Nanowire growth
The device with a dual electrolyte permeable layer system ensures uniform nanowire growth on conductive surfaces, addressing issues of lateral growth and stability, facilitating stable connections in electronic components.
Patent Information
- Application Number
- JP2024522112
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-10-12
- Filing Date
- 2022-09-28
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2042-09-28
AI Technical Summary
Existing methods for growing nanowires on conductive surfaces face challenges in achieving uniform growth while minimizing lateral growth and ensuring stability, leading to undesirably large gaps and connections between components.
A device comprising a conductive surface, a foil with flow channels, a first electrolyte permeable layer, and a second electrolyte permeable layer with different compressibility properties is used to evenly distribute electrolyte and press the foil onto the surface, limiting lateral growth and ensuring uniform nanowire formation.
The solution enables uniform and stable growth of nanowires, allowing for strong and close connections between components without the need for high-temperature processes, suitable for applications in electronics like mobile phones and tablets.
Smart Images

Figure 2024538075000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to the growth of nanowires on a surface. [Background technology]
[0002] It is known to grow nanowires on conductive surfaces by electrolytic deposition from an electrolyte. An example is described in US Pat. No. 5,399,663. In this case, a foil is applied to the surface to be grown. The foil has continuous channels, called pores in US Pat. No. 5,399,663. Nanowires can be grown in these channels. The foil can then be removed, for example by etching, to expose the grown nanowires.
[0003] Nanowires can also be used in particular to connect components to one another. For this purpose, nanowires are grown on the surface of one or both components. These components are then bonded together such that the nanowires of one component are connected to the surface of the other component, or such that the nanowires on the surfaces of the two components are connected to one another. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] German Patent Application Publication No. 10 2017 104 906 Summary of the Invention [Problem to be solved by the invention]
[0005] It is desirable for the nanowires to grow uniformly on the surface. This requires that the electrolyte be distributed uniformly on the foil. For this reason, according to Patent Document 1, a sponge is provided as a means for supplying the electrolyte. The electrolyte can be distributed on the foil via the sponge.
[0006] The foil can also be pressed against the surface by the sponge. This is to prevent material from being deposited in undesired locations between the nanowire growth surface and the foil. Without such pressing, material could accumulate between the nanowire growth surface and the foil outside the area where the nanowires are intended to be grown. This effect is referred to below as "lateral growth". If lateral growth is undesired, it may also be called "parasitic lateral growth". Such lateral growth can be prevented by pressing the foil sufficiently hard against the nanowire growth surface. However, this approach can clog the pores of the sponge or block the channels in the foil, resulting in non-uniform nanowire growth.
[0007] Despite these problems of lateral growth, it is desirable to press the foil against the surface to be grown during nanowire growth. This allows the nanowire to grow directly on the surface. If the foil is not placed flush on the surface on which the nanowire is to be grown, excess material will accumulate between the growth surface and the foil. This can lead to instability of the nanowire. Furthermore, thickened areas of the deposited material may form early on, sometimes called bumps. These bumps can lead to undesirable large gaps between the surfaces of the components to be connected. Furthermore, these bumps can only allow components to be connected at a relatively large distance from each other. In particular, in the case of contacts with areal extent, the geometric height of the connection or the overall thickness of the components to be connected to each other can be larger than desired. This is particularly important for geometrically challenging modules such as mobile phones, tablets, televisions, etc.
[0008] Although the solution in US Pat. No. 5,633,363 may already give good results, in this case a compromise must nevertheless be found between uniform growth of the nanowires and pressing of the foil onto the growth surface.
[0009] Based on the above-mentioned prior art, it is an object of the present invention to provide a method for growing nanowires particularly uniformly, particularly with little lateral growth and particularly stably.
[0010] This object is achieved by a method and an apparatus as set forth in the independent claims. Further advantageous configurations are set forth in the dependent claims. The features recited in the claims and in the description can be combined with one another in any manner which is technically significant. [Means for solving the problem]
[0011] According to the present invention, there is provided an apparatus for fabricating a plurality of nanowires, the apparatus comprising: A conductive surface; a foil having a plurality of flow channels extending from a first side of the foil to a second side of the foil opposite the first side; a first electrolyte permeable layer; a second electrolyte permeable layer that is more compressible than the first electrolyte permeable layer; and a conductive surface, the conductive surface being arranged in the above order, the conductive surface further comprising an electrode, and the device is configured to grow nanowires on the conductive surface by electrolytic deposition of an electrolyte into each of the channels of the foil by applying a voltage between the conductive surface and the electrode.
