of the total length. This makes it easier to insert the lower claw portion 33 of the gripping portion 29 between the upper and lower interleaf papers 13 in the stacking direction, and allows all of the gripping portions 29 of the interleaf paper removal robot 27 to grip one side 13a of the interleaf paper 13. Therefore, poor gripping of the interleaf paper 13 is suppressed, and the interleaf paper 13 can be smoothly removed.
[0045] As a result, the glass plate package 17 including the glass plate laminate 10 is a package that contains the glass plate laminate 10 from which the interleaf paper 13 can be smoothly removed by the interleaf paper removal robot 27, thereby improving the ease of unpacking.
[0046] However, if the length of the interleaf paper 13 protruding from the glass plate 11 is too short, the end face of the glass plate 11 may not be adequately protected by the interleaf paper 13, or it may be difficult to hold down the side 13a of the interleaf paper 13 from the side. Furthermore, the interleaf paper 13 protruding from the glass plate 11 overhangs rather than sagging, so that the sides 13a of the upper and lower interleaf papers 13 tend to align with each other. Furthermore, if the length of the interleaf paper 13 protruding from the glass plate 11 is too long, the protruding portion of the interleaf paper 13 may sag too much due to its own weight, so that the sides 13a of the upper and lower interleaf papers 13 tend to align with each other or to come into close contact with each other. Therefore, if the length of the interleaf paper 13 protruding from the glass plate 11 is too short or too long, it may be difficult for the interleaf paper 13 to be gripped by the gripping portion 29 of the interleaf paper removal robot 27.
[0047] In the glass plate laminate 10 according to this embodiment, the protruding length of one side 13a of the interleaf paper 13 from the glass plate 11 is preferably 10 mm or more and 110 mm or less. In this way, by setting the protruding length of one side 13a of the interleaf paper 13 from the glass plate 11 to 10 mm or more and 110 mm or less, the one side 13a of the interleaf paper 13 can be made to hang down appropriately. Therefore, while the end face of the glass plate 11 is sufficiently protected, poor gripping caused by the side 13a of the interleaf paper 13 being aligned with the side 13a of the interleaf paper 13 on the lower side in the stacking direction can be further prevented.
[0048] In addition, the interleaf paper 13 may be manufactured with the fibers aligned in one direction during the manufacturing process. In the interleaf paper 13 having a grain direction, which is the orientation direction of the fibers, the stiffness and tensile strength, in particular, differ depending on the grain direction, and the amount of deflection due to its own weight also differs.
[0049] In the glass sheet laminate 10 according to the present embodiment, when the interleaf paper 13 has horizontal streaks in which the streaks of aligned fibers are arranged substantially parallel to the side 13a, the overhang length of the side 13a is preferably 20 mm to 80 mm, more preferably 25 mm to 75 mm, and even more preferably 30 mm to 70 mm. In this way, when the interleaf paper 13 has horizontal streaks, if the overhang length of the side 13a of the interleaf paper 13 is 20 mm to 80 mm, the side 13a of the interleaf paper 13 is allowed to hang down appropriately, and poor gripping caused by the side 13a of the interleaf paper 13 lining up with the side 13a of the interleaf paper 13 on the lower side in the stacking direction can be further prevented.
[0050] Furthermore, in the glass sheet laminate 10 according to this embodiment, when the interleaf paper 13 has vertical streaks in which the streaks of aligned fibers are arranged substantially perpendicular to the side 13a, the overhang length of the side 13a is preferably 20 mm to 110 mm, more preferably 20 mm to 80 mm, even more preferably 25 mm to 75 mm, and particularly preferably 30 mm to 70 mm. Thus, in the case of vertical streaks, if the overhang length of the side 13a of the interleaf paper 13 is 20 mm to 110 mm, the side 13a of the interleaf paper 13 is allowed to hang down appropriately, and poor gripping caused by the side 13a of the interleaf paper 13 lining up with the side 13a of the interleaf paper 13 on the lower side in the stacking direction can be further prevented. EXAMPLES
[0051] <Hawk insertion test> (Test Method) In a glass plate laminate consisting of 20 sheets of glass plate and slip paper, a test was conducted in which the lower claw of the gripping part was inserted between the first and second slip paper, which was the uppermost sheet. Note that a stainless steel claw with a thickness of 0.5 mm was used as the lower claw. The insertion test was performed 20 times under each condition, varying the length of protrusion from the glass plate and the amount of misalignment between the slip sheets, and the success rate (number of successful insertions / number of trials) was calculated. Note that one side of the first slip sheet and one side of the second slip sheet were arranged parallel to each other.
