Manufacturing method of heat sink
By employing knockout pins with a circular tip and sub-knockout pins to form elliptical pin fins, the method addresses the high costs and deformation issues in existing heat sink manufacturing, achieving efficient and cost-effective production with improved heat dissipation.
Patent Information
- Application Number
- JP2023084132
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-22
- Publication Date
- 2024-12-04
AI Technical Summary
Existing methods for manufacturing heat sinks with elliptical pin fins are costly and prone to deformation during processing, leading to high mold costs and product prices due to the need for complex cutting and machining to remove burrs and excess metal.
A method for manufacturing heat sinks with elliptical pin fins using knockout pins with a circular tip diameter equal to or smaller than the minor axis of the pin fins, combined with sub-knockout pins if necessary, to minimize gaps and deformations during forging, allowing for efficient production and reduced machining costs.
This approach enables the production of heat sinks with high heat dissipation performance at lower costs by minimizing deformation and machining requirements, thus reducing overall manufacturing expenses.
Smart Images

Figure 2024167797000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a heat sink. [Background technology]
[0002] A heat sink having a structure including a plate-shaped base and a plurality of pin fins provided on one surface of the base is known. A forging method is known as a method for manufacturing a heat sink having such a structure. As a forging method, a metal material, which is a raw material of the heat sink, is placed on a die having a plurality of holes, and a punch is used to press the metal material toward the die, thereby stretching the metal material in the outer circumferential direction of the die to form a base, and causing the metal material to flow into each of the plurality of holes to form pin fins. Known forging methods using a die include a burr removal method (also called a semi-closed method) and a closed method. The burr removal method is a method in which a gap is provided between the punch and the die, and the metal material that does not flow into the plurality of holes is allowed to flow out from the gap to the outside. The closed method is a method in which the metal material is sealed between the punch and the die without providing a gap between the punch and the die (see, for example, Patent Documents 1 and 2).
[0003] In forging equipment, knockout pins (knock pins) are set into the die holes used to form the pin fins, and knockout pins are generally of the same shape as the die holes. The reason for this is that if a knockout pin with a different shape than the die hole is used, a large gap will be created between the die hole and the knockout pin. As a result, the forging material will flow into the gap during forging, causing burrs and excess material, which will require post-processing (removal by deburring or machining).
[0004] Many pin fins are cylindrical in shape, and when forming them, it is common to use a die (lower mold) with a cylindrical hole and a long, thin cylindrical knockout pin of the same shape as the hole. If the knockout pin is cylindrical, techniques such as centerless grinding can be used, which means that it can be produced in a relatively short amount of time and is relatively easy to process, making it possible to produce a pin at low cost and with high precision.
[0005] For the reasons stated above, when forming elliptical pin fins, it is optimal to use a die (lower die) with an elliptical cylindrical hole and a knockout pin with the same elliptical cylindrical shape as the hole. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2008-155237 A [Patent Document 2] JP 2019-107679 A [Patent Document 3] JP 2014-75385 A Summary of the Invention [Problem to be solved by the invention]
[0007] However, when manufacturing a long and thin elliptical cylindrical knockout pin, it is not possible to use the centerless grinding method, and it is necessary to use a cutting method, etc. In that case, when manufacturing a long and thin pin, the processing is very difficult because the product needs to be held and deformation (bending) occurs during processing, and it takes a long time to manufacture, so the manufacturing cost becomes very high. This leads to increased mold costs, and when molding is performed using such molds, the product price becomes high.
[0008] On the other hand, when the pin fins have an irregular shape such as an elliptical shape, particularly in a cooler that uses a liquid such as a refrigerant, it is expected that the cooling efficiency will be improved while suppressing an increase in pressure loss of the refrigerant (for example, see Patent Document 3).
[0009] When forming elliptical pin fins, if a cylindrical knockout pin is used in a die (lower die) with an elliptical cylindrical hole, a gap will occur between the die hole and the tip of the knockout pin, resulting in burrs and excess material, but these can be removed by machining in post-processing. Since the cutting process costs less than the die manufacturing cost, the product price is also cheaper.
[0010] In addition, in order to suppress deformation of the pin during forging and knocking out, it is desirable for the diameter of the tip of the knockout pin to be approximately the same dimension as the minor axis of the elliptical die hole (approximately 0.01 to 0.5 mm smaller than the minor axis).
[0011] The present invention has been made in consideration of the above circumstances, and has an object to provide a method for manufacturing a heat sink that can be manufactured inexpensively while providing a heat sink with high heat dissipation performance. [Means for solving the problem]
[0012] In order to solve the above problems, the present invention provides the following means.
