METAL SUBSTRATE STRUCTURE FOR SEMICONDUCTOR POWER MODULE, METHOD FOR ATTACHING TERMINAL TO METAL SUBSTRATE STRUCTURE, AND SEMICONDUCTOR POWER MODULE

Laser welding with protrusions and spacer elements on metal substrates addresses the reliability issues of terminal attachment, ensuring stable and damage-resistant semiconductor power modules for high-voltage applications.

JP2024541509APending Publication Date: 2024-11-08HITACHI ENERGY LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2024531301
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-11-26
Filing Date
2022-10-27
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

Conventional insulated metal substrates face challenges in reliably attaching terminals due to potential damage from welding processes, especially ultrasonic welding, which can cause thermal and mechanical stress leading to resin layer deformation and cracking, limiting their use in high-voltage power modules.

Method used

A method involving laser welding with strategically designed protrusions and spacer elements on the metal substrate structure, combined with anti-reflection coatings and controlled laser parameters, to securely attach terminals while minimizing thermal shock and mechanical stress on the resin layer.

Benefits of technology

This approach enables stable and reliable attachment of terminals, reducing the risk of resin layer damage and enabling high-voltage power module functionality without cracking, thus ensuring reliable operation from 0.5kV to 10.0kV.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024541509000001_ABST
    Figure 2024541509000001_ABST
Patent Text Reader

Abstract

A method for attaching a terminal (4) to a metal substrate structure (3) for a semiconductor power module (10) includes providing at least one terminal (4) and providing the metal substrate structure (3) with a top metal layer (17), a bottom metal layer (19), and an insulating resin layer (18) disposed between the top metal layer (17) and the bottom metal layer (19). The method further includes bonding the at least one terminal (4) to the top metal layer (17) of the metal substrate structure (3) by laser welding with a laser beam (6).
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a method for attaching a terminal to a metal substrate structure of a semiconductor power module with an insulating resin sheet, and further relates to a semiconductor power module for a semiconductor device. The present disclosure further relates to a corresponding metal substrate structure. [Background technology]

[0002] Conventional insulated metal substrates form the technology for low and medium power semiconductor packages that simultaneously have low insulation and low thermal requirements. Terminals are provided on the insulated metal substrate and reliable connection of the terminals on the insulated metal substrate is required. Summary of the Invention [Means for solving the problem]

[0003] Embodiments of the present disclosure relate to methods for attaching terminals to metal substrate structures that can contribute to low-cost metal substrate structures for semiconductor power modules that can function reliably even in high voltage power module applications. Further embodiments of the present disclosure relate to corresponding metal substrate structures for semiconductor devices and semiconductor power modules.

[0004] According to one embodiment, a method for attaching a terminal to a metal substrate structure for a semiconductor power module includes providing at least one terminal and providing the metal substrate structure with a top metal layer, a bottom metal layer, and an insulating resin layer disposed between the top metal layer and the bottom metal layer. The top metal layer is provided and fabricated from an integral part having at least one protrusion having a given locally enhanced thickness of up to 2.0 mm thicker than adjacent regions of the top metal layer. The protrusion is formed on an upper surface of the top metal layer at a location configured to be coupled to at least one terminal. The method further includes coupling the at least one terminal to the protrusion of the top metal layer of the metal substrate structure by laser welding with a laser beam.

[0005] The described method allows the realization of laser welded joint connections on insulated metal substrates, which can contribute to a stable and reliable functioning of semiconductor power modules, even in high voltage power module applications. The method contributes to a reliable attachment of the terminals on the insulated metal substrate by laser welding. The intentionally formed protrusions allow the protection of the resin layer against thermal shocks and may be formed integrally with the circuit metallization, which has a locally greater thickness at the location of the terminal base. The protrusions provide a longer thermal path between the welding location and the resin layer, as well as a stronger lateral heat diffusion in the substrate metallization, but also in the mechanical strengthening of the substrate.

[0006] In the context of the present disclosure, it is recognized that conventional insulated metal substrates realize technology for low and medium power semiconductor packages that simultaneously have low insulation requirements and low heat resistance requirements. When the reliability requirements are low, the terminals can be soldered or glued onto the substrate, for example. Usually, welding provides better reliability, but the welding process can be critical to the substrate structure. In consideration of the conventional configuration of such insulated metal substrates, the corresponding terminals are typically connected to the top metallization using welding technology to provide a joint connection that can be critical for a stable process on the substrate and the resin isolation sheet below the metallization. The welding process can lead to damage to the substrate structure, and ultrasonic welding in particular has a strong effect of thermal and mechanical stress combined with heat on the substrate structure due to the friction and pressure between the terminal base and the substrate. Here, the resin sheet is strongly endangered by deformation and crack formation. When applying ultrasonic welding of the terminal base to the circuit metallization of the insulated metal substrate, the corresponding failure mode must be considered.

