Oxidation and neutralization treatment method
By recycling detoxification waste liquid as a neutralizing agent, the method addresses the cost limitations of oxidative neutralization in nickel hydrometallurgy by effectively reusing alkaline components, thereby reducing the need for new agents and lowering operational costs.
Patent Information
- Application Number
- JP2023085090
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-24
- Publication Date
- 2024-12-05
AI Technical Summary
The existing oxidative neutralization methods in the nickel hydrometallurgical process are limited in reducing the cost of neutralizing agents, particularly sodium carbonate, due to the loss of carbonate radicals during the production of nickel carbonate, which are not fully reused.
The method involves reusing detoxification waste liquid as a neutralizing agent in the oxidative neutralization treatment, incorporating steps to recycle and reuse alkaline components like sodium hydroxide, sodium carbonate, and sodium hypochlorite generated during the detoxification process, thereby reducing the need for new neutralizing agents.
This approach significantly reduces the consumption and cost of new neutralizing agents by utilizing the alkaline components from detoxification waste liquid, enhancing the efficiency and reducing the overall chemical costs.
Smart Images

Figure 2024168416000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an oxidation neutralization treatment method, and more particularly to a method for producing a neutralized precipitate by adding an oxidizing agent and a neutralizing agent to water to be treated, such as an aqueous nickel chloride solution. [Background technology]
[0002] In the nickel hydrometallurgical process, nickel sulfide is leached with chlorine, impurities are removed from the resulting nickel chloride aqueous solution, and electrolytic nickel is recovered by electrowinning. The oxidation neutralization method is known as a method for removing impurities from nickel chloride aqueous solution.
[0003] The oxidation neutralization process requires an oxidizing agent and a neutralizing agent, and the cost of these chemicals accounts for the majority of the operating costs. In particular, when nickel carbonate is used as a neutralizing agent in the oxidation neutralization process carried out in the nickel hydrometallurgical process, nickel carbonate is produced using purchased sodium carbonate as a carbonating agent, so the more nickel carbonate is consumed, the higher the chemical cost becomes.
[0004] Regarding this point, Patent Document 1 discloses the production of nickel carbonate using the aqueous sodium carbonate solution obtained in the in-system neutralization detoxification step. This makes it possible to produce the amount of nickel carbonate required for the oxidation neutralization treatment while reducing the amount of purchased sodium carbonate used, thereby reducing chemical costs. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2005-248245 A Summary of the Invention [Problem to be solved by the invention]
[0006] However, in the method disclosed in Patent Document 1, since sodium carbonate is reacted with an aqueous solution of nickel chloride in the production of nickel carbonate, a considerable amount of sodium carbonate is lost, including the amount that contributes to an increase in pH. Therefore, not all of the carbonate radicals of the sodium carbonate obtained in the neutralization detoxification step can be reused as nickel carbonate used as a neutralizing agent in the oxidation neutralization treatment, and there is a limit to the effect of reducing chemical costs. Therefore, there is a demand for further reducing the cost required for the neutralizing agent in the oxidation neutralization treatment.
