Moisture-resistant chemiluminescent marking system and composition
Moisture-resistant chemiluminescent marking systems, formulated as gels or waxes with dual-compartment delivery, address the sensitivity issues of CIPO and CPPO, achieving extended shelf life and improved performance across varied temperatures and humidities.
Patent Information
- Application Number
- JP2024519809
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-10-07
- Filing Date
- 2022-10-07
- Publication Date
- 2024-10-10
AI Technical Summary
Current chemiluminescent marking systems face challenges due to the sensitivity of bis{3,4,6-trichloro-2-[(3-methylbutoxy)carbonyl]phenyl}oxalate (CIPO) and bis{3,4,6-trichloro-2-[(pentyloxy)carbonyl]phenyl}oxalate (CPPO) to moisture and temperature, leading to degradation and reduced shelf life, making commercialization difficult.
Development of moisture-resistant chemiluminescent marking systems with a wide operating temperature range, formulated as gels or waxes, using dual-compartment delivery systems and incorporating components like oxalate esters, fluorescent agents, inorganic salts, peroxides, and catalysts, which are encapsulated to maintain stability.
The systems exhibit extended shelf life, improved performance under humid conditions, wider temperature range functionality, and ease of use, allowing reuse over multiple days with simpler production methods.
Smart Images

Figure 2024537085000001 
Figure 2024537085000002 
Figure 2024537085000003
Abstract
Description
[Technical field]
[0001] FIELD OF THE DISCLOSURE
[0002] Embodiments of the present invention relate to chemiluminescent compounds; chemiluminescent marking systems, and more particularly, to formulations and processes for producing chemiluminescent marking systems that are moisture resistant and have a wide operating temperature range.
[0002] (CROSS REFERENCE TO RELATED APPLICATIONS) In accordance with 37 C.FR 1.76, a claim of priority is contained in the Application Data Sheet filed contemporaneously herewith. Accordingly, this invention claims priority to U.S. Provisional Patent Application No. 63 / 253,368, entitled "Moisture Resistant Chemiluminescent Marking Systems and Compositions," filed October 7, 2021. The contents of the above-referenced applications are incorporated herein by reference in their entirety. [Background technology]
[0003] Chemiluminescent systems are well known in the art. Generally, such systems consist of an energy molecule, a fluorophore, an oxidizer, and a catalyst that, when combined, produce actinic light. Such systems have a wide range of applications, from novelty light sticks to military applications as training munitions and marking systems. Although chemiluminescent light generating systems offer advantages over other light systems, such as the ability to be stored in plastic cartridges or to produce light without generating heat, there are several persistent problems with the use of chemiluminescence in marking devices.
[0004] An effective chemiluminescent marking system requires a long shelf life, feasibility of manufacturing on a commercial scale, ease of use, performance (brightness and duration of usable light), water resistance, and compatibility with a wide range of temperatures. Many of the problems associated with chemiluminescent marking systems result from the moisture and temperature sensitivity of the oxalates used, particularly bis{3,4,6-trichloro-2-[(3-methylbutoxy)carbonyl]phenyl}oxalate (CIPO) and / or bis{3,4,6-trichloro-2-[(pentyloxy)carbonyl]phenyl}oxalate (CPPO). CPPO, the most commonly used oxalate, is moisture and temperature sensitive. Chemiluminescent systems using CPPO are difficult to encapsulate, spray dry, or prill. The temperatures required for prilling cause degradation of CPPO. Previous methods of encapsulating CPPO or solutions containing CPPO have used coacervation by several techniques. However, most of these methods require aqueous solutions at some stage in the process. A drawback of these processes is that the CPPO degrades because it is very difficult to reduce the residual moisture to an acceptable level. The degradation process, once started, cannot be stopped, shortening the shelf life and compromising the performance of the final product. As a result, attempts have been made to commercialize CPPO-based marking devices, but have not been feasible. Therefore, what is needed in the art is a moisture-resistant, wide operating temperature range chemiluminescent marking system that overcomes the drawbacks associated with current chemiluminescent marking systems. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] U.S. Provisional Patent Application No. 63 / 253,368 Summary of the Invention
[0006] Embodiments of the present invention provide formulations and processes for making chemiluminescent marking systems that are moisture resistant and have a wide operating temperature range. The improved chemiluminescent marking systems are designed to have one or more of the following properties compared to current systems: extended shelf life, ease of use, superior performance under humid conditions, performance over a wider operating temperature range, the ability to reuse the same device in multiple environments, days, and easier means of production. The improved chemiluminescent marking systems can take the form of a gel or wax and may have a wide range of applications in more diverse environments, including, but not limited to, marking interior or exterior walls, metal rails, polymeric surfaces, and wooden structures that are exposed to a variety of temperature and humidity conditions.
