Airbag fabric for vehicles

By controlling tenacity and DPF in airbag fabrics, recycled polymers are effectively integrated, addressing quality issues and ensuring mechanical integrity and efficiency in airbag manufacturing.

JP2024541262AInactive Publication Date: 2024-11-08INVISTA TEXTILES (U K) LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2024525683
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2022-01-10
Filing Date
2023-01-06
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing airbag manufacturing processes face challenges in incorporating recycled polymers due to quality issues such as inconsistent feedstock, contaminants, and increased fuzz content, which affect the mechanical properties and efficiency of the final product.

Method used

The use of tenacity and denier per filament (DPF) as control parameters to incorporate recycled polymeric material into airbag fabrics, with specific ranges for weft and warp yarns, along with optimized processing conditions to minimize fuzz and maintain mechanical integrity.

Benefits of technology

This approach enables the production of airbag fabrics with improved consistency and quality, suitable for commercial use, by balancing recycled polymer content with virgin material to achieve desired mechanical properties and reduced fuzz levels.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024541262000001
    Figure 2024541262000001
  • Figure 2024541262000002
    Figure 2024541262000002
  • Figure 2024541262000003
    Figure 2024541262000003
Patent Text Reader

Abstract

The vehicle airbag fabric includes a weft yarn and a warp yarn. The weft yarn contains 1% to 100% by weight of recycled polymeric material, has a denier per filament (dpf) of 1 to 6, a tenacity of 65 to 80 cN / tex, and a fuzz content of 150 or less fuzz per million linear meters of yarn. The warp yarn contains an equal or less amount of recycled polymeric material per unit weight than the weft yarn, has a denier per filament (dpf) of 1 to 6, and has a fuzz content less than the fuzz content of the weft yarn.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to fabrics suitable for making vehicle airbags and containing recycled polymeric materials. [Background technology]

[0002] Inflatable airbags are a major component of vehicle safety systems. Airbags are typically made from woven synthetic fibers, such as nylon or polyester yarns. As with many other industries around the world, net carbon neutrality and other sustainability efforts are increasingly being sought in automotive manufacturing. One means of addressing this growing need is to use recycled polymers in the airbag fiber manufacturing process. Historically, airbags have typically been made from virgin or newly manufactured polymers, as fibers produced using recycled polymers are typically not of suitable quality for the desired end use.

[0003] Polymers can be recycled by different means, including mechanical regrind and remelting and / or chemically breaking down the polymer chains back into monomeric components. The sources of regenerated polymer feedstocks and their respective qualities can vary based on the steps in the supply chain. Typical sources can include scrap from polymer and / or fiber manufacturing processes, scrap from fabric weaving and / or cutting processes, and fabric from decommissioned airbag modules (both pre- and post-deployment). In addition to the quality of the final product, other challenges introduced through the use of recycled polymers include traceability, consistency, and process efficiency. Traceability must be maintained throughout the process for quality control. Consistency of the regenerated feedstock is important to achieve the physical property targets and consistency required for the final textile product.

[0004] Contaminants potentially introduced in various steps of the process create challenges in the fiber spinning process as they reduce the quality of the polymer and result in an increased content of broken filaments or "fuzz". The additional thermal history of the polymer processed through mechanical regeneration can also result in an increased fuzz content in the fiber spinning due to the formation of pyrolysis products. To ensure that the product is suitable for the required end use, limitations are placed on the allowable fuzz content in the warp and weft yarns, meaning that it can withstand the mechanical and tensile stresses of weaving and maintain an acceptable level of efficiency in downstream processing. The quality of the feedstock, the fiber manufacturing process, and the desired fabric properties must be optimized to achieve a quality end product suitable for use in commercial airbag weaving.

[0005] EP 2687628 B1 discloses a fabric for use in forming vehicle airbags, in which at least some of the yarns, particularly the weft yarns, are formed partially or entirely from recycled polymeric materials. However, EP 2687628 B1 does not mention possible control parameters that may allow the recycled polymeric materials to be successfully incorporated into the airbag fabric with minimal loss of performance in the final airbag. The present disclosure seeks to address this issue. Summary of the Invention

[0006] In accordance with the present disclosure, it has now been discovered that tenacity and denier per filament (DPF) can be used as control parameters to successfully incorporate recycled polymeric material into at least the fill yarns of an airbag fabric. In some embodiments of the disclosed fabric, recycled polymeric material can be incorporated into both the warp and fill yarns of the airbag fabric.

