Semiconductor substrate manufacturing and reuse
By forming porous layers in semiconductor wafers to enable exfoliation and separation, the method addresses high wafer costs by allowing multiple reuse and reducing material loss, thus lowering the cost of semiconductor device production.
Patent Information
- Application Number
- JP2024523846
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-05-12
- Filing Date
- 2022-10-21
- Publication Date
- 2024-10-04
AI Technical Summary
The high cost of silicon carbide wafers used in semiconductor devices is a significant portion of the overall fabrication cost, necessitating a method to reduce material loss and reuse these wafers to achieve cost reduction.
A method involving the formation of porous layers in semiconductor wafers to facilitate exfoliation and separation, allowing the reuse of non-porous parts for further device fabrication, including the creation of epitaxial layers and doped regions, followed by separation along porous layers using various external forces.
Enables multiple reuse of semiconductor wafers by reducing material loss and maintaining the quality of epitaxial layers, thereby lowering the overall cost of semiconductor device production.
Smart Images

Figure 2024536590000001_ABST
Abstract
Description
[Background technology]
[0001] Wafer costs for semiconductor devices grown on silicon carbide wafers / base materials tend to be high, where "silicon carbide wafers / base materials" refers to the growth substrate on which epitaxial semiconductor layers are grown. In contrast, a "substrate" can be or include the wafer and, optionally, the epitaxial and metallization layers. Such semiconductor devices can be based on silicon carbide (SiC) or other materials (e.g., GaN, GaAs, etc.) that can be grown on SiC.
[0002] Wafer costs represent a significant portion of the overall fabrication costs of semiconductor devices grown on SiC. Reducing these costs therefore creates a competitive advantage. One way to reduce wafer costs is to reduce material loss of wafer material during production, for example, by using standard wafers several times and / or by reducing losses during wafer production. Summary of the Invention
[0003] According to one embodiment of a method for processing a semiconductor wafer, the method includes forming one or more epitaxial layers on a first major surface of the semiconductor wafer; forming one or more porous layers in the semiconductor wafer or in the one or more epitaxial layers, where the semiconductor wafer, the one or more epitaxial layers, and the one or more porous layers collectively form a substrate; forming doped regions of semiconductor devices in the one or more epitaxial layers; and separating a non-porous part of the semiconductor wafer from a remainder of the substrate along the one or more porous layers after forming the doped regions of the semiconductor devices.
[0004] Those skilled in the art will recognize additional features and advantages upon reading the following detailed description, and upon viewing the accompanying drawings.
[0005] The elements of the drawings are not necessarily to scale relative to each other. Like reference numbers indicate corresponding like parts. Features of the various illustrated embodiments may be combined unless they are exclusive of each other. The embodiments are illustrated in the drawings and detailed in the following description. [Brief description of the drawings]
[0006] [Figure 1] 1 is a schematic diagram of one embodiment of a method for reuse of semiconductor wafers. [Diagram 2] FIG. 2 is a simplified block diagram of the method of FIG. 1. [Diagram 3] FIG. 13 is a block diagram of another embodiment of a method for reuse of semiconductor wafers. [Figure 4] FIG. 13 is a block diagram of another embodiment of a method for reuse of semiconductor wafers. [Diagram 5] FIG. 2 is a partial cross-sectional view of one embodiment of a porosified layer for semiconductor wafer delamination / separation. [Figure 6] FIG. 13 is a partial cross-sectional view of another embodiment of a porosified layer for semiconductor wafer delamination / separation. [Figure 7] 1A-1D are respective partial cross-sectional views of different embodiments for forming a homogeneous porous layer for delamination / separation of a semiconductor wafer. [Figure 8] FIG. 1 illustrates a partial cross-sectional view of one embodiment of a porous multi-layer stack for delamination / separation of semiconductor wafers. [Figure 9] FIG. 2 illustrates a partial cross-sectional view of one embodiment of a device substrate attached to a front carrier. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0007] The embodiments described herein provide a method for multiple semiconductor wafer reuse using a porous semiconductor layer for epitaxy and for splitting. Device structures are fabricated on a pretreated semiconductor wafer with a porous surface layer. After device fabrication, the semiconductor wafer is separated (peeled) from the remainder of the substrate at the porous layer and reused.
[0008] 1 illustrates one embodiment of the method. The method includes (a) providing a semiconductor wafer 100 that is ready for subsequent epitaxy. (b) One or more porous layers 102 are formed at and below a first major surface 104 of the semiconductor wafer 100. (c) One or more epitaxial layers 106 are grown on the first major surface 104 (e.g., front side) of the semiconductor wafer 100. (d) Front side processing is then performed up to a certain point, e.g., front side metallization and / or passivation, to create a substrate 108 that includes a non-porous part 110 of the wafer 100, one or more porous layers 102, and device structures 111. The device structure 111 may include drain regions, buffer layers, body zones, source zones, emitter zones, gates, current spreading layers, etc. formed in the one or more epitaxial layers 106, and front-side metallization, passivation, etc. formed on the one or more epitaxial layers 106.
[0009] 1 further includes (e) attaching a temporary or permanent carrier 112 to the front side of the substrate 108 to stabilize the substrate 108. The semiconductor wafer 100 is delaminated (f) by using the porous layer(s) 102 as a separation layer. That is, the non-porous part 110 of the semiconductor wafer 100 is separated from the remainder 108' of the substrate 108 along the porous layer(s) 102. The delamination or separation process, upon separation, produces a reclaimed wafer 114 and a device substrate 116 that constitutes the remainder 108' of the substrate 108.
[0010] For reclaimed wafers 114, the reclaimed wafers 114 may be refurbished (g) and optionally further processed, for example to increase the wafer thickness, as described later herein. The refurbished reclaimed wafers 114 may be used again (a->f) to form another device substrate. The device substrate 116 may undergo further processing steps such as, for example, preparing a surface 118 of the device substrate 116 defined by separating it from the non-porous part 110 of the semiconductor wafer 100 (h), forming metallization and / or ohmic contacts 120 on the prepared backside 118 of the device substrate 116 (i), attaching a carrier 122 to the metallized backside 118 of the device substrate 116 (j), removing the carrier 112 from the front side 124 of the device substrate 116 (k), testing the device substrate 116 (l), singulating the device substrate 116 into individual dies (chips) 126 (m) and removing the backside carrier 122, as well as further back-end "BE" assembly (n), such as plating, as described in more detail later herein.
[0011] Figure 2 shows the same method shown in Figure 1, but in less detail. The letters (a)-(n) used in the figures to indicate different processing steps do not necessarily imply or suggest a required processing order, unless otherwise specified.
[0012] Figure 3 shows another embodiment of the method shown in Figure 1, with the same level of detail used in Figure 2. In Figure 3, testing (l) of the device substrate 116 is performed earlier in the process. In particular, the device substrate 116 is tested (l) prior to peeling / separating (f) the non-porous part 110 of the semiconductor wafer 100 from the remainder 108' of the substrate 108.
[0013] Figure 4 illustrates another embodiment of the method shown in Figure 1, with the same level of detail used in Figure 2. As in Figure 3, in Figure 4 the device substrate 116 is tested (l) prior to peeling / separating (f) the non-porous part 110 of the semiconductor wafer 100 from the remainder 108' of the substrate 108. In Figure 4, singulation (m) of the device substrate 116 into individual dies (chips) 126 is also performed prior to peeling / separating (f) the non-porous part 110 of the semiconductor wafer 100 from the remainder 108' of the substrate 108.
[0014] 3 and 4 performs device testing before the front carrier 112 is attached to the substrate 108. Furthermore, no testing is required after peeling / separating (f) the non-porous part 110 of the semiconductor wafer 100 from the remainder 108' of the substrate 108.
[0015] 2-4, further die testing may be performed after singulation, but prior to other post-die fabrication processes. For example, individual die (chips) 126 may be tested after singulation, but prior to pick-and-place, molding, packaging, assembly, etc.
[0016] Steps (a)-(n) illustrated in Figures 1-4 are described in more detail below.
[0017] Step (a): Wafer preparation The semiconductor wafer 100 may be crystalline, e.g., monocrystalline or at least partially monocrystalline, e.g., at the front side surface 104 on which epitaxy is performed, so that one or more epitaxial layers 106 may be grown with a sufficiently low crystal defect density to support device fabrication. The semiconductor wafer 100 may be a SiC wafer (i.e., may include or consist of SiC), e.g., off-axis or on-axis 4H-SiC, 3C-SiC, 6H-SiC, etc. However, the reuse method is not limited to SiC as a wafer material, but may also be used for other wafer materials, such as Si, GaN, GaAs, Ga2O3, etc., or for substrates composed of two or more layers of different materials. In plan view, the semiconductor wafer 100 may have a circular, elliptical or polygonal (e.g., rectangular or hexagonal) shape, optionally with so-called flats or notches. The diameter of the semiconductor wafer 10 can be 100 mm, 150 mm, 200 mm, or even larger.
[0018] The semiconductor wafer 100 may have a standard thickness. The standard thickness may vary depending on the wafer diameter. Typically, 100 mm and 150 mm wafers (initially) have a thickness of 350 μm (e.g., with an accuracy of at most ±40 μm or at most ±25 μm). However, the starting wafer 100 may have a thickness below the standard thickness (e.g., 200 μm for 100 mm or 150 mm wafers). For larger wafer diameters, the standard thickness may be higher to allow mechanical stability of the semiconductor wafer 100 during processing. The semiconductor wafer 100 may alternatively have a thickness smaller or larger than the standard thickness. For example, the reuse method may start with a thicker initial wafer (e.g., above or with a standard thickness), the thickness of which may be reduced in each cycle of the reclaiming steps (a)-(g). That is, the reclaimed wafer 114 may have a thickness smaller than the initial wafer 100. If the porous layer(s) 102 are formed in the epitaxial layer(s) 106 rather than in the initial wafer 100, the entire semiconductor wafer 100 is non-porous and available for reuse after the peeling / separation step (f).
