Process and associated equipment for producing steel strip for electrical applications
Patent Information
- Application Number
- JP2024520941
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-10-07
- Filing Date
- 2022-10-06
- Publication Date
- 2024-11-20
AI Technical Summary
Existing coating equipment for electrical steel strips is limited by variations in line speed due to integration with annealing furnaces, leading to non-uniform varnish layers and restricted production line speeds.
A device comprising a coating roll and an applicator roll, with specific surface patterns and hardness, ensures uniform varnish application over a wide range of line speeds by using a chamber doctor blade system and synchronized roll rotation, maintaining optimal contact pressure and viscosity control.
Achieves uniform varnish coating across the width of the steel strip without patterns, allowing for a wide range of line speeds and improved production efficiency.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an apparatus and a method for the continuous production of steel strip coated with a homogeneous varnish layer for electrical applications. [Background technology]
[0002] The term "electrical applications" relates to the use of steel strip for manufacturing articles with specific magnetic properties, such as the stators and rotors of electric motors, transformers, and wind turbines. Steels for electrical applications are also known as electrical steels and generally contain 0 to 6 weight percent silicon. Electrical steels can be divided into two categories: non-oriented steels and oriented steels.
[0003] Electrical steel is usually coated with a varnish to insulate the steel, to prevent electrical flow and to reduce eddy currents. The varnish is generally an aqueous solution containing 25-75 weight percent resin and 5-15 weight percent solvent (such as alcohol), with the remainder consisting of water. The varnishing process comprises at least two steps, in the first step the varnish is coated in the form of a wet film, and in the second step the varnish is cured to obtain a net-like dry film. The thickness of the wet film is usually 1.5 μm to 15 μm, to obtain a dry film thickness of 0.8 μm to 5 μm.
[0004] In the manufacturing process, varnishing is performed after annealing. Depending on the architecture of the manufacturing line, the varnishing section may or may not be coupled with the annealing furnace. Whether the varnishing section is coupled with the annealing furnace or not affects the manufacturing line speed. Furthermore, the varnish needs to be reticulated in the drying step at peak metal temperature (PMT), which also limits the maximum line speed. As a result, the line speed is limited to 30-300 m.min -1 can vary up to
[0005] The '196 patent is directed to coating a thin, uniform layer of insulating lacquer on electrical steel strip at high speeds in a consistent manner. The apparatus includes an engraved pick-up roll and an applicator roll having a substantially flat surface without grooves or other indentations.
[0006] EP 3143179 discloses a process and equipment for uniformly coating packaging steel with a passivation layer. The apparatus comprises a chamber doctor blade, a coating roll and an applicator roll. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] U.S. Patent No. 6,277,196 [Patent Document 2] European Patent No. 3143179 Summary of the Invention [Problem to be solved by the invention]
[0008] The object of the present invention is to provide an apparatus and a method which allows uniform varnishing of electrical steel strip for a wide range of line speeds. As a result, the varnish layer on the steel should not exhibit any patterns. In fact, most of the coating installations for electrical steel are coupled with annealing furnaces which leads to line speed variations. [Means for solving the problem]
[0009] This is achieved by providing an apparatus according to any one of claims 1 to 6. This is also achieved by providing a method according to any one of claims 7 to 14.
[0010] Other features and advantages will become apparent from the following description of the invention. [Brief description of the drawings]
[0011] [Figure 1] FIG. 1 illustrates one embodiment of the present invention. [Diagram 2] FIG. 2 illustrates a second embodiment of the present invention. [Diagram 3] FIG. 1 shows the effect of applicator roll hardness and speed line on maximum varnish thickness. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] The invention relates to a coating installation 1 for the continuous production of varnish-coated steel strip S for electrical applications, comprising a tank 2, a coating roll 3 and an applicator roll 4, as shown in FIG. The tank 2 is configured to contain a varnish solution and the coating roll 3 is in contact with the varnish solution; The covering roll 3 is configured to contact the applicator roll 4 and to transfer the varnish onto the applicator roll 4 uniformly in the strip width direction, The applicator roll 4 is configured to contact the steel strip S and to uniformly coat the strip across its width, the surface of the applicator roll having a hardness of 40 to 60 Shore A.
[0013] 2 shows a steel strip S proceeding through a varnishing installation along a direction D. The strip first passes through a coating device 1 intended to apply a varnish solution and then a drying unit 5 intended to remove the water content of the varnish and then to reticulate the varnish. A device 6 for measuring the thickness of the coated varnish can be arranged between the coating device 1 and the drying unit 5 and can be connected to a control unit 9 of the coating device 1.
[0014] In the embodiment shown in FIG. 2, the coating apparatus 1 is capable of coating two sides of the strip simultaneously, however, in alternative embodiments, the coating apparatus 1 may be comprised of only the left side portion 1A or the right side portion 1B of the apparatus so as to coat only a single side of the strip.
[0015] An embodiment of the left part 1A of the coating device 1 is shown in Figure 1. The right part 1B is not depicted since it is symmetrical to the left part 1A with respect to the strip S.
[0016] As shown in Fig. 1, the device consists of a first roll 4, which is an applicator roll 4, which is in contact on the one hand with the strip S and on the other hand with a second roll 3, which is a covering roll 3. During the production process, the covering roll 3 rotates and is in contact with the varnish solution contained in a tank 2, which is deposited on the strip S. Contact between the covering roll and the varnish solution can be achieved by immersing said covering roll in said varnish solution. The tank 2 is preferably equipped with a wiping device which squeezes the solution onto the surface of the covering roll 3.
[0017] The wiping device makes it possible to ensure that the coating roll 3 is coated with the required amount of solution, which is deposited to obtain the required wet varnish thickness. This wiping device is preferably equipped with a doctor blade. This device can consist of two blades, for example a first blade, which is located at the point where the coating roll 3 enters the tank 2 and allows to remove the residual varnish solution remaining from the previous passage of the coating roll 3 through the tank 2, and a second blade, which is located at the point where the coating roll 3 leaves the tank 2 and allows to remove the excess solution. The blades can be made, for example, of plastic, stainless steel or carbon fiber. The device can also be a single blade, for example a stainless steel blade, which is located at the point where the coating roll 3 leaves the tank 2.
[0018] The tank is preferably a chamber doctor blade, as shown in Figure 1. The chamber doctor blade system uses two doctor blades with an enclosed varnish chamber to distribute the varnish to the coated roll. Typically, the first blade acts as a metering blade, wiping excess varnish from the coated roll, and the second blade acts as a capture or containment blade, retaining the varnish within the chamber.
[0019] This varnish solution has a viscosity of 2.5 × 10 at 20 °C. -2 4.0 x 10 at Pa.s ~20°C -1 In a first example, the solution contains 30-50% by weight of dry extract, which is composed of acrylic resin and phosphate pigment, 5-10% by weight of co-solvent (alcohol), and the remainder is water. In another example, the solution contains 40-60% by weight of dry extract, which is a mixture of polyurethane resin with aluminum and silicon oxide, 5-10% by weight of co-solvent (alcohol), and the remainder is water.
[0020] The covering roll 3 is a ceramic coated roll with an engraved surface. More precisely, the covering roll 3 is engraved with any pattern or cell structure. For example, the pattern can be hexagonal cells of 60° or 30° or 70°, a line pattern, a cobra pattern. The cells of the covering roll are filled with a varnish solution. The surface of the covering roll can be made of ceramic. The cells of the covering roll can be etched with a laser or a mechanical tool.
[0021] Even if the covering roll is patterned, it is designed to transfer the varnish uniformly onto the applicator roll, meaning that the pattern is not transferred to the applicator roll, resulting in a uniform varnish thickness across the width.
[0022] In a first preferred embodiment, the covering roll 3 has a plurality of 60° hexagonal shaped cells, the number of lines is 50 to 200 lines / centimeter, and the volume is 5×10 per square meter of the roll surface. -6 ~6×10 -5 m 3 , preferably 1×10 per square meter of roll surface -6 ~5×10 -5 m 3 It is.
[0023] In a second preferred embodiment, the coating roll 3 has a roll surface 1 m2 1x10 -5 ~8×10 -5 m 3 It has a cobra pattern with a cell volume of
[0024] In a third preferred embodiment, the coating roll 3 has a roll surface 1 m 2 1x10 -5 ~4×10 -5 m 3 The cell has a square pattern with a cell volume of .
[0025] The surface of the covering roll 3 coated with the varnish solution comes into contact with the applicator roll 4 after passing through the tank 2. The covering roll 3 can rotate either clockwise or vice versa. The applicator roll 4 itself is preferably driven in the opposite direction of rotation to the one of the covering rolls 3.
[0026] The applicator roll 4, or at least its surface, is preferably made of a material that allows optimal transfer of the solution, i.e., transfer that minimizes loss of the solution, for example due to absorption by the material from which the roll or its surface is made, or, conversely, due to excessive slippage of the solution on the surface of the roll. This material may also exhibit resistance to chemicals as well as to mechanical wear. Preferably, the applicator roll 3 is made of an elastomer. In a first preferred embodiment, the applicator roll is made of chlorosulfonated polyethylene. In a second preferred embodiment, the applicator roll is made of polyurethane.
[0027] The applicator roll is configured to uniformly coat the strip across its width so that there is no varnish pattern on the resulting coated strip. To achieve such uniform coating, the applicator roll surface is a substantially flat surface without grooves or other indentations.
[0028] Preferably, the applicator roll 3 has a roughness Ra of 0.5 μm to 3.5 μm. If the applicator roll roughness Ra exceeds 3.5 μm, inhomogeneity of the coated varnish may appear. Even more preferably, the applicator roll has a roughness Ra of 0.6 to 1.5 μm.
[0029] The applicator roll has a hardness of 40 Shore A to 60 Shore A. The hardness can be measured according to the ASTM D2240 standard.
[0030] If the hardness is less than 40 Shore A, the life of the applicator roll due to the coating process is significantly reduced. Preferably, the applicator roll 3 has a hardness of at least 45 Shore A, such a minimum hardness provides a better life and also provides good deformation of the roll resulting in a uniform coating.
[0031] If the hardness is greater than 60 Shore A, the maximum varnish wet thickness becomes too limited, especially at low line speeds.
[0032] Indeed, in figure 3 the maximum varnish wet thickness that can be applied with the application roll is plotted as a function of the speed line. It is plotted for several hardnesses of the roll surface, namely 40 and 60 Shore A (according to the invention) and 80 Shore A. All curves are plotted for a total force applied to the application roll of 3000 N per meter of strip width and a viscosity of 0.12 Pa.s at 20°C.
[0033] For the coating roll according to the invention, the maximum wet thickness that can be coated is at least 30 mm.min. -1 It can be observed that for the velocity lines, the difference is at least 15 μm.
[0034] As a result, the claimed hardness of the applicator roll accommodates a wide range of varnish coating wet thicknesses while still ensuring sufficient durability.
[0035] The invention also relates to a method for the continuous production of varnished steel strip, carried out by an apparatus such as previously described, A layer of varnish is deposited on at least one surface of the strip, the layer of varnish having a wet thickness of 1.5 μm to 15 μm, the varnish having a viscosity of 2.5×10 at 20° C. -2 4.0 x 10 at Pa.s ~20°C -1 It has a viscosity of Pa.s. The coating roll is supplied with varnish by contacting it with the varnish contained in the tank, the applicator roll is in contact with the coating roll and the steel strip, and the steel strip is coated with the coating roll for a period of at least 30 mm.min. -1 Travel at a speed of .
[0036] Preferably, the steel strip is an electrical steel strip. Even more preferably, the steel strip is a non-oriented electrical steel strip. The non-oriented electrical steel strip preferably contains 1.5 to 4 weight percent silicon.
[0037] Preferably, the steel strip has a rolling speed of 30 to 500 mm.min. -1 More preferably, the steel strip is moved at a speed of 30 to 300 m.min. -1 It is traveling at a speed of .
[0038] The contact pressure between the covering roll 3 and the applicator roll 4 must be sufficient to transfer the varnish solution from the covering roll to the applicator roll, but not so great as to cause splashing which may result in loss of solution and thus in a non-optimal transfer of the solution. This pressure between the two rolls can be applied, for example, by means of a cylinder attached to the covering roll 3. The total force F applied to the covering roll 3 is RR It is preferable that the load is 500 to 3000 N per 1 m of the width of the strip.
[0039] Following this contact, the applicator roll 4 is covered with the wet varnish solution which is to be deposited on the strip S.
[0040] The contact pressure between the applicator roll 4 and the strip must not be so high that there is a risk of excessive wiping off of the deposited wet varnish solution film, nor must it be so low that there is a risk of insufficient wetting of the strip with the solution. Furthermore, a minimum pressure must be exerted on the strip by the roll in order to compensate for potential flatness defects of the strip. This pressure between the applicator roll 4 and the strip S can be exerted, for example, by means of at least one cylinder attached to the applicator roll. The total force F exerted on the applicator roll 4 is TB It is preferable that the load is 2000 to 6000 N per meter of the width of the strip.
[0041] The rotation speed of the applicator roll 4 and the covering roll 3 can be synchronized with the displacement speed of the strip.
[0042] In one embodiment of the present invention, the thickness of the deposited wet varnish thickness is measured using a thickness measuring device 6 .
[0043] Additionally, or in an additional embodiment of the invention, the rotation speed of the coating roll 3 can be controlled by a control unit 9 shown in Figure 1. This control unit 9 is connected to a device for measuring the wet varnish thickness. If the thickness is less than the target thickness, the speed of the coating roll 3 is increased and vice versa.
[0044] The thickness can be measured, for example, using electromagnetic radiation gauges, which are preferably installed as close as possible to the coating device 1, since water can evaporate very quickly from the film and cause significant fluctuations in the measurements.
[0045] Following the step of depositing the wet varnish layer, the strip is subjected to a drying step, which is carried out by means of a drying unit 5.
[0046] Preferably, following this drying step, the thickness of the deposited varnish layer is between 0.8 μm and 5 μm after drying.
[0047] This drying unit 5 is for example a drying tunnel equipped with nozzles that inject air towards the coated ribbon at a temperature between 120° C. and 350° C. The drying unit can also be an inductor that raises the temperature of the ribbon to a PMT preferably between 220° C. and 290° C.
Claims
1. A coating installation 1 for the continuous production of varnish-coated steel strip S for electrical applications, comprising a tank 2, a coating roll 3 and an applicator roll 4, The tank 2 is configured to contain a varnish solution and the coating roll 3 is in contact with the varnish solution; The covering roll 3 is configured to contact the applicator roll 4 and to uniformly transfer the varnish onto the applicator roll 4 in the strip width direction; The coating device 1, wherein the coating roll 4 is configured to contact the steel strip S and to uniformly coat the steel strip across the width of the steel strip, and the surface of the coating roll has a hardness of 40 to 60 Shore A.
2. The apparatus of claim 1 , wherein the surface of the applicator roll has a hardness of 40 to 55 Shore A.
3. The apparatus of claim 1 , wherein the surface of the applicator roll is made of an elastomer.
4. The apparatus of claim 3 , wherein the surface of the applicator roll is made of polyurethane.
5. An apparatus according to any one of claims 1 to 4, wherein the reservoir is a chambered doctor blade.
6. An apparatus according to any one of the preceding claims, wherein the tank is equipped with a wiping device (10).
7. A method for the continuous production of varnished steel strip, carried out by an apparatus according to any one of claims 1 to 4, comprising the steps of: A layer of varnish is deposited on at least one surface of the strip, the layer of varnish having a wet thickness of 1.5 μm to 15 μm, the varnish having a viscosity of 2.5×10 at 20° C. -2 Pa.s ~ 4.0 x 10 at 20°C -1 It has a viscosity of 100 Pa.s. The coating roll is supplied with varnish by contacting it with the varnish contained in the tank, the applicator roll is in contact with the coating roll and the steel strip, and the steel strip is fed at a rate of at least 30 m.min. -1 A method of traveling at a speed of.
8. The method of claim 7 , wherein the steel strip is electrical steel.
9. The method of claim 8, wherein the steel strip is a non-oriented electrical steel.
10. The method of claim 7, wherein the varnish is a water-based varnish.
11. 8. The method according to claim 7, wherein the total force exerted on the covering roll to contact the applicator roll is between 500 and 3000 N per meter width of the coated strip.
12. 8. The method according to claim 7, wherein the total force exerted on the applicator roll to contact the strip is between 2000 and 6000 N per meter width of coated strip.
13. 8. The method according to claim 7, wherein after deposition of the varnish, the steel strip is subjected to a drying step.
14. The method according to claim 7, wherein the thickness of the deposited varnish layer is between 0.8 μm and 5 μm after drying.