[0007] In view of the above circumstances, an object of the present invention is to provide an oxidation neutralization treatment method capable of reducing the cost required for a neutralizing agent. [Means for solving the problem]
[0008] The first embodiment of the oxidation neutralization treatment method comprises an oxidation neutralization step of adding an oxidizing agent and a neutralizing agent to the water to be treated in a reaction tank to produce a neutralized precipitate by an oxidation neutralization reaction, and a detoxification step of contacting exhaust gas with an aqueous sodium hydroxide solution to discharge a detoxification waste liquid containing unreacted sodium hydroxide, and is characterized in that the detoxification waste liquid is supplied to the reaction tank as part of the neutralizing agent. The oxidation neutralization treatment method of the second aspect is characterized in that, in the first aspect, the remainder of the neutralizing agent is carbonate, the exhaust gas includes annular gas of the reaction tank containing carbon dioxide generated in the oxidation neutralization process, and the detoxification waste liquid includes sodium carbonate produced in the detoxification process. The oxidation neutralization treatment method of the third aspect is characterized in that, in the first or second aspect, the oxidant is chlorine gas, the exhaust gas contains collected gas from the reaction tank containing unreacted chlorine gas in the oxidation neutralization process, and the detoxification waste liquid contains sodium hypochlorite produced in the detoxification process. The oxidation neutralization treatment method of a fourth aspect is characterized in that, in any one of the first to third aspects, the water to be treated is an aqueous nickel chloride solution or an aqueous cobalt chloride solution. Effect of the Invention
[0009] According to the present invention, the detoxification waste liquid is reused as a neutralizing agent in the oxidation neutralization process, so that the consumption of new neutralizing agent can be reduced, and the cost required for the neutralizing agent can be suppressed. Moreover, since the detoxification waste liquid is supplied to the reaction tank as it is, all of the alkaline components contained in the detoxification waste liquid can be used as a neutralizing agent. Therefore, the cost required for the neutralizing agent can be further reduced compared to the case where nickel carbonate is produced using the detoxification waste liquid. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is an overall flow diagram of a nickel hydrometallurgical process. [Diagram 2] FIG. 2 is an explanatory diagram of an oxidation neutralization treatment facility in the first embodiment. [Diagram 3] FIG. 11 is an explanatory diagram of an oxidation neutralization treatment facility in a second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Next, an embodiment of the present invention will be described with reference to the drawings. [First embodiment] The oxidation neutralization treatment method according to the first embodiment of the present invention is a method for producing a neutralized precipitate by adding an oxidizing agent and a neutralizing agent to water to be treated. For example, impurities contained in the water to be treated are removed by the oxidation neutralization method.
[0012] Examples of the water to be treated include an aqueous solution of nickel chloride and an aqueous solution of cobalt chloride. The water to be treated may contain impurities. Examples of impurities contained in the aqueous solution of nickel chloride include iron, lead, manganese, and cobalt. Examples of impurities contained in the aqueous solution of cobalt chloride include iron, lead, and manganese. The water to be treated is subjected to an oxidation neutralization treatment to remove impurities. However, impurities that cannot be completely removed may remain in the water to be treated after the treatment.
[0013] The oxidation neutralization treatment method of this embodiment is preferably applied to the deironization step and the deleading step of the nickel hydrometallurgical smelting process described below. Therefore, the following description will be given taking as an example the treatment of an aqueous nickel chloride solution in the deironization step and the deleading step. However, the oxidation neutralization treatment method of this embodiment is not limited to the deironization step and the deleading step, and may be applied to any process step. Furthermore, the water to be treated is not limited to an aqueous nickel chloride solution.
[0014] As shown in Figure 1, in the nickel hydrometallurgical process, the raw material nickel sulfide is first treated in the leaching process to obtain leachate. Nickel matte and nickel-cobalt mixed sulfide can be used as nickel sulfide.
[0015] The leaching process includes a chlorine leaching process and a cementation process. In the chlorine leaching process, the metals contained in the solid matter in the raw slurry are substantially all leached into the liquid by the oxidizing power of the chlorine gas blown into the leaching tank. In the cementation process, the chlorine leaching solution is brought into contact with nickel sulfide, preferably nickel matte, to carry out a substitution reaction between copper and nickel. As a result, for example, nickel in the nickel matte is leached into the liquid, and copper ions in the liquid are precipitated in the form of copper sulfide or metallic copper. The leaching solution obtained in the leaching process is mainly composed of an aqueous nickel chloride solution, and contains impurities such as copper, iron, and lead in addition to cobalt.
[0016] In the iron removal process, impurities such as iron and arsenic are removed from the leachate (nickel chloride aqueous solution) by oxidation neutralization. In this process, an oxidizing agent is applied to the leachate to adjust the redox potential (based on Ag / AgCl electrode, the same applies below) to 400-1,100mV, while a neutralizing agent is added to adjust the pH to 1.5-3. The oxidation neutralization reaction causes impurities such as iron and arsenic contained in the leachate to precipitate as hydroxides or oxides. The precipitate is removed by solid-liquid separation, resulting in a deironized final solution from which impurities have been removed.
