Polyamic acid, polyimide film and flexible metal foil laminate using same
A polyimide film with specific components and composition achieves low dielectric loss and high-temperature storage modulus, addressing insulation and signal delay issues in high-frequency communications.
Patent Information
- Application Number
- JP2024529854
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-22
- Filing Date
- 2022-11-21
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2042-11-21
AI Technical Summary
Existing polyimide films do not possess adequate low dielectric properties and moisture resistance, which are crucial for maintaining insulation and reducing signal delay in high-frequency communications, especially in flexible thin circuit boards.
A polyimide film composed of specific components, including biphenyltetracarboxylic dianhydride, pyromellitic dianhydride, and p-phenylenebis(trimellitate anhydride), copolymerized with m-tolidine and paraphenylenediamine, to achieve low dielectric loss and high-temperature storage modulus, enhancing mechanical and thermal properties.
The film exhibits a dielectric loss factor of 0.003 or less at 10 GHz and a storage modulus of 100 MPa or more at 300°C, ensuring insulation stability and minimizing signal transmission delay in high-frequency electronic components.
Smart Images

Figure 2024542498000001 
Figure 2024542498000002 
Figure 2024542498000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a polyamic acid having both an excellent high-temperature storage modulus and low dielectric properties, a polyimide film, and a flexible metal foil laminate using the same. [Background technology]
[0002] Polyimide (PI) is a polymeric material based on imide rings, which have excellent chemical stability along with a rigid aromatic main chain, and has the highest levels of heat resistance, chemical resistance, electrical insulation, chemical resistance, and weather resistance among organic materials. In particular, due to its excellent electrical properties such as excellent insulating properties, i.e., low dielectric constant, it has been attracting attention as a highly functional polymer material in the electrical, electronic and optical fields.
[0003] 2. Description of the Related Art Recently, with the trend towards lighter and smaller electronic products, flexible thin circuit boards with high integration density have been actively developed. Such thin circuit boards tend to have a structure in which a circuit containing metal foil is formed on a polyimide film that has excellent heat resistance, low temperature resistance and insulating properties, but is also easily flexible. Flexible metal clad laminates are mainly used for such thin circuit boards, and an example is Flexible Copper Clad Laminate (FCCL), which uses a thin copper plate as a metal foil. Polyimide is also used as a protective film and insulating film for thin circuit boards.
[0004] Meanwhile, as electronic devices are increasingly equipped with a variety of functions, they are required to have high computing and communication speeds. To meet this demand, thin circuit boards capable of high-speed communication at high frequencies have been developed. To realize high-frequency and high-speed communication, insulators with high impedance that can maintain electrical insulation even at high frequencies are required. Since impedance is inversely proportional to the frequency and dielectric constant (Dk) formed in the insulator, the dielectric constant must be as low as possible to maintain insulation even at high frequencies. However, in the case of ordinary polyimide, the dielectric properties are not currently at a level excellent enough to maintain sufficient insulation for high-frequency communications.
[0005] In addition, the lower the dielectric properties of the insulator, the less stray capacitance (stray capacitance) is required for thin circuit boards. It is known that it is possible to reduce the capacitance and noise generation, and to largely eliminate the causes of communication delays. Therefore, the low dielectric properties of polyimide are currently recognized as the most important factor in the performance of thin circuit boards.
[0006] In particular, in the case of high-frequency communication, dielectric loss due to polyimide is inevitable. The dielectric dissipation factor (Df) indicates the degree of electrical energy wasted in a thin circuit board and is closely related to the signal transmission delay that determines the communication speed. Therefore, keeping the dielectric dissipation factor of polyimide as low as possible is recognized as an important factor in the performance of thin circuit boards.