[0052] (Glass plate and interleaving paper) (1) Glass plate Size: long side 470mm, short side 370mm Thickness: 0.5mm (2) Interleaf paper Size: long side 500mm, short side 400mm Clark stiffness for horizontal bars: 17.5 cm 3 / 100 Clark stiffness for vertical grain: 52cm 3 / 100
[0053] (Test Results) The test results for horizontal stripes, with the stripe direction parallel to one side, are shown in Table 1 and Figure 13, while the test results for vertical stripes, with the stripe direction perpendicular to one side, are shown in Table 2 and Figure 14. Note that a positive deviation is the deviation when the first slip sheet is shifted outward relative to the second slip sheet, and a negative deviation is the deviation when the first slip sheet is shifted inward relative to the second slip sheet.
[0054] [Table 1]
[0055] [Table 2]
[0056] As shown in Table 1 and Figure 13, in the case of horizontal stripes, if the protrusion length was between 20mm and 80mm, which is in the range of around 50mm, the claw could be inserted without any problems even if the misalignment between the first and second sheets was 1mm. In particular, if the protrusion length was 100mm or less and the misalignment between the first and second sheets was 3mm or more, the insertion of the claw was generally successful (success rate of 95-100%). Also, if the protrusion length was 50mm and the misalignment between the first and second sheets was 1mm or more, the insertion of the claw had a high success rate (success rate of 90% or more). As shown in Table 2 and Figure 14, in the case of vertical stripes, if the overhang length was between 20 mm and 110 mm, the claws could be inserted without any problem even if the misalignment between the first and second sheets was 1 mm. In particular, when the overhang length was 100 mm, the insertion of the claws was generally successful (success rate of 95% or more) if the misalignment between the first and second sheets was 1 mm or more. Thus, in the case of vertical stripes, the stiffness of the interleaf paper is stronger, so it is presumed that a longer overhang length of the interleaf paper will create a gap between the interleaf sheets and make it easier for the claws to insert them than in the case of horizontal stripes.
[0057] <Interleaf removal test> (Test Method) In a glass plate laminate in which glass plates and slip sheets are alternately stacked, a slip sheet removal test was conducted in which the long side of the first slip sheet, which is the topmost slip sheet, was grasped and removed using multiple (6) gripping parts arranged in a straight line. The slip sheet removal test was carried out for four patterns of glass plate laminates in which glass plates and slip sheets of different sizes were laminated, and for Test Examples 1 to 18 in which the lamination conditions were varied. Note that in Test Examples 1 to 14, the glass plate laminates were arranged horizontally on a flat pallet, and in Test Examples 15 to 18, the glass plate laminates were arranged vertically on the base of a vertical pallet. The lamination conditions were mainly changed in the angle of the long side of the first laminate relative to the second laminate (the second sheet of laminate), the amount of deviation of the long side of the first laminate relative to the second laminate (the amount of deviation of the intersection of the diagonals of the first laminate relative to the intersection of the diagonals of the second laminate in the direction in which the short side of the second laminate extends), and the difference in the overhang length of both ends of the long side of the first laminate. The difference in the overhang length between both ends of the long side of the second interleaf paper was set to 0 mm. In other words, the long side of the second interleaf paper was parallel to the edge of the glass plate in a plan view. Test Examples 2 to 6, 9, 10, 12, 13, and 15 to 17 are working examples, and Test Examples 1, 7, 8, 11, 14, and 18 are comparative examples.
