AI device cell with improved phase change material domain
By integrating undoped or nitrogen-doped GST layers as a buffer between doped GST and heater/top metal, the oxidation issues in AI device cells are mitigated, ensuring thermal stability and resistance in PCM cells.
Patent Information
- Application Number
- JP2024501272
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-09-24
- Filing Date
- 2022-08-11
- Publication Date
- 2024-10-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Certain phase change materials (PCM) like doped germanium-antimony-tellurium (GST) can cause oxidation issues affecting heaters and top metals within artificial intelligence device cells.
Incorporating a buffer layer of undoped or nitrogen-doped GST layers between the doped GST layer and the heater and top metal to prevent oxidation, using silicon dioxide-doped GST layers to isolate the doped GST layer, thereby maintaining thermal stability and resistance.
The solution prevents oxidation of heaters and top metals, enhancing thermal stability and resistance drift while reducing moisture damage in PCM cells.
Smart Images

Figure 2024536667000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to artificial intelligence, and more particularly to artificial intelligence device cells. Artificial intelligence devices use phase change materials (PCMs) in cells that store information. For example, the phase of the PCM can be changed or altered to represent a change in the stored state or information of the artificial intelligence device. However, some PCM materials (e.g., doped germanium-antimony-tellurium (GST)) can cause problems for other elements of the cell. For example, oxygen from doped GST can adversely affect the heater or top metal in the cell. Summary of the Invention
[0002] According to one embodiment, an apparatus includes a heater, a phase change material region, and a top metal layer. The phase change material region includes a doped GST layer and a first GST layer. The first GST layer is between the doped GST layer and the heater, and the doped GST layer is doped differently than the first GST layer. The phase change material region is located between the heater and the top metal layer. Other embodiments include methods for configuring the apparatus.
[0003] According to another embodiment, an apparatus includes a heater and a phase change material region including a doped GST layer disposed over a first GST layer, the first GST layer being between the doped GST layer and the heater, the doped GST layer being differently doped than the first GST layer. Other embodiments include methods for configuring the apparatus. [Brief description of the drawings]
[0004] [Figure 1] FIG. 1 is a diagram illustrating an example of a system.
[0005] [Diagram 2] FIG. 2 is a diagram for explaining an example of a PCM cell in the system of FIG.
[0006] [Diagram 3] 3 is a diagram illustrating an example of a PCM area in the PCM cell of FIG. 2.
[0007] [Figure 4] 3 is a flow chart illustrating an example of a method for forming the PCM cell of FIG. 2.
[0008] [Figure 5A] 3A-3C are diagrams illustrating the steps of forming the PCM cell of FIG. 2.
[0009] [Figure 5B] 3A-3C are diagrams illustrating the steps of forming the PCM cell of FIG. 2.
[0010] [Figure 5C] 3A-3C are diagrams illustrating the steps of forming the PCM cell of FIG. 2.
[0011] [Figure 5D] 3A-3C are diagrams illustrating the steps of forming the PCM cell of FIG. 2.
[0012] [Figure 5E] 3A-3C are diagrams illustrating the steps of forming the PCM cell of FIG. 2.
[0013] [Figure 5F] 3A-3C are diagrams illustrating the steps of forming the PCM cell of FIG. 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] The present disclosure contemplates an artificial intelligence device cell with a phase change material (PCM) region, which includes a buffer layer that separates a doped germanium-antimony-tellurium (GST) layer from a heater and a top metal in the cell. For example, a GST layer may be formed above and below a doped GST layer such that the GST layer is between the doped GST layer and the heater and the top metal. The doped GST layer may be doped differently than the other GST layers. For example, the doped GST layer may be doped with silicon dioxide, and the other GST layers are undoped or doped with nitrogen or another dopant that does not include oxygen. As a result, the GST layer may, in certain embodiments, prevent the doped GST layer from oxidizing and adversely affecting the heater and the top metal.
[0015] 1 illustrates an example of a system 100. The system 100 may be a computing system including a processor 102 and a memory 104. The processor 102 and the memory 104 may implement an artificial intelligence device that uses PCM to store state or information. The processor 102 and the memory 104 perform the functions or operations of the computing system described herein.