[0007] In addition, the more moisture contained in the polyimide film, the larger the dielectric constant becomes, and the greater the dielectric loss becomes. Although polyimide film is suitable as a material for thin circuit boards due to its excellent inherent properties, it is relatively vulnerable to moisture due to the imide group exhibiting polarity, which may cause a deterioration in its insulating properties. Therefore, there is a need to develop a polyimide film that has dielectric properties, particularly a low dielectric loss factor, while maintaining a certain level of mechanical and thermal properties specific to polyimide. [Prior art documents] [Patent documents]
[0008] [Patent Document 1] Republic of Korea Patent Publication No. 10-2015-0069318 Summary of the Invention [Problem to be solved by the invention]
[0009] In order to solve the above problems, an object of the present invention is to provide a polyamic acid, a polyimide film, and a flexible metal foil laminate using the same, which have both an excellent high-temperature storage modulus and low dielectric properties. Therefore, a substantial object of the present invention is to provide specific examples thereof. [Means for solving the problem]
[0010] In order to achieve the above object, one embodiment of the present invention relates to a polymerizable composition comprising a dianhydride acid component including biphenyltetracarboxylic dianhydride (BPDA), pyromellitic dianhydride (PMDA) and p-phenylenebis(trimellitate anhydride) (TAHQ); and a diamine component including m-tolidine and paraphenylenediamine (PPD), A polyamic acid is provided.
[0011] Other embodiments of the present invention include biphenyltetracarboxylic dianhydride (BPDA), pyromellitic dianhydride (PMDA) and p-phenylenebis(trimellitate anhydride). anhydride, TAHQ, and A diamine component including m-tolidine and paraphenylenediamine (PPD) is subjected to an imidization reaction of a polyamic acid solution including the diamine component, A polyimide film is provided.
[0012] Yet another embodiment of the present invention is a laminate comprising the polyimide film and a thermoplastic resin layer, A multilayer film is provided.
[0013] Yet another embodiment of the present invention is a method for manufacturing a laminate comprising the polyimide film and an electrically conductive metal foil, A flexible metal foil laminate is provided.
[0014] Yet another embodiment of the present invention includes the flexible metal foil laminate, Provide electronic components. Effect of the Invention
[0015] As described above, the present invention provides a polyamic acid and a polyimide film which are composed of specific components and have a specific composition ratio and have both excellent high-temperature storage modulus and low dielectric properties. This makes it useful for various fields where such properties are required, particularly for electronic parts such as flexible metal foil laminates. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0016] Hereinafter, embodiments of the present invention will be described in more detail. Prior to this, the terms and words used in this specification and claims should not be interpreted limited to their ordinary or dictionary meanings, but should be interpreted with meanings and concepts that correspond to the technical ideas of the present invention, in accordance with the principle that an inventor can appropriately define the concepts of terms in order to explain his / her invention in the best possible way. Therefore, it should be understood that the configuration of the embodiment described in this specification is merely one of the most preferred embodiments of the present invention and does not fully represent the technical ideas of the present invention, and that there may be various equivalents and modifications that can replace them at the time of this application.
[0017] In this specification, the singular expression includes the plural expression unless the context clearly indicates otherwise. It should be understood that in this specification, the terms "comprise", "comprise", "have" and the like are intended to specify the presence of embodied features, numbers, steps, components, or combinations thereof, and do not preclude the possibility of the presence or addition of one or more other features, numbers, steps, components, or combinations thereof.
[0018] Whenever an amount, concentration, or other value or parameter is given herein as a range, a preferred range or a list of an upper preferred value and a lower preferred value, it should be understood to specifically disclose all ranges formed by any pair of any upper range limit or preferred value, and any lower range limit or preferred value, regardless of whether a range is otherwise disclosed. Where a range of numerical values is recited herein, unless otherwise stated, the range is intended to include the endpoints thereof, and all integers and fractions within the range. It is not intended that the scope of the invention be limited to the specific values recited when defining a range.
[0019] As used herein, "dianhydride acid" is intended to include precursors or derivatives thereof which may not technically be dianhydrides but which nevertheless must react with a diamine to form a polyamic acid which is then converted back to a polyimide.
[0020] As used herein, "diamine" is intended to include precursors or derivatives thereof, which may not technically be diamines, but which nevertheless must react with a dianhydride to form a polyamic acid, which is then converted back to a polyimide.
[0021] The polyamic acid according to the present invention is copolymerized with a dianhydride component including biphenyltetracarboxylic dianhydride (BPDA), pyromellitic dianhydride (PMDA), and p-phenylenebis(trimellitate anhydride, TAHQ), and a diamine component including m-tolidine and paraphenylenediamine (PPD).
[0022] In one embodiment, the polyamic acid has a biphenyltetracarboxylic dianhydride content of 15 mol % or more and 70 mol % or less, a pyromellitic dianhydride content of 10 mol % or more and 50 mol % or less, and a p-phenylenebis(trimellite The content of the carboxylic acid anhydride may be 5 mol % or more and 75 mol % or less.
