Bevel cleaning strip

The vacuum transfer and hydrogen-containing gas mixture method addresses fluoropolymer deposition issues by efficiently removing polymer films and layers on semiconductor wafers, reducing defects and oxidation, and maintaining silicon nitride integrity.

JP2024538796APending Publication Date: 2024-10-23LAM RES CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2024522469
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-22
Filing Date
2022-10-17
Publication Date
2024-10-23

AI Technical Summary

Technical Problem

Existing semiconductor wafer etching processes result in fluoropolymer deposition on sidewalls and the backside of the bevel, leading to corrosion and defect formation due to exposure to moisture and reactive species, and current stripping methods damage silicon nitride layers or fail to remove backside polymer effectively.

Method used

A method involving a vacuum transfer from an etching chamber to a stripping chamber using a hydrogen-containing gas mixture (CO2, CO, N2O, NO, NO2) to generate radicals that remove polymer-containing films and layers without breaking vacuum, minimizing oxidation and corrosion.

Benefits of technology

Effectively strips polymer from sidewalls and the backside of the wafer while reducing damage to silicon nitride layers, thereby minimizing defects and contamination in subsequent processing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024538796000001_ABST
    Figure 2024538796000001_ABST
Patent Text Reader

Abstract

A method is provided for stripping a polymer-containing sidewall film from an etch feature and a polymer-containing deposition layer from a backside of a bevel portion of a wafer having a stack including at least one silicon nitride-containing layer. A plasma is generated from a strip gas, the strip gas including a hydrogen (H2)-containing gas and at least one of CO2, CO, N2O, NO, and NO2, and the plasma generates radicals from the strip gas. The wafer is exposed to the radicals, and the radicals remove the polymer-containing sidewall film and the polymer-containing deposition layer.
Need to check novelty before this filing date? Find Prior Art

Description

[Background technology]

[0001] [CROSS REFERENCE TO RELATED APPLICATIONS] This application claims the benefit of priority to U.S. Application No. 63 / 270,764, filed October 22, 2021, which is incorporated by reference herein for all purposes.

[0002] The Background Art provided herein is intended to present the contents of the present disclosure generally, and the inventions of the presently named inventors are not admitted expressly or impliedly as prior art to the present disclosure to the extent that they are described in this Background Art section and in a manner that is not prior art at the time of filing.

[0003] The present disclosure relates to methods for forming semiconductor devices on semiconductor wafers. In particular, the present disclosure relates to etching features in a stack that includes at least one silicon nitride-containing layer. In such processes, fluoropolymers can deposit on the sidewalls of the etched features. Fluoropolymers can also deposit on the backside of the beveled portion of the wafer. Summary of the Invention

[0004] To achieve the foregoing in accordance with the objectives of the present disclosure, a method is provided for stripping a polymer-containing sidewall film from an etch feature and a polymer-containing deposition layer from a backside of a bevel portion of a wafer having a stack including at least one silicon nitride-containing layer. A plasma is generated from a strip gas, the strip gas including a hydrogen (H2)-containing gas and at least one of CO2, CO, N2O, NO, and NO2, and the plasma generates radicals from the strip gas. The wafer is exposed to the radicals, and the radicals remove the polymer-containing sidewall film and the polymer-containing deposition layer.

[0005] In another embodiment, a method is provided for processing a stack including at least one silicon nitride-containing layer on a wafer having a bevel. At least one feature is etched in the at least one silicon nitride-containing layer, the etching of the at least one feature forms a polymer-containing sidewall film on the at least one feature and forms a polymer-containing deposition layer on a backside of the bevel of the wafer, and the etching is provided in an etch chamber under vacuum. The wafer is transferred from the etch chamber to a strip chamber without breaking vacuum. The polymer-containing sidewall film and the polymer-containing deposition layer are stripped, including generating a plasma from a strip gas, the strip gas including a hydrogen (H2)-containing gas and at least one of CO2, CO, N2O, NO, and NO2, and the plasma generates radicals from the strip gas. The wafer is exposed to the radicals, and the radicals remove the polymer-containing sidewall film and the polymer-containing deposition layer.

[0006] In another embodiment, a method is provided for stripping a polymer-containing sidewall film from an etch feature and a polymer-containing deposition layer from a backside of a bevel of a wafer having a stack including at least one silicon nitride-containing layer. A plasma is generated from a strip gas, the strip gas including at least one of CO2, CO, N2O, NO, and NO2, and the plasma generates radicals from the strip gas. The wafer is exposed to the radicals, and the radicals remove the polymer-containing sidewall film and the polymer-containing deposition layer.

[0007] These and other features of the present disclosure are described in more detail below in the detailed description taken in conjunction with the following figures. [Brief description of the drawings]

[0008] The present disclosure is illustrated by way of example, and not by way of limitation, in the figures of the accompanying drawings, in which like numerals refer to like elements and in which:

[0009] [Figure 1] 1 is a high level flow chart of one embodiment.

[0010] [Diagram 2] 1 is a schematic diagram of a platform used in one embodiment.

[0011] [Diagram 3] 1 is a schematic diagram of a strip tool used in one embodiment.

[0012] [Figure 4] 2 is an enlarged cross-sectional view of a stack that is processed in one embodiment.

[0013] [Diagram 5] FIG. 2 is an enlarged cross-sectional view of a bevel portion of a wafer used in one embodiment.

[0014] [Figure 6] FIG. 1 is a schematic diagram of a computer system that can be used to implement one embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] The present disclosure will now be described in detail with reference to several preferred embodiments thereof as illustrated in the accompanying drawings. In the following description, several specific details are set forth in order to provide a thorough understanding of the present disclosure. However, it will be apparent to one skilled in the art that the present disclosure may be practiced without some or all of these specific details. In other instances, well-known process steps and / or structures have not been described in detail in order not to unnecessarily obscure the present disclosure.

[0016] Dry etching of memory holes using etching techniques is typically associated with the deposition of polymers on the wafer surface and on the backside of the wafer (bevel). Once etched, the wafer is typically transferred from the vacuum environment to a containment (e.g., atmospheric air-sealed container (FOUP)) for further processing. Reactive species remaining on the sidewalls of the memory hole structures are exposed to the atmosphere, resulting in high levels of sidewall damage that cause corrosion and defect formation of contact features. Such corrosion and defect formation are time and moisture dependent.

[0017] Therefore, post-etch strip of polymer is a common process used in three-dimensional NAND (3D NAND) manufacturing with silicon nitride (SiN, also known as nitride) layers. A typical polymer removal gas is oxygen (O2) with forming gas (FG). Forming gas is a dilute hydrogen (H2) gas. A typical forming gas consists of about 4% H2 and about 96% nitrogen (N2). Another polymer removal gas is O2, N2, and FG. Such strip chemistries can strip polymer from the front side of the wafer and the back side of the wafer. Such strip chemistries can damage silicon nitride-containing layers in silicon oxide / silicon nitride / silicon oxide / silicon nitride (ONON) stacks, resulting in high oxidation levels and / or strong corrosion of the silicon nitride layer. This leads to a significant increase in contact sidewall roughness and a significant increase in contact critical dimension. Limiting the O2 exposure by time or flow rate cannot solve this fundamental limitation. On the other hand, O2-free strip cannot strip the polymer from the backside of the wafer. When the polymer is not stripped from the backside of the wafer, particle defects will be caused by polymer delamination and chamber contamination in subsequent processing.

[0018] FIG. 1 is a high level flow chart of one embodiment. In this embodiment, a wafer is placed in an etch chamber (step 104). In this embodiment, a stack including a silicon nitride layer is on the wafer. In this embodiment, the stack includes an ONON stack under a carbon-containing mask. A more detailed description of the etch chamber and associated platform used in one embodiment is provided below. Features are etched in the stack on the wafer (step 108). Etching the features deposits a polymer-containing sidewall film on the sidewalls of the etched features and a polymer-containing deposition layer on the bevel of the backside of the wafer. In this embodiment, the polymer-containing deposition layer and the polymer-containing sidewall film are fluoropolymer deposits that include carbon and fluorine.

[0019] The wafer is transferred from the etch chamber to the strip chamber (step 112). In this embodiment, the platform includes both the etch chamber and the strip chamber. The platform can transfer the wafer from the etch chamber to the strip chamber without breaking vacuum. Keeping the wafer under vacuum during transfer from the etch chamber to the strip chamber prevents the fluoropolymer sidewall film from being exposed to moisture, which can cause corrosion of the stack in the fluoropolymer sidewall film. The platform reduces damage to the stack by not breaking vacuum during transfer of the wafer from the etch chamber to the strip chamber.

[0020] The polymer-containing sidewall film and the polymer-containing deposition layer are stripped in a strip chamber (step 116). A plasma is generated from a strip gas, the strip gas including a hydrogen (H2)-containing gas and at least one of carbon dioxide (CO2), carbon monoxide (CO), nitrous oxide (N2O), nitric oxide (NO), and nitrogen dioxide (NO2). In this embodiment, the H2-containing gas is a forming gas. In this embodiment, the forming gas is H2 diluted with nitrogen (N2). In this embodiment, the forming gas has about 4% H2. In this embodiment, the strip gas is primarily composed of CO2 and a forming gas of about 4% H2 and about 96% N2. Thus, the strip gas in such an embodiment is fluorine and halogen free. In various embodiments, the forming gas may be primarily composed of 0.1%-4% H2 and 96%-99.9% N2. In other embodiments, an inert gas may be added to the strip gas. Examples of inert gases may be helium (He), argon (Ar), and neon (Ne). The plasma generates radicals from the strip gas. Such radicals may include H, O, C, NO, and N radicals. The radicals strip the polymer-containing sidewall film and the polymer-containing backside deposition layer, with little damage or oxidation of the silicon nitride layer. The wafer and stack may be subjected to further processing. The wafer and stack are removed from the platform and exposed to the atmosphere.

[0021] The use of a forming gas stripping gas containing at least one of CO, CO2, N2O, NO, and NO2 provides a unique ability to strip polymer from the wafer surface, sidewalls of patterned structures, and the backside of the wafer (bevel). This combination allows for high polymer stripping rates while providing significantly less surface oxidation compared to stripping gases of O2 and forming gas. Oxidation and / or corrosion of the SiN layer using a stripping gas containing O2 is undesirable in some applications. If the stripping gas is only forming gas, the fluorocarbon deposition layer on the backside of the wafer is not adequately removed. As a result, the remaining fluorocarbon deposition layer will become a contaminant in subsequent processing and increase the number of defective devices.

[0022] In some embodiments, the strip gas provides a CO2 flow in the range of 30 sccm to 3 L / min. In other embodiments, the strip gas provides a CO2 flow rate in the range of 150 to 1000 sccm. In some embodiments, the ratio of the CO2 flow rate to the forming gas flow rate is in the range of 1:100 to 5:1.

[0023] In embodiments where the SiN-containing layer is etched at a wafer support cryogenic temperature below -10°C, ammonium salts (NH4X) can be deposited along with the polymer-containing deposits on the backside of the wafer bevel. It has been found that the use of a strip gas including CO2 and forming gas increases the removal rate of the ammonia salts associated with the polymer-containing deposits. Removal of the ammonia salts reduces contaminants in subsequent processes. As a result, the strip gas provides improved strip after the cryogenic etching process. In other embodiments, the cryogenic etching process is performed at a temperature below -10°C.

[0024] Other embodiments may use a strip gas consisting primarily of CO2 and H2. For example, the strip gas may be 90%-99.9% CO2 and 0.1%-10% H2. Thus, the strip gas may consist primarily of an H2-containing gas and at least one of CO2, CO, N2O, NO, and NO2. The H2-containing gas may consist primarily of a forming gas consisting of N2 and H2, or H2 only. During strip, the wafer temperature is maintained at a temperature in the range of 20°C-500°C. A pressure of approximately 750 mT (milliTorr) is provided. Typically, the pressure is in the range of 100-2000 mT.

[0025] In other embodiments, the strip gas is H2 free or has less than 0.1% H2. In such embodiments, the strip gas consists essentially of at least one of CO2, CO, N2O, NO, and NO2. In other such embodiments, the strip gas consists essentially of an inert gas and at least one of CO2, CO, N2O, NO, and NO2, and the inert gas is at least one of He, Ne, Ar, and N2.

[0026] FIG. 2 is a top schematic view of a platform 200 using one embodiment. The FOUP 202 stores unprocessed wafers before they are processed and then stores processed wafers once all processing is completed on the platform 200. The FOUP 202 can store a large number of wafers, usually as many as 25. An atmospheric transfer module (ATM) 214 is used to transfer wafers to and from the FOUP 202. The load lock station 205 represents at least one device that operates to transfer wafers between the atmosphere of the ATM 214 and the vacuum of the vacuum transfer module (VTM) 212. The VTM 212 is a part of the platform 200 that connects multiple processing chambers. There may be different types of processing chambers. In this embodiment, the multiple processing chambers include an etching chamber 208, a strip chamber 220, and an additional processing chamber 228. In this embodiment, the etching chamber 208 is a capacitively coupled dielectric etching chamber. In other embodiments, the etching chamber 208 may be inductively coupled. A robotic system in the vacuum transfer module 212 uses an end effector to move wafers between the load lock station 205 and the processing chambers. The ATM 214 uses a robotic system to transfer wafers between the FOUP 202 and the load lock station 205. A controller 235 may be used to control the entire platform 200, or multiple controllers 235 may be used to control different portions of the platform 200 or different processing chambers.

[0027] 3 is a schematic diagram of a strip chamber 220 that may be used in one embodiment. In one or more embodiments, the strip chamber 220 includes a reactor chamber 310 surrounded by chamber walls 312, a showerhead 306 with gas inlets, and a wafer support 308. In the reactor chamber 310, a wafer 314 is placed on the wafer support 308. A gas source 316 is connected to a remote plasma generator 320. The remote plasma generator 320 is connected to the reactor chamber 310 through the showerhead 306. A radio frequency (RF) source 330 provides RF power to the remote plasma generator 320 at one or more of the following frequencies: 27 megahertz (MHz), 13.56 MHz, 60 MHz, 2 MHz, and 400 kHz. A support temperature controller 340 is used to control the temperature of the wafer support 308. A controller 335 is controllably connected to an exhaust pump 352, the support temperature controller 340, and the gas source 316. In some embodiments, capacitively or inductively coupled energy may be provided to the strip chamber 220 using electrodes or a helical coil. In one embodiment, inductively coupled RF power is used to provide 200 W to 5000 W of RF energy to the strip chamber 220 to generate radicals in the strip chamber 220. In other embodiments, the strip chamber 220 does not use a remote plasma, but instead generates a plasma within the strip chamber.

[0028] FIG. 4 is an enlarged schematic cross-sectional view of a portion of stack 404 over a portion of wafer 314 after etching etch features 440 into the stack. In this embodiment, stack 404 includes multiple bilayers 412. In this example, one or more layers may be disposed between wafer 408 and multiple bilayers. In this embodiment, each bilayer 412 includes a silicon oxide layer 424 and a silicon nitride layer 428. A fluoropolymer sidewall film 445 is deposited on the sidewalls of etch features 440. FIG. 5 is an enlarged cross-sectional view of a bevel portion of wafer 314 with fluoropolymer deposition layer 504. Various embodiments can strip fluoropolymer sidewall 445 and fluoropolymer deposition layer 504 while minimizing erosion and oxidation of silicon nitride layer 428.

[0029] 6 is a high-level block diagram illustrating a computer system 600 suitable for implementing the controllers 235 and 535 used in the embodiments. The computer system 600 may be one or more computer systems for implementing the controllers 235 and 535. Computer systems may have many physical forms, ranging from integrated circuits, printed circuit boards, and small handheld devices to large supercomputers. The computer system 600 includes one or more processors 602 and may further include an electronic display device 604 (for displaying images, text, and other data), a main memory 606 (e.g., random access memory (RAM)), a storage device 608 (e.g., a hard disk drive), a removable storage device 610 (e.g., an optical disk drive), a user interface device 612 (e.g., a keyboard, a touch screen, a keypad, a mouse, or other pointing device, etc.), and a communication interface 614 (e.g., a wireless network interface). The communication interface 614 allows software and data to be transferred between the computer system 600 and external devices over a link. The system may include a communication infrastructure 616 (eg, a communication bus, crossover bar, or network) to which the aforementioned devices / modules are connected.

[0030] Information communicated through communications interface 614 may be in the form of signals (e.g., electronic, electromagnetic, optical, or other signals that may be received by communications interface 614 over a communications link that transmits the signals) and may be implemented using wire or cable, fiber optics, telephone line, cellular phone link, radio frequency link, and / or other communications channels. It is contemplated that such communications interfaces may enable one or more processors 602 to receive information from a network or output information to a network in the course of performing the method steps described above. Additionally, method embodiments may be implemented solely in a processor, in cooperation with a remote processor that performs some of the processing, or may be implemented over a network such as the Internet.

[0031] The term "non-transitory computer-readable medium" is generally used to refer to media such as main memory, secondary memory, removable storage, and storage devices (e.g., hard disks, flash memory, disk drive memory, CD-ROMs, and other forms of persistent memory), and is not to be construed to include transitory objects such as carrier waves or carrier signals. Examples of computer code include machine code (e.g., produced by a compiler) and files having high-level code that are executed by a computer using an interpreter. A computer-readable medium may also be computer code transmitted by a computer data signal embodied in a carrier wave and representing a sequence of instructions executable by a processor.

[0032] Although the present disclosure has been described in terms of several preferred embodiments, there are changes, modifications, permutations, and various substitute equivalents that fall within the scope of the present disclosure. It should also be noted that there are many alternative ways of implementing the methods and apparatuses of the present disclosure. Thus, the following appended claims are intended to be construed to include all such changes, modifications, permutations, and various substitute equivalents that fall within the true spirit and scope of the present disclosure. The expression "A, B, or C" as used herein should be construed to mean logic using a non-exclusive logical "OR" ("A OR B OR C"), and should not be construed to mean "only one of A or B or C". Each step in a process may be optional and not required. Different embodiments may omit one or more steps or provide steps in a different order. Also, various embodiments may provide different steps simultaneously rather than sequentially.

Claims

1. 1. A method for stripping a polymer-containing sidewall film from an etch feature and a polymer-containing deposition layer from a backside of a bevel of a wafer having a stack including at least one silicon nitride-containing layer, comprising: generating a plasma from a stripping gas, the stripping gas comprising: Hydrogen (H 2 ) containing gas; CO 2 , C.O., N 2 O, NO, and NO 2 wherein the plasma generates radicals from the strip gas; and exposing the wafer to the radicals, the radicals removing the polymer-containing sidewall film and the polymer-containing deposition layer; A method comprising:

2. 2. The method of claim 1 , The H 2 The contained gas is H 2 and, N 2 and a forming gas comprising: The forming gas is 0.1% to 4% H 2 That is, the method.

3. 3. The method of claim 2, The strip gas is mainly composed of the forming gas and CO 2 , C.O., N 2 O, NO, and NO 2 and at least one of:

4. 3. The method of claim 2, The strip gas is primarily comprised of the forming gas, at least one inert gas, and CO 2 , C.O., N 2 O, NO, and NO 2 The method comprises at least one of the following:

5. 2. The method of claim 1 , The method wherein the strip gas is halogen-free.

6. 1. A method for processing a stack including at least one silicon nitride-containing layer on a wafer having a bevel, comprising: Etching at least one feature in the at least one silicon nitride containing layer, the etching of the at least one feature including forming a polymer-containing sidewall film in the at least one feature and forming a polymer-containing deposition layer on a backside of the beveled portion of the wafer, the etching being provided in a vacuum etch chamber; transferring the wafer from the etch chamber to a strip chamber without breaking the vacuum; Stripping the polymer-containing sidewall film and the polymer-containing deposition layer, generating a plasma from a stripping gas, the stripping gas comprising: Hydrogen (H 2 ) containing gas; CO 2 , C.O., N 2 O, NO, and NO 2 wherein the plasma forms radicals from the strip gas; and exposing the wafer to the radicals, the radicals removing the polymer-containing sidewall film and the polymer-containing deposition layer; A method comprising:

7. 7. The method of claim 6, The H 2 The contained gas is H 2 and, N 2 and a forming gas comprising: The forming gas is 0.1% to 4% H 2 That is, the method.

8. 8. The method of claim 7, The strip gas is mainly composed of the forming gas and CO 2 , C.O., N 2 O, NO, and NO 2 and at least one of:

9. 8. The method of claim 7, The strip gas is primarily comprised of the forming gas, at least one inert gas, and CO 2 , C.O., N 2 O, NO, and NO 2 The method comprises at least one of the following:

10. 7. The method of claim 6, The method wherein the strip gas is halogen-free.

11. 7. The method of claim 6, The method wherein the step of stripping the polymer is carried out at a temperature in the range of 20°C to 500°C.

12. 7. The method of claim 6, The method, wherein the polymer-containing deposition layer and the polymer-containing sidewalls comprise a fluoropolymer.

13. 13. The method of claim 12, The method, wherein the polymer-containing deposition layer further comprises an ammonium salt.

14. 1. A method for stripping a polymer-containing sidewall film from an etch feature and a polymer-containing deposition layer from a backside of a bevel of a wafer having a stack including at least one silicon nitride-containing layer, comprising: generating a plasma from a strip gas, the strip gas comprising CO 2 , C.O., N 2 O, NO, and NO 2 wherein the plasma generates radicals from the strip gas; and exposing the wafer to the radicals, the radicals removing the polymer-containing sidewall film and the polymer-containing deposition layer; A method comprising:

15. 15. The method of claim 14, The strip gas is mainly CO 2 , C.O., N 2 O, NO, and NO 2 The method comprises at least one of the following:

16. 15. The method of claim 14, The strip gas mainly comprises at least one inert gas and CO 2 , C.O., N 2 O, NO, and NO 2 and at least one of: