Joining equipment, nozzle cartridge and joining method

The bonding device and method utilize a nozzle cartridge with biased magnetic nozzles to address thermal deformation and misalignment issues in induction heating, ensuring precise and uniform bonding of components on flexible substrates with varying heights, thereby improving workability and efficiency.

JP2024169818AInactive Publication Date: 2024-12-06WONDER FUTURE
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023086587
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-26
Publication Date
2024-12-06
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing induction heating methods for soldering electronic components on flexible substrates face issues such as thermal deformation of the substrate, misalignment of components, and increased cycle time due to height variations in plastic molded products, leading to reduced reliability and workability.

Method used

A bonding device and method using a nozzle cartridge with biased nozzles containing magnetic material, which applies induction heating through an induction coil to locally heat the conductive connection material, suppressing substrate heating and preventing component displacement, allowing for precise and uniform bonding of components on substrates with varying heights or sizes.

Benefits of technology

The solution effectively suppresses thermal deformation and misalignment, enables simultaneous and precise bonding of components, reduces cycle time, and improves workability by stabilizing the mounting state and enhancing induction heating efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024169818000001_ABST
    Figure 2024169818000001_ABST
Patent Text Reader

Abstract

To provide joining equipment which conductively joins a component to a metal layer formed on a substrate, by means of induction heating, and which suppresses positional deviation and withdrawal of the component to thereby materialize uniform and highly efficient joining of the component, and to provide a nozzle cartridge.SOLUTION: Joining equipment is provided, conductively joining a metal layer 62 formed on a substrate 61 to a component 41, the joining equipment comprises a heating device which performs induction heating on a conductive connection material 51 interposed between the metal layer and the component. The heating device includes an induction coil 31 which has a space portion inside in a planar view and a nozzle cartridge which is disposed in the space portion of the induction coil. The nozzle cartridge includes one or more nozzles 11 including a magnetic substance and a housing in which the nozzles are housed. At least one of the nozzles is energized by energization means 12 in such a manner that a nozzle distal end 111 protrudes from the housing, and the nozzle distal end presses the component toward the metal layer when performing the induction heating on the conductive connection member by applying an AC voltage to the induction coil.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a bonding apparatus that conductively bonds a metal layer formed on a substrate to a component, a nozzle cartridge used in the bonding apparatus that conductively bonds a metal layer formed on a substrate to a component, and a bonding method that conductively bonds a metal layer formed on a substrate to a component. [Background technology]

[0002] As electronic devices become smaller and lighter, flexible substrates are used as substrates on which minute electronic components are mounted. Conventionally, polyimide resin has been used as the resin constituting flexible substrates. However, in order to reduce costs, etc., flexible substrates are being constituted by using polyester-based resins, polyolefin-based resins, etc. instead of polyimide resins.

[0003] When mounting electronic components, the reflow method has been used, in which electronic components and solid solder are placed on a flexible board at room temperature, and then the components are soldered by heating to a temperature at which the solder melts. However, soldering by the reflow method requires that the entire board on which the electronic components are mounted be placed in a reflow oven and heated to a temperature at which the solder melts or higher. The reflow method applies excessive heat to areas other than the area to be soldered, which increases the thermal load on the electronic components and board. This has led to problems such as (i) the reliability of electronic components decreasing due to initial thermal deterioration, and (ii) when polyester resin, polyolefin resin, or the like is used as the resin constituting the flexible board, the melting point of the resin is lower than that of polyimide resin, so the board may be deformed by heating during soldering to mount the electronic components. In order to avoid such problems, the use of special solder that melts at a low temperature has been considered, but this is cost-prohibitive.

[0004] Furthermore, when soldering by the reflow method, if the area of ​​the electrode (copper foil) formed on the flexible board is large and has a large heat capacity, it is necessary to heat it for a long time in the reflow furnace to ensure the soldering. In such cases, there is a risk that initial thermal degradation of the electronic components soldered to the part with the small area of ​​the electrode (copper foil) and low heat capacity may progress, and on the other hand, if the heating time in the reflow furnace is limited, even if the soldering of the part with low heat capacity is reliable, the soldering of the part with high heat capacity may become unstable, which may result in a decrease in reliability in terms of thermal degradation of the electronic components and the electrical and mechanical functions of the soldering.

[0005] To address these problems, a method is known in which induction heating is used to locally heat the parts to be joined for soldering. In the induction heating method, an electronic component and solder are placed on the parts to be joined, a heat-generating member that generates heat by induction heating is brought into contact with the parts to be joined, an AC voltage is applied to an induction coil to generate a magnetic flux, which induces heating of the heat-generating member, and the generated heat is transferred to the solder to melt it.

[0006] Patent Document 1 discloses a circuit board to which electronic components are soldered by electromagnetic induction heating, the circuit board being characterized by comprising a non-heat-resistant sheet, a circuit provided on one side of the non-heat-resistant sheet, a circuit-side terminal provided on the circuit, and a conductive pad provided on the other side of the non-heat-resistant sheet at a position corresponding to the circuit-side terminal. Furthermore, as a mounting method for soldering electronic components to the circuit board, a mounting method is disclosed in which the terminal of the electronic component is opposed to the circuit-side terminal via solder, the conductive pad is heated by the electromagnetic induction heating on the other side of the non-heat-resistant sheet, and the heat generated by the conductive pad is conducted to the solder via the non-heat-resistant sheet and the circuit-side terminal to melt the solder. It is said that these make it possible to provide a soldering technology that can be used even when the metal terminal area is narrow and small.