[0019] The semiconductor wafer 100 may already have been pre-processed to enable epitaxial growth. However, preparing the semiconductor wafer 100 for epitaxial growth may be required even for the first process cycle. In general, preparing the semiconductor wafer 100 for epitaxial growth may involve at least one of the following processes. Combinations of the processes identified below are possible, and some of the processes may fall into two or more of the aforementioned categories. Wafer preparation processes include: cleaning; mechanical grinding (polishing); treatment with a blast of fine materials (e.g., sand blasting or dry ice blasting); chemical mechanical polishing (CMP); plasma treatment with chemical and / or mechanical process components, such as, for example, reactive ion etching, wet etching, dry etching, or subsequent wet etching, for example, with hot KOH, KMnO4, etc., ion implantation, for example, with HF:HNO3; laser-assisted surface treatment; temperature treatment, such as baking, in a gas atmosphere, for example, hydrogen, or a mixture of various gas species, or, for example, repeated thermal oxidation at about 1200° C. with subsequent oxide removal, where at least a few nanometers (nm) may be removed; and thermal reactions, for example, with other materials, such as metals.
[0020] Step (b): Porosification The porous layer(s) 102 are created by porosifying the semiconductor material of the semiconductor wafer 100 or of one or more epitaxial layers 106. The porosification process can be influenced by the doping concentration of the semiconductor material to be porosified. For example, a higher doping concentration can result in a higher porosity. The desired doping concentration can be provided by at least one of an initial substrate doping and by an implantation step with a subsequent temperature treatment. For example, the doping concentration of the semiconductor material to be porosified can be modified by adjusting one or more of the implantation energy, the implantation angle, and the channeling implant. In another approach, the doping concentration of the semiconductor material to be porosified is modified by varying the vertical and / or lateral doping concentration of the semiconductor material to be porosified.
[0021] Porosity is a combination of pore density and pore size (e.g., pore diameter) in a semiconductor material. Greater porosity can result from a lower pore density combined with a larger pore size, or a higher pore density combined with a lower pore size, or even both, a combination of a higher pore density and a larger pore size. The semiconductor wafer 100 can be made porosified prior to epitaxial growth, or an epitaxial layer(s) 106 can be grown on the wafer 100, and then one or more of these layers are made porosified.
[0022] The porosified layer(s) 102 may have varying doping concentrations in a direction perpendicular (vertical) to the first major surface 104 of the semiconductor wafer 100 and / or in a direction parallel (lateral) to the first major surface 104 of the semiconductor wafer 100. This allows for creating a stack of multiple porosified layers 102 with different pore sizes, as shown, for example, in FIG. 6. Such varying doping concentrations may be created, for example, by tuning the doping concentration during the epitaxial growth process. Alternatively or additionally, varying doping concentrations may be created by implanting dopants into the semiconductor wafer 100 and / or the epitaxial layer(s) 106.
[0023] Semiconductor materials can be made porous, for example, by an anodic porosification process. In general, anodic porosification is carried out in an electrolyte solution that can include, for example, an acid component, an alkaline component, or a salt component, and can optionally include further additives, such as surfactants, such as IPA, ethanol, etc. For example, the electrolyte solution can be or include a fluorine-based chemistry (e.g., aqueous HF solution) or an alkaline etch chemistry (e.g., TMAH, KOH). The anodic porosification process can be driven by exposure to UV (ultraviolet) radiation. Porosification can also be performed in the so-called "breakdown" region, where charge carriers are induced via a sufficiently high electric field. Other additives in the etch chemistry affect the etch rate and porosity.
[0024] The pores represent voids in the semiconductor material. The porosity may vary with depth depending on the porosification conditions. For example, the porosity can be varied by varying the current and / or voltage of the electrochemical process and / or the composition of the electrolyte solution. The semiconductor material is weakened by the pores (voids) so that sufficient stress can be generated to split the substrate 108 at the weakened (porosified) part. However, the porosity (e.g., density and size of the pores) should be low enough that all subsequent process steps can be performed without local or complete delamination of the porous layer(s) 102 before the peeling / separation step (f). That is, the porosity of the porous layer(s) 102 should be high enough to ensure good peeling properties, but low enough to avoid the porous layer(s) 102 peeling off. For example, the porous layer(s) 102 used for peeling should have a high porosity (e.g., the highest porosity in the stack). Additionally or alternatively, the porous layer 102 used for exfoliation may have a pore structure (e.g., pore configuration or distribution) such that the porous layer 102 is the weakest porous layer in the stack. For example, in this porous layer 102, the combined pores may occupy at least the same amount of space or occupy more space than the non-porous area surrounding the pores (e.g., on average, the distance between the pores is less than the diameter of the pores). Depending on the pore configuration, for larger pores, a lower pore density may be sufficient, and for smaller pores, a higher pore density may be required.
[0025] In one embodiment, one or more semiconductor layers 106 are epitaxially grown on the porous layer(s) after the porosification step (b). The surface of the top porous layer 102 should therefore enable a high quality epitaxial layer(s) 106. For this, the top porous layer 102 should have a high crystalline quality. This can be ensured by utilizing a so-called skin layer. Such a skin layer is an extremely thin surface layer that occurs during porosification and has an extremely low pore density compared to the porosified layer below. The skin layer may have the following properties: monocrystalline, low surface roughness, small pore diameter (preferably less than 200 nm, e.g. less than 100 nm, e.g. less than 70 nm, e.g. about 50 nm), small pore density. For example, in the case of pore density, the distance between the pores may be, on average, larger than the diameter of the pores, and therefore the pores (voids) occupy less space than the non-porous regions. In terms of porosity, the pores may occupy less than 50% of the space of the non-porous regions). The naturally occurring skin layer can be extremely thin (e.g., 20-50 nm) and inhomogeneous. The thickness and homogeneity of the skin layer can be influenced as described below.
[0026] FIG. 5 illustrates an embodiment in which a porosified layer 200 for exfoliation / separation is formed on or in the semiconductor wafer 100 and a skin layer 202 is formed on the porosified exfoliation / separation layer 200. The thickness of the skin layer 202 can be, for example, in the range of 100 nm to 500 nm. The thickness of the porosified exfoliation / separation layer 200 can be, for example, in the range of 1 μm to 10 μm. Such a layer stack can be realized by forming layers with different average doping concentrations, since porosification by electrochemical etching is significantly accelerated with increasing doping concentration. Thus, the skin layer 202 can have a higher average doping concentration than the non-porous part 100 of the semiconductor wafer 100, and the porosified exfoliation / separation layer 200 can have a higher average doping concentration than the skin layer 202. For example, the non-porous part 100 of the semiconductor wafer 100 has a thickness of about 5e18 cm. -3and the porosified release / separation layer 200 may have an average doping concentration of about 1e20 cm -3 and the skin layer 202 may have an average doping concentration of about 1e17 cm -3 The average doping concentration may be
[0027] The areas with different doping shown in Fig. 5 may be structured or have a varying thickness across the semiconductor wafer 100 as required by the individual application. Different doping regions may be provided via implantation and / or during epitaxy. For example, different doping regions may be provided by (i) locally compensating the n-doping in the surface layer 202 by acceptor implantation or by implanting impurities with deep energy levels, such as vanadium and / or titanium impurities, (ii) increasing the n-doping in the layer 200 to be made porous by donor implantation, and / or (iii) by implantation and electrically directed diffusion.
[0028] Additionally or alternatively, FIG. 6 illustrates a patterned mask 300 that is lightly doped (e.g., approximately 1e17 cm -3 3 shows an embodiment in which a mask 300 is used on a semiconductor layer 302. The mask 300 can be, for example, a nitride mask (kept longer) or a resist mask (removed before finishing the entire porosification step). The mask 300 can have openings 304 with a width or diameter d1 in the range of 100 nm and a distance d2 between the openings 304 in the micron (μm) range. The application of an electric field accelerates vertical porosification in the dopant-implanted regions 306. In the lightly doped regions 308 shielded by the mask 300, porosity is applied along the electric field lines, and in this case the electric field peaks, and the surface should not undergo further porosification, but rather in the more heavily doped (e.g., about 1e20 cm -3) The underlying layer 310 has a higher porosity as well. By suitable selection of the doping concentration and the spacing d2 and width d1 of the mask openings 304, the thickness, and therefore the stability, of the skin layer 302 can be specifically controlled.
[0029] The electrochemical formation of pores in semiconductor materials is strongly dependent on the applied electric current. In order to generate a homogeneous porous layer across the entire substrate wafer, the electric current flowing through the material should be homogeneous. For this reason, the pore morphology and depth are highly dependent on the doping uniformity within the semiconductor material to be made porous. Therefore, making a semiconductor material porous is a process that is highly dependent on the doping uniformity of the semiconductor material.
[0030] Porosification can exploit this dependence on doping in two ways: (i) creating a stack of multiple layers with different porosity, and (ii) using a (low-doped) wafer or a low-conductivity layer as an etch stop during pore formation.
