Method for producing bis(pyrrolidino)butane in the liquid phase
The described process for producing BPB using a copper-aluminum catalyst in a liquid phase reactor addresses the challenges of high conversions and selectivity, ensuring stable and efficient production of BPB.
Patent Information
- Application Number
- JP2024520912
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-05-18
- Filing Date
- 2022-09-30
- Publication Date
- 2024-10-09
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing methods for producing bis(pyrrolidino)butane (BPB) face challenges in achieving high conversions, high yields, and high selectivity while maintaining catalyst stability and minimizing runaway risks.
A process involving the reaction of pyrrolidine (PYR) with hydrogen in the presence of a catalyst comprising oxygen-containing compounds of copper and aluminum, optionally with zirconium, in a liquid phase, using a fixed bed reactor, and optimizing conditions such as temperature, pressure, and molar ratios to enhance conversion and selectivity.
The process achieves high molar conversions and selectivity of BPB, with improved stability and safety, allowing for efficient production of BPB with reduced catalyst degradation risks.
Smart Images

Figure 2024536947000001 
Figure 2024536947000002 
Figure 2024536947000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a process for the production of bis(pyrrolidino)butane (BPB), which comprises the reaction of pyrrolidine (PYR) in the presence of hydrogen, a catalyst, and optionally 1,4-butanediol (BDO) in the liquid phase. [Background technology]
[0002] WO 2021 / 011521 A1 (Huntsman) teaches polyurethane formulations that include bis(pyrrolidino)butane as a catalyst.
[0003] US 2007 / 0232833 A1 (BASF AG) relates to a process for the preparation of amines by reaction in the gas phase of a primary alcohol with hydrogen and nitrogen compounds in the presence of a catalyst comprising an oxygen-containing compound of aluminum and / or zirconium and an oxygen-containing compound of copper.
[0004] US 2011 / 0172430 A1 (BASF SE) relates to a process for the preparation of amines by reaction in the gas phase of primary alcohols with hydrogen and nitrogen compounds in the presence of a catalyst comprising an oxygen-containing compound of aluminum and copper.
[0005] US 2010 / 0056364 A1 (BASF AG) relates to catalysts for the hydrogenation of carbonyl groups, such catalysts including oxygen-containing compounds of aluminum, copper and lanthanum, as well as metallic copper and graphite.
[0006] US 2014 / 0018547 A1 (BASF SE) describes a process for preparing pyrrolidine by reacting 1,4-butanediol (BDO) with ammonia in the presence of hydrogen and a supported metal-containing catalyst, the catalytically active mass of the catalyst before its reduction with hydrogen containing oxygen-containing compounds of aluminum, copper, nickel and cobalt, and oxygen-containing compounds of tin, calculated as SnO, in the range of 0.2-5.0 wt.%, and the reaction is carried out in a liquid.
[0007] US 2011 / 0137030 A1 (BASF SE) relates to a process for preparing amines by reacting primary or secondary alcohols, aldehydes and / or ketones with hydrogen and a nitrogen compound selected from the group consisting of ammonia and primary and secondary amines in the presence of a supported copper-, nickel- and cobalt-containing catalyst, the catalytically active material of the catalyst before its reduction with hydrogen comprises oxygen compounds of aluminum, copper, nickel and cobalt and 0.2-5.0% by weight of oxygen compounds of tin, calculated as SnO. The reaction of 1,4-butanediol with pyrrolidine is not taught therein.
[0008] Timofeev et al. (Russian Journal of Organic Chemistry, 2016, Vol. 52) teach the production of bis(pyrrolidino)butane as a by-product obtained by the reaction of 1,4-butanediol with ammonia in the presence of a nickel / copper / chromium catalyst.
[0009] Ballantine et al. (Journal of Molecular Catalysis, 30 (1985) 373-388) teach the use of ion-exchanged montmorillonite as a catalyst to react pyrrolidine to give ring-opened products such as bis(pyrrolidino)butane. Summary of the Invention [Problem to be solved by the invention]
[0010] The technical problem that the present invention aims to solve was to find a new process for the preparation of bis(pyrrolidino)butane. The intention was to find a process which could be carried out with high conversion, high yield, including space-time yield, and high selectivity, while at the same time having high mechanical stability of the catalyst molding and a low "runaway risk". [Means for solving the problem]
[0011] The above technical problem can be solved by the method according to claim 1.
[0012] Any catalyst having hydration activity can be used for the preparation of bis(pyrrolidino)butane. Preferably, the catalytically active mass of the catalyst before its reduction with hydrogen comprises an oxygen-containing compound of copper and an oxygen-containing compound of aluminum and / or zirconium. In this regard, it was surprising that the use of such a catalyst is suitable for the preparation of bis(pyrrolidino)butane (BPB) based on the reaction of pyrrolidine (PYR) in the presence of hydrogen. According to US 2007 / 0232833 A1, US 2011 / 0172430 A1, US 2011 / 0137030 A1 and US 2014 / 0018547 A1, these catalysts are suitable for the amination of alcohols, aldehydes and ketones, respectively, or for the hydrogenation of carbonyl groups in the case of US 2010 / 0056364 A1. There is no suggestion in these documents that the respective catalysts are suitable for the reaction of pyrrolidine according to the present invention. Similarly, Ballantine et al. (Journal of Molecular Catalysis, 30 (1985) 373-388) teach a particular ion-exchanged montmorillonite for use in catalyzing the reaction of pyrrolidine. There is also no suggestion that other catalysts, particularly those taught in the art referenced above, may function similarly. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] Bis(pyrrolidino)butane or 1,4-di(pyrrolidin-1-yl)butane has the following formula: [ka] It is also called "BPB".
[0014] Without wishing to be bound by any theory or in any way limit the scope of the invention, the reaction of PYR according to the present invention occurs according to the following reaction scheme (Scheme 1).
[0015] Scheme 1: Preparation of bis(pyrrolidino)butane (BPB) from pyrrolidine (PYR). [ka] In the first step, two pyrrolidine molecules react to give 4-(pyrrolidin-1-yl)butan-1-amine. In the next step, 4-(pyrrolidin-1-yl)butan-1-amine reacts with another pyrrolidine molecule to produce BPB and release ammonia. In addition, bis(4-(pyrrolidinyl)butyl)amine can be produced as an unwanted by-product, which has the formula: [ka]
[0016] Optionally, the reaction can be carried out in the presence of BDO. This means that the reaction can be carried out without or in the presence of BDO. Carrying out the reaction in the absence of BDO means that BDO is not actively added. The possibility that trace amounts of BDO are present, for example in the ppm range or less, as a contaminant contained in PYR, cannot be excluded. Preferably, the reaction according to the present invention is carried out in the presence of 1,4-butanediol (BDO).
[0017] Without wishing to be bound by any theory or in any way limit the scope of the present invention, the reaction of PYR in the presence of BDO according to the present invention occurs according to the following reaction scheme (Scheme 2).
[0018] Scheme 2: Preparation of bis(pyrrolidino)butane (BPB) from butanediol (BDO) and pyrrolidine (PYR). [ka] In the first step, PYR reacts with BDO to produce 4-(pyrrolidin-1-yl)butan-1-ol and release water. In the next step, 4-(pyrrolidin-1-yl)butan-1-ol reacts with another pyrrolidine molecule to produce BPB and release water. In addition, bis(4-(pyrrolidinyl)butyl)amine can be produced as an unwanted by-product.
[0019] In the presence of BDO, PYR can react primarily via both Scheme 1 and Scheme 2. The choice of which scheme to use depends on the reaction conditions, including but not limited to the conversion of BDO and the molar ratio of BDO to PYR. However, it is believed that in most cases, the formation of BPB occurs primarily according to Scheme 2. This is especially true with respect to the preferred reaction conditions set forth herein.
[0020] The water generated during the reaction process outlined in Scheme 2 above generally does not have a destructive effect on conversion, reaction rate, selectivity, and catalyst life, and is therefore conveniently removed only during work-up of the reaction product, e.g., by distillation.