[0007] The chemiluminescent marking system includes a first chemiluminescent reactant component that comprises a chemiluminescent reactant mixture and a second chemiluminescent reactant component that comprises a chemiluminescent reactant mixture, whereby chemiluminescent light is generated upon contact between the first chemiluminescent reactant component and the second chemiluminescent reactant component.
[0008] It is therefore an object of the present invention to provide an improved chemiluminescent marking system. It is a further object of the present invention to provide a moisture resistant chemiluminescent marking system.
[0009] It is yet another object of the present invention to provide a chemiluminescent marking system with improved thermal stability capable of performing over a wider operating temperature range.
[0010] It is yet another object of the present invention to provide an improved chemiluminescent marking system which is less susceptible to degradation.
[0011] It is yet another object of the present invention to provide an improved chemiluminescent marking system that has an extended shelf life.
[0012] It is a further object of the present invention to provide a moisture resistant chemiluminescent marking system in the form of a gel that has functionality, i.e., stronger and / or longer light output, over a wider operating temperature range.
[0013] It is yet another object of the present invention to provide a moisture resistant chemiluminescent marking system in wax form that has functionality, i.e., stronger and / or longer light output over a wider operating temperature range.
[0014] It is yet another object of the present invention to provide an improved chemiluminescent marking system in an encapsulated form.
[0015] It is a further object of the present invention to provide an improved chemiluminescent marking system that indicates the ability to perform a chemiluminescent reaction after prilling.
[0016] It is yet another object of the present invention to provide an improved chemiluminescent marking system which is easy to use.
[0017] It is yet another object of the present invention to provide an improved chemiluminescent marking system which functions under wet conditions.
[0018] It is a further object of the present invention to provide an improved chemiluminescent marking system which functions over a wider temperature range.
[0019] It is yet another object of the present invention to provide an improved chemiluminescent marking system which can be configured to allow reuse of the same device over several days.
[0020] It is yet another object of the present invention to provide an improved chemiluminescent marking system designed to provide easier means of manufacture.
[0021] Other objects and advantages of the present invention will become apparent from the following description taken in conjunction with the accompanying drawings which set forth, by way of illustration and example, certain embodiments of the invention. All drawings contained herein constitute a part of this specification and include illustrative embodiments of the invention and illustrate various objects and features of the invention. [Brief description of the drawings]
[0022] The patent or application contains at least one drawing executed in color. Copies of this patent or patent application including color drawing(s) will be provided by the Office upon request and payment of the necessary fee. [Figure 1] 1 is a data table of Light Output Readings (LOP) associated with an embodiment described in Example 2, a wax marking system. [Diagram 2] 1 is a data table of Light Output Readings (LOP) associated with an embodiment described in Example 3, a wax marking system. [Figure 3A] Photograph of the light output, upon initial start-up, of the wax marking system described in Example 4, spread onto a piece of steel that had been conditioned overnight in a freezer (−16° C.), when the lights were turned on. [Figure 3B] Photograph of the light output, with the lights off, at initial start-up of the wax marking system described in Example 4 spread onto a piece of steel that had been conditioned overnight in a freezer (-16°C). [Figure 3C] Photograph of the light output after 1 hour of the wax marking system described in Example 4 spread onto a piece of steel that had been conditioned overnight in a freezer (−16° C.). [Figure 3D] Photograph of the light output after 2 hours of the wax marking system described in Example 4 spread onto a piece of steel that had been conditioned overnight in a freezer (−16° C.). [Figure 3E] Photograph of the light output after 3 hours of the wax marking system described in Example 4 spread onto a piece of steel that had been conditioned overnight in a freezer (−16° C.). [Figure 3F]Photograph of the light output after 4 hours of the wax marking system described in Example 4 spread onto a piece of steel that had been conditioned overnight in a freezer (−16° C.). [Figure 3G] Photograph of the light output after 5 hours of the wax marking system described in Example 4 spread onto a piece of steel that had been conditioned overnight in a freezer (−16° C.). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0023] While the invention may be embodied in various forms, with the understanding that the present disclosure is to be considered as an example of the invention, preferred, but not limiting, embodiments are shown in the drawings and will be described below, without the intention of limiting the invention to the specific embodiments shown.