[0017] In the solvent extraction process, the cobalt contained in the iron-removal final solution is separated by solvent extraction to obtain a crude nickel chloride aqueous solution and a crude cobalt chloride aqueous solution. The nickel concentration in the crude nickel chloride aqueous solution is 160 to 200 g / L. The crude nickel chloride aqueous solution also contains impurities such as lead, manganese, cobalt, and zinc. The cobalt contained in the iron-removal final solution is extracted into the organic solvent and selectively separated from the nickel chloride in the iron-removal final solution, but a very small amount of cobalt still remains in the extraction residue (crude nickel chloride aqueous solution).
[0018] The crude cobalt chloride aqueous solution is purified in a purification process to remove impurities, and the resulting high-purity cobalt chloride aqueous solution is sent to the cobalt electrolysis process, where electrolytic cobalt is produced by electrowinning.
[0019] In the deleading process, impurities are removed from the crude nickel chloride aqueous solution to produce a high-purity nickel chloride aqueous solution. In the deleading process, an oxidizing agent is applied to the crude nickel chloride aqueous solution to adjust the redox potential to 600-1,200 mV, while a neutralizing agent is added to adjust the pH to 4-6. Impurities such as lead, manganese, and cobalt contained in the crude nickel chloride aqueous solution are coprecipitated with nickel precipitates by the oxidation-neutralization reaction. A high-purity nickel chloride aqueous solution is obtained by removing the precipitates through solid-liquid separation.
[0020] After the deleading process, other purification processes may be performed as necessary. For example, trace amounts of zinc remaining in the nickel chloride aqueous solution may be removed by adsorption onto an anion exchange resin. The high-purity nickel chloride aqueous solution is sent to the nickel electrolysis process. In the nickel electrolysis process, electrolytic nickel is produced by electrowinning.
[0021] In the iron removal process and lead removal process, an oxidation neutralization treatment facility AA shown in Fig. 2 is used. The oxidation neutralization treatment facility AA has a reaction tank 10 and a detoxification tower 20. The oxidation neutralization process is carried out in the reaction tank 10, and the detoxification process is carried out in the detoxification tower 20.
[0022] Water to be treated is continuously supplied to the reaction tank 10. In the case of the iron removal process, the water to be treated is the leachate obtained in the leaching process, and in the case of the lead removal process, the water to be treated is the crude nickel chloride aqueous solution obtained in the solvent extraction process. In either case, the water to be treated is an aqueous nickel chloride solution containing impurities. If necessary, the water to be treated may be a diluted solution obtained in the previous process.
[0023] An oxidizing agent and a neutralizing agent are supplied to the reaction tank 10. The oxidizing agent and the neutralizing agent are added to the water to be treated in the reaction tank 10, and a neutralized precipitate is produced by an oxidation neutralization reaction (oxidation neutralization step). The reaction tank 10 is equipped with an agitator 11 for agitating the water to be treated with the oxidizing agent and the neutralizing agent.
[0024] The oxidizing agent is not particularly limited as long as it can increase the redox potential of the nickel chloride aqueous solution, but chlorine gas, which does not increase impurities, is preferable. Nickel carbonate, sodium carbonate, calcium carbonate, nickel hydroxide, sodium hydroxide, calcium hydroxide, etc. can be used as the neutralizing agent. Among these, nickel carbonate and nickel hydroxide are preferable because they do not increase impurities in the nickel chloride aqueous solution.
[0025] The amount of oxidizing agent added is adjusted so that the redox potential of the water to be treated falls within a range suitable for oxidation neutralization treatment. The redox potential suitable for the iron removal process is 400 to 1,100 mV, and the redox potential suitable for the lead removal process is 600 to 1,200 mV. The amount of neutralizing agent added is adjusted so that the pH of the water to be treated falls within a range suitable for oxidation neutralization treatment. The pH suitable for the iron removal process is 1.5 to 3, and the pH suitable for the lead removal process is 4 to 6.
[0026] The slurry containing the neutralized precipitate is continuously discharged from the reaction tank 10. The slurry is separated into a post-treatment liquid and a neutralized precipitate. The post-treatment liquid is a final deironization liquid in the case of the deironization process, and is a high-purity nickel chloride aqueous solution in the case of the deleading process.
[0027] The oxidation neutralization treatment equipment AA may have a plurality of reaction tanks 10. A plurality of reaction tanks 10 may be connected in series to perform the oxidation neutralization treatment in stages. In this case, the liquid to be treated is continuously supplied to the most upstream reaction tank 10 and flows in sequence to the downstream reaction tanks 10.
[0028] Chlorine gas supplied as an oxidizing agent is absorbed by the water to be treated, and almost the entire amount contributes to the oxidation neutralization reaction. Nevertheless, in order to prevent chlorine gas, which is a toxic gas, from leaking outside the reaction tank 10, a circular collection pipe 12 is connected to the gas phase of the reaction tank 10, and the inside of the reaction tank 10 is kept at negative pressure by an induced draft fan. The gas drawn by the induced draft fan (hereinafter referred to as "circular collection gas") is sent to the detoxification tower 20 through the circular collection pipe 12.
[0029] In the iron removal process and lead removal process, the pH of the water to be treated is in the acidic range, and carbonate ions are difficult to dissolve in the liquid. Therefore, when carbonates such as nickel carbonate, sodium carbonate, and calcium carbonate are used as neutralizing agents, the carbonate ions dissolved in the liquid become carbon dioxide and are distributed in the gas phase. The generated carbon dioxide is discharged as a reflux gas and sent to the detoxification tower 20.
[0030] A packing layer 21 filled with packing materials is formed in the middle of the detoxification tower 20. A nozzle 22 is disposed above the packing layer 21, and an absorbing liquid consisting of an aqueous sodium hydroxide solution is sprayed from the nozzle 22. The sprayed absorbing liquid flows down along the surface of the packing materials and is then temporarily stored in the bottom of the detoxification tower 20.
[0031] A supply pipe 23 for exhaust gas to be detoxified is connected to the side wall of the detoxification tower 20 below the packing layer 21. The exhaust gas introduced into the detoxification tower 20 rises toward the top of the tower and comes into countercurrent gas-liquid contact with the absorbing liquid while passing through the packing layer 21. By contacting the exhaust gas with the absorbing liquid consisting of an aqueous sodium hydroxide solution, harmful components contained in the exhaust gas are captured by the absorbing liquid (detoxification process). The exhaust gas detoxified in this manner is released into the atmosphere from the top of the detoxification tower 20.
[0032] The absorbing liquid is temporarily stored at the bottom of the detoxification tower 20, and then discharged as abatement waste liquid. The absorbing liquid stored at the bottom of the detoxification tower 20 may be returned to the nozzle 22 at the top to circulate the absorbing liquid within the detoxification tower 20. In this case, the sodium hydroxide contained in the absorbing liquid is gradually consumed as the detoxification process progresses. Therefore, a part of the absorbing liquid stored at the bottom of the detoxification tower 20 is discharged as abatement waste liquid, and a supplementary amount of new absorbing liquid is supplied to the detoxification tower 20.
[0033] The collecting gas from the reaction tank 10 is introduced as exhaust gas into the detoxification tower 20. The collecting gas from the reaction tank 10 in the iron removal step and the collecting gas from the reaction tank 10 in the lead removal step may be introduced into separate detoxification towers 20, or may be introduced into the same detoxification tower 20. Exhaust gas generated in other steps of the hydrometallurgical process may also be introduced into the detoxification tower 20.
[0034] In this embodiment, the detoxification waste liquid discharged from the detoxification tower 20 is supplied to the reaction tank 10. The detoxification waste liquid is used as a part of the neutralizing agent in the oxidation neutralization process. Therefore, the neutralizing agent supplied to the reaction tank 10 is partly the detoxification waste liquid, and the remainder is a new neutralizing agent such as nickel carbonate. A part of the sodium hydroxide contained in the absorption liquid is consumed by the detoxification process. In other words, the detoxification waste liquid contains unreacted sodium hydroxide. In particular, in order to reduce the harmful components contained in the exhaust gas to a concentration that is safe and environmentally acceptable, it is necessary to increase the pH of the absorption liquid to about 9 to 11, and in this case, a considerable amount of sodium hydroxide remains in the detoxification waste liquid. By supplying the detoxification waste liquid directly to the reaction tank 10, the sodium hydroxide contained in the detoxification waste liquid can be used as a neutralizing agent in the oxidation neutralization process.