[0016] The processor 102 is any electronic circuit, including, but not limited to, one or a combination of a microprocessor, a microcontroller, an application specific integrated circuit (ASIC), an application specific instruction set processor (ASIP), and / or a state machine that is communicatively coupled to the memory 104 and controls the operation of the computing system. The processor 102 may be 8-bit, 16-bit, 32-bit, 64-bit, or any other suitable architecture. The processor 102 may include an arithmetic logic unit (ALU) for performing arithmetic and logical operations, processor registers for providing operands to the ALU and storing results of the ALU operations, and a control unit for retrieving instructions from memory and executing the instructions by managing the cooperation of the ALU, registers, and other elements. The processor 102 may include other hardware that runs software that controls and processes information. The processor 102 executes software stored in the memory 104 to perform any of the functions described herein. The processor 102 processes information (e.g., information received from the memory 104) to control the operation and running of the computing system. The processor 102 is not limited to a single processing device, but may encompass multiple processing devices.
[0017] The memory 104 may store data, operational software, or other information for the processor 102, either permanently or temporarily. The memory 104 may include any one or combination of volatile or non-volatile local or remote devices suitable for storing information. For example, the memory 104 may include a random access memory (RAM), a read-only memory (ROM), a magnetic storage device, an optical storage device, or any other suitable information storage device, or a combination of these devices. Software represents any suitable set of instructions, logic, or code embodied in a computer-readable storage medium. For example, the software may be embodied in the memory 104, a disk, a CD, or a flash drive. In certain embodiments, the software may include applications executable by the processor 102 to perform one or more of the functions described herein.
[0018] The system 100 includes (e.g., as part of the memory 104) a PCM cell 106, which may also be referred to as a phase change memory cell. In a particular embodiment, the PCM cell 106 is part of the memory 104. The PCM cell 106 includes a PCM that changes phase based on an amount of heat applied to the PCM (e.g., by applying a voltage or current to a heating element connected to the PCM). The phase of the PCM cell 106 may be used to represent a state or information of an artificial intelligence device. For example, one or more PCM cells 106 may be used to store different states of a neural network. As another example, one or more PCM cells 106 may be used to store values of nodes of a graph or tree. The phase of one or more PCM cells 106 may be adjusted to represent changes in the neural network, graph, or tree. A notable difference between the PCM cell 106 and a conventional memory is that the PCM cell 106 may not be limited to storing binary states (e.g., 0 or 1). Rather, the phase of the PCM cell 106 can be used to represent a number of different states.
[0019] The processor 102 and memory 104 implement the machine learning model 108 using PCM cells 106. For example, the machine learning model 108 can use the PCM cells 106 to store state information. As the state information changes (e.g., during training of the machine learning model 108), the phase of the PCM cells 106 is adjusted to represent the change in state information. With enough PCM cells 106, the PCM cells 106 can store the machine learning model 108.
[0020] Figure 2 illustrates an example of a PCM cell 106 in the system 100 of Figure 1. The PCM region 218 of the PCM cell 106 includes another layer that protects other elements within the PCM cell 106 from oxidation. As a result, the PCM cell 106 has improved thermal stability, improved resistance drift, and reduced oxidation in certain embodiments. Additionally, the PCM cell 106 may not be susceptible to moisture damage.
[0021] The PCM cell 106 includes a substrate 202 that serves as a base for the PCM cell 106. The substrate 202 may include any suitable material (e.g., silicon, metal oxide, or gallium arsenide). The pads 204, 206, and 208 are formed in the substrate 202. The pads 204, 206, and 208 may include any suitable conductive material. The pads 204, 206, and 208 conduct current to and from other elements of the PCM cell 106 that are connected to the pads 204, 206, and 208. A dielectric 209 is disposed over the substrate 202. The dielectric 209 may include any suitable insulating material (e.g., silicon nitride). The dielectric 209 may cover the substrate 202 and the pads 204, 206, and 208.
