Forming device and forming method

The shaping device and method utilize electromagnets and controlled current application to address uneven pressure issues, achieving precise and wrinkle-free shaping of laminates with complex geometries.

JP2024168442AActive Publication Date: 2024-12-05MITSUBISHI HEAVY IND LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023085135
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-24
Publication Date
2024-12-05
Estimated Expiration
2043-05-24

AI Technical Summary

Technical Problem

Existing methods for shaping laminates with reinforcing fibers struggle to accurately form concave or convex shapes due to uneven pressure distribution, leading to wrinkles and inadequate shaping forces, particularly in regions not initially in contact with the mold.

Method used

A shaping device and method using a mold with electromagnets arranged along the longitudinal direction, a flexible sheet member, and a current supply system to control magnetic forces, allowing selective current application to each electromagnet, shaping the laminate to follow the mold's surface.

Benefits of technology

The solution effectively suppresses wrinkles by controlling magnetic forces to match the mold's shape, ensuring precise and wrinkle-free formation of laminates with complex geometries.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024168442000001_ABST
    Figure 2024168442000001_ABST
Patent Text Reader

Abstract

To suppress defects, such as wrinkles, in a laminate when a laminate is formed by a forming die having a forming surface that includes a curved region.SOLUTION: A forming device 100 has: a forming die 10 having a forming surface 10a that includes a convex surface 13 and a concave surface 14, with multiple electromagnets 16a to 16s arranged; a current supply unit capable of selectively supplying electric current to each of the multiple electromagnets; and a sheet member 20 formed of an elastic material containing a magnetic material, which has flexibility and is arranged in a state where a laminate 200 is sandwiched between it and the forming surface 10a. The plurality of electromagnets are arranged at intervals from a first end 10a1 to a second end 10a2 of the forming surface 10a in the width direction WD, and the current supply unit provides current to the electromagnets, thereby forming the laminate 200, which is positioned between the electromagnet supplied with current and the corresponding area of the sheet member 20, in a shape that conforms to the forming surface 10a.SELECTED DRAWING: Figure 7
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a shaping device and a shaping method for shaping a laminate formed by stacking a plurality of sheet materials containing reinforcing fibers. [Background technology]

[0002] Composite structural members used in aircraft, automobiles, etc. have any cross-sectional shape, and a method for manufacturing them is known in which a laminate made of a plurality of laminated sheet materials containing reinforcing fibers is pressed against a forming mold to form the desired shape (see, for example, Patent Document 1). Patent Documents 1 and 2 disclose a method for forming the laminate into a Z shape by placing the laminate in a forming mold having a Z-shaped cross section and sealing it with a vacuum bag, and reducing the pressure in the space sealed by the vacuum bag.

[0003] Other known shaping methods include a technique in which an upper and lower mold are attracted to each other by magnetic force to shape a laminate placed between the upper and lower molds (see, for example, Patent Document 2), and a technique in which a laminate made of multiple laminated sheet materials containing magnetic reinforcing fibers is pressed against a shaping mold by magnetic force to assist shaping using a vacuum bag (see, for example, Patent Document 3). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] U.S. Pat. No. 1,155,069 [Patent Document 2] U.S. Patent No. 8,268,226 [Patent Document 3] US Patent Application Publication No. 2011 / 0180209 Summary of the Invention [Problem to be solved by the invention]

[0005] However, in Patent Document 1, in the recessed area of ​​the shaping mold, the pressure applied to the laminate by decompressing the space sealed by the vacuum bag is lower than in other areas, making it difficult to faithfully fold the laminate along the shape of the shaping mold. In particular, if the area of ​​the laminate that is not in contact with the shaping mold before decompression by the vacuum bag and is pressed against the shaping mold after decompression by the vacuum bag begins is large, wrinkles may occur in the laminate after shaping.

[0006] In addition, in Patent Document 2, since the entire area of ​​the laminate placed on the lower mold is shaped by the upper mold at the same time, when a concave or convex laminate is shaped, wrinkles may occur in the concave or convex area. In addition, in Patent Document 3, since the magnitude of the shaping force for shaping the laminate depends on the magnetism of the reinforcing fibers in each area of ​​the laminate, wrinkles may occur in the concave or convex area when a concave or convex laminate is shaped because an appropriate shaping force is not generated in the concave or convex area.

[0007] The present disclosure has been made in consideration of the above circumstances, and aims to provide a shaping device and a shaping method that can suppress the problem of wrinkles occurring in a laminate when the laminate is shaped using a shaping mold having a shaping surface that includes at least one curved region that is concave or convex. [Means for solving the problem]

[0008] A shaping device according to one embodiment of the present disclosure is a shaping device that shapes a laminate formed by stacking a plurality of sheet materials containing reinforcing fibers, and includes a shaping mold having a shaping surface that extends along the longitudinal direction and includes at least one curved region that is concave or convex along the width direction, and in which a plurality of electromagnets that generate magnetic force are arranged on the shaping surface, a current supply unit that can selectively supply current to each of the plurality of electromagnets, and a sheet member that is formed of an elastic member containing a magnetic material, is flexible, and is arranged in a state in which the laminate is sandwiched between the shaping surface and the plurality of electromagnets, the plurality of electromagnets are formed to extend in the longitudinal direction, and are arranged at intervals from a first end to a second end of the shaping surface in the width direction, and the current supply unit supplies current to the electromagnets to shape the laminate that is arranged between the electromagnet to which current is supplied and the sheet member in the region corresponding to the electromagnet so as to conform to the shape of the shaping surface.