[0021] According to the present invention, the reaction of PYR (alone or in the presence of BDO) is carried out in the presence of a heterogeneous catalyst (catalyst). Preferably, the catalytic active mass before its reduction with hydrogen comprises an oxygen-containing compound of copper and an oxygen-containing compound of aluminum and / or zirconium. Specific embodiments of such catalysts are detailed below. Unless otherwise stated, such heterogeneous catalysts are simply referred to as "catalysts".
[0022] In accordance with the present invention, the reaction of PYR (either alone or in the presence of BDO) is carried out in the presence of hydrogen. The main purpose of hydrogen in either reaction (i.e., PYR alone or in the presence of BDO) is to maintain catalyst activity during operation.
[0023] The catalyst is preferably arranged as a fixed bed in a reactor, especially for continuous processes. Suitable reactors for continuous or discontinuous operation ("batch") are described in more detail below.
[0024] The PYR can be used as a solution, for example as an aqueous solution, in particular as an aqueous solution having a strength of 75 to 95% by weight, or without a solvent. Very particularly, the PYR is solvent-free (preferred purity is 95 to 100% strength by weight, in particular 98 to 100% strength by weight).
[0025] The BDO can be used as a solution, for example as an aqueous solution, in particular as an aqueous solution with a concentration of 75-95% by weight, or without a solvent. Very particularly, the BDO is solvent-free (preferred purity is 95-100% by weight, in particular 98-100% by weight).
[0026] The process can be carried out continuously or discontinuously, with a continuous process being preferred.
[0027] The process can be carried out in one or more reactors. Suitable reactors for continuous and discontinuous processes are outlined below.
[0028] PYR and, where applicable, BDO are used as starting materials.
[0029] The reaction is carried out in the liquid phase, which means that PYR and, if applicable, BDO are reacted in the liquid phase. In the case of a continuous process, PYR and, if applicable, BDO are preferably fed simultaneously to the reactor. The preferred reaction conditions are detailed below. Depending on the environment (e.g. weather conditions), it may be advantageous to use heat tracing to avoid the formation of solids in the starting materials and / or products.
[0030] In a batch process (i.e., a discontinuous process), PYR and, if applicable, BDO are added to a reactor. The catalyst is preferably used in an amount of 0.1-10 parts by weight per 100 parts by weight of PYR or, if applicable, BDO. Hydrogen is added until the desired reaction pressure (defined further below) is achieved. Preferably, the batch reaction is carried out in a stirred tank reactor. In the case of the reaction of PYR without BDO, the reaction is preferably carried out in a stirred tank reactor in which the evolved ammonia is continuously removed from the reactor.
[0031] Preferably, the continuous reaction is carried out in a tubular reactor, a reactor with external or internal recirculation, a plug flow reactor or a spray reactor. In a preferred embodiment, the conversion is carried out in a tubular reactor. It is also possible to use a tube bundle reactor or a single-stream plant. In a single-stream plant, the tubular reactor can consist of several individual tubular reactors connected in series.
[0032] Reaction conditions: Unless otherwise stated, the reaction conditions specified below refer to both types of reactions, i.e., without BDO and in the presence of BDO.
[0033] It has been found that selectivity can be improved if the reaction is carried out at a significantly higher temperature, for example the reaction is carried out at a temperature above 170°C, preferably at least 180°C, more preferably at least 188°C, even more preferably at least 189°C, particularly preferably at least 195°C, or even at least 198°C.
[0034] In a preferred embodiment, the reaction is carried out at a temperature in the range of 180 to 300°C, more preferably 180 to 230°C, even more preferably 180 to 220°C, particularly preferably 180 to 210°C, or even 180 to 200°C.
[0035] In a more preferred embodiment, the reaction is carried out at a temperature in the range of 188 to 230°C, more preferably 188 to 220°C, even more preferably 188 to 210°C, and particularly preferably 188 to 200°C.
[0036] In an even more preferred embodiment, the reaction is carried out at a temperature in the range of 190 to 230°C, more preferably 190 to 220°C, even more preferably 190 to 210°C, and particularly preferably 190 to 200°C.
[0037] In a particularly preferred embodiment, the reaction is carried out at a temperature in the range of 195 to 230°C, more preferably 195 to 220°C, even more preferably 195 to 210°C, and particularly preferably 195 to 200°C.
[0038] In a very particularly preferred embodiment, the reaction is carried out at a temperature in the range from 198 to 230°C, more preferably from 198 to 220°C, even more preferably from 198 to 210°C and particularly preferably from 198 to 200°C.
[0039] The reaction can be carried out adiabatically, isothermally, or quasi-isothermally (i.e., isothermally). Preferably, in each case, the temperature in the reactor is within the respective range according to the preceding paragraph.
[0040] It has been found that selectivity can be improved if the reaction pressure is fairly low, for example below 150 bar. In this application all pressures refer to absolute pressures. Preferably, the reaction is carried out at an absolute pressure below 150 bar, even more preferably below 149 bar.
[0041] In a preferred embodiment, the reaction is carried out at an absolute pressure in the range of 20 to 150 bar (for example 45 to 150 bar or 55 to 150 bar), preferably 65 to 149 bar, more preferably 70 to 140 bar, even more preferably 75 to 130 bar, particularly preferably 80 to 130 bar. The process according to the invention provides high selectivity even in the case of low pressures, for example 50 bar or 60 bar. Thus, in another preferred embodiment, the reaction is carried out at an absolute pressure in the range of 20 to 130 bar, preferably 50 to 130 bar, more preferably 55 to 100 bar, even more preferably 55 to 90 bar.
[0042] All pressures are stated in the unit "bar" and can be converted to "Pa", "hPa", or "MPa" (1 bar = 100,000 Pa = 1000 hPa = 0.1 MPa).
[0043] When the reaction is carried out in the presence of BDO, the molar conversion of BDO is usually at least 90%, preferably at least 95%, more preferably at least 98%, particularly preferably at least 99% or even 100%.
[0044] When the reaction is carried out without BDO, the molar conversion of PYR is usually 60% or more, preferably 60 to 90%, and more preferably in the range of 60 to 100%.
[0045] Conversion rate refers to the molar amount of BDO or PYR consumed during condensation. The respective conversion rates can be adjusted by selecting appropriate reaction conditions as known to those skilled in the art. Such reaction conditions include, but are not limited to, reaction temperature and reaction pressure.
[0046] When the reaction is carried out in the presence of BDO, the molar ratio of PYR to BDO is preferably at least 1.5: 1. It is understood that the molar ratio refers to the molecules (not their functional groups) prior to the reaction.
[0047] It has been found that a molar ratio of PYR to BDO of 2:1 or greater, and even more preferably greater than 2:1, can improve selectivity. For example, the molar ratio of PYR to BDO is in the range of 2:1 to 10:1. Preferably, the molar ratio of PYR to BDO is greater than 2:1 to 10:1, more preferably greater than 2:1 to 9:1, even more preferably greater than 2:1 to 6:1, particularly preferably greater than 2:1 to 4:1, or even greater than 2:1 to 3:1.
[0048] For continuous processes in which the reaction is carried out in the presence of BDO, the process is typically carried out at a liquid hourly space velocity over the catalyst of 0.05-5, preferably 0.1-2, more preferably 0.2-1 kg BDO / (L catalyst This is done in .h). catalyst means the bulk volume of the catalyst in the reactor.
[0049] For continuous processes where the reaction is carried out in the absence of BDO, the process is carried out at a liquid hourly space velocity over the catalyst of 0.05 to 5, preferably 0.1 to 2, more preferably 0.2 to 1 or 0.15 to 0.8 kg PYR / (L catalyst This is done within the scope of .h).