[0023] Furthermore, based on 100 mol % of the total content of the diamine components, the content of the m-tolidine may be 20 mol % or more and 45 mol % or less, and the content of the paraphenylenediamine may be 55 mol % or more and 80 mol % or less.
[0024] In one embodiment, the polyamic acid may be a block copolymer comprising two or more blocks.
[0025] The polyimide film according to the present invention is obtained by subjecting a polyamic acid solution containing a dianhydride acid component including biphenyltetracarboxylic dianhydride (BPDA), pyromellitic dianhydride (PMDA), and p-phenylenebis(trimellitate anhydride, TAHQ) and a diamine component including m-tolidine and paraphenylenediamine (PPD) to an imidization reaction.
[0026] In one embodiment, the polyimide film may have a biphenyltetracarboxylic dianhydride content of 15 mol% or more and 70 mol% or less, a pyromellitic dianhydride content of 10 mol% or more and 50 mol% or less, and a p-phenylene bis(trimellitate anhydride) content of 5 mol% or more and 75 mol% or less, based on a total content of the dianhydride acid components of 100 mol%.
[0027] As the content of the p-phenylene bis(trimellitate anhydride) increases, the measured dielectric loss factor of the polyimide film decreases, and at the same time, the storage modulus at high temperature (300° C.) decreases.
[0028] Furthermore, based on 100 mol % of the total content of the diamine components, the content of the m-tolidine may be 20 mol % or more and 45 mol % or less, and the content of the paraphenylenediamine may be 55 mol % or more and 80 mol % or less.
[0029] In one embodiment, the polyamic acid solution that is imidized to prepare the polyimide film may be a block copolymer including two or more blocks.
[0030] In one embodiment, the first block of the block copolymer may have a biphenyltetracarboxylic dianhydride content of 50 mol % or more and 60 mol % or less, based on 100 mol % of the total content of dianhydride acid components in the polyimide film, and the second block may have a m-tolidine content of 30 mol % or more and 40 mol % or less, based on 100 mol % of the total content of diamine components in the polyimide film. For example, the first block is obtained by imidizing biphenyltetracarboxylic dianhydride and paraphenylenediamine, and the second block is obtained by imidizing m-tolidine and pyromellitic dianhydride.
[0031] In addition, all of the biphenyltetracarboxylic dianhydride in the first block is imidized with paraphenylenediamine, and all of the m-tolidine in the second block is imidized with pyromellitic dianhydride.
[0032] The m-tolidine has a methyl group that exhibits hydrophobicity, and contributes to the low moisture absorption property of the polyimide film and the resulting low dielectric property of the polyimide film.
[0033] The polyimide chain derived from the biphenyltetracarboxylic dianhydride has a structure called a charge transfer complex (CTC), i.e., a regular linear structure in which an electron donor and an electron acceptor are located close to each other, and intermolecular interactions are strengthened. This structure has the effect of preventing hydrogen bonding with moisture, which has an effect of lowering the moisture absorption rate, thereby maximizing the effect of lowering the moisture absorption of the polyimide film.
[0034] In one embodiment, the dianhydride component may further include a pyromellitic dianhydride, which is a dianhydride component having a relatively rigid structure and is preferred in that it can impart suitable elasticity to the polyimide film.
[0035] In order for the polyimide film to simultaneously satisfy the appropriate elasticity and moisture absorption rate, the content ratio of the dianhydride is particularly important. For example, the lower the content ratio of biphenyltetracarboxylic dianhydride, the less likely it is that the low moisture absorption rate due to the CTC structure will be achieved.
[0036] In addition, biphenyltetracarboxylic dianhydride contains two benzene rings corresponding to the aromatic moiety, whereas pyromelitic dianhydride contains one benzene ring corresponding to the aromatic moiety.