[0009] A shaping method according to one embodiment of the present disclosure is a shaping method for shaping a laminate obtained by stacking a plurality of sheet materials including reinforcing fibers, the method comprising: a laminate installation step of installing the laminate on a shaping mold having a shaping surface including at least one of a concave-shaped or convex-shaped curved region extending along the longitudinal direction and along the width direction, and having a plurality of electromagnets arranged thereon for generating a magnetic force on the shaping surface; a sheet member installation step of installing a flexible sheet member formed of an elastic member including a magnetic material with the laminate sandwiched between the shaping surface and the electromagnet; and a shaping step of selectively supplying current to each of the plurality of electromagnets, thereby shaping the laminate arranged between the electromagnet to which current is supplied and the sheet member in the region corresponding to the electromagnet so as to conform to the shape of the shaping surface, the plurality of electromagnets being formed to extend in the longitudinal direction and arranged at intervals from the first end to the second end of the shaping surface in the width direction. Effect of the Invention

[0010] According to the present disclosure, it is possible to provide a shaping device and a shaping method that can suppress the problem of wrinkles occurring in a laminate when the laminate is shaped using a shaping mold having a shaping surface that includes at least one curved region that is concave or convex. [Brief description of the drawings]

[0011] [Figure 1] FIG. 2 is a perspective view showing a lower mold and a laminate according to an embodiment of the present disclosure, illustrating the state before the laminate is shaped. [Diagram 2] FIG. 2 is a perspective view showing a lower mold and a laminate according to an embodiment of the present disclosure, illustrating the state after the laminate has been shaped. [Diagram 3] FIG. 2 is a cross-sectional view of the shaping mold near the longitudinal center portion, showing the state before the laminate and sheet member are placed in the shaping mold. [Figure 4] 1 is a cross-sectional view of the shaping mold near the longitudinal center portion thereof, showing the state after the laminate and sheet member have been placed in the shaping mold. FIG. [Diagram 5] FIG. 2 is a block diagram showing a configuration of a current supply unit. [Figure 6] 2 is a flowchart showing a method for shaping a laminate according to the present embodiment. [Figure 7] FIG. 2 is a cross-sectional view of the shaping mold near the longitudinal center portion, showing the state during the shaping process. [Figure 8] FIG. 2 is a cross-sectional view of the shaping mold near the longitudinal center portion, showing the state during the shaping process. [Figure 9] 1 is a cross-sectional view of a shaping mold near the longitudinal center portion, showing the state after the shaping process is completed. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] Hereinafter, a shaping device 100 according to an embodiment of the present disclosure and a shaping method using the same will be described with reference to the drawings. Fig. 1 is a perspective view showing a shaping mold 10 and a laminate 200 according to this embodiment, showing a state before shaping the laminate 200. Fig. 2 is a perspective view showing a shaping mold 10 and a laminate 200 according to this embodiment, showing a state after shaping the laminate 200.

[0013] The shaping device 100 of this embodiment is a device that shapes a laminate 200, which is made by stacking a plurality of sheet materials, along the shape of the shaping surface 10a of the shaping mold 10. As shown in FIG. 1, the laminate 200 before shaping is made by stacking a plurality of sheet-like layers of composite material in a flat shape. The laminate 200 is made by stacking a plurality of sheet-like layers of composite material. The composite material that constitutes the laminate 200 is a sheet-like intermediate molding material that is semi-integrated by attaching a matrix resin to reinforcing fibers.

[0014] 2, the sheet member 20 is a sheet-like member arranged with the laminate 200 sandwiched between the sheet member 20 and the shaping surface 10a of the shaping mold 10. The sheet member 20 is a flexible member formed of an elastic member (e.g., a member formed of a rubber material) containing a magnetic material (e.g., magnetized iron powder). The sheet member 20 is attracted toward the shaping surface 10a by the magnetic force generated by a plurality of electromagnets 16 arranged in the shaping mold 10.

[0015] The reinforcing fibers contained in the composite material are, for example, carbon fibers, glass fibers, aramid fibers, etc. The matrix resin contained in the composite material can be a thermosetting resin or a thermoplastic resin. Examples of the thermosetting matrix resin include epoxy resin, unsaturated polyester, vinyl ester, phenol, cyanate ester, polyimide, etc.

[0016] Examples of thermoplastic matrix resins include polyether ether ketone (PEEK), polyethylene terephthalate (PET), polybutylene terephthalate (PBT), nylon 6 (PA6), nylon 66 (PA66), polyphenylene sulfide (PPS), polyetherimide (PEI), polyether ketone ketone (PEKK), and the like.

[0017] The shaping mold 10 may include a heating mechanism (not shown) capable of heating the matrix resin to a temperature equal to or higher than the softening temperature. By heating the matrix resin to a temperature equal to or higher than the softening temperature using the heating mechanism, the laminate 200 containing the matrix resin can be shaped to conform to the surface shape of the shaping mold 10.

[0018] A flat laminate of a plurality of sheet-like reinforcing fibers (dry fabric) not including a matrix resin may be used as the laminate 200. When using a dry fabric, the laminate 200 shaped according to the surface shape of the shaping mold 10 is placed in a molding die (not shown), and a resin material is injected into the molding die to impregnate the reinforcing fibers and form the laminate 200, which is called an RTM (Resin Transfer Molding) method.

[0019] In the laminate 200 formed by the dry fabric, it is preferable to sprinkle a powdered resin (powder binder) on the surface of each of the multiple dry fabric layers to temporarily bond adjacent dry fabrics together. As the powder binder, a thermosetting resin or a thermoplastic resin can be used.

[0020] The shaping device 100 shown in Figures 1 and 2 is arranged in a three-dimensional space. The X-axis, Y-axis, and Z-axis shown in Figures 1 and 2 are axes that intersect with each other in the three-dimensional space. The X-axis is an axis that extends parallel to the installation surface S on which the shaping mold 10 is installed, and the Z-axis is an axis that extends in a direction perpendicular to the installation surface S on which the shaping mold 10 is installed. The Y-axis is an axis that is perpendicular to both the X-axis and the Z-axis.