[0022] The dielectric 209 has one or more heaters formed therein. In the example of FIG. 2, the dielectric 209 has heaters 210 and 212 formed therein, each extending through the dielectric 209 to the pads 206 and 208. The heaters 210 and 212 connect to the pads 206 and 208 such that current can be conducted from the pads 206 and 208 to the heaters 210 and 212. The heaters 210 and 212 may include multiple layers of resistive material. For example, the heaters 210 and 212 may include alternating layers of titanium nitride and tantalum nitride. In some embodiments, the heaters 210 and 212 may include alternating layers of low resistance material and high resistance material. The heaters 210 and 212 generate heat when current is applied to the heaters 210 and 212 from the pads 206 and 208. Adjusting the amount of current applied to heaters 210 and 212 adjusts the amount of heat produced by heaters 210 and 212. For example, increasing the current applied to heaters 210 and 212 increases the amount of heat produced by heaters 210 and 212. As another example, decreasing the current applied to heaters 210 and 212 decreases the heat produced by heaters 210 and 212. In some embodiments, the width of heaters 210 and 212 is less than or equal to 40 nanometers.
[0023] In some embodiments, liners 214 and 216 are formed (e.g., by deposition) over the heaters 210 and 212. The liners 214 and 216 may include a resistive material that improves resistance drift of the PCM cell 106. The liners 214 and 216 are optional, and some embodiments of the PCM cell 106 do not include the liners 214 and 216.
[0024] A PCM region 218 is formed over the dielectric 209 and the heaters 210 and 212. The PCM region 218 includes a PCM and a protective layer. In the example of FIG. 2, the PCM region 218 includes a GST layer 220 formed (e.g., by deposition) over the dielectric 209. In an embodiment including the liners 214 and 216, the GST layer 220 is formed such that the liners 214 and 216 are in the GST layer 220. The PCM region 218 also includes a doped GST layer 222 formed (e.g., by deposition) over the GST layer 220. The doped GST layer 222 may include GST that is doped using any suitable material, such as silicon dioxide. Additionally, another GST layer 224 is formed (e.g., by deposition) over the doped GST layer 222. The doped GST layer 222 may be doped differently than the GST layers 220 and 224. For example, doped GST layer 222 may be doped with silicon dioxide, and GST layers 220 and 224 are undoped or doped with nitrogen or another dopant that does not include oxygen. As a result, GST layers 220 and 224 protect other elements of PCM cell 106 from oxidation caused by doped GST layer 222 (e.g., deposition of doped GST layer 222). In some embodiments, GST layers 220 and 224 and doped GST layer 222 are formed in one chamber during the manufacturing process.
[0025] The thickness of doped GST layer 222 may be greater than the thickness of GST layers 220 and 224. For example, doped GST layer 222 may be 80 nanometers thick, and GST layers 220 and 224 may each be 1-5 nanometers thick. In some embodiments, doped GST layer 222 is at least 10 times thicker than GST layers 220 and 224. Thus, GST layers 220 and 224 are thick enough to block oxygen from doped GST layer 222, but not so thick as to affect the resistance of doped GST layer 222.
[0026] When pads 206 and 208 apply current to heaters 210 and 212, heaters 210 and 212 generate heat. The heat is transferred to PCM region 218, causing doped GST layer 222 to change phase. By adjusting the current applied to heaters 210 and 212, the amount of heat applied to doped GST layer 222 is adjusted. Thus, the phase of doped GST layer 222 is changed and controlled. GST layers 220 and 224 protect heaters 210 and 212, liners 214 and 216 (if present), and top metal 226 from oxidation caused by doped GST layer 222.
[0027] A top metal layer 226 is formed (e.g., by deposition) on GST layer 224. Further, a mask 228 is formed (e.g., by deposition) on top metal 226. Since doped GST layer 222 is doped differently than GST layers 220 and 224, GST layers 220 and 224 protect heaters 210 and 212 and top metal 226 from oxidation caused by doped GST layer 222.
