Semiconductor wafer thinned by horizontal stealth lasing
The horizontal stealth lasing process addresses the inefficiencies of traditional back-grinding by forming pinpoint holes in semiconductor wafers, enhancing yield and surface quality while reducing manufacturing time and debris.
Patent Information
- Application Number
- JP2024529690
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-06-15
- Filing Date
- 2023-05-06
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2043-05-06
AI Technical Summary
Traditional back-grinding processes for thinning semiconductor wafers result in non-uniform thickness, cracks, reduced yield, and debris generation, increasing manufacturing costs and time.
A horizontal stealth lasing process is employed to thin semiconductor wafers by forming localized pinpoint holes at different radii using a rotating laser, followed by a vertical stealth dicing process to separate individual semiconductor dies, eliminating the need for back-grinding.
The process significantly reduces manufacturing time, enhances wafer and die yields, prevents cracks, and eliminates debris, resulting in a smooth and uniform wafer surface.
Smart Images

Figure 2024538469000001_ABST
Abstract
Description
[Technical field]
[0001] (CROSS REFERENCE TO RELATED APPLICATIONS) This application claims the benefit of the entire contents of U.S. Non-provisional Application No. 17 / 841,357, entitled "Semiconductor Wafer Thinned by Horizontal Stealth Lasing," filed June 15, 2022, the entire contents of which are incorporated herein by reference for all purposes. [Background technology]
[0002] Strong growth in the demand for portable consumer electronics has driven the need for high-capacity storage devices. To meet the ever-increasing demand for storing and exchanging digital information, non-volatile semiconductor memory devices such as flash memory storage cards are widely used. The portability, versatility, and rugged design of such memory devices, as well as their high reliability and large capacity, make them ideal for use in a wide variety of electronic products, including digital cameras, digital music players, video game consoles, computer SSDs, PDAs, and cellular phones.
[0003] Currently, wafers are shipped from wafer fabs typically at a thickness of 760 microns to prevent damage during shipping, and are then thinned once the individual semiconductor dies are defined within the wafer. To maximize the storage capacity of a storage device of a given form factor, the semiconductor dies and the wafers from which they are manufactured are being manufactured to ever decreasing thicknesses. Wafers are now, for example, 36 microns, 25 microns, and even thinner.
[0004] A common method of thinning semiconductor wafers includes a backgrinding process in which the inactive backside of the wafer is thinned using multiple grinding wheels while the active front side of the wafer is covered with protective tape and supported on a chuck. Traditional backgrinding processes have several drawbacks including non-uniform thickness across the wafer surface. Backgrinding can also subject the wafer to forces that can cause cracks, especially considering the fragile thickness of current semiconductor wafers. Cracked dies must be scrapped, thus reducing yield. Additionally, detection of cracks also requires additional screening / inspection steps, increasing manufacturing costs and processing time. Traditional backgrinding processes also generate debris and foreign matter that can cause cracks or adversely affect the manufacturing of dies on the wafer. [Brief description of the drawings]
[0005] [Figure 1] 1 is a flow chart for forming a semiconductor wafer and a semiconductor die in accordance with an embodiment of the present technique.
[0006] [Diagram 2] 1 is a front view of a semiconductor wafer showing a first major surface of the wafer.
[0007] [Diagram 3] 2 is an enlarged cross-sectional edge view showing circuit layers formed on a substrate within a semiconductor die.
[0008] [Figure 4] FIG. 1 is a perspective view of a horizontal stealth lasing process for thinning a semiconductor wafer, in accordance with an embodiment of the present technique.
[0009] [Diagram 5] 1 is a cross-sectional top view of a wafer being thinned by a horizontal stealth lasing process in accordance with an embodiment of the present technique; FIG.
[0010] [Figure 6-7] 1A-1C are cross-sectional side views illustrating a horizontal stealth lasing process for thinning a semiconductor wafer at two different points during the process, in accordance with an embodiment of the present technique.
[0011] [Figure 8] FIG. 1 is a perspective view of a horizontal stealth lasing process for thinning a semiconductor wafer in accordance with an alternative embodiment of the present technique.
[0012] [Figure 9] FIG. 1 is a perspective view of a horizontal stealth lasing process for thinning a semiconductor wafer in accordance with a further alternative embodiment of the present technique.
[0013] [Figure 10] 1 is an edge view of a wafer after a stealth lasing process in accordance with an embodiment of the present technique.
