Medical Ventilation Filters

A composite vent filter with a fluoropolymer membrane and thermoplastic polymer layers addresses the challenge of balancing airflow and bonding strength, achieving reduced air flow loss and improved structural integrity for safe medical procedures.

JP2024536139AInactive Publication Date: 2024-10-04ENTEGRIS INC
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2024519297
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-09-29
Filing Date
2022-09-27
Publication Date
2024-10-04
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing disposable medical filters face challenges in achieving sufficient airflow rates while maintaining effective laminations due to the difficulty in balancing air permeability and bonding strength during the lamination process, which can lead to air entering the patient's bloodstream and unsuccessful injections.

Method used

A composite vent filter structure comprising a fluoropolymer membrane and two air-permeable thermoplastic polymer layers with specific melting points, one ranging from 95°C to 180°C and the other from 220°C to 265°C, is used to create a laminate that maintains high airflow rates and structural integrity without adhesives, achieved through preheating and controlled lamination.

Benefits of technology

The solution results in a composite filter with reduced air flow loss and enhanced bond strength, ensuring effective ventilation during medical procedures while preventing air entry into the patient's bloodstream.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024536139000001_ABST
    Figure 2024536139000001_ABST
Patent Text Reader

Abstract

The present disclosure provides improved vent filters useful in disposable in-line transfusion systems. In a first aspect, the present disclosure provides a filter comprising: (i) a layer comprising a fluoropolymer membrane; and (ii) a layer comprising at least two air-permeable thermoplastic polymer layers, the air-permeable thermoplastic polymer layers being comprised of a first polymer layer and a second polymer layer, the first polymer layer being in bonding contact with the fluoropolymer membrane and having a melting point of about 95° C. to about 180° C., and the second polymer layer being in bonding contact with the first polymer layer and having a melting point of about 220° C. to about 265° C. These filters exhibit excellent bond strength between the various layers while maintaining a significant amount of the original fluoropolymer membrane air flow rate.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates generally to venting filters and, more particularly, to venting filters useful in disposable in-line transfusion systems. [Background technology]

[0002] The use of disposable, i.e., single-use, medical filters, such as in-line vent filter devices, during the administration of intravenous fluids to patients is a common practice in modern clinical care. Slow and incomplete venting during the use of disposable medical filters is an issue that has historically presented several difficulties. If the air in the infusion filter is not vented at the beginning of the infusion process, the infusion cannot be performed successfully. Furthermore, if the air in the infusion filter is not effectively vented during the infusion process, the air may enter the patient's bloodstream, with pulmonary embolism as a potential adverse outcome.

[0003] Traditionally, breathable membranes on disposable medical filters are generally composite structures of polyester (e.g., poly(ethylene terephthalate)) nonwoven fibers and poly(tetrafluoroethylene) microporous membranes, created through a lamination process. Because the filter is in direct contact with the transfusion, no adhesives are used during lamination to avoid extractable materials. During the high temperature lamination process, it is inherently difficult to balance the necessary desired air permeability of the resulting laminated composite filter against the bonding strength between the polyester nonwoven membrane and the poly(tetrafluoroethylene) membrane. Often, when high temperatures and / or compression are utilized, the resulting laminate exhibits low air permeability, i.e., high air flux losses. Thus, there continues to be a need for such breathable membranes with effective lamination while still exhibiting sufficient air flow rates. Summary of the Invention

[0004] The present disclosure provides an improved vent filter useful in a disposable in-line blood transfusion system. In a first aspect, the present disclosure provides a vent filter comprising: (i) a layer comprising a fluoropolymer film; (ii) a layer including at least two air-permeable thermoplastic polymer layers, the air-permeable thermoplastic polymer layers being composed of a first polymer layer and a second polymer layer; Including, A filter is provided, the filter comprising a first polymeric layer in bonding contact with the fluoropolymer membrane and having a melting point of about 95°C to about 180°C, and a second polymeric layer in bonding contact with the first polymeric layer and having a melting point of about 220°C to about 265°C.

[0005] In some embodiments, the air-permeable thermoplastic polymeric layers may be of the same or different polymer classes and may be selected from thermoplastic polymers such as polyesters and polyolefins. Other thermoplastic polymers may also be utilized, provided they have the necessary melting temperatures as described herein. Advantageously, these air-permeable thermoplastic polymeric layers are constructed from woven or non-woven fiber structures. The air-permeable thermoplastic polymeric layers are advantageously constructed from a material that is compatible with and therefore capable of thermal bonding to the filter housing, which is often constructed from acrylonitrile butadiene styrene copolymer (ABS), acrylonitrile-styrene copolymer (AS), or methyl methacrylate-acrylonitrile-butadiene-styrene copolymer (MABS).

[0006] In one embodiment, by utilizing a polyester layer component having at least two layers, one composed of a low melt polyester and one of a high melt polyester, the resulting laminate provides a good balance of high (residual) air flow with good structural integrity while eliminating the need for adhesives or other means to achieve proper lamination of a poly(tetrafluoroethylene) (PTFE) membrane layer and a structural polymer, such as poly(ethylene terephthalate) (PET), with the polyester.

[0007] In one embodiment, the low melt polymer layer is poly(ethylene terephthalate) having a melt temperature of about 95° C. to about 180° C., or about 150° C. to 180° C. As used herein, the term "poly(ethylene terephthalate)" refers to a polyester composed primarily of residues of terephthalic acid and ethylene glycol, but also encompasses such polymers in which the diacid and / or glycol are other than terephthalic acid and ethylene glycol. Such modifications to polymers, including air permeable (e.g., woven or nonwoven) materials, are well known to those skilled in the art and can be designed for desired physical properties, such as modulus of elasticity, melt temperature, compatibility with other polymers, etc.

[0008] This low melt temperature polyester can be heat fused with a high melt polyester to form a bilayer structure that effectively serves as a support layer for a fluoropolymer (e.g., poly(tetrafluoroethylene) or "PTFE") layer while maintaining sufficient air flow so that the resulting composite filter can effectively act as a vent filter. Such a bilayer material is commercially available from Asahi Kasei under the product name C5030. In this product C5030, the low melt layer is PET having a melting point of about 150°-180°C and a softening temperature of about 125°C, and the high melt layer is PET having a melting point of about 260°C.

[0009] By preheating the polyester substrate layer and the microporous fluoropolymer layer prior to introduction into the laminator, the low melting polyester layer can be sufficiently melted to allow for thermal welding (i.e., bonding) with the PTFE layer, while effectively "stretching" the chains or chain segments on the poly(tetrafluoroethylene) before they are fixed during the compression stage when the layers are laminated together under elevated heat and compression. It has been found that by applying an appropriate compression force under a constant (stretching) tension, it is possible to reduce the shrinkage of the poly(tetrafluoroethylene) layer, thereby maintaining high membrane porosity, thereby greatly reducing the air flow loss of the resulting composite filter structure. The resulting composite filter exhibits excellent bond strength while at the same time maintaining a significant amount of the original fluoropolymer membrane air flow rate. In general, the starting air flow rate of the fluoropolymer membrane was about 0.25 liters / min, and the composite membrane, i.e., the air flow loss rate after lamination, was only about 30% to about 50%. [Brief description of the drawings]

[0010] [Figure 1] FIG. 1 shows an exemplary lamination operation illustrating one embodiment of the present disclosure in which a PTFE microporous membrane is laminated to a polyester nonwoven material, the material including at least two layers, the layer that is ultimately in bonding contact with the PTFE microporous membrane being a relatively low melting point polyester. [Diagram 2] 1 illustrates a cross-section of an exemplary composite filter structure of the present disclosure, in which a PTFE microporous membrane (9) is in bonding contact with a polyester nonwoven layer (10), which in turn is in contact with a polyester nonwoven layer (11). As described herein, polyester nonwoven layer (10) is a polyester with a lower melting point than polyester nonwoven layer (11). [Diagram 3]FIG. 1 illustrates the structure and operation of a typical disposable in-line infusion vent filter device. A polyester / PTFE composite membrane is bonded to the structure via a polyester layer, while the PTFE layer faces downward and contacts the liquid being infused into the patient. The polyester layer is typically heat welded to the in-line infusion device structure. The directional flow of the infused liquid is shown from left to right, with the exhausting air flowing upward. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] As used in this specification and the appended claims, the singular forms "a," "an," and "the" include plural referents unless the content clearly dictates otherwise. As used in this specification and the appended claims, the term "or" is generally employed in its sense including "and / or" unless the content clearly dictates otherwise.