[0012] The device allows the production of a plurality of nanowires on a conductive surface, in particular by electrolytic deposition growth. The conductive surface may be part of a conductor. If it is intended to produce nanowires on a non-conductive or poorly conductive object, the surface of the object or part of it may be metallized to obtain a conductive surface.
[0013] A nanowire is taken here to mean any object with a shape similar to a wire and a size in the nanometer range. The nanowire may for example have a circular, elliptical or polygonal base. In particular, the nanowire may have a hexagonal base. The nanowires are preferably made of a metal, for example copper. The nanowires are preferably all made of the same material. The nanowires are preferably perpendicular to the surface. In this case, the nanowires are arranged in a lawn-like manner.
[0014] The nanowires preferably have a length in the range of 100 nm [nanometers] to 100 μm [micrometers], particularly in the range of 500 nm to 50 μm. Furthermore, the nanowires preferably have a diameter in the range of 10 to 10,000 nm, particularly in the range of 30 to 4,000 nm. The "diameter" here refers to the circular base surface, and a similar definition of diameter is used in the case of other base surfaces. It is particularly preferred that all nanowires used have the same length and the same diameter.
[0015] Nanowires can in particular be used to connect components to each other. For example, nanowires can be grown on a contact surface of a first component and on a contact surface of a second component. In this case, the two contact surfaces are used as conductive surfaces of the device. The two components can then be brought into contact with each other so that the nanowires of the two contact surfaces are in contact with each other. Due to the large surface area of the nanowires, a mechanically stable connection is formed, which is either electrically conductive in the case of electrically conductive nanowires or thermally conductive in the case of thermally conductive nanowires, or both. This connection can be made without great expense. In particular, no high temperatures are required, as are required for traditional connection techniques in the electronics industry, for example soldering. This connection can be strengthened by temporarily pressing the components together with high pressure. Alternatively, the components can be connected to each other if the nanowires are grown only on the contact surface of the first component. The components are brought together and heated (for example to at least 90° C.) so that the nanowires are connected to the contact surface of the second component. In both cases, an adhesive can be used to further strengthen the connection.
[0016] The device further comprises a foil having a plurality of channels extending from a first side of the foil to a second side of the foil opposite the first side. Each channel is continuous and extends through the foil. Each channel is arranged and configured in the same way as the nanowires to be grown. The nanowires can be produced by electrolytic deposition growth, filling each channel with material. After the nanowires have been grown, the foil can be removed, for example by etching, to expose the nanowires which may be used, for example, to connect components together.
[0017] The device further comprises a first electrolyte permeable layer and a second electrolyte permeable layer. The two electrolyte permeable layers are used together to distribute the electrolyte evenly on the foil in order to grow each nanowire evenly. The foil may also be pressed onto the conductive surface by the two electrolyte permeable layers to limit lateral growth and prevent excessive accumulation of material between the foil and the conductive surface. By this separation into a first electrolyte permeable layer and a second electrolyte permeable layer, which is more easily compressed, these advantages can be achieved to a certain extent at the same time. The first electrolyte permeable layer is less compressible than the second electrolyte permeable layer. This causes the second electrolyte permeable layer to be compressed in particular when a force is applied to the second electrolyte permeable layer in the direction of the conductive surface. In this case, the foil is pressed onto the conductive surface or the lithography layer or both by the first electrolyte permeable layer. This prevents excessive accumulation of material between the foil and the conductive surface. As a result, the lateral growth is limited. When the second electrolyte permeable layer is compressed, the electrolyte may not be uniformly supplied from the second electrolyte permeable layer onto the first electrolyte permeable layer. However, since the first electrolyte permeable layer is less compressed than the second electrolyte permeable layer, the first electrolyte permeable layer is not compressed as strongly as the second electrolyte permeable layer. This keeps the pores of the first electrolyte permeable layer more open than the pores of the second electrolyte permeable layer. This compensates for the electrolyte supply from the second electrolyte permeable layer to the first electrolyte permeable layer, which may be non-uniform. As a result, the electrolyte is uniformly supplied from the first electrolyte permeable layer onto the foil, and each nanowire can be grown uniformly in each flow path of the foil. The device has two electrolyte permeable layers with different properties. The device may also have three or more electrolyte permeable layers. This allows for a finer functional distribution in the individual electrolyte permeable layers, and the above advantages can be achieved accordingly.