[0031] For etch stop, a low conductive epitaxial layer, or a low conductive wafer region, or a low conductive buried wafer region, induced by implantation of a suitable dopant resulting in counterdoping. A good (high) conductive layer with a higher doping concentration can be epitaxially grown on top of the low conductive part or fabricated via implantation. The good conductive layer allows the formation of a homogeneous porous layer. Epitaxial materials show less doping variation than the base material, which may open the possibility of achieving a homogeneous porous structure by adding a homogeneously doped layer on top of the base material.
[0032] FIG. 7 shows different embodiments for forming a homogeneous porous layer. The embodiment shown in FIG. 7 is shown using a base SiC wafer 400. However, as previously explained, the reuse method described herein is not limited to SiC as a wafer material, but can also be used for other wafer materials, such as Si, GaN, GaAs, Ga2O3, or for substrates composed of two or more layers of different materials. According to the embodiment shown in FIG. 7, the thickness variation of the resulting porous layer 102 is <<±1 μm, and a homogeneous pore morphology is achieved across the base SiC wafer 400.
[0033] In one embodiment, a homogeneously doped epitaxial (EPI) layer 402 is grown on a base SiC wafer 400. An upper part of the homogeneously doped epitaxial layer 402 is porosified to form a homogeneous porous layer 404. A lower part of the homogeneously doped epitaxial layer 402 remains non-porous and acts as an etch stop 406.
[0034] In another embodiment, a low conductivity epitaxial layer, low conductivity wafer region, or low conductivity buried wafer region 408 is formed by induced implantation of a dopant that provides counterdoping. A higher conductivity layer 410 is formed on the low conductivity epitaxial layer, low conductivity wafer region, or low conductivity buried wafer region 408. The higher conductivity layer 410 has a higher average doping concentration than the low conductivity epitaxial layer, low conductivity wafer region, or low conductivity buried wafer region 408. A homogeneous porous layer 404 is then formed in the higher conductivity layer 410. In one embodiment, a lower part 412 of the higher conductivity layer 410 remains non-porous under the homogeneous porous layer 404. In another embodiment, the entire higher conductivity layer 410 is converted to the homogeneous porous layer 404. In either case, the low conductivity epitaxial layer, low conductivity wafer region, or low conductivity buried wafer region 408 acts as an etch stop.
[0035] For porous multi-layer stacks, to further control the homogeneity of pore formation, a highly doped semiconductor layer can be epitaxially grown on top of an underlying lightly doped portion (e.g., layer or wafer), and the porosification step (b) is applied to both doped semiconductor layers.
[0036] 8 shows an embodiment of a porous multi-layer stack. A first porous layer 500 has an average pore density greater than the average pore density of the non-porous part 110 of the semiconductor wafer 100. A second porous layer 502 above the first porous layer 500 has an average pore density greater than the average pore density of the non-porous part 110 of the semiconductor wafer 100 and less than the average pore density of the first porous layer 500. In an embodiment, the second porous layer 502 is a skin layer as described herein. An additional porous layer 504 may be formed below the first porous layer 500 and have an average pore density greater than the average pore density of the non-porous part 110 of the semiconductor wafer 100 and less than the average pore density of the first porous layer 500. Separately or in combination, an additional porous layer 506 may be formed between the first porous layer 500 and the second porous layer 502 and have an average pore density greater than the average pore density of the second porous layer 502 and less than the average pore density of the first porous layer 500.
[0037] Additionally or alternatively to the porosification embodiments described above, lateral variations in doping can be implemented in the layer 120 to be porosified adjacent to the surface of the layer 102 by masked implantation. For example, increased doping can be created in the regions of the mask openings 304 shown in Figure 6 to accelerate the vertical porosification rate in the exposed regions 306. The mask openings 304 can have, for example, a stripe or hole shape, whereby the spacing d2 and width d1 of the openings 304 can be selected to allow for extensive, defect-free epitaxial overgrowth of the porosified layer surface.
[0038] Step (c): Epitaxy Epitaxial growth can be performed on the skin layer of a new wafer or a reclaimed wafer. Skin layer surface preparation for epi growth compatibility can be achieved either in situ by a pre-growth etch under a gas flow of one or more different gas species (e.g., hydrogen) or through other methods as described above with respect to wafer preparation step (a). Thus, the etch removal depth can be limited in such a way that parts of the skin layer remain on the reclaimed wafer over the entire surface area of the reclaimed wafer.
[0039] The epi process can be tuned to provide overgrowth of the pores in the skin layer. After a few layers (e.g., at least 2 or at least 3 or at least 10 times the thickness of the pore size in the skin layer, e.g., less than 500 nm or less than 300 nm or less than 200 nm for pore diameters of approximately 50 nm), the epi process conditions can be changed from lateral overgrowth.
[0040] The first part of the epi for overgrowing the holes, optionally together with some of the skin layers and porous layers, may be part of the final device structure, e.g., drain layer, emitter layer, buffer layer, as described in more detail later in this specification. The first part of the epi may have a varying dopant concentration, e.g., in the lateral direction, which may be seen in the final device. For example, the hole distribution may reflect the dopant distribution within the first part of the epi. During overgrowth, the dopant may deposit differently in the region of the holes than outside the holes. The first part of the epi may also result in a reduction of defects, which may result in, for example, so-called basal plane dislocations in the subsequent epitaxial layers.
[0041] The epilayer stack may include a device epi including, for example, a highly doped drain or emitter layer, a buffer layer on the highly doped drain or emitter layer, and a drift layer on the buffer layer, etc. The drain / emitter layer, buffer layer, and drift layer may each have a constant doping concentration level throughout their respective depths or may have a doping concentration gradient within their respective layer thicknesses.
[0042] The epi may also include a multi-stack structure, where a first epitaxial layer is followed by a device epi with or without a drain / emitter or buffer layer separating the two layers. The first layer of epi, including the first part that overgrows the holes, has a high doping level and serves as structural support after the exfoliation / separation step (f).
[0043] Epitaxy can also be performed on new or reclaimed wafers 100 prior to substrate porosification. In this case, the porosification process is not applied to the semiconductor wafer 100, but rather to the epitaxial layer 106. Thereby, epi growth can start with or without a low doped layer, which acts as a porosification stop layer, followed by a layer with a high doping concentration. Epi can also include multilayer stacks with strongly varying doping levels and / or doping species, as well as vertical doping concentration gradients, to induce various degrees of porosification depth in the subsequent porosification process. Applying the porosification process to the epitaxial layer(s) 106 has at least the following advantages: (i) porosification can be controlled via different dopant concentrations in the epitaxial layer 106, and (ii) no part of the semiconductor wafer 100 is deformed, i.e., after peeling / separation, the wafer 100 continues to have the same initial thickness and can be reused an infinite number of times without thickening the wafer again.
[0044] Step (d): Front side processing Device preparation follows the epitaxial growth. The required doping regions of the device can be fabricated by implantation in the epitaxial layer 106 and / or by doping during the epitaxial process. The device structure 111 can be a structure of a semiconductor device, for example a diode, such as a MPS (Merged pin / Schottky) diode or a Schottky diode, or a power transistor device, such as a MOSFET (Metal Oxide Semiconductor Field Effect Transistor), a JFET (Junction Field Effect Transistor), an IGBT (Insulated Gate Bipolar Transistor), a FINFET (Fin Field Effect Transistor), or even a combination thereof. If the device structure 111 comprises a Schottky contact, the front-side metallization can comprise a Schottky contact metal. Additionally or alternatively, and in the absence of a Schottky contact, the front-side metallization can comprise an ohmic contact metal.
[0045] For example, the first deposited epitaxial layer 106 may be an n-doped drain or emitter layer with a thickness in the range of 10 μm to 50 μm for a power MOSFET or power diode, or a p-doped emitter layer for an IGBT. The second epitaxially deposited layer 106 may be a buffer layer that prevents punch-through of the space charge layer towards the backside emitter or drain layer. The thickness of the buffer layer may be in the range of 2 μm to 30 μm. An n-type drift zone layer 106 may be deposited by epitaxial techniques on the buffer layer, or on the n-doped drain or emitter layer if the buffer layer is omitted. The thickness of the drift zone layer depends on the targeted breakdown voltage. For 1200V devices, the thickness of the drift zone layer may be in the range of 12 μm. For 3.3 kV devices, the thickness of the drift zone layer may be in the range of 35 μm. The doping level of the drift zone layer may be adjusted according to the desired breakdown voltage. For a 1200V device, the doping level of the drift zone layer is approximately 10 × 16 cm -3For a 3.3 kV device, the doping level of the drift zone layer can be in the range of 10 × 15 cm -3 Further front side structures 111, such as p-body and n-type source regions for power MOSFETs or IGBTs, or p-emitters for power diodes, can be realised by masked ion implantation with subsequent annealing steps at high temperatures, e.g. above 1500° C. In case of switchable devices, gate structures, which can be planar or trench based, can additionally be realised.
[0046] The individual epitaxial layers 106 described above can be grown in a single epitaxial growth process, optionally with adaptation of epitaxial conditions throughout the process, or in several epitaxial processes with other intermediate processing steps. The device structures 111 can be processed until a front-side metallization and / or passivation layer is applied. Thus, after the front-side processing step (d), the substrate 108 has a front-side with the device structures 111 and possibly a front-side metallization and / or passivation layer. The back-side of the substrate 108 corresponds to the back-side of the semiconductor wafer 100. After the front-side device preparation, the entire substrate 108 comprises the semiconductor wafer 100 with the porous layer(s) 102, the epitaxial layer(s) 106 including the device structures 111, and optionally the front-side metallization and / or passivation structure.