[0012] The term "about" generally refers to a range of numbers that are considered equivalent to a stated value (e.g., having the same function or result). In many cases, the term "about" may include numbers that are rounded to the nearest significant figure.

[0013] Numeric ranges expressed using endpoints include all numbers subsumed within that range (eg, 1 to 5 includes 1, 1.5, 2, 2.75, 3, 3.80, 4, and 5).

[0014] In a first aspect, the present disclosure provides a method for producing a thermoplastic polymeric material comprising: (i) a layer comprising a fluoropolymer membrane; and (ii) a layer comprising at least two air-permeable thermoplastic polymer layers, the air-permeable thermoplastic polymer layers being comprised of a first polymer layer and a second polymer layer, the first polymer layer being in bonding contact with the fluoropolymer membrane and being capable of being heated to a temperature between about 95° C. and about 180° C., between about 95° C. and about 170° C., between about 95° C. and about 160° C., between about 95° C. and about 150° C., between about 95° C. and about 180° C., between about 95° C. and about 190° C., between about 95° C. and about 160° C., between about 95° C. and about 190° C., between about 95° C. and about The present invention provides filters having melting points of 5°C to about 140°C, about 95°C to about 130°C, about 110°C to about 170°C, about 110°C to about 160°C, about 110°C to about 150°C, about 110°C to about 140°C, about 110°C to about 130°C, about 125°C to about 170°C, about 125°C to about 160°C, about 125°C to about 150°C, about 150°C to about 180°C, about 150°C to about 170°C, and all ranges and subranges therebetween. In some embodiments, the second polymer layer is in bonding contact with the first polymer layer and has a melting point of about 220°C to about 265°C, about 220°C to about 260°C, about 220°C to about 255°C, about 220°C to about 250°C, about 230°C to about 265°C, about 230°C to about 260°C, about 230°C to about 255°C, about 230°C to about 250°C, about 240°C to about 265°C, about 240°C to about 260°C, about 240°C to about 255°C, about 240°C to about 250°C, and all ranges and subranges therebetween.

[0015] In some embodiments, the first and second polyester layers are comprised of about 70 to about 100 weight percent, about 70 to about 95 weight percent, about 70 to about 90 weight percent, about 80 to about 100 weight percent, about 70 to about 90 weight percent, or about 90 to about 100 weight percent poly(ethylene terephthalate). In another embodiment, the melting point of the first polyester is about 150° to about 180° C. In another embodiment, the melting point of the second polyester layer is about 260° C.

[0016] Advantageously, the bond strength exhibited by the laminated filter structure is greater than or equal to about 0.17 MPa (megapascals), greater than or equal to about 0.2 MPa, greater than or equal to about 0.25 MPa, greater than or equal to about 0.3 MPa, greater than or equal to about 0.35 MPa, greater than or equal to about 0.4 MPa, greater than or equal to about 0.45 MPa, greater than or equal to about 0.5 MPa, greater than or equal to about 0.55 MPa, or greater than or equal to about 0.6 MPa.

[0017] In some embodiments, the filter exhibits an air flow rate of about 0.125 to about 0.210 liters / minute, about 0.125 to about 0.200 liters / minute, about 0.125 to about 0.175 liters / minute, about 0.125 to about 0.150 liters / minute, about 0.150 to about 0.210 liters / minute, about 0.150 to about 0.200 liters / minute, about 0.150 to about 0.175 liters / minute, about 0.175 to about 0.210 liters / minute, about 0.175 to about 0.200 liters / minute, and all ranges and subranges therebetween. In some embodiments, the filter exhibits an air flow rate within any of the above ranges in combination with a bond strength greater than or equal to about 0.2 MPa, greater than or equal to about 0.25 MPa, greater than or equal to about 0.3 MPa, greater than or equal to about 0.35 MPa, greater than or equal to about 0.4 MPa, greater than or equal to about 0.45 MPa, greater than or equal to about 0.5 MPa, greater than or equal to about 0.55 MPa, or greater than or equal to about 0.6 MPa.