[0024] The embodiments of the invention described herein are directed to a chemiluminescent marking system and a method for its manufacture. The chemiluminescent marking system is designed to be moisture resistant and emit light over a wider temperature range. Thus, the moisture resistant, wide operating temperature range chemiluminescent marking system embodiments can be used in a wide variety of environments. The chemiluminescent marking system of the present invention can provide a formulation or composition that improves one or more of the following attributes over current chemiluminescent systems: 1) extended shelf life, 2) ease of use, 3) better performance under humid conditions, 4) performance over a wider operating temperature range, 5) the ability to reuse the same device over several days, and 6) easier means of production. The chemiluminescent marking system formulation can be formulated directly or in an encapsulated form. As with other chemiluminescent systems, the first part of the moisture resistant, wide operating temperature range chemiluminescent marking system can include at least one oxalate ester, at least one fluorescent agent, and at least one inorganic salt, commonly referred to as an oxalate composition, in an organic carrier solvent. The moisture resistant, wide operating temperature range chemiluminescent marking system may include a second part, an activator composition, which may include at least one peroxide and at least one catalyst in an organic carrier solvent. The individual components of the moisture resistant, wide operating temperature range chemiluminescent marking system may be formulated into the marking system directly, in prilled form, or in encapsulated form.
[0025] In an exemplary embodiment, the moisture resistant, wide operating temperature range chemiluminescent marking system may be a gel. In another exemplary embodiment, the moisture resistant, wide operating temperature range chemiluminescent marking system may be a wax. The gel or wax according to the moisture resistant, wide temperature chemiluminescent marking system embodiments may be formulated to be deliverable by a variety of mechanisms, including the use of a wide variety of commercially available containers ranging from dual syringes, dual compartment squeeze containers, dual chamber pressurized systems (aerosol or bag-on-valve systems), and advanced containers with various push-up or screw mechanisms. The delivery mechanism or vehicle associated with the delivery of the moisture resistant, wide operating temperature range chemiluminescent marking system gel or wax may depend on the rheology and the desired application.
[0026] Gel Markers: Chemiluminescent gels suitable for use as markers can be made by combining a mixture of components, a suitable oxalate as the energy component (hereafter referred to as the gel oxalate mixture), and a peroxygen-containing component with a catalyst (hereafter referred to as the gel activator mixture). The gel oxalate mixture can be composed of a suitable solvent or solvent mixture, a chemiluminescent dye or dye mixture, one form of bis{3,4,6-trichloro-2-[(phenylmethoxy)carbonyl]phenyl}oxalate (CBzPO) and / or bis{3,4,6-trichloro-2-[(cyclohexylmethoxy)carbonyl]phenyl}oxalate (CyHMPO), referred to as oxalate esters, one or more rheology adjusting agents, and a salt that generates heat in combination with peroxygen if the application warrants use over a wider operating temperature range. The gel activator mixture is composed of a suitable solvent or solvent mixture, one or more forms of peroxygen, one or more suitable catalysts, and one or more rheology adjusting agents.
[0027] Specific examples of solvents used in the gel oxalate mixture include, but are not limited to, benzoates, dialkyl glycol ethers, glycol diesters, dialkyl polyglycol ethers, polyglycol diesters, dialkyl malonates, 2-alkyl dialkyl malonates, 2,2-dialkyl malonates, dialkyl adipates, glyceryl triesters, acetyl trialkyl citrates, phthalates, terephthalates, and various alkane-based solvents including ISOPARS®. A single solvent or a combination of solvents in various ratios may be optimal. When two solvents are used, the ratios may vary depending on the solvents selected and their solubility with each other, including but not limited to a range of 95% and 5% to 50% and 50% for the two solvents. A preferred range is 80% and 20% to 60% and 40% for the two solvents. In the case of three solvents, the chemiluminescent marking system gel embodiment may include ratios ranging from 5:5:90 to a ratio of 60% of one solvent, with the remaining mixture equal to 40% being preferably composed of the two other solvents. The ratio range can be varied and will vary depending on the choice of dye, oxalate ester, and rheology adjustment reagent. The total amount of solvents used may be 90%-50% of the total mass of the oxalic acid gel mixture, with the preferred amount being 85%-60%. The total mass of the oxalic acid gel mixture used may depend on the desired application.