[0037] An increase in the content of pyromellitic dianhydride in the dianhydride acid component can be understood as an increase in the imide groups in the molecule based on the same molecular weight, which can be understood as a relative increase in the ratio of imide groups derived from the pyromellitic dianhydride in the polyimide polymer chain compared to the imide groups derived from biphenyltetracarboxylic dianhydride. That is, an increase in the content of pyromellitic dianhydride is seen as a relative increase in imide groups with respect to the entire polyimide film, which makes it difficult to expect a low moisture absorption rate. Conversely, if the content ratio of the pyromellitic dianhydride is decreased, the components having a relatively rigid structure are decreased, and the elasticity of the polyimide film may be decreased below a desired level. For this reason, when the content of the biphenyltetracarboxylic dianhydride is higher than the above range or the content of the pyromellitic dianhydride is lower than the above range, the mechanical properties of the polyimide film are deteriorated, and it is not possible to ensure a suitable level of heat resistance for producing a flexible metal foil laminate. Conversely, if the content of the biphenyltetracarboxylic dianhydride is below the above range or the content of the pyromellitic dianhydride is above the above range, it is difficult to achieve an appropriate level of dielectric constant and dielectric loss factor, which is not preferable.
[0038] In one embodiment, the polyimide film may have a dielectric loss factor (Df) of 0.003 or less and a storage modulus measured at 300° C. of 100 MPa or more. For example, the dielectric loss factor of the polyimide film may be 0.0028 or less, 0.0027 or less, 0.0026 or less, or 0.0025 or less.
[0039] The polyimide film may have a storage modulus measured at 300° C. of 2,000 MPa or less, or 1,900 MPa or less. In this regard, the dielectric loss factor (Df) and storage modulus measured at 300°C all exceeded the In the case of the added polyimide film, it can be used as an insulating film for flexible metal foil laminates. Furthermore, even if the manufactured flexible metal foil laminates are used as electrical signal transmission circuits that transmit signals at high frequencies of 10 GHz or more, the insulation stability is ensured and signal transmission delays can be minimized.
[0040] The polyimide film satisfying all of the above requirements is a novel polyimide film that has not been known before. The dielectric loss factor (Df) of the polyimide film will be described in detail below.
[0041] <Dielectric loss factor> "Dielectric loss factor" refers to the force dissipated by a dielectric (or insulator) when molecular friction impedes molecular motion induced by an alternating electric field. The dielectric loss factor is usually used as an index of how easily a charge is lost (dielectric loss): the higher the dielectric loss factor, the easier it is to lose a charge, and conversely, the lower the dielectric loss factor, the harder it is to lose a charge. In other words, the dielectric loss factor is a measure of power loss, and the lower the dielectric loss factor, the faster the communication speed can be maintained while mitigating signal transmission delays caused by power loss. This is a strong requirement for polyimide films, which are insulating films, and the polyimide film of the present invention has a dielectric loss factor of 0.003 or less at a very high frequency of 10 GHz.
[0042] In the present invention, the polyamic acid can be produced, for example, by (1) A method in which the entire amount of the diamine component is placed in a solvent, and then the dianhydride component is added in an amount substantially equimolar to the diamine component to polymerize it; (2) A method in which the entire amount of the dianhydride component is placed in a solvent, and then a diamine component is added in an amount substantially equimolar to the dianhydride component to polymerize it; (3) A method in which a part of the diamine component is placed in a solvent, a part of the dianhydride component is mixed with the reaction components in a ratio of about 95 to 105 mol %, the remaining diamine component is added, and the remaining dianhydride component is added successively thereto, so that the diamine component and the dianhydride component are polymerized in substantially equimolar amounts; (4) A method in which a dianhydride component is placed in a solvent, a part of the components in the diamine compound is mixed in a ratio of 95 to 105 mol % relative to the reactive components, and then another dianhydride component is added, followed by the remaining diamine component, so that the diamine component and the dianhydride component are substantially equimolar, thereby polymerizing the mixture; (5) A method of forming a first composition by reacting some diamine components and some dianhydride acid components in a solvent so that one of them is in excess, and forming a second composition by reacting some diamine components and some dianhydride acid components in another solvent so that one of them is in excess, and then mixing the first and second compositions to complete polymerization, in which if the diamine component is in excess when the first composition is formed, the dianhydride acid component is in excess in the second composition, and if the dianhydride acid component is in excess in the first composition, the diamine component is in excess in the second composition, and the first and second compositions are mixed to polymerize so that the total diamine components and dianhydride acid components used in these reactions are substantially equimolar.
[0043] However, the polymerization method is not limited to the above example, and the first to third polyamic acids can be produced by any known method.