[0018] In one embodiment, the filter exhibits an air flow rate of about 0.125 to about 0.175 liters / minute and a bond strength greater than or equal to about 0.35 MPa. In another embodiment, the filter exhibits an air flow rate of about 0.175 to about 0.210 liters / minute and a bond strength greater than or equal to about 0.2 MPa.

[0019] Referring to FIG. 1, in one embodiment, a poly(tetrafluoroethylene) (PTFE) microporous membrane is placed on a roll (1) and fed to a preheat roller (3) before being fed into a laminator (8). Similarly, a polyester nonwoven material, for example a combined low melt and high melt bi-layer nonwoven material (such as the Asahi Kasai C5030 material referenced above), is placed on a roll (2) and then fed to a preheat roller (3) with the low melt polyester layer facing upwards so that it is in contact with the PTFE membrane layer. The preheat roller (3) is generally operated at a temperature of about 50° to 260° C., or about 100° to about 230° C. To achieve lamination of the low melt layer of the bi-layer material to the PTFE layer and to form the desired composite, the bi-layer polyester nonwoven material is advantageously fed to a preheat roller below the PTFE layer as shown, and then sent to a laminator (8) which includes heating and compression rollers (4) and (5). Rollers (4) and (5) are generally arranged such that the compression pressure exerted on the combined layers is about 0.05 to about 0.4 MPa, about 0.05 to about 0.3 MPa, about 0.05 to about 0.2 MPa, about 0.1 to about 0.4 MPa, about 0.1 to about 0.3 MPa, about 0.1 to about 0.2 MPa, about 0.2 to about 0.4 MPa, or about 0.2 to about 0.3 MPa, and the (extension) tension exerted on the combined layers is about 0.05 to about 0.3 Newtons (N), about 0.05 to about 0.2 N, about 0.1 to about 0.3 N, or about 0.1 to about 0.2 N. The temperature of rollers (4) and (5) is generally from about 140° C. to 210° C., from about 140° C. to 200° C., from 140° C. to 175° C., from about 150° C. to 210° C., from about 150° C. to 200° C., from about 150° C. to 175° C., from about 160° C. to 210° C., from about 160° C. to 200° C., from about 160° C. to 175° C., from about 175° C. to 210° C., from about 175° C. to 200° C., and all ranges and subranges therebetween. The residence time in laminator (8) is advantageously only that time necessary to achieve the desired lamination, which is generally from about 1 to about 60 seconds, but can be empirically determined given the selection of PTFE, polyester layers and their associated physical properties.Following this heating and compression step, the composite filter material is oriented by use of rollers (6) and then collected on a storage roller (7). The heated rollers referred to herein may be constructed from any suitable material, such as stainless steel, PTFE coated rollers, etc. The heated and compressed rollers (4) and (5) referred to herein may be constructed from any suitable material, such as stainless steel, rubber, etc.

[0020] Accordingly, in another aspect, the present disclosure provides a composite fluoropolymer thermoplastic polymer filter structure comprising: (i) a fluoropolymer membrane; and (ii) a bonding layer comprising at least two air-permeable thermoplastic polymer layers, the air-permeable thermoplastic polymer layers being comprised of a first polymer layer having a melting point of about 95° to about 180° C. and a second polymer layer having a melting point of about 220° to about 265° C., the first polymer layer being in bonding contact with the fluoropolymer membrane to form a composite fluoropolymer thermoplastic polymer filter structure. A process for laminating a. applying a tie layer to a fluoropolymer membrane, whereby a first polymeric layer of the tie layer is contacted with the fluoropolymer membrane on a surface having a temperature of about 50° to about 260° C. to form a combined tie layer and fluoropolymer structure; and then b. subjecting the combined tie layer and fluoropolymer structure to a temperature of about 140° C. to about 210° C. while applying a pressure of about 0.05 to about 0.4 MPa and an elongation tension of about 0.05 to about 0.3 Newtons on the combined tie layer and fluoropolymer structure; c. cooling the resulting fluoropolymer thermoplastic polymer composite filter structure; The present invention provides a process including:

[0021] Once this lamination process is complete, the resulting fluoropolymer thermoplastic polymer composite structure can be actively cooled or simply allowed to cool to room temperature (step c).