[0050] When the reaction is carried out in the presence of BDO, the amount of hydrogen is, for example, 65 to 181 NL, preferably 70 to 150 NL, more preferably 80 to 130 NL, even more preferably 85 to 120 NL, particularly preferably 85 to 110 NL, or even 85 to 100 NL per mole of BDO.
[0051] NL means standard liter, i.e. liter (of hydrogen molecules) under standard conditions (STP). Standard conditions are understood as follows: Standard pressure = 101325 Pa = 1013.25 hPa = 101.325 kPa = 1.01325 bar. Standard temperature=273.15K=0℃.
[0052] Considering the above definition of NL, the above ranges can be converted to the molar amount of hydrogen per mole of BDO. Thus, the molar ratio of hydrogen to BDO is, for example, 2.9 to 8.1, preferably 3.1 to 6.7, more preferably 3.6 to 5.8, even more preferably 3.8 to 5.4, particularly preferably 3.8 to 4.9, or even 3.8 to 4.5.
[0053] When the reaction is carried out without BDO, the amount of hydrogen is, for example, 20-150NL, preferably 20-140NL per mole of PYR, and thus the molar ratio of hydrogen to PYR is, for example, 0.9-6.7, preferably 0.9-6.3.
[0054] catalyst: Preferred embodiments of the catalysts used in the process according to the invention are detailed below.
[0055] The catalytically active mass of the catalyst after its final heat treatment and before its reduction with hydrogen is defined as the sum of the masses of the catalytically active components. Such components include, in particular, oxygen-containing compounds of the respective metals. Oxide support materials, such as aluminum oxide (Al2O3), are considered to be included in the catalytically active material. The catalyst is preferably used in the form of a catalyst consisting only of the catalytically active material and, if appropriate, a shaping aid (e.g. graphite or stearic acid) if the catalyst is used as a shaped body, i.e. without further catalytically active components. It should be noted that in any description of the composition of the catalytically active mass defined herein, the term "before its reduction with hydrogen" means that the final heat treatment has been carried out.
[0056] In a preferred embodiment, the catalytically active mass of the catalyst before its reduction with hydrogen comprises oxygen-containing compounds of copper, oxygen-containing compounds of aluminum and / or zirconium, and at least one oxide selected from the group consisting of oxygen-containing compounds of nickel, cobalt, tin, molybdenum and lanthanum.
[0057] In another preferred embodiment, the catalytically active mass of the catalyst prior to its reduction with hydrogen comprises oxygen-containing compounds of copper and oxygen-containing compounds of aluminum.
[0058] In yet another preferred embodiment, the catalytically active mass of the catalyst prior to its reduction with hydrogen comprises oxygen-containing compounds of copper and nickel and oxygen-containing compounds of aluminum and / or zirconium, with the oxygen-containing compounds of aluminum being preferred.
[0059] In yet another preferred embodiment, the catalytically active mass of the catalyst prior to its reduction with hydrogen comprises oxygen-containing compounds of copper, nickel and cobalt and oxygen-containing compounds of aluminum and / or zirconium, with the oxygen-containing compounds of aluminum being preferred.
[0060] In yet another preferred embodiment, the catalytically active mass of the catalyst prior to its reduction with hydrogen comprises oxygen-containing compounds of copper, oxygen-containing compounds of aluminum, and at least one oxide selected from the group consisting of oxygen-containing compounds of nickel, cobalt, tin, molybdenum, and lanthanum.
[0061] Unless otherwise specified, in each case the reported concentrations (wt %) of the catalyst components relate to the catalytically active mass of the as-prepared catalyst after its final heat treatment and before its reduction with hydrogen.
[0062] In yet another preferred embodiment, the catalytically active mass of the catalyst before its reduction with hydrogen further comprises oxygen-containing compounds of copper, oxygen-containing compounds of aluminum and / or zirconium and optionally at least one oxide selected from the group consisting of oxygen-containing compounds of nickel, cobalt, tin, molybdenum and lanthanum, provided that the sum of the catalytically active mass of said compounds, calculated as CuO, ZrO2 and / or Al2O3 and, if applicable, NiO, CoO, SnO, MoO3 and / or La2O3, is 50-100% by weight, preferably 70-100% by weight, particularly preferably 80-100% by weight, more preferably 90-100% by weight and very particularly preferably 95-100% by weight.
[0063] In yet another preferred embodiment, the catalytically active mass of the catalyst prior to its reduction with hydrogen comprises oxygen-containing compounds of aluminum, copper, nickel and cobalt, and 0.2 to 5.0 wt. % oxygen-containing compounds of tin, calculated as SnO.
[0064] For example, the catalytic activity mass of the catalyst, prior to reduction with hydrogen, is in the range of 15 to 80 wt.%, in particular 30 to 70 wt.%, more particularly 35 to 65 wt.%, of an oxygen-containing compound of aluminum, calculated as Al2O3; 1-20 wt. %, in particular 2-18 wt. %, more particularly 5-15 wt. % of oxygen-containing compounds of copper, calculated as CuO; 5-35 wt.%, in particular 10-30 wt.%, more particularly 12-28 wt.%, very particularly 15-25 wt.% of oxygen-containing compounds of nickel, calculated as NiO; 5-35 wt.%, in particular 10-30 wt.%, more particularly 12-28 wt.%, very particularly 15-25 wt.% of oxygen-containing compounds of cobalt, calculated as CoO; %. Preferably used is the catalyst disclosed in WO 2011 / 067199 A1 (BASF SE), which comprises 0.2 to 5.0 wt. %, in particular 0.4 to 4.0 wt. %, more particularly 0.6 to 3.0 wt. %, more particularly 0.7 to 2.5 wt. % of oxygen-containing compounds of tin, calculated as SnO.
[0065] The catalytically active mass of such a catalyst after its final heat treatment and before its reduction with hydrogen is defined as the sum of the masses of the catalytically active components and essentially comprises oxygen-containing compounds of the following components: aluminium, copper, nickel, cobalt and tin.
[0066] The sum of the above-mentioned components of the catalytically active composition is usually 70 to 100 wt%, preferably 80 to 100 wt%, more preferably 90 to 100 wt%, in particular more than 95 wt%, very particularly more than 98 wt%, in particular more than 99 wt%, for example particularly preferably 100 wt%.
[0067] In this catalyst, the nickel to copper molar ratio is preferably greater than 1, more preferably greater than 1.2, and even more preferably in the range of 1.8 to 8.5.
[0068] The BET specific surface area (ISO 9277:1995) of the catalyst is preferably 30 to 250 m 2 / g range, especially 90-200m 2 / g range, more specifically 130-190m 2 / g (in each case before reduction with hydrogen). These ranges are achieved in particular at calcination temperatures during catalyst preparation in the range of 400°C to 600°C, in particular in the range of 420°C to 550°C.
[0069] In particular, the catalysts disclosed, for example, in Example 5, pages 28 and 29 of WO 2011 / 067199 A1 may be employed.
[0070] For example, in another particular embodiment, the catalytic activity mass of the catalyst prior to its reduction with hydrogen is: % by weight, preferably 20 to 65% by weight, more preferably 22 to 40% by weight, of oxygen-containing compounds of zirconium, calculated as ZrO2; % by weight, particularly preferably 2 to 25 wt. % of oxygen-containing compounds of copper, calculated as CuO; % by weight, preferably 15 to 50% by weight, more preferably 21 to 45% by weight, of oxygen-containing compounds of nickel, calculated as NiO, with a nickel to copper molar ratio of more than 1, in particular more than 1.2, and very particularly preferably 1.8 to 8.5, being preferred; The catalysts disclosed in EP 696 572 A1 (BASF SE) which contain 0-5 wt. %, in particular 0.1-3 wt. %, of oxygen-containing compounds of molybdenum, calculated as MoO3, are also preferably used.
[0071] In particular, the catalyst disclosed for example in EP 696 572 A1, page 8, has the composition 31.5 wt. % ZrO2, 50 wt. % NiO, 17 wt. % CuO and 1.5 wt. % MoO3.