[0021] The shaping mold 10 is a block-shaped mold having a shaping surface 10a for shaping the laminate 200, and is formed of, for example, a metal material. The shaping mold 10 has, as the shaping surface 10a for shaping the laminate 200, an upper surface 11, a side surface 12, a convex surface (curved region) 13, a concave surface 14 (curved region), and a bottom surface 15.

[0022] Fig. 3 is a cross-sectional view of the shaping mold 10 near the center in the longitudinal direction LD, showing the state before the laminate 200 and the sheet member 20 are placed in the shaping mold 10. Fig. 4 is a cross-sectional view of the shaping mold 10 near the center in the longitudinal direction LD, showing the state after the laminate 200 and the sheet member 20 are placed in the shaping mold 10.

[0023] As shown in Figures 3 and 4, the top surface 11 of the shaping mold 10 is a surface that extends flatly along the X-axis. The side surface 12 of the shaping mold 10 is a surface that extends flatly along the Z-axis. The bottom surface 15 of the shaping mold 10 is a surface that extends flatly along the X-axis.

[0024] Convex surface 13 is a surface connecting top surface 11 and side surface 12, and has an arc shape in which the normal direction of the surface gradually changes from a surface along the X axis to a surface along the Z axis as it approaches side surface 12 from top surface 11 along the X axis. Convex surface 13 is a portion that includes a convex shape along the width direction WD parallel to the X axis.

[0025] The concave surface 14 is a surface connecting the side surface 12 and the bottom surface 15, and has an arc shape in which the normal direction of the surface gradually changes from a surface along the Z axis to a surface along the X axis, and then to a surface intersecting the X axis, as it approaches the bottom surface 15 from the side surface 12 along the Z axis. The concave surface 14 is a portion that includes a concave shape along the width direction WD. The top surface 11, the side surface 12, and the bottom surface 15 are non-curved regions in which the change in curvature along the width direction WD is smaller than that of the convex surface 13 and the concave surface 14, respectively.

[0026] The shape of the shaping mold 10 shown in FIG. 3 and FIG. 4 may be other forms. For example, the upper surface 11 may be a surface extending in a direction different from the X-axis. The side surface 12 may be a surface extending in a direction different from the Z-axis. The convex surface 13 may be any convex shape other than a circular arc shape. The concave surface 14 may be any concave shape other than a circular arc shape. The bottom surface 15 may be a surface extending in a direction parallel to the X-axis or in a direction inclined downward from the X-axis. The shaping mold 10 may have a shaping surface 10a that extends along the longitudinal direction LD and includes at least one curved region of a concave shape or a convex shape along the width direction WD.

[0027] As shown in Fig. 3 and Fig. 4, a plurality of electromagnets 16a, 16b, 16c, 16d, 16e, 16f, 16g, 16h, 16i, 16j, 16k, 16l, 16m, 16n, 16o, 16p, 16q, 16r, and 16s (hereinafter also referred to as electromagnets 16) are arranged in the shaping mold 10 so as to form a part of the shaping surface 10a. The plurality of electromagnets 16 generate a magnetic force on the shaping surface 10a by a current supplied from a current supply unit 30. The plurality of electromagnets 16 may be embedded in the vicinity of the shaping surface 10a of the shaping mold 10 without forming a part of the shaping surface 10a.

[0028] Each of the electromagnets 16 is formed to extend along the longitudinal direction LD, and is arranged at intervals from the first end 10a1 to the second end 10a2 of the shaping surface 10a in the width direction WD. The arrangement interval (first arrangement interval) of the electromagnets 16 in the width direction WD on the convex surface 13 and the concave surface 14 (curved regions) is narrower than the arrangement interval (second arrangement interval) of the electromagnets 16 in the width direction WD on the top surface 11, the side surface 12, and the bottom surface 15 (non-curved regions). The arrangement interval is the distance between the center positions of a pair of electromagnets 16 adjacent to each other in the width direction WD on the shaping surface 10a.

[0029] Next, the current supply unit 30 of the shaping apparatus 100 will be described with reference to Fig. 5. Fig. 5 is a block diagram showing the configuration of the current supply unit 30. As shown in Fig. 5, the current supply unit 30 has a power source 31, a relay 32, a breaker 33, a voltage conversion unit 34, and a current control unit 35. The current supply unit 30 is a device capable of selectively supplying current to each of the multiple electromagnets 16.

[0030] The current supply unit 30 selectively supplies current to each of the multiple electromagnets 16, thereby causing the desired electromagnet 16 to generate a magnetic force. The current supply unit 30 supplies current to the desired electromagnet 16, thereby shaping the laminate 200 disposed between the electromagnet 16 to which the current is supplied and the sheet member 20 in the area corresponding to the electromagnet 16, so as to conform to the shape of the shaping surface 10a.

[0031] The current supply unit 30 supplies a voltage from the power source 31 to the voltage conversion unit 34, and supplies the voltage converted by the voltage conversion unit 34 to the current control unit 35. The current control unit 35 selectively applies a voltage to the electromagnets 16, thereby selectively supplying a current to each of the electromagnets 16. When an AC voltage is supplied from the power source 31, the voltage conversion unit 34 converts the AC voltage into a DC voltage. When a DC voltage is supplied from the power source 31, the voltage conversion unit 34 converts the voltage value of the DC voltage into a desired voltage value.

[0032] The relay 32 is a device that switches between a state in which voltage is supplied from the power source 31 to the voltage conversion unit 34 and a state in which it is not supplied. The breaker 33 is a safety device that cuts off the supply of voltage from the power source 31 to the voltage conversion unit 34 when the voltage value supplied from the power source 31 to the voltage conversion unit 34 exceeds a predetermined threshold voltage.

[0033] Next, a method for shaping the laminate 200 of this embodiment will be described with reference to the drawings. Fig. 6 is a flow chart showing the method for shaping the laminate 200 of this embodiment.