[0028] Contacts 230 and 232 are formed in the PCM cell 106 such that electrical connection can be made to the pad 204, the top metal 226, and the mask 228. In the example of FIG. 2, contact 230 is formed from the top of the PCM cell 106 to the mask 228. Contact 230 allows electrical connection to be made to the mask 228 and the top metal 226. Contact 232 is formed from the top of the PCM cell 106 to the pad 204. Contact 232 allows electrical connection to be made to the pad 204. In some embodiments, contacts 230 and 232 are formed through an interlevel dielectric that is separate from dielectric 209. The interlevel dielectric may include any suitable insulating material.
[0029] Some embodiments of the PCM cell 106 include different structures of the PCM region 218. FIG. 3 illustrates an example of a PCM region 302 that may be implemented in the PCM cell 106 of FIG. 2. As seen in FIG. 3, the PCM region 302 includes multiple layers of alternating GST and doped GST. As in the example of FIG. 2, the doped GST layer is doped differently than the other GST layers. For example, the doped GST layer may be doped with silicon dioxide, while the other GST layers are undoped or doped with nitrogen or another dopant that does not include oxygen. The PCM region 302 includes a GST layer 304 at the bottom of the PCM region 302. A doped GST layer 306 is formed on the GST layer 304. Another GST layer 308 is formed on the doped GST layer 306. Another doped GST layer 310 is formed on the GST layer 308. A GST layer 312 is formed on top of the doped GST layer 310. A further doped GST layer 314 is formed on top of the GST layer 312, and a GST layer 316 is formed on top of the doped GST layer 314. The PCM region 302 may include any suitable number of layers of GST and doped GST.
[0030] Figure 4 is a flow chart illustrating an example method 400 for forming the PCM cell 106 of Figure 2. In a particular embodiment, a semiconductor manufacturing machine or worker performs the method 400. Performing the method 400 forms the PCM cell 106, including the protective layer.
[0031] In block 402, a heater 210 is formed on a pad 206. The pad 206 may be formed in a substrate 202 that serves as a base for the PCM cell 106. The heater 210 may include multiple layers of resistive material. A current may be applied from the pad 206 to the heater 210 to generate heat in the heater 210.
[0032] In block 404, a GST layer 220 is formed over the heater 210. For example, the GST layer 220 may be deposited over the heater 210. In some embodiments, a liner 214 is formed over the heater 210 prior to forming the GST layer 220 over the heater 210. In these embodiments, the liner 214 is located in the GST layer 220 after the GST layer 220 is formed over the heater 210.
[0033] At block 406, a doped GST layer 222 is formed on the GST layer 220. For example, the doped GST layer 222 may be deposited on the GST layer 220. The doped GST layer 222 may include GST that is doped with any suitable material (e.g., silicon dioxide or nitrogen). Then, at block 408, another GST layer 224 is formed on the doped GST layer 222. In certain embodiments, the GST layer 220, the doped GST layer 222, and the GST layer 224 may all be deposited in one chamber of a semiconductor manufacturing process.
[0034] In block 410, a top metal 226 is formed on the GST layer 224. In some embodiments, a mask 228 is then formed on the top metal 226. In block 412, a contact 230 is formed above the top metal 226. In some embodiments, the contact 230 is formed on the mask 228 that is formed on the top metal 226. The contact 230 allows for an electrical connection to be made to the top metal 226.
[0035] In some embodiments, doped GST layer 222 is significantly thicker than GST layers 220 and 224. For example, doped GST layer 222 may be 80 nanometers thick, while GST layers 220 and 224 are 1-5 nanometers thick. In some embodiments, doped GST layer 222 is at least 10 times thicker than GST layers 220 and 224. As a result, GST layers 220 and 224 protect heater 210 and top metal 226 from oxidation caused by doped GST layer 222. Furthermore, GST layers 220 and 224 do not significantly affect the resistance of doped GST layer 222.
[0036] 5A-5F illustrate the steps of forming the PCM cell 106 of FIG. 2. As seen in FIG. 5A, a dielectric 209 is formed on a substrate 202. Pads 204, 206, and 208 are formed in the substrate 202. The substrate 202 may include any suitable material, such as silicon, a metal oxide, or gallium arsenide. The dielectric 209 may include any suitable insulating material. In some embodiments, the dielectric 209 has a thickness of about 50 nanometers.