[0007] By using the described method for manufacturing metal substrate structures, it is possible to counteract the aforementioned negative effects caused by the laser welding process. Also, the risk of cracks or damage to the resin layer can be reduced, resulting in a stable semiconductor power module that functions reliably even in high voltage power module applications, for example from 0.5 kV to 10.0 kV. One or more terminals can be welded directly to the metal top layer, for example to form a direct copper-to-copper contact. Instead of a direct contact, an additional spacer element can be placed between the lower faces of the mutually facing terminals and the upper face or the top face of the metal top layer.

[0008] The resin layer forms the dielectric layer and can be realized as a prepreg sheet that is assembled between two metal plates, one above the other, which form the metal top layer and the other below. Such a metallization sheet or plate is bonded to the insulator of the dielectric resin layer, for example by a lamination process. The required metallization structure of the metal top layer can then be carried out by subsequent steps of masking and etching processes to locally remove the conductive metal, creating the final metallization structure. Alternatively, the upper metallization structure can be formed, for example by cutting or stamping, before the formation of the finished metal substrate structure.

[0009] Alternatively, the resin layer can be formed by molding. For such molded dielectric layers, the molding substance realizes a pumpable substance with predetermined material properties. The pumpable substance is a liquid or viscous feedstock of the resin layer to be formed. For example, the molding substance is an epoxy and / or ceramic-based liquid. Alternatively or additionally, the feedstock of the dielectric layer may be a thermosetting or thermoplastic resin material such as polyamide, PBT, PET, etc. Alternatively or additionally, the feedstock of the dielectric layer may include inorganic fillers for improved thermal conductivity and / or CTE adjustment for the metal top layer and / or metal bottom layer. For example, the molded dielectric layer includes a resin-based dielectric material with a ceramic filler material, such as Al2O3, AlN, BN, Si3N4 or SiO2. For example, the dielectric layer is an epoxy with filler. The dielectric layer can also be based on other materials suitable for transfer, injection or compression molding, or other applicable molding techniques such as bismaleimide, cyanate ester, polyimide and / or silicone. Alternatively or additionally, the dielectric layer may comprise a ceramic material and / or a hydroset material, or a combination of two or more of the aforementioned components.

[0010] By aligning the metal top layer and the metal bottom layer with respect to each other with a predetermined distance between them, the thickness after the molding dielectric layer is substantially predetermined. For example, the thickness is defined along the stacking direction of the metal substrate structure, which may represent the z-direction. However, alignment can also be performed in the perpendicular x- and y-directions, for example for proper positioning of the metal pattern with respect to the x- and y-directions. For example, alignment can be realized by placing the metal top layer on a release film or liner, or by other fixation, for example in a mold chase of a molding tool. This allows the provided metallization structure of the metal top layer to be accurately positioned with respect to the metal bottom layer, which can be useful, for example, when the metal top layer includes separate metal pads due to different operating potentials. In the case of lamination, the thickness of the resin layer is given by the thickness and behavior of the laminated layers.

[0011] According to an embodiment of the method, at least one terminal is provided with one or more coatings partially or completely covering a predetermined surface of the respective terminal. The terminal may include an anti-reflective coating on an upper surface configured to face the impinging laser beam during laser welding. The irradiation efficiency of the laser beam may be improved, for example, by an anti-reflective coating arranged on the upper side of the terminal base. Alternatively or additionally, the terminal may include a coating made of a noble metal, for example silver or gold, on a lower surface configured to face the metallic top layer of the metal substrate structure during laser welding, for example to prevent oxidation or for an improved laser welding process.

[0012] According to a further embodiment of the method, the laser parameters of the laser beam can be given to have a beneficial effect on the laser welding. Thus, the laser beam or the corresponding laser source used for the laser welding can be configured to provide a power of 300-3000 W. Alternatively or additionally, the laser beam or the laser source for the laser welding can be configured to provide a moving speed of 1-200 mm / s guided along the upper surface of the at least one terminal facing the impinging laser beam. Thus, the welding does not have to be performed only at one limited point, but the laser spot of the laser beam providing the welding process can be moved at the aforementioned speed to provide a joint connection over a defined area.

[0013] The laser beam can also be configured to oscillate at a predetermined frequency, so the laser spot position can oscillate or oscillate at frequencies up to 2 kHz to have a beneficial effect on the welding process.

[0014] According to a further embodiment of the method, the step of coupling the at least one terminal to the metal substrate structure by laser welding includes aligning the terminal and the metal substrate structure relative to one another such that upper surfaces of the metal top layer contact lower surfaces of opposing terminals, and the method further includes laser welding the terminal with a laser beam such that a weld joint between the terminal and the metal substrate structure is formed, securely bonding the at least one terminal and the metal top layer.

[0015] According to a further embodiment of the method, the terminal and the metal substrate structure are aligned relative to each other at a predetermined distance between them, which defines a gap of up to 500 μm between the upper surface of the metal top layer and the lower surface of the terminal, which face each other. The laser welding of the terminal by the laser beam is performed in such a way that the terminal melts locally and a welded joint between the terminal and the metal substrate structure is formed by a drop or run or deformation of the molten metal part (held by surface tension) and firmly bonds at least one terminal and the metal top layer. By using such a configuration, improved positioning of the terminal and protection of the insulated metal substrate structure against heat can be realized, which is achieved by forming a small gap of up to several hundred microns between the metal top layer and the terminal. The terminal can have an L-shape with a terminal body and a terminal base, the terminal base can be held in place, while the laser welded joint connection is provided by a drop or deformation of the molten material from the terminal base.