[0007] Patent Document 2 discloses a soldering device for soldering an electronic component to an electrode formed on a substrate by an IH reflow method, the device comprising a heating means for melting solder interposed between the electrode and the electronic component to solder the electronic component to the electrode, the heating means including a coil having a space inside in a plan view, a plurality of ferrites arranged in the space of the coil, an adjustment mechanism for independently adjusting the distance between each of the ferrites and the electrode formed on the substrate, and a power source for applying an AC voltage to the coil to inductively heat the electrode formed on the substrate, the distance between each of the ferrites and the electrode formed on the substrate being adjusted in advance by the adjustment mechanism so that the temperature of each of the electrodes heated by induction heating is uniform for the plurality of electrodes arranged inside the coil when an AC voltage is applied to the coil. This soldering device is said to be capable of uniformly soldering a plurality of electronic components to the electrodes formed on the substrate at the same time using induction heating. [Prior art documents] [Patent documents]

[0008] [Patent Document 1] International Publication No. 2020 / 250427 [Patent Document 2] JP 2018-148136 A Summary of the Invention [Problem to be solved by the invention]

[0009] The mounting method disclosed in Patent Document 1 is a method of thermally conducting the heat of a heating element heated by induction heating to the electrodes and solder of the substrate in contact with the heating element, and is therefore unsatisfactory in terms of heating efficiency. In addition, the heating element heated by induction heating also heats the vicinity of the electrodes of the substrate in contact with the heating element, which may cause thermal deformation of the substrate. Furthermore, when mounting a minute electronic component on a substrate, the portion to be soldered is small, which may make it difficult to accurately bring the heating element into contact with the solder joint portion on the substrate.

[0010] The bonding device disclosed in Patent Document 2 is capable of suppressing thermal deformation of the board during induction heating and is capable of simultaneously soldering multiple electronic components with good uniformity. However, there was a risk of the electronic components placed on the bonding target becoming misaligned or coming off due to the influence of the magnetic flux generated in the induction coil during induction heating, causing a "chip jump" phenomenon.

[0011] In addition, when multiple metal electrodes (metal terminals) are provided on a plastic molded product made of polyester resin or polyolefin resin, and electronic components are mounted on the multiple metal electrodes (metal terminals) using the IH reflow method, the position of the nozzle (stage position) of the heating device that uses induction heating and the position of the metal electrodes (metal terminals) (work position) must be positioned for each part to be heated so that they meet specified conditions. In this case, due to the height variation that is unique to plastic molded products, it takes time to position them, which increases the cycle time and reduces workability. Furthermore, due to the height variation that is characteristic of plastic molded products, there was a risk of "chip skipping" and variations in the mounting state after IH reflow heating. In particular, with the IH reflow method, the distance between the nozzle tip and the metal electrode (metal terminal) is the biggest factor that affects the induction heating temperature during mounting, so it was necessary to make the heat distribution uniform and mount the components at a stable heating temperature.

[0012] One of the problems that the present invention aims to solve is to provide a bonding device that uses induction heating to conductively bond a component to a metal layer formed on a substrate, which can suppress heating of the substrate, prevent a rise in temperature of the component body and suppress initial thermal degradation, easily conductively bond even small components, suppress misalignment and detachment of components ("chip jump") during induction heating, conductively bond and mount multiple components simultaneously with high uniformity and high precision even when multiple components are placed on the substrate with varying heights or when multiple components of different sizes are placed on the substrate, suppress variations in mounting state due to substrates, reduce cycle time and improve workability, and has high induction heating efficiency.

[0013] One of the problems that the present invention aims to solve is a nozzle cartridge used in a bonding device that conductively bonds a component to a metal layer formed on a substrate using induction heating, the nozzle cartridge having one or more nozzles including a magnetic material and a housing that houses the nozzle, at least one of the nozzles is biased so that a nozzle tip protrudes from the housing, and the nozzle tip presses the component against the metal layer when an AC voltage is applied to the induction coil to inductively heat the conductive connecting material, the nozzle cartridge can suppress heating of the substrate, can prevent a temperature rise in the component body and suppress initial thermal deterioration, can easily conductively bond even minute components, can suppress the phenomenon of component misalignment and detachment ("chip jump") during induction heating, can conductively bond and mount the components simultaneously with high uniformity and high precision even when multiple components are placed on the substrate with height variations or when multiple components of different sizes are placed on the substrate, can suppress variations in mounting state due to substrates, can reduce cycle time and improve workability, and is to provide a nozzle cartridge for use in a bonding device with high induction heating efficiency.

[0014] One of the problems that the present invention aims to solve is to provide a bonding method that utilizes induction heating to conductively bond a component to a metal layer formed on a substrate, which can suppress heating of the substrate, prevent a rise in temperature of the component body and suppress initial thermal degradation, easily conductively bond even small components, suppress misalignment and detachment of components ("chip jump") during induction heating, conductively bond and mount multiple components simultaneously with high uniformity and high precision even when multiple components are placed on the substrate with varying heights or when multiple components of different sizes are placed on the substrate, suppress variations in mounting state due to substrates, reduce cycle time and improve workability, and provide a bonding method with high induction heating efficiency. [Means for solving the problem]

[0015] According to one embodiment of the present invention, a bonding device for conductively bonding a metal layer formed on a substrate and a component includes a heating device that heats a conductive connecting material interposed between the metal layer and the component by induction heating, the heating device having an induction coil having a space inside when viewed in a plane, and a nozzle cartridge that is placed in the space of the induction coil, the nozzle cartridge having one or more nozzles containing a magnetic material and a housing that houses the nozzles, at least one of the nozzles is biased so that a nozzle tip protrudes from the housing, and the nozzle tip presses the components against the metal layer when an AC voltage is applied to the induction coil to inductively heat the conductive connecting material. The substrate is preferably made of an insulating material, and the metal layer preferably has an area that can be locally heated by induction heating. At least one of the nozzles is preferably a nozzle made of a magnetic material or a nozzle made of a magnetic material and having a spacer at the tip thereof. The magnetic material is preferably soft ferrite. The housing is preferably made of a material containing one or more resins selected from the group consisting of polyether ketone-based resins, polyether ether ketone-based resins, polyimide-based resins, polyamide-based resins, polyamideimide-based resins, polyoxymethylene-based resins, polysulfone-based resins, and polysulfide-based resins.

[0016] A nozzle cartridge according to one embodiment of the present invention is used in a bonding device that conductively bonds a metal layer formed on a substrate to a component, and is disposed in a space of an induction coil having a space inside when viewed from above, which is included in a heating device that heats a conductive connecting material interposed between the metal layer and the component by induction heating. The nozzle cartridge has one or more nozzles and a housing that houses the nozzles, at least one of which is a nozzle including a magnetic material, and at least one of the nozzles is biased so that a nozzle tip protrudes from the housing.