[0037] Heaters 210 and 212 are then formed through dielectric 209. As seen in FIG. 5B, heaters 210 and 212 are formed through dielectric 209 into pads 206 and 208, respectively. Heaters 210 and 212 may include alternating layers of resistive material. Upon application of current to heaters 210 and 212 through pads 206 and 208, heaters 210 and 212 generate heat. Liners 214 and 216 are then formed over heaters 210 and 212, as seen in FIG. 5C. Liners 214 and 216 may be deposited over heaters 210 and 212. Additionally, liners 214 and 216 are formed over dielectric 209. Liners 214 and 216 are optional, and in some embodiments, liners 214 and 216 are not included.
[0038] A PCM region 218 is then formed on the dielectric 209. As seen in FIG. 5D, the PCM region 218 is formed on the dielectric 209 above the heaters 210 and 212. In embodiments including liners 214 and 216, the liners 214 and 216 are located in the PCM region 218 after the PCM region 218 is formed. Additionally, the PCM region 218 includes a GST layer 220 formed (e.g., by deposition) on the dielectric 209. A doped GST layer 222 is formed (e.g., by deposition) on the GST layer 220, and a GST layer 224 is formed (e.g., by deposition) on the doped GST layer 222. The thickness of the doped GST layer 222 may be significantly greater than the thicknesses of the GST layers 220 and 224. In some embodiments, the doped GST layer 222 is at least 10 times thicker than the GST layers 220 and 224. When a current is applied to the heaters 210 and 212 such that they generate heat, the heat changes the phase of the doped GST layer 222. The amount of heat produced by the heaters 210 and 212 may be adjusted to adjust the phase of the doped GST layer 222.
[0039] Then, as seen in FIG. 5E, a top metal 226 is formed on the GST layer 224. Then, a mask 228 is formed on the top metal 226. In a particular embodiment, the GST layers 220 and 224 protect the heaters 210 and 212 and the top metal 226 from oxidation caused by the doped GST layer 222. In other words, the GST layers 220 and 224 prevent oxygen in the doped GST layer 222 from propagating to the heaters 210 and 212 and the top metal 226. As a result, in a particular embodiment, the GST layers 220 and 224 prevent adverse effects on the heaters 210 and 212 and the top metal 226. Then, as seen in FIG. 5F, contacts 230 and 232 are formed. The contacts 230 are formed to the mask 228 such that the contacts 230 allow electrical connections to be made to the mask 228 and the top metal 226. Contacts 232 are formed to pads 204 such that contacts 232 allow electrical connection to be made to pads 204 .
[0040] In summary, the artificial intelligence device cell includes a PCM region 218 that includes a buffer layer that separates the doped GST layer 222 from the heater 210 and the top metal 226. For example, the GST layers 220 and 224 may be formed above and below the doped GST layer 222 such that the GST layers 220 and 224 are located between the doped GST layer 222 and the heater 210 and the top metal 226. As a result, the GST layers 220 and 224 can, in certain embodiments, prevent the doped GST layer 222 from oxidizing and adversely affecting the heater 210 and the top metal 226.
[0041] The description of various embodiments of the present invention is presented for illustrative purposes, and the description is not intended to be exhaustive or limited to the disclosed embodiments. Many changes and modifications that do not depart from the scope of the present invention will be apparent to those skilled in the art. The terminology used in this specification is selected to best explain the principles of the present invention, practical applications, or technical improvements in science and technology found in the market, or to enable those skilled in the art to understand the embodiments disclosed in this specification.