[0034] In step S101 (laminate placement step), an operator places the laminate 200 on the shaping mold 10 so as to face the shaping surface 10a of the shaping mold 10. In step S102 (sheet member placement step), the worker places the sheet member 20 in a state in which the laminate 200 is sandwiched between the sheet member 20 and the shaping surface 10a.

[0035] When the hardness of the laminate 200 is relatively low and the shape of the laminate 200 deforms along the shaping surface 10a of the shaping mold 10 due to the weight of the laminate 200 and the sheet member 20, performing steps S101 and S102 results in the state shown in Figure 4.

[0036] In addition, if the hardness of the laminate 200 is relatively high and the shape of the laminate 200 does not deform along the shaping surface 10a of the shaping mold 10 due to the weight of the laminate 200 and the sheet member 20 as shown in Figure 4, a current having a lower current value than the current value supplied to the multiple electromagnets 16 in step S103 may be supplied to all of the multiple electromagnets 16 before performing step S103.

[0037] By supplying current to all of the electromagnets 16 before executing step S103, all of the electromagnets 16 generate magnetic force, and the sheet members 20 arranged in the areas corresponding to the electromagnets 16 are attracted toward the shaping surface 10a. When the sheet members 20 are attracted toward the shaping surface 10a, the laminate 200 is deformed along the shaping surface 10a of the shaping mold 10, and is in the state shown in FIG.

[0038] The current value is set lower than the current value supplied to the multiple electromagnets 16 in step S103 because if the current value supplied to all of the multiple electromagnets 16 were the same as in step S103, the entire area of ​​the sheet member 20 would be attracted toward the shaping surface 10a, and the laminate 200 would deform along the shaping surface 10a in a state where wrinkles would occur in some parts.

[0039] In step S103 (shaping step), the worker operates the current supply unit 30, which selectively supplies current to each of the multiple electromagnets 16, thereby shaping the laminate 200 to conform to the shape of the shaping surface 10a.

[0040] Here, the operation of the current supply unit 30 selectively supplying current to each of the electromagnets 16 in the shaping process will be described with reference to the drawings. Figures 7 and 8 are cross-sectional views of the shaping mold 10 in the vicinity of the center part in the longitudinal direction LD, showing the state during the shaping process. Figure 9 is a cross-sectional view of the shaping mold 10 in the vicinity of the center part in the longitudinal direction LD, showing the state after the shaping process is completed.

[0041] As shown in Figures 7-9, the first end region 200a of the laminate 200 is provided in the region where the electromagnet 16a is provided, and the second end region 200b of the laminate 200 is provided in the region where the electromagnet 16s is provided. The current supply unit 30 gradually shapes the laminate 200 corresponding to each region along a first direction DR1 in the shaping surface 10a from the concave surface 14 to the side surface 12, from the side surface 12 to the convex surface 13, and from the convex surface 13 to the top surface 11. The current supply unit 30 also gradually shapes the laminate 200 corresponding to each region along a second direction DR2 in the shaping surface 10a from the concave surface 14 to the bottom surface 15.

[0042] In step S104, the current control unit 35 of the current supply unit 30 starts supplying current to the electromagnet 16n, which is disposed at the center position (predetermined position) of the width direction WD of the concave surface 14, among the multiple electromagnets 16. The laminate 200, which is disposed between the electromagnet 16n to which current is supplied and the sheet member 20 in the region corresponding to the electromagnet 16n, is shaped to conform to the shape of the shaping surface.

[0043] After starting the supply of current to the electromagnet 16n, the current control unit 35 starts supplying current to the electromagnets 16 in stages from the position where the electromagnet 16n is disposed toward the first end 10a1 and the second end 10a2 of the shaping surface 10a in response to the lapse of a predetermined time (at least one second or more). After the current control unit 35 starts supplying current to a certain electromagnet 16 and a predetermined time (at least one second or more) has elapsed, the current control unit 35 starts supplying current to other adjacent electromagnets 16, and this operation is repeated continuously for the plurality of electromagnets 16.

[0044] 7 shows a state in which the current control unit 35 starts supplying current to the electromagnets 16m and 16o adjacent to the electromagnet 16n in the width direction WD after starting supplying current to the electromagnet 16n. As shown in FIG. 7, the sheet member 20 in the areas corresponding to the electromagnets 16n, 16m, and 16o is attracted to the shaping surface 10a by the magnetic force generated by the electromagnets 16n, 16m, and 16o, and the laminate 200 in the areas corresponding to the electromagnets 16n, 16m, and 16o is shaped along the shape of the concave surface 14.

[0045] After starting the supply of current to the electromagnet 16m, the current control unit 35 starts supplying current to the electromagnet 16l adjacent to the first end 10a1 side of the shaping surface 10a in response to the lapse of a predetermined time. After that, the current control unit 35 starts supplying current to the electromagnets 16k, 16j, and 16i in stages each time the predetermined time elapses.

[0046] Similarly, the current control unit 35 starts supplying current to the electromagnet 16p adjacent to the second end 10a2 side of the shaping surface 10a in response to the lapse of a predetermined time after starting the supply of current to the electromagnet 16o. After that, the current control unit 35 starts supplying current to the electromagnets 16q, 16r, and 16s in stages each time a predetermined time passes, resulting in the state shown in FIG.

[0047] As shown in FIG. 8, the magnetic force generated by the electromagnets 16i-16s attracts the sheet member 20 in the area corresponding to the electromagnets 16i-16s to the shaping surface 10a, and the laminate 200 in the area corresponding to the electromagnets 16i-16s is shaped to conform to the shape of the concave surface 14.

[0048] After starting the supply of current to the electromagnet 16i, the current control unit 35 starts supplying current to the electromagnet 16h adjacent to the first end 10a1 side of the shaping surface 10a in response to the lapse of a predetermined time. After that, the current control unit 35 starts supplying current to the electromagnets 16g, 16f, 16e, 16d, 16c, 16b, and 16a in stages each time the predetermined time elapses, resulting in the state shown in FIG.