[0017] A bonding method according to one embodiment of the present invention is a bonding method for conductively bonding a metal layer formed on a substrate to a component, in which a conductive connecting material interposed between the metal layer and the component is heated by induction heating to conductively bond the metal layer to the component, the induction heating being performed using a heating means having an induction coil having a space inside when viewed in a plane, and a nozzle cartridge placed in the space of the induction coil, the nozzle cartridge having one or more nozzles containing a magnetic material and a housing that houses the nozzles, at least one of the nozzles being biased so that a nozzle tip protrudes from the housing, and the nozzle tip pressing each of the components against the metal layer when an AC voltage is applied to the induction coil to induction heat the conductive connecting material. Effect of the Invention

[0018] According to the present invention, in a bonding device that utilizes induction heating to conductively bond a component to a metal layer formed on a substrate, heating of the substrate can be suppressed, a rise in temperature of the component body can be prevented and initial thermal deterioration can be suppressed, even small components can be conductively bonded easily, and the phenomenon of component misalignment and detachment ("chip jump") during induction heating can be suppressed. Even if multiple components are placed on the substrate with varying heights or multiple components of different sizes are placed on the substrate, they can be conductively bonded and mounted simultaneously with high uniformity and high precision, variations in the mounting state due to the substrate can be suppressed, cycle time can be reduced and workability can be improved, and a bonding device with high induction heating efficiency is provided.

[0019] According to the present invention, there is provided a nozzle cartridge used in a bonding device that utilizes induction heating to conductively bond a component to a metal layer formed on a substrate, the nozzle cartridge having one or more nozzles including a magnetic material and a housing that houses the nozzle, at least one of the nozzles is biased so that a nozzle tip protrudes from the housing, and the nozzle tip presses the component toward the metal layer when an AC voltage is applied to the induction coil to inductively heat the conductive connecting material, the nozzle cartridge can suppress heating of the substrate, can prevent a temperature rise in the component body and suppress initial thermal deterioration, can easily conductively bond even minute components, can suppress the phenomenon of component misalignment and detachment ("chip fly") during induction heating, can conductively bond and mount the components simultaneously with high uniformity and high precision even when multiple components are placed on the substrate with height variations or when multiple components of different sizes are placed on the substrate, can suppress variations in mounting state due to substrates, can reduce cycle time and improve workability, and provides a nozzle cartridge for use in a bonding device with high induction heating efficiency.

[0020] According to the present invention, in a bonding method for conductively bonding a component to a metal layer formed on a substrate using induction heating, it is possible to suppress heating of the substrate, prevent a rise in temperature of the component body and suppress initial thermal deterioration, easily conductively bond even small components, and suppress the phenomenon of component misalignment and separation ("chip jump") during induction heating. Furthermore, even when multiple components are placed on the substrate with height variations or when multiple components of different sizes are placed on the substrate, they can be conductively bonded and mounted simultaneously with high uniformity and high precision, suppressing variations in the mounting state due to the substrate, reducing cycle time and improving workability, and providing a bonding method with high induction heating efficiency.

[0021] The present invention provides a nozzle cartridge for an induction heating device of a bonding device that has two or more nozzles, preferably four or more nozzles, when mounting by an IH reflow method, and can improve workability by the number of nozzles. Furthermore, since it is possible to suppress variations in mounting conditions depending on the board, it is possible to improve repeatability of the mounting conditions, stabilize the quality of boards on which components are mounted, and improve OEE (Overall Equipment Effectiveness; an index used to increase the efficiency of production equipment calculated and determined by the operating rate, performance, and quality, which is the "Overall Equipment Effectiveness" proposed by the Japan Institute of Plant Maintenance). In addition, by using a nozzle cartridge having multiple nozzles whose nozzle tips are biased toward the board by a biasing means during mounting, even if the height positions (Z-axis values) of the tops of multiple components present on the same surface are not uniform, it is possible to suppress the variation in the distance between the nozzle tips and the tops of the components, and it is possible to suppress the variation in the pressing force that presses the components against the board. This makes it possible to perform stable component mounting at a stable induction heating temperature. [Brief description of the drawings]

[0022] [Figure 1]1 is a schematic diagram showing an embodiment of a bonding device of the present invention. [Diagram 2] FIG. 2 is a schematic diagram showing an embodiment of a substrate on which a nozzle cartridge and conductively joined components are mounted in the present invention. [Diagram 3] FIG. 2 is a schematic diagram showing an embodiment of conductive bonding between a substrate (metal layer) and a component using a nozzle cartridge in the present invention. [Figure 4] FIG. 13 is a schematic diagram showing another embodiment of a substrate on which a nozzle cartridge and conductively joined components are mounted in the present invention. [Diagram 5] FIG. 4 is a schematic diagram showing another embodiment of conductively bonding a substrate (metal layer) and a component using a nozzle cartridge in the present invention. [Figure 6] FIG. 13 is a schematic diagram showing another embodiment of a substrate on which a nozzle cartridge and conductively joined components are mounted in the present invention. [Figure 7] FIG. 2 is a schematic diagram showing an embodiment of a nozzle of a nozzle cartridge according to the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0023] The joining device, nozzle cartridge, and joining method according to the present invention will be described in detail below. The joining device, nozzle cartridge and joining method according to the present invention are not limited to the embodiments shown below, and may include various modifications, changes and improvements to the disclosed elements (including elements described in the claims, specification and drawings) within the scope of the present invention and based on the technical idea of ​​the present invention. Also, various combinations, substitutions or selections of the disclosed elements are possible within the scope of the technical idea of ​​the present invention.

[0024] In addition, the drawings disclosed herein are schematic diagrams and are not necessarily strictly illustrated. In addition, in the drawings, the same reference numerals are used for substantially the same configurations, and duplicated descriptions may be omitted or simplified. The disclosed elements in the specification and drawings are provided to enable those skilled in the art to fully understand the present disclosure, and are not intended to limit the subject matter described in the claims.