[0028] Specific examples of chemiluminescent dyes for use with the oxalic acid gel mixture include, but are not limited to, 9,10-bisphenylanthracene and halogenated derivatives of this compound, 9,10-bis(phenylethynyl)anthracene and alkylated, nitrated, halogenated, alkoxylated and arylated derivatives of this dye, 9-phenyl-10-(phenylethynyl)anthracene and alkylated, nitrated, halogenated, alkoxylated and arylated derivatives of this dye, perylene dyes, rubrene and alkylated, halogenated and phenylated derivatives of this dye, acridone, and 15,16-dialkyloxyviolathrones and derivatives or isomers of this dye. The preferred total concentration of dyes is, but is not limited to, 0.2% to 1%.
[0029] Specific examples of forms of CBzPO and / or CyHMPO include, but are not limited to, pure purified compounds, prilled particles, spray-dried particles, polymer-coated prilled particles, and polymer-coated spray-dried particles. Forms of CBzPO and / or CyHMPO can be dispersed in the formulation when hot, warm, or cold, depending on the form used or the end product required. Preferred concentrations of oxalate esters include, but are not limited to, 5%-35%. The concentration of oxalate esters may depend on the solvent mixture and application parameters.
[0030] Specific examples of rheology adjusting agents for oxalic acid gel mixtures include, but are not limited to, one or more GEON® resins, one or more fumed silicas, one or more low melting point fatty acid esters, one or more glyceryl triesters, polyethylene waxes, and one or more paraffins. The total concentration of the rheology adjusting reagent is not limited and may be 5% to 40%. A preferred concentration may be 7% to 25%. The total concentration of the rheology adjusting reagent used may depend on the desired application.
[0031] Specific examples of solvents for the gel activator mixture include, but are not limited to, dialkyl phthalates, tertiary alcohols, trialkyl citrates, and dialkyl 2,2-dialkyl malonates.
[0032] Specific examples of peroxygen for the gel activator mixture include, but are not limited to, hydrogen peroxide, urea peroxide, percarbonates, bicarbonates, alkaline peroxides, and alkaline earth peroxides in regular or encapsulated form.
[0033] Specific examples of catalysts for gel activators include, but are not limited to, salicylates, halogenated salicylates, benzoates, alkylated or halogenated benzoates, tertiary alkyl amines, carbonates, and bicarbonates.
[0034] Specific examples of rheology adjusting agents for use with the gel activator mixture include, but are not limited to, one or more GEON® resins, one or more fumed silicas, one or more low melting point fatty acid esters, one or more glyceryl triesters, polyethylene waxes, and one or more paraffins. The total concentration of the rheology adjusting agent may be, but is not limited to, 5% to 30%, with a preferred concentration being, but is not limited to, 7% to 25%. The total concentration of the rheology adjusting agent may depend on the desired application.
[0035] In use, the oxalate gel and the activator gel are placed in a dual chamber apparatus where the two gels are separated by a barrier such as a polyethylene, polypropylene, or special plasticized foil barrier. The dual chamber apparatus may be a commercially available dual chamber syringe, a foil split squeeze tube, or a dual chamber caulking apparatus. If deemed necessary based on the viscosity and ease of mixing of the two components, the apparatus may include a static mixer.
[0036] Wax Markers: Chemiluminescent waxes suitable for use as markers may be produced by the combination of an energetic component (hereafter referred to as a wax oxalate mixture), a peroxygen-containing component and a catalyst (hereafter referred to as a wax activator mixture). The wax oxalate mixture may include a suitable solvent or solvent mixture, a chemiluminescent dye or dye mixture, a form of CBzPO and / or CyHMBPO, and one or more rheology adjusting reagents. The wax activator mixture may be composed of a suitable solvent or solvent mixture, one or more forms of peroxygen, one or more suitable catalysts, one or more rheology adjusting reagents, and, if the application warrants use over a wider operating temperature range, a salt that generates heat in combination with the peroxygen.
[0037] Specific examples of solvents that can be used in the wax-oxalate mixture include, but are not limited to, one or more alkane-based solvents, including benzoates, dialkyl glycol ethers, glycol diesters, dialkyl polyglycol ethers, polyglycol diesters, dialkyl malonates, 2-alkyl dialkyl malonates, 2,2-dialkyl malonates, dialkyl adipates, glyceryl triesters, acetyl trialkyl citrates, phthalates, terephthalates, and ISOPARS®. A single solvent or a combination of solvents in various ratios may be optimal. If two solvents are used, the ratios may vary depending on the solvents selected and their solubility in each other, and may include, but are not limited to, a range between 95% and 5% to 50% and 50% for the two solvents. A preferred range is 80% and 20% to 60% and 40%. In the case of three solvents, a mixture consisting of a ratio of 60% of one solvent and the remaining 40% of the two other solvents is preferred, ranging from a ratio of 5:5:90. The range of ratios will vary depending on the choice of dye, oxalate ester, and rheology modifying agent. The total amount of solvent used may be 90%-50% of the total weight of the oxalate-wax mixture, with the preferred amount being 85%-60%. The total amount of solvent used may vary depending on the application and other ingredients used.
[0038] Specific examples of chemiluminescent dyes for wax-oxalate mixtures include, but are not limited to, 9,10-bisphenylanthracene and halogenated derivatives of this compound, 9,10-bis(phenylethynyl)anthracene and alkylated, nitrated, halogenated, alkoxylated, and arylated derivatives of this dye, 9-phenyl-10-(phenylethynyl)anthracene and alkylated, nitrated, halogenated, alkoxylated, and arylated derivatives of this dye, perylene dyes, rubrene and alkylated, halogenated, and phenylated derivatives of this dye, acridone, and 15,16-dialkyloxyviolathrone and derivatives or isomers of this dye. The preferred total concentration of dyes is, but is not limited to, 0.3% to 1%. The total concentration of dyes may be modified to include ranges outside the preferred range depending on the application and other ingredients used.
[0039] Specific examples of forms of CBzPO and / or CyHMPO can be, but are not limited to, pure purified compounds, prilled particles, spray-dried particles, polymer-coated prilled particles, and polymer-coated spray-dried particles. The forms of CBzPO and / or CyHMPO can be dispersed in the formulation when hot, warm, or cold, depending on the form used or the end product required. The preferred concentration of oxalate ester is, but is not limited to, 5%-35%. The concentration of oxalate ester used can depend on the solvent mixture and application parameters.
[0040] Specific examples of rheology control agents for wax-oxalic acid mixtures include, but are not limited to, one or more GEON® resins, one or more fumed silicas, one or more low melting point fatty acid esters, one or more glyceryl triesters, one or more paraffin and polyethylene waxes. The total concentration of the rheology control agent may be between 15% and 80%, but is not limited thereto, with the preferred concentration being between 30% and 70%. The total concentration of the rheology control agent used may vary depending on the desired application.
[0041] Specific examples of salts that will generate heat in combination with peroxygen include, but are not limited to, sodium thiosulfate, potassium thiosulfate, cobalt acetate, copper acetate, lead acetate, cupric chloride, ferric chloride, calcium iodide, potassium iodide, silver nitrate, and combinations thereof. The total concentration of the salts is between 0% and 7%, but is not limited thereto, with the preferred concentration being between 2% and 5%, depending on the desired application.
[0042] The oxalic wax can be cast, prilled, or extruded into pieces of the desired size. If desired, these particles may be coated with an inert material. This may be done to facilitate packaging, extend shelf life, or provide some protection over a wider range of temperatures.
[0043] (Example) Unless otherwise indicated, all numbers expressing quantities of ingredients, reaction conditions, and so forth used in the specification and claims are to be understood as modified by the term "about." Accordingly, unless otherwise indicated, the numerical parameters set forth in the following specification and appended claims are approximations that may vary depending upon the desired properties sought to be obtained by the present disclosure.
[0044] As used herein, the use of "about" includes values or amounts up to 20% higher or lower than the stated value, concentration, or amount.
[0045] As used herein, the light emitted by the marking system was measured using a light meter with a probe selected according to the light emitted (infrared, visible, etc.). For example, for emissions in the visible spectrum, an irradiance probe was used. One of ordinary skill in the art would know how to select an appropriate probe to measure the wavelength of light that the marking system is designed to emit. All temperatures are reported in degrees Celsius. All percentages are by weight.