[0049] As shown in Figure 9, when the shaping process is completed, the magnetic force generated by the electromagnets 16a-16s attracts the sheet member 20 in the area corresponding to the electromagnets 16a-16s to the shaping surface 10a, and the laminate 200 in the area corresponding to the electromagnets 16a-16s is shaped to conform to the shape of the concave surface 14.

[0050] As described above, in step S103, the current control unit 35 starts supplying current to the electromagnet 16n disposed at the center position of the width direction WD of the concave surface 14, and then starts supplying current in stages from the center position of the width direction WD of the concave surface 14 to the electromagnets 16m, 16l, 16k, 16j, 16i, 16h, 16g, 16f, 16e, 16d, 16c, 16b, and 16a in this order toward the first end portion 10a1. Similarly, the current control unit 35 starts supplying current to the electromagnet 16n disposed at the center position of the width direction WD of the concave surface 14, and then starts supplying current in stages from the center position of the width direction WD of the concave surface 14 to the electromagnets 16o, 16p, 16q, 16r, and 16s in this order toward the second end portion 10a2.

[0051] In step S104 (curing step), the resin material impregnated into the multiple reinforcing fiber sheets of the laminate 200 is cured. If the resin material is thermosetting, the resin material is heated to a curing temperature or higher to cure the resin material. If the resin material is a thermoplastic resin, the resin material is cooled to a temperature lower than the softening temperature to cure the resin material. Through the above steps S101 to S104, a composite material molding method is performed in which the shaping device 100 is used to shape the laminate 200 to form a composite material.

[0052] The actions and effects of the shaping apparatus 100 of the present embodiment described above will be described. According to the shaping device 100 of this embodiment, a shaping mold 10 having a shaping surface 10a including a convex surface 13 and a concave surface 14 along the width direction WD is provided with a plurality of electromagnets 16 that generate a magnetic force on the shaping surface 10a. The plurality of electromagnets 16 are formed to extend in the longitudinal direction LD, and are arranged at intervals from a first end 10a1 to a second end 10a2 of the shaping surface 10a in the width direction WD.

[0053] The current supply unit 30 supplies current to the electromagnets 16 to generate a shaping force that attracts the flexible sheet member 20 containing a magnetic material toward the shaping surface 10a, and shapes the laminate 200 disposed between the electromagnets 16 to which the current is supplied and the sheet member 20 in the area corresponding to the electromagnets 16 to conform to the shape of the shaping surface 10a. Since the current supply unit 30 can selectively supply current to each of the multiple electromagnets 16, the current supply to the multiple electromagnets 16 is started stepwise from the position corresponding to the concave surface 14 in the width direction WD toward the first end 10a1 and the second end 10a2, thereby suppressing the occurrence of wrinkles in the laminate 200 compared to the case where the current supply is started simultaneously to the multiple electromagnets 16.

[0054] According to the shaping device 100 of this embodiment, the first arrangement interval of the multiple electromagnets 16 on the convex surface 13 and the concave surface 14 (curved regions) is narrower than the second arrangement interval of the multiple electromagnets 16 on the top surface 11, the side surface 12 and the bottom surface 15 (non-curved regions), thereby appropriately suppressing the occurrence of wrinkles in the curved regions where the curvature changes greatly.

[0055] Other Embodiments In the above description, the current control unit 35 starts supplying current to the electromagnet 16n disposed at the center position of the width direction WD of the concave surface 14, and then starts supplying current to the electromagnets 16 in stages from the center position of the width direction WD of the concave surface 14 toward the first end 10a1 and the second end 10a2, but other aspects may be used. For example, the current control unit 35 may start supplying current to the electromagnets 16 in stages from the first end 10a1 toward the second end 10a2. In this case, the current control unit 35 starts supplying current in stages to the electromagnets 16a, 16b, 16c, 16d, 16e, 16f, 16g, 16h, 16i, 16j, 16k, 16l, 16m, 16n, 16o, 16p, 16q, 16r, and 16s in this order.

[0056] Also, for example, the current control unit 35 may start supplying current to the electromagnets 16 in a stepwise manner from the second end 10a2 toward the first end 10a1. In this case, the current control unit 35 starts supplying current in a stepwise manner to the electromagnets 16s, 16r, 16q, 16p, 16o, 16n, 16m, 16l, 16k, 16j, 16i, 16h, 16g, 16f, 16e, 16d, 16c, 16b, and 16a in this order.

[0057] In addition, the current control unit 35 may start supplying current to an electromagnet 16 positioned at any position between the first end 10a1 and the second end 10a2, and then gradually start supplying current to the multiple electromagnets 16 toward the first end 10a1 and the second end 10a2.

[0058] The current control unit 35 may supply the same current value to the electromagnets 16a, or may supply different current values. For example, when the thickness of the laminate 200 varies in the width direction WD, the current control unit 35 may increase the current value as the thickness of the laminate 200 increases. That is, the current control unit 35 may control the current value such that the magnetic force with which the electromagnet 16 attracts the sheet member 20 increases as the thickness of the laminate 200 increases.

[0059] Specifically, in step S103 (shaping process), when the first thickness of the laminate 200 arranged in the area corresponding to the first electromagnet 16 is thicker than the second thickness of the laminate 200 arranged in the area corresponding to the second electromagnet 16, the current control unit 35 controls the current supply unit 30 to make the first current value larger than the second current value.

[0060] In the above description, the shaping mold 10 is described as bending the laminate 200 at both the convex surface 13 and the concave surface 14 to shape it into a substantially Z-shape, but other embodiments are also possible. For example, the shaping mold 10 may shape the laminate 200 into a convex shape (L-shape) only by the convex surface 13, the top surface 11 adjacent to the convex surface 13, and the side surface 12, or may shape the laminate 200 into a concave shape (L-shape) only by the concave surface 14, the side surface 12 adjacent to the concave surface 14, and the bottom surface 15.