[0072] The catalytically active mass of the catalyst after its final heat treatment and before its reduction with hydrogen is defined as the sum of the masses of the catalytically active components and essentially comprises oxygen-containing compounds of the following components: zirconium, copper, nickel and molybdenum.
[0073] The sum of the above-mentioned components of the catalytically active composition is usually 70 to 100 wt%, preferably 80 to 100 wt%, more preferably 90 to 100 wt%, in particular more than 95 wt%, very particularly more than 98 wt%, in particular more than 99 wt%, for example particularly preferably 100 wt%.
[0074] For example, in another particular embodiment, the catalytic active mass prior to its reduction with hydrogen is: 20 to 75% by weight of aluminum oxide, calculated as Al2O3; 20 to 75% by weight of oxygen-containing compounds of copper, calculated as CuO; 0-2% by weight of oxygen-containing compounds of sodium, calculated as Na2O; The catalysts disclosed in WO 2010 / 031719 A1 (BASF SE) which contain less than 5% by weight of oxygen-containing compounds of nickel, calculated as NiO, are preferably used.
[0075] The catalytically active composition of such a catalyst after its final heat treatment and before its reduction with hydrogen is defined as the sum of the catalytically active components and the catalyst support material described above, and is comprised of the following components: It essentially comprises aluminum oxide (Al2O3), an oxygen-containing compound of copper, if applicable an oxygen-containing compound of nickel, and preferably an oxygen-containing compound of sodium.
[0076] The sum of the abovementioned components of the catalytically active composition, calculated as Al2O3, CuO, NiO (if applicable) and Na2O, is usually between 70 and 100% by weight, preferably between 80 and 100% by weight, particularly preferably between 90 and 100% by weight, more preferably between 98 and 100% by weight, more preferably 99% by weight and very particularly preferably 100% by weight.
[0077] The catalytically active composition of the catalyst used in the process according to the invention after its final heat treatment and before its reduction with hydrogen comprises 20 to 75% by weight, preferably 25 to 65% by weight and particularly preferably 30 to 55% by weight of aluminium oxide (Al2O3), 20 to 75% by weight, preferably 30 to 70% by weight, particularly preferably 40 to 65% by weight and very particularly preferably 45 to 60% by weight of oxygen-containing compounds of copper, calculated as CuO, 0 to 2% by weight, preferably 0.05 to 1% by weight and particularly preferably 0.1 to 0.5% by weight of oxygen-containing compounds of sodium, calculated as Na2O and less than 5% by weight, for example 0.1 to 4% by weight, preferably less than 1% by weight, for example 0 to 0.8% by weight of oxygen-containing compounds of nickel, calculated as NiO.
[0078] For example, in another preferred embodiment, the catalytically active mass prior to its reduction with hydrogen is 20-85% by weight of aluminum oxide (Al2O3) and / or zirconium dioxide (ZrO2), 1-70% by weight of oxygen-containing compounds of copper calculated as CuO, 0-50% by weight of oxygen-containing compounds of magnesium calculated as MgO, oxygen-containing compounds of chromium calculated as Cr2O3, oxygen-containing compounds of zinc calculated as ZnO, oxygen-containing compounds of barium calculated as BaO, and / or oxygen-containing compounds of calcium calculated as CaO, The catalysts disclosed in DE 10 2004 023 529 A1 (BASF SE) which contain 0 to 30% by weight of oxygen-containing compounds of nickel, calculated as NiO, are preferably used.
[0079] The catalytically active composition of the catalyst after its final heat treatment and before its reduction with hydrogen is defined as the sum of the catalytically active components and the catalyst support material described above, and is comprised of the following components: It consists essentially of aluminum oxide (Al2O3), and / or zirconium dioxide (ZrO2), and oxygen-containing compounds of copper, and optionally oxygen-containing compounds of magnesium, and / or oxygen-containing compounds of chromium, and / or oxygen-containing compounds of zinc, and / or oxygen-containing compounds of barium, and / or oxygen-containing compounds of calcium, and optionally oxygen-containing compounds of nickel, the amount of these oxygen-containing compounds of nickel, calculated as NiO, being 0-30% by weight.
[0080] The sum of the abovementioned components of the catalytically active composition, calculated as Al2O3, ZrO2, CuO, MgO, Cr2O3, ZnO, BaO, CaO and NiO, is usually between 70 and 100% by weight, preferably between 80 and 100% by weight, particularly preferably between 90 and 100% by weight and very particularly preferably 100% by weight.
[0081] The catalytic activity composition of the catalyst after its final heat treatment and before its reduction with hydrogen is 20 to 85% by weight, preferably 25 to 80% by weight, particularly preferably 30 to 75% by weight of aluminum oxide (Al2O3) and / or zirconium dioxide (ZrO2), 1 to 70% by weight, preferably 2 to 65% by weight, particularly preferably 5 to 60% by weight and very particularly preferably 20 to 60% by weight of oxygen-containing compounds of copper, calculated as CuO, 0 to 50% by weight, preferably 0 to 30% by weight, particularly preferably 0 to 20% by weight, of oxygen-containing compounds of magnesium, calculated as MgO, and / or oxygen-containing compounds of chromium, calculated as Cr2O3, and / or oxygen-containing compounds of zinc, calculated as ZnO, and / or oxygen-containing compounds of barium, calculated as BaO, and / or oxygen-containing compounds of calcium, calculated as CaO, %.
[0082] In the above embodiment, aluminum oxide (Al2O3) is preferred.
[0083] For example, in another preferred embodiment, the catalyst prior to its reduction with hydrogen is (1) An oxide material, (a) 50-80 wt. % of oxygen-containing compounds of copper, calculated as CuO; (b) 15-35 wt. % oxygen-containing compounds of aluminum, calculated as Al2O3; (c) 2 to 20 wt. % of an oxygen-containing compound of lanthanum, calculated as La2O3; an oxide material, the total weight percent of which is the sum of oxygen-containing compounds of copper, aluminum, and lanthanum, is in the range of 80 to 100 wt%; (2) Graphite and at least one compound selected from the group consisting of metallic copper powder, copper foil, cement powder, and mixtures thereof; Including, (2) is present in an amount of 1 to 40% by weight based on the total weight of the oxide material, provided that the graphite is present in an amount of 0.5 to 5% by weight based on the total weight of the oxide material; The total content of (1) and (2) is at least 95% by weight of the catalyst; The catalysts disclosed in US 2010 / 0056364 A1 (BASF SE) are preferably used.
[0084] The composition of the oxide material is based on the total weight of the oxide material after its final heat treatment (ie, calcination) and before its reduction with hydrogen.
[0085] For such catalysts, reference is made to the (heterogeneous) catalyst rather than to its catalytically active mass, since the definition also includes graphite, which, unlike oxygen-containing compounds of copper, aluminum, lanthanum and metallic copper, does not constitute a catalytically active material.
[0086] Preferably, the catalyst prior to its reduction with hydrogen is (1) An oxide material, (a) 55-75 wt. % oxygen-containing compounds of copper, calculated as CuO; (b) 20-30 wt. % of oxygen-containing compounds of aluminum, calculated as Al2O3; (c) 3 to 15 wt. % of an oxygen-containing compound of lanthanum, calculated as La2O3; an oxide material, the total weight percent of which is the sum of oxygen-containing compounds of copper, aluminum, and lanthanum, is in the range of 95 to 100 wt%; (2) Graphite and at least one compound selected from the group consisting of metallic copper powder, copper foil, cement powder, and mixtures thereof; Including, (2) is present in an amount of 1 to 40% by weight based on the total weight of the oxide material, provided that the graphite is present in an amount of 0.5 to 5% by weight based on the total weight of the oxide material; The combined content of (1) and (2) is at least 95% by weight of the catalyst.
[0087] In general, powdered copper, copper foil, or powdered cement, or graphite, or mixtures thereof, are added to the oxide material in an amount in the range of 1 to 40% by weight, preferably in the range of 2 to 20% by weight, particularly preferably in the range of 3 to 10% by weight, based on the total weight of the oxide material.