[0046] The general procedure for making the oxalic acid mixture is as follows: Solvents (non-solid and solid) were placed in a suitable vessel equipped with a means of heating and stirring and purged with nitrogen to reduce moisture. Contents were heated and stirred until homogenous. Polyethylene, paraffin wax, or other organic rheology modifier was added. Heat was increased as necessary to dissolve these materials. Dye was added and stirred until completely dissolved. Upon completion, internal temperature was adjusted to below 120°C as needed. Oxalate salt (CyHMPO or CBzPO) was added and stirred to dissolve. Heat was turned off and sodium thiosulfate was immediately added. Fumed silica was added and stirrer speed was increased. Stirring was continued until the mixture was cool enough to pour into a container or mold.
[0047] The general procedure for making the activator mixture is as follows: Solvents (non-solid and solid) were placed in a suitable vessel equipped with a means of heating and stirring and purged with nitrogen to reduce moisture. The contents were heated and stirred until homogeneous. Polyethylene, paraffin wax, or other organic rheology modifiers were added. Heat was increased as necessary to dissolve these materials. The desired catalyst was added and stirred until fully incorporated. The heat of the mixture was reduced to below 90°C if heated above that temperature to incorporate materials. Peroxygen was added. Mixing speed was increased and fumed silica was added as needed. The mixture was stirred continuously until it was cool enough to be poured into containers or molds.
[0048] The light output of the various formulations was measured in the following manner. The procedure involved mixing equal amounts of oxalate wax and activator wax in a beaker with a flat-edged spatula for 2-5 minutes until a homogenous mixture was obtained. This mixture was then poured into an aluminum mold that allowed it to be placed on a polypropylene mesh on card stock. This resulted in a wax slab approximately 1 / 8 inch thick. Once the mold was removed, the card stock containing the wax could be mounted on a holder that maintained a constant distance from the detector for all tests. All values are in lux.
[0049] (Example 1: Gel Marking System) An exemplary embodiment of the gel marker includes a gel oxalate mixture and a gel activator mixture. The oxalate gel mixture was made using a solution of butyl benzoate containing 0.2% 2-methyl-9,10-bis(phenylethynyl)anthracene (MBPEA). This was warmed to dissolve 5% CBzPO. As the mixture cooled, 8% fumed silica was added in small increments using a high shear mixer. Once the mixture was cool enough, it was placed in a container for distribution or storage.
[0050] A gel activator mixture was made using 5% of triethyl citrate and 50% hydrogen peroxide without any stabilizer. To this, 0.06% sodium salicylate was added. After addition, the high shear mixer speed was increased and 8% fumed silica was added in small increments until the mixture was homogenous. This was then placed in a container for distribution or storage.
[0051] (Example 2: Wax marking system) A two-component chemiluminescence system was prepared consisting of a wax-oxalate mixture consisting of 14.5% microcrystalline wax, 19.5% didodecyl succinate, 19.5% low-density polyethylene wax, 29% butyl benzoate, 0.33% 2-methyl-9,10-bis(2-phenylethynyl)anthracene, 0.02% rubrene, 0.1% hydrophobic fumed silica, 12% CyHMPO, and 5% sodium thiosulfate; and a wax activation system consisting of 32.5% glycerol tribenzoate, 39% triethyl citrate, 13.3% microcrystalline wax, 2.5% hydrophobic fumed silica, 2.5% hydrophilic fumed silica, 10% 50% hydrogen peroxide, and 0.2% sodium salicylate.
[0052] The two-component chemiluminescence system was tested by thoroughly mixing 2g of the wax oxalate mixture with 2g of the wax activator mixture for 5 minutes to obtain a consistent composition. This was placed onto a test card using a mold. The test card was placed into a holder used for the light output reading (LOP). The data collected is shown in Table 10 (see Figure 1). All values are in lux.
[0053] (Example 3: Wax marking system) A two-part chemiluminescent wax marking system was prepared containing an oxalate wax mixture consisting of 26% microcrystalline wax, 34.7% cetyl palmitate, 28.9% butyl benzoate, 0.4% 2-methyl-9,10-bis(2-phenylethynyl)anthracene, 0.02% rubrene, and 10% CBzPO; and a wax activator system consisting of 33.3% glycerol tribenzoate, 39.1% triethyl citrate, 12.7% microcrystalline wax, 2.4% hydrophobic fumed silica, 2.4% hydrophilic fumed silica, 9.8% 50% aqueous hydrogen peroxide, and 0.2% sodium salicylate.