[0035] Furthermore, when carbonate is used as a neutralizing agent in the oxidation neutralization process, carbon dioxide is generated and is contained in the collected gas in the reaction tank 10. When the collected gas containing carbon dioxide is introduced as exhaust gas into the abatement tower 20, the carbon dioxide reacts with sodium hydroxide to generate sodium carbonate. Therefore, the abatement waste liquid also contains sodium carbonate. If such abatement waste liquid is supplied to the reaction tank 10, sodium carbonate can also be used as a neutralizing agent in the oxidation neutralization process.
[0036] In order to capture carbon dioxide in an aqueous sodium hydroxide solution, it is preferable that the pH of the aqueous sodium hydroxide solution is as high as possible. Specifically, the pH of the aqueous sodium hydroxide solution is preferably 9 or higher. However, since increasing the pH increases the amount of sodium hydroxide used to generate the absorbing solution, it is industrially preferable to keep the pH at 11 or lower.
[0037] The chlorine gas supplied to the reaction tank 10 as an oxidizing agent is basically absorbed in almost its entirety by the water to be treated, but a small amount of chlorine gas escapes unreacted into the gas phase of the reaction tank 10. Therefore, the collected gas in the reaction tank 10 contains unreacted chlorine gas. When the collected gas containing chlorine gas is introduced as exhaust gas into the detoxification tower 20, the chlorine gas reacts with sodium hydroxide to produce sodium hypochlorite. Therefore, the detoxification waste liquid also contains sodium hypochlorite. If such a detoxification waste liquid is supplied to the reaction tank 10, sodium hypochlorite can be used as an oxidizing agent for the oxidation neutralization treatment.
[0038] As described above, by reusing the decontamination waste liquid as a neutralizing agent in the oxidation neutralization process, the consumption of new neutralizing agents (nickel carbonate, etc.) can be reduced accordingly. This makes it possible to reduce the cost required for the neutralizing agent. In particular, in this embodiment, the decontamination waste liquid is supplied as is to the reaction tank 10, so that all of the alkaline components (sodium hydroxide, sodium carbonate) contained in the decontamination waste liquid can be used as neutralizing agents. This makes it possible to reduce the cost required for the neutralizing agent compared to the case where nickel carbonate is produced using the decontamination waste liquid.
[0039] In addition, when carbonate is used as a neutralizing agent, carbon dioxide is generated and captured in the absorption liquid. Therefore, when the wastewater from the abatement process is discharged from the system, carbon is also discharged from the system. If the wastewater from the abatement process is reused within the system, the amount of carbon discharged from the system can be reduced accordingly, which contributes to carbon neutrality.
[0040] When a plurality of reaction tanks 10 are connected in series to perform the oxidation neutralization treatment stepwise, the detoxification waste liquid may be supplied to any of the reaction tanks 10. However, since the detoxification waste liquid contains components that do not contribute to neutralization, it is preferable to supply the detoxification waste liquid to the upstream reaction tank 10 in order to ensure a residence time for the neutralization reaction.
[0041] Second Embodiment Next, an oxidation neutralization treatment method according to a second embodiment of the present invention will be described. As shown in Figure 1, the nickel hydrometallurgy process includes a purification process for the crude cobalt chloride aqueous solution. This purification process includes several detailed processes. One of the detailed processes is the thin liquid neutralization process. In the thin liquid neutralization process, the thin liquid generated at each stage of the purification process for the crude cobalt chloride aqueous solution is treated. The thin liquid is a cobalt chloride aqueous solution with a cobalt concentration of 5 to 50 g / L.
[0042] By subjecting the thin liquid to oxidation neutralization treatment, cobalt contained in the thin liquid is recovered as hydroxide. The recovered cobalt hydroxide is repeatedly fed into the system, thereby increasing the cobalt recovery rate. In addition, water is fed into the system as washing water, etc., and the water balance in the system is maintained by discharging the filtrate obtained by solid-liquid separation after oxidation neutralization to the outside of the system. The oxidation neutralization treatment method of this embodiment is applied to this thin liquid neutralization step. Note that the oxidation neutralization treatment is performed not only for the purpose of removing impurities contained in the water to be treated as in the first embodiment, but also for the purpose of recovering a target substance contained in the water to be treated as in this embodiment.
[0043] In the thin liquid neutralization step, an oxidation neutralization treatment equipment BB shown in Fig. 3 is used. The oxidation neutralization treatment equipment BB has a reaction tank 10 and a detoxification tower 20. The water to be treated is continuously supplied to the reaction tank 10. The water to be treated is a thin liquid (aqueous solution of cobalt chloride).
[0044] An oxidizing agent and a neutralizing agent are supplied to the reaction tank 10. The oxidizing agent and the neutralizing agent are added to the water to be treated in the reaction tank 10, and a neutralized precipitate is generated by an oxidation-neutralization reaction (oxidation-neutralization step). Although not particularly limited, chlorine gas is preferably used as the oxidizing agent, and sodium hydroxide is preferably used as the neutralizing agent. The neutralized precipitate contains cobalt hydroxide.
[0045] The slurry containing the neutralized precipitate is continuously discharged from the reaction tank 10. The slurry is separated into a post-treatment liquid and a neutralized precipitate. The neutralized precipitate is repeatedly returned to the system to recover cobalt.
[0046] The oxidation neutralization treatment equipment BB may have a plurality of reaction tanks 10. A plurality of reaction tanks 10 may be connected in series to carry out the oxidation neutralization treatment in stages.
[0047] A sodium hydroxide solution is supplied to the detoxification tower 20 as an absorbing liquid. Gas discharged from various parts of the hydrometallurgical process is also introduced to the detoxification tower 20 as an exhaust gas. The exhaust gas contains, for example, carbon dioxide, chlorine, sulfur dioxide, etc. The exhaust gas may or may not contain the reflux gas from the reaction tank 10.
[0048] The exhaust gas is brought into contact with an absorbing solution made of an aqueous sodium hydroxide solution, so that harmful components contained in the exhaust gas are captured by the absorbing solution (detoxification process). The exhaust gas that has been detoxified in this manner is released into the atmosphere from the top of the detoxification tower 20.
[0049] The absorption liquid is temporarily stored at the bottom of the detoxification tower 20, and then discharged as detoxification waste liquid. This detoxification waste liquid is supplied to the reaction tank 10. The detoxification waste liquid is used as part of the neutralizing agent in the oxidation neutralization process. The detoxification waste liquid contains unreacted sodium hydroxide. By supplying the detoxification waste liquid as it is to the reaction tank 10, the sodium hydroxide contained in the detoxification waste liquid can be used as the neutralizing agent in the oxidation neutralization process.
[0050] When the exhaust gas introduced into the detoxification tower 20 contains carbon dioxide, the detoxification waste liquid contains sodium carbonate. This sodium carbonate can also be used as a neutralizing agent in the oxidation neutralization process. When the exhaust gas introduced into the detoxification tower 20 contains chlorine gas, the detoxification waste liquid contains sodium hypochlorite. This sodium hypochlorite can be used as an oxidizing agent in the oxidation neutralization process.
[0051] In this way, the waste liquid from the detoxification process is reused as a neutralizing agent in the oxidation neutralization process, so that the consumption of new neutralizing agent can be reduced, and therefore the cost required for the neutralizing agent can be reduced.
[0052] When a plurality of reaction tanks 10 are connected in series to perform the oxidation neutralization treatment stepwise, the detoxification waste liquid may be supplied to any of the reaction tanks 10. However, since the detoxification waste liquid contains components that do not contribute to neutralization, it is preferable to supply the detoxification waste liquid to the upstream reaction tank 10 in order to ensure a residence time for the neutralization reaction. EXAMPLES
[0053] Example 1 The nickel hydrometallurgical refining process shown in Figure 1 was carried out. In the deleading process, impurities contained in the crude nickel chloride aqueous solution were removed by the oxidation neutralization method using three reactors connected in series. Each reactor had a capacity of 50 m 3 The nickel concentration of the crude nickel chloride aqueous solution supplied to the first tank was 120-125g / L. The flow rate of the crude nickel chloride aqueous solution to the first tank was 2,500-3,000L / min. The nickel content of the neutralized precipitate generated in the deleading process was 56-60%.