[0025] [Joining equipment] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, an embodiment of the joining device of the present invention will be described in detail with reference to the drawings as appropriate. FIG. 1 is a schematic diagram showing an embodiment of the bonding apparatus of the present invention. The bonding apparatus 1 shown in Fig. 1 is a bonding apparatus that conductively bonds a component 41 to a metal layer 62 (located below the component 41 and not shown in Fig. 1) formed on a substrate 61 placed on a mounting table 81. The bonding apparatus 1 is equipped with a heating device 71 that inductively heats a conductive connection material 51 (located below the component 41 and not shown in Fig. 1) interposed between the metal layer 62 and the component 41. The conductive connection material 51 is melted and / or thermally cured by the induction heating by the heating device 71, and the component 41 is conductively bonded to the metal layer 62.

[0026] The heating device 71 has an induction coil 31 having a space inside in a plan view, and a nozzle cartridge 10 disposed in the space inside the induction coil 31. The nozzle cartridge 10 includes a nozzle 11 and a housing 21 that houses the nozzle 11. In FIG. 1, a heating device 71 has four nozzles 11 and a nozzle cartridge 10 having a housing 21 for accommodating the nozzles 11, which is disposed in the inner space of an induction coil 31. The nozzle cartridge 10 can accommodate a plurality of nozzles in one housing. The nozzle cartridge 10 may be configured by connecting a plurality of housings 21, each housing containing one nozzle. The connection method is not particularly limited, but may be, for example, a method using an adhesive, a string-like member, a tape-like member, a screw, or the like. When the housings 21, each housing containing one nozzle, are connected so as to be independently movable and configured so that their movements can be controlled by a camera, a sensor, or the like, it is possible to quickly and reliably position the housings 21 on the target on which the conductive bond is to be formed.

[0027] The induction coil 31 may be parallel to the substrate 61 in plan view and have a space inside, and the shape and the like are not particularly limited. The induction coil 31 is connected to a power source 32, and when an AC voltage is applied, a magnetic flux is generated in the space inside the induction coil 31. The shape of the induction coil 31 is approximately U-shaped in FIG. 1, but is not particularly limited as long as it has a space inside in plan view and can generate a magnetic flux in the space inside. The induction coil 31 is disposed at a predetermined distance in a direction perpendicular to the surface of the substrate 61 (metal layer 62 formed on the substrate). The predetermined distance between the induction coil 31 and the surface of the substrate 61 (metal layer 62 formed on the substrate) can be appropriately adjusted according to the position where the magnetic flux is concentrated, and the like. The induction coil 31 is made of, for example, a material with excellent conductivity, such as high-purity aluminum, copper, silver, gold, various alloys, or the like. Since induction coil 31 may generate heat when an AC voltage is applied thereto, induction coil 31 may be formed in a pipe shape so that it can be cooled by circulating a refrigerant inside.

[0028] The nozzle cartridge 10 has one or more nozzles 11 and a housing 21 that houses the nozzles 11, and one or more of the nozzles 11 are nozzles that include a magnetic body, and at least one of the nozzles 11 is biased by a biasing means 12 (not shown in FIG. 1) so that at least the tip of the nozzle 11 protrudes from the housing 21. The nozzle cartridge 10 shown in FIG. 1 has four nozzles 11 (four nozzles x one row). The number of nozzles 11 that the nozzle cartridge 10 has is not particularly limited, and is, for example, two or more, preferably four or more, and is, for example, 50 or less, preferably 20 or less. If the number of nozzles is large, the number of components that can be mounted on a board in one operation increases, but problems may occur in terms of costs, manufacturing of the nozzle cartridge, etc.

[0029] All of the nozzles 11 in the nozzle cartridge 10 may be nozzles containing a magnetic material, or some of the nozzles may be nozzles containing a magnetic material and the rest may be nozzles not containing a magnetic material. At least one of the nozzles 11 may be a nozzle made of a magnetic material. At least one of the nozzles 11 may be a nozzle at least partially made of a magnetic material. For example, such a nozzle may be a nozzle made of a magnetic material and having a spacer at the tip. In addition, for example, a nozzle may be a rod-shaped magnetic material having a part of the side surface covered with a non-magnetic material such as resin, and the tip of the rod-shaped magnetic material may be configured to be movable in a direction perpendicular to the surface of the substrate 61.

[0030] The magnetic material contained in the nozzle 11 may have a high magnetic permeability so long as it can transmit the magnetic flux generated inside the induction coil 31 to the metal layer 62 without attenuation. There are no particular limitations on the magnetic material. For example, ferrite can be used, and it is more preferable to use soft ferrite, which is a soft magnetic material mainly composed of iron oxide. Soft ferrite contains an oxide made of metal elements such as iron, nickel, zinc, manganese, and copper, and oxygen, and can exhibit various magnetic properties by changing the composition. Soft ferrite has a high electrical resistance and hardly passes any current, so eddy currents are unlikely to occur in the soft ferrite during induction heating. Therefore, since it is possible to prevent the soft ferrite itself from generating heat during induction heating, it is possible to form the housing of the nozzle cartridge from resin, and even if the nozzle having the soft ferrite is close to the metal layer 62 or the component 41, the influence of heat on the substrate 61 can be reduced.

[0031] The shape of the nozzles 11 and the arrangement of the nozzles 11 in the nozzle cartridge 10 are not particularly limited, and can be changed as appropriate depending on the type, size, arrangement, etc. of the components 41 mounted on the board 61. The length of the nozzle 11 is not particularly limited. For example, it is preferably in the range of 30 to 40 mm. The nozzle 11 is preferably shaped so that it can come as close as possible to the inner diameter surface of the induction coil 31.

[0032] The housing 21 that houses the nozzle 11 is made of an insulating material. For example, the housing 21 can be made of a material containing one or more resins selected from the group consisting of polyetherketone-based resins, polyetheretherketone-based resins, polyimide-based resins, polyamide-based resins, polyamideimide-based resins, polyoxymethylene-based resins, polysulfone-based resins, and polysulfide-based resins.