[0088] The cements preferably used are high alumina cements, which particularly preferably consist essentially of aluminium oxide and calcium oxide, particularly preferably of about 75-85% by weight aluminium oxide and about 15-25% by weight calcium oxide. It is furthermore possible to use cements based on magnesium oxide / aluminium oxide, calcium oxide / silicon oxide and calcium oxide / aluminium oxide / iron oxide.
[0089] In particular, the oxide material may have at least one further component selected from the group consisting of the elements Re, Fe, Ru, Co, Rh, Ir, Ni, Pd and Pt, with a content of less than or equal to 10% by weight, preferably less than or equal to 5% by weight, based on the total weight of the oxide material.
[0090] Preferably, the compound according to (2) is selected from the group consisting of metallic copper powder, copper foil, and mixtures thereof, and more preferably, the compound according to (2) is metallic copper.
[0091] For example, the catalysts disclosed in paragraph
[0085] of US Patent Application Publication No. 2010 / 0056364A1 are particularly suitable.
[0092] Post-processing: The reaction discharge is advantageously depressurized, the excess hydrogen and optionally any excess PYR present therein are then removed, and the resulting crude reaction product is purified, for example by fractional rectification. The excess hydrogen is advantageously recycled to the reaction, as are any incompletely reacted BDO or excess PYR, if applicable.
[0093] In the case of a continuous process involving the presence of BDO, water is produced during the reaction (see also Scheme 2 above). When the reactor effluent is cooled, BPB and water may form solids. To prevent the formation of such solids, the reactor outlet is preferably kept at a temperature in the range of 40-120°C, more preferably 60-110°C, even more preferably 80-100°C. This is usually achieved by using heat tracing. The reactor effluent may also be diluted with a solvent, preferably tetrahydrofuran (THF) or methanol, more preferably methanol. In addition, to further prevent the formation of such solids, the reactor outlet is preferably kept at a temperature in the range of 40-80°C, more preferably 45-75°C, even more preferably 50-70°C. This is achieved by using heat tracing.
[0094] In the case of a continuous process involving the presence of BDO, the process according to the invention preferably comprises working up the reaction product by the following steps: a) Removal of water by distillation; b) Removal of low boiling solvents by distillation; c) Removal of BPB by distillation to separate it from high boiling solvents.
[0095] Low boiling solvents are compounds that have a boiling point lower than BPB, such as PYR, N-propylpyrrolidine, N-butylpyrrolidine, 4-pyrrolidin-1-ylbutan-1-ol, 4-pyrrolidin-1-ylbutan-1-amine, and small amounts of water.
[0096] A high boiling compound is a compound having a boiling point higher than BPB, for example, bis(4-(pyrrolidinyl)butyl)amine.
[0097] If an excess of PYR is used, the process according to the invention preferably comprises working up the reaction product of the reaction by the following steps: a) Removal of water by distillation; b) Removal of PYR by distillation and recycling of the PYR to the reaction; c) Removal of low boiling solvents by distillation; d) Removal of BPB by distillation to separate it from high boiling solvents.
[0098] The low boiling point solvent removed according to step c) above may also contain a small amount of PYR that was not removed in step b).
[0099] In the case of a continuous process in the absence of BDO, the process according to the invention preferably comprises working up the reaction product of the reaction by the following steps: a) Removal of ammonia by distillation; b) Removal of low boiling solvents by distillation; c) Removal of BPB by distillation to separate it from high boiling solvents.
[0100] Low boiling solvents are compounds that have a boiling point lower than that of BPB, such as PYR, N-propylpyrrolidine, N-butylpyrrolidine, and 4-pyrrolidin-1-ylbutan-1-amine.
[0101] High boiling solvents are compounds that have a boiling point higher than BPB, such as bis(4-(pyrrolidinyl)butyl)amine.
[0102] The distillation as described above is preferably carried out in a suitable column. By removal by distillation is meant that the corresponding compounds pass into the gas phase and are thereby removed. The gaseous components can be withdrawn from the respective column either as a head stream or as a side stream.
[0103] The following examples serve merely to illustrate the invention and therefore are not intended to limit the invention in any manner. EXAMPLES
[0104] catalyst: The catalyst was prepared according to Example 4 of WO 2011 / 067199 A1 (BASF SE), and its composition (based on the respective oxides) is as follows: NiO (23.1wt%), CoO (24.6wt%), CuO (12.5wt%), SnO (1.8wt%), Al2O3 (38.0wt%).
[0105] Example 1 - Response of PYR to BPB A heated tubular reactor with an inner diameter of 14 mm and a total volume of 95 mL, fitted with a thermocouple in the center, was loaded with 4-5 wire mesh rings at the bottom, a layer of glass beads (15 mL), 50 mL of the amination catalyst (in the form of reduced and passivated 3 × 3 mm tablets) on top, and finally the remaining part was loaded with glass beads (15 mL) and 4-5 wire mesh rings again. Prior to the reaction, the catalyst was activated up to 240 °C. Thereby, the catalyst was heated up to 80 °C with a nitrogen flow of 50 NL / h. The temperature was then increased by 20 K every hour until 150 °C was reached. After 1 hour at 150 °C, a hydrogen flow of 5 NL / h and a nitrogen flow of 45 NL / h were used. Every 20 min, the hydrogen gas flow was increased by 5 NL / h, whereas the nitrogen gas flow was decreased. The total gas flow was kept constant at 50 NL / h. When 50 NL / h hydrogen and 0 NL / h nitrogen were reached, the temperature was raised stepwise (10 K / h) to 240°C with the same hydrogen gas flow rate. After reaching 240°C, the temperature and hydrogen gas flow rate were maintained for 24 hours. The reactor was cooled to 160°C. Heat tracing before and after the reactor was kept at 30-60°C. The hydrogen flow rate was reduced to 10 NL / h and a pressure of 120 bar was used. 30 g / h PYR was metered from bottom to top through the reactor. The reactor was kept at the temperature and absolute pressure shown in Table 1 below. The mixture leaving the reactor was diluted with THF (26 g / h), cooled to 60°C, depressurized to standard pressure and then kept at this temperature by heat tracing. Samples were taken from the reaction mixture at different time points and analyzed by gas chromatography. For this purpose, an "RTX-5 Amine" GC column was used with the following parameters: RTX-5-Amin (30 m × 0.32 mm × 1.5 μm) 60 °C - 5 °C / min - 280 °C - 10 min - 20 °C / min - 300 °C - 10 min Flow rate: 0.837 mL / min He.
[0106] "NL" means standard liter, i.e. volume at standard pressure (STP).
[0107] The results are shown in Table 1 below.
[0108] Example 2 - Reaction of PYR and BDO with BPB A heated tubular reactor with an inner diameter of 14 mm and a total volume of 95 mL, fitted with a thermocouple in the center, was loaded with 4-5 wire mesh rings at the bottom, a layer of glass beads (15 mL), 50 mL of the amination catalyst (in the form of reduced and passivated 3 × 3 mm tablets) on top, and finally the remaining part was loaded with glass beads (15 mL) and 4-5 wire mesh rings again. Prior to the reaction, the catalyst was activated up to 240 °C. Thereby, the catalyst was heated up to 80 °C with a nitrogen flow of 50 NL / h. The temperature was then increased by 20 K every hour until 150 °C was reached. After 1 hour at 150 °C, a hydrogen flow of 5 NL / h and a nitrogen flow of 45 NL / h were used. Every 20 min, the hydrogen gas flow was increased by 5 NL / h, whereas the nitrogen gas flow was decreased. The total gas flow was kept constant at 50 NL / h. When 50 NL / h hydrogen and 0 NL / h nitrogen were reached, the temperature was increased stepwise (10 K / h) to 240°C with the same hydrogen gas flow rate. After reaching 240°C, the temperature and hydrogen gas flow rate were maintained for 24 hours. The reactor was cooled to 160°C. Heat tracing before and after the reactor was kept at 30-60°C. The hydrogen flow rate was reduced to 10 NL / h and a pressure of 120 bar was used. A mixture of 10 g / h BDO and 15.7 g / h or 16.6 g / h PYR, respectively, was metered from bottom to top through the reactor. The reactor was kept at the temperature and absolute pressure shown in Table 2 below. The mixture leaving the reactor was diluted with THF or methanol (26 g / h), cooled to 60°C, depressurized to standard pressure and then kept at this temperature by heat tracing. Samples were taken from the reaction mixture at different time points and analyzed by gas chromatography. For this purpose, an "RTX-5 Amine" GC column was used with the following parameters: RTX-5-Amin (30 m × 0.32 mm × 1.5 μm) 60 °C - 5 °C / min - 280 °C - 10 min - 20 °C / min - 300 °C - 10 min Flow rate: 0.837 mL / min He.