[0061] The shaping device and the shaping method according to the above-described embodiments can be understood, for example, as follows. The shaping device according to the first aspect of the present disclosure is a shaping device (100) for shaping a laminate (200) formed by stacking a plurality of sheet materials including reinforcing fibers, and includes a shaping mold (10) having a shaping surface (10a) including at least one curved region (13) having a concave or convex shape extending along a longitudinal direction (LD) and along a width direction (WD) and on which a plurality of electromagnets (16) for generating a magnetic force are arranged, a current supply unit (30) capable of selectively supplying a current to each of the plurality of electromagnets, and a shaping member (10) formed by an elastic member including a magnetic material. and a sheet member (20) that is formed to be flexible and is arranged with the laminate sandwiched between the shaping surface, the multiple electromagnets are formed to extend in the longitudinal direction and are arranged at intervals from a first end (10a1) to a second end (10a2) of the shaping surface in the width direction, and the current supply unit supplies current to the electromagnets, thereby shaping the laminate that is arranged between the electromagnet to which current is supplied and the sheet member in the area corresponding to the electromagnet, so that it conforms to the shape of the shaping surface.

[0062] According to the shaping device of the first aspect of the present disclosure, a shaping mold having a shaping surface including at least one of a concave and convex curved region along the width direction is provided with a plurality of electromagnets that generate a magnetic force on the shaping surface. The electromagnets are formed to extend in the longitudinal direction and are spaced apart from each other from a first end to a second end of the shaping surface in the width direction.

[0063] The current supply unit generates a shaping force that attracts the flexible sheet member containing the magnetic material toward the shaping surface by supplying a current to the electromagnet, and shapes the laminate placed between the electromagnet to which the current is supplied and the sheet member in the area corresponding to the electromagnet so as to conform to the shape of the shaping surface. Since the current supply unit can selectively supply current to each of the multiple electromagnets, for example, by gradually starting the supply of current to multiple electromagnets adjacent to each other along the width direction, it is possible to suppress defects such as wrinkles occurring in the laminate compared to the case where the supply of current is started simultaneously to the multiple electromagnets.

[0064] The shaping device according to the second aspect of the present disclosure is the first aspect, further comprising the following configuration: the current supply unit starts supplying current to the electromagnets arranged at predetermined positions in the width direction, and then starts supplying current to the electromagnets in stages from the predetermined position toward the first end and / or the second end. According to the shaping device of the second aspect of the present disclosure, by gradually starting the supply of current to multiple electromagnets from a predetermined position in the width direction toward the first end and / or the second end, it is possible to suppress the defect of wrinkles occurring in the laminate compared to when the supply of current is started to the multiple electromagnets simultaneously.

[0065] The shaping device according to the third aspect of the present disclosure is the second aspect, further comprising the following configuration: the predetermined position is a position corresponding to the curved region (13), and the current supply unit starts supplying current to the electromagnets arranged at the predetermined position, and then starts supplying current to the electromagnets in stages from the predetermined position toward the first end and the second end. According to the shaping device of the third aspect of the present disclosure, by gradually starting the supply of current to the multiple electromagnets from a position corresponding to the curved region in the width direction toward each of the first end and the second end, it is possible to suppress the problem of wrinkles occurring in the laminate compared to when the supply of current is started to the multiple electromagnets simultaneously.

[0066] The shaping device according to the fourth aspect of the present disclosure is the second aspect, and further includes the following configuration: the predetermined position is the first end, and the current supply unit starts supplying current to the electromagnets arranged at the predetermined position, and then starts supplying current to the electromagnets in stages from the predetermined position toward the second end. According to the shaping device of the fourth aspect of the present disclosure, by gradually starting the supply of current to multiple electromagnets from the first end to the second end in the width direction, it is possible to suppress the problem of wrinkles occurring in the laminate compared to when the supply of current is started to the multiple electromagnets simultaneously.

[0067] The shaping device according to a fifth aspect of the present disclosure is any one of the first to fourth aspects, further comprising the following configuration: the shaping surface includes a non-curved region (11, 12, 15) having a smaller change in curvature along the width direction than the curved region, and a first arrangement interval in the width direction of the plurality of electromagnets in the curved region is narrower than a second arrangement interval in the width direction of the plurality of electromagnets in the non-curved region. According to the shaping device of the fifth aspect of the present disclosure, by making the first arrangement spacing of the multiple electromagnets in the curved region narrower than the second arrangement spacing of the multiple electromagnets in the non-curved region, it is possible to appropriately suppress the occurrence of wrinkles in the curved region where the change in curvature is large.

[0068] The shaping device according to a sixth aspect of the present disclosure is any one of the first to fourth aspects, further including the following configuration: That is, the current supply unit makes a first current value supplied to a first electromagnet included in the plurality of electromagnets different from a second current value supplied to a second electromagnet included in the plurality of electromagnets. According to the shaping device of the sixth aspect of the present disclosure, by making the first current value supplied to the first magnet and the second current value supplied to the second magnet different, it is possible to impart a shaping force of an appropriate magnitude according to the thickness to each region of a laminate having different thicknesses, for example.

[0069] The shaping device according to the seventh aspect of the present disclosure is the sixth aspect, further comprising the following configuration: That is, the current supply unit makes the first current value larger than the second current value when a first thickness of the laminate arranged in a region corresponding to the first electromagnet is larger than a second thickness of the laminate arranged in a region corresponding to the second electromagnet. According to the shaping device of the seventh aspect of the present disclosure, when the first thickness of the laminate arranged in the area corresponding to the first electromagnet is thicker than the second thickness of the laminate arranged in the area corresponding to the second electromagnet, the first current value can be made greater than the second current value, and the shaping force generated by the first electromagnet can be made greater than the shaping force generated by the second electromagnet.