[0013] A first aspect of the present invention is a method for manufacturing a heat sink having a plate-shaped base portion and a plurality of pin fins standing on one surface of the base portion, at least some of the pin fins having an elliptical or approximately elliptical shape when viewed in a plane, in which forging and ejection are performed using a knockout pin having a circular tip shape and a diameter equal to or less than the minor axis of the elliptical or approximately elliptical shape of the pin fin.
[0014] In a second aspect of the present invention, in the manufacturing method of a heat sink according to the first aspect, in addition to the knock-out pin, at least one sub-knock-out pin having a circular tip shape with a diameter of less than or equal to {(major axis of the elliptical or approximately elliptical shape-minor axis of the elliptical or approximately elliptical shape)÷2} is further used in the same die hole to perform forging and ejection.
[0015] A third aspect of the present invention is the method for producing a heat sink according to the first aspect, wherein the circular tip diameter of the knockout pin is in the range of φ0.1 mm to 20 mm.
[0016] A fourth aspect of the present invention relates to the method for manufacturing a heat sink according to the second aspect, wherein the diameter of the circular tip of the knockout pin and the sub knockout pin is in the range of φ0.1 mm to 20 mm. Effect of the Invention
[0017] According to the method for manufacturing a heat sink of the present invention, it is possible to provide a method for manufacturing a heat sink that has high heat dissipation performance and can be manufactured inexpensively. [Brief description of the drawings]
[0018] [Figure 1] FIG. 1 is a cross-sectional view of a forging device that can be used in the manufacturing method of a heat sink of this embodiment, and shows a schematic diagram of a state before starting forging of a metal material M. [Diagram 2] FIG. 1 is a cross-sectional view of a forging device that can be used in the method for producing a heat sink of this embodiment, and shows a schematic diagram of a state immediately after pressure application of a metal material M begins. [Diagram 3] FIG. 1 is a cross-sectional view of a forging device that can be used in the method for producing a heat sink of this embodiment, and shows a schematic diagram of a state immediately after pressing of a metal material M is completed. [Figure 4] FIG. 1 is a cross-sectional view of a forging device that can be used in the manufacturing method of a heat sink of this embodiment, and shows a schematic diagram of a state immediately after starting to eject metal material M from a die. [Diagram 5] 1A is a schematic diagram showing a case where the gap between the knockout pin and the die is large, and FIG. 1B is a schematic diagram showing a defect that may occur in a case such as that shown in FIG. [Figure 6] 4 is a schematic diagram showing an example of a relationship between a knockout pin and a through hole of a die used in the method for manufacturing a heat sink of the present embodiment. FIG. [Figure 7]10A to 10C are schematic diagrams showing other examples of the relationship between the knockout pins and the through holes of the die used in the method for manufacturing the heat sink of the present embodiment. [Figure 8] 13 is a schematic diagram showing yet another example of the relationship between the knockout pin and the through hole of the die used in the method for manufacturing the heat sink of the present embodiment. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] Hereinafter, a heat sink and a method for manufacturing a heat sink according to an embodiment of the present invention will be described in detail with reference to the drawings. The drawings used in the following description may show characteristic parts in an enlarged scale for the sake of convenience in order to make the characteristics of the present invention easier to understand, and the dimensional ratios of each component may differ from the actual ones. The materials, dimensions, etc. exemplified in the following description are merely examples, and the present invention is not limited thereto, and may be modified as appropriate within the scope of the effects of the present invention.
[0020] The heat sink manufacturing method of this embodiment is a method for manufacturing a heat sink having a plate-shaped base portion and a number of pin fins standing on one surface of the base portion, where at least some of the pin fins have an elliptical or approximately elliptical shape in a planar view, and forging and ejection are performed using a knockout pin having a circular tip shape and a diameter equal to or less than the minor axis of the elliptical or approximately elliptical shape of the pin fin. In this specification, the term "approximately elliptical shape" is intended to allow a processing error of about several percent with respect to a strict elliptical shape, within the scope of the effects of the present invention.
[0021] The method for manufacturing a heat sink includes a preparation step of preparing a die, and a pressurization step of pressing a metal material against the die in a sealed or semi-sealed state. The pressurization step can be performed using a forging device. It is preferable to use a material with good thermal conductivity as the metal material for the forging base material. Examples of the metal material include, but are not limited to, aluminum and copper.
[0022] Fig. 1 is a cross-sectional view of a forging device that can be used in the manufacturing method of a heat sink according to this embodiment. Reference symbol M is a metal material (forged blank). Fig. 1 shows a schematic state of the metal material M before the start of forging, and Figs. 2 to 4 show a schematic state of the metal material M immediately after pressure application starts, immediately after pressure application is completed, and immediately after the start of ejection of the forged blank, respectively.
[0023] 1, the forging device 100 has a punch (upper die) 111, a die (lower die) 112, and a die holder 114. The die 112 has a forming hole 112A formed as a downward recess on the upper surface side thereof, and a metal material (forging blank) M, which is the material of the heat sink, is placed on the forming hole 112A.