[0044] In one embodiment, a method for producing a polyimide film according to the present invention includes the steps of: Polyamic acid is produced by polymerizing dianhydride components including biphenyltetracarboxylic dianhydride (BPDA), pyromellitic dianhydride (PMDA), and p-phenylenebis(trimellitate anhydride, TAHQ) with diamine components including m-tolidine and paraphenylenediamine (PPD). and forming a film of a precursor composition containing the polyamic acid on a support, and then imidizing the film.
[0045] In the present invention, the polymerization method of the polyamic acid as described above can be defined as a random polymerization method, and the polyimide film prepared from the polyamic acid of the present invention prepared by the above process can be preferably applied in terms of maximizing the effect of the present invention, which is to reduce the dielectric loss factor (Df) and moisture absorption rate. However, in the above polymerization method, the length of the repeating unit in the polymer chain is relatively short as described above, so that there may be a limit to the excellent properties of the polyimide chain derived from the dianhydride acid component. Therefore, the polymerization method of polyamic acid that can be particularly preferably used in the present invention is the block polymerization method.
[0046] On the other hand, the solvent for synthesizing the polyamic acid is not particularly limited, and any solvent that dissolves the polyamic acid can be used, but an amide-based solvent is preferable. Specifically, the solvent may be an organic polar solvent, more specifically, an aprotic polar solvent, for example, one or more selected from the group consisting of N,N-dimethylformamide (DMF), N,N-dimethylacetamide, N-methyl-pyrrolidone (NMP), gamma-butyrolactone (GBL), and diglyme, but is not limited thereto, and may be used alone or in combination of two or more kinds as needed. In one example, the solvent is preferably N,N-dimethylformamide or N,N-dimethylacetamide.
[0047] In addition, in the process for producing the polyamic acid, a filler may be added for the purpose of improving various properties of the film such as sliding properties, thermal conductivity, corona resistance, loop hardness, etc. The filler to be added is not particularly limited, but preferred examples include silica, titanium oxide, alumina, silicon nitride, boron nitride, calcium hydrogen phosphate, calcium phosphate, mica, etc.
[0048] The particle size of the filler is not particularly limited and may be determined depending on the film properties to be modified and the type of filler to be added. In general, the average particle size is 0.05 to 100 μm, preferably 0.1 to 75 μm, more preferably 0.1 to 50 μm, and particularly preferably 0.1 to 25 μm. If the particle size is below this range, the modifying effect is unlikely to be achieved, whereas if it exceeds this range, the surface properties may be significantly damaged or the mechanical properties may be significantly reduced.
[0049] The amount of the filler to be added is not particularly limited, and may be determined depending on the film properties to be modified, the particle size of the filler, etc. In general, the amount of the filler to be added is 0.01 to 100 parts by weight, preferably 0.01 to 90 parts by weight, and more preferably 0.02 to 80 parts by weight, relative to 100 parts by weight of polyimide. If the amount of the filler added is less than this range, the modifying effect of the filler is unlikely to be exhibited, and if the amount exceeds this range, the mechanical properties of the film may be significantly damaged. The method of adding the filler is not particularly limited, and any known method may be used.
[0050] In the production method of the present invention, the polyimide film is produced by a thermal imidization method and a chemical imidization method.
[0051] Alternatively, the imidization method may be a hybrid imidization method in which a thermal imidization method and a chemical imidization method are performed in parallel.
[0052] The thermal imidization method is a method in which a chemical catalyst is excluded and the imidization reaction is induced by a heat source such as hot air or an infrared dryer. The thermal imidization method can imidize the amic acid groups present in the gel film by heat-treating the gel film at a variable temperature in the range of 100 to 600°C, specifically, 200 to 500°C, more specifically, 300 to 500°C. However, even during the process of forming the gel film, a portion of the amic acid (approximately 0.1 mol % to 10 mol %) is imidized, and therefore the polyamic acid composition can be dried at a variable temperature in the range of 50°C to 200°C, which also falls within the category of the thermal imidization method.
[0053] In the case of the chemical imidization method, a polyimide film can be produced using a dehydrating agent and an imidization agent by methods known in the art.
[0054] As an example of the composite imidization method, a polyimide film can be produced by adding a dehydrating agent and an imidization agent to a polyamic acid solution, heating the solution at 80 to 200°C, preferably 100 to 180°C, partially curing and drying the solution, and then heating the solution at 200 to 400°C for 5 to 400 seconds.
[0055] The present invention provides a multilayer film comprising the above-mentioned polyimide film and a thermoplastic resin layer, and a flexible metal foil laminate comprising the above-mentioned polyimide film and an electrically conductive metal foil.
[0056] As the thermoplastic resin layer, for example, a thermoplastic polyimide resin layer can be used.
[0057] The metal foil used is not particularly limited, but when the flexible metal foil laminate of the present invention is used for electronic or electrical equipment, the metal foil may be, for example, copper or a copper alloy, stainless steel or an alloy thereof, nickel or a nickel alloy (including alloy 42), aluminum or an aluminum alloy.
[0058] In general flexible metal foil laminates, copper foils such as rolled copper foils and electrolytic copper foils are often used, and are also preferably usable in the present invention. In addition, the surface of these metal foils may be coated with an anti-rust layer, a heat-resistant layer, or an adhesive layer.
[0059] In the present invention, the thickness of the metal foil is not particularly limited, and may be any thickness that allows the metal foil to exhibit sufficient function depending on the application.
[0060] The flexible metal foil laminate according to the present invention may have a structure in which a metal foil is laminated on one side of the polyimide film, or an adhesive layer containing a thermoplastic polyimide is added to one side of the polyimide film, and the metal foil is laminated in a state of being attached to the adhesive layer.
[0061] The present invention further provides an electronic component including the flexible metal foil laminate as an electrical signal transmission circuit, the electrical signal transmission circuit being an electronic component that transmits signals at a high frequency of at least 2 GHz, particularly at least 5 GHz, and more particularly at least 10 GHz.
[0062] The electronic component may be, for example, but is not limited to, a communication circuit for a mobile terminal, a communication circuit for a computer, or a communication circuit for an aerospace application. EXAMPLES
[0063] The functions and effects of the present invention will be described in more detail below through specific examples of the present invention, however, these examples are merely presented as examples of the present invention and do not define the scope of the invention.
[0064] <Production Example> NMP was added to a 500 ml reactor equipped with a stirrer and nitrogen inlet / outlet tubes while injecting nitrogen, and the temperature of the reactor was set to 30°C. Then, paraphenylenediamine (PPD) and m-tolidine as diamine components, biphenyltetracarboxylic dianhydride (BPDA), pyromellitic dianhydride (PMDA), and p-phenylenebis(trimellitate anhydride) (TAHQ) as dianhydride components were added in a specified order, and the temperature was raised to 40°C under a nitrogen atmosphere, and the mixture was stirred for 120 minutes while being heated to produce a polyamic acid having a viscosity of 200,000 cP at 23°C.
[0065] The prepared polyamic acid was rotated at a high speed of 1,500 rpm or more to remove air bubbles. The degassed polyimide precursor composition was then applied to a glass substrate using a spin coater. The composition was then dried for 30 minutes at 120°C under a nitrogen atmosphere to prepare a gel film. The gel film was then heated to 450°C at a rate of 2°C / min, heat-treated at 450°C for 60 minutes, and cooled to 30°C at a rate of 2°C / min to obtain a polyimide film.
[0066] Then, the polyimide film was peeled off from the glass substrate by dipping in distilled water. The thickness of the polyimide film was 15 μm. The thickness of the polyimide film was measured using an Anritsu Electric Film Thickness Tester.
[0067] <Examples 1 to 7 and Comparative Examples 1 to 3> Polyimide films were produced according to the above-mentioned Production Example, except that the components and their contents were changed as shown in Table 1 below.
[0068] [Table 1]
[0069] <Experimental Example>Evaluation of dielectric loss factor and storage modulus The dielectric loss factor and storage modulus of each of the polyimide films produced in Examples 1 to 7 and Comparative Examples 1 to 3 were measured, and the results are shown in Table 2 below.
[0070] (1) Measurement of dielectric loss factor (Df) The dielectric loss factor (Df) was measured at 10 GHz using a Keysight network analyzer and a QWED SPDR resonator after drying the sample in an oven at 130°C for 30 minutes and leaving it in an environment at 23°C and 50% relative humidity for 24 hours.
[0071] (2) Measurement of storage modulus The storage modulus of each film was determined using DMA, and the value at 300°C was measured.
[0072] [Table 2]
[0073] As shown in Table 2, the polyimide films prepared according to the embodiments of the present invention not only exhibit a very low dielectric loss factor of 0.003 or less, but also have a desired storage modulus at high temperatures. Such results are achieved by the components and composition ratios specified in this application, and it is understood that the content of each component plays a decisive role.
[0074] In contrast, the polyimide films of Comparative Examples 1 to 3, which have components different from those of the Examples, exhibit significantly reduced storage modulus characteristics at high temperatures, making it difficult to use them in electronic components that transmit signals at high frequencies.
[0075] The present invention has been described above with reference to an embodiment thereof. However, a person having ordinary knowledge in the field to which the present invention pertains will be able to make various applications and modifications within the scope of the present invention based on the above content. [Industrial Applicability]
[0076] As described above, the present invention provides a polyamic acid and polyimide film having excellent high-temperature storage modulus and low dielectric properties, which are composed of specific components and a specific composition ratio, and is useful in various fields requiring such properties, particularly in electronic components such as flexible metal foil laminates.
Claims
1. dianhydride acid components including biphenyltetracarboxylic dianhydride (BPDA), pyromellitic dianhydride (PMDA) and p-phenylenebis(trimellitate anhydride) (TAHQ); and a diamine component including m-tolidine and paraphenylenediamine (PPD), Polyamic acid.
2. Based on 100 mol% of the total content of the dianhydride acid components, the content of the biphenyltetracarboxylic dianhydride is 15 mol% or more and 70 mol% or less, the content of the pyromellitic dianhydride is 10 mol% or more and 50 mol% or less, and the content of the p-phenylene bis(trimellitate anhydride) is 5 mol% or more and 75 mol% or less. The polyamic acid according to claim 1 .
3. the content of the m-tolidine is 20 mol % or more and 45 mol % or less, based on 100 mol % of the total content of the diamine components; The content of the paraphenylenediamine is 55 mol% or more and 80 mol% or less. The polyamic acid according to claim 1 .
4. The polyamic acid is a block copolymer containing two or more blocks. The polyamic acid according to claim 1 .
5. dianhydride acid components including biphenyltetracarboxylic dianhydride (BPDA), pyromellitic dianhydride (PMDA) and p-phenylenebis(trimellitate anhydride) (TAHQ); and a diamine component including m-tolidine and paraphenylenediamine (PPD), Polyimide film.
6. Based on 100 mol% of the total content of the dianhydride acid components, the content of the biphenyltetracarboxylic dianhydride is 15 mol% or more and 70 mol% or less, the content of the pyromellitic dianhydride is 10 mol% or more and 50 mol% or less, and the content of the p-phenylene bis(trimellitate anhydride) is 5 mol% or more and 75 mol% or less. The polyimide film according to claim 5 .
7. the content of the m-tolidine is 20 mol % or more and 45 mol % or less, based on 100 mol % of the total content of the diamine components; The content of the paraphenylenediamine is 55 mol% or more and 80 mol% or less. The polyimide film according to claim 5 .
8. The polyamic acid is a block copolymer containing two or more blocks. The polyimide film according to claim 5 .
9. The first block of the block copolymer has a biphenyltetracarboxylic dianhydride content of 100 moles per 100 moles of the total dianhydride acid content of the polyimide film. % or more and 60 mol % or less, based on the mol % of the content of the m-tolidine in the second block is 30 mol % or more and 40 mol % or less based on 100 mol % of the total content of diamine components in the polyimide film; The polyimide film according to claim 8.
10. The dielectric loss factor (Df) is 0.003 or less, The storage modulus measured at 300°C is 100 MPa or more. The polyimide film according to claim 5 .
11. A polyimide film according to any one of claims 5 to 10, and a thermoplastic resin layer. Multilayer film.
12. A polyimide film according to any one of claims 5 to 10, and an electrically conductive metal foil. Flexible metal foil laminate.
13. The flexible metal foil laminate of claim 12, Electronic components.
Citation Information
Patent Citations
Polyimide precursor resin composition, polyimide resin film, flexible printed wiring board, circuit-fitted suspension, and hard disc drive
JP2014208793A
Polyimide resin precursor
JP2017132898A
Polyimide film
JP2017179150A
Multilayer polyimide film
JP2021074894A