[0070] A shaping method according to an eighth aspect of the present disclosure is a shaping method for shaping a laminate obtained by stacking a plurality of sheet materials containing reinforcing fibers, and includes a laminate installation step (S101) for installing the laminate in a shaping mold having a shaping surface including at least one of a concave-shaped or convex-shaped curved region extending along the longitudinal direction and along the width direction and having a plurality of electromagnets arranged thereon for generating magnetic force on the shaping surface, a sheet member installation step (S102) for installing a flexible sheet member formed of an elastic member including a magnetic material with the laminate sandwiched between the shaping surface and the electromagnet, and a shaping step (S103) for selectively supplying current to each of the plurality of electromagnets, thereby shaping the laminate arranged between the electromagnet to which current is supplied and the sheet member in the region corresponding to the electromagnet so as to conform to the shape of the shaping surface, and the plurality of electromagnets are formed to extend in the longitudinal direction and are arranged at intervals from a first end to a second end of the shaping surface in the width direction.

[0071] According to the shaping method of the eighth aspect of the present disclosure, a shaping mold having a shaping surface including at least one of a concave and convex curved region along the width direction is provided with a plurality of electromagnets that generate a magnetic force on the shaping surface. The electromagnets are formed to extend in the longitudinal direction and are spaced apart from each other from a first end to a second end of the shaping surface in the width direction.

[0072] In the shaping process, a shaping force is generated that attracts a flexible sheet member containing a magnetic material toward the shaping surface by selectively supplying a current to each of the electromagnets, and the laminate disposed between the electromagnets to which the current is supplied and the sheet member in the area corresponding to the electromagnet is shaped to conform to the shape of the shaping surface. For example, by gradually starting the supply of current to the electromagnets adjacent in the width direction, the problem of wrinkles occurring in the laminate can be suppressed compared to the case where the supply of current is started simultaneously to the electromagnets.

[0073] The shaping method according to a ninth aspect of the present disclosure is the eighth aspect, further comprising the following configuration: In other words, the shaping step starts supplying current to the electromagnets arranged at predetermined positions in the width direction, and then starts supplying current to the electromagnets in stages from the predetermined positions toward the first end or the second end. According to the shaping method of the ninth aspect of the present disclosure, by gradually starting the supply of current to multiple electromagnets from a predetermined position in the width direction toward the first end or the second end, it is possible to suppress the problem of wrinkles occurring in the laminate compared to when the supply of current is started to the multiple electromagnets simultaneously.

[0074] The shaping method according to a tenth aspect of the present disclosure is the ninth aspect, further comprising the following configuration: the predetermined position is a position corresponding to the curved region, and the shaping step starts supplying current to the electromagnets arranged at the predetermined position, and then starts supplying current to the electromagnets in stages from the predetermined position toward the first end and the second end. According to the shaping method of the tenth aspect of the present disclosure, by gradually starting the supply of current to multiple electromagnets from a position corresponding to the curved region in the width direction toward each of the first end and the second end, it is possible to suppress the defect of wrinkles occurring in the laminate compared to when the supply of current is started to the multiple electromagnets simultaneously.

[0075] The shaping method according to an eleventh aspect of the present disclosure is the ninth aspect, further comprising the following configuration: the predetermined position is the first end, and the shaping step starts supplying current to the electromagnets arranged at the predetermined position, and then starts supplying current to the electromagnets in stages from the predetermined position toward the second end. According to the shaping method of the eleventh aspect of the present disclosure, by gradually starting the supply of current to multiple electromagnets from the first end to the second end in the width direction, it is possible to suppress the defect of wrinkles occurring in the laminate compared to when the supply of current is started to the multiple electromagnets simultaneously.

[0076] The shaping method according to a twelfth aspect of the present disclosure is any one of the eighth to eleventh aspects, further comprising the following configuration: the shaping surface includes a non-curved region having a smaller change in curvature along the width direction than the curved region, and a first arrangement interval in the width direction of the plurality of electromagnets in the curved region is narrower than a second arrangement interval in the width direction of the plurality of electromagnets in the non-curved region. According to the shaping method of the twelfth aspect of the present disclosure, by making the first arrangement spacing of the multiple electromagnets in the curved region narrower than the second arrangement spacing of the multiple electromagnets in the non-curved region, it is possible to appropriately suppress the occurrence of wrinkles in the curved region where the change in curvature is large.

[0077] The shaping method according to a thirteenth aspect of the present disclosure is any one of the eighth to eleventh aspects, further including the following configuration: That is, the current supply unit makes a first current value supplied to a first electromagnet included in the plurality of electromagnets different from a second current value supplied to a second electromagnet included in the plurality of electromagnets. According to the shaping method of the thirteenth aspect of the present disclosure, by making the first current value supplied to the first magnet and the second current value supplied to the second magnet different, it is possible to impart a shaping force of an appropriate magnitude according to the thickness to each region of a laminate having different thicknesses, for example.

[0078] The shaping method according to the fourteenth aspect of the present disclosure is the thirteenth aspect, further comprising the following configuration: That is, the current supply unit makes the first current value larger than the second current value when a first thickness of the laminate arranged in a region corresponding to the first electromagnet is larger than a second thickness of the laminate arranged in a region corresponding to the second electromagnet. According to the shaping method of the fourteenth aspect of the present disclosure, when the first thickness of the laminate arranged in the area corresponding to the first electromagnet is thicker than the second thickness of the laminate arranged in the area corresponding to the second electromagnet, the first current value can be made greater than the second current value, and the shaping force generated by the first electromagnet can be made greater than the shaping force generated by the second electromagnet. [Explanation of symbols]

[0079] 10 Shaping mold 10a Shaping surface 10a1 1st end 10a2 2nd end 11 Top surface (non-curved area) 12 Sides (non-curved areas) 13 Convex surface (curved area) 14 Concave surface (curved area) 15 Bottom surface (non-curved area) 16,16a,16b,16c,16d,16e,16f,16g,16h,16i,16j,16k,16l,16m,16n,16o,16p,16q,16r,16s electromagnet 20 Sheet material 30 Current supply section 31 Power supply 32 Relay 33 Breaker 34 Voltage conversion section 35 Current control section 100 Shaping equipment 200 Laminate 200a 1st end area 200b Second end area DR1 1st direction DR2 2nd direction LD Longitudinal WD Width direction

Claims

1. A shaping device for shaping a laminate obtained by stacking a plurality of sheet materials containing reinforcing fibers, A shaping mold having a shaping surface including at least one of a concave and convex curved region extending along the longitudinal direction and along the width direction, and a plurality of electromagnets that generate a magnetic force on the shaping surface are arranged; a current supply unit capable of selectively supplying current to each of the plurality of electromagnets; A sheet member formed of an elastic member containing a magnetic material and having flexibility, the sheet member being disposed in a state in which the laminate is sandwiched between the sheet member and the shaping surface; The electromagnets are formed to extend in the longitudinal direction and are spaced apart from each other from a first end to a second end of the shaping surface in the width direction, The current supply unit supplies current to the electromagnet, thereby shaping the laminate, which is placed between the electromagnet to which current is supplied and the sheet member in the area corresponding to the electromagnet, to conform to the shape of the shaping surface.

2. The shaping device according to claim 1, wherein the current supply unit starts supplying current to the electromagnets arranged at a predetermined position in the width direction, and then starts supplying current to the plurality of electromagnets in stages from the predetermined position toward the first end and / or the second end.

3. the predetermined position is a position corresponding to the curved region, The shaping device according to claim 2, wherein the current supply unit starts supplying current to the electromagnets arranged at the predetermined position, and then starts supplying current to the plurality of electromagnets in stages from the predetermined position toward the first end and the second end.

4. the predetermined position is the first end, The shaping device according to claim 2 , wherein the current supply unit starts supplying current to the electromagnets arranged at the predetermined position, and then starts supplying current to the plurality of electromagnets in stages from the predetermined position toward the second end.

5. The shaping surface includes a non-curved region having a smaller change in curvature along the width direction than the curved region, The shaping device according to claim 1 , wherein a first arrangement interval in the width direction of the plurality of electromagnets in the curved region is narrower than a second arrangement interval in the width direction of the plurality of electromagnets in the non-curved region.

6. The shaping device according to any one of claims 1 to 4, wherein the current supply unit differentiates a first current value supplied to a first electromagnet included in the plurality of electromagnets from a second current value supplied to a second electromagnet included in the plurality of electromagnets.

7. The shaping device according to claim 6, wherein the current supply unit makes the first current value greater than the second current value when a first thickness of the laminate arranged in an area corresponding to the first electromagnet is greater than a second thickness of the laminate arranged in an area corresponding to the second electromagnet.

8. A method for shaping a laminate obtained by stacking a plurality of sheet materials containing reinforcing fibers, comprising: A laminate installation process in which the laminate is installed in a shaping mold having a shaping surface including at least one of a concave shape or a convex shape extending along the longitudinal direction and along the width direction, and a plurality of electromagnets that generate a magnetic force on the shaping surface are arranged; a sheet member setting process in which a flexible sheet member formed of an elastic member containing a magnetic material is placed in a state in which the laminate is sandwiched between the sheet member and the shaping surface; A shaping process is provided in which a current is selectively supplied to each of the plurality of electromagnets, thereby shaping the laminate disposed between the electromagnets to which a current is supplied and the sheet member in a region corresponding to the electromagnet, so as to conform to the shape of the shaping surface; A shaping method in which the multiple electromagnets are formed to extend in the longitudinal direction and are arranged at intervals from a first end to a second end of the shaping surface in the width direction.

9. The shaping method according to claim 8, wherein the shaping process starts supplying current to the electromagnets arranged at a predetermined position in the width direction, and then starts supplying current to the plurality of electromagnets in stages from the predetermined position toward the first end and / or the second end.

10. the predetermined position is a position corresponding to the curved region, The shaping method according to claim 9, wherein the shaping process starts supplying current to the electromagnets arranged at the predetermined position, and then starts supplying current to the plurality of electromagnets in stages from the predetermined position toward the first end and the second end.

11. the predetermined position is the first end, The shaping method according to claim 9, wherein the shaping process starts supplying current to the electromagnets arranged at the predetermined position, and then starts supplying current to the plurality of electromagnets in stages from the predetermined position toward the second end.

12. The shaping surface includes a non-curved region having a smaller change in curvature along the width direction than the curved region, The shaping method according to any one of claims 8 to 11, wherein a first widthwise arrangement interval of the plurality of electromagnets in the curved region is narrower than a second widthwise arrangement interval of the plurality of electromagnets in the non-curved region.

13. The shaping method according to any one of claims 8 to 11, wherein the shaping process differs between a first current value supplied to a first electromagnet included in the plurality of electromagnets and a second current value supplied to a second electromagnet included in the plurality of electromagnets.

14. The shaping method according to claim 13, wherein the shaping step makes the first current value greater than the second current value when a first thickness of the laminate arranged in a region corresponding to the first electromagnet is greater than a second thickness of the laminate arranged in a region corresponding to the second electromagnet.

Citation Information

Patent Citations

  • Apparatus for manufacturing trimmer used for construction

    JP1991244504A

  • Manufacturing method of preform, and method for manufacturing fiber-reinforced plastic

    JP2016010926A

  • Method for manufacturing fiber-reinforced composite material

    JP2018149750A

  • Molding device and molding method

    JP2022113386A

  • Method and system of forming a composite laminate

    US11155069B2