[0109] "NL" means standard liter, i.e. volume at standard pressure (STP).
[0110] The results are shown in Table 2 below.
[0111] [Table 1]
[0112] [Table 2]
[0113] Discussion of results: Regarding Table 1 (reactions of PYR alone): Comparison of entries 1 and 2 shows that increasing the temperature from 188° C. to 198° C. increases both the conversion of PYR and the selectivity to BPB, resulting in an overall increase in the yield of BPB.
[0114] Regarding Table 2 (reaction of BDO with PYR): Temperature: A comparison of entries 1 and 2 shows that increasing the temperature from 188° C. to 198° C. increases the selectivity of BPB.
[0115] Pressure: A comparison of entries 3, 4 and 5 shows that operating at reaction pressures below 150 bar increases the selectivity.
[0116] A comparison of the molar ratios: entries 2 and 3 shows that improved selectivity can be achieved when molar ratios greater than 2:1 are realized.
[0117] Amount of hydrogen: A comparison of entry 3 with entry 6 shows that selectivity improves when the amount of hydrogen is less than 182 NL H2 per mole of BDO. A comparison of entry 4 with entry 7 shows that selectivity also improves when the amount of hydrogen is greater than 64 NL H2 per mole of BDO.
[0118] Preferred embodiments of the invention including corresponding combinations of features are outlined in paragraphs 1-45 below.
[0119] Paragraph 1. The present invention relates to a process for the preparation of bis(pyrrolidino)butane (BPB), comprising the reaction of pyrrolidine (PYR) in the presence of hydrogen in the liquid phase, a heterogeneous catalyst (catalyst), and optionally 1,4-butanediol (BDO), preferably wherein the catalytically active mass of the catalyst, before its reduction by hydrogen, comprises an oxygen-containing compound of copper and an oxygen-containing compound of aluminum and / or zirconium.
[0120] Paragraph 2. The process of paragraph 1, wherein the reaction is carried out at a temperature above 170°C, preferably at least 180°C, more preferably at least 188°C, even more preferably at least 189°C, particularly preferably at least 195°C, or even at least 198°C.
[0121] Paragraph 3. The process according to paragraph 1, wherein the reaction is carried out at a temperature in the range of 180 to 300°C, more preferably 180 to 230°C, even more preferably 180 to 220°C, particularly preferably 180 to 210°C, or even 180 to 200°C.
[0122] Paragraph 4. The method according to paragraph 1, wherein the reaction is carried out at a temperature in the range of 188 to 230°C, more preferably 188 to 220°C, even more preferably 188 to 210°C, and particularly preferably 188 to 200°C.
[0123] Paragraph 5. The method according to paragraph 1, wherein the reaction is carried out at a temperature in the range of 190 to 230°C, more preferably 190 to 220°C, even more preferably 190 to 210°C, and particularly preferably 190 to 200°C.
[0124] Paragraph 6. The process according to paragraph 1, wherein the reaction is carried out at a temperature in the range of 195 to 230°C, more preferably 195 to 220°C, even more preferably 195 to 210°C, and particularly preferably 195 to 200°C.
[0125] Paragraph 7. The method according to paragraph 1, wherein the reaction is carried out at a temperature in the range of 198 to 230°C, more preferably 198 to 220°C, even more preferably 198 to 210°C, and particularly preferably 198 to 200°C.
[0126] Paragraph 8. The process of any one of paragraphs 1 to 7, wherein the reaction is carried out at an absolute pressure of less than or equal to 150 bar, preferably less than 150 bar, more preferably less than 149 bar.
[0127] Paragraph 9. The method according to any one of paragraphs 1 to 8, wherein the reaction is carried out at an absolute pressure in the range of 20 to 150 bar (e.g. 45 to 150 bar or 55 to 150 bar), preferably 65 to 149 bar, more preferably 70 to 140 bar, even more preferably 75 to 130 bar, particularly preferably 80 to 130 bar, or the reaction is carried out at an absolute pressure in the range of 20 to 130 bar, preferably 50 to 130 bar, more preferably 55 to 100 bar, even more preferably 55 to 90 bar.
[0128] Paragraph 10. The method of any one of Paragraphs 1 to 9, wherein the PYR is solvent-free.
[0129] Paragraph 11. The method of any one of Paragraphs 1 to 10, wherein the catalyst is configured as a fixed bed reactor.
[0130] Paragraph 12. The method of any one of paragraphs 1 to 11, wherein the method is performed continuously.
[0131] Paragraph 13. The process of any one of paragraphs 1 to 12, wherein the reaction is carried out in a tubular reactor.
[0132] Paragraph 14. The method of any one of paragraphs 1 to 13, wherein the reaction is carried out in the presence of 1,4-butanediol (BDO).
[0133] Paragraph 15. The method of any one of Paragraphs 1 to 14, wherein the molar ratio of PYR to BDO is 1.5:1 or more, preferably 2:1 or more, more preferably greater than 2:1.
[0134] Paragraph 16. The process according to paragraph 14, wherein the molar ratio of PYR to BDO is in the range of from 2:1 to 10:1, preferably in the range of from greater than 2:1 to 10:1, more preferably in the range of from greater than 2:1 to 9:1, even more preferably in the range of from greater than 2:1 to 6:1, particularly preferably in the range of from greater than 2:1 to 4:1, or even in the range of from greater than 2:1 to 3:1.
[0135] Paragraph 17. The method according to any one of paragraphs 14 to 16, wherein the amount of hydrogen is between 65 and 181 NL, preferably between 70 and 150 NL, more preferably between 80 and 130 NL, even more preferably between 85 and 120 NL, particularly preferably between 85 and 110 NL, or even between 85 and 100 NL, per mole of BDO.
[0136] Paragraph 18. The method of any one of Paragraphs 14 to 17, wherein the BDO is solvent-free.
[0137] Paragraph 19. The process according to any one of Paragraphs 14 to 18, wherein the molar conversion of BDO is at least 90%, preferably at least 95%, more preferably at least 98%, particularly preferably at least 99% or even 100%.
[0138] Paragraph 20. The process of any one of Paragraphs 12 to 19, wherein the reactor outlet is diluted with a solvent, preferably tetrahydrofuran (THF) or methanol, more preferably methanol.
[0139] Paragraph 21. The process of any one of Paragraphs 1 to 19, wherein the reactor outlet is maintained at a temperature in the range of 40 to 120°C, preferably 60 to 110°C, more preferably 80 to 100°C.
[0140] Paragraph 22. The method of paragraphs 20 or 21, such method further comprising working up the reaction product of the reaction by: a) Removal of water by distillation; b) Removal of low boiling solvents by distillation; c) Removal of BPB by distillation to separate it from high boiling solvents.
[0141] Paragraph 23. The method comprises the steps of: (a) preparing a catalyst having a liquid hourly space velocity of 0.05-5, preferably 0.1-2, more preferably 0.2-1 or 0.15-0.8 kg BDO / L catalyst The method according to any one of paragraphs 12 and 13 and paragraphs 14 to 22, wherein the method is carried out within the scope of .h).
[0142] Paragraph 24. The method of any one of paragraphs 1 to 13, wherein the reaction is carried out in the absence of BDO.
[0143] Paragraph 25. The method comprises the steps of: providing a liquid hourly space velocity over the catalyst of from 0.05 to 5, preferably from 0.1 to 2, more preferably 0.2-1kg PYR / (L catalyst .h). The method according to any one of paragraphs 12 and 13 and paragraph 24, carried out within the scope of the present invention.
[0144] Paragraph 26. The method of any one of Paragraphs 12 and 13 and Paragraphs 24 and 25, wherein such method further comprises working up the reaction product of the reaction by: a) Removal of ammonia by distillation; b) Removal of low boiling solvents by distillation; c) Removal of BPB by distillation to separate it from high boiling solvents.
[0145] Paragraph 27. The method of any one of Paragraphs 1 to 26, wherein the catalytically active mass of the catalyst before its reduction with hydrogen comprises an oxygen-containing compound of copper, an oxygen-containing compound of aluminum and / or zirconium, and at least one oxide selected from the group consisting of oxygen-containing compounds of nickel, cobalt, tin, molybdenum and lanthanum.
[0146] Paragraph 28. The method of any one of Paragraphs 1 to 26, wherein the catalytically active mass of the catalyst prior to its reduction with hydrogen comprises an oxygen-containing compound of copper and an oxygen-containing compound of aluminum.
[0147] Paragraph 29. The method of any one of Paragraphs 1 to 28, wherein the catalytically active mass of the catalyst prior to its reduction with hydrogen comprises at least one oxide selected from the group consisting of oxygen-containing compounds of copper, oxygen-containing compounds of aluminum, and oxygen-containing compounds of nickel, cobalt, tin, molybdenum, and lanthanum.
[0148] Paragraph 30. The method of any one of Paragraphs 1 to 26, wherein the catalytically active mass of the catalyst prior to its reduction with hydrogen comprises oxygen-containing compounds of aluminum, copper, nickel and cobalt, and 0.2 to 5.0% by weight of oxygen-containing compounds of tin, calculated as SnO.
[0149] Paragraph 31. The catalytic activity mass of the catalyst before its reduction with hydrogen is: in the range of 15-80% by weight of oxygen-containing compounds of aluminum, calculated as Al2O3; in the range of 1-20% by weight of oxygen-containing compounds of copper, calculated as CuO; in the range of 5 to 35 weight percent of oxygen-containing compounds of nickel, calculated as NiO; 5-35% by weight of oxygen-containing compounds of cobalt, calculated as CoO; 27. The method of any one of paragraphs 1 to 26, comprising in the range of 0.2 to 5.0 weight percent of a tin-oxygen-containing compound, calculated as SnO.
[0150] Paragraph 32. The catalytic activity mass of the catalyst before its reduction with hydrogen is: 20-85% by weight of oxygen-containing compounds of zirconium, calculated as ZrO2; 1 to 30% by weight of oxygen-containing compounds of copper, calculated as CuO; 14 to 70% by weight of an oxygen-containing compound of nickel, calculated as NiO; 27. The method of any one of paragraphs 1 to 26, comprising: 0 to 5 weight percent of an oxygen-containing compound of molybdenum, calculated as MoO3.
[0151] Paragraph 33. The method of Paragraph 32, wherein the molar ratio of nickel to copper is greater than 1.
[0152] Paragraph 34. The method of Paragraphs 32 or 33, wherein the catalytically active mass of the catalyst prior to its reduction with hydrogen is free of oxygen-containing compounds of molybdenum.
[0153] Paragraph 35. The catalyst before its reduction with hydrogen is (1) An oxide material, (a) 50 to 80 weight percent of oxygen-containing compounds of copper, calculated as CuO; (b) 15 to 35 weight percent of oxygen-containing compounds of aluminum, calculated as Al2O3; (c) 2 to 20 weight percent of an oxygen-containing compound of lanthanum, calculated as La2O3; an oxide material, the total weight percent of which is the sum of oxygen-containing compounds of copper, aluminum, and lanthanum, is in the range of 80 to 100 wt%; (2) Graphite and at least one compound selected from the group consisting of metallic copper powder, copper foil, cement powder, and mixtures thereof; Including, (2) is present in an amount of 1 to 40% by weight based on the total weight of the oxide material, provided that the graphite is present in an amount of 0.5 to 5% by weight based on the total weight of the oxide material; 27. The method of any one of paragraphs 1 to 26, wherein the combined content of (1) and (2) is at least 95% by weight of the catalyst.
[0154] Paragraph 36. The catalyst before its reduction with hydrogen: (1) An oxide material, (a) 55 to 75 weight percent of oxygen-containing compounds of copper, calculated as CuO; (b) 20 to 30 weight percent of oxygen-containing compounds of aluminum, calculated as Al2O3; (c) 3 to 15 weight percent of an oxygen-containing compound of lanthanum, calculated as La2O3; an oxide material, the total weight percent of which is the sum of oxygen-containing compounds of copper, aluminum, and lanthanum, is in the range of 95 to 100 wt%; (2) Graphite and at least one compound selected from the group consisting of metallic copper powder, copper foil, cement powder, and mixtures thereof; Including, (2) is present in an amount of 1 to 40% by weight based on the total weight of the oxide material, provided that the graphite is present in an amount of 0.5 to 5% by weight based on the total weight of the oxide material; 27. The method of any one of paragraphs 1 to 26, wherein the combined content of (1) and (2) is at least 95% by weight of the catalyst.
[0155] Paragraph 37. The catalytic activity mass of the catalyst before its reduction with hydrogen is: 20 to 75% by weight of aluminum oxide, calculated as Al2O3; 20 to 75% by weight of oxygen-containing compounds of copper, calculated as CuO; 0-2% by weight of oxygen-containing compounds of sodium, calculated as Na2O; 27. The method of any one of paragraphs 1-26, comprising less than 5 wt. % oxygen-containing compounds of nickel, calculated as NiO.
[0156] Paragraph 38. The catalytic activity mass of the catalyst before its reduction with hydrogen is: 25 to 65% by weight of aluminum oxide, calculated as Al2O3; 30-70% by weight of oxygen-containing compounds of copper, calculated as CuO; 0.05 to 1% by weight of oxygen-containing compounds of sodium, calculated as Na2O; 27. The method of any one of paragraphs 1-26, comprising less than 1 wt. % oxygen-containing compounds of nickel, calculated as NiO.
[0157] Paragraph 39. The catalytic activity mass of the catalyst before its reduction with hydrogen is: 20 to 85% by weight of aluminum oxide (Al2O3) and / or zirconium dioxide (ZrO2); 1 to 70% by weight of oxygen-containing compounds of copper calculated as CuO, and 0 to 50% by weight of oxygen-containing compounds of magnesium calculated as MgO, oxygen-containing compounds of chromium calculated as Cr2O3, oxygen-containing compounds of zinc calculated as ZnO, oxygen-containing compounds of barium calculated as BaO, and / or oxygen-containing compounds of calcium calculated as CaO, 27. The method of any one of paragraphs 1 to 26, comprising: 0 to 30 wt. % of an oxygen-containing compound of nickel, calculated as NiO.
[0158] Paragraph 40. The catalytic activity mass of the catalyst before its reduction with hydrogen is: 25 to 85% by weight of aluminum oxide (Al2O3); 2 to 65% by weight of oxygen-containing compounds of copper, calculated as CuO, and 0 to 30% by weight of oxygen-containing compounds of magnesium, calculated as MgO, oxygen-containing compounds of chromium, calculated as Cr2O3, oxygen-containing compounds of zinc, calculated as ZnO, oxygen-containing compounds of barium, calculated as BaO, and / or oxygen-containing compounds of calcium, calculated as CaO; 27. The method of any one of paragraphs 1 to 26, comprising 5 to 28 weight percent of an oxygen-containing compound of nickel, calculated as NiO.