[0054] Experiments were also conducted simultaneously to demonstrate the water resistance of these formulations. The containers used to mix these waxes were filled halfway with water and observed in a dark room while light output experiments were conducted (see Figure 1). During the experiments, the waxes submerged in water continued to glow with an intensity similar to that of the wax above the water surface. As a result, moderate moisture is not expected to dramatically affect the performance of the formulations in outside laboratory conditions.
[0055] (Example 4: Wax marking system) A two-component chemiluminescent wax marking system was prepared consisting of a wax-oxalate mixture consisting of 15% microcrystalline wax, 20% didodecyl succinate, 29.6% butyl benzoate, 20% LDPE wax, 29.5% butyl benzoate, 0.4% 2-methyl-9,10-bis(2-phenylethynyl)anthracene, 0.1% hydrophobic fumed silica, 5% sodium thiosulfate, and 10% CBzPO; and a wax activator system consisting of 32.5% glycerol tribenzoate, 39% triethyl citrate, 13.3% microcrystalline wax, 2.5% hydrophobic fumed silica, 2.5% hydrophilic fumed silica, 10% 50% hydrogen peroxide, and 0.2% sodium salicylate.
[0056] A sample mixture (14, see Figures 3A-3G) of 1g of oxalic acid wax mixture and 1g of wax activator mixture was mixed as described in the previous example. Half of this was spread on a steel plate 16 that had been conditioned overnight in a freezer (-16°C) and the other half was spread on a similarly treated piece of plywood (not shown). To document their performance, photographs were taken first and then at hourly intervals over a period of 5 hours. See Figures 3A-3G. After each photograph was taken, the wood and steel were immediately placed back in the freezer. Good light was produced during the 5 hours the materials were tested. Figures 3A-3G show the test results for the metal. The test results for the wood were similar.
[0057] While particular forms of the invention are illustrated, it should be understood that the invention is not limited to the particular forms or configurations described and illustrated herein. It will be apparent to those skilled in the art that various modifications can be made without departing from the scope of the invention, and that the invention should not be considered as limited to what is shown and described in the specification and any figures / figures contained herein.
[0058] Those skilled in the art will readily appreciate that the present invention is well adapted to carry out the objects and obtain the ends and advantages mentioned, as well as those inherent therein. The embodiments, methods, procedures, and techniques described herein are representative of presently preferred embodiments, are intended to be illustrative, and are not intended to limit the scope of the invention. Those skilled in the art will envision modifications and other uses which are encompassed within the spirit of the invention and are defined by the appended claims. Although the invention has been described in connection with certain preferred embodiments, it should be understood that the invention as claimed should not be unduly limited to such specific embodiments. Indeed, various modifications of the described modes for carrying out the invention which are obvious to those skilled in the art are intended to be within the scope of the following claims.
Claims
1. A chemiluminescent marking system that is moisture resistant and has a wide operating temperature range, a first portion having at least one oxalate ester comprising at least one bis{3,4,6-trichloro-2-[(phenylmethoxy)carbonyl]phenyl}oxalate or bis{3,4,6-trichloro-2-[(cyclohexylmethoxy)carbonyl]phenyl}oxalate and at least one fluorescent agent; and a second part comprising at least one peroxide and at least one catalyst; having Contact between the first portion and the second portion results in the generation of chemiluminescence. A chemiluminescent marking system comprising:
2. 2. The moisture resistant, wide operating temperature range chemiluminescent marking system of claim 1, wherein one or more components of the first portion are in a prilled form.
3. 10. The moisture resistant, wide operating temperature range chemiluminescent marking system of claim 1, wherein one or more components of the first part are in encapsulated form.
4. 2. The moisture resistant, wide operating temperature range chemiluminescent marking system of claim 1, wherein one or more components of the second portion are in a prilled form.
5. 10. The moisture resistant, wide operating temperature range chemiluminescent marking system of claim 1, wherein one or more components of the second part are in encapsulated form.
6. 2. The moisture resistant, wide operating temperature range chemiluminescent marking system of claim 1, wherein the marking system is in the form of a gel.
7. 10. The moisture resistant, wide operating temperature range chemiluminescent marking system of claim 1, wherein said marking system is in the form of a wax.
8. 2. The moisture resistant, wide operating temperature range chemiluminescent marking system of claim 1, wherein the first part further comprises at least one organic salt that generates heat upon combination with the at least one peroxide.
9. 9. The moisture resistant, wide operating temperature range chemiluminescent marking system of claim 8, wherein the at least one organic salt that generates heat in combination with the at least one peroxide comprises sodium thiosulfate, potassium thiosulfate, cobalt acetate, copper acetate, lead acetate, cupric chloride, ferric chloride, calcium iodide, potassium iodide, silver nitrate, or combinations thereof.
10. 10. The moisture resistant, wide operating temperature range chemiluminescent marking system of claim 1, wherein the first part, the second part, or a combination thereof, comprises one or more rheology adjusting agents.
11. The moisture resistant, wide operating temperature range chemiluminescent marking system of claim 10, characterized in that the one or more rheology adjusting agents include one or more resins, one or more fumed silicas, one or more low melting point fatty acid esters, one or more glyceryl triesters, polyethylene wax, or one or more paraffins.
12. 2. The moisture resistant, wide operating temperature range chemiluminescent marking system of claim 1, wherein the at least one peroxide is hydrogen peroxide, sodium peroxide, sodium perborate, sodium pyrophosphate peroxide, urea peroxide, histidine peroxide, t-butyl hydroperoxide, peroxybenzoic acid, sodium percarbonate, or a mixture thereof.
13. 2. The moisture resistant, wide operating temperature range chemiluminescent marking system of claim 1, wherein the first portion or the second portion is stored in a delivery vehicle.
14. 2. The moisture resistant, wide operating temperature range chemiluminescent marking system of claim 1, wherein the bis{3,4,6-trichloro-2-[(phenylmethoxy)carbonyl]phenyl}oxalate or the bis{3,4,6-trichloro-2-[(cyclohexylmethoxy)carbonyl]phenyl}oxalate includes pure purified compounds, prilled particles, spray-dried particles, polymer-coated prilled particles, and polymer-coated spray-dried particles.
15. 1. A chemiluminescent gel marking system comprising: a first chemiluminescent reactant component having a chemiluminescent reactant gel including at least one oxalate ester including bis{3,4,6-trichloro-2-[(phenylmethoxy)carbonyl]phenyl}oxalate or bis{3,4,6-trichloro-2-[(cyclohexylmethoxy)carbonyl]phenyl}oxalate, at least one fluorescent agent, and one or more rheology adjusting reagents; and a second chemiluminescent reactant component having a chemiluminescent reactant gel including at least one peroxygen, at least one catalyst, and one or more rheology adjusting reagents; having contact of the first chemiluminescent reactant component with the second chemiluminescent reactant component results in the generation of chemiluminescent light; A chemiluminescent gel marking system comprising:
16. 16. The chemiluminescent gel marking system of claim 15, wherein said first chemiluminescent reactant component further comprises at least one organic salt that combines with said peroxygen to generate heat.
17. 1. A chemiluminescent wax marking system comprising: a first chemiluminescent reactant component having a chemiluminescent reactant wax comprising at least one oxalate ester comprising bis{3,4,6-trichloro-2-[(phenylmethoxy)carbonyl]phenyl}oxalate or bis{3,4,6-trichloro-2-[(cyclohexylmethoxy)carbonyl]phenyl}oxalate, at least one fluorescent agent, and one or more rheology adjusting agents; and a second chemiluminescent reactant component having a chemiluminescent reactant wax that includes at least one peroxygen, at least one catalyst, and one or more rheology adjusting agents; having contact of the first chemiluminescent reactant component with the second chemiluminescent reactant component results in the generation of chemiluminescent light; A chemiluminescent wax marking system comprising:
18. 20. The chemiluminescent wax marking system of claim 17, wherein said first chemiluminescent reactant component further comprises at least one organic salt that combines with said peroxygen to generate heat.
19. 20. The chemiluminescent wax marking system of claim 17, wherein the first chemiluminescent reactant component is cast or prilled.
20. 20. The chemiluminescent wax marking system of claim 17, wherein the first chemiluminescent reactant component is extruded into small pieces.
21. 20. The chemiluminescent wax marking system of claim 17, wherein said first chemiluminescent reactant component is coated with an inert material.
Citation Information
Patent Citations
Luminous paper, making method thereof and method for drawing luminous color pattern
CN106087549A
Chemiphotogenerating formulation and apparatus containing side-chain oxalate esters
JP2013507451A
Viscous chemiluminescent component and distribution means
JP2014501921A
Combined thermal and chemiluminescent reaction system
US20120097063A1
Chemical lighting system comprising a polymeric chemiluminescent composition and an activating liquid comprising hydrogen peroxide
US3816325A