[0024] The punch 111 presses the metal material M toward the die 112. A plurality of through holes 113 (113a, 113b, 113c, 113d) that penetrate in the vertical direction are formed in the bottom wall of the forming hole 112A in the die 112. A knockout pin 118 is arranged in each through hole 113 so as to be slidable in the vertical direction. The punch 111 is movable up and down along the inner wall of the die 112.
[0025] The die holder 114 has an anvil 115, cylindrical knockout pins 118 (118a, 118b, 118c, 118d), a knockout plate 119, and an ejector 120. The anvil 115 has a bottom plate 116 and a cylindrical die support 117 arranged around the bottom plate 116. The bottom plate 116 has an opening in the center into which the ejector 120 is inserted. The knockout pins 118a, 118b, 118c, 118d are inserted into a plurality of through holes 113a, 113b, 113c, 113d of the die 112. The knockout pins 118a, 118b, 118c, 118d are supported by the knockout plate 119. The knockout plate 119 is arranged on the bottom plate 116 and the ejector 120. The ejector 120 is movable in the vertical direction. In accordance with the vertical movement of the ejector 120, the knockout pins 118a, 118b, 118c, and 118d move in the vertical direction via the knockout plate 119.
[0026] In the illustrated example, fin forming recess 142 is defined by through hole 113 and knock out pin 118 , more specifically, by the inner circumferential surface of through hole 113 and the upper end surface of knock out pin 118 . In this example, through holes 113 are formed in die 112 to form fin forming recesses 142, but the present invention is not limited to this, and bottomed holes may be formed in die 112 to form fin forming recesses 142 using the bottomed holes. Furthermore, a portion of fin forming recesses 142 may be configured with through holes 113. For example, half of fin forming recesses 142 may be configured with through holes 113, and the remaining half may be configured with bottomed holes.
[0027] When the punch 111 is driven into the die 112, the space surrounded by the tip surface of the punch 111 and the forming hole 112A of the die 112 is formed as the base forming portion 141, and the space between the outer peripheral surface of the punch 111 and the inner peripheral surface of the forming hole 112A above the outer periphery of the base forming portion 141 is formed as the burr forming portion 143.
[0028] An example of a process for producing a heat sink by performing a forging process using such a forging apparatus 100 will be described with reference to Figs.
[0029] First, the die 112 is placed on the die support 117 of the die holder 114. Next, the knockout pins 118a, 118b, 118c, and 118d are inserted into the through holes 113a, 113b, 113c, and 113d of the die 112, and the knockout pins 118a, 118b, 118c, and 118d are pushed in until they come into contact with the knockout plate 119. Next, the position of the knockout plate 119 is adjusted to set the positions of the upper ends of the knockout pins 118a, 118b, 118c, and 118d, i.e., the depths of the through holes 113a, 113b, 113c, and 113d.
[0030] Next, the metal material M is placed at the center of the die 112 (the center in the X direction and the Y direction). There is no limitation on the shape of the metal material M as long as it can be accommodated in the forming hole 112A of the die 112. The shape of the metal material M may be a square plate shape (hexahedron), a round plate shape, or an irregular shape. In order to suppress the positional deviation in the forming hole 112A of the die 112, it is preferable that the shape of the metal material M is close to the shape of the forming hole 112A. The metal material M may be chamfered. The metal material M may be cut out from a rolled material by trimming or machining. The metal material M may be manufactured by cutting or cutting out a flat or round extrusion material or a square or round continuous cast rod. The metal material M may be annealed (O treatment) to improve ductility. The metal material M may be lubricated by applying a lubricant to the surface. The annealing treatment may be performed after the lubricating treatment.
[0031] Next, after the metal material M is set in the forming hole 112A, the punch 111 is lowered to pressurize the metal material M. Immediately after the punch 111 starts to pressurize the metal material M, as shown in FIG. 2, the metal material M is divided into metal flowing toward the center (inner diameter direction) and metal flowing toward the outside (outer diameter direction). Of these, the metal flowing toward the center flows into the through hole 113 (fin forming recess 142) in the central portion. The metal flowing toward the outside flows into the through hole 113 (fin forming recess 142) in the outer periphery and into the flash forming portion 143 between the punch 111 and the inner peripheral surface of the forming hole 112A. Here, the amount of metal flowing in the center of the base forming portion 141 is sufficiently secured, so that the fin forming recess 142 in the central portion is sufficiently filled with metal.
[0032] Pressurization continues, and when it is completed, as shown in FIG. 3, a forged product 10 (see FIG. 4) having the base portion 2, the pin fins 3, and the burrs 10a is formed integrally therewith.