[0047] Before the front-side carrier 112 is attached and even before the front-side metallization is deposited, the dicing streets may be porosified during the front-side device processing, e.g., by forming a vertical porous layer before the peel / separation step (f), in order to reduce, e.g., sidewall damage and kerf loss produced in conventional separation techniques (e.g., laser, mechanical) with unwanted effects.
[0048] Step (e): Front carrier 8 shows one embodiment of the substrate 108 prior to the peeling / separating step (f). A carrier 112 is attached to the front side of the substrate 108. The carrier 112 mechanically stabilizes the substrate 108 during and after the peeling / separating step (f). The carrier 112 may be attached to the front side metallization 600. Material options and dimensions of the carrier 112 are described in more detail later herein.
[0049] A further embodiment includes performing a singulation (chip separation) step (m) on already separated dies 126 supported by a front side carrier 112, prior to both the peeling / separation step (f) and the backside conditioning and metallization steps (h), (i), for example as shown in Figure 4. According to this embodiment, the permanent or temporary backside carrier or support structure 122 may be omitted.
[0050] Step (f): Peeling / Separation After device preparation, the non-porous part 110 of the semiconductor wafer 100 is peeled / separated from the remainder 108′ of the wafer 100. The porous layer(s) 102 serve as a separation initiation point where one or more cracks are induced. Therefore, no additional crack induction, for example by laser radiation, is required. However, such additional means may still be used in the final process, for example, pulsed laser radiation may be focused at a location in the porous layer(s) 102 where the laser radiation is absorbed in a linear or nonlinear absorption process, resulting in modification of the semiconductor material. Optionally, the laser absorption in the porous layer(s) 102 may be enhanced by a high doping level in the porous layer(s) 102. For example, common acceptor or donor dopants may be selected, or alternatively dopants with deep energy levels, such as vanadium (V) and / or titanium (Ti), and / or by sufficient thermal treatment of the porous layer(s) 102 to create carbon or graphene layers on the pore sidewalls in the porous layer(s) 102. Further strategies may be used to facilitate the exfoliation / separation step (f), such as proton or helium implantation into the porous layer(s) 102 to enhance pore density and / or stress at a certain depth in the porous layer(s) 102.
[0051] If there is vertical variation in hole density, e.g., due to varying hole size and hole distance, the split / separation will occur in the region where the porosified layer(s) 102 is least stable, e.g., where the hole density is highest or the hole structure allows for the easiest splitting, e.g., is weakest. If the least stable porous layer 102 is located in a deeper region of the porous layer stack, which can be helpful for defect-free epitaxial SiC growth on the skin layer, the split / separation will occur predominantly in the region of the weakest porous layer 102, and therefore some part of the porous layer 102 may remain on the backside of the wafer 100 after splitting / separation. For example, further backside conditioning may be required, as described in more detail later herein.
[0052] Typically, separation begins in the porous layer 102 or the least stable porous layer, and one or more cracks are induced through the semiconductor material, preferably along the porous layer 102 or the least stable porous layer 102. However, the crack(s) may also exit the porous layer 102 or the least stable porous layer 102 into the adjacent semiconductor material. If the crack(s) exit in the direction of the underlying semiconductor wafer 100, the damage may be removed in a later refurbishment process step. The crack(s) may also exit in the direction of the device layer. In this case, an additional crack-stop layer may be advantageous, which may be placed between the porous layer(s) 102 and the device layer. Such a crack-stop layer may be fabricated, for example, by anodization of the part of the porous layer 102 next to the device layer after the device layer has been fabricated. Such a crack-stop layer may additionally or alternatively be located on the wafer side of the porous layer(s) 102. Alternatively, the semiconductor layer (porous or non-porous) between the porous layer(s) 102 and the device layer may be selected to be thick enough to prevent the crack(s) from extending into the device layer.
[0053] An external force can be applied to the substrate 108 to induce at least one crack along the porous layer(s) 102 to separate the non-porous part 110 of the semiconductor wafer 100 from the remainder 108' of the substrate 109. Several methods can be used alone or in combination to apply the external force.
[0054] In one embodiment, the external force is applied by thermally assisted splitting. A layer, either organic-based, inorganic-based, or a combination thereof, with a different coefficient of thermal expansion (CTE) than the substrate 108 or wafer material, particularly the porous semiconductor material, is applied to the wafer 100 / substrate 108. The layer can be polymer, metal, hybrid polymer, ceramic (e.g., particularly polymer). The layer can be attached to the backside or frontside or even both sides of the substrate 108. Depending on the choice of layer, either cooling or heating can be used to generate stress across / on the wafer 100 / substrate 108 to separate the non-porous part 110 of the semiconductor wafer 100 from the remainder 108' of the substrate 108.
[0055] In another embodiment, the external force is applied by a thermal gradient. One side of the substrate 108 can be cooled. Optionally, the other side of the substrate 108 can be heated. The thermal gradient creates stress in the material that breaks along the porous layer(s) 102, which differs from the thermally assisted splitting embodiment where the stress is generated by a CTE mismatch.
[0056] In another embodiment, the external force is applied by water jets and / or air jets. Fluid-driven separation is implemented either by water (e.g., similar to ELTRAN® by Canon) or by gas. The fluid (e.g., water / gas) is applied at the edge of the substrate 108, preferably to the porous layer(s) 102.
[0057] In another embodiment, the external force is applied by laser cutting at least partially from the edge of the substrate 108. A laser can be focused from the edge of the substrate 108 to the porous layer(s) 102 such that the focal point is at the porous layer(s) 102. The laser wavelength can be selected such that the absorption is maximum in the porous layer(s) 102. The laser treatment can be combined with the absorption enhancement in the porous layer(s) described earlier herein. For example, the doping concentration of the porous layer(s) 102 can be modified such that the maximum absorption of the laser light occurs within the porous layer(s) 102.
[0058] In another embodiment, the external force is applied by pressure. Similar to the nut opening machine, but the wafer 100 must be held. For example, both sides of the substrate 108 can be fixed in a chamber and high pressure is applied to the chamber environment. A sudden (very fast) pressure release results in the formation of one or more cracks in the weakest layer, which is the porous layer(s) 102.
[0059] In another embodiment, the external force is applied by etching. The porous layer(s) 102 can be removed by an etchant, e.g., a liquid etchant. The etchant can be selected such that the etchant etches the porous semiconductor material faster (e.g., at least 10 times faster) than the non-porous semiconductor material 110. Possible etchants can be alkaline (e.g., KOH, TMAH) or fluorine-based (NH4F, HF, HBF4). Alternating etching and water rinsing, e.g., etch-rinse-dry-etch-rinse, etc., can be implemented to etch only the porous layer(s).
[0060] In another embodiment, the external force is applied by immersion in a fluid and cooling. The substrate 108 may be immersed in a fluid that has a higher volume at a lower temperature (e.g., in a frozen condensed state) than at a higher temperature (e.g., in a liquid condensed state). For example, the fluid may be water. The fluid penetrates the pores at the open edges of the substrate 108. The fluid may be cooled such that it expands and causes damage to the porous layer(s) 102. The process acts on the outer part such that a repetition of the process occurs, e.g., immersion-cooling-immersion-cooling, etc., and / or in combination with other processes.
[0061] In another embodiment, the force is applied by oxidation: via routine oxidation, etching, and rinsing of the porous layer(s) 102 in a closed loop until the surface is completely removed, e.g., oxidize-etch-rinse-dry-oxidize-etch....etc. After porosification, an oxidation process including a subsequent CMP treatment can be performed to expose the skin layer for epi growth.
[0062] In another embodiment, the external force is applied by ultrasonic vibration. For example, sound waves can be applied to the substrate 108. The waves can have a frequency in the kHz regime, for example at least 20 kHz and at most 60 kHz, for example 30-50 kHz, for example 35-45 kHz. To apply ultrasonic waves, the substrate 108 can be maintained in a container filled with a fluid, for example pure water. An ultrasonic generator for applying ultrasonic waves can be, for example, a device similar to an ultrasonic cleaning apparatus.
[0063] In another embodiment, the external force is applied by torsional stress. A torsional force is applied to one or more porous layers 102 while the substrate 108 is held in place. For example, the substrate 108 may be attached to a chuck holder, for example, by adhesive forces. The substrate 108 is then twisted to induce stress through the chuck holder relative to the wafer 100.
[0064] In another embodiment, the external force is applied by mechanical lifting: a substantially normal force is applied to one or more porous layers 102 while the substrate 108 is held in place. For example, the substrate 108 may be attached to a rigid carrier and a prying force is used to peel / separate the non-porous part 110 of the wafer 100 from the remainder 108' of the substrate 108.
[0065] In another embodiment, the external force is applied by a tensile force. A tensile force is applied to one or more porous layers 102 while the substrate 108 is held in place. For example, a chuck holder (or similar structure) may be attached to the substrate 108 by a strong adhesive. The tensile force is applied to the chuck holder and at the substrate 108. Instead of a chuck holder, tape may be used, for example, on only one side, for example, in combination with a chuck, or on both sides.
[0066] In another embodiment, the external force is applied by electromagnetic (pulsation) force. The substrate 108 can be attached (for example adhesively) to an electrode (negative or positive) and the wafer 100 has some doping level that makes the wafer 100 attracted to a certain potential. An additional electrode is placed above the wafer 100 and a high voltage is applied between the two electrodes, which thus attracts the substrate 108 to the upper electrode. The upper part of the substrate 108 is pulled away from the lower part of the substrate 108 by these forces, where the porous layer(s) 102 act as a weak point. The substrate 108 can be placed backside up or frontside up, depending on whether the device substrate 116 or the reclaimed wafer 114 should be attracted to the upper electrode. Two electrostatic chucks can be used to create a break between the porous layer(s) 102.