[0058] (Glass plate laminate) (1) Test Examples 1 to 8 Glass plate size: long side 3370mm, short side 2940mm, thickness: 0.5mm Insertion paper size: long side 3470mm, short side 3040mm Length of slip sheet overhang in the long side direction: 50 mm Length of interleaf paper protruding in the short side direction: 50 mm (2) Test Examples 9 to 11 Glass plate size: long side 2620mm, short side 2200mm, thickness: 0.5mm Insertion paper size: long side 2720mm, short side 2300mm Length of slip sheet overhang in the long side direction: 50 mm Length of interleaf paper protruding in the short side direction: 50 mm (3) Test Examples 12 to 14 Glass plate size: long side 2250mm, short side 1950mm, thickness: 0.5mm Insertion paper size: long side 2350mm, short side 2050mm Length of slip sheet overhang in the long side direction: 50 mm Length of interleaf paper protruding in the short side direction: 50 mm (4) Test Examples 15-18 Glass plate size: long side 1800mm, short side 1500mm, thickness: 0.5mm Size of interleaf paper: long side 1890mm, short side 1550mm Length of slip sheet overhang in the long side direction: 45 mm Length of interleaf paper protruding in the short side direction: 50 mm In addition, in Test Examples 15 to 18 in which the sheets were stacked on an inclined base, the protruding length of the interleaf paper in the short side direction on the lower side of the inclination was set to 0 mm.
[0059] (Test Results) The test results are shown in Table 3. The meanings of ◎, ◯, △, and × in the evaluation results in Table 3 are as follows: ◎: The first interleaf paper was picked up by all gripping parts of the interleaf removal robot, and the first interleaf paper was removed stably. ○: Part of the gripping part of the slip sheet removal robot was unable to grasp the first slip sheet, but the first slip sheet was removed without any problems. △: A part of the gripping portion of the slip sheet removal robot was not able to grasp the first slip sheet, and there were cases where the first slip sheet could not be removed, but this was at a level that was practically acceptable. ×: The first interleaf paper could not be gripped by most of the gripping parts of the interleaf removal robot, and the first interleaf paper could not be removed satisfactorily in most trials. In other words, the level was not suitable for practical use. In addition, in the misalignment amounts on the long sides of the first and second interleaving papers in Table 3, a positive misalignment amount is the amount of misalignment when the first interleaving paper is misaligned outward relative to the second interleaving paper, and a negative misalignment amount is the amount of misalignment when the first interleaving paper is misaligned inward relative to the second interleaving paper.
[0060] [Table 3]
[0061] Test Example 1: In Test Example 1, in which there was no difference in the protruding length between the first and second interleaf sheets, the first interleaf sheet could not be removed satisfactorily (evaluation: ×). Test Examples 2 to 4: In Test Examples 2 to 4 in which the difference in overhang length between the first and second interleaf sheets was 1 mm or more and this range was 85% or more, the first interleaf sheet could be stably removed (evaluated as ⊚). Test Example 5: The difference in the protruding length between the first and second interleaf sheets was 1 mm or more, and in Test Example 5 where this range accounted for 83%, the first interleaf sheet could be removed without any problems (evaluation ◯). Test Example 6: The difference in the protruding length between the first and second interleaf sheets was 1 mm or more, and in Test Example 6 where this range accounted for 71%, the first interleaf sheet could be removed at a level that was practically acceptable (evaluation △). Test Example 7: The difference in the protruding length between the first and second interleaf sheets was 1 mm or more, and in Test Example 7, in which the difference was 55%, the first interleaf sheet could not be removed satisfactorily (evaluation: ×). Test Example 8: In Test Example 8, where the difference in overhang length between both ends of the long side of the first interleaf was 152 mm, the difference in overhang length between the first interleaf and the second interleaf was 1 mm or more, and although this range was 86%, the first interleaf could not be removed satisfactorily (evaluation: ×). Also, in Test Example 8, uncovered portions of the glass plate were generated, and the glass plate could not be adequately protected. Test Example 9: The difference in the protruding length between the first and second interleaf sheets was 1 mm or more, and in Test Example 9 where this range accounted for 63%, the first interleaf sheet could be removed at a level that was practically acceptable (evaluation △). Test Example 10: The difference in the protruding length between the first and second interleaf sheets was 1 mm or more, and in Test Example 10 in which this range accounted for 81%, the first interleaf sheet could be removed stably (evaluated as ⊚). Test Example 11: In Test Example 11, where the difference in overhang length between both ends of the long side of the first interleaf was 115 mm, the difference in overhang length between the first interleaf and the second interleaf was 1 mm or more, and although this section was 83%, the first interleaf could not be removed well (evaluation: ×). Also, in Test Example 11, uncovered portions of the glass plate were generated, and the glass plate could not be adequately protected. Test Example 12: The difference in the protruding length between the first and second interleaf sheets was 1 mm or more, and in Test Example 12 in which this range accounted for 63%, the first interleaf sheet could be removed at a level that was practically acceptable (evaluation △). Test Example 13: The difference in the protruding length between the first and second interleaf sheets was 1 mm or more, and in Test Example 13 where this range accounted for 83%, the first interleaf sheet could be removed stably (evaluated as ⊚). Test Example 14: The difference in the protruding length between the first and second interleaf sheets was 1 mm or more, and in Test Example 14, where this range was 85%, the first interleaf sheet could be removed at a level that was practically acceptable (evaluation: △). However, in Test Example 14, uncovered portions of the glass plate were generated, and the glass plate could not be adequately protected. Test Example 15: The difference in the protruding length between the first and second interleaf sheets was 1 mm or more, and in Test Example 15 where this range was 100%, the first interleaf sheet could be removed stably (rating ⊚). Test Example 16: The difference in the protruding length between the first and second interleaf sheets was 1 mm or more, and in Test Example 16 in which this range accounted for 70%, the first interleaf sheet could be removed at a level that was practically acceptable (evaluation △). Test Example 17: The difference in the protruding length between the first and second interleaf sheets was 1 mm or more, and in Test Example 17 where this range was 95%, the first interleaf sheet could be removed stably (rating ⊚). Test Example 18: The difference in the protruding length between the first and second interleaf sheets was 1 mm or more, and in Test Example 18, where this range was 92%, the first interleaf sheet could be removed at a level that was practically acceptable (evaluation △). However, in Test Example 18, uncovered portions of the glass plate were generated, and the glass plate could not be adequately protected.
[0062] As described above, if there is no difference in the protruding length between the first and second interleaf sheets, the first and second interleaf sheets will be aligned, and it is presumed that the first interleaf sheet cannot be removed satisfactorily (Test Example 1). In contrast, when there is a difference of 1 mm or more in the overhanging length between the first and second interleaf sheets and this difference accounts for 60% or more, it is estimated that the first interleaf sheet can be removed by the gripping portion (Test Examples 2-6, 9, 10, 12, 13, 15-17). In particular, when the angle between the long sides of the first and second interleaf sheets was 0°, the first interleaf sheet could be smoothly removed by moving it in parallel (Test Examples 2, 3, and 15). Furthermore, when there was no misalignment between the long sides of the first and second interleaving papers and the angle between the long sides of the first and second interleaving papers was small (for example, 0.1° or less), the area in which there was a difference in the protruding length between the first and second interleaving papers became narrower, making it difficult to remove the first interleaving paper (Test Example 7). Furthermore, when there is no misalignment between the long sides of the first and second interleaf sheets and the angle between the long sides of the first and second interleaf sheets is large (for example, 2.4° or more), even if the section in which there is a difference in the overhang length between the first and second interleaf sheets is sufficient, the first interleaf sheet will not be able to cover the glass plate and will not be able to adequately protect the glass plate (Test Examples 8, 11, 14, and 18).