[0014] [Figure 11] 1 is an edge view of a thinned wafer and removal of a substrate layer of the wafer in accordance with an embodiment of the present technique; FIG.
[0015] [Figure 12] FIG. 1 is a perspective view of a vertical stealth lasing process for dicing semiconductor dies from a semiconductor wafer in accordance with an embodiment of the present technique.
[0016] [Figure 13] 1 is a perspective view of a die cut from a wafer thinned by a stealth lasing process in accordance with an embodiment of the present technique; FIG.
[0017] [Figure 14] 1 is a cross-sectional side view of a semiconductor device including a semiconductor die cut from a wafer thinned by a stealth lasing process in accordance with an embodiment of the present technique. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] The present technology will now be described with reference to the drawings, which generally relate to a method of thinning a semiconductor wafer by a horizontal stealth lasing process, and the semiconductor wafers, dies, and devices formed thereby. After an integrated circuit layer is formed on a semiconductor wafer, the wafer may be thinned by supporting the active surface of the wafer on a rotating chuck and focusing a horizontally oriented laser through the outer edge of the wafer in multiple cycles at different radii within the rotating wafer. Upon completion of the multiple cycles, a portion of the wafer substrate may be removed to leave the wafer thinned to its final thickness. A vertical stealth lasing process may then be performed to dice individual semiconductor dies from the thinned wafer.
[0019] It is understood that the present invention can be embodied in many different forms and should not be construed as being limited to the embodiments set forth herein. Rather, these embodiments are provided so that this disclosure will be thorough and complete, and will fully convey the invention to those skilled in the art. Indeed, the present invention is intended to cover alternatives, modifications, and equivalents of these embodiments that are included within the scope and spirit of the invention as defined by the appended claims. Furthermore, in the following detailed description of the present invention, numerous specific details are set forth in order to provide a thorough understanding of the present invention. However, it will be apparent to one skilled in the art that the present invention can be practiced without such specific details.
[0020] The terms "top" and "bottom", "upper" and "lower", and "vertical" and "horizontal" as may be used herein are for illustration and explanation purposes only and are not meant to limit the description of the technology, as the locations and orientations of the items referred to are interchangeable. Also, as used herein, the terms "substantially", "approximately" and / or "about" mean that a specified dimension or parameter may vary within acceptable manufacturing tolerances for a given application. In one embodiment, the acceptable manufacturing tolerance is 0.15 mm, or ±2.5% of a given dimension.
[0021] For purposes of this disclosure, a connection may be a direct connection or an indirect connection (e.g., a connection through one or more other parts). In some cases, when a first element is referred to as being connected, secured, attached, or coupled to a second element, the first element and the second element may be directly connected, secured, attached, or coupled to one another, or indirectly connected, secured, attached, or coupled to one another. When a first element is referred to as being directly connected, secured, attached, or coupled to a second element, there are no intervening elements between the first element and the second element (except perhaps for things like adhesives or molten metals used to connect, secure, attach, or couple the first element and the second element).
[0022] Next, an embodiment of the present technology will be described with reference to the flowchart of FIG. 1 and the diagrams of FIG. 2 to FIG. 14. First, with reference to the flowchart of FIG. 1, a semiconductor wafer 100 may start as an ingot of wafer material that may be formed in step 200. In one example, the ingot from which the wafer 100 is formed may be single crystal silicon grown according to either the Czochralski (CZ) or floating zone (FZ) process. However, in further embodiments, the wafer 100 may be formed from other materials and by other processes.
[0023] In step 202, a semiconductor wafer 100 may be cut from an ingot and polished on both a first major surface 102 (FIG. 2) and a second major surface 104 (FIG. 3) opposite the first major surface 102 to provide a smooth surface. In step 204, the wafer may be trimmed along its periphery to ensure that the edges of the wafer 100 at the periphery are vertical (parallel to the central axis of rotation of the wafer). These vertical edges prevent refraction of the laser by the peripheral edges, as described below.