[0067] Step (g): Refurbishment of reclaimed wafers After the delamination / separation process (f), the reclaimed wafer 114 may be refurbished, for example, as described above with respect to the wafer preparation step (a). For example, the reclaimed wafer 114 may require conditioning (refurbishment) for epitaxial growth. Conditioning of the device substrate 116 is described in more detail later herein. An epi-ready wafer may require a surface roughness with an rms (root mean square) value of less than 50 nm, for example, less than 30 nm, for example, less than 10 nm, for example, even less than 5 nm or 1 nm.
[0068] After the peeling / separation process (f), remaining parts (e.g., remnants, residues, residual porous parts, etc.) of the porous layer(s) 102 may be present at the separation surface of the reclaimed wafer 114 and at the separation surface of the device substrate 116. Also, those surfaces may be roughened by the peeling / separation process. In addition to or instead of the general treatment options described above with respect to the wafer preparation step (a), the following optional steps may be used.
[0069] At least a part of the remaining porous part of the porous layer(s) 102 can be removed, for example, by one of the methods described above with respect to the wafer preparation step (a). The porous material can be selectively etched since, compared to non-porous materials, the porous material has a surface area that is approximately 1000 times larger due to the porous structure, and the etching rate correlates to the surface area. The parameters of the porosification can be chosen in situ such that the porous layer(s) 102 are unstable and can be peeled off or mechanically peeled off. Thermal oxidation at about 1200° C. of the porous layer(s) 102, for example, 10-20 nm, is sufficient for complete oxidation and subsequent removal of the formed oxide. The porous layer(s) 102 can also be removed by grinding / polishing. In this case, cost reduction is the main consideration, since the porous layer(s) 102 becomes much more unstable. Damage implantation and subsequent wet chemical etching, for example with HF / HNO3, can be used. This method is particularly suitable for layer thicknesses in the range of 1 μm. With the aid of deposition of a metal layer, e.g. Ti, Ni, Mo, and a temperature step, silicidation can be performed, and in a subsequent step the formed carbon and metal silicides can be removed. In general, the porous layer(s) is / are first removed by at least one of the above methods, and the surface is then smoothed / prepared, e.g. by CMP or some other surface preparation method. The thickness of the reclaimed wafer 114 can also be increased, either by depositing a monocrystalline, e.g. SiC layer, a polycrystalline, e.g. SiC layer, or a combination of monocrystalline and polycrystalline, e.g. SiC layer, on the wafer backside, e.g. as previously described herein with respect to the epitaxy step (c). Depending on the release / separation method, bevel reshaping may be required, for example grinding, sawing, plasma etching, laser ablation, EDM / ECDM (electrical (chemical) discharge machining), etc.
[0070] After the peeling / separation step (f), the device substrate 116 comprises the epitaxial layer(s) 106 including the device structures 111 and (optionally) front-side metallization and / or passivation structures. The device substrate 116 may still be attached to the front-side carrier 112, for example as shown in Figure 9. Optionally, on the back side, the device substrate 116 may comprise the porous layer(s) 102 and / or portions of the wafer 100.
[0071] The thickness of the device substrate 116 after peeling / separation can be, for example, at least 5 μm and at most 100 μm. After backside conditioning, the thickness of the device substrate 116 can be reduced even further by at least 500 nm, depending on the thickness of the remaining porous layer 102. Handling such an extremely thin device substrate is very cumbersome in the following process steps.
[0072] Step (h): Back side adjustment The backside of the device substrate 116, i.e., the side where the peeling / separation occurred, may comprise a remaining porous part of the porous layer(s) 102 and / or a remaining part of the wafer 100. The backside of the device substrate 116 may further have damage similar to that of the reclaimed wafer 114, e.g., higher surface roughness.
[0073] The remaining porous part of the porous layer(s) 102 and possibly the remaining part of the wafer 100 may be removed or at least a part of the porous layer(s) 102 may remain on the backside of the device substrate 116. In some embodiments, the processing of the device substrate 116 starts with damage removal on the backside to remove the remaining porous part of the porous layer(s) 102 and possibly the remaining part of the wafer 100. Damage removal may comprise, for example, mechanical grinding and / or chemical mechanical polishing (CMP) and / or etching or other mechanical methods such as sandblasting, water jetting, etc. At least some of the general treatment options described above with respect to the wafer preparation step (a) may be used to condition the backside of the device substrate 116. The final roughness of the backside surface may have an rms value of less than 2 μm, for example between 1 nm and 100 nm, or even less than 50 nm.
[0074] Additionally or alternatively, residual porous parts of the porous layer(s) 102 and possibly residual parts of the wafer 100 may remain at the backside of the device substrate 116. The backside of the device substrate 116 may be porosified again to create a backside porous layer. This additional porosification may be performed either with the residual porous parts of the porous layer(s) 102 and possibly residual parts of the wafer 100 still present at the backside or after removal of such residual parts. This may result in a roughened backside, e.g., rms values of more than 50 nm or more than 100 nm or more than 500 nm. The roughened backside may additionally or alternatively be created by means other than the backside porous layer, e.g., by mechanical and / or chemical treatment. The rough backside surface structure may help to achieve better ohmic contact and / or better adhesion between the (subsequently formed) backside metallization and the semiconductor material of the device substrate 116.
[0075] Step (i): Backside metallization After backside conditioning, an ohmic backside contact may be deposited and the required contact structure at the backside of the device substrate 116 may be defined. The ohmic contact may be formed by application of at least one of implantation, annealing, and metallization of the device substrate backside. All equipment used may be capable of processing wafers mounted on a frontside carrier 121 or any of the other options previously described herein for frontside processing (d).
[0076] Steps (j), (k) and (l): Backside Carrier Installation, Frontside Carrier Removal and Testing Further possibilities for ultra-thin wafer processing in the backend-of-line process (after metallization) include continuing with the front side carrier 112 and removing the front side carrier 112 only after the device substrate 116 is attached to the sawing tape. In this case, electrical testing (l) occurs prior to attachment of the front side carrier 112 or only at die level in the backend, as shown, for example, in Fig. 3. The front side carrier 112 can instead be replaced with a permanent support structure on the backside of the device substrate 116, e.g., backside carrier 112, extensive (thick) backside metallization, glass ring, according to the device geometry, as shown, for example, in Figs. 1 and 2.
[0077] Depending on the process flow, the carrier 122 may be attached to the backside of the device substrate 116. The backside carrier 122 may be removed after the testing step (l). In this case, the backside carrier 122 is a temporary carrier. Alternatively, at least a portion of the carrier 122 may remain on the backside of the device substrate 116 during further processing steps and even in the final product. In this case, the backside carrier 122 is a permanent carrier.
[0078] Depending on the choice of the front side carrier 112, the front side carrier 112 may be completely removed from the device substrate 116 before or after the test step (l), or at least a part of the front side carrier 112 may remain on the device substrate 116. This may happen, for example, if the remaining part of the front side carrier 112 does not completely cover the front surface of the device substrate 116, leaving the electrical contacts of the device structures 111 accessible for the electrical test step (l). For example, if the front side carrier 112 includes or is a grid, the electrical contacts of the device structures 111 may be accessible through openings in the grid, and the test step (l) may also be performed with the grid of the front side carrier 112 attached to the device substrate 116. The same applies for a front side carrier 112 following the shape of a ring. In such cases where a portion of the front side carrier 112 remains on the device substrate 116, the front side carrier 112 or at least a portion of the front side carrier 112 may be removed after the testing step (l) or may even remain on the device substrate 116 during the singulation step (m) and residues of the front side carrier 112 may be present in the final device. For example, the singulation step (m) is performed through the front side carrier 112. After all front side and back side processing steps have been performed, the device may undergo an electrical testing step (l). However, the testing step (l) may be performed earlier, as shown in FIG. 4.
[0079] Steps (m) and (n): Singulation and further back-end assembly After the testing step (l), the device substrate 116 is diced into individual dies (chips) 126 along so-called kerf areas of the device substrate 116. Each die 126 may comprise, for example, at least one transistor and / or diode cell. Dicing may be performed by using a mechanical saw, ultrasonic dicing, laser dicing, scribe and break, reactive ion etching, etc.
[0080] For porosification, the wafer edge (bevel) may or may not be excluded from processing. Prior to the detachment / separation step (f), proper edge connection, lateral access to the porous layer(s) 102 should be ensured by a beveling procedure, e.g., mechanical, chemical, laser or fluid-assisted beveling procedure. After the detachment / separation step (f) and when processing ultra-thin wafers, special precautions should be taken for wafer edge geometry and embedding of sensitive wafer edges (wafer bevel) throughout the process.
[0081] Carrier embodiment Each of the carriers described below can be a single material or can be a carrier system with multiple layers and / or complex structures. The front side carrier 112 and / or back side carrier 122 provide mechanical stabilization to the entire substrate 108 during and / or after processing. The shape of the carrier 112, 122 can be similar to or even equivalent to the shape of the substrate 108. In some embodiments, the carrier 112, 122 can have a diameter larger than the substrate 108, e.g., at least 0.1% larger. For example, in such an embodiment, the carrier 112, 122 can protect the bevel of the wafer 100. In other embodiments, the carrier 112, 122 can have a diameter that is at most, e.g., 80% or 90% or 100% of the diameter of the substrate 108. For example, the carrier 112, 122 in this case can be or can include a thick metal on the back side of the substrate 108. The diameter of the carriers 112, 122 may be, for example, the largest diameter, for example, in the case of asymmetric and / or non-circular carriers.