[0022] 2, the composite filter structure may, for example, be comprised of one poly(tetrafluoroethylene) (PTFE) layer (9) in bonding contact with a low melt polyester layer (10), which in turn is in bonding contact with a high melt polyester layer (11), the latter serving to provide sufficient structural integrity for the overall filter structure.

[0023] Fluoropolymer membrane materials (e.g., PTFE) useful in the present disclosure are known microporous membrane structures, many variations of which are commercially available and can be obtained or made depending on the desired performance criteria. PTFE membranes are inherently hydrophobic and oleophobic, and in one embodiment, exhibit an air flow rate of about 0.25 to about 0.3 liters / min, a thickness of about 50 to about 60 μm, and a bubble point in ethyl alcohol of greater than about 0.17 MPa.

[0024] Polyester nonwoven materials useful in the present disclosure are widely available commercially. Such polyesters having the desired melting points for use as described herein can be obtained and include Product Type MB-12D available from Mitsubishi Paper Mills Limited, as well as Product Type C5030 available from Asahi Kasei Corporation and sold under the trademarks Precise™ and ELTAS™.

[0025] Suitable fluoropolymers effective as hydrophobic breathable membranes are commercially available. Exemplary PTFE membranes include those sold by Donaldson Company under the trademark Tetratex®, such as product names TX1302, TX1320, and TX1333. The thickness of such membranes is, in one embodiment, about 50 to about 70 μm.

[0026] Any of the filters described above can be an in-line vent filter device, for example as shown in FIG. 3. The in-line vent filter device 12 can have any of the composite membranes 13 described herein bonded to the in-line vent filter structure via a layer including at least two air-permeable thermoplastic layers, such as, for example, two polyester nonwoven layers, with the fluoropolymer layer facing downward and in contact with the liquid being infused into the patient. The composite membrane 13 is typically heat welded to the in-line vent filter device structure. The infusion liquid is shown being infused into the in-line vent filter device and flowing from left to right through the device, with air filtered through the composite membrane 13 exiting through the top of the device 12. EXAMPLES

[0027] Test Method: Bond strength test: A composite membrane with a diameter of 10 mm is placed in the membrane holder with the PTFE side facing upwards. Water pressure is applied from the downstream side starting from 0.15 MPa with an increasing rate of 0.02 MPa / 15 seconds. After 15 seconds under pressure, observe whether there are any air bubbles on the membrane surface (membrane and support are laminated). If there is no bulge or bump, it means that the bond strength is adequate at this strength. Then the pressure continues to increase until a bulge is observed during the 15 seconds pressure hold. If a bulge is observed, the composite membrane is considered to have peeled off.

[0028] Air Flow Measurement: A composite membrane of 8 mm diameter is placed in the membrane holder. The air flow rate (L / min) is then measured as the air passing rate in liters per minute at a pressure of 10 KPa. A rotameter flowmeter was used to measure the air flow rate.

[0029] Air Flow Loss Rate: The air flow loss rate (AFLR) is determined according to the following formula: AFLR=(PTFE air flow rate-composite membrane air flow rate) / (PTFE air flow rate)×100%.

[0030] In carrying out the examples described below, the lamination operation shown in FIG. 1 was utilized, and references to roller numbers refer to the corresponding rollers in FIG.

[0031] Example 1: The temperature of Roller-3 is set at 150°C, the temperature of Roller-4 is set at 200°C, the lamination pressure between Roller-4 and Roller-5 is set at 0.2MPa, and the temperature of Roller-6 is set at room temperature. After the temperature is stabilized, the PET nonwoven fabric and the PTFE membrane are successively put into Roller-3, Roller-4 and Roller-5, and Roller-6 under 0.1N (Newton) tension at a speed of 2 meters / min, and the resulting membrane is shown in Example 1 of Table 1.

[0032] Comparative Example 1: The temperature of Roller-3 is set at room temperature, the temperature of Roller-4 is set at 200°C, the lamination pressure between Roller-4 and Roller-5 is set at 0.2MPa, and the temperature of Roller-6 is set at room temperature. After the temperature is stabilized, the PET nonwoven fabric and the PTFE membrane are successively put into Roller-3, Roller-4 and Roller-5, and Roller-6 under 0.1N tension at a speed of 2m / min, and the resulting membrane is shown in Comparative Example 1.

[0033] Comparative Example 2: The temperature of Roller-3 is set at room temperature, the temperature of Roller-4 is set at 220°C, the lamination pressure between Roller-4 and Roller-5 is set at 0.1MPa, and the temperature of Roller-6 is set at room temperature. After the temperature is stabilized, the PET nonwoven fabric and the PTFE membrane are successively put into Roller-3, Roller-4 and Roller-5, and Roller-6 at a speed of 1m / min under 0.25N tension, and the resulting membrane is shown in Comparative Example 2.

[0034] Comparative Example 3: The temperature of Roller-3 is set at room temperature, the temperature of Roller-4 is set at 180°C, the lamination pressure between Roller-4 and Roller-5 is set at 0.3MPa, and the temperature of Roller-6 is set at room temperature. After the temperature is stabilized, the PET nonwoven fabric and the PTFE membrane are successively put into Roller-3, Roller-4 and Roller-5, and Roller-6 under 0.2N tension and at a speed of 1.5m / min, and the resulting membrane is shown in Comparative Example 3. TIFF2024536139000002.tif79170

[0035] This data shows the improvement in bond strength due to the preheat step utilized in Example 1, while minimizing air flow loss during lamination.

[0036] Aspects In a first aspect, the present disclosure provides a method for producing a pharmaceutical composition comprising: (i) a layer comprising a fluoropolymer film; (ii) a layer including at least two air-permeable thermoplastic polymer layers, the air-permeable thermoplastic polymer layers being composed of a first polymer layer and a second polymer layer; Including, a first polymeric layer in bonding contact with the fluoropolymer membrane and having a melting point of about 95° C. to about 180° C.; A filter is provided in which a second polymeric layer is in bonding contact with the first polymeric layer and has a melting point of about 220°C to about 265°C.

[0037] In a second aspect, the present disclosure provides a filter of the first aspect, wherein the filter exhibits an air flow rate of about 0.125 to about 0.175 liters / minute and exhibits a bond strength greater than or equal to about 0.35 MPa.

[0038] In a third aspect, the present disclosure provides the filter of the first aspect, wherein the filter exhibits an air flow rate of about 0.175 to about 0.210 liters / minute and exhibits a bond strength greater than or equal to about 0.2 MPa.

[0039] In a fourth aspect, the present disclosure provides the filter of any one of the first, second, or third aspects, wherein the air-permeable thermoplastic polymeric layer is constructed from nonwoven fibers.

[0040] In a fifth aspect, the present disclosure provides the filter of any one of the first to fourth aspects, wherein the fluoropolymer membrane is constructed from poly(tetrafluoroethylene).

[0041] In a sixth aspect, the present disclosure provides the filter of any one of the first to fifth aspects, wherein the thermoplastic polymeric layer is comprised of a polymer selected from polyester and polyolefin.

[0042] In a seventh aspect, the present disclosure provides a method for producing a pharmaceutical composition comprising: (i) at least one layer comprising a poly(tetrafluoroethylene) membrane; (ii) a layer including at least two polyester nonwoven layers, the polyester nonwoven layers being composed of a first polyester layer and a second polyester layer; a first polyester layer in bonding contact with a poly(tetrafluoroethylene) membrane and having a melting point of about 95°C to about 180°C; and a second polyester layer in bonding contact with the first polyester layer and having a melting point of about 220°C to about 265°C.

[0043] In an eighth aspect, the present disclosure provides the filter of the seventh aspect, wherein the filter exhibits an air flow rate of about 0.125 to about 0.175 liters / minute and exhibits a bond strength greater than or equal to about 0.35 MPa.

[0044] In a ninth aspect, the present disclosure provides the filter of the seventh aspect, wherein the first and second polyester layers are comprised of about 70 to about 100 weight percent poly(ethylene terephthalate).

