Shrink-wrapped blasting charges and their manufacturing method

JP2024168266APending Publication Date: 2024-12-05ANCHOR INC
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023084785
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-23
Publication Date
2024-12-05

AI Technical Summary

Benefits of technology

【0006】 本発明によれば、図4及び図5に示すように、裸アンコは軟質の熱収縮性フィルムでシュリンク包装されるので、裸アンコの性状を実質的に変えることがない。しかも、軟質の熱収縮性フィルムでシュリンクして密封されるので、包装による容積増加は10%以内に留まり、自動装填機による自動装填に支障のないシュリンク包装アンコを提供することができる。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024168266000001_ABST
    Figure 2024168266000001_ABST
Patent Text Reader

Abstract

To provide shrink-wrapped blasting charges (filling materials).SOLUTION: A manufacturing method of shrink-wrapped blasting charges (filling material) according to the present invention includes the steps of: longitudinally dividing a long, deformable rod-shaped clay body having a diameter that can be inserted into a blasting hole; forming short rod-shaped filling material into short pieces, which are transported while being arranged at predetermined intervals along their longitudinal direction on a heat-shrinkable soft synthetic resin film 4 transported by a belt conveyor 3; forming a pre-packaged body 10 in which the short rod-shaped filling material is stored within a tubular film, preferably in a degassable manner by using a pillow packaging machine or the like, between adjacent rod-shaped filling materials transported at a predetermined speed; and heating the pre-packaged body to shrink the tubular film while degassing, thereby sealing the short rod-shaped filling material within the pre-packaged body.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a shrink-wrapped filling material, which is a soft solid blasting charge (filling material) package, and is produced by wrapping the material in a heat-shrinkable film and then heat-shrinking the film, and a method for producing the same. [Background technology]

[0002] In general, in civil engineering works such as tunnel construction sites, after the drilling process in which a dedicated tool (bit) is attached to the tip of a long, thin rod and struck and rotated to open about 100 holes about 1 to 2 m deep, as shown in Figure 7(a), explosives are pushed into the drilled holes to a designated position using a long, thin loading rod, and the holes are completely blocked with a soft, solid, clay-like filling (anko) to increase the effect of the explosives when blasting, as shown in Figure 7(b). Since such a loading operation is dangerous, it has recently been done by operating a machine such as an automatic loading machine from a distance, as shown in Figure 8(a), and the filling is passed from a chute through the loading machine to a loading hose, and from there through a loading pipe to block the drilled hole behind the explosives in the drilled hole. Normally, the filling, which is a soft solid, is stored in a polyethylene bag, one by one, to prevent drying during storage. However, as shown in Figure 6, when storing the soft solid filling, it is stored in a wide plastic bag, so there is a lot of space around the filling, and air remains around the filling, which gets caught in various parts of the machine during the automatic loading process, causing problems with automatic operation. In other words, the loading procedure is as follows: first, the parent die (explosive + detonator) is attached to the end of the loading pipe, and air is pumped into the end of the blasting hole. Next, a specified number of additional dies (explosive only) is set using the operation button at hand, and the additional die firing command button is pressed, and the set number of additional dies are pumped and loaded continuously into the hole. Once the loading of all the additional dies is confirmed, the next command to load filling is issued, and a specified number of continuously shaped fillings are pumped through the same loading device, so in the automatic filling process shown in Figure 6, the margins of the packaging film get caught in various parts of the machine, causing problems with automatic operation.

[0003] Since it is difficult to store bar-shaped bean paste, which is a soft solid, tightly packed in a plastic bag, it is stored in a wide plastic bag, which increases the volume by 10% to 15% compared to bare bean paste. Therefore, for automatic loading, there is a demand to wrap it with adhesive tape or the like to make it compact, but this may change the properties of the bare bean paste, and such post-processing is a large cost burden for the production of bean paste, which costs about 10 yen per stick. Summary of the Invention [Problem to be solved by the invention]

[0004] Therefore, it is desirable to provide shrink-wrapped filling that can be sealed without destroying the properties of the soft filling, to prevent the filling from drying out, and that can be packaged in a manner that does not interfere with the automatic loading of the filling as shown in Fig. 8(b). [Means for solving the problem]

[0005] In light of the problems with bean paste packaging, the inventors conducted extensive research and discovered that the technology of shrink-packaging food in a soft, heat-shrinkable film is optimal for mass-producing bean paste that prevents the bare bean paste from drying out while ensuring properties that do not interfere with the filling of the holes in the bean paste, and that does not interfere with automatic loading of the bean paste. The present invention provides shrink-wrapped paste produced based on such a viewpoint, and is characterized in that it is produced by a method comprising the steps of: A) cutting long, deformable rod-shaped clay bodies with a diameter that can be inserted into a blast hole in the longitudinal direction to form short rod-shaped paste (blasting charge); B) transporting the rod-shaped paste while arranging it at predetermined intervals in the longitudinal direction on a heat-shrinkable soft synthetic resin film transported by a belt conveyor; C) forming a pre-packaged body in which short rod-shaped paste is stored in a tubular film, preferably in a degassable manner using a pillow packaging machine or the like, between adjacent rod-shaped paste bodies transported at a predetermined speed; and D) heating the pre-packaged body, shrinking the tubular film while degassing, to seal the short rod-shaped paste in the pre-packaged body. Effect of the Invention

[0006] According to the present invention, the properties of the bare filling material are not substantially changed since the bare filling material is shrink-wrapped with a soft heat-shrinkable film as shown in Figures 4 and 5. Moreover, since the filling material is shrunk and sealed with a soft heat-shrinkable film, the increase in volume due to packaging is kept within 10%, and it is possible to provide a shrink-wrapped filling material that does not interfere with automatic loading by an automatic loading machine.

[0007] In the present invention, the cylindrical film for shrink-wrapping the bean paste may be made of the most popular PET (polyethylene terephthalate), low-cost PO (polyolefin), PS (polystyrene), environmentally friendly films made from sugarcane raw materials, PVC (polyvinyl chloride), PP (polypropylene), PE (polyethylene), and multi-layered films of PE and PP. In particular, films with a maximum shrinkage stress in the width direction of 400 g / mm at 60 to 140°C during the heat shrinking process are suitable. 2 Maximum shrinkage stress in the length direction is 500g / mm 2 It is preferable that the thermal shrinkage rate of the cylindrical film before shrinking is less than 1 / 2 mm, and if the entire circumference in the width direction of the cylindrical film before shrinking is large enough to enclose the maximum circumference in the width direction of the packaged item, the properties of the bare filling material will not be changed by shrink wrapping. The above cylindrical film is selected so that the thermal shrinkage rate does not substantially change the properties of the bare filling material by shrink wrapping and the increase in volume is small.

[0008] That is, in this shrink-wrapping, the film after heat shrinking is soft and appropriate, so there is no possibility of the filling being tightened more than necessary. The shrink-wrapped filling is soft, so there is no risk of it being crushed by the shrink-wrapping, which would reduce the sealing effect of the filling. Therefore, there is no hindrance to the sealing work, as in the case of wrapping each product manually using plastic wrap.

[0009] In the shrink packaging method of the present invention, the filling material to be packaged is rod-shaped, and the filling material is arranged so that its long dimension is parallel to or perpendicular to the length direction of the tubular film, and the filling material of the packaged material is contained within the soft tubular film. [Brief description of the drawings]

[0010] [Figure 1] 1 is a perspective view showing a first embodiment of a shrink packaging method according to the present invention; [Diagram 2] FIG. 2 is a perspective view showing a second embodiment of the shrink packaging method of the present invention. [Diagram 3] FIG. 11 is a perspective view showing a third embodiment of the shrink packaging method of the present invention. [Figure 4] 1 is a photograph of an actual bean paste shrink-wrapped by the method of the present invention. [Figure 5(a)] 1 is a schematic diagram of anko shrink-wrapped by the method of the present invention (a). [Figure 5(b)] FIG. 2 is a cross-sectional view along line AA of a schematic diagram of an paste shrink-wrapped by the method of the present invention. [Figure 6] This is a photo of the traditional bean paste packaging. [Figure 7(a)] Schematic diagram showing the drilling process inside the tunnel (a). [Figure 7(b)] Schematic diagram (b) showing the process of loading explosives and filling material inside the tunnel. [Figure 8(a)] 1 is a schematic diagram showing an entire automatic loading device. [Figure 8(b)] FIG. 2 is an enlarged view of the automatic loading process of explosives and filling material in a schematic diagram showing the entire automatic loading device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] The shrink packaging method of the present invention is characterized in that, when forming a preliminary package, one open end of the tubular film to be used for packaging is folded under the packaged item or pushed inward without being hermetically sealed, and the other open end is hermetically sealed or similarly folded under the packaged item and heat shrunk in an unsealed state. When sealing all four sides, providing ventilation holes helps to reduce residual air and tightly seal the film to the bare filling.

[0012] FIG. 1 shows a schematic diagram of the process of one embodiment of the shrink packaging method of the present invention. In the figure, 1 is a blasting charge (anko), which is formed into a soft, deformable, long, rod-shaped solid by adding the required additives such as antistatic agents to clay, and is cut to a predetermined length by a cutter 2 and sent onto a belt conveyor 3. 4 is a roll of heat-shrinkable synthetic resin film, in which a sheet of film is folded back to back into a cylindrical shape by a folding machine 5, and the cut short anko 1 is folded into this one by one, and in the figure, the upper part is sealed by a sealing machine 6, pressed by a pressing machine 7, cut to a predetermined length by a cutting machine 8, forming an anko pre-package 10, and heated by a shrink heater 9 to shrink package it. This is called pillow packaging because it resembles a pillow. Although FIG. 1 shows a horizontal pillow packaging machine, it is also possible to move the film vertically to form a vertical bag and store it. In addition, the shrink packaging methods shown in FIG. 2 and FIG. 3 can also be applied. FIG. 2 shows an L-shaped three-sided packaging machine that uses a folded original roll film (half-folded film) 4', melts the three sides of the film except the fold with an L-shaped seal 11, forms a prepackage 10 with a U-shaped seal line, and shrinks it with a shrink heater 9. Although it is a medium-to-low speed machine, it has the characteristic that the packaging dimensions of the prepackage 10' with one side open can be easily changed. On the other hand, FIG. 3 shows a pillow-shaped three-sided packaging machine that uses a flat original roll film 4'' and wraps it like a pillow seam with a lower center seal 11', melts the film with a pair of upper and lower front and rear seals 12, 12, seals the film in an H shape (three sides), forms a prepackage 10, and shrinks it with a shrink heater 9, and has the characteristic that it can wrap items of a certain size at high speed. The same members as in FIG. 1 are given the same numbers, and detailed explanations are omitted.

[0013] The film to be formed into such a cylindrical shape is not limited as long as it has heat shrinkability. Examples of such films include the most popular PET (polyethylene terephthalate), low-cost PO (polyolefin), PS (polystyrene), environmentally friendly films made from sugarcane raw materials, PVC (polyvinyl chloride), PP (polypropylene), PE (polyethylene), and multi-layered films of PE and PP. These films have a maximum shrinkage stress in the width direction of 400 g / mm at 60 to 140°C using a shrink heater 9. 2 Maximum shrinkage stress in the length direction is 500g / mm 2 It is preferable that the width of the tubular film before shrinking is large enough to enclose the maximum widthwise circumference of the packaged item, and the package can be wrapped without changing the properties of the bare filling.

[0014] In the present invention, as shown in Fig. 1, a long rod-shaped filling material is first cut to a predetermined size to form a bare filling material 1. Next, the filling material is placed at regular intervals on a heat-shrinkable synthetic resin film 4 transported by a belt conveyer 3, and is stored in a cylindrical film 2. If the bare filling material 1 is rod-shaped as in this embodiment, it is placed so that the long direction of the filling material 1 and the length direction of the cylindrical film 2 are parallel to each other.

[0015] The heat-shrinkable synthetic resin film used in the present invention is not particularly limited, and various shrink films used in conventional shrink packaging may be used, but a soft film that does not impair the properties of the padding 1 after shrink packaging is selected. Specifically, polyethylene resin film, polypropylene resin film, ethylene-vinyl acetate copolymer film, crosslinked polyethylene resin film, or multilayer films in which these resin films are laminated, or ethylene-vinyl alcohol copolymer film, multilayer films including an oxygen barrier resin layer such as vinylidene chloride resin, etc. are preferably used.

[0016] In the present invention, when a film having a small shrinkage stress in any direction is used as the heat-shrinkable synthetic resin film, the filling 1 is not tightly compressed when heat-shrinking. Preferably, the maximum shrinkage stress in the width direction at 60 to 140°C is 400 g / mm 2 Maximum shrinkage stress in the length direction is 500g / mm 2 It is preferable to use the following films:

[0017] In addition, the heat shrinkage rate of the film is preferably selected to be 5 to 85% in the width direction and 5 to 85% in the length direction, taking into consideration the physical properties after shrinking. Therefore, a uniaxially stretched film or a biaxially stretched film can be appropriately used as the heat shrinkable synthetic resin film. The heat shrinkage rate is the heat shrinkage rate at 80°C for 4 seconds according to ASTM D2732.

[0018] The tubular film 4 can be appropriately selected from the following: one formed into a tubular shape with no joints by inflation molding or the like during film formation, as shown in Figure 1; one formed by stacking two films and joining each of a pair of opposing side edges to form a tubular shape; one folded in half and the free ends overlapped and joined; one folded in half and a pair of opposing side edges of a film folded inward and overlapped and joined together;

[0019] When packaging filling material, it may be desirable to position the seam below the filling material 1 to be packaged, or to use a film with no seam.

[0020] In this process, it is sufficient if the tubular film 4 can accommodate the packaged item 1 with ease, and it is preferable to set the width of the tubular film 2 to match the size of the packaged item 1 so that the entire widthwise circumference of the tubular film 2 is 105 to 110% of the widthwise outer circumference of the packaged item 1.

[0021] Next, the open end of the tubular film 4 containing the filling 1 is folded downward to form the preliminary package 10. At this time, both open ends 3 may be folded in, but one open end is usually hermetically sealed. The hermetically sealing can be performed by any suitable method such as conventional heat fusion or adhesion using an adhesive.

[0022] Next, the preliminary packaging body 10 is heated to thermally shrink the tubular film 4 and adhere it to the filling material 1, which is the packaged item, to obtain the shrink-packaged filling material W. There are no particular limitations on the method for heating the preliminary packaging body 10, and hot air, heated steam, infrared rays, etc. can be used.

[0023] In the present invention, at least one open end 3 of the tubular film 2 in the preliminary packaging body 10 is folded under the packaged item 1, and the films are simply in contact with each other but are not sealed. Therefore, the air inside the preliminary packaging body 10 that has expanded once due to heating is discharged to the outside through the contacted portion by the pressure exerted by the contraction of the tubular film 4, and the tubular film 4 comes into contact with the filling 1 of the packaged item. EXAMPLES

[0024] A long stick of bean paste was cut in the longitudinal direction to make a preliminary package 10.

[0025] As a packaging film, a cross-linked biaxially oriented polyolefin multilayer film (heat shrinkage rate: 67% in the longitudinal direction and 70% in the transverse direction at 120°C, maximum shrinkage stress is 110g / mm at 120°C) was used. 2 ) and a commercially available stretch & shrink packaging machine was used as the packaging machine. The bare filling 1 was set so that the entire circumference in the width direction of the film was 105% of the outer circumference, the film was cut so that the length was about 5 cm, and both ends were folded under the bare filling 1 to form a preliminary package 10. The preliminary package was then passed through a shrink heater 9 set at 140°C for 3 seconds to heat shrink the preliminary package, thereby obtaining a shrink-packaged filling W of the present invention.

[0026] The obtained shrink-wrapped filling W does not move inside the package because the film is in moderate contact with the bare filling 1 as shown in Fig. 4, and the properties of the bare filling 1 are not impaired because the bare filling 1 is not constricted by the film. Fig. 5(a) is a schematic perspective view, and (b) is a cross-sectional view.

[0027] According to the shrink packaging method of the present invention, the air inside the film is discharged from the part of the film that is folded under the packaged item, and the film is heat-shrunk well, so that the film can be tightly attached to the packaged item and packaged. Furthermore, even if the packaged item is soft, the packaged product of the present invention produced by this packaging method does not crush the packaged item and does not interfere with sealing of the punched holes.

[0028] Furthermore, in the shrink packaging method of the present invention, the maximum shrinkage stress in the width direction of the tubular film at 60 to 140°C is set to 400 g / mm 2 The maximum shrinkage stress in the length direction is 500g / mm 2 By setting the following, even when packaging soft filling material, the film can be shrink-wrapped to a suitable degree without excessively constricting the product due to film shrinkage. Therefore, according to the present invention, filling material can be shrink-wrapped without being crushed, and a shrink-wrapped filling material for automatic loading can be provided without any problems. (Comparison of loading efficiency and blasting efficiency)

[0029] It has been reported that when a package (Fig. 6) in which the filling material is wrapped in a conventional wrapping film using the remote explosive loading device of Fig. 8(b) is used, the volume ratio increases by 10 to 15% or more, but compared to manual loading, the loading length is shortened by about 30 to 40% for the same material, and the loading time is shortened by about 50%. When the shrink-wrapped filling material of the present invention of Fig. 4 is used, the increase in the volume ratio is 10% or less, preferably 5% or less, and the comparison of loading efficiency and blasting efficiency is as follows. Although the charging length and charging time are not so improved as in the case of Figure 6, there are almost no charging errors, so the total charging time is shortened. Moreover, the packing density is improved and the blasting efficiency is increased, so the amount of powder (Kg / hole) is saved.

Claims

1. A) A process of cutting a deformable rod-shaped clay body with a diameter that can be inserted into a blast hole into a predetermined length in the longitudinal direction to form a short rod-shaped anko (blasting charge); B) conveying the divided rod-shaped paste while arranging it at a predetermined interval on a heat-shrinkable soft synthetic resin film conveyed by a belt conveyer; C) packaging the rod-shaped bean paste conveyed at a predetermined speed in a tubular film using a packaging machine such as a pillow packaging machine to form a pre-packaged body containing the rod-shaped bean paste; D) heating the pre-packaged body to shrink the cylindrical film and seal it tightly against the stick-shaped bean paste, A method for producing shrink-wrapped filling material, comprising shrinking a cylindrical film of a prepackaged body to obtain a short, rod-shaped filling material that is tightly sealed.

2. The method for producing shrink-wrapped filling material according to claim 1, wherein the heat-shrinkable synthetic resin film is one selected from the group consisting of PET (polyethylene terephthalate), PO (polyolefin), PS (polystyrene), environmentally friendly films made from sugar cane raw materials, PVC (polyvinyl chloride), PP (polypropylene), PE (polyethylene), and multi-layered films of PE and PP.

3. When the heat-shrinkable synthetic resin film is heat-shrinked in the heating step (D), the maximum shrinkage stress in the width direction at 60 to 140°C is 400 g / mm 2 The maximum shrinkage stress in the longitudinal direction is 500 g / mm 2 The method for producing shrink-wrapped filling material according to claim 2, which has soft deformability of a rod-shaped filling material, as described below.

4. A shrink-wrapped filling material produced by the shrink wrapping method described in claim 1, which is produced by wrapping a short rod-shaped filling material in a tubular film made of a heat-shrinkable synthetic resin film, heat-shrinking it and sealing it, and which has soft properties and deformability substantially the same as that of bare filling material when subjected to external pressure.

5. The shrink-wrapped filling material according to claim 4, wherein the heat-shrinkable synthetic resin film is one selected from the group consisting of PET (polyethylene terephthalate), PO (polyolefin), PS (polystyrene), environmentally friendly films made from sugarcane raw materials, PVC (polyvinyl chloride), PP (polypropylene), PE (polyethylene), and multi-layered films of PE and PP, and the volume increase rate is within 10%.

Citation Information

Patent Citations

  • Blasting charging product

    JP2015172479A

  • Edged rotating roll

    JP2020138243A

  • Shaped seal bar and knife for sealing and cutting a contoured shape for a flow wrap machine

    US20050262812A1