[0042] In the foregoing, reference has been made to the embodiments presented in this disclosure. However, the scope of the present invention is not limited to the specific embodiments described. Instead, any combination of these features and elements, whether associated with different embodiments or not, is contemplated to realize and implement the contemplated embodiments. Furthermore, while the embodiments disclosed herein may realize advantages over other possible solutions or prior art, whether or not a particular advantage is realized by a given embodiment does not limit the scope of the present invention. Thus, the aspects, features, embodiments, and advantages described herein are merely exemplary and should not be considered elements or limitations of the appended claims unless expressly recited in the claims. Similarly, references to "the present invention" should not be construed as a generalization of any of the inventive subject matter disclosed herein, and should not be considered elements or limitations of the appended claims unless expressly recited in the claims.
[0043] While the forgoing is directed to embodiments of the present invention, other embodiments may be devised without departing from the basic scope of the invention, the scope of which is determined by the claims which follow.
[0044] In the preferred embodiment of the present invention described above, there is provided a device comprising a phase change material region including a heater; and a doped GST layer disposed on a first GST layer, where the first GST layer is between the doped GST layer and the heater, and the doped GST layer has a different doping than the first GST layer. The device preferably further comprises a liner located on the heater. The phase change material region preferably further comprises a second GST layer, where the doped GST layer is between the first GST layer and the second GST layer, and the doped GST layer has a different doping than the second GST layer. The phase change material region may further comprise a second doped GST layer and a third GST layer, where the second doped GST layer is between the second GST layer and the third GST layer, and the second doped GST layer has a different doping than the second and third GST layers.
Claims
1. heater; a phase change material region having a doped germanium-antimony-tellurium (GST) layer and a first GST layer, where the first GST layer is between the doped GST layer and the heater, and the doped GST layer is doped differently than the first GST layer; and a top metal layer, where the phase change material region is located between the heater and the top metal layer. An apparatus comprising:
2. The apparatus of claim 1 further comprising a liner overlying the heater.
3. The apparatus of claim 2 , wherein the liner is located within the first GST layer.
4. The device of claim 1 , wherein the doped GST layer is at least 10 times thicker than the first GST layer.
5. 2. The device of claim 1 , wherein the phase change material region further comprises a second GST layer, the doped GST layer being between the first GST layer and the second GST layer, the doped GST layer being differently doped than the second GST layer.
6. 6. The device of claim 5, wherein the phase change material region further comprises a second doped GST layer and a third GST layer, the second doped GST layer being located between the second GST layer and the third GST layer, the second doped GST layer being differently doped than the second GST layer and the third GST layer.
7. The device of claim 1 further comprising a contact, the top metal layer being between the contact and the phase change material region.
8. The apparatus of claim 1 , wherein the heater is formed in a dielectric and the phase change material region is located above the dielectric.
9. forming a heater on the pad; forming a phase change material region over the heater, the phase change material region having a doped GST layer and a first GST layer, the first GST layer being between the doped GST layer and the heater, the doped GST layer being differently doped than the first GST layer; and forming an upper metal layer over the phase change material region; A method for providing the above.
10. The method of claim 9 , further comprising forming a liner over the heater prior to forming the phase change material region.
11. The method of claim 10 , wherein after forming the phase change material region, the liner is located in the first GST layer.
12. The method of claim 9 , wherein the doped GST layer is at least 10 times thicker than the first GST layer.
13. 10. The method of claim 9, wherein the phase change material region further comprises a second GST layer, the doped GST layer being between the first GST layer and the second GST layer, the doped GST layer being differently doped than the second GST layer.
14. 14. The method of claim 13, wherein the phase change material region further comprises a second doped GST layer and a third GST layer, the second doped GST layer being located between the second GST layer and the third GST layer, the second doped GST layer being differently doped than the second GST layer and the third GST layer.
15. 10. The method of claim 9, further comprising forming a contact, the top metal layer being between the contact and the phase change material region.
16. The method of claim 9 , wherein the heater is formed in a dielectric and the phase change material region is located above the dielectric.
Citation Information
Patent Citations
Multi-level programmable pcram memory
US20090180314A1
Integrated circuit including memory element doped with dielectric material
US20090237983A1
Multiple phase change materials in an integrated circuit for system on a chip application
US20150214479A1
Phase change memory having a composite memory element
US20170263863A1
Phase change memory using multiple stacks of PCM materials
WO2021161117A1