[0045] In a tenth aspect, the present disclosure provides the filter of the seventh aspect, wherein the first polyester has a melting point of about 150 to about 180°C.

[0046] In an eleventh aspect, the present disclosure provides a composite fluoropolymer thermoplastic polymer filter structure comprising: (i) a fluoropolymer membrane; and (ii) a bonding layer comprising at least two air-permeable thermoplastic polymer layers, the air-permeable thermoplastic polymer layers being comprised of a first polymer layer having a melting point of about 95° to about 180° C. and a second polymer layer having a melting point of about 220° C. to about 265° C., the first polymer layer being in bonding contact with the fluoropolymer membrane to form a composite fluoropolymer thermoplastic polymer filter structure. A process for laminating a. applying a tie layer to a fluoropolymer membrane, whereby a first polymeric layer of the tie layer is contacted with the fluoropolymer membrane on a surface having a temperature of about 50° to about 260° C. to form a combined tie layer and fluoropolymer structure; and then b. subjecting the combined tie layer and fluoropolymer structure to a temperature of about 140° C. to about 210° C. while applying a pressure of about 0.05 to about 0.4 MPa and an elongation tension of about 0.05 to about 0.3 Newtons on the combined tie layer and fluoropolymer structure; c. cooling the resulting fluoropolymer thermoplastic polymer composite filter structure; The present invention provides a process including:

[0047] In a twelfth aspect, the present disclosure provides the process of the eleventh aspect, wherein the fluoropolymer is poly(tetrafluoroethylene).

[0048] In a thirteenth aspect, the present disclosure provides the process of the eleventh or twelfth aspect, wherein the first polymeric layer is comprised of a polyester.

[0049] In a fourteenth aspect, the present disclosure provides the process of the eleventh, twelfth, or thirteenth aspects, wherein the second polymeric layer is comprised of a polyester.

[0050] In a fifteenth aspect, the present disclosure provides the process of any one of the eleventh to fourteenth aspects, wherein the first polymeric layer is comprised of poly(ethylene terephthalate) having a melting point of about 95° to about 180° C.

[0051] In a sixteenth aspect, the present disclosure provides the process of any one of the eleventh to fifteenth aspects, wherein the second polymeric layer is comprised of a poly(terephthalate) having a melting point of about 220° to about 265° C.

[0052] In a seventeenth aspect, the present disclosure provides the process of any one of the eleventh to fifteenth aspects, wherein the first polymeric layer is poly(ethylene terephthalate) having a melting point of about 150° to about 180° C.

[0053] In an eighteenth aspect, the present disclosure provides the process of any one of the eleventh to seventeenth aspects, wherein the fluoropolymer thermoplastic polymer composite filter structure exhibits an air flow rate of about 0.125 to about 0.175 liters per minute and a bond strength of greater than or equal to about 0.35 MPa.

[0054] In a nineteenth aspect, the present disclosure provides the process of any one of the eleventh to seventeenth aspects, wherein the fluoropolymer thermoplastic polymer composite filter structure exhibits an air flow rate of about 0.175 to about 210 liters / min and exhibits a bond strength greater than or equal to about 0.2 MPa.

[0055] In a twentieth aspect, the present disclosure provides an in-line vent filter device comprising the filter of any one of the first to tenth aspects.

[0056] Although several exemplary embodiments of the present disclosure have been described above, those skilled in the art will readily appreciate that still other embodiments may be made and used within the scope of the claims appended hereto. Numerous advantages of the present disclosure covered by this document have been set forth in the above description. However, it will be understood that the present disclosure is in many respects merely exemplary. The scope of the present disclosure is, of course, defined in the language in which the appended claims are expressed.

Claims

1. (i) a layer comprising a fluoropolymer film; (ii) a layer comprising at least two air-permeable thermoplastic polymer layers, the air-permeable thermoplastic polymer layers being composed of a first polymer layer and a second polymer layer; Including, the first polymeric layer is in bonding contact with the fluoropolymer membrane and has a melting point of about 95°C to about 180°C, and the second polymeric layer is in bonding contact with the first polymeric layer and has a melting point of about 220°C to about 265°C.

2. 10. The filter of claim 1, wherein the filter exhibits an air flow rate of about 0.125 to about 0.175 liters per minute and exhibits a bond strength of greater than or equal to about 0.35 MPa.