[0024] In step 206, the first major surface 102 may undergo various processing steps to separate the wafer 100 into respective semiconductor dies 106 (one of which is numbered in FIG. 1 and FIG. 2) and form integrated circuits of each semiconductor die 106 on and / or in the active areas of the die in the first major surface 102. These various processing steps may include photolithography, etching, and metallization steps to deposit metal layers, vias, and contacts for transferring signals to and from the integrated circuits. FIG. 3 is a cross-sectional side view of an exemplary semiconductor die 106 of the wafer 100 showing an integrated circuit layer 110 formed in a silicon substrate region 112. The integrated circuit layer 110 may generally include an integrated circuit 114 electrically coupled to a surface die bond pad 116 by a metallization layer 118. The integrated circuit 114 may be formed by various processes including, for example, deposition, patterning, and doping of metals, metal oxides, and silicon.
[0025] After forming the integrated circuit 114, a metallization layer 118 may be defined including metal interconnects 120 and vias 124 stacked sequentially in a dielectric film 128. As known in the art, the metal interconnects 120, vias 124, and dielectric film 128 may be formed, for example, by a damascene process using photolithography and thin film deposition, one layer at a time. The metal interconnects 120 and vias 124 may be used to form conductive nodes for transferring signals and voltages between the die bond pads 116 and the integrated circuit 114. A passivation layer 130 may be formed on top of the top dielectric film layer 128. The passivation layer 130 may be etched to expose the die bond pads 116.
[0026] In an embodiment, the semiconductor die 106 may be a flash memory die, such as, for example, a 2D NAND flash memory or a 3D BiCS (Bit Cost Scaling), V-NAND or other 3D flash memory, although other types of die 106 may be used. These other types of semiconductor die include, but are not limited to, RAM, controller, SOC (System on Chip), processor, or other types of semiconductor die. The number of die 106 shown on the wafer 100 in FIG. 2 is for illustrative purposes, and in further embodiments, the wafer 100 may include more semiconductor die 106 than shown. Similarly, the number of bond pads 116 on each semiconductor die 106 is shown for illustrative purposes, and in further embodiments, each die 106 may include more die bond pads than shown.
[0027] After forming the integrated circuit layer 110 in step 206, a tape layer may be laminated onto the active first major surface 102 in step 210. The wafer 100 may then be flipped over and thinned in step 212. In accordance with aspects of the present technique, the wafer 100 may be thinned by performing a horizontal stealth lasing step, as will now be described with reference to FIGS. 4-12. Referring to the perspective view of FIG. 4, the wafer 100 may be supported on a chuck 134 or other supporting surface such that the tape layer 136 separates the active surface 102 from the chuck 134. The second major surface 104 faces upward. In an embodiment, the chuck 134 is oriented about a central axis A. C The wafer 100 is configured to rotate about a central axis A. C Be of the same mind regarding this.
[0028] A laser assembly 140 is provided to emit a pulsed laser beam deep into the wafer 100, specifically into the silicon substrate region 112, through the outer circumferential edge 138 of the wafer. The laser assembly 140 may include a laser generator 142 for generating a laser beam 144 and optics 146 for focusing the laser beam 144 to a point within the wafer 100, as described below. The laser generator may generate an infrared or near infrared laser, for example at a wavelength of 1342 nm. Other wavelength lasers are contemplated. The peak power and beam area of the laser generator 142 together define the peak power density of the laser beam 144, as follows: Peak power density W / m 2 = peak power (W) / beam area (m 2 ). In one example, the peak power of the laser generator 142 may be 2 W and the beam diameter may be approximately 2-4 μm. These values are for illustrative purposes only and may vary in further embodiments. In one example, the laser generator may pulse the laser beam 144 at 90 KHz.
[0029] The optics 146 may include, for example, a collimating lens that can focus the parallel wavelengths of light from the laser generator 142 to a focal point of maximum energy. The laser assembly 140 is shown diagrammatically and may include additional components for laser generation and focusing, including a controller for controlling the intensity and pulse frequency of the laser.
[0030] The laser assembly 140 is aligned in the xy plane (center axis A C In a further embodiment, the laser beam 144 is configured to emit a horizontal beam along the central axis A CLaser beam 144 can be non-horizontal, provided that it is emitted in a plane perpendicular to the z-axis. In accordance with the present technique, laser assembly 140 is positioned along a vertical z-axis and emits beam 144 onto silicon substrate region 112 in a plane that corresponds to the final thickness of wafer 100. In embodiments, this final thickness can be between 20 μm and 100 μm, including 25 μm and 36 μm, although it is understood that laser assembly 140 can be positioned to achieve other final thicknesses for wafer 100 within or outside this range.
[0031] Once the vertical height of the laser assembly 140 is set, the optical system 146 is aligned with, for example, the central axis A of rotation of the wafer 100. C The laser beam 144 is focused at a predetermined first radius (as described below) adjacent the outer edge 138 of the wafer 100. The wafer 100 is then rotated a full cycle (360°) on the chuck 134 while the laser emits pulses of light at the predetermined frequency. After the first cycle is completed, the radius at which the laser is focused is then adjusted to a new radius and the wafer is again rotated a full cycle while the laser emits pulses of light at the predetermined frequency. This process may continue for multiple cycles at increasing radii until the laser is focused at or near the outer edge 138 of the wafer 100.
[0032] Referring to FIG. 5, a cross-sectional top view of the wafer 100 is shown. In the illustrated example, the laser assembly 140 was focused at three different radii, namely r1, r2, and r3. The laser assembly emitted a pulse at each radius at a predetermined frequency as the wafer 100 rotated on the chuck 134. When the laser beam hits the peak power density during the pulse at the focal point, the wafer absorbs the energy and localized pinpoint holes 150 are made at radii r1, r2, and r3 in the horizontal plane of the laser beam and below the surface of the wafer. Multiple pinpoint holes 150 are made at each radius. In one example, the pinpoint holes 150 may be made once every 5 μm to 10 μm around a given radius, although in further embodiments the pinpoint holes 150 may be placed closer to each other than that range or farther away from each other. FIG. 5 shows a simplified example for illustrative purposes and there may be more radii at which the laser cycle is performed. For example, for a 300 mm wafer, there may be 250 different cycles, each performed at equally spaced radii.
[0033] In one embodiment, the pulse rate of the laser generator 140 is constant. Given that circumferential arc lengths at radii near the center of the wafer have shorter lengths and fewer pinpoint holes than circumferential arc lengths at outer radii, the angular velocity of the chuck 134 can be varied to keep the number of pinpoint holes per unit length at a given radius constant. In one example, the rotating chuck maintains a constant linear velocity of about 700 mm per second. Thus, the angular velocity of the chuck varies as follows: ω=v / r ω=700mm / r where ω is the angular velocity, v is the linear velocity, and r is the radius. It is understood that in further embodiments, the linear velocity may be higher or lower. In further embodiments, the speed of the rotating chuck may be kept constant, and the predetermined pulse frequency of the laser generator 142 may vary with the radial distance from the central axis of rotation.
[0034] 6 and 7 are side views illustrating how the optics 146 can control the focus of the laser assembly 140 at different radii of a given plane within the wafer 100. The optics 146 can be mounted for translational movement on the fixture 152. As an example, the optics 146 can be mounted on a pinion gear that is driven to rotate by a motor along a stationary rack within the fixture. In further embodiments, other drive systems are contemplated for translating the optics within the fixture 152.
[0035] The optics 146 may focus the laser to a point some predetermined distance forward from the optics 146. If the optics are positioned near the laser generator (FIG. 6), the laser beam 144 will be focused to a radius close to the outer periphery of the wafer 100. Once a cycle at a given radius is completed, the optics may translate along the fixture 152 in the direction of arrow 154 to a new radius where the laser beam 144 is focused, and a new cycle begins. The laser generator 142 is configured such that the optics 146 focuses the laser beam 144 on the central axis A of the wafer 100. C In a further embodiment, the laser continues to generate pinpoint holes 150 at different radii until it is focused at or near the central axis A. C It may start at or near the fixture 152 and move outward such that the optics translates on the fixture 152 in the direction opposite to arrow 154. The laser assembly 140 and fixture 152 are shown generally in Figures 6 and 7, and in further embodiments, both may vary in composition.
[0036] Thinning the wafer 100 according to aspects of the present technique provides several advantages, including reduced wafer production time. For example, the time it takes to thin a single wafer can be calculated by dividing the sum of the circumferential arc lengths spanned by the laser over the various radii by the linear velocity of the rotating chuck. The sum of the circumferential lengths spanned by the laser over all radii is given by the following formula: CL tot =CL1+CL2+CL3+…+CL n where CL1 is the arc length of the circumference at the first radius, CL2 is the arc length of the circumference at the second radius, ..., n is the total number of cycles (e.g., 250). Since the arc length of the circumference is equal to 2πr, CL tot =2π(r1+r2+r3+…+r n ) If the radii are equally spaced, the total radial distance can be summed as the total number of cycles multiplied by the sum of the first radius and the last radius divided by 2. (r1+r2+r3+…+r n )=250(r1+r n ) / 2 The first radius is the central radius A C Taking an example where the starting radius is 0.6 mm from the center radius and the final radius is 150 mm from the center radius, the total circumferential arc length distance traveled by the laser is: CL tot =2π*250(0.6mm+150mm) / 2 CL tot =118,221mm If the linear rotational speed of the chuck 134 is 700 mm / sec, the total time to thin the wafer according to the present technique is: T tot =CL tot / V チャック T tot =118,221mm / 700mm / s=169 seconds In comparison, wafer thinning by conventional backgrinding takes 500-600 seconds per wafer. Therefore, this technique improves wafer thinning time by approximately 300%-360%.
[0037] The speed of the wafer thinning operation according to the present technique can be further reduced by adding additional laser assemblies. FIG. 8 is a perspective view of a wafer being thinned by a pair of laser assemblies 140. Each laser assembly 140 is structurally and operationally identical to one another and may be as described above. The two laser assemblies 140 direct their respective beams 144 in the same horizontal plane (central axis A C100) into the wafer 100. The laser assemblies may be spaced 180° apart from each other, although in further embodiments this need not be the case.
[0038] In one embodiment, the optics 146 of both laser assemblies 140 direct their laser beams 144 along a central axis A C The lasers may be controlled to focus at radii at the same distance from the laser assemblies 140. Thus, upon rotation of 180°, a complete cycle of pinpoint holes 150 may be made around the circumference at a given radius. As a result, the time to thin the wafer may be further cut in half. In a further embodiment, each laser may be focused at a different radius, so that a full cycle still requires 360°, but the number of cycles is cut in half, again cutting the overall time to thin the wafer in half. To further reduce the wafer thinning process time, the wafer thinning setup can include three, four, or more laser assemblies 140.
[0039] In the embodiment described herein, the horizontal stealth lasing process is performed by forming localized pinpoint holes 150 at different radii as the wafer 100 rotates. However, in a further embodiment shown in FIG. 9, the localized pinpoint holes 150 may be formed in rows along a straight line through the wafer while the wafer is stationary (not rotating). In this embodiment, the laser is mounted on a fixture configured to move the laser generator along the y-axis (into and out of the page of FIG. 9) and to move the optics 146 along the x-axis to form multiple rows of pinpoint holes 150. In this embodiment, the optics 146 are configured to move across the entire diameter of the wafer 100 (whereas the optics 146 in the embodiment of FIG. 4 only needs to move across the radial distance of the wafer 100). In a further example, in the embodiment of FIG. 9, a second laser assembly 140 may be provided (as in FIG. 8). In such an embodiment, each laser may form pinpoint holes 150 along a straight line across half of the wafer. Thus, the laser assembly 140 on the left side of the wafer 100 creates a pinpoint hole 150 on the left side of the wafer, and the laser assembly 140 on the right side of the wafer 100 creates a pinpoint hole 150 on the right side of the wafer.
[0040] FIG. 10 is a side view of the wafer 100 after all cycles of the stealth horizontal lasing process of step 212 are completed. As the cycles of the pinpoint holes 150 are completed at each radius, a crack naturally propagates between the holes in the [1,1,0] crystal plane (in the x,y plane of FIG. 4), thereby effectively decoupling the first portion 100a from the second portion 100b in the xy plane 156. This first portion 100a is the portion of the wafer that includes the active surface with the integrated circuits, and is the wafer 100 at its final thickness. The second portion is a portion of the silicon substrate area 112 that may be discarded. In one example, the wafer may have a total thickness of 760 μm before the horizontal lasing portion of the technique. In one example, the final thickness of the first portion 100a of the wafer 100 may be 32 μm. Thus, the thickness of the silicon substrate area to be removed may be about 728 μm. These values are for illustrative purposes only and may vary in further embodiments. For example, the thickness of the finished wafer 100 may be 25 μm or less. If the finished wafer 100 is 25 μm, then the thickness of the removed wafer portion 100b may be approximately 735 μm.
[0041] 11 is an edge view showing the removal of portion 110b of wafer 100 by vacuum chuck 158 after the stealth horizontal lasing process of step 212. A portion of silicon substrate area 112 remains as part of first portion 100a, hereinafter again referred to simply as wafer 100. Severed portion 100b may be discarded. A new second major (back) surface 104 is the surface of substrate wafer 100 defined by the removal of portion 100b.
[0042] In an embodiment, after the stealth lasing step 212, the second major surface 104 may undergo a polishing step, for example using a Z3 polishing wheel rotated against the back surface. In a further embodiment, the horizontal stealth lasing step 212 may leave the back surface 104 without requiring further polishing.
[0043] The wafer 100 may then be diced at step 214. The dicing of the wafer may be performed by a vertical stealth dicing process, as shown in FIG. 12. The vertical stealth dicing process may use a laser assembly 160 including a laser generator 162 that generates a laser beam 164 and an optical system 166 for focusing the laser beam 164 to a point below the surface of the wafer 100. The vertical laser assembly 160 may form a layer of voids in a vertical plane (orthogonal to the faces 102, 104) around the contour of each semiconductor die 106 in the wafer 100. The vertical laser assembly 160 may be structurally and operationally identical to the horizontal laser assembly 140, and may actually be the same laser assembly rotated from a horizontal orientation to a vertical orientation above the wafer 100. In further embodiments, the vertical laser assembly 160 may be structurally and / or operationally different from the horizontal laser assembly 140.
[0044] At least a portion of the vertical laser assembly 160 is mounted for translational movement over the wafer 100 in the xy plane. With the wafer 100 still supported on the chuck 134 or other support surface such that the taped first major surface 102 rests against the chuck, the laser assembly 160 can emit a pulsed laser beam 164 that is focused to a point below the plane 104 of the wafer using optics 166. When the laser beam strikes the peak power density at the focus, the wafer absorbs the energy and a pinpoint hole 170 is created below the surface of the wafer.
[0045] The vertical laser assembly can be moved in rows (along the x-axis) and columns (along the y-axis) in the xy plane and activated at multiple points such that multiple closely spaced pinpoint holes 170 are formed at the mid-depth of the wafer (between the first major surface 102 and the second major surface 104). The rows and columns of pinpoint holes 170 define the final shape and contour of each semiconductor die 106 diced from the wafer 100, as shown in FIG. 12. The laser assembly 160 can form a single layer of pinpoint holes 170, or multiple layers of vertically aligned pinpoint holes 170 at multiple depths, by adjusting the vertical position of the optics 166. Once one or more layers of pinpoint holes 170 are created, cracks naturally propagate from holes 170 to first major surface 102 and second major surface 104 in the [1,0,1] and [0,1,1] crystallographic planes, thereby effectively dicing each semiconductor die 106 from wafer 100. Although a vertical stealth dicing process has been described for dicing wafer 100, it will be appreciated that in further embodiments, wafer 100 may be diced by other techniques, including by a dicing blade.
[0046] After the horizontal stealth lasing step 212 and the vertical stealth lasing step 214 are completed, in step 218, a layer of die attach film (DAF) adhered to a flexible dicing tape may be applied to the second major surface 104 of the wafer 100. In further embodiments, the DAF tape and dicing tape may be applied to the surface 104 before the horizontal stealth lasing step 212 and / or the vertical stealth lasing step 214. In step 220, the wafer is flipped over on the support chuck so that the DAF and dicing tape face the chuck, and the tape layer 136 laminated on the first major surface 102 may be removed. The flexible dicing tape may be stretched along orthogonal axes in step 224 to separate the individual semiconductor dies 106. Then, in step 226, the individual semiconductor dies 106 may be removed by a pick-and-place robot.
[0047] 13 shows a perspective view of a sample semiconductor die 106 thinned by the horizontal stealth lasing process of the present technique. Although die bond pads 116 are shown, as mentioned above, the number and location of die bond pads 116 are shown by way of example, and in further embodiments, die 106 may include more die bond pads at other locations. Surface 104 (covered by DAF tape 176) is smooth and uniform.
[0048] 14 is a side view of a completed semiconductor device 180 including semiconductor dies 106 thinned by a horizontal stealth lasing process in accordance with an embodiment of the present technique. In the embodiment shown, the semiconductor device 180 includes four semiconductor dies 106 picked up from the wafer 100 and dumped into a die stack 182 built on top of a substrate 184. However, in further embodiments, the die stack 182 may include other numbers of semiconductor dies 106 including, for example, 2, 8, 16, 32, 64. The dies are secured within the die stack 182 and on the substrate 184 using a DAF layer 176 at the bottom of each die 106. A controller die 186 may be attached to the substrate 184, which may be an ASIC in an embodiment, to control the transfer of data to and from the dies 106 in the stack 182.
[0049] The dies 106 may be electrically connected to each other and to the substrate 184 using bond wires 188, although in further embodiments, the dies 106 may be electrically connected to each other and to the substrate 184 by other schemes including, for example, via silicon vias (TSVs). To leave space for the connection of the bond wires 188 to the bond pads 116 on each semiconductor die 106 in the stack 182, the dies 106 are stacked in a stepped offset fashion relative to each other. In the embodiment of FIG. 14, all of the dies in the stack 182 may be stepped offset in the same direction. In further embodiments, they may be stacked in groups in a stepped fashion in opposite directions.
[0050] The die 106, 186 and bond wires 188 may be encapsulated in a molding compound 190, which may be, for example, an epoxy resin, a phenolic resin, a fused silica, a crystalline silica, carbon black, and / or a metal hydroxide. Other molding compounds are contemplated. In an embodiment, the semiconductor device 180 may be used as a BGA (ball grid array) package soldered to a host device, such as a printed circuit board. In such an embodiment, the semiconductor device 180 may further include solder balls 192 on a bottom surface of the substrate 184 to physically and electrically couple the semiconductor device 180 to the host device. In a further embodiment, the semiconductor device 180 may be used as a LGA (land grid array) package configured for insertion into and removal from a slot of a host device. In such an embodiment, the solder balls 192 may be replaced with contact fingers (not shown) on the bottom surface of the substrate 184 for mating with pins in a host device slot. It is understood that in further embodiments, the semiconductor device 180 may have other configurations.
[0051] Horizontal stealth dicing for thinning the wafer 100 as described above offers several advantages. As described above, horizontal stealth dicing can significantly reduce the production time in thinning the wafer, thereby improving wafer and die yields. It is noted that, as described in the Background, a conventional backgrinding process can result in cracks in semiconductor wafers, especially those semiconductor wafers that are currently made at thin and fragile thicknesses. Horizontal stealth dicing according to the present technique eliminates wafer cracking due to the backgrinding process. The elimination of such cracks improves wafer and die yields and eliminates the need for additional screening / inspection steps. It is also known to thin wafers by a vertical stealth dicing process. However, such a process can result in a rough or uneven second major surface, which can result in weakness or cracks in the completed semiconductor die. The horizontal stealth dicing process results in a smooth, uniform, and strong second major surface 104.
[0052] Additionally, conventional backgrinding processes generate debris and contaminants that can cause cracks or adversely affect the assembly process. Elimination of the backgrinding process prevents this debris and contaminant generation, thereby further improving yield and die quality. Furthermore, the multiple backgrinding wheels required for conventional wafer thinning add significant time, expense, and complexity to the packaging process. The elimination of the backgrinding wheels by the present technology improves each of these packaging parameters.
[0053] In summary, an example of the present technology relates to a semiconductor die including a first major surface, a plurality of integrated circuits formed on the first major surface of the wafer, a second major surface opposite the first major surface, the second major surface being defined by a plurality of localized pinpoint holes generated by a laser, and a die attach film (DAF) layer covering the second major surface.
[0054] In another example, the present technology relates to a semiconductor wafer including a first major surface, a plurality of semiconductor dies including integrated circuits formed on the first major surface of the wafer, and a second major surface opposite the first major surface, the second major surface being defined by a plurality of localized pinpoint holes generated by a laser.
[0055] In a further example, the present technology relates to a method of separating semiconductor dies from a wafer including a plurality of semiconductor dies, the wafer including a first major planar surface, a second major planar surface, and an outer edge extending between the first major planar surface and the second major planar surface, the method including forming integrated circuits in the first major planar surface; thinning the wafer by applying one or more laser beams through the outer edge of the wafer; and dicing the semiconductor dies from the thinned wafer.
[0056] The foregoing detailed description of the invention has been presented for purposes of illustration and description. It is not intended to be exhaustive or to limit the invention to the precise form disclosed. Many modifications and variations are possible in light of the above teachings. The described embodiments are selected to best explain the principles of the invention and its practical application and to enable others skilled in the art to best utilize the invention in various embodiments and with various modifications suited to the particular uses contemplated. It is intended that the scope of the invention be defined by the claims appended hereto.
Claims
1. 1. A semiconductor die comprising: A first major surface; a plurality of integrated circuits formed on the first major surface of the die; a second major surface opposite the first major surface, the second major surface being defined by a plurality of localized pinpoint holes generated by a laser; a die attach film (DAF) layer covering the second major surface.
2. The semiconductor die of claim 1 , wherein the plurality of laser-generated localized pinpoint holes are applied by a laser assembly emitting a beam parallel to the second major surface.
3. The semiconductor die of claim 1 , wherein the plurality of laser-generated localized pinpoint holes are formed in a radial pattern on the second major surface.
4. The semiconductor die of claim 1 , wherein the plurality of laser-generated localized pinpoint holes are formed in a linear pattern on the second major surface.
5. The semiconductor die of claim 1 , wherein the second major surface is also polished.
6. 10. The semiconductor die of claim 1, wherein the semiconductor die has an edge between the first major surface and the second major surface, the edge being defined by a laser applied perpendicular to the second major surface.
7. 10. The semiconductor die of claim 1, wherein the semiconductor die has a thickness between the first major surface and the second major surface of between 25 microns and 36 microns.
8. The semiconductor die of claim 1 , wherein the semiconductor die is a flash memory semiconductor die.
9. A semiconductor wafer, A first major surface; a plurality of semiconductor dies including integrated circuits formed on the first major surface of the wafer; a second major surface opposite the first major surface, the second major surface being defined by a plurality of localized pinpoint holes generated by a laser.
10. 10. The semiconductor wafer of claim 9, wherein the second major surface comprises a first portion of the semiconductor wafer substrate that is severed from a second portion of the semiconductor wafer substrate by a horizontal stealth lasing process.
11. 10. The semiconductor wafer of claim 9, wherein the plurality of laser-created localized pinpoint holes are applied by a laser assembly emitting a laser beam parallel to the second major surface.
12. 12. The semiconductor wafer of claim 11, wherein the laser assembly cycles off and on as the laser beam is moved relative to the semiconductor wafer until a peak power density is reached at a predetermined frequency.
13. 1. A method of separating semiconductor dies from a wafer including a plurality of semiconductor dies, the wafer including a first major planar surface, a second major planar surface, and an outer edge extending between the first major planar surface and the second major planar surface, each die including a plurality of integrated circuits formed in the first major planar surface of the wafer, the method comprising: thinning the wafer by applying one or more laser beams through the outer edge of the wafer; and dicing the semiconductor die from the thinned wafer.
14. 14. The method of claim 13, wherein the step of thinning the wafer by directing one or more laser beams through the outer edge of the wafer comprises creating a pinpoint hole in a plane parallel to the first major plane of the wafer and a crack propagating between the pinpoint hole to separate a portion of the wafer at the plane.
15. 14. The method of claim 13, wherein for the step of thinning the wafer, the wafer is supported on the chuck such that the first major plane faces the chuck.
16. The method of claim 14 , wherein the chuck rotates during the step of thinning the wafer.
17. 16. The method of claim 15, wherein the focus of the laser is adjusted to different radial positions of the wafer as the wafer rotates on the chuck to generate pinpoint holes at the different radial positions in a plane parallel to the first major surface.
18. 15. The method of claim 14, wherein during the step of thinning the wafer, the focus of the laser is linearly adjusted to produce a plurality of rows of pinpoint holes in a plane parallel to the first major surface.
19. 14. The method of claim 13, wherein the step of thinning the wafer by directing one or more laser beams through the outer edge of the wafer comprises creating a pinpoint hole in a plane parallel to the first major surface of the wafer from a pair of laser assemblies.
20. 14. The method of claim 13, wherein the step of dicing the semiconductor die from the thinned wafer comprises creating pinpoint holes in a plane orthogonal to the first major plane of the wafer and a crack propagating between the pinpoint holes to dice the die from the wafer.
Citation Information
Patent Citations
Process and apparatus for producing substrate
JP2006245498A
Method for processing semiconductor wafer
JP2010267639A
Laser processing device and laser processing method
JP2020069532A
Semiconductor device including vertical bond pads
JP2021180301A
Semiconductor device including dual pad wire bond interconnection
US20180190621A1