[0063] The present invention is not limited to the above-described embodiment, and can be appropriately modified, improved, etc. In addition, the material, shape, size, number, arrangement location, etc. of each component in the above-described embodiment are arbitrary as long as the present invention can be achieved, and are not limited.
[0064] Here, the features of the embodiments of the glass sheet laminate and the glass sheet package according to the present invention described above will be briefly summarized and listed in the following [1] to [5]. [1] A glass plate laminate (10) in which interleaf papers (13) are arranged on the front and back surfaces of glass plates (11) and laminated together, The interleaf paper (13) is arranged to cover the glass plate (11), A first side (side 13a) of the interleaf paper (13) adjacent to the upper side of the glass plate (11) in the stacking direction is the difference between the protruding lengths (P1, P2) of both ends of the first side from the glass plate (11) is 110 mm or less, a section of one side of the interleaf paper (13) adjacent to the glass plate (11) on the lower side in the stacking direction, the section being shifted by an amount of shift of 1 mm or more from a second side (side 13a) that is the side located below the first side, as viewed in the stacking direction, occupies 60% or more of the entire length of the first side. [2] The glass plate laminate according to [1], wherein the length of the interleaving paper (13) protruding from the glass plate (11) at the first side (side 13a) is 10 mm or more and 110 mm or less. [3] The glass sheet laminate according to [2], wherein the interleaf paper (13) is arranged such that a grain direction, which is a fiber orientation direction, is approximately parallel to the first side (side 13a), and the protruding length is 20 mm or more and 80 mm or less. [4] The glass sheet laminate according to [2], wherein the interleaf paper (13) is arranged such that a grain direction, which is a fiber orientation direction, is approximately perpendicular to the first side (side 13a), and the protruding length is 20 mm or more and 110 mm or less. [5] A glass sheet laminate (10) according to any one of [1] to [4] and a base (15), The glass plate package is obtained by packaging the glass plate laminate in a state where the glass plate laminate is placed on a base.
[0065] This application is based on Japanese patent application No. 2023-081622 filed on May 17, 2023, the contents of which are incorporated herein by reference. [Explanation of symbols]
[0066] 10: Glass plate laminate 11: Glass plate 13: Interleaf paper 13a: One side 15: Pedestal 17: Glass plate packaging P1, P2: overhang length
Claims
1. A glass plate laminate in which interleaf papers are arranged on the front and back surfaces of glass plates, the interleaf paper is disposed so as to cover the glass plate, A first side, which is one side of the interleaf paper adjacent to the upper side of the glass plate in the stacking direction, a difference in the protrusion length from the glass plate at both ends of the first side is 110 mm or less; a section of one side of the interleaf paper adjacent to the lower side of the glass plate in the stacking direction, the section being shifted by an amount of shift of 1 mm or more as viewed in the stacking direction with respect to a second side that is a side located on the lower side of the first side, is 60% or more of a total length of the first side; Glass sheet laminate.
2. The length of the interleaf paper protruding from the glass plate at the first side is 10 mm or more and 110 mm or less. The glass sheet laminate according to claim 1 .
3. The interleaf paper is arranged such that a grain direction, which is a fiber orientation direction, is substantially parallel to the first side, and the protruding length is 20 mm or more and 80 mm or less. The glass sheet laminate according to claim 2.
4. The interleaf paper is arranged such that a grain direction, which is a fiber orientation direction, is substantially perpendicular to the first side, and the protruding length is 20 mm or more and 110 mm or less. The glass sheet laminate according to claim 2.
5. The glass sheet laminate according to any one of claims 1 to 4, and a base, The glass plate laminate is packaged in a state in which the glass plate laminate is placed on the base. Glass plate packaging.
Citation Information
Patent Citations
Glass-plate packing body
WO2021106451A1