3. 10. The filter of claim 1, wherein the filter exhibits an air flow rate of about 0.175 to about 0.210 liters per minute and exhibits a bond strength of greater than or equal to about 0.2 MPa.

4. 4. The filter of claim 1, wherein the air-permeable thermoplastic polymeric layer is constructed from non-woven fibers.

5. 5. The filter of claim 1, wherein the fluoropolymer membrane is constructed from poly(tetrafluoroethylene).

6. 6. The filter of any one of claims 1 to 5, wherein the thermoplastic polymeric layer is comprised of a polymer selected from polyesters and polyolefins.

7. (i) at least one layer comprising a poly(tetrafluoroethylene) membrane; (ii) a layer comprising at least two polyester nonwoven layers, the polyester nonwoven layers being comprised of a first polyester layer and a second polyester layer; Including, the first polyester layer is in bonding contact with the poly(tetrafluoroethylene) membrane and has a melting point of about 95°C to about 180°C, and the second polyester layer is in bonding contact with the first polyester layer and has a melting point of about 220°C to about 265°C.

8. 8. The filter of claim 7, wherein the filter exhibits an air flow rate of about 0.125 to about 0.175 liters per minute and a bond strength of greater than or equal to about 0.35 MPa.

9. 9. The filter of claim 7 or 8, wherein the first and second polyester layers are comprised of from about 70 to about 100 weight percent poly(ethylene terephthalate).

10. 11. The filter of any one of claims 7 to 10, wherein the melting point of the first polyester is from about 150 to about 180°C.

11. A process for laminating (i) a fluoropolymer membrane and (ii) a tie layer, the process comprising: applying said tie layer to said fluoropolymer membrane, said tie layer comprising at least two air-permeable thermoplastic polymer layers, said air-permeable thermoplastic polymer layers being comprised of a first polymer layer having a melting point of about 95° to about 180° C. and a second polymer layer having a melting point of about 220° to about 265° C., thereby contacting said first polymer layer of said tie layer with said fluoropolymer membrane on a surface having a temperature of about 50° to about 260° C. to form a combined tie layer and fluoropolymer structure; b. subjecting the combined tie layer and fluoropolymer structure to a temperature of about 140° C. to about 210° C. while applying a pressure of about 0.05 to about 0.4 MPa and an elongation tension of about 0.05 to about 0.3 Newtons on the combined tie layer and fluoropolymer structure to form a composite fluoropolymer thermoplastic polymer filter structure; c. cooling the resulting fluoropolymer thermoplastic polymer composite filter structure; The process includes:

12. The process of claim 11 , wherein the fluoropolymer is poly(tetrafluoroethylene).

13. 13. The process of claim 11 or 12, wherein the first polymeric layer is composed of polyester.

14. 14. The process of any one of claims 11 to 13, wherein the second polymeric layer is composed of polyester.

15. 15. The process of any one of claims 11 to 14, wherein the first polymeric layer is composed of poly(ethylene terephthalate) having a melting point of about 95° to about 180°C.

16. 16. The process of any one of claims 11 to 15, wherein the second polymeric layer is comprised of poly(terephthalate) having a melting point of about 220° to about 265°C.

17. 15. The process of any one of claims 11 to 14, wherein the first polymeric layer is poly(ethylene terephthalate) having a melting point of about 150° to about 180°C.

18. 18. The process of any one of claims 11 to 17, wherein the fluoropolymer thermoplastic polymer composite filter structure exhibits an air flow rate of about 0.125 to about 0.175 liters / minute and a bond strength of greater than or equal to about 0.35 MPa.

19. 18. The process of any one of claims 11 to 17, wherein the fluoropolymer thermoplastic polymer composite filter structure exhibits an air flow rate of about 0.175 to about 0.210 liters / minute and a bond strength of greater than or equal to about 0.2 MPa.

20. An in-line vent filter device comprising a filter according to any one of claims 1 to 10.

Citation Information

Patent Citations

  • Assembly of supporting membrane

    JP1996243359A

  • Filter material

    JP2021511208A

  • Filter medium and air filter unit using the same

    JP3467779B2