[0018] The foil can be pressed against the conductive surface by the first and second electrolyte permeable layers. This pressing allows the second electrolyte permeable layer to supply the first electrolyte permeable layer and the first electrolyte permeable layer to supply the foil. If there is only one electrolyte permeable layer, it may be easily compressed so that the electrolyte can be supplied by pressing. In this case, the electrolyte permeable layer as a spring system can compensate for local unevenness on the nanowire growth surface or on the foil or both and ensure that the foil is pressed uniformly on the growth surface over the entire growth surface. However, this method increases the density of the electrolyte permeable layer with increasing applied force, resulting in the formation of zones inside the electrolyte permeable layer that are difficult for the electrolyte to access. This can lead to local depletion of electrolyte during nanowire growth. This can lead to non-uniform nanowire growth. Furthermore, the pores of the electrolyte permeable layer can become clogged or the flow channels of the foil can become blocked.
[0019] Alternatively, the electrolyte permeable layer may be compressible to such an extent that the above mentioned drawbacks do not occur. In this case, the microcavities of the electrolyte permeable layer can remain constant as the applied force increases. This allows good electrolyte mixing in the electrolyte permeable layer to be achieved over a wide range of applied forces. However, a drawback of a less compressible electrolyte permeable layer is that it cannot adequately compensate for the unevenness of the nanowire growing surface and / or foil. Thus, there may be zones on the growing surface where the foil is pressed quite firmly onto the growing surface and zones where there are still gaps between the surface and the foil.
[0020] The device overcomes the aforementioned drawbacks. By combining two electrolyte permeable layers, on the one hand, a spring effect can be achieved to compensate for unevenness. On the other hand, clogging of the foil flow paths can be prevented even when a large force is applied, and good electrolyte mixing can be maintained. This is because the electrolyte can first be roughly spread by the second electrolyte permeable layer and then dispensed by pressing the second electrolyte permeable layer onto the first electrolyte permeable layer. The first electrolyte permeable layer can then be configured to dispense the electrolyte well, even though it only needs to be finely spread and is difficult to compress. In the first electrolyte permeable layer, which is difficult to compress, the pores can be more easily kept open.
[0021] The first electrolyte-permeable layer preferably has negligible compressibility, sometimes referred to as incompressible, which should be understood to mean that the first electrolyte-permeable layer is not significantly compressed by forces normally encountered during operation of the device.
[0022] The first electrolyte permeable layer and the second electrolyte permeable layer are permeable to the electrolyte. This is not limited to a specific direction. In particular, the electrolyte can not only permeate the first electrolyte permeable layer and the second electrolyte permeable layer in a direction perpendicular to the conductive surface, but also move parallel to the conductive surface inside the first electrolyte permeable layer or inside the second electrolyte permeable layer. Thus, the electrolyte can spread parallel to the conductive surface by the first electrolyte permeable layer and the second electrolyte permeable layer. This allows each nanowire to grow particularly uniformly. The first electrolyte permeable layer and the second electrolyte permeable layer are preferably porous, which can also be said to have an originally open structure.
[0023] The first electrolyte permeable layer and the second electrolyte permeable layer are preferably porous. In that case, these layers may be called the first porous layer and the second porous layer. Here, the term "porous" means that the first electrolyte permeable layer and the second electrolyte permeable layer are porous and can allow the electrolyte to permeate therethrough.
[0024] The first electrolyte permeable layer and / or the second electrolyte permeable layer may each be formed as a fabric.
[0025] The foil is preferably configured to be permeable to the electrolyte only in a direction perpendicular to the foil. The electrolyte cannot therefore move parallel to the conductive surface through the foil. This distinguishes the foil in particular from the first and second electrolyte permeable layers. The foil is therefore not porous in the sense of the term. To emphasise this, the foil channels are not referred to as pores here. The foil channels are preferably not branched from each other. The channels are preferably separated from each other. The channels therefore do not form a network of channels that branch or are connected to each other.
[0026] The device further comprises an electrode. The device preferably further comprises a voltage source connected on the one hand to the conductive surface and on the other hand to the electrode, by means of which a voltage can be applied between the conductive surface and the electrode for growing each nanowire.
[0027] The components of the device are arranged in the following order: conductive surface, foil, first electrolyte permeable layer, second electrolyte permeable layer, preferably followed in this order by an electrode following the second electrolyte permeable layer.
[0028] The electrode is preferably located on the second electrolyte permeable layer. However, it is also conceivable, for example, to provide an intermediate layer between the electrode and the second electrolyte permeable layer, for example in the form of a further electrolyte permeable layer. The second electrolyte permeable layer is preferably located on the first electrolyte permeable layer. However, it is also conceivable, for example, to provide an intermediate layer between the second electrolyte permeable layer and the first electrolyte permeable layer, for example in the form of a further electrolyte permeable layer. The first electrolyte permeable layer is preferably located on the foil. However, it is also conceivable, for example, to provide an intermediate layer between the first electrolyte permeable layer and the foil, for example in the form of a further electrolyte permeable layer. In both cases, "located" means that there is a direct contact between the respective components.
[0029] The foil may be located on the conductive surface, although this is not essential. This is particularly true if the conductive surface is formed in a recess in the lithographic layer. In that case, the foil is preferably located on the lithographic layer. Depending on the configuration of the lithographic layer and the conductive surface, an open space may be formed between the conductive surface and the foil. During the growth of the nanowires, this open space is filled with the material of the nanowire. Only afterwards does the channel of the foil fill with said material.
[0030] The conductive surface, the foil, the first electrolyte-permeable layer and the second electrolyte-permeable layer preferably form a layer structure. The direction perpendicular to the conductive surface may be called the stacking direction. The foil, the first electrolyte-permeable layer and the second electrolyte-permeable layer are preferably formed perpendicular to the stacking direction, respectively. This is particularly true in the preferred case where the foil is constructed in layers. The electrodes are also preferably part of the layer structure. The electrodes are also preferably constructed as layers, in particular perpendicular to the stacking direction.
[0031] The device is configured to grow nanowires on the conductive surface by applying a voltage between the conductive surface and the electrode, resulting in electrolytic deposition of an electrolyte in each of the foil's channels. The nanowires can be grown by providing an electrolyte. The electrolyte is preferably a liquid capable of electrolytically depositing the material of the nanowires. During the growth of the nanowires, the electrolyte is arranged in such a way that both the electrode and the conductive surface are in contact with the electrolyte and are connected to each other via the electrolyte. This is possible in particular by filling the channels of the foil, the pores of the first electrolyte permeable layer and the pores of the second electrolyte permeable layer with the electrolyte. For example, the electrolyte may be introduced into the second electrolyte permeable layer and spread over the channels of the foil by the second electrolyte permeable layer and the first electrolyte permeable layer. The device may for example comprise a chamber for the electrolyte. This chamber is filled with the electrolyte during the growth of the nanowires.
[0032] The device allows nanowires to be provided over a large area of the substrate. However, the device is also particularly suitable for growing nanowires on structured substrates. For example, the surface of the substrate can be structured by lithographic means in such a way that the nanowires grow only in recesses in the lithographic layer. The device allows particularly strong restriction of lateral growth, so that regions with nanowires can be arranged particularly close together without electrical contact between adjacent regions with nanowires. For example, the conductive pads are spaced apart from one another by a small distance and are electrically insulated from one another, but on these conductive pads the nanowires can be grown without lateral growth that would short-circuit the conductive pads. The device thus allows nanowires to be grown in order to connect components with a number of electrical contacts to one another. The conductive pads on which the nanowires are grown allow the formation of a number of electrically conductive connections between two components that are separate from one another, which at the same time connect the components to one another mechanically strong or thermally conductive or both.
[0033] In one preferred embodiment of the device, the first electrolyte permeable layer and the second electrolyte permeable layer are configured to be porous, with the second electrolyte permeable layer having a larger average pore size than the first electrolyte permeable layer.
[0034] In this embodiment, the second electrolyte permeable layer is more porous than the first electrolyte permeable layer. This results in the second electrolyte permeable layer having a relatively large average pore size. The second electrolyte permeable layer is therefore highly permeable to the electrolyte, which allows the electrolyte to spread particularly well. However, if the second electrolyte permeable layer is located directly on the foil, a large pore size is disadvantageous. When the second electrolyte permeable layer is pressed onto the foil, some of the multiple flow paths of the foil may be blocked by the material of the second electrolyte permeable layer. To prevent this, the first electrolyte permeable layer is provided. Since its pores are smaller, it is more likely that the electrolyte is actually supplied to each of the flow paths through one of the pores of the first electrolyte permeable layer. This is also due to the fact that the first electrolyte permeable layer is less compressible than the second electrolyte permeable layer. Therefore, even when a relatively large pressing force is applied, the pores of the first electrolyte permeable layer remain open.
[0035] In the uncompressed state, the first electrolyte permeable layer preferably has a number of pore openings on its surface such that there are, on average, multiple pore openings within an area the size of the cross-sectional area of one flow channel in the foil, and thus each flow channel may be supplied with electrolyte via multiple pore openings.
[0036] The second electrolyte permeable layer preferably has an average pore size 1 to 20 times larger than that of the first electrolyte permeable layer.The second electrolyte permeable layer preferably has pores 1 to 20 times larger than that of the first electrolyte permeable layer.
[0037] The pores of the second electrolyte permeation layer preferably have a size in the range of 30 to 400 nm, and particularly preferably in the range of 100 to 220 nm.
[0038] In another preferred embodiment of the device, in the uncompressed state, the second electrolyte permeable layer extends longer in a direction perpendicular to the conductive surface than the first electrolyte permeable layer.
[0039] As a result, the uncompressed second electrolyte permeable layer has a larger extent in the stacking direction than the uncompressed first electrolyte permeable layer. This can also be said to mean that the second electrolyte permeable layer is thicker than the first electrolyte permeable layer when both are uncompressed. In the uncompressed state, the second electrolyte permeable layer extends 2 to 20 times longer than the first electrolyte permeable layer in the direction perpendicular to the conductive surface.
[0040] It was found that the best results were obtained in terms of uniformity of growth of each nanowire and limitation of lateral growth by dividing it between the first and second electrolyte permeable layers as described above. The second electrolyte permeable layer is relatively large and can be compressed sufficiently. The first electrolyte permeable layer, which is less compressible, does not need to be larger to perform its function. This is because the electrolyte only needs to be finely spread in the first electrolyte permeable layer.
[0041] In another preferred embodiment of the device, the first electrolyte permeable layer is formed from cellulose.
[0042] It has been found that cellulose is a particularly suitable material for the first electrolyte permeable layer. It is therefore preferred that the first electrolyte permeable layer is formed solely from cellulose. However, the above-mentioned advantages are already achieved if the first electrolyte permeable layer has a certain proportion of cellulose. It is preferred that the first electrolyte permeable layer is formed to at least 50% from cellulose.
[0043] In another preferred embodiment of the device, the second electrolyte permeable layer is a sponge.
[0044] In another preferred embodiment, the apparatus further comprises a pressing device for generating a force in the direction of the conductive surface in the second electrolyte permeable layer.
[0045] The pressing device preferably comprises a plunger. With this pressing device the layers of the layer structure described above can be compressed. This makes it possible in particular to press the foil onto the conductive surface, for example onto the lithographic layer. It is thus possible to prevent lateral growth. If an electrode is located on the second electrolyte permeable layer, the plunger preferably engages the electrode. The electrode may be part of the plunger.
[0046] Instead of a pressing device, the second electrolyte permeable layer can also be pressed, for example manually, towards the conductive surface.
[0047] In another preferred embodiment, the apparatus further comprises a substrate having a lithographic layer, the lithographic layer having one or more recesses, and the conductive surface being formed in the recess or recesses.
[0048] This lithography layer is preferably located on a substrate. The foil is preferably located on the lithography layer. The conductive surface on which the nanowires are grown is formed in a recess or recesses of the lithography layer. The substrate is preferably a semiconductor substrate, for example made of silicon. This substrate may be configured as a wafer. To obtain a conductive surface, the substrate may be metallized in the recess or recesses of the lithography layer. This allows the growth of the nanowires to be locally restricted. If the substrate itself is already conductive, the substrate surface in the recess or recesses of the lithography layer itself can be considered as a conductive surface on which the nanowires are grown. The lithography layer preferably has a size in the range of 0.1 to 10 μm [micrometers] in the direction perpendicular to the conductive surface.
[0049] In particular, in this embodiment, an open space may be formed between the conductive surface and the foil, during nanowire growth this open space is filled with nanowire material, and then nanowires are also grown in each of the channels of the foil.
[0050] The lithography layer preferably has a plurality of recesses. The recesses are preferably arranged regularly. In this case, the pitch is preferably within the range of 1 to 10 μm [micrometers]. The pitch here refers to the center distance between adjacent recesses.
[0051] According to a further aspect of the invention, a method is proposed for producing a plurality of nanowires using the apparatus constructed as described above, in which nanowires are grown on a conductive surface by electrolytic deposition from an electrolyte in each of the channels of the foil by applying a voltage between the conductive surface and an electrode.
[0052] The above-mentioned advantages and features of the apparatus are applicable and transferable to the present method and vice versa. The apparatus is preferably configured to operate in accordance with the present method.
[0053] In one preferred embodiment of the method, the second electrolyte permeable layer is at least temporarily pressed towards the conductive surface.
[0054] The invention will now be explained in more detail with the aid of the figures, which show preferred exemplary embodiments, to which the invention is not limited, and the figures and the size ratios shown are only approximate. [Brief description of the drawings]
[0055] [Figure 1] FIG. 1 shows an apparatus according to the present invention for producing a plurality of nanowires. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0056] FIG. 1 shows an apparatus 1 for producing a plurality of nanowires 2: The device 1 comprises a substrate 12 with a lithographic layer 13. The lithographic layer 13 has a recess 14 in which a metallization layer 15 is formed. The lithographic layer 13 limits the metallization layer 15 to the recess 14 and does not extend over the entire substrate 12. On the side of the metallization layer 15, which is the upper side of Fig. 1, a conductive surface is formed, referenced 3. On this conductive surface 3, a nanowire 2 can be grown. The lithographic layer 13 limits the growth of the nanowire 2 to the area of the recess 14.
[0057] The device 1 further comprises a foil 4 with a number of channels 5. Each channel 5 extends from a first side 6 of the foil 4 to a second side 7 of the foil 4 opposite the first side 6. The foil 4 lies on a lithographic layer 13. The foil 4 may lie on a metallization layer 15 in the recesses 14, but this is not necessary. In the example of FIG. 1, the foil 4 is shown spaced apart from the metallization layer 15. This space is shown schematic and relatively large for the purposes of illustration. In practice, it is in principle possible for the foil 4 and the metallization layer 15 to overlap one another. However, the overlap is not so tight that it may actually occur that, between the foil 4 and the metallization layer 15, local electrolytic deposition of material between the foil 4 and the conductive surface 3 during the growth of each nanowire 2.
[0058] The device 1 further comprises a first electrolyte permeable layer 8 located on the foil 4 and a second electrolyte permeable layer 9 located on the first electrolyte permeable layer 8. The first electrolyte permeable layer 8 and the second electrolyte permeable layer 9 are configured to be porous. The second electrolyte permeable layer 9 is more compressible than the first electrolyte permeable layer 8, has a larger average pore size than the first electrolyte permeable layer 8, and extends longer than the first electrolyte permeable layer 8 in a direction perpendicular to the conductive surface. The first electrolyte permeable layer 8 is formed from cellulose. The second electrolyte permeable layer 9 is a sponge.
[0059] The device 1 further comprises an electrode 10 located on the second electrolyte permeable layer 9. The device 1 further comprises a plunger as a pressing device 11 for generating a force on the second electrolyte permeable layer 9 in the direction of the conductive surface 3. In the embodiment shown in the figures, the pressing device 11 is located on the electrode 10 and can apply a force via the electrode 10 to the second electrolyte permeable layer 9 in the direction of the conductive surface 3. Due to this force, the foil 4, the first electrolyte permeable layer 8 and the second electrolyte permeable layer 9 are compressed between the lithographic layer 13 or the conductive surface 3 and the electrode 10.
