Improved CO2 hydrogenation catalysts for commercial production of syngas
A low-cost, high-efficiency catalyst using metal-aluminate spinels converts CO2 and H2 into syngas, addressing commercial viability issues by maintaining performance and selectivity for over 1,000 hours, enabling large-scale production of low-carbon fuels and chemicals.
Patent Information
- Application Number
- JP2024525087
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-16
- Filing Date
- 2022-11-04
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2042-11-04
AI Technical Summary
Current catalysts for converting mixtures of CO2 and H2 into syngas are not commercially viable due to high costs, unsuitable operating conditions, limited lifespan, and inefficiencies, making large-scale production of low-carbon fuels and chemicals challenging.
Development of a catalyst composed of low-cost metals, such as alkali and alkaline earth metals, transition metals, and rare earth metals, supported on alumina, which are impregnated and fired at high temperatures, forming metal-aluminate spinels, ensuring stability and efficiency up to 2,100°F, with conversion efficiencies of 80% to 100% and CO selectivity over 99%, without coking or significant degradation.
The catalyst achieves high conversion efficiency and selectivity, maintaining performance for over 1,000 hours with minimal reduction, suitable for large-scale industrial use in tubular or packed bed reactors, producing low-carbon syngas for fuels and chemicals.
Smart Images

Figure 2024543324000001_ABST
Abstract
Description
[Technical field]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS N / A
[0002] Federally Sponsored Research Statement N / A
[0003] Names of parties to the joint research agreement N / A
[0004] References to sequence listings, tables and computer programs N / A
[0005] 2. Background of the Invention The impact of ever-increasing CO2 levels on climate change caused by anthropogenic activities has been widely documented (Shukla et al., IPCC, 2019). Between 1970 and the end of 2019, increases in the greenhouse gases CO2, CH4, N2O, and H2O have increased the Earth's radiative forcing by an average of 3.03 watts per square meter (W / m 2 ) and at the same time the global average temperature increased by 1.18 °C (2.13 °F). Climate models predict that the global average temperature could reach +2.00 °C (+3.60 °F) in 2026-2028 and +2.36 °C (+4.28 °F) by the end of 2031 compared to the global average temperature in 1970. Two-thirds of these increases are due to CO2, so a rapid reduction in CO2 emissions and atmospheric CO2 is required by 2030 at the latest (Schuetzle, 2020).
[0006] CO2 can be efficiently captured from flue gases produced by industrial processes. Because CO2 is a useful carbon source, the highest priority should be to utilize this carbon source for the production of low-carbon fuels and chemicals, rather than sequestering it in geological formations (Hepburn et al., 2019). CO2 can also be captured from the air (called Direct Air Capture-DAC), which allows the capture of CO2 from any location in the world, without being tied to an industrial source (Artz et al., 2018).
[0007] Few suitable geological formations exist for the sequestration of captured CO2, making it much more feasible to produce fuels and chemicals from CO2, which is also a valuable feedstock that can be used to produce low-carbon fuels and chemicals.
[0008] Syngas can potentially be commercially produced from the catalytic conversion of a mixture of low-carbon H2 and captured CO2. This catalytic process is called CO2 hydrogenation, or the reverse water gas shift (RWGS) reaction (Equation 1) (Daza et al., 2016; Vogt et al., 2019; Chen et al., 2020). CO2+ H2= CO + H2O Equation 1
[0009] The reaction is endothermic and requires heat to proceed: high temperatures and efficient catalysts are required to convert CO2 to CO on a large scale with minimal or no coking (carbon formation) or catalyst degradation over time.
[0010] To date, a commercially viable catalyst has not yet been developed for the efficient production of syngas from a mixture of H and CO; therefore, improved catalysts and processes have been developed and are described herein below for the efficient and commercial production of low-carbon syngas from a mixture of low-carbon H and captured CO.
[0011] This low-carbon syngas is an excellent feedstock for producing a wide range of other chemical products, including liquid and gaseous hydrocarbon fuels, alcohols, acetic acid, dimethyl ether, and many other chemicals (Olah et al., 2009; Centi et al., 2009; Jianget et al., 2010; Schuetzle et al., 2010-2020; Fischer et al., 2016; Gumber et al., 2018; Tan et al., 2018; Li et al., 2019; NAS, 2019).
[0012] A number of patent applications, patents, and publications have described the development of RWGS catalysts for the conversion of H2 and CO2 mixtures to syngas (Bahmanpour et al., 2021). The next emerging approach involves an electrolysis process for the conversion of CO2 and H2O mixtures to syngas (Wang et al., 2016). However, this electrolysis approach is in the early research and development stages and is not currently considered a viable commercial-scale process.
[0013] Most of these RWGS catalysts described in the current art either operate at conditions that are not suitable for industrially relevant process conditions or have significant limitations such as high cost, incompatibility with large scale production or limited operational life. Therefore, the present inventors have developed a catalyst of the present invention that is commercially viable and meets the following specifications as outlined in Table 1:
[0014] Table 1 - Quality and performance specifications for efficient catalytic conversion of H2 / CO2 mixtures to synthesis gas 1. The catalyst is made by impregnating a base material that does not chemically react with metals with one or more low-cost metals selected from alkali metals (Group 1), alkaline earth metals (Group 2), transition metals, and rare earth metals, and then calcining the impregnated base material. The catalyst does not contain precious metals. 2. One or more metals are formulated as metal salts (eg, nitrates, acetates, carbonates, etc.) or metal hydroxides, and impregnated onto a chemically inert substrate at a concentration of 0.0 to about 35% by weight. 3. The inert substrate is one or more metal-alumina spinels produced by calcining a stoichiometric mixture of alumina and one of the following metals: Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce, at temperatures up to 2,100°F. 4. The catalyst contains low cost components without any precious metals including Rh, Pt, Au, Ag, Pd or Ir. 5. The catalyst is robust. By robust, we mean a hardness of between 3 Mohs and 10 Mohs, and more preferably between 4 Mohs and 7 Mohs (or equivalent on the Rockwell scale). 6. The catalyst is chemically and physically stable at temperatures up to 2,100° F. By chemically and physically stable, it is meant that the surface area of the catalyst as measured by the Brunauer-Emmet-Teller (BET) method is essentially the same before and after heat treatment, and is considered stable when there is a 0-20% change in the measurement, preferably a 0-10% change, and more preferably a 0-5% change. 7. The catalyst can be easily loaded into the catalytic reactor (e.g., tubular reactor or packed bed reactor). The pressure drop from the top to the bottom of the catalytic reactor is preferably 0-50 psi, more preferably 0-25 psi, and more preferably 0-10 psi. 8. It is recommended that the catalyst activation can be carried out in situ in the reactor. It is recommended that the activation gas for the catalyst activation process is readily available. Preferably, the catalyst activation can be achieved by using a gas comprising hydrogen. More preferably, the catalyst activation can be achieved by using a gas comprising hydrogen and carbon dioxide. 9. The conversion efficiency from CO2 to CO is 2,000hr -1 ~1,000,000hr -1 At this space velocity, the ratio is 70% to 100%, and preferably 75% to 100%. 10. The conversion of CO2 to CO occurs at temperatures between 1,300°F and 1,800°F and pressures above 50 psi. 11. The catalyst does not coke (e.g., form carbon deposits), where non-coking means that the percent carbon measured on the catalyst during the conversion of carbon dioxide to carbon monoxide is 0-1 wt.%, more preferably 0-0.1 wt.%. 12. During testing under the proposed commercial operating conditions, the catalyst meets performance criteria such that the degradation of CO2 conversion is 0-1% per 1000 hours of operation, more preferably 0-0.5% per 1000 hours of operation.
[0015] FIELD OF THEINVENTION The field of the invention is the application of improved catalysts for the conversion of renewable H2 and captured CO2 to syngas, which is then used simultaneously to produce low carbon fuels and chemicals. The improved catalysts use low cost metals, can be commercially and economically mass produced, and are chemically and physically stable at temperatures up to 2,100°F. CO2 conversion efficiencies are 80%-100% with CO selectivity greater than 99%. The catalysts operate at 1,300-1,800°F, 75-450 psi, and space velocities of 2,000-100,000hr with H2:CO2 mixtures. -1 The catalyst is robust and the CO2 conversion loss is 0-1.0% per 1000 hours. [Background technology]
[0016] 2. Description of Related Art Iwanani et al. (1995) developed catalysts consisting of transition metals with precious metals (e.g., Ni, Fe, Ru, Rh, Pt, W, Pd, Mo) on ZnO / Al2O3 substrates for the conversion of mixtures of CO2 and H2 to CO, specifically targeting catalytic performance in H2S-containing sources. They demonstrated that a 12.4% Ni / 21.2% Zn catalyst could be run for 3,000 hours at 1,100°F without significant loss of catalytic activity after 150 hours. -1A relatively low CO2 conversion of up to 37% was achieved at 1000 sintering, but no longer term tests were performed. This catalyst does not meet any of the specifications in Table 1.
[0017] Dupont et al (2003) developed a catalyst consisting of 0.78% ZnO / 0.21% Cr2O3 / 0.01% NiO for the conversion of H2 / CO2 (3.5 / 1.0 v / v) mixture to CO. At 4950°F, 580 psi pressure, 5.0 hr -1 The CO2 conversion efficiency at this space velocity was 36%, with selectivities of 92% CO and 48% CH. No data was presented on the efficiency of the catalyst over time. This catalyst does not meet all of the criteria outlined in Table 1.
[0018] Kim et al. (2014) reported that BaZr 0.8 Y 0.16 Zinc 0.04 The CO2 hydrogenation efficiency of the O3 perovskite catalyst was measured at 1,110°F and 15 psi with a 1 / 1 H2 / CO2 blend. They achieved a low CO2 conversion of 38% with a CO selectivity of 97%. The catalyst was only run for 5 hours, so the long-term catalyst durability was not measured.
[0019] Chen et al. (2015) reported that a nano-intermetallic catalyst (InNi3Co) exhibited activity and selectivity for the RWGS reaction. 0.5 The catalyst was prepared by carburizing an In-Ni intermetallic compound, which resulted in the formation of dual active sites on the catalyst surface. The catalyst was successfully synthesized at 1125°F and a gas flow rate of 30,000 hr. -1A CO2 conversion of 52-53% was achieved over 150 hours under these conditions. The catalyst can meet criteria #3 and #7 due to its structure. The catalyst is difficult and expensive to manufacture in multi-ton quantities (criteria #1 and #2) and it is unclear whether it can be used commercially in conventional catalytic reactors (criteria #5 and #6). The catalyst does not meet the efficiency requirements for CO2 to CO conversion (criterion #8) and selectivity for CO production. The catalyst was only tested for 150 hours, so its stability and lifetime are unknown.
[0020] Daza and Kuhn (2016) developed a La / Sr (3.0 / 1.0 w / w) catalyst impregnated on an FeO3 substrate. They observed 16% conversion of H2 / CO2 (1.0 / 1.0 v / v) to CO at 1,300°F and 15 psi with a selectivity of 95%. The conversion to CO2 and CO selectivity remained relatively constant over the course of the 150-hour test. This catalyst meets criteria #1, #7, and #9 shown in Table 1. The catalyst was only operated for 150 hours, so its long-term life is unknown.
[0021] Daza et al. (2016) 0.75 Sr 0.25 The CO2 hydrogenation efficiency of FeO3 perovskite catalyst was measured at 1,020°F and 15 psi with a 1 / 1 H2 / CO2 (v / v) blend. They achieved a very low CO2 conversion of 15%, with a CO selectivity of 95%. The catalyst run time was less than 24 hours, so long-term catalyst durability was not measured. In summary, there is no published data to date that indicates that perovskites can be acceptable catalysts for CO2 hydrogenation.
[0022] Alumina has been widely studied as a catalyst support for both CO hydrogenation (2) and dry reforming of methane (DRM). The advantages of alumina are mainly due to its large surface area, low cost, and stability at high temperatures. It is also relatively inexpensive compared to other support materials. Yang et al. (2018) synthesized a 10% Ni / 20% CeO2 catalyst on γ-Al2O3. They tested this catalyst with a 4 / 1 H2 / CO2 (v / v) blend at 1,300°F, 15 psi, and a space velocity of 400 k hr. -1 They observed 67% CO2 conversion, 90% CO selectivity, and 10% CH4 selectivity. The catalyst efficiency decreased by 37% after 50 hours due to carbon formation and Ni sintering. Therefore, this is not a commercially viable catalyst.
[0023] Although Ni catalysts on Al2O3 substrates have potential as RWGS catalysts, they are prone to the formation of spinel nickel aluminate NiAl2O4, which may result in at least some loss of activity (Ryu et al., 2021). However, the resistance of Ni / Al2O3 to coke formation is highly dependent on the structure and composition of the catalyst. At high temperatures, the resistance to coke formation is improved as a result of the formation of the spinel phase NiAl2O4. This is a result of the strengthening of the Ni-O bonds of NiAl2O4 to the NiO crystals, which in turn strengthens the Ni2 + This makes it difficult to reduce nickel to elemental nickel (Hu et al, 2004).
[0024] Magnesia is a promising support due to its enhanced chemisorption of CO2 and high basicity. The advantages of magnesia and alumina can be combined in MgO-Al2O3 mixed support. The improvement of basicity and the effect of specific surface area have been reported by Jun et al., who used catalysts for dry reforming of methane (Jun et al., 2015). The effect of Mg / Al on catalytic activity and catalyst life remains to be elucidated. Also, none of the reported catalysts fully meets the requirements mentioned in Table 1.
[0025] Depending on the reaction conditions and preparation method of the catalyst, any mixed MgO-Al2O3 system doped with nickel will form spinels from each component. Based on a systematic study of varying nickel content in NiMgx1-xAl2O4, Park et al. (2021) reported that RWGS conversion was favored at higher magnesium atomic ratios. This result was supported by DFT calculations, which showed that CO selectivity increased with increasing magnesium content. Zhang et al. (2021) described a 0.43% Ni on MgAl2O4 catalyst for CO2 hydrogenation of a 1 / 1H2 / CO2 blend at 1,472°F. They reported a CO2 conversion efficiency of 46% after 75 hours, with no significant decrease in conversion efficiency. However, this efficiency does not meet the 70% to 100% CO2 conversion efficiency at 1,300°F and above 50 psi, as outlined in Table 1. The selectivity for CO production was not reported and the long-term catalyst deactivation is unknown.
[0026] The preparation of mixed Ni-Mg-Al-O phases has also been reported for dry reforming of methane (DRM) where hydrotalcite-like mixed layered hydroxides were pyrolyzed to show high activity and improved stability (Bhattacharyya et al.). Bhattacharyya et al. also compared the catalytic activity with a commercial NiO supported catalyst. Hydrotalcite is a naturally occurring layered mineral discovered in Sweden in 1842 and has the chemical formula Mg6Al2(OH). 16Hydrotalcite has the formula CO3-4H2O, and its name is derived from the material's high water content and resemblance to talc. Hydrotalcite can be easily synthesized by coprecipitation (Cavani et al, 1991). Many minerals with different molecular compositions but similar empirical elemental structures have been reported. The term hydrotalcite (hydrotalcite-like compounds - HT, layered double hydroxides - LDH) is used to describe a large group of natural minerals and synthetic materials that have the typical layered structure of hydrotalcite. The general formula of hydrotalcite can be summarized as follows: [M 2+ 1-x M 3+ x (OH)2][(A n- x / n )·mH2O] where M 2+ ,M 3+ are divalent and trivalent cations, A is the interlayer anion, and x is the mole fraction of trivalent cations. [M 2+ 1-x M 3+ x (OH)2][M 2+ 1-x M 3+ x The (OH)2] part represents the composition of the brookite-like layer, and the [(A n- x / n )·mH2O] represents the composition of the interlayer space.
[0027] In the synthesis of DRM catalysts, nickel has been introduced by various methods, including wet impregnation, ion exchange, and co-precipitation. Nickel-based hydrotalcite-based catalysts have been considered and well studied for DRM.
[0028] Ni-hydrotalcite catalysts with low nickel content show high activity for CO2 conversion, suggesting the simultaneous occurrence of reverse water gas shift (RWGS) (Lin et al., 2021). Based on the cation exchange capacity of the brookite layer, the anion exchange capacity of the interlayer, the surface tunable basicity, and the adsorption capacity, numerous heterogeneous catalysts have been developed (Debek et al., 2017; US8388987B2, 2013). Hydrotalcites are also used in the production and processing of polymers, as a neutralizing additive, or as part of building materials (Figueras et al., 2010; Sikander et al., 2017). However, to the best of our knowledge, there have been no reports of the application of hydrotalcite in commercial RWGS catalysts, with or without additional metal active sites, such as Ni.
[0029] Hydrotalcite-based materials have also been reported as potential solid adsorbents for pressure swing CO2 adsorption, a technique known as adsorption-enhanced water gas shift (SEWGS). Hydrotalcite has shown high thermal and mechanical stability, and has demonstrated sufficiently high cycle capacity and fast adsorption kinetics. The regeneration step (desorption of CO2 by feeding water vapor to the adsorbent) is slow, limiting the cycle capacity of the adsorbent. Higher operating temperatures have been found to be advantageous as they enhance the desorption kinetics. Steam induces the desorption of available second adsorption sites for CO2 that are not desorbable by N2 (Boon et al, 2014). Calcination of hydrotalcite leads to dehydration, dihydroxylation, and decarbonation, ultimately resulting in the formation of spinel. While the formation of the spinel phase from alumina and magnesia precursors occurs at temperatures above 1500 °C, the spinel phase is formed at significantly lower temperatures during calcination of hydrotalcite. When hydrotalcite precursors are applied in the synthesis of commercial RWGS catalysts, the spinel phase is formed at temperatures as low as 700 °C (Jatav et al., 2016).
[0030] Bahmanpour et al. (2019) studied in situ formed Cu-Al spinel as an active substrate for CO2 hydrogenation with H2 to produce syngas. They formed Cu-Al spinel with excess Cu at different weight ratios by using coprecipitation and subsequent hydrogen treatment. A 4% Cu catalyst on Cu-Al spinel was found to be the most efficient in CO2 conversion. A low CO2 conversion of 47% at 1,110°F was achieved at relatively high space velocity with no detectable deactivation after 40 hours of testing. In contrast, 4% Cu on gamma alumina converted 33% CO2 at 1,110°F. This catalyst meets criterion #1 and could meet criteria #2, #3, #5, #6, and #7. However, copper-containing catalysts tend to deactivate over time by sintering at high temperatures, which is especially problematic in Cu-rich formulations. Furthermore, the catalyst formulations must be tested for 1,000 hours or more to assess long-term life (Criterion #10).
[0031] Table 2 summarizes the catalytic systems mentioned above and other potential catalysts for catalytic CO2 hydrogenation to CO. Most of these catalysts have only been tested for less than 48 hours, which is not long enough to evaluate the durability of the catalyst. Commercial catalysts are expected to have a lifespan of at least 2 years, so the degradation of CO2 conversion should be between 0% and 1.0% per 1000 hours.
[0032] These catalysts are required to operate efficiently at pressures of 50 psi or more, preferably 150 psi or more, in order to operate in commercial reactors. The catalysts listed in Table 2 are all evaluated at 15 psi, except for Dupont et al., 2003, Kharaji et al., 2012, and Chen et al., 2019, which tested the catalysts at 300, 150, and 145 psi, respectively.
[0033] [Table 2-1] [Table 2-2] [Table 2-3] Summary of the Invention
[0034] The present invention relates generally to the production of low carbon syngas from captured CO2 and renewable H2. The H2 is produced from water using a renewable electricity powered electrolyser or from other methods in low carbon H2 production. The improved catalyst uses low cost metals, can be commercially economically mass produced, and is chemically and physically stable at temperatures up to 2,100°F. CO2 conversion efficiencies are 80%-100% with CO selectivity greater than 99%. The catalyst is optimized for use with H2:CO2 mixtures at temperatures between 1,300-1,800°F, pressures between 75-450 psi, and space velocities between 2,000-100,000 hr -1The conversion to syngas occurs without sintering or coke formation over the entire operating range. The catalyst is stable with a CO2 conversion loss of 0-1.0% per 1000 hours. This syngas can be used to synthesize low carbon fuels and chemicals or to produce purified H2. The H2 can be used for low carbon chemical synthesis at the production site or compressed for transport. [Brief description of the drawings]
[0035] [Figure 1] FIG. 1 shows a typical relationship between the conversion of CO2 to CO and temperature using the improved catalyst of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0036] This section describes improved catalyst formulations that have been demonstrated to meet the performance and quality requirements shown in Table 1.
[0037] In these embodiments, four improved CO2 hydrogenation or reverse water gas shift (RWGS) catalysts are described.
[0038] Type A. Metal-spinel catalysts -Pure alumina is an amphoteric material and can react with both acids and bases. Depending on the form and crystal structure present, the basicity of alumina can be complex. Acidic aluminas catalyze reactions that are typically catalyzed by acids (Pines et al, 1960). However, some spinels produced from high temperature calcination of alumina with group 1 metals (Li, Cs, Rb) and group 2 metals (Mg, Ca, Sr, Ba, Be) form metal aluminates with defined, usually basic, surface properties due to the high surface concentration of hydroxyl (-OH) groups.
[0039] When the H2 / CO2 mixture reacts with these hydroxy groups according to Equation 2, formate salts are formed. H2+CO2=HCOO-metal aluminate+H2O (Eq. 2)
[0040] These formates decompose rapidly at high temperatures in the presence of H2 to form CO (Equation 3) with high selectivity. Thus, some of these spinels are excellent CO2 hydrogenation catalysts. 2HCOO-metal aluminate+H2=2CO+2H2O (Formula 3)
[0041] The spinels of the present invention are any class of minerals or synthetically produced minerals having the general chemical form AB2X4. In the present invention, X is oxygen and B may be selected from the group including aluminum, iron, chromium, cobalt and vanadium. A is selected from the group including Mg, Zn, Fe, Mn, Cu, Ni, Li, Cs, Rb, Mg, Ca, Sr, Ba, Be and Ti. In one embodiment of the present invention, the catalyst is a metal aluminate where B is aluminum and X is oxygen.
[0042] Type B. Metal-impregnated metal-spinel catalysts- Selected Group 1 (alkali metals such as Li, Cs, Rb, etc.) and / or Group 2 (alkaline earth metals such as Mg, Ca, Sr, Ba, Be, etc.) elements, when impregnated at appropriate levels on selected spinels, increase the surface abundance of hydroxyl groups, thereby improving their CO2 hydrogenation efficiency. The addition of these elements is believed to promote CO2 chemisorption due to their effect on basicity, total pore volume and surface area. The dopants can be Ni, Cu, Ce, Zr, Ti, La or early numbered lanthanide elements. When two or more impregnated metals on metal aluminate spinels are calcined at temperatures up to 2,100°F, a solid solution is formed. This solid solution represents an excellent catalyst for CO2 hydrogenation. Since Ni and Mg both crystallize in a face-centered cubic structure and have similar electronegativity and valence, Ni and Mg form a solid solution Ni2Mg on Mg-aluminates at 2,050°F. Ni also forms a solid solution with Cu (NiCu3) at 2,050° F. because both Ni and Cu crystallize in a face-centered cubic structure and have similar atomic radii, electronegativities, and valences. A solid solution is formed when two of the metals impregnated onto a metal aluminate spinel have similar crystal structures, atomic radii, electronegativities, and valences. The dopant may be present as an additional framework and not incorporated into the spinel, may be supported on the metal-spinel catalyst, may both be supported on the spinel, especially at high concentrations, or may be present adjacent to each other in a physical mixture.
[0043] RWGS catalysts are operated in the temperature range of 1,300-1,800°F to achieve CO2 conversion efficiency greater than 70%, where the sintering rate is high as many materials approach their melting point. It is recommended that the solid solutions used in the catalysts are solid at these temperatures. Thus, viable solid solutions are those formed in the range of 1,850-2,100°F. Ni2Mg and NiCu3 are stable solids at the operating temperatures of these catalysts and have excellent performance as CO2 hydrogenation catalysts. The solid solution Cu2Mg is formed from 2 moles of Cu and 1 mole of Mg at 1,300°F, but is liquid at the operating temperature of the catalyst, making it an unsuitable candidate.
[0044] Type C. Engineered layered solids -Hydrotalcite-based materials are used as catalysts for RWGS. These materials include natural hydrotalcites as well as highly engineered synthetic anionic clays or layered double hydroxides (LDHs). Natural hydrotalcites can be used as additives or as precursors for further synthesis. Synthetic hydrotalcites are commercially available or can be prepared by co-precipitation methods.
[0045] Hydrotalcite is a layered double hydroxide (LDH)-Mg6Al2CO3(OH) 16 ·4H2O. Several structures exist containing loosely bound carbonate ions, which are known for their ion exchange and CO2 adsorption capabilities. Upon calcination, the material decomposes to a high surface area spinel that can be easily rehydrogenated or recarboxylated. Complete pyrolysis results in a spinel known for its hardness and durability.
[0046] LDH has a brookite (Mg(OH)2) structure, 2 + Ion M 3+ They are structurally derived by isomorphous substitution with ions. The LDH layers are positively charged, and charge neutrality is achieved by the presence of anions between the lamellae. M 3+ Al 3+When LHDs are combined with hydrotalcite, the mineral hydrotalcite is obtained. The uniquely large surface area of LHDs and their surface basicity significantly enhance the performance of RWGS. The surface area, chemical composition and basicity of the layered solids have been designed to optimize the performance of commercial RWGS catalysts.
[0047] Type D. Perovskite Catalyst - Similar to type A materials, perovskite materials can also be used as improved RWGS catalysts. Perovskite materials have the general chemical form ABX3. In the present invention, X is oxygen. A and B are cations. The perovskite material can be selected from simple perovskites, where A is selected from the group including Sr, Ca, Ba, Mg, Fe, La, Ca, Pb, or Bi, and B is selected from the group including Al, Ti, Rb, Si, Fe, Yb, or Mn. In addition, solid solution perovskite materials such as lanthanum strontium manganite, lanthanum aluminate-strontium aluminum tantalate (LSAT), lead scandium tantalate, or lead zirconate tantalate can also be used. These catalysts include perovskites or mixtures of various perovskites.
[0048] In the following embodiments describing preferred catalyst compositions and catalytic performance, certain specific details are provided to provide a thorough understanding of various embodiments. Unless the context requires otherwise, throughout this specification and the following claims, the term "comprises" and variations thereof are to be interpreted in an open and inclusive sense, i.e., "including but not limited to."
[0049] Catalyst Composition Embodiments 1. A reverse water gas shift (RWGS) catalyst for converting a mixture of H2 and CO2 to synthesis gas, the conversion comprising the process steps of: a) introducing a mixture of H2 and CO2, or b) a mixture of H2, CO2 and light hydrocarbons into a catalytic reactor of a catalytic conversion system, thereby producing synthesis gas or carbon monoxide; A reverse water gas shift (RWGS) catalyst for further reacting the product of the catalytic reactor, thereby producing at least one product selected from the list consisting of liquid fuels, methanol, propane, naphtha, and chemicals.
[0050] 2. The reverse water gas shift (RWGS) catalyst of embodiment 1, comprising: a) 10 m 2 / g~1000m 2 / g of surface area, said metal spinel being a. Group 2 metals which are calcined with alumina, thereby forming Mg-aluminate, Ca-aluminate, Sr-aluminate, Ba-aluminate and Be-aluminate. b. Group 1 metals calcined with alumina, thereby forming Li-aluminate, Rb-aluminate and Cs-aluminate. c. Transition metals which are calcined with alumina, thereby forming Fe-aluminate, Co-aluminate, Ni-aluminate, Cu-aluminate, Zn-aluminate. d. Rare earth metals calcined with alumina, thereby forming La-aluminate, Ce-aluminate. e. The above metal spinels may be present individually or as mixed oxides in part or in whole. A reverse water gas shift (RWGS) catalyst (Type A) comprising a metal aluminate spinel selected from the group consisting of:
[0051] 3. A reverse water gas shift (RWGS) catalyst employing one of the metal-alumina spinels described in embodiment 2, impregnated with a metal dopant, such as, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce (Type B). The metal dopant may not be chemically bonded to the spinel. In some embodiments, only one of the above elements may be added, while in other embodiments, the catalyst formulation may include a complex mixture of more than one of the above elements.
[0052] Metal dopants may be introduced by impregnation, or in some cases, by physically mixing a solid precursor with the spinel. The amount of metal precursor may range from 0-35% by weight of the metal salt (e.g., nitrate, acetate, carbonate, etc.), metal hydroxide, or metal oxide. The formed material is then calcined at temperatures up to 2,100° F., thereby forming a 5 mm spinel. 2 / g~1000m 2 A catalyst is synthesized which is a metal-alumina spinel impregnated with metal having a surface area of 1 / g.
[0053] 4. The reverse water gas shift (RWGS) catalyst (Type C) of embodiment 1 containing an artificial layered solid, which may represent 100% of the solid catalyst without additional additives. The reverse water gas shift (RWGS) catalyst (Type C) employs the use of an artificial layered solid impregnated with a metal dopant, such as, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce. The metal precursor may be a metal salt (e.g., nitrate, acetate, carbonate, etc.), metal hydroxide, or metal oxide. The artificial layered solid may embody 0-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation, or 80-90% of the catalyst formulation. The remaining portion of the formulation may be dopants or other additives necessary to form a commercial catalyst. The metal dopant may not be chemically bonded to the artificial layered solid. In some embodiments, only one of the above elements may be added, while in other embodiments, the catalyst formulation may include a complex mixture of more than one of the above elements.