[0016] In the context of the present disclosure, it is recognized that, despite being a less critical circumstance compared to ultrasonic welding, the laser welding process of copper terminals on the circuit metallization of a metal substrate structure formed by a metal top layer beneficially includes features for minimizing the thermal shock to the heat-sensitive insulating resin sheet or layer. On the one hand, the thermal shock to the resin layer can be reduced by protective features that reduce the heat flow to the resin layer. On the other hand, the shock can be reduced by features that additionally or alternatively reduce the thermal effort required to achieve the laser welded terminal bonding.

[0017] Additionally, the separate spacer elements may form predetermined protrusions on the surface of a top metal layer, such as a copper foil or sheet or block.

[0018] According to a further embodiment, the method includes providing a metal spacer element configured to form a protrusion for the at least one terminal and bonding the metal spacer element to a metal top layer of the metal substrate structure. The method further includes bonding the at least one terminal to the metal spacer element by laser welding with a laser beam such that a welded joint between the terminal and the metal spacer element is formed, firmly bonding the at least one terminal and the metal spacer element. The metal spacer element can be provided in the form of a metal block or spring, for example, having a thickness of 0.5 mm to 2.0 mm. The thickness relates to a dimension along a stacking direction of the metal substrate structure and the at least one terminal, and can also represent the height of the protrusion extending above the adjacent top surface of the metal top layer.

[0019] Mounting additional metal blocks or springs on the top surface of the metal substrate structure at the location where the terminal base is joined by laser welding contributes to protecting the resin layer against thermal shock. The metal blocks or springs can be joined to the circuit metallization or metal top layer by soldering, gluing, sintering, or any other suitable joining method.

[0020] According to a further embodiment of the method, the metallic spacer element comprises a coating layer on an upper surface configured to face the lower surface of the at least one terminal during laser welding. The metallic spacer element may be fully or partially coated with a noble metal such as silver or gold or nickel or other metals on its upper surface for an improved joining process to the terminal. Alternatively or additionally, the metallic spacer element may be fully or partially coated with a noble metal on its lower surface for an improved joining process to the metal top layer.

[0021] According to a further embodiment of the method, at least one terminal comprises a terminal base configured to be bonded with the metal top layer and comprising a structure prepared for improved laser welding. Such a welded structure can be realized by a thinned area, a slot, a groove and / or a recess in the terminal base. Alternatively or additionally, the complete terminal base may be formed thinner than the body of the terminal. For example, the thickness range of the thinned terminal base may be between 0.3 and 0.8 times the thickness of the terminal body.

[0022] Such a particular terminal structure can beneficially influence the laser welding process and contribute to reducing the heating power or energy impact of the laser irradiation by the laser beam on the terminal base. Therefore, one option is to partially or completely reduce the thickness of the terminal base. The complete terminal base or at least the welded area of ​​the terminal base can be thinned compared to adjacent parts such as the vertical body part of the terminal. Alternatively, the terminal base can be locally thinned, for example by implementing one or more grooves, recesses and / or slots in the terminal base.

[0023] The welding process can be performed on such thinner sections, resulting in less metal being melted and less of a consequence of lateral heat dissipation, thereby reducing the laser energy required to achieve the laser weld connection.

[0024] The implementation of holes or slots in the terminal base can enable direct irradiation of the interface, particularly the edges of the holes or slots between the substrate metallization formed by the metal top layer, for example, and the terminal base, so that less metal needs to be melted to achieve the laser welded joint connection. Additionally, lateral heat spread within the terminal base can be prevented or reduced by the holes, slots, or grooves.

[0025] The terminal base can be welded to a metal top layer or metal spacer element such that the weld connection includes multiple small localized spots on the terminal base to reduce thermal shock during laser welding with sufficient pauses for cooling between preparations of a single weld spot. Here, the total thermal energy may not be reduced, but the thermal energy per spot and the pauses in the process facilitate sufficient heat dissipation, resulting in less temperature rise in the resin layer. Additionally, the terminal base can be specifically designed to beneficially affect the formation of multiple weld locations, for example due to holes, slots and / or grooves prepared for welding.

[0026] According to a further embodiment of the method, the step of providing a metal substrate structure comprises providing a top metal layer, providing a bottom metal layer, and providing a dielectric material in the form of a molding substance. The method further comprises aligning the top metal layer and the bottom metal layer with respect to each other with a predetermined distance therebetween, and introducing the provided molding substance between the aligned top metal layer and the bottom metal layer, thereby forming an insulating resin layer, for example by molding by injection molding, compression molding and / or transfer molding.

[0027] Furthermore, according to one embodiment of the method, the step of bonding at least one terminal to the top metal layer by laser welding can be performed before the top metal layer is bonded to the resin layer and / or the bottom metal layer. Thus, a laser welded connection between the terminal and the top metal layer can be performed, and then the top metal layer is bonded to the dielectric resin layer and / or the bottom metal layer. In other words, the bond between the top metal layer and the resin layer and / or the bottom metal layer is subsequently processed into a bond between the terminal and the top metal layer by welding. Thus, mechanical stresses from bonding the terminal and / or thermal stresses from laser welding are kept away from the resin layer, contributing to avoid cracking or other damage to the resin layer.

[0028] By using the described manufacturing or mounting method, it is possible to counteract the negative effects of using a laser welding process. Thus, the risk of crack or damage formation can be reduced and a stable semiconductor power module is realized that allows the semiconductor power module to function reliably. One or more terminals can be welded directly to the surface of the metal top layer, for example, to form a direct copper-to-copper contact. Alternatively, there can be spacer elements arranged between the lower surfaces of the mutually facing terminals and the upper surface or top surface of the metal top layer.

[0029] Finally, it is pointed out that all proposed features and methods can be used alone, but also in combination of two or more.

[0030] According to one embodiment, a metal substrate structure for a semiconductor power module includes a top metal layer, a bottom metal layer, and an insulating resin layer disposed therebetween and bonded to both the top metal layer and the bottom metal layer, and further includes at least one terminal bonded to the top metal layer by laser welding.

[0031] At least one terminal may include an anti-reflective coating on a top surface of the terminal base configured to face the impinging laser beam during laser welding and / or a coating on a bottom surface of the terminal base configured to face the metal top layer of the metal substrate structure during laser welding.

[0032] According to a further embodiment, the metal substrate structure comprises a metal spacer element configured to form a protrusion for at least one terminal and bonded to the metal top layer. The metal spacer element is further bonded to the at least one terminal by laser welding with a laser beam such that a weld joint is formed between the terminal and the metal spacer element, firmly bonding the at least one terminal and the metal spacer element. Such a protrusion can be formed by a separate element on the metal top layer and / or may be formed integrally with the metal top layer.

[0033] According to one embodiment, a semiconductor power module for a semiconductor device comprises an embodiment of the described metal substrate structure and is electrically interconnected with at least one terminal of the metal substrate structure. The semiconductor power module may further comprise a heat sink coupled with the metal bottom layer of the metal substrate structure to dissipate heat during operation of the semiconductor power module. Thus, the semiconductor power module may comprise a separate heat sink. Alternatively or additionally, the metal bottom layer of the metal substrate structure may act as a heat sink itself, for example, configured with ribs or protrusions on the bottom side relative to the stacking direction to provide beneficial heat dissipation. The metal bottom layer may further function as a base plate of the semiconductor power module. The semiconductor power module including the metal substrate structure may further be partially or completely encapsulated by a resin or dielectric gel made by molding or potting. The terminal may function as a power terminal or as an auxiliary terminal, for example used for signal wiring.

[0034] Additionally, a semiconductor power module may include two or more embodiments of the aforementioned metal substrate structures. Electronic devices may include chips, integrated circuits, and / or other discrete devices.

[0035] As a result of the described metal substrate structures being capable of being manufactured by the described embodiments of the method, and as a result of the described semiconductor power modules including embodiments of the metal substrate structures, the described features and characteristics of the method are also disclosed with respect to the metal substrate structures and the semiconductor power modules, and vice versa. Thus, the present disclosure includes several aspects, and all features described with respect to one of the aspects are also disclosed herein with respect to the other aspects, even if each feature is not expressly mentioned in the context of a particular aspect.

[0036] The present disclosure relates to laser welding of power and auxiliary terminals on insulated metal substrates or insulated metal base plates as well as on substrate structures based on alternative metal substrate construction techniques such as stamped and formed metal substrate structures. For example, the insulated metal substrate comprises a relatively thick metal base or bottom layer, for example made of aluminum and / or copper. The insulated metal substrate further comprises an insulating sheet based on a resin material forming a resin layer and a circuit metallization consisting of aluminum and / or copper forming a metal top layer. The resin material used for the insulating sheet is typically a thermosetting resin containing a thermally conductive inorganic filler material. This filler material consists mostly of aluminum nitride (AlN), silicon nitride (Si3N4), boron nitride (BN), or ceramic particles prepared from aluminum oxide (Al2O3) or silicon oxide (SiO2). The resin insulating layer can have a thickness of 100-200 μm and the circuit metallization of the metal top layer may have a thickness of 150-500 μm.

[0037] The terminals can be realized as main and / or auxiliary terminals made of copper or copper alloys and are laser welded to the circuit metallization of the insulated metal substrate. With laser welding, a laser beam is applied from the top surface of the terminal base, resulting in intense local heating. A controlled local melting of the materials of the terminal base and the substrate surface occurs, forming a highly reliable joint material connection. Depending on the type and material of the terminal, the terminal base can have a thickness of 0.5-2.0 mm. For an improved welding process or for protection against, for example, oxidation, the substrate top surface and / or the terminal base may be coated by a metal layer, made for example from nickel, silver and / or gold.

[0038] Considering laser welding to securely bond the terminals to the metal top layer or optional metal spacer element, thermal shock is a fundamental consideration when welding the terminals to the circuit metallization of the insulated metal substrate. Nevertheless, thermal shock of the laser welding process causing local melting of the terminal base occurs, and additional measures and / or features may be useful to prevent or counteract damage to the resin layer during welding. One or more of the following features may be used to improve the thermal situation during laser welding by improving protection of the resin layer or reducing the total amount of heat.

[0039] Localized thicker board metallization at the base of the terminals to mechanically reinforce the board locally and reduce thermal effects on the resin sheet Additional platelets attached to the board surface at the terminal locations to locally mechanically reinforce the board and reduce thermal shock to the resin sheet Coating of the terminals and / or substrate with precious metals or other metals, e.g. nickel, to prevent oxidation and make bonding more effective Anti-reflective coating on the terminals to avoid laser reflections and reduce power for more effective welding Thinner terminal base for more effective welding with less power and less material melting (completely or locally) Slits or holes at the base of the terminal and welding of the edges of the slits or holes to locally concentrate the temperature (avoiding lateral spreading) Gap between terminal base and board surface during welding process Multiple localized laser welded connections.

[0040] Any such option may be applied alone, but combinations of two or more of these options are also possible.

[0041] The proposed process of laser welding of the terminal base on the insulated metal substrate has a strong possibility of significantly reducing the mechanical effects on the resin insulating sheet, for example, compared to ultrasonic welding. Moreover, by applying one or more of the proposed features, the thermal shock of the laser welding process can be reduced. A successful welding process is possible without damaging the heat- and pressure-sensitive resin layer, making the use of this relatively cost-effective substrate technology interesting. Such a method of mounting or manufacturing metal substrate structures can be interesting for large power modules and modules, even for higher voltage classes. If replacing the conventional standard configuration of a ceramic substrate soldered to a base plate by an insulated metal substrate, significant cost reductions can be possible. On the one hand, material costs can be reduced, and on the other hand, several process steps, such as the joining process between the substrate and the base plate in the power module assembly, are removed from the process flow. However, the described method also makes it possible to manufacture metal substrate structures and semiconductor power modules that can be applied in miscellaneous products, in particular low-voltage industrial and automotive products.

[0042] Exemplary embodiments are described below with the aid of schematic diagrams and reference numbers. BRIEF DESCRIPTION OF THE DRAWINGS [Brief description of the drawings]

[0043] [Figure 1] 1 is a side view of one embodiment of a method for attaching terminals to a metal substrate structure of a semiconductor power module. [Diagram 2] 11 is a side view of a further embodiment of a method for attaching a terminal to a metal substrate structure of a semiconductor power module using a platelet. [Diagram 3] 1 is a side view of an embodiment of a terminal for attachment to a metal substrate structure. [Figure 4] 1 is a side view of an embodiment of a terminal for attachment to a metal substrate structure. [Diagram 5]FIG. 2 is a top view of an embodiment of a terminal base of a terminal. [Figure 6] FIG. 2 is a top view of an embodiment of a terminal base of a terminal. [Figure 7] FIG. 2 is a top view of an embodiment of a terminal base of a terminal. [Figure 8] FIG. 2 is a top view of an embodiment of a terminal base of a terminal. [Figure 9] 4 is a flow chart of a method for attaching one embodiment of a terminal to a metal substrate structure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0044] The accompanying drawings are included to provide further understanding. It should be understood that the embodiments shown in the figures are illustrative representations and are not necessarily drawn to scale. The same reference numbers indicate elements or components having the same functions. Insofar as the elements or components correspond to each other with respect to their functions in different figures, the description thereof will not be repeated for each of the following figures. For clarity, elements may not be labeled with corresponding reference numbers in all figures in some cases.

[0045] 1 shows a side view of one embodiment of method steps for attaching terminals 4 to a metal substrate structure 3 of a semiconductor power module 10 for a semiconductor device. The semiconductor power module 10 comprises a metal substrate structure 3 having a top metal layer 17, a bottom metal layer 19, and an insulating resin layer 18 disposed between the top metal layer 17 and the bottom metal layer 19. The electronic device may include, for example, a chip and a power semiconductor device.

[0046] The semiconductor power module 10 further comprises a heat sink 1 having a rib structure bonded to a metal substrate structure 3 by a bonding layer 2 and / or a layer of thermal interface material. With respect to the illustrated stacking direction A, the terminals 4 should be bonded to the top metal layer 17 and below the heat sink 1 are bonded to the bottom metal layer 19 via the bonding layer 2.

[0047] In this regard, terms such as "above," "under," "top," "upper," and "bottom" refer to the orientation or direction as shown in the figures and relative to stacking direction A. Thus, the height or thickness of a described element is relative to stacking direction A, and lateral directions B and C are oriented perpendicular to stacking direction A (see Figures 1-8).

[0048] The thickness of the insulating resin layer 18 may be, for example, 100-200 μm. The thickness of the circuit metallization formed by the metal top layer 17 may be 150-500 μm. The thickness of the metal bottom layer 19, which may realize a base plate, may be 2-3 mm and may be configured to dissipate heat from the metal substrate structure 3 and the semiconductor power module 10. The resin layer 18 may include an epoxy resin material, but other types of resins are also possible, such as thermosetting or thermoplastic resins. The resin layer 18 may be formed as a resin sheet or as a prepreg sheet that is assembled or laminated between the two metal layers 17, 19. Alternatively or additionally, the metal substrate structure 3 comprises a resin layer 18 formed by molding, for example by injection, transfer or compression molding. The resin of the resin layer may include inorganic fillers, ceramic materials such as AlN, Si3N4, BN, Al2O3 or SiO2. The metallic bottom layer 19 can be made of or include copper and / or aluminum and / or corresponding alloys. The circuit metallization formed by the metallic top layer 17 can be made of or include copper and / or aluminum and / or corresponding alloys. Furthermore, the metallic top layer 17 can be partially or completely coated, and the corresponding coating of the circuit metallization can be made of or include nickel and / or gold and / or silver and / or other metals.

[0049] The method steps for attaching a terminal 4 to a metal substrate structure 3 may follow the flow chart shown in Figure 9. Thus, according to the embodiment shown in Figure 1, at least one terminal 4 is provided in step S1. The terminal 4 is provided with an anti-reflective coating 5 on its upper surface 41.

[0050] In step S2, the metal substrate structure 3 is provided with a top metal layer 17, a bottom metal layer 19 and an insulating resin layer 18 disposed therebetween.

[0051] In optional step S3, additional metal spacer elements 7 can be provided to form protrusions for the terminals 4 on the upper surface 171 of the metal top layer 17 (see FIG. 2). The spacer elements 7 are bonded to the upper metallization at the terminal locations.

[0052] In a further step S4, the terminals 4 are bonded to the metal top layer 17 of the metal substrate structure 3 by laser welding using a laser beam 6 such that a weld joint 16 between the terminals 4 and the metal top layer 17 is formed, firmly bonding the terminals 4 and the metal top layer 17. An anti-reflective coating 5 partially or completely covers the top surface 41 of the terminals 4 facing the impinging laser beam 6, improving the laser welding process.

[0053] The terminal 4 may be provided with an L-shape in side view, as shown in Figures 3 and 4. The terminal 4 thus comprises a terminal body 13 and a terminal base 12, made either integrally or formed as a separate piece. The terminal base 12 is configured to be joined with the metal top layer 17 and may be provided with structures prepared for laser welding having one or more of thinned areas (see Figure 3) and / or slots, grooves 20 and / or recesses 15 (see Figures 4-8). Such structures may be actual openings or recesses and / or thinned sections only.

[0054] Such modifications of the terminal base 12 can contribute to an improved laser welding process and attachment of the terminal to the metal substrate structure 3. Also, thermal stresses affecting the resin layer 18 are reduced. The terminal base 12 can be provided with a completely reduced thickness or with a welded area with a reduced thickness less than the thickness of the vertical terminal body 13 of the terminal 4. Alternatively or additionally, one or more grooves 20 or other local recesses 15 can favorably influence the laser welding process performed at the bottom of such recess openings (see Figs. 4 to 8). This also applies to the implementation of holes or slots, where the laser welding can be performed directly at the edges of such holes or slots 20, for example at the interface between the terminal base 12 and the metallization. The laser welding process can also be performed for several small local spots on the terminal base 12, as shown in Figs. 5 and 6. This can also be applied to a terminal base 12 that has been thinned so that several local weld spots are formed.

[0055] The terminal 4 can be made of or contain copper and / or a copper alloy and can realize a main or auxiliary terminal for electrical connection to the electronics of the semiconductor power module 10. The terminal base 12 can have a thickness with respect to the stacking direction A of 1 mm, 1.5 mm or 2 mm. The terminal base 12 can be partially or completely thinned to have a thickness of 0.5 mm or less. Thus, the terminal base 12 can have a thickness of 0.5 to 2 mm. If there is a locally thinned portion, this portion may have a thickness of at least 0.25 mm. Furthermore, the terminal 4 can be provided with a terminal coating layer 9 partially or completely covering the lower surface 42 of the terminal base 12. The terminal coating layer 9 can have a beneficial effect on the laser welding process and may be made of or include nickel, gold, silver and / or other metals. Such a coating can also be useful for mounting the terminal 4 in combination with an additional metal spacer element 7 (see FIG. 2).

[0056] When such an additional spacer is provided, the method for attaching the terminal 4 includes bonding a metal spacer element 7 to the metal top layer 17 of the metal substrate structure 3 and bonding the terminal 4 to the metal spacer element 7 by laser welding using a laser beam 6 such that a weld joint 16 between the terminal 4 and the metal spacer element 7 is formed, securely bonding the terminal 4 and the metal spacer element 7.