[0033] At least one of the nozzles 11 is biased by biasing means 12 so that at least a tip 111 of the nozzle 11 protrudes from the housing 21. The biasing means is not particularly limited, and may be a spring member such as a coil spring or a leaf spring, or a member that exerts a biasing force by compression (for example, a foam such as urethane foam or sponge, rubber, or a damper with air or water sealed inside).

[0034] In the bonding apparatus 1, the heating device 71 can be made movable in the X direction, the Y direction, and the Z direction, whereby the positional relationship between the nozzle 11 (nozzle tip portion 111) and the component 41 can be adjusted. Furthermore, in the bonding apparatus 1, the mounting table 81 can be made movable in the X, Y and Z directions, whereby the positional relationship between the nozzle 11 (nozzle tip portion 111) and the component 41 can be adjusted. In the present invention, either or both of the heating device 71 and the mounting table 81 can be made movable. For example, (i) The heating device 71 is movable in the X direction and the Z direction, and the mounting table 81 is movable in the Y direction. (ii) The heating device 71 is movable in the X direction, and the mounting table 81 is movable in the Y direction and the Z direction. (iii) Both the heating device 71 and the mounting table 81 are movable in the X direction, the Y direction, and the Z direction. With the above configuration, the positional relationship between the nozzle 11 (nozzle tip portion 111) and the component 41 can be adjusted.

[0035] There is no particular limitation on the means for moving the heating device 71 and / or the mounting table 81. For example, a moving means such as an actuator (e.g., a robot cylinder, a linear slider, etc.) provided in the heating device 71 or connected to the heating device 71 can be used. Similarly, a moving means such as an actuator provided in the mounting table 81 or connected to the mounting table 81 can be used.

[0036] The substrate 61 placed on the mounting table 81 is not particularly limited as long as it is made of an insulating material. For example, it may be a flexible base material such as a film or sheet or a resin molded product such as a housing made of a resin such as polyester resin, polyamideimide resin, polyimide resin, polyamide resin, polyetheretherketone resin, polysulfone resin, polyphenylene sulfide resin, polyethersulfone resin, fluororesin, ABS resin, polyphenylene oxide resin, acrylic resin, polycarbonate resin, polybutadiene resin, polyurethane resin, polyolefin resin, polyvinyl chloride resin, or polystyrene resin.

[0037] The metal layer 62 is a conductive metal material layer partially laminated on the substrate 61 by pasting, printing, etching, etc., and may be, for example, an electrode in a circuit. Examples of the metal constituting the metal layer 62 include one or more selected from the group consisting of copper, silver, aluminum, gold, nickel, tin, solder, bismuth, zinc, and alloys containing two or more of these metals. In the present invention, the substrate 61 and the metal layer 62 may be integrated into one body, such as a circuit board having a printed circuit formed on its surface, or an interposer having electrode pads formed on both sides. In the present invention, it is preferable that the metal layer 62 has an area that can be locally heated by induction heating. The area of ​​the metal layer 62 can be, for example, 0.25 mm×0.25 mm or more. If it is not possible to increase the area of ​​the metal layer 62, a metal pad for auxiliary heating can be provided adjacent to the metal layer 62 and / or on the surface of the substrate 61 opposite to the surface on which the metal layer 62 is provided.

[0038] There are no particular limitations on the component 41 as long as it can be conductively bonded to the metal layer 62 on the substrate 61. The component 41 is preferably an electronic component having a component body 411 and a component conductive part 412 (e.g., an electrode part / terminal, etc.). Examples of the component 41 include one or more components selected from the group consisting of a capacitor, a resistor, an LED element, a semiconductor element, a sensor element, an LSI, an IC, an inductor, a transistor, a diode, a liquid crystal display element, a piezoelectric element, a resistor, a filter, a quartz oscillator, a quartz oscillator, a connector, a switch, a volume, a relay, and the like.

[0039] The conductive connecting material 51 is not particularly limited as long as it melts or thermosets when heated and can conductively connect the metal layer 62 and the component 41 (component conductive portion 412). For example, it may be one or more types selected from the group consisting of solder, a thermosetting conductive adhesive containing a thermosetting resin and a conductive material, a thermosetting conductive paste containing a thermosetting resin and a conductive material, and the like.

[0040] When conductive bonding is performed using the bonding apparatus 1 shown in FIG. 1, the heating device 71 and / or the substrate 61 move, and the tip of the nozzle 11 presses the component 41 against the biasing force of the biasing means 12 (not shown in FIG. 1), and an AC voltage is applied from the power source 32 to the induction coil 31. A magnetic flux φ is generated in the space inside the induction coil 31 to which the AC voltage is applied. The magnetic flux φ is transmitted through the nozzle 11 (magnetic body 112 in the nozzle 11) of the nozzle cartridge 10 arranged in the space inside the induction coil 31, and is irradiated perpendicularly from the tip 111 of the nozzle 11 to the metal layer 62 formed on the substrate 61. As a result, the metal layer 62 is induction-heated, and the conductive connection material 51 provided between the metal layer 62 and the component 41 (component conductive portion 412) is heated and melted or thermally reacted, so that the metal layer 62 and the component 41 (component conductive portion 412) are conductively bonded to each other.

[0041] Generally, when conductively joining a metal layer formed on a substrate to a component, if the magnetic flux φ generated in the space inside an induction coil to which an AC voltage is applied is irradiated onto the metal layer to induce heating, the component placed on the metal layer may be displaced from its designated position due to the influence of the magnetic flux φ. When conductive bonding is performed with the bonding apparatus of the present invention, the tip 111 of the nozzle 11 is in a state of pressing the component 41 against the biasing force of the biasing means 12. Even when an AC voltage is applied from the power source 32 to the induction coil 31 and a magnetic flux φ is generated in the space inside the induction coil 31, it is possible to prevent the component 41 from being displaced from a predetermined position due to the influence of the magnetic flux φ. This allows stable conductive bonding of the metal layer 62 formed on the substrate 61 and the component 41.

[0042] 1, by arranging one or more nozzles 10 including a magnetic body 112 in the space inside the induction coil 31, the magnetic flux φ generated in the space inside the induction coil 31 can be irradiated so as to be focused on the metal layer 62 on the substrate 61 without being attenuated through the nozzle 10. This makes it possible to efficiently use the magnetic flux φ for induction heating the metal layer 62, and thus makes it possible to efficiently perform conductive bonding.