[0060] The device 1 is configured such that the nanowires 2 can be grown on the conductive surface 3 by applying a voltage between the conductive surface 3 and the electrode 10, resulting in electrolytic deposition of an electrolyte in the respective channels 5 of the foil 4. This is possible in that the electrode 10 and the conductive surface 3 are in contact with the electrolyte, so that the latter are connected to one another by the electrolyte. For this purpose, in particular the respective channels 5 of the foil 4, the respective pores of the first electrolyte permeable layer 8 and the respective pores of the second electrolyte permeable layer 9 may be filled with the electrolyte. Then, in the region of the recesses 14, a material is electrolytically deposited from the electrolyte onto the conductive surface 3. As shown, insofar as there is a gap between the conductive surface 3 and the foil 4, a filling material 16 is first formed, after which the respective channels 5 of the foil 4 are filled with the deposited material, which constitutes the nanowires 2.
[0061] After the nanowires 2 have grown, the pressing device 11, the electrode 10, the second electrolyte permeable layer 9 and the first electrolyte permeable layer 8 can be removed. For example, the foil 4 can be dissolved by etching to expose the nanowires 2. Similarly, the lithography layer 13 can be chemically removed. As a result, the nanowires 2 remain on the conductive pads on the substrate 12, which are formed by the metallization layer 15 and the filling material 16.
[0062] This project has received funding from the European Union's research and innovation programme Horizon 2020 (grant agreement no. 830061). [Explanation of symbols]
[0063] 1 device 2. Nanowires 3 Conductive surface 4. Foil 5 Flow Path 6 First side of foil 7 Second side of foil 8 First electrolyte permeable layer 9 Second electrolyte permeable layer 10 electrodes 11 Pressing device 12 Substrate 13 Lithography Layer 14 Recess 15 Metallization layer 16 Filling material
Claims
1. An apparatus (1) for producing a plurality of nanowires (2), comprising: An electrically conductive surface (3); A foil (4), The foil (4) has a plurality of flow channels (5) extending from a first surface (6) of the foil (4) to a second surface (7) of the foil (4) opposite the first surface (6). Foil (4), A first electrolyte permeable layer (8); a second electrolyte permeable layer (9) which is more easily compressed than the first electrolyte permeable layer (8); Equipped with These components are arranged in the above order, The device (1) further comprises an electrode (10), the device (1) being configured such that nanowires (2) can be grown on the conductive surface (3) by electrolytic deposition from an electrolyte in each of the channels (5) of the foil (4) by applying a voltage between the conductive surface (3) and the electrode (10); Device (1).
2. 2. A device (1) according to claim 1, The first electrolyte permeable layer (8) and the second electrolyte permeable layer (9) are configured to be porous, The second electrolyte permeable layer (9) has an average pore size larger than that of the first electrolyte permeable layer (8). Device (1).
3. 3. A device (1) according to claim 1 or 2, In an uncompressed state, the second electrolyte permeable layer (9) extends longer than the first electrolyte permeable layer (8) in a direction perpendicular to the conductive surface (3). Device (1).
4. A device (1) according to any one of claims 1 to 3, The first electrolyte permeable layer (8) is formed of cellulose. Device (1).
5. A device (1) according to any one of claims 1 to 4, The second electrolyte permeable layer (9) is a sponge. Device (1).
6. A device (1) according to any one of claims 1 to 5, The device (1) further comprises a pressing device (11) for generating a force in the direction of the conductive surface (3) on the second electrolyte permeable layer (9). Device (1).
7. A device (1) according to any one of claims 1 to 6, The apparatus (1) further comprises a substrate (12) having a lithographic layer (13), The lithographic layer (13) has one or more recesses (14), the conductive surface (3) is formed in the recess (14) or recesses (14); Device (1).
8. A method for producing a plurality of nanowires (2) using the device (1) according to any one of claims 1 to 7, comprising the steps of: growing the nanowires (2) on the conductive surface (3) by electrolytic deposition from an electrolyte in each of the channels (5) of the foil (4) by applying a voltage between the conductive surface (3) and the electrode (10); method.
9. 9. The method of claim 8, the second electrolyte permeable layer (9) is at least temporarily pressed towards the conductive surface (3); method.
Citation Information
Patent Citations
Metal wire preparation method, metal wire and clamp
CN111996560A
Nanowire structure
JP2011518945A
Thermal interface materials using metal nanowire arrays and sacrificial templates
JP2018510264A
Apparatus and method for providing a multiplicity of nanowires - Patent Application 20070122999
JP2020515712A
Arrangement and method for providing a plurality of nanowires
DE102017104906A1