[0054] An oxidizing agent and a neutralizing agent were added to the first and second tanks. Only an oxidizing agent was added to the third tank. Chlorine gas was used as the oxidizing agent, and nickel carbonate was used as the neutralizing agent. The amount of nickel carbonate added was adjusted so that the pH of the crude nickel chloride aqueous solution in the first tank was 5.0 to 5.1. In addition, the amount of chlorine gas blown in was adjusted so that the redox potential of the crude nickel chloride aqueous solution in the first tank was 900 to 1,000 mV.
[0055] The collected gas from the first to third reaction tanks was introduced into the detoxification tower. The detoxification waste liquid discharged from the detoxification tower was supplied to the first tank. The alkali concentration (total concentration of sodium hydroxide and sodium carbonate) of the detoxification waste liquid was 1.1 mol / L, and the pH was 9.0 to 9.5. The supply rate of the detoxification waste liquid to the first tank was 8 L / min. As a result, the amount of nickel carbonate used per ton of neutralized precipitate generated in the lead removal process was 2.00 t.
[0056] Comparative Example 1 In Example 1, the detoxification waste liquid discharged from the detoxification tower was not supplied to the reaction tank. As a result, the amount of nickel carbonate used per ton of neutralized sediment produced in the deleading step was 2.06 t.
[0057] From the above, it was confirmed that by supplying the decontamination waste liquid to the reaction tank, the amount of nickel carbonate used per ton of neutralized sediment can be reduced by approximately 3%, from 2.06 t to 2.00 t.
[0058] Example 2 We carried out the operation of the nickel hydrometallurgy process shown in Figure 1. In the thin solution neutralization process, which is included in the purification process of the crude cobalt chloride aqueous solution, cobalt contained in the thin solution was recovered by the oxidation neutralization method using two reaction tanks connected in series. Chlorine gas was used as the oxidizing agent, and sodium hydroxide was used as the neutralizing agent.
[0059] The waste liquid discharged from the detoxification tower was supplied to the first tank. The amount of the waste liquid supplied was set to 5% of the flow rate of the thin liquid supplied to the first tank.
[0060] Comparative Example 2 In Example 2, the detoxification waste liquid discharged from the detoxification tower was not supplied to the reaction tank.
[0061] When the amount of sodium hydroxide newly supplied to the reaction tank was checked, it was confirmed that the amount of sodium hydroxide used in Example 2 was 80% of that in Comparative Example 2. From the above, it was confirmed that the amount of sodium hydroxide used could be reduced by 20% by supplying the detoxification waste liquid to the reaction tank. [Explanation of symbols]
[0062] AA, BB oxidation neutralization treatment equipment 10 Reactor 11 Mixer 12. Ring collection piping 20 Abatement tower 21 Filling layer 22 Nozzle 23 Supply piping
Claims
1. an oxidation / neutralization step of adding an oxidizing agent and a neutralizing agent to the water to be treated in the reaction tank to generate a neutralized precipitate by an oxidation / neutralization reaction; A detoxification step of contacting the exhaust gas with an aqueous sodium hydroxide solution to discharge a detoxification waste liquid containing unreacted sodium hydroxide, The detoxified waste liquid is supplied to the reaction tank as a part of the neutralizing agent. The oxidation and neutralization treatment method according to the present invention is characterized in that
2. the remainder of the neutralizing agent is a carbonate; The exhaust gas includes an exhaust gas from the reaction tank containing carbon dioxide generated in the oxidation neutralization step, The detoxification waste liquid contains sodium carbonate produced in the detoxification process.
2. The method for oxidation and neutralization treatment according to claim 1.
3. the oxidizing agent is chlorine gas; The exhaust gas includes an exhaust gas from the reaction tank containing unreacted chlorine gas in the oxidation neutralization step, The detoxification waste liquid contains sodium hypochlorite produced in the detoxification process.
2. The method for oxidation and neutralization treatment according to claim 1.
4. The water to be treated is an aqueous solution of nickel chloride or cobalt chloride.
4. The method for oxidation and neutralization treatment according to claim 1,
Citation Information
Patent Citations
Method for manufacturing calcium carbonate
JP2002293537A
Process of refining nickel leachate
JP2005248245A
Method for removal of chlorine gas
JP2008110339A
Integrating carbon storage and metal value recovery through selective hydrometallurgy
JP2023553314A
Method for absorbing chlorine from a gas containing chlorine and carbon dioxide
WO2007134717A1