[0043] In the present invention, by forming the tip portion 111 of the nozzle 11 into a tapered shape, it is possible to concentrate the magnetic flux φ more locally. For example, if the area of ​​the tip 111 of the nozzle 11 arranged opposite a small-area component 41 is larger than the area of ​​the metal layer 62, the magnetic flux φ irradiated from the tip 111 of the nozzle 11 is irradiated to areas other than the metal layer 62. Therefore, if other components 41 or conductive objects are placed near the component 41 or the metal layer 62, they will also be heated by induction heating. For this reason, the area of ​​the end face of the nozzle 11 can be changed according to the size of the metal layer 62 or the component 41. In the present invention, the area of ​​the tip 111 of the nozzle 11 can be similar to the area of ​​each component 41 or each metal layer 62 .

[0044] A magnetic flux φ is irradiated perpendicularly from the tip 111 of the nozzle 11 to the metal layer 62 formed on the substrate 61, and the amount of heat generated in the induction-heated metal layer 62 can be controlled by adjusting the amount of current flowing through the induction coil 31 and the distance D between the nozzle 11 and the metal layer 62 on the substrate 61. When it is difficult to control the amount of heat by the amount of current flowing through the induction coil 31, the amount of heat can be controlled by attaching a spacer 113 to the tip 111 of the nozzle 11, utilizing the property that the amount of heat of the metal layer 62 heated by induction heating attenuates in proportion to the square of the distance D between the nozzle 11 and the metal layer 62 on the substrate 61. In particular, even when a plurality of nozzles 11 are provided inside the induction coil 31 or when the sizes of the components and the areas of the metal layers are different, by attaching the spacer 113 to the tip 111 of the nozzle 11, the temperatures of the metal layers can be made similar when the metal layers 62 are heated by induction heating through each nozzle 11.

[0045] Even when multiple components 41 of different sizes are mounted on a substrate 61, the bonding device 1 of the present invention can simultaneously perform conductive bonding and mounting with high uniformity and precision by adjusting the area of ​​the metal layer 62 according to the size of the components 41, thereby suppressing variations in the mounting state between each substrate. The amount of heat generated by induction heating of the metal layer 62 on which the components 41 are mounted by the magnetic flux φ generated inside the induction coil 31 varies depending on the size of the metal layer 62. When a plurality of components 41 of different types and sizes are placed on the board 61, the bonding device 1 of the present invention can simultaneously perform conductive bonding and mounting with high uniformity and high precision, even if the areas of the metal layers 62 on which the components 41 are mounted are different, because there is little variation in the amount of heat transferred from the induction-heated metal layers 62 to the conductive connecting materials 51.

[0046] The bonding apparatus 1 of the present invention can adjust the area of ​​the tip 111 of the nozzle 11 in accordance with the area of ​​the surface of each metal layer 62 . When the area of ​​the tip 111 of the nozzle 11 changes, the density of the magnetic flux φ irradiated from the tip 111 of the nozzle 11 to each metal layer 62 changes. A metal layer 62 with a large area has a lower resistance value than a metal layer 62 with a small area, and the eddy current generated in the metal layer 62 with a large area is larger than the eddy current generated in the metal layer 62 with a small area, so that the amount of heat applied to each metal layer 62 changes. Taking these factors into consideration, the amount of heat applied to each metal layer 62 can be adjusted so that the temperature of each metal layer 62 that is induction heated is uniform.

[0047] The bonding device 1 of the present invention can limit the area to be subjected to induction heating to the metal layer 62 on which the component 41 is mounted in the space inside the induction coil 31. The metal layer 62, which is the target part of the conductive bonding, is directly heated by induction heating, not by heat conduction from a heating element (such as a soldering iron) or by heating the whole part using a reflow furnace or the like, so the amount of heat applied to the board 61 can be suppressed. As a result, even if the board 61 is made of a material with low heat resistance, thermal deformation can be suppressed. In addition, since it is not necessary to directly contact the heating element with the part to be bonded, even small parts can be easily conductively bonded.

[0048] Even if the type and size of the component 41 are the same, the magnetic flux φ generated inside the induction coil 31 is not necessarily uniform. In the space inside the induction coil 31 in a plan view, the distribution of the generated magnetic flux φ varies. In addition, the distribution of the generated magnetic flux φ changes in the space inside the induction coil 31 in a plan view depending on the shape of the induction coil 31. Furthermore, when the substrate 61 is made of a flexible substrate or a resin molded product, the magnetic flux φ irradiated to the metal layer 62 varies due to warping or bending of the flexible substrate, or warping, bending, or unevenness of the resin molded product. Taking these factors into consideration, by grasping and adjusting the magnetic flux φ irradiated from the nozzle 11 to the metal layer 62, the amount of heat applied to the metal layer 62 can be adjusted, and highly uniform and precise conductive bonding can be performed simultaneously for mounting, thereby suppressing variations in the mounting state between each board.

[0049] The density of the magnetic flux φ generated inside the induction coil 31 can be measured by obtaining a temperature profile by induction heating using a temperature measurement board having a temperature sensor attached to one or more metal layers 62. Depending on the obtained temperature profile, the temperature uniformity of each metal layer 62 heated by induction heating can be improved by adjusting the distance D between each nozzle 11 and the metal layer 62 on the board 61, adjusting the shape of the nozzle tip, etc.

[0050] In the bonding apparatus 1 of the present invention, various nozzle cartridges are prepared in advance in which the distance between each nozzle 11 and the metal layer 62 formed on the substrate 61 is adjusted, and the nozzle cartridges can be configured to be replaceable depending on the type, size, arrangement, etc. of the components 41 to be mounted on the substrate 61.

[0051] FIG. 2 is a schematic diagram showing one embodiment of a substrate on which a nozzle cartridge and conductively joined parts are mounted in the present invention.