[0007] Thus, in one aspect, the present application provides a vehicle airbag fabric, comprising: (a) a weft yarn containing 1% by weight or more and 100% by weight or less of recycled polymer material, (i) having a denier per filament (dpf) of 1 to 6, for example, a denier per filament (dpf) of 2 to 4, (ii) having a tenacity of 65 to 80 cN / tex; (iii) a weft yarn having a fuzz content of 150 or less fuzz per million linear meters of yarn; (b) a warp yarn containing an equal or less amount of recycled polymer per unit weight than the weft yarn; (i) the warp yarns have a denier per filament (dpf) of 1 to 6, for example, a denier per filament (dpf) of 2 to 4, (ii) providing a vehicle airbag fabric in which the warp yarns have a fuzz content that is less than the fuzz content of the weft yarns;

[0008] In a further aspect, the present application provides a vehicle airbag fabric, comprising: (a) a weft yarn containing 1% by weight or more and 100% by weight or less of recycled polymer material, (i) a weft yarn having a tenacity of 65 to 80 cN / tex; (b) a warp yarn containing an equal or less amount of recycled polymer per unit weight than the weft yarn; (i) the tenacity of the warp yarns is within ±10% of the tenacity of the weft yarns; (ii) providing a vehicle airbag fabric in which the warp yarns have less fuzz per million linear meters than the weft yarns; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Disclosed is a vehicle airbag fabric that includes warp and weft yarns, where at least a portion of the weft yarns, and possibly at least a portion of the warp yarns, contain recycled polymeric material. The remainder of both the weft and warp yarns are comprised of virgin polymeric material. Typically, the virgin polymer of each of the weft and warp yarns is comprised at least in part of nylon, such as nylon 6,6. Similarly, at least a portion of the recycled polymeric material is comprised of nylon, such as nylon 6,6.

[0010] In one embodiment, the vehicle airbag fabric disclosed herein comprises: (a) a weft yarn containing 1% by weight or more and 100% by weight or less of recycled polymer material, (i) having a denier per filament (dpf) of 1 to 6, for example, a denier per filament (dpf) of 2 to 4, (ii) having a tenacity of 65 to 80 cN / tex; (iii) a weft yarn having a fuzz content of 150 fuzz or less per million linear meters of yarn; (b) a warp yarn containing an equal or less amount of recycled polymer per unit weight than the weft yarn; (i) the warp yarns have a denier per filament (dpf) of 1 to 6, for example, a denier per filament (dpf) of 2 to 4, (ii) the warp yarns have a fluff content that is less than the fluff content of the weft yarns;

[0011] In a further embodiment, the vehicle airbag fabric disclosed herein comprises: (a) a weft yarn containing 1% by weight or more and 100% by weight or less of recycled polymer material, (i) a weft yarn having a tenacity of 65 to 80 cN / tex; (b) a warp yarn containing an equal or less amount of recycled polymer per unit weight than the weft yarn; (i) the tenacity of the warp yarns is within ±10% of the tenacity of the weft yarns; (ii) the warp yarns have less fuzz per million linear meters than the weft yarns;

[0012] As used herein, the term "fuzz" refers to discontinuous filaments in a fiber bundle that are visible on the surface of a yarn or fabric. As disclosed herein, "fuzz" is measured by optical detection. Fuzz concentration is expressed as the number of visually observable discontinuities ("fuzz") per million linear meters of fiber. Fuzz can significantly reduce manufacturing process efficiency and result in inadequate quality of the final fabric. In particular, above the 150 fuzz per million linear meters threshold, the quality of the weft yarn has been found to adversely affect runnability and efficiency of the weaving process and / or degrade fabric properties and / or quality through the generation of fabric defects. Generally, fuzz levels below the 150 fuzz per million linear meters threshold are preferred for the weft yarn, such as fuzz of 50 or less per million linear meters, and even fuzz of 5 or less per million linear meters. The fuzz level of the warp yarn is maintained below the fuzz level of the weft yarn, preferably below 5 fuzz per million linear meters. Recycled polymer materials

[0013] Recycled polymeric materials may be sourced through various steps in the supply chain ranging from batch polymerization waste to airbag modules salvaged at the end of a vehicle's life. Additionally, there are non-airbag sources of recycled polymeric materials available that can be used. The use of clean feedstock sources (such as fabric from undeployed vs. scrap deployed airbags) minimizes the adverse impact of contaminants. Recycled polymeric material feedstocks can be sourced via post-industrial and post-consumer routes and can include other alternatives to traditional nylon-6,6.

[0014] Different levels and qualities of recycled polymeric materials can be incorporated into as-produced nylon-6,6 (virgin polymer) for spinning into fibers. Impurities in recycled polymeric materials can include moisture, spin finishes, carbon, and additives intentionally introduced during initial manufacturing / processing, to name just a few. Impurity levels can vary widely depending on the source of recycled polymeric material feedstock. The specific ranges of moisture, spin finish, and carbon disclosed herein can be tolerated in recycled polymeric materials and mixed-virgin recycled polymeric materials by adjusting the tenacity, DPF, and percentage of recycled polymeric material in the final product to provide mixed-virgin recycled polymeric material fibers with fuzz of 0 to 150 per million linear meters of yarn. In general, it is desirable to minimize the content of reinforcing compounds in recycled polymeric materials, for example, it is desirable to minimize the content of glass fibers in recycled polymeric materials.

[0015] Reclaimed polymers can be processed by different means such as chemical or mechanical regeneration. Chemical regeneration can be used to depolymerize the input material back to its constituent monomers if a suitable depolymerization method is available. Mechanical regeneration is more commonly used, where scrap material is processed by regrind and reextrusion. In this process, it is important to control the filtration rate of the extruded material to improve contaminant removal. Furthermore, as with any fiber manufacturing process, it is important to control the effects of the reextrusion process itself, including controlling the cleanliness of the extruder to avoid further introduction of contaminants, controlling the formation of pyrolytic species in the extrusion process (controlling the process temperature, maintaining appropriate process shear rates and residence times, eliminating cold zones, etc.). Pellet size consistency and moisture content should also be controlled. In certain circumstances, additives such as RV or heat stabilizers can be used to optimize certain parameters of the reclaimed polymer material. Textile Manufacturing Process

[0016] In an embodiment, the introduction of recycled polymers into the fiber manufacturing process is optimized to improve the quality of the final product. The recycled polymeric material should be appropriately blended with the virgin polymer to ensure consistent polymer properties and quality. Furthermore, the recycled polymeric material may be introduced into the polymer remelt process through a side stream when blended with the virgin polymer to avoid an additional heat exposure step. It is desirable to provide recycled polymeric material with substantially the same particle shape and particle size distribution as the virgin polymer. It has been found that uniform shape and distribution facilitates uniform mixing and incorporation of the recycled polymeric material into the final mix-virgin recycled polymer composition.

[0017] After extrusion of the mixed-virgin recycled polymer composition, the resulting yarn is quenched (cooled) before drawing. The quenching process should be optimized to balance the final fiber properties, such as variable denier, and fuzz formation. In general, it has been found that a gentler quenching process (lower quench air flow, delayed quenching) results in lower fuzz formation.

[0018] To improve the quality of the final product, the production rate (polymer throughput in the fiber manufacturing process) should also be optimized. The throughput can be reduced to achieve improved fuzz levels.

[0019] Ideally, the number of times a polymer has been recycled should be known and controlled. More regeneration iterations are desirable from an overall sustainability perspective, as they allow for circularity in the supply chain and reduce the amount of virgin material utilized. However, the number of times a polymer is recycled must be balanced by its increased thermal history.

[0020] The percentage of recycled polymeric material content can be varied to improve the quality of the final product. A lower percentage of recycled polymeric material content can be used to improve the fuzz level. Suitable ranges of recycled polymeric material content include: 1% by weight or more and 100% by weight or less of weft yarn, 20% by weight or more and 60% by weight or less of weft yarn, and The weft is 30% by weight or more and 50% by weight or less.

[0021] Typically, the warp yarns contain equal or less recycled polymer per unit weight than the weft yarns.

[0022] Increasing yarn tenacity is achieved by increasing the draw during the fiber spinning process, but with a trade-off of increasing the fuzz content. The objective is to optimize the balance between these two properties. The trade-off between tenacity and increased fuzz content is influenced by the percentage of regenerated content in the fiber as well as the quality of the regenerated feedstock.

[0023] Suitable ranges of tenacity in the weft yarn include the following: 65cN / tex or more - 80cN / tex or less, and Between 70cN / tex and 80cN / tex.

[0024] Generally, the warp tenacity is maintained within ±10% of the weft tenacity.

[0025] Suitable ranges of denier per filament (dpf) for both warp and weft yarns include the following: 1.0dpf or more to 6.0dpf or less, 1.5dpf or more to 4.5dpf or less, and 2.0dpf or more and 4.0dpf or less. From both a spinning standpoint and other industry requirements, a lower denier per filament (dpf) is preferred, for example, low denier per filament (dpf) products can be quenched more quickly than their higher dpf counterparts, resulting in less spherulite growth and less fuzz forming during the subsequent spinning process.

[0026] The disclosed airbag fibers can include additives to protect the recycled polymeric material polymer from thermal degradation and chain branching. Such additives can include phosphinate compounds and metal halides. Metal halides are suitable as thermal protectants in virgin nylon polymer spinning. In the disclosed process, increased concentrations of metal halides (above levels typically used in virgin nylon polymer spinning) are suitable to provide additional protection against the additional heat exposure associated with mechanical regeneration.

[0027] The disclosed airbag fabric may include recycled yarns that contain chemical markers that identify it as recycled material. Suitable chemical markers include trace colors, pigments or fluorescent agents, metals, halides, molecular tags or other easily detectable materials.

[0028] The quality of the recycled polymeric material feedstock is important to control, since the introduction of contaminants or other impurities will adversely affect the efficiency of the spinning process and the quality of the spun recycled fibers. Examples of such contaminants can include spin finish content from the fiber spinning process, increased or fluctuating moisture content from waterjet weaving, and silicone coatings from downstream processing steps, as well as polyacrylic acid sizes or oils and fats from warp pre-treatment to act as weaving aids. The properties of the recycled polymeric material can be controlled to optimize fiber spinning performance. Examples of suitable variables and values ​​include moisture content (e.g., less than 1500 ppm for polyamides), metal contamination (e.g., less than 50 ppm), finish oil content (e.g., less than 2 wt%), to name just a few. One way to tailor the recycled polymeric material composition is to preferentially source materials from known "clean" sources, such as fiber manufacturing and waterjet weaving scraps. Another method is by additional processing of the feedstock material, such as separation of the silicone coating from the substrate material prior to recycling processing, use of washing and / or drying processes to remove spin finishes and / or residual sizing or other weaving aids and control moisture content prior to processing, use of a vented extruder during the remelting step to remove undesirable gaseous by-products, or some combination of these.

[0029] Another potential control parameter is the relative viscosity (RV) variation of the recycled polymer material. Size control during the re-pelletization process of the recycled polymer material is important for this step. Furthermore, blend consistency is improved when blending with virgin polymer pellets. Blending prior to pellet consumption can also help reduce the variation of polymer properties, whether in blends with virgin material or within many recycled polymer material pellets. A batch mixer or flow channel blender can be used to achieve this blending.

[0030] Due to the source of recycled polymeric material feedstock, the re-pelletized polymer can have a higher RV than the comparable virgin material. In order to control the resulting RV of the blended (virgin and recycled polymeric material) polymer and to minimize additional thermal degradation caused by further increasing the thermal history of the recycled material, the recycled polymeric material pellets can be co-fed to a virgin polymer remelting system before extrusion. This also helps to control the color difference of the recycled polymer compared to virgin polymer. The recycled polymeric material pellets can optionally be conditioned in a separate system to the virgin polymer pellets before co-fed if some RV increase is desired before extrusion.

[0031] Feedstock processed through mechanical regeneration has a higher level of degradation due to the additional thermal history of the polymer from the re-pelletization and polymer extrusion process prior to spinning. One way to minimize thermal degradation is to feed the shredded regenerated polymer material feedstock directly to the extruder, eliminating the re-pelletization step. Additionally, various additives can be used to protect the regenerated polymer material from thermal degradation and chain branching. Such additives can include phosphinate compounds and metal halides. Metal halides are already commonly used as thermal protectants in virgin nylon polymer spinning, but increased concentrations can be used to provide additional protection against the additional thermal exposure associated with mechanical regeneration. As discussed above, the re-extrusion process itself can be controlled to limit the introduction of contaminants and the formation of other decomposition species, such as carbon formed by oxidative degradation. Polymer quality, which is influenced by both the quality of the feedstock and the effects of the regeneration process itself, is important in the downstream fiber spinning process. Polymer quality is suitably controlled, for example, to maintain an acceptable pack pressure rise rate (less than 0.25 psi / kg). Increased pack filtration can be used to improve fiber spinning performance (and reduce fuzz formation). These benefits are balanced against the increased rate of pressure rise across the filtration pack.

[0032] Fibers are then formed by extruding filaments of molten polymer containing a percentage of recycled polymeric material content through a spinneret at high temperature and pressure The filaments are then quenched in air, coated with a lubricant, drawn between a pair of heated godets, lightly textured to provide sufficient entanglement to create a coherent fiber bundle, and wound onto a tubular core to form a bobbin.

[0033] Woven fabrics can then be formed from the warp and weft yarns using weaving techniques known in the art. Due to the mechanical and tensile stresses of weaving, the fiber fuzz content in both the warp and weft bobbins must be controlled to maintain suitable fabric quality and loom efficiency. The use of recycled polymeric materials can increase the level of fuzz generated during fiber spinning if the recycled polymeric materials are of lower quality than virgin polymers or contain contaminants. In the process of the present invention, several solutions are used to control the generation of fuzz so that the spinning process can operate at an acceptable efficiency. Such solutions can include reducing the throughput of the spinning process, reducing the tenacity of the final fiber product, manipulating the level of recycled polymeric material content used in the spinning process, limiting the number of times the material can be recycled, and / or using different levels of recycled polymeric material in the warp and weft bobbins. Due to the stresses of warp / beaming, the fuzz limitation is more limited in the warp direction. In order to meet these limitations at a particular fiber tenacity while maximizing the overall recycled polymeric material content in the fabric, a higher fluff content is tolerated so that more recycled polymeric material content can be used in the weft fiber spinning process.

[0034] Maintaining a minimum elongation in the spun fibers is important to maintain efficiency during the weaving process and to maintain performance in the final fabric. As polymer quality degrades, factors such as thermal degradation and other contaminants can cause the elongation of the spun fibers to begin to decrease as well. One solution to this problem is to reduce the tenacity of the spun fibers, such as to 65-80 cN / tex, thereby maintaining elongation.

[0035] The number of repeated regeneration steps that a polymer undergoes should also be adjusted to avoid loss of physical properties and to control the effects of increased thermal and / or oxidative degradation and contamination. To control the effects of repeated regeneration, polymers that have been regenerated more than once can be used in combination with polymers undergoing their first regeneration treatment. The balance of these two types of regenerated polymers can be manipulated depending on factors such as spinning performance and / or desired fiber tenacity.

[0036] The invention will now be described in more detail with reference to the following non-limiting examples, the results of which are shown in Table 1 below.

[0037] In the examples and the remainder of the specification, the following tests are used to obtain the results given.

[0038] The fuzz level is measured using online optical detection. Each yarn line passes an infrared sensor. Disturbances in the infrared beam indicate the presence of fuzz. The number of detected fuzz is then normalized to a linear meter length in millions of meters.

[0039] Fiber breaking strength and elongation at break are measured according to ASTM D885.

[0040] Denier is measured according to ASTM D1907.

[0041] Tenacity is calculated using the fiber breaking strength and denier.

[0042] The construction (also known as fabric count) is measured in accordance with ISO 7211-2 (1984).

[0043] Fabric tensile strength (N) (also known as ultimate force) and elongation at ultimate force (%) are tested according to standard ISO 13934-1 (2013) with the following modifications: The initial gauge (clamp) length set on the Instron tensile testing machine is 200 mm. The crosshead speed on the Instron is set at 200 mm / min. Fabric samples are first cut to size 350x60mm, then frayed by unraveling the yarn lines on the long sides to a test width of 50mm. Tensile tests are performed on five warp direction and five weft direction specimens cut from each test fabric in a diagonal cross pattern, avoiding any area within 200 mm of the fabric selvedge. The reported results for maximum force (also known as breaking force or breaking load) are the average of the maximum force results of 5 warp direction specimens and 5 (separate) weft direction specimens tested in Newtons (N). The reported result for elongation at maximum force (also known as elongation or extensibility) is the average (%) of the elongation results at maximum force of 5 warp direction specimens and 5 (separate) weft direction specimens tested. Tear strength is measured according to EASC 9904 0180 3.17 which specifies the test standard ISO 13937-2 with the following modifications: o Cut sample IAW with section 4.07 with a slit extending from the midpoint of the edge to the center as shown.

[0044] Tear strength (also known as tear force) is measured according to ISO 13937-2(2000) with the following modifications: The size of the fabric sample is 150mm x 200mm (with a 100mm slit extending from the midpoint of the narrow end to the centre. Tear tests are performed on five warp direction and five weft direction specimens cut from each test fabric in a diagonal cross pattern, avoiding any area within 200 mm of the fabric selvedge. Warp direction tear results are taken from samples tested where the tear is lengthwise (i.e. the warp thread line tears) whereas weft direction results are taken from samples tested where the tear is widthwise (i.e. the weft thread line tears). Each leg of the specimen is folded in half and secured in Instron clamp grips in accordance with Annex D / D.2 of ISO 13937-2. Evaluation of test results shall be in accordance with Section 10.2 "Calculation using electronic devices" of ISO13937-2. The reported results for longitudinal tear force are the average of the tear force results of five warp direction specimens in Newtons (N), while for transverse tear force they are the average of the tear force results of five weft direction specimens.

[0045] Stiffness is measured according to ASTM D4032-08(2016) with the following modifications: The plunger stroke speed is 2000mm / min. Stiffness tests are performed on five warp direction and five weft direction specimens cut from each test fabric in a diagonal cross pattern, avoiding any area within 200mm of the fabric selvedge. o Each 200 x 100 mm sample is single folded across the narrow dimension before being placed on the instrument testing platform for testing. o The reported results for warp stiffness (in Newtons) are the average of the stiffness results of the five warp direction specimens, while the results for weft stiffness are the average of the five weft direction samples. Warp stiffness results are taken from samples tested whose longest dimension (200mm) is parallel to the fabric warp direction, while weft stiffness results are taken from samples tested whose longest dimension (200mm) is parallel to the fabric weft direction.

[0046] Edge comb resistance (also known as edge pull-out test) is measured in Newtons (N) and is tested according to standard ASTM D6479-15(2020), but with the following modifications: The edge distance is 5 mm, which is the distance between the end of the test specimen (positioned during the test on a narrow protrusion machined in the test specimen holder) and the line of the pin that performs the "pulling", i.e. this is the length of the thread line section that is pulled out during the test. Edge comb resistance tests are performed on five warp direction and five weft direction specimens cut from each test fabric in a diagonal cross pattern, avoiding any area within 200mm of the fabric selvedge. Warp direction edge comb resistance results are obtained from testing samples whose major dimension is parallel to the warp yarns, while weft direction results are obtained from testing samples whose major dimension is parallel to the weft yarns. The reported results for warp edge comb resistance are the average of the edge comb resistance results of five warp direction samples in Newtons (N), while for weft edge comb resistance they are the average of the results of five weft direction samples.

[0047] Static air permeability (l / dm 2 / min) is tested according to test standard ISO 9237 (1995), but with the following modifications: ○Test area is 100cm 2 It is. ○The test pressure (partial vacuum) is 500 Pa. Each individual test value is corrected for edge leakage. Static air permeability testing is performed at six sites on the test fabric in a sampling pattern across and along the fabric to test six separate areas of warp and weft yarn lines within the fabric. Static air permeability results reported are in l / dm 2 The average of six corrected measurements is taken in units of / min.

[0048] Dynamic air permeability is tested according to test standard ASTM D6476-12(2021) with the following modifications: The limits of the measured pressure range (as set on the test instrument) are 30 to 70 kPa. The starting pressure (as set on the test fixture) is adjusted to achieve a peak pressure of 100 + / - 5 kPa. The test head volume should be 400 cm unless the specified starting pressure can be achieved with this head. 3 where other interchangeable test heads (volumes 100, 200, 800 and 1600 cm) may be used as found appropriate for the fabric under test. 3 ) should be used. The Dynamic Air Permeability Test is performed at six sites on the test fabric in a sampling pattern across and along the fabric to test six separate areas of warp and weft yarn lines within the fabric. Dynamic Air Permeability results reported are the average of six DAP measurements in mm / sec. Comparative Example 1

[0049] The airbags are made from conventional 100% virgin nylon 6,6 polymer in both the warp and weft fibers. The fiber properties are suitable for use in airbag weaving. The results are reported in column C1 of Table 1 below. Comparative Example 2

[0050] The airbags are made from 100% post-industrial mechanically regenerated nylon 6,6 polymer material in both warp and weft fibers. The tenacity is significantly reduced to maintain acceptable elongation and fuzz levels, but the final fabric properties (tensile, tear) are outside the desired range for airbag applications. The results are reported in column C2 of Table 1 below. Comparative Example 3

[0051] Airbags are made from 50% post-industrial mechanically recycled nylon 6,6 polymer material in both warp and weft fibers without process optimization to ensure end-use suitability. Tenacity is maintained at standard virgin airbag levels and fiber dpf is not optimized. As a result, fiber elongation and fuzz levels are not suitable for use in airbag fabric weaving. Results are reported in column C3 of Table 1 below. Example 1 of the present invention

[0052] The airbags are made from 30% post-industrial mechanically regenerated nylon 6,6 polymer material in both warp and weft fibers, with the remainder of both warp and weft fibers being virgin nylon 6,6 polymer. The tenacity is reduced to maintain acceptable fiber elongation and fuzz levels. The resulting fabric properties are suitable for airbag end use. The results are reported in column I1 of Table 1 below. Example 2 of the present invention

[0053] The airbag is made from warp fibers containing 20% ​​post-industrial mechanically regenerated nylon 6,6 polymer material and weft fibers containing 50% post-industrial mechanically recycled nylon 6,6 polymer material. The remainder of both the warp and weft fibers is virgin nylon 6,6 polymer. Fiber tenacity is adjusted to balance final fabric properties with acceptable elongation and fuzz content. Results are reported in Table 1, column I2 below. [Table 1]

Claims

1. 1. A vehicle airbag fabric comprising: (a) a weft yarn containing from 1% by weight to 100% by weight of recycled polymer material, (i) having a denier per filament (dpf) of 1 to 6, inclusive, for example, a denier per filament (dpf) of 2 to 4, inclusive; (ii) having a tenacity of 65 to 80 cN / tex; (ii) a weft yarn having a fluff content of 150 fluffs or less per million linear meters of yarn; (b) a warp yarn containing an equal or less amount of recycled polymer per unit weight than the weft yarn; (i) the warp yarns have a denier per filament (dpf) of 1 to 6, for example, a denier per filament (dpf) of 2 to 4, (ii) the warp yarns have a fuzz content that is less than the fuzz content of the weft yarns.

2. 2. The fabric of claim 1, wherein said warp yarns and said weft yarns differ in tenacity by no more than 10%.

3. 1. A vehicle airbag fabric comprising: (a) a weft yarn containing from 1% by weight to 100% by weight of recycled polymer material, (i) a weft yarn having a tenacity of 65 to 80 cN / tex; (b) a warp yarn containing an equal or less amount of recycled polymer per unit weight than the weft yarn; (i) the tenacity of the warp yarns is within ±10% of the tenacity of the weft yarns; (ii) the vehicle airbag fabric, wherein said warp yarns have less fuzz per million linear meters than said weft yarns.

4. The fabric of claim 3, wherein the weft yarns have a denier per filament (dpf) of 1 to 6, for example, a denier per filament (dpf) of 2 to 4, inclusive.

5. 5. The fabric of claim 3 or claim 4, wherein the warp yarns have a denier per filament (dpf) of ≥ 1 to ≤ 6, such as ≥ 2 to ≤ 4.

6. The fabric according to any one of claims 1 to 5, wherein the weft yarns contain from 20% to 60% by weight of recycled polymeric material.

7. The fabric according to any one of claims 1 to 6, wherein the weft yarns contain from 30% to 50% by weight of recycled polymeric material.

8. A fabric according to any one of claims 1 to 7, wherein the weft yarns have a fluff content of 50 fluffs or less, such as 5 fluffs or less, per million linear metres of yarn.

9. The fabric of any one of claims 1 to 8, wherein the recycled polymeric material contains a chemical marker that identifies it as a recycled material.

10. 10. The fabric of claim 9, wherein the chemical marker is at least one selected from the group consisting of a colorant, a fluorescent agent, a metal, and a halide.

11. The fabric according to any one of claims 1 to 10, wherein the warp and weft yarns are at least partially composed of nylon.

12. The fabric of any one of claims 1 to 11, wherein the recycled polymeric material is at least partially composed of nylon.

Citation Information

Patent Citations

  • Airbaggewebe

    DE202012008550U1

  • Improvements in or relating to air-bag material

    EP2687628A1

  • load limit web

    JP2002518604A

  • Method for producing woven fabric for airbag

    JP2007046193A

  • Fabric for non-coated airbags

    WO2013168730A1