[0057] Arranging metal spacer elements 7, for example in the form of metal blocks or spring structures, between the circuit metallization of the metal top layer 17 and the terminals 4 also allows for an improvement of the laser welding process and protection of the resin layer 18. The metal spacer elements 7 may have a thickness of 0.5 mm to 2.0 mm. The metal spacer elements 7 can be manufactured, for example, via a stamping tool. Instead of or in addition to separate metal spacer elements 7, the circuit metallization of the metal top layer 17 can be provided with a locally enhanced thickness itself, which is intentionally formed in the stacking direction A and with a height of up to 2.0 mm relative to adjacent areas of the metal top layer 17. Such protrusions are formed at the positions of the metal top layer 17 where the terminals 4 are to be attached.

[0058] The metallic spacer elements 7 may be made of or include copper and / or a copper alloy. The spacer coating layer 8 may be disposed on the upper surface or top surface 71 of the metallic spacer elements 7 partially or completely covering the top surface 71. Alternatively or additionally, a coating may be present on the bottom surface of the spacer elements 7.

[0059] The spacer coating layer may be made of or include nickel, gold, silver and / or other metals. The metal spacer elements 7 may be connected to the upper surface 171 of the metal top layer 17 by soldering, sintering, gluing and / or other applicable joining methods.

[0060] Furthermore, the laser welding process can be configured to provide certain parameters to beneficially influence the formation of one or more weld joints 16. Thus, the laser power of the laser beam 6 can be 300-3000 W. The speed of the laser spot of the laser beam 6 on the upper surface 41 of the terminal 4 can be 1-200 mm / s. The oscillation frequency of the laser spot for providing the oscillation can be 2 kHz or less. Such an oscillation can present an oscillation of the position of the irradiation point to prevent excessively strong local heating and can occur in addition to the laser movement described above.

[0061] Furthermore, the arrangement for attaching the terminals 4 to the metal substrate structure 3 can be arranged to provide for direct contact between the terminals 4 and the metal top layer 17 or the metal spacer element 7. Alternatively, a predefined gap of up to 500 μm can be set in the stacking direction between the abovementioned joining partners. The latter can provide a further beneficial arrangement for improved positioning of the terminals 4 and protection of the insulated metal substrate structure 3 against heat. The terminal base 12 is held in place, while the drop and / or deformation of molten material from the terminal base 12 provides the laser welded joint connection.

[0062] The described embodiment of the method for mounting and / or manufacturing the metal substrate structure 3 with one or more terminals 4 attached thereto makes it possible to reduce the risk of formation of cracks or damage in the resin layer. Thus, by this method, a stable semiconductor power module 10 is possible, which allows reliable functioning even in high voltage power module applications, for example in the voltage range from 0.5 kV to 10.0 kV.

[0063] 1-9 represent improved metal substrate structures 3, semiconductor power modules 10, and manufacturing methods, and therefore do not constitute an exhaustive list of all embodiments. Actual arrangements and methods may differ from the embodiments shown, for example, for the metal substrate structures 3 and semiconductor power modules 10. [Explanation of symbols]

[0064] Reference sign 1 Heatsink 2 Bonding Layer 3 Metal substrate structure 4 Terminals 41 Top of terminal 42 Bottom surface of terminal 5. Anti-reflective coating 6 Laser Beam 7 Metal Spacer Elements 71 Top surface of metal spacer element 8 Spacer Coating Layer 9 Terminal coating layer 10. Semiconductor power modules 11 Bonding layer 12 Terminal base 13 Terminal body 14 Base structure 15 Recess 16 Welded joints 17 Metal Top Layer 171 Top surface of top metal layer 18 Resin layer 19 Metal Bottom Layer 20 slots / grooves A Stacking direction B. Horizontal C Lateral direction S(i) Steps of a method for manufacturing a metal substrate structure for a semiconductor power module

Claims

1. A method for attaching a terminal (4) to a metal substrate structure (3) for a semiconductor power module (10), comprising the steps of: Providing at least one terminal (4); providing said metal substrate structure (3) with a metal top layer (17), a metal bottom layer (19) and an insulating resin layer (18) arranged between said metal top layer (17) and said metal bottom layer (19), said metal top layer (17) being made from an integral part having at least one protrusion having a given locally enhanced thickness of 0.5 mm to a maximum of 2.0 mm thicker than adjacent areas of said metal top layer (17), said protrusion being formed at a position on an upper surface (171) of said metal top layer (17) configured to be coupled to said at least one terminal (4); bonding said at least one terminal (4) to said protruding portion of said metal top layer (17) of said metal substrate structure (3) by laser welding using a laser beam (6); A method comprising:

2. 2. The method according to claim 1, wherein at least one of the metal substrate structure (3) and the at least one terminal (4) is provided with a structure prepared for laser welding having at least one of a thinned area, a slot, a groove (20), a hole, a coating (5, 8, 9), an opening and a recess (15), such that the bonding of the at least one terminal (4) to the metal top layer (17) of the metal substrate structure (3) by laser welding is controlled to form at least one weld joint (16) and to minimize thermal shock to the insulating resin layer (18).

3. Providing the at least one terminal (4) 3. The method of claim 1 or 2, comprising providing the at least one terminal (4) with at least one of an anti-reflective coating (5) on a top surface (41) configured to face an impinging laser beam (6) during laser welding, and a coating (9) on a bottom surface (42) configured to face the metal top layer (17) of the metal substrate structure (3) during laser welding.

4. Coupling the at least one terminal (4) to the metal substrate structure (3) by laser welding includes: aligning the terminals (4) and the metal substrate structure (3) relative to each other such that the upper surfaces (171) of the metal top layer (17) contact the opposing lower surfaces (42) of the terminals (4); laser welding said terminal (4) with said laser beam (6) such that a weld joint (16) between said terminal (4) and said metal substrate structure (3) is formed and said at least one terminal (4) and said top metal layer (17) are securely bonded together; 2. The method of any one of the preceding claims, comprising:

5. Coupling the at least one terminal (4) to the metal substrate structure (3) by laser welding includes: aligning the terminals (4) and the metal substrate structure (3) relative to one another at a predetermined distance defining a gap of up to 500 μm between the upper surface (171) of the metal top layer (17) and the lower surface (42) of the terminals (4) facing each other; laser welding the terminal (4) with the laser beam such that the terminal (4) is locally melted and a welded joint (16) is formed between the terminal (4) and the metal substrate structure (3) by a drop or run or deformation of the molten terminal material, firmly bonding the at least one terminal (4) and the metal top layer (17); The method according to any one of claims 1 to 3, comprising:

6. providing a metal spacer element (7) configured to form a protrusion for said at least one terminal (4); bonding said metal spacer element (7) to said metal top layer (17) of said metal substrate structure (3); bonding said at least one terminal (4) to said metallic spacer element (7) by laser welding using a laser beam (6) such that a weld joint (16) between said terminal (4) and said metallic spacer element (7) is formed and said at least one terminal (4) and said metallic spacer element (7) are securely bonded together; 2. The method of any one of the preceding claims, comprising:

7. Providing said metal spacer element (7) comprises:

7. The method of claim 6, comprising providing the metallic spacer element (7) with a coating layer (8) on an upper surface (71) configured to face a lower surface (42) of the at least one terminal (4) during laser welding and / or a coating layer on a lower surface configured to face an upper surface (171) of the metallic top layer (17) during laser welding.

8. 8. The method according to claim 6 or 7, wherein the metal spacer element (7) is provided in the form of one of a block and a spring having a thickness of 0.5 mm to 2.0 mm with respect to a stacking direction (A) of the metal substrate structure (3) and the at least one terminal (4).

9. The method according to any one of claims 6 to 8, wherein the metallic spacer elements (7) are bonded to the metallic top layer (17) by at least one of soldering, sintering and gluing.

10. Providing the at least one terminal (4) 10. The method according to any one of claims 6 to 9, further comprising providing the at least one terminal (4) with a terminal base (12) configured to be coupled with the metal top layer (17), the terminal base (12) comprising a structure prepared for laser welding having at least one of a thinned area, a slit, a groove (20), a hole, an opening and a recess (15).

11. 11. The method according to claim 10, wherein the laser welding is performed in the thinned areas and / or in the grooves (20) and / or in the recesses (15) and / or on the edges of the holes and / or on the edges of the slits.

12. A semiconductor power module (10), a metal substrate structure (3) having a metal top layer (17), a metal bottom layer (19), and an insulating resin layer (18) bonded between both the metal top layer (17) and the metal bottom layer (19), the metal top layer (17) being made from an integral part having at least one protrusion having a given locally enhanced thickness of 0.5 mm to a maximum of 2.0 mm thicker than adjacent areas of the metal top layer (17), the protrusion being formed at a position on an upper surface (171) of the metal top layer (17); at least one terminal (4) coupled to said protrusion of said metal top layer (17) by laser welding; A semiconductor power module (10).

13. 13. The semiconductor power module (10) of claim 12, wherein the at least one terminal (4) comprises at least one of an anti-reflective coating (5) on a top surface (41) configured to face an impinging laser beam (6) during laser welding and a coating (9) on a bottom surface (42) configured to face the metal top layer (17) of the metal substrate structure (3) during laser welding.

14. 14. The semiconductor power module (10) according to claim 12 or 13, comprising a metallic spacer element (7) configured to form a protrusion for the at least one terminal (4) and coupled to the metal top layer (17), the metallic spacer element (7) being coupled to the at least one terminal (4) by laser welding with a laser beam (6) such that a welded joint (16) is formed between the terminal (4) and the metallic spacer element (7) and such that the at least one terminal (4) and the metallic spacer element (7) are firmly bonded.

Citation Information

Patent Citations

  • Method of and device for laser beam machining

    JP1999123585A

  • Semiconductor device and manufacturing method thereof

    JP2005109147A

  • Manufacturing method, manufacturing apparatus, jig assembly, semiconductor module, and vehicle

    JP2021144984A

  • Power semiconductor device and method for producing same

    WO2018207856A1