[0052] 2, the nozzle cartridge 10 has a housing 21 that houses four nozzles 11. Inside the housing 21, four nozzle / biasing means storage sections 24 that store the nozzles 11 and the biasing means 12 are provided, and further, a housing internal space section 23 that is connected to the nozzle / biasing means storage sections 24 is provided, and the housing internal space section 23 communicates with the outside via a first ventilation port 221 and a second ventilation port 222. By supplying air to the housing internal space 23 from the first ventilation port 221 and / or the second ventilation port 222, heat can be discharged from within the housing 21, particularly within the nozzle / actuating means storage section 24, which is generated by induction heating due to the magnetic flux φ generated from the induction coil 31 when the actuating means is made of metal, and overheating inside the nozzle can be suppressed.

[0053] 2, the substrate on which the component to be conductively bonded is mounted has a configuration in which a component body 411 facing the tip portion 111 of the nozzle 11, a component conductive portion 412, a conductive connecting material 51, a metal layer 62, a substrate 61, and a magnetic member 63 are laminated in this order. The component body 411 and the component conductive portion 412 form the component 41.

[0054] 2, a magnetic member 63 is provided parallel to the substrate 61 at a position opposite to the side where the induction coil 31 is disposed and facing at least a plurality of nozzles 11. This allows the magnetic flux φ generated by the induction coil 31 and irradiated from the nozzle 11 to pass through the substrate 61 and be transmitted to the magnetic member 63, so that the magnetic flux φ generated by the induction coil 31 can be more reliably irradiated to the metal layer 62. As a result, the conductive joining of the component 41 can be more reliably performed. There is no particular limitation on the shape of the magnetic member 63. For example, it may be in the shape of a plate or a rod.

[0055] FIG. 3 is a schematic diagram showing one embodiment of the present invention when a substrate (metal layer) and a component are conductively joined using a nozzle cartridge. 3 has four nozzles 11 and a housing 21 that houses the nozzles 11, and the four nozzles 11 are biased by a biasing means 12 so that nozzle tip portions 111 protrude from the housing 21. When an AC voltage is applied from a power source 32 to the induction coil 31 to inductively heat the conductive connecting material 51, each nozzle tip portion 111 of the four nozzles 11 presses a component 41 against a substrate 61 (metal layer 62). This prevents "component fly-off" of component 41 when the magnetic flux φ generated in the internal space of induction coil 31 to which AC voltage from power source 32 is applied is transmitted through nozzle 11 of nozzle cartridge 10 arranged in the internal space of induction coil 31 and irradiated perpendicularly from tip 111 of nozzle 11 to metal layer 62 formed on substrate 61. Furthermore, the metal layer 62 is induction heated, and the conductive connecting material 51 provided between the metal layer 62 and the component 41 (component conductive portion 412) is heated and melts or undergoes a thermal reaction, thereby conductively joining the metal layer 62 and the component 41 (component conductive portion 412).

[0056] FIG. 4 is a schematic diagram showing another embodiment of a nozzle cartridge and a substrate on which conductively bonded components are mounted in accordance with the present invention, and is a schematic diagram showing an embodiment of a nozzle cartridge 10 having 14 nozzles 11 (7 nozzles x 2 rows), an induction coil 31, a power source 32 for applying an AC voltage to the induction coil 31, and a substrate 61 on which conductively bonded components 41 are mounted.

[0057] In Figure 4, the nozzle cartridge 10 contains 14 nozzles 11 (7 nozzles x 2 rows) in a housing 21, and each nozzle 11 is biased by a biasing means 12 so that the tip of the nozzle 11 protrudes from the housing 21. The tip of each nozzle 11 that is biased by the biasing means 12 and protrudes from the housing 21 is arranged to face a component 41 placed on a metal layer 62 (not shown in FIG. 4) on a substrate 61. The nozzle cartridge 10 is disposed in a space inside an induction coil 31 which has a space inside in a plan view.

[0058] FIG. 5 is a schematic diagram showing one embodiment of the conductive joining of a component 41 and a metal layer 62 (not shown in FIG. 5) on a substrate 61 by induction heating using the nozzle cartridge 10 shown in FIG. 4.

[0059] 5, the nozzle cartridge 10 has 14 nozzles 11 (7 nozzles x 2 rows) and a housing 21 that houses the nozzles 11, and the nozzles 11 are biased by a biasing means 12 so that a nozzle tip 111 (not shown in FIG. 5) protrudes from the housing 21. The tip 111 of the nozzle 11 presses the component 41 against the biasing force of the biasing means 12 against the substrate 61 (metal layer 62) when an AC voltage is applied from a power source 32 to the induction coil 31 to inductively heat the conductive connecting material 51. This prevents "component fly-off" of component 41 when the magnetic flux φ generated in the space inside induction coil 31 to which an AC voltage is applied is transmitted through nozzle 11 of nozzle cartridge 10 arranged in the space inside induction coil 31 and irradiated perpendicularly from tip 111 of nozzle 11 to metal layer 62 formed on substrate 61. Furthermore, the metal layer 62 is induction heated, and the conductive connecting material 51 provided between the metal layer 62 and the component 41 (component conductive portion 412) is heated and melts or undergoes a thermal reaction, thereby conductively joining the metal layer 62 and the component 41 (component conductive portion 412).

[0060] FIG. 6 is another schematic diagram showing another embodiment of a nozzle cartridge and a substrate on which conductively joined components are mounted in accordance with the present invention, in which a nozzle cartridge 10 having seven nozzles 11 (7 nozzles x 1 row) is used instead of the nozzle cartridge 10 having 14 nozzles 11 shown in FIG. 4. It should be noted that the nozzle cartridge 10 may be a nozzle cartridge having any number of nozzles other than the nozzle cartridge 10 shown in FIG. 4 and FIG.

[0061] FIG. 7 is a schematic diagram showing one embodiment of a nozzle included in the nozzle cartridge of the present invention. The nozzle 11 shown in 7A in FIG. 7 is formed entirely of a magnetic material 112, and the tip 111 of the nozzle 11 has a shape tapered toward the substrate 61 (in 7A, the tip is a pyramid with a flat surface). The tip 111 of the nozzle 11 may have a cone shape or a pyramid shape, for example. The tip of the tip 111 may be flat, pointed, or rounded. As described above, the density of the magnetic flux φ irradiated from the tip 111 of the nozzle 11 to each metal layer 62 can be changed depending on the area of ​​the tip 111 of the nozzle 11. For example, when the area of ​​the tip 111 of the nozzle 11 is increased, the density of the magnetic flux φ irradiated from the tip 111 of the nozzle 11 to each metal layer 62 can be increased.

[0062] The nozzle 11 shown in FIG. 7B has a main body formed of a magnetic body 112 and a spacer 113 provided at a tip portion 111 of the nozzle 11 that faces the substrate 61. FIG. 7C is an exploded view of the nozzle 11 shown in FIG. 7B. The shape of the nozzle tip 111 of the spacer 113 facing the substrate is not particularly limited. In 7B and 7C, the shape of the spacer 113 (the shape of the nozzle tip 111) is tapered toward the substrate 61. The spacer 113 is integrated with the magnetic body 112 by means of adhesion, fitting, or the like.

[0063] 7, the nozzle 11 may be provided with a recess or groove for preventing the nozzle from coming off the housing, or a protrusion that functions as a retainer. Also, a notch, a recess, a protrusion, etc. for connecting with the biasing means 12 may be provided at the rear end of the nozzle on the opposite side to the nozzle tip 111.

[0064] [Nozzle cartridge] The nozzle cartridge of the present invention is a nozzle cartridge used in a bonding device that conductively bonds a metal layer formed on a substrate to a component, the nozzle cartridge being disposed in a space of an induction coil having a space inside in a planar view, the induction coil being included in a heating device that induction heats a conductive connecting material interposed between the metal layer and the component, the nozzle cartridge having one or more nozzles and a housing that houses the nozzles, at least one of the nozzles being a nozzle including a magnetic material, and at least one of the nozzles being biased so that a nozzle tip protrudes from the housing. The nozzle cartridge according to the present invention is substantially the same as that described above for the nozzle cartridge included in the heating device provided in the bonding apparatus according to the present invention.

[0065] [Joining method] The bonding method of the present invention is a bonding method for conductively bonding a metal layer formed on a substrate and a component, the bonding method conductively bonding the metal layer and the component by induction heating a conductive connecting material interposed between the metal layer and the component, the induction heating is performed using a heating means having an induction coil having a space inside when viewed in a plane, and a nozzle cartridge placed in the space of the induction coil, the nozzle cartridge having one or more nozzles containing a magnetic material and a housing that houses the nozzles, at least one of the nozzles is biased so that a nozzle tip protrudes from the housing, and the nozzle tip presses the components against the metal layer when an AC voltage is applied to the induction coil to induction heat the conductive connecting material. The joining method according to the present invention is essentially equivalent to a joining method using the joining apparatus according to the present invention, and the members and conditions, etc. used in the joining method are essentially similar to the members and operating conditions, etc., of the joining apparatus according to the present invention. [Explanation of symbols]

[0066] 1 Bonding equipment 10 Nozzle Cartridge 11 Nozzle 111 Nozzle tip 112 Magnetic material 113 Spacer 12. Actuation means 21 Cabinet 221 First Vent 222 Second Vent 23. Space inside the case 24 Nozzle / biasing means storage section 31 Induction Coil 32 Power supply 41 parts 411 Parts body 412 Component Conductive Part 51 Conductive connecting materials 61 Substrate 62 Metal layer 63 Magnetic materials 71 Heating device 81 Placement table

Claims

1. A bonding apparatus for conductively bonding a metal layer formed on a substrate to a component, comprising: the joining device includes a heating device for inductively heating a conductive connecting material interposed between the metal layer and the component; the heating device includes an induction coil having a space inside in a plan view, and a nozzle cartridge disposed in the space of the induction coil; the nozzle cartridge has one or more nozzles including a magnetic material and a housing that houses the nozzles; At least one of the nozzles is biased so that a nozzle tip portion protrudes from the housing, the nozzle tip presses each of the components against the metal layer when applying an AC voltage to the induction coil to inductively heat the conductive connecting material; The joining device.

2. The substrate is made of an insulating material, The bonding apparatus according to claim 1 , wherein the metal layer has an area that can be locally heated by induction heating.

3. 3. The bonding apparatus according to claim 1, wherein at least one of the nozzles is a nozzle made of a magnetic material or a nozzle made of a magnetic material and having a spacer at a tip thereof.

4. The joining device according to claim 1 or 2, wherein the magnetic body is soft ferrite.

5. 3. The bonding device according to claim 1 or 2, wherein the housing is made of a material containing one or more resins selected from the group consisting of polyetherketone-based resins, polyetheretherketone-based resins, polyimide-based resins, polyamide-based resins, polyamideimide-based resins, polyoxymethylene-based resins, polysulfone-based resins, and polysulfide-based resins.

6. A nozzle cartridge for use in a bonding device that conductively bonds a metal layer formed on a substrate to a component, comprising: the nozzle cartridge is disposed in a space of an induction coil having a space therein in a plan view, the induction coil being included in a heating device that induction heats a conductive connecting material interposed between the metal layer and the component; The nozzle cartridge has one or more nozzles and a housing that houses the nozzles, At least one of the nozzles is a nozzle including a magnetic material; At least one of the nozzles is biased so that a nozzle tip portion protrudes from the housing. The nozzle cartridge.

7. A bonding method for conductively bonding a metal layer formed on a substrate to a component, comprising the steps of: the bonding method includes induction heating a conductive connecting material interposed between the metal layer and the component to conductively bond the metal layer and the component, the induction heating is performed by using a heating means having an induction coil having a space inside in a plan view and a nozzle cartridge disposed in the space of the induction coil; the nozzle cartridge has one or more nozzles including a magnetic material and a housing that houses the nozzles; At least one of the nozzles is biased so that a nozzle tip portion protrudes from the housing, the nozzle tip presses each of the components against the metal layer when applying an AC voltage to the induction coil to inductively heat the conductive connecting material; The bonding method.

Citation Information

Patent Citations

  • Solder joint device

    JP2018148136A

  • Circuit board and mounting method

    WO2020250427A1