[0033] After the base portion 2 and the pin fins 3 are thus formed, as shown in Fig. 4, the ejector 120 is moved upward to move the knockout pins 118a, 118b, 118c, and 118d upward via the knockout plate 119, thereby pushing out the pin fins. As a result, the forged material 10 is removed from the die 112. This forged material 10 is subjected to finishing such as trimming to remove burrs 10a and the like, thereby obtaining a heat sink as a forged product.
[0034] 5(a), if the gap S between the knockout pin 118 and the through-hole 113 of the die 112 is large, the knockout pin 118 cannot be stably fixed. In this case, as shown in FIG. 5(b), problems such as bending or breaking of the knockout pin 118 due to the molding load may occur.
[0035] FIG. 6 is a schematic diagram showing an example of the relationship between a knockout pin and a through hole of a die used in the method for producing a heat sink according to this embodiment. The knockout pin 18 has a circular tip and a diameter equal to or smaller than the minor axis of the elliptical or nearly elliptical pin fin. In order to form an elliptical or nearly elliptical pin fin, the die through hole (die hole) 13 is elliptical or nearly elliptical. In order to suppress deformation of the knockout pin during forging and knocking, it is preferable that the diameter of the tip of the knock pin is approximately the same as the minor axis of the elliptical die hole (approximately 0.01 to 0.5 mm smaller than the minor axis).
[0036] In this way, when forming elliptical or approximately elliptical pin fins, if a cylindrical knockout pin 18 is used in a die having an elliptical-cylindrical die hole 13, a gap will occur between the die hole 13 and the tip of the knockout pin 18, resulting in burrs and excess material, but this can be removed by machining in post-processing. By using a cylindrical knockout pin rather than an elliptical-cylindrical knockout pin in this way when forming elliptical or approximately elliptical pin fins, the cutting process costs are cheaper than the die production costs, and the product price is also cheaper.
[0037] FIG. 7 is a schematic diagram showing an example of the relationship between another example of a knockout pin and a through hole of a die used in the method for manufacturing a heat sink according to the present embodiment. In the example shown in FIG. 7, a cylindrical knock having a diameter almost equal to the minor axis of the elliptical die hole 13 is used. In addition to the out pin 18, sub knockout pins 18-1 and 18-2 having a circular tip shape with a diameter of less than (longer diameter of the ellipse shape of the die hole 13--short diameter of the ellipse shape)÷2 are arranged on both sides of the knockout pin 18. As shown in Figure 7, when the long diameter of the elliptical shape of the die hole 13 and the diameter of the knockout pin 18 + the diameter of the sub knockout pin 18-1 + the diameter of the sub knockout pin 18-2 approximately match, the knockout pin and the sub knockout pin can be stably fixed.
[0038] FIG. 8 is a schematic diagram showing the relationship between a knockout pin and a through hole of a die in yet another example used in the method for manufacturing a heat sink according to the present embodiment. In the example shown in Figure 8, in addition to a cylindrical knockout pin 18 with a diameter approximately the same as the minor axis of the elliptical die hole 13, a sub-knockout pin 18-1 having a circular tip shape with a diameter of less than (major axis of the elliptical shape of the die hole 13 - minor axis of the elliptical shape) ÷ 2 is arranged on one side of the knockout pin 18.
[0039] The diameter of the circular tip of the knockout pin and the sub knockout pin is preferably in the range of φ0.1 mm to 20 mm. [Explanation of symbols]
[0040] 2 Base 3. Pinfin 13 Through hole (die hole) 111 Punch (upper die) 112 Die (lower die) M Metal materials (forging materials)
Claims
1. A method for manufacturing a heat sink having a plate-shaped base and a plurality of pin fins standing on one surface of the base, at least some of the pin fins having an elliptical or nearly elliptical shape in a plan view, comprising the steps of: A method for manufacturing a heat sink, comprising the steps of: performing forging and ejecting using a knockout pin having a circular tip shape and a diameter equal to or smaller than the minor axis of the elliptical or nearly elliptical shape of the pin fin;
2. 2. The method for manufacturing a heat sink according to claim 1, wherein in addition to the knockout pin, at least one sub-knockout pin having a circular tip shape with a diameter of less than or equal to {(major axis of the elliptical or approximately elliptical shape-minor axis of the elliptical or approximately elliptical shape)÷2} is further used in the same die hole to be forged and ejected.
3. The method for manufacturing a heat sink according to claim 1, wherein the circular tip diameter of the knockout pin is in the range of φ0.1 mm to 20 mm.
4. The method for manufacturing a heat sink according to claim 2 , wherein the circular tip diameter of the knockout pin and the sub knockout pin is in the range of φ0.1 mm to 20 mm.
Citation Information
Patent Citations
Knock-out device for forging and forging apparatus
JP2008155237A
Cooling device and semiconductor device
JP2014075385A
Forging apparatus
JP2019107679A