[0054] Metal dopants may be introduced by impregnation, or in some cases, by physically mixing the solid precursor with the artificial layered solid. The formed material is then calcined at temperatures up to 2,100° F. This reverse water gas shift (RWGS) catalyst (Type C) employs the use of naturally occurring layered solids impregnated with metal dopants, including but not limited to Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce. The metal precursors may be metal salts (e.g., nitrates, acetates, carbonates, etc.), metal hydroxides, or metal oxides. The naturally occurring layered solids may represent 0-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation, or 80-90% of the catalyst formulation. The remaining portion of the formulation may be dopants or other additives required to form a commercial catalyst. The metal dopants may not be chemically bound to the artificial layered solid. In some embodiments, only one of the above elements may be added, while in other embodiments, the catalyst formulation may include a complex mixture of more than one of the above elements. The metal dopants may be introduced by impregnation, or in some cases, by physically mixing a solid precursor with the artificial layered solid. The formed material is then calcined at a temperature of up to 2,100°F.
[0055] 5. The reverse water gas shift (RWGS) catalyst of embodiment 3, wherein the catalyst comprises the following components: a) 10 m 2 / g~1000m 2 % Mg salt. 2 / g~1000m 2 The Mg-alumina spinel according to embodiment 2, having a surface area of 5m / g, wherein the Mg-alumina spinel is mixed with up to 35% by weight of CaCO3, MgCO3, SrCO3, CaO, MgO or SrO.2 / g~1000m 2 d) 10m Mg-alumina spinel according to embodiment 2, having a surface area of 10m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce. 2 / g~1000m 2 A Ca-alumina spinel according to embodiment 2 having a surface area of at least 10 m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce; and 2 / g. e) 10m 2 / g~1000m 2 The Mg-alumina spinel according to embodiment 2, having a surface area of 1 / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher order mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce, and natural or artificial layered solids comprising 5-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation. The resulting formulation is calcined at a temperature of up to 2,100°F, resulting in a 5m 2 / g~1000m 2 A metal-impregnated Mg-alumina spinel with a surface area of 1 / g is obtained.
[0056] 6. The reverse water gas shift (RWGS) catalyst of embodiment 3, wherein the catalyst comprises the following components: a) 10 m 2 / g~1000m 2 % Ca salt.2 / g~1000m 2 Ca-alumina spinel according to embodiment 2, having a surface area of 5m / g, mixed with up to 35% by weight of CaCO3, MgCO3, SrCO3, CaO, MgO or SrO. 2 / g~1000m 2 d) 10m Ca-alumina spinel according to embodiment 2, having a surface area of 10m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce. 2 / g~1000m 2 A Ca-alumina spinel according to embodiment 2 having a surface area of at least 10 m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce; and 2 / g. e) 10m 2 / g~1000m 2 The Ca-alumina spinel according to embodiment 2, having a surface area of 1 / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher order mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce, and natural or artificial layered solids comprising 5-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation. The resulting formulation is calcined at a temperature of up to 2,100°F, resulting in a 5m 2 / g~1000m 2 A metal-impregnated Ca-alumina spinel with a surface area of 1000 nm / g is obtained.
[0057] 7. The reverse water gas shift (RWGS) catalyst of embodiment 3, wherein the catalyst comprises the following components: a) 10 m 2 / g~1000m 2 %. 2 / g~1000m 2 The Sr-alumina spinel according to embodiment 2, having a surface area of 10 m / g, wherein the Sr-alumina spinel is mixed with up to 35 wt. % of CaCO3, MgCO3, SrCO3, CaO, MgO or SrO. 2 / g~1000m 2 d) 10m Sr-alumina spinel according to embodiment 2, having a surface area of 10m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce. 2 / g~1000m 2 3. The Sr-alumina spinel of embodiment 2 having a surface area of at least 10 m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce; 2 / g. e) 10m 2 / g~1000m 2The Sr-alumina spinel according to embodiment 2, having a surface area of 1 / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher order mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce, and natural or artificial layered solids comprising 5-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