[0082] Either the carrier 112, 122, e.g. the mechanically stabilizing part of the carrier 112, 122, and / or the optional fixing layer of the carrier system, may completely cover the substrate 108, e.g. the front side or the back side, or the carrier 112, 122 may divide the covered surface into sections along the surface of the substrate 108. In the latter case, the mechanically stabilizing part of the carrier 112, 122 and / or the optional fixing layer may have the shape of a ring, a grid, and / or may be present only in the peripheral region of the substrate 108, e.g. crossed rings at the outer part of the substrate 108. The carrier 112, 122 may either be reversible or permanently bonded to the substrate.
[0083] The reversible carrier system can be an adhesive tape (heat released, UV released, solvent released), an adhesive (organic or inorganic composition) layer combined with a rigid support (e.g., transparent substrate, non-transparent substrate, polymer film), a fixed or movable electrostatic chuck, a fixed or movable vacuum chuck, a movable vacuum carrier, a magnetic based carrier.
[0084] The permanent carrier system may be attached, for example, via organic and / or inorganic adhesives (glass frits can be organic before firing and inorganic after firing), other attachment options described below. In the case of glass carriers, e.g., glass grids / rings, the permanent carrier system may be attached via solder glass or laser welding processes, which may require an additional absorbing layer between the glass carrier and the substrate 108 to allow for absorbing the laser light. The permanent carrier system may be attached via aerobic and / or anaerobic adhesives, diffusion soldering layer(s), etc. Materials for the permanent carrier system may include glass, e.g., hot embossed glass, such as in the form of glass grids, glass rings, etc., semiconductors, e.g., Si, polysilicon, SiC, poly-SiC, etc., metals, insulators, e.g., glass, etc. The shape of the permanent carrier system may be a structured support system aligned with the kerf area on the front side. Alignment with the kerf area results in alignment with some of the front side structures 11, so that subsequent processing, e.g., dicing, may be performed with the attached carrier. This occurs, for example, in the case of a grid-like structure, where the grid lines are aligned with the kerf area of the substrate (chip), one option being a glass grid. The permanent carrier system can have the shape of a glass grid and / or a ring.
[0085] The front side carrier 112 provides mechanical stabilization to the whole substrate 108 during peeling / separation and to the device substrate 116 after peeling / separation. The front side carrier 112 also protects the device structures 111 on the front side. Possible materials for the front side carrier 112 can be Si, SiC, glass, poly-SiC, ceramic, magnetic materials, polymer films. The polymer films can have a thickness of several tens of μm or even several hundreds of μm. The topography of the device structures 111 can be embedded, for example, by potting material and / or adhesive and / or non-adhesive layers between the carrier 112 and the substrate 108 or in the openings of the carrier 112, for example in the openings of a grid-shaped carrier or a ring-shaped carrier. If a (e.g., glass) grid or (e.g., glass) ring is used as the front carrier 112, and if thermally assisted splitting is used for peeling / separation, the peeling / separation may involve applying a layer on the back side of the substrate 108 and additionally on the outside of the carrier 112 facing away from the substrate 108, e.g., as in a sandwich.
[0086] The backside carrier 122 mechanically stabilizes the device substrate 116 during the test step (l) and during subsequent process steps. The backside carrier 122 may include electrical structures, e.g., contact pads to enable electrical testing. After the test step (l), the backside carrier 122 may be removed from the backside of the substrate 108 / 116 or may remain on the substrate 108 / 116. If the backside carrier 122 is removed from the substrate 108 / 116, the following carriers may be used: a ring on the peripheral area, a movable vacuum chuck, a movable electrostatic chuck, a movable GelPak chuck, a conductive tape. If the backside carrier 122 remains on the substrate 108 / 116, the following carriers may be used: the carrier 122 may comprise a conductive part, e.g., made of a metal aligned with the device on the front side. Between the conductive portions, the carrier 122 may comprise a material that can be singulated and that is aligned with a so-called kerf of the device substrate 116 where the singulation, e.g., dicing, breaking, laser machining, etc., is performed. The backside carrier 122, e.g., the conductive portions of the carrier 122, may be soldered to the backside metallization 120. After singulation, the conductive portions are still in contact with the device structures 111.
[0087] For front and back side carrier support solutions combinations of the above described embodiments may also be used, either on both sides or on one side, for example very thick back side metal combined with a ring structure or glass grid on the front side, or a glass grid may be provided on the back side and the openings filled with conductive material.
[0088] Various embodiments of the non-ablative multi-beam splitting technique, the sub-critical crack technique, and the shape change compensation technique are described herein, each of which may be used with any of the other embodiments unless otherwise specified.
[0089] While the disclosure is not so limited, the following numbered examples illustrate one or more aspects of the disclosure.
[0090] Example 1. A method of processing a semiconductor wafer, the method including forming one or more epitaxial layers on a first major surface of the semiconductor wafer; forming one or more porous layers in the semiconductor wafer or in the one or more epitaxial layers, the semiconductor wafer, the one or more epitaxial layers, and the one or more porous layers collectively forming a substrate; forming doped regions of semiconductor devices in the one or more epitaxial layers; and separating a non-porous part of the semiconductor wafer from a remainder of the substrate along the one or more porous layers after forming the doped regions of the semiconductor devices.
[0091] Example 2. The method of Example 1, wherein forming one or more porous layers comprises porosifying a semiconductor material of the semiconductor wafer or of one or more epitaxial layers.
[0092] Example 3. The method of example 2, wherein the porosifying comprises an electrochemical process using an electrolyte solution.
[0093] Example 4. The method of Example 3, wherein the electrolyte solution comprises a fluorine-based chemistry or an alkaline etch chemistry.
[0094] Example 5. The method of example 3 or 4, wherein the electrochemical process is an anodic porosification process driven by ultraviolet radiation.
[0095] Example 6. The method of any one of Examples 3 to 5, further comprising varying the current and / or voltage of the electrochemical process and / or the composition of the electrolyte solution such that the porosity of the one or more porous layers varies in a direction perpendicular to the first major surface of the semiconductor wafer.
[0096] Example 7. The method of any one of Examples 2 to 6, wherein the porosifying comprises inducing charge carriers in the semiconductor material via an electric field.
[0097] Example 8. The method of any one of Examples 2 to 7, further comprising modifying the doping concentration of the semiconductor material to be porosified prior to porosifying.
[0098] Example 9. The method of example 8, wherein modifying the doping concentration of the semiconductor material to be made porous comprises increasing the doping concentration of the semiconductor material to be made porous.
[0099] Example 10. The method of example 8 or 9, wherein modifying the doping concentration of the semiconductor material to be made porous includes adjusting one or more of implant energies, implant angles, and channeling implants.
[0100] Example 11. The method of any one of Examples 8 to 10, wherein modifying the doping concentration of the semiconductor material to be made porous comprises varying the vertical doping concentration and / or the lateral doping concentration of the semiconductor material to be made porous.
[0101] Example 12. The method of any one of Examples 1 to 11, wherein the one or more porous layers are formed in a semiconductor wafer such that the semiconductor wafer has a porous part that includes the one or more porous layers and a non-porous part that excludes the one or more porous layers.
[0102] Example 13. The method of Example 12, further comprising reusing the non-porous part of the semiconductor wafer after separating the non-porous part semiconductor wafer from the one or more epitaxial layers along the one or more porous layers.
[0103] Example 14. The method of any one of Examples 1 to 11, wherein one or more porous layers are formed in the one or more epitaxial layers, and the entire semiconductor wafer is non-porous and separated from the one or more epitaxial layers along the one or more porous layers.
[0104] Example 15. The method of Example 14, further comprising reusing the entire semiconductor wafer after separating the entire semiconductor wafer from the one or more epitaxial layers.
[0105] Example 16. The method of example 14 or 15, further comprising varying a porosification rate in the one or more porous layers by varying a dopant concentration in the one or more epitaxial layers.
[0106] Example 17. The method of any one of Examples 1 to 16, wherein forming one or more porous layers includes forming a stack of porous layers having different pore sizes in the semiconductor wafer or in one or more epitaxial layers.
[0107] Example 18. The method of example 17, wherein forming a stack of porous layers with different pore sizes comprises vertically and / or laterally varying the doping concentration of the semiconductor material to be made porous.
[0108] Example 19. The method of any one of Examples 1 to 18, further comprising varying the porosity of the one or more porous layers in a direction perpendicular to the first major surface of the semiconductor wafer.
[0109] Example 20. The method of any one of Examples 1 to 19, wherein forming the one or more porous layers includes forming a first porous layer having a first average pore density, and forming a second porous layer above the first porous layer having a second average pore density less than the first average pore density.
[0110] Example 21. The method of example 20, wherein forming one or more epitaxial layers includes forming one or more epitaxial layers on the second porous layer.
[0111] Example 22. The method of example 21, wherein the second porous layer is monocrystalline, has an average pore diameter of less than 200 nm, and has a thickness in the range of 20 nm to 500 nm.
[0112] Example 23. The method of example 21 or 22, wherein the first porous layer has a thickness in the range of 1 μm to 10 μm.
[0113] Example 24. The method of any one of Examples 20 to 23, wherein the second average pore density is such that the average distance between the pores of the second porous layer is greater than the average diameter of the pores.
[0114] Example 25. The method of any one of Examples 20 to 24, wherein the separating includes separating the non-porous part of the semiconductor wafer from the remainder of the substrate along the first porous layer.
[0115] Example 26. The method of any one of Examples 20 to 25, wherein the average doping concentration of the first porous layer is greater than the average doping concentration of the second porous layer, and the average doping concentration of the second porous layer is greater than the average doping concentration of the semiconductor wafer.
[0116] Example 27. The method of any one of Examples 20 to 26, wherein the first and second porous layers are structured and / or have varying thicknesses.
[0117] Example 28. The method of any one of Examples 20 to 27, further comprising compensating the n-type doping in the second porous layer by acceptor implantation or by implanting vanadium and / or titanium impurities.
[0118] Example 29. The method of any one of Examples 20 to 28, wherein forming a second porous layer above the first porous layer comprises forming a lightly doped epitaxial layer on the first porous layer, forming a mask on the lightly doped epitaxial layer, and injecting dopants into the lightly doped epitaxial layer through openings in the mask and at an electric field intensity that induces hole formation in regions of the lightly doped epitaxial layer aligned with the openings in the mask.
[0119] Example 30. The method of any one of Examples 20 to 29, wherein forming the one or more porous layers further comprises forming an additional porous layer below the first porous layer and having an average pore density less than the first average pore density.
[0120] Example 31. The method of any one of Examples 20 to 30, wherein forming the one or more porous layers further comprises forming an additional porous layer between the first porous layer and the second porous layer and having an average pore density less than the first average pore density and greater than the second average pore density.
[0121] Example 32. The method of any one of Examples 1 to 31, wherein forming the one or more porous layers includes forming a low conductivity epitaxial layer, low conductivity wafer region, or low conductivity buried wafer region induced by implantation of a dopant providing counterdoping, forming a higher conductivity layer on the low conductivity epitaxial layer, low conductivity wafer region, or low conductivity buried wafer region having a higher average doping concentration than the low conductivity epitaxial layer, low conductivity wafer region, or low conductivity buried wafer region, and forming a homogeneous porous layer in the higher conductivity layer.
[0122] Example 33. The method of example 32, wherein the thickness variation of the homogeneous porous layer is less than ±1 μm.
[0123] Example 34. The method of any one of Examples 1 to 33, wherein forming the one or more porous layers includes forming a mask on the epitaxial layer or on the first major surface of the semiconductor wafer, injecting dopants through openings in the mask, and applying an electric field to the regions where the dopants are implanted to accelerate vertical porosification.
[0124] Example 35. The method of any one of Examples 1 to 34, wherein forming the one or more epitaxial layers includes forming a first epitaxial layer by epitaxial lateral overgrowth of pores in an uppermost one of the one or more porous layers.
[0125] Example 36. The method of example 35, wherein the first epitaxial layer has a lateral dopant concentration that varies based on pore location in an uppermost one of the one or more porous layers.
[0126] Example 37. The method of example 35 or 36, wherein forming a doped region of a semiconductor device in one or more epitaxial layers includes forming a drain or emitter layer above the first epitaxial layer, forming a buffer layer on the drain or emitter layer, and forming a drift layer on the buffer layer.
[0127] Example 38. The method of Example 37, wherein the drain layer or emitter layer has a thickness in the range of 10 μm to 50 μm, the buffer layer has a thickness in the range of 2 μm to 30 μm, and the drift layer has a thickness in the range of 12 μm to 35 μm.
[0128] Example 39. The method of any one of Examples 1 to 38, wherein the semiconductor device is a power transistor device.
[0129] Example 40. The method of any one of Examples 1 to 39, further comprising forming metallization and / or passivation on the one or more epitaxial layers.
[0130] Example 41. The method of any one of Examples 1 to 40, further comprising singulating the substrate into a plurality of dies.
[0131] Example 42. The method of example 41, wherein singulating is performed after separating.
[0132] Example 43. The method of example 41 or 42, further comprising attaching a carrier to a side of the substrate opposite the non-porous part of the semiconductor wafer prior to separating, the carrier remaining attached to the substrate during separating.
[0133] Example 44. The method of example 43, wherein singulating is performed before both separating and attaching the carrier.
[0134] Example 45. The method of example 43 or 44, further comprising testing the semiconductor device on a side of the substrate opposite the non-porous part of the semiconductor wafer prior to attaching the carrier.
[0135] Example 46. The method of any one of Examples 41 to 46, further comprising, prior to the separating, forming a first metallization on a first side of the substrate opposite the non-porous part of the semiconductor wafer, and, after the separating, forming a second metallization on a second side of the substrate exposed by the separating and opposite the first side.
[0136] Example 47. The method of any one of Examples 40 to 46, further comprising, prior to singulating, porosifying dicing streets along which the substrate is to be singulated.
[0137] Example 48. The method of example 47, wherein porosifying the dicing streets is performed prior to separating.
[0138] Example 49. The method of any one of Examples 40 to 48, further comprising, prior to separating, attaching a first carrier to a first side of the substrate opposite the non-porous part of the semiconductor wafer, and, after separating, forming a metallization on a second side of the substrate exposed by separating and opposite the first side, attaching a second carrier to the metallization, and, after attaching the second carrier, removing the first carrier.
[0139] Example 50. The method of any one of Examples 1 to 49, further comprising inducing one or more cracks that extend at least partially through the one or more porous layers to aid in the separation.
[0140] Example 51. The method of example 50, wherein inducing one or more cracks comprises irradiating the one or more porous layers with laser light.
[0141] Example 52. The method of example 50 or 51, wherein inducing one or more cracks comprises applying an external force.
[0142] Example 53. The method of example 52, wherein applying an external force includes applying a layer to the substrate having a different thermal expansion coefficient than the one or more porous layers, and cooling or heating the layer.
[0143] Example 54. The method of example 53, wherein the layer is a polymer, a metal, a hybrid polymer, or a ceramic.
[0144] Example 55. The method of any one of Examples 52 to 54, wherein applying an external force includes applying a thermal gradient across the substrate.
[0145] Example 56. The method of any one of Examples 52 to 55, wherein applying an external force includes applying a fluid to the one or more porous layers from a side of the substrate.
[0146] Example 57. The method of any one of Examples 52 to 56, wherein applying an external force comprises applying laser light to the one or more porous layers from the side of the substrate.
[0147] Example 58. The method of Example 57, further comprising modifying the doping concentration of the one or more porous layers such that maximum absorption of the laser light occurs within the one or more porous layers.
[0148] Example 59. The method of any one of Examples 52 to 58, wherein applying the external force includes clamping the substrate in the chamber on an opposite side of the substrate and applying pressure to the chamber environment while the substrate is clamped in the chamber.
[0149] Example 60. The method of any one of Examples 52 to 59, wherein applying an external force includes etching the one or more porous layers.
[0150] Example 61. The method of example 60, wherein the etching is performed with an etchant that etches the one or more porous layers at least 10 times faster than non-porous parts of the semiconductor wafer.
[0151] Example 62. The method of example 61, wherein the etchant is alkaline or fluorine-based.
[0152] Example 63. The method of any one of Examples 52 to 62, wherein applying an external force includes alternating between etching and rinsing the one or more porous layers.
[0153] Example 64. The method of any one of Examples 52 to 63, wherein applying an external force includes immersing the substrate in a fluid having a higher volume at a lower temperature and a lower volume at a higher temperature, where the fluid penetrates into pores in the one or more porous layers at the edge of the substrate, cooling the fluid such that the fluid expands and damages the one or more porous layers in the region of the edge of the substrate, and repeating the immersion and cooling until a non-porous part of the semiconductor wafer is removed from the remainder of the substrate.
[0154] Example 65. The method of any one of Examples 52 to 64, wherein applying the external force includes oxidizing parts of the one or more porous layers, etching the oxidized parts of the one or more porous layers, rinsing the etched parts of the one or more porous layers, and repeating the oxidizing, etching, and rinsing until a non-porous part of the semiconductor wafer is removed from a remainder of the substrate.
[0155] Example 66. The method of any one of Examples 52 to 65, wherein applying an external force comprises applying ultrasonic vibrations to the one or more porous layers.
[0156] Example 67. The method of example 66, wherein the substrate is in a container filled with liquid during the application of ultrasonic vibrations.
[0157] Example 68. The method of example 66 or 67, wherein the ultrasonic vibrations are applied within a frequency range of 20 kHz to 60 kHz.
[0158] Example 69. The method of any one of Examples 52 to 68, wherein applying an external force includes applying a torsional force to the one or more porous layers while the substrate is held in place.
[0159] Example 70. The method of any one of Examples 52 to 69, wherein applying an external force includes applying a substantially normal force to the one or more porous layers while the substrate is held in place.
[0160] Example 71. The method of any one of Examples 52 to 70, wherein applying an external force includes applying a tensile force to the one or more porous layers while the substrate is held in place.
[0161] Example 72. The method of any one of Examples 52 to 71, wherein applying an external force includes applying an electromagnetic force to the substrate.
[0162] Example 73. The method of example 72, wherein the electromagnetic force is applied to the substrate by a first electrostatic chuck disposed adjacent to a first side of the substrate and a second electrostatic chuck disposed adjacent to a second side of the substrate opposite the first side.
[0163] Example 74. The method of any one of Examples 1 to 73, further comprising forming one or more carbon and / or graphene layers on pore sidewalls in the one or more porous layers prior to isolating.
[0164] Example 75. The method of Example 74, wherein forming the one or more carbon layers and / or graphene layers comprises heat treating the one or more porous layers.
[0165] Example 76. The method of any one of Examples 1 to 75, further comprising injecting protons and / or helium into the one or more porous layers prior to isolating.
[0166] Example 77. The method of any one of Examples 1 to 76, further comprising forming a crack-stopping layer between the one or more porous layers and the device layer of the one or more epitaxial layers prior to separating.
[0167] Example 78. The method of Example 77, wherein forming the crack-stopping layer comprises performing anodization of the porous layer closest to the device layer after forming the device layer.
[0168] Example 79. The method of any one of Examples 1 to 78, further comprising forming a crack-stopping layer between the one or more porous layers and a non-porous part of the semiconductor wafer prior to separating.
[0169] Example 80. The method of example 79, wherein forming a crack-stop layer includes performing anodization of the porous layer closest to the semiconductor wafer.
[0170] Example 81. The method of any one of Examples 1 to 80, wherein the thickness of the remainder of the substrate after separating is in the range of 5 μm to 100 μm.
[0171] Example 82. The method of any one of Examples 1 to 81, further comprising removing the remaining porous part from the remainder of the substrate after the separating.
[0172] Example 83. The method of Example 82, wherein removing the remaining porous part from the remainder of the substrate comprises mechanically grinding and / or chemical-mechanical polishing and / or etching and / or sandblasting and / or water-jetting a surface of the remaining substrate defined by separation from the non-porous part of the semiconductor wafer.
[0173] Example 84. The method of Example 82 or 83, wherein the surface of the remainder of the substrate defined by separation from the non-porous part of the semiconductor wafer has an rms (root-mean-square) surface roughness of less than 2 μm after removing the remaining porous part from the remainder of the substrate.
[0174] Example 85. The method of example 84, wherein the rms surface roughness is in the range of 1 nm to 100 nm.
[0175] Example 86 The method of any one of Examples 82 to 85, further comprising porosifying the remaining side of the substrate from which the remaining porous part was previously removed.
[0176] Example 87. The method of example 86, further comprising forming metallization on the porosified side of the remainder of the substrate.
[0177] Example 88. The method of any one of Examples 1 to 87, further comprising, after separating, porosifying a side of the remainder of the substrate defined by separating it from the non-porous part of the semiconductor wafer.
[0178] Example 89. The method of example 88, further comprising forming metallization on the porosified side of the remainder of the substrate.
[0179] Terms such as "first", "second", etc. are used to describe and are not limiting of various elements, regions, sections, etc. Like terms refer to like elements throughout the description.
[0180] As used herein, terms such as "having," "containing," "including," "comprising," and the like are open-ended terms indicating the presence of stated elements or features, but do not exclude additional elements or features. The articles "a," "an," and "the" are intended to include the plural as well as the singular, unless the context clearly indicates otherwise.
[0181] Although specific embodiments have been shown and described herein, those skilled in the art will appreciate that various alternative and / or equivalent implementations may be substituted for the specific embodiments shown and described without departing from the scope of the present invention. This application is intended to cover any adaptations or variations of the specific embodiments described herein. Accordingly, it is intended that the present invention be limited only by the claims and their equivalents.
Claims
1. 1. A method for processing a semiconductor wafer, the method comprising: forming one or more epitaxial layers over a first major surface of the semiconductor wafer; forming one or more porous layers in the semiconductor wafer or in the one or more epitaxial layers, the semiconductor wafer, the one or more epitaxial layers, and the one or more porous layers collectively forming a substrate; forming a doped region of a semiconductor device in the one or more epitaxial layers; separating a non-porous part of the semiconductor wafer from a remainder of the substrate along the one or more porous layers after forming the doped regions of the semiconductor device; A method comprising:
2. and forming the one or more porous layers comprises porosifying a semiconductor material of the semiconductor wafer or of the one or more epitaxial layers, the porosifying comprising an electrochemical process using an electrolyte solution, the method comprising: Varying the current and / or voltage of the electrochemical process and / or the composition of the electrolyte solution such that the porosity of the one or more porous layers is varied in a direction perpendicular to the first major surface of the semiconductor wafer. The method of claim 1 further comprising:
3. forming the one or more porous layers comprises porosifying a semiconductor material of the semiconductor wafer or of the one or more epitaxial layers, the method comprising: modifying the doping concentration of the semiconductor material to be made porous prior to said making porous. The method of claim 1 further comprising:
4. The method of claim 3 , wherein modifying the doping concentration of the semiconductor material to be made porosity comprises increasing the doping concentration of the semiconductor material to be made porosity.
5. 2. The method of claim 1, wherein the one or more porous layers are formed in the semiconductor wafer such that the semiconductor wafer has a porous part that includes the one or more porous layers and a non-porous part that excludes the one or more porous layers.
6. reusing the non-porous part of the semiconductor wafer after separating the non-porous part semiconductor wafer from the one or more epitaxial layers along the one or more porous layers. The method of claim 5 further comprising:
7. 10. The method of claim 1 , wherein the one or more porous layers are formed in the one or more epitaxial layers, and the entire semiconductor wafer is non-porous and separated from the one or more epitaxial layers along the one or more porous layers.
8. Reusing the entire semiconductor wafer after separating the entire semiconductor wafer from the one or more epitaxial layers. The method of claim 7 further comprising:
9. 10. The method of claim 1 , wherein forming the one or more porous layers comprises forming a stack of porous layers having different pore sizes in the semiconductor wafer or in the one or more epitaxial layers.
10. forming the one or more porous layers forming a first porous layer having a first average pore density; forming a second porous layer above the first porous layer, the second porous layer having a second average pore density less than the first average pore density; Including, The method of claim 1 , wherein the first and second porous layers are structured and / or have varying thicknesses.
11. forming the one or more porous layers forming a low conductivity epitaxial layer, a low conductivity wafer region, or a low conductivity buried wafer region induced by implantation of a dopant providing counterdoping; forming a higher conductivity layer on the low conductivity epitaxial layer, the low conductivity wafer region, or the low conductivity buried wafer region, the higher conductivity layer having a higher average doping concentration than the low conductivity epitaxial layer, the low conductivity wafer region, or the low conductivity buried wafer region; forming a homogeneous porous layer in said more conductive layer; The method of claim 1 , comprising:
12. forming the one or more porous layers forming a mask on an epitaxial layer or on the first major surface of the semiconductor wafer; implanting dopants through openings in the mask; applying an electric field to the dopant-implanted region to accelerate vertical porosification; The method of claim 1 , comprising:
13. forming the one or more epitaxial layers forming a first epitaxial layer by epitaxial lateral overgrowth of pores in an uppermost one of said one or more porous layers; The method of claim 1 , comprising:
14. The method of claim 13 , wherein the first epitaxial layer has a lateral dopant concentration that varies based on pore location in the uppermost one of the one or more porous layers.
15. Singulating the substrate into a plurality of dies. Further comprising: The method of claim 1 , wherein the singulating is performed after the separating.
16. Singulating the substrate into a plurality of dies; attaching a carrier to a side of the substrate opposite the non-porous portion of the semiconductor wafer prior to said separating. Further comprising: The method of claim 1 , wherein the carrier remains attached to the substrate during the separating.
17. The method of claim 16 , wherein said singulating is performed before both said separating and said attaching said carrier.
18. Singulating the substrate into a plurality of dies; forming a first metallization on a first side of the substrate opposite the non-porous part of the semiconductor wafer prior to said separating; forming a second metallization on a second side of the substrate exposed by said separating and opposite the first side after said separating; The method of claim 1 further comprising:
19. inducing one or more cracks extending at least partially through said one or more porous layers to assist in said separating. Further comprising: The method of claim 1 , wherein said inducing said one or more cracks comprises irradiating said one or more porous layers with laser light.
20. inducing one or more cracks extending at least partially through said one or more porous layers to assist in said separating. Further comprising: The method of claim 1 , wherein the inducing the one or more cracks comprises applying an external force.
21. applying the external force applying a layer to the substrate having a different coefficient of thermal expansion than the one or more porous layers; cooling or heating said layer; 21. The method of claim 20, comprising:
22. applying the external force applying a thermal gradient across said substrate; 21. The method of claim 20, comprising:
23. applying the external force applying laser light to the one or more porous layers from the side of the substrate; 21. The method of claim 20, comprising:
24. modifying the doping concentration of said one or more porous layers such that maximum absorption of said laser light occurs within said one or more porous layers.
24. The method of claim 23, further comprising:
25. applying the external force applying ultrasonic vibrations to said one or more porous layers.
21. The method of claim 20, comprising:
26. 26. The method of claim 25, wherein the substrate is in a liquid-filled container during the applying of the ultrasonic vibrations.
27. removing the remaining porous part from the remainder of the substrate after said separating. The method of claim 1 further comprising:
28. removing the remaining porous part from the remainder of the substrate; mechanically grinding and / or chemical-mechanical polishing and / or etching and / or sandblasting and / or water-blasting the surface of the remaining portion of the substrate defined by said separation from the non-porous part of the semiconductor wafer.
28. The method of claim 27, comprising:
29. porosifying the remaining side of the substrate from which the remaining porous part was previously removed.
28. The method of claim 27, further comprising:
30. forming a metallization on the porous side of the remainder of the substrate; 30. The method of claim 29, further comprising:
Citation Information
Patent Citations
Method for manufacturing, use and utilizing method of semiconductor wafer
JP2000349264A
Three dimensional porous structure and manufacturing method thereof
JP2006108366A
Process and apparatus for producing SOI substrate
JP2009302405A
Formation of semiconductor device in silicon carbide
JP2019176142A
Semiconductor device with a porous portion, wafer composite and method of manufacturing a semiconductor device
US20200286730A1