[0159] Paragraph 41. The method of any one of Paragraphs 1 to 26, wherein the catalytically active mass of the catalyst before its reduction with hydrogen comprises oxygen-containing compounds of copper and nickel and oxygen-containing compounds of aluminum and / or zirconium.
[0160] Paragraph 42. The method of any one of Paragraphs 1 to 26, wherein the catalytically active mass of the catalyst before its reduction with hydrogen comprises oxygen-containing compounds of copper, nickel and cobalt and oxygen-containing compounds of aluminum and / or zirconium.
[0161] Paragraph 43. The method of any one of Paragraphs 1 to 26, wherein the catalytically active mass of the catalyst prior to its reduction with hydrogen comprises oxygen-containing compounds of copper, nickel and aluminum.
[0162] Paragraph 44. The method of any one of Paragraphs 1 to 26, wherein the catalytically active mass of the catalyst prior to its reduction with hydrogen comprises oxygen-containing compounds of copper, nickel, cobalt and aluminum.
[0163] Paragraph 45. The method according to any one of paragraphs 1 to 26, further comprising the step of: providing that the catalytically active mass of the catalyst before its reduction with hydrogen comprises oxygen-containing compounds of copper, oxygen-containing compounds of aluminum and / or zirconium and, optionally, at least one oxide selected from the group consisting of oxygen-containing compounds of nickel, cobalt, tin, molybdenum and lanthanum, if the sum of the catalytically active mass of said compounds, calculated as CuO, ZrO2 and / or Al2O3 and, where applicable, NiO, CoO, SnO, MoO3 and / or La2O3, is between 50 and 100% by weight, preferably between 70 and 100% by weight, particularly preferably between 80 and 100% by weight, more preferably between 90 and 100% by weight and very particularly preferably between 95 and 100% by weight.
Claims
1. A process for the production of bis(pyrrolidino)butane (BPB) comprising the reaction of pyrrolidine (PYR) in the presence of hydrogen, a heterogeneous catalyst (catalyst), and optionally 1,4-butanediol (BDO) in the liquid phase.
2. 2. The method of claim 1, wherein the catalytically active mass of the catalyst prior to its reduction with hydrogen comprises oxygen-containing compounds of copper and oxygen-containing compounds of aluminum and / or zirconium.
3. 3. The process according to claim 1 or 2, wherein the reaction is carried out at a temperature in the range of from 180 to 300°C, more preferably from 180 to 230°C, even more preferably from 180 to 220°C, particularly preferably from 180 to 210°C, or even from 180 to 200°C.
4. 4. The process according to any one of claims 1 to 3, wherein the reaction is carried out at an absolute pressure in the range of from 20 to 150 bar (e.g. from 45 to 150 bar or from 55 to 150 bar), preferably from 65 to 149 bar, more preferably from 70 to 140 bar, even more preferably from 75 to 130 bar, particularly preferably from 80 to 130 bar.
5. The method according to any one of claims 1 to 4, wherein the method is carried out continuously.
6. The process according to any one of claims 1 to 5, wherein the reaction is carried out in the presence of 1,4-butanediol (BDO).
7. 7. The process according to claim 6, wherein the molar ratio of PYR to BDO is in the range of from 2:1 to 10:1, preferably in the range of from greater than 2:1 to 10:1, more preferably in the range of from greater than 2:1 to 9:1, even more preferably in the range of from greater than 2:1 to 6:1, particularly preferably in the range of from greater than 2:1 to 4:1, or even in the range of from greater than 2:1 to 3:
1.
8. 8. The process according to claim 6 or 7, wherein the amount of hydrogen is from 65 to 181 NL, preferably from 70 to 150 NL, more preferably from 80 to 130 NL, even more preferably from 85 to 120 NL, particularly preferably from 85 to 110 NL, or even from 85 to 100 NL per mole of BDO.
9. A process according to any one of claims 5 to 8, wherein the reactor outlet is maintained at a temperature in the range of from 40 to 120°C, preferably from 60 to 110°C, more preferably from 80 to 100°C.
10. 10. The process according to any one of claims 1 to 9, wherein the catalytically active mass of the catalyst before its reduction with hydrogen comprises at least one oxide selected from the group consisting of oxygen-containing compounds of copper, oxygen-containing compounds of aluminium and / or zirconium, and oxygen-containing compounds of nickel, cobalt, tin, molybdenum and lanthanum.
11. 10. The method according to any one of claims 1 to 9, wherein the catalytically active mass of the catalyst before its reduction with hydrogen comprises oxygen-containing compounds of aluminium, copper, nickel and cobalt, and oxygen-containing compounds of tin, calculated as SnO, in an amount ranging from 0.2 to 5.0% by weight.
12. The catalytic activity mass of the catalyst prior to its reduction with hydrogen is 15 to 80% by weight of Al 2 O 3 and an oxygen-containing compound of aluminum calculated as 1-20% by weight of oxygen-containing compounds of copper, calculated as CuO; 5-35% by weight of oxygen-containing compounds of nickel, calculated as NiO; 5-35% by weight of oxygen-containing compounds of cobalt, calculated as CoO; 0.2 to 5.0 wt. % of tin oxygen-containing compounds, calculated as SnO.
13. The catalytic activity mass of the catalyst prior to its reduction with hydrogen is 20 to 85% by weight of ZrO 2 and an oxygen-containing compound of zirconium, calculated as 1-30% by weight of oxygen-containing compounds of copper, calculated as CuO; 14 to 70% by weight of oxygen-containing compounds of nickel, calculated as NiO; 0 to 5% by weight of MoO 3 and an oxygen-containing compound of molybdenum, calculated as:
14. The catalytic activity mass of the catalyst prior to its reduction with hydrogen is (1) An oxide material, (a) 50-80 wt. % of oxygen-containing compounds of copper, calculated as CuO; (b) 15 to 35 wt. % Al 2 O 3 and an oxygen-containing compound of aluminum calculated as (c) 2 to 20 wt % of La 2 O 3 and an oxygen-containing compound of lanthanum, calculated as a total weight percent of the oxide material, the total weight percent of the copper, aluminum, and lanthanum oxygen-containing compounds being in the range of 80 to 100 wt %; (2) graphite and at least one compound selected from the group consisting of metallic copper powder, copper foil, cement powder, and mixtures thereof; Including, (2) is in the range of 1 to 40% by weight based on the total weight of the oxide material, and the graphite is present in an amount of 0.5 to 5% by weight based on the total weight of the oxide material; The total content of (1) and (2) is at least 95% by weight of the catalyst; The method according to any one of claims 1 to 9.
15. The catalytic activity mass of the catalyst prior to its reduction with hydrogen is 20 to 75% by weight of Al 2 O 3 and aluminum oxide, calculated as 20-75% by weight of oxygen-containing compounds of copper, calculated as CuO; 0 to 2% by weight of Na 2 Oxygen-containing compounds of sodium, calculated as O; less than 5% by weight of oxygen-containing compounds of nickel, calculated as NiO; The method according to any one of claims 1 to 9, comprising:
16. The catalytic activity mass of the catalyst prior to its reduction with hydrogen is 20 to 85% by weight of aluminum oxide (Al 2 O 3 ) and / or zirconium dioxide (ZrO 2 )and, 1-70% by weight of oxygen-containing compounds of copper, calculated as CuO; 0-50% by weight of oxygen-containing compounds of magnesium, calculated as MgO, Cr 2 O 3 oxygen compounds of chromium, calculated as CrO, oxygen compounds of zinc, calculated as ZnO, oxygen compounds of barium, calculated as BaO, and / or oxygen compounds of calcium, calculated as CaO; 0-30% by weight of oxygen-containing compounds of nickel, calculated as NiO; The method according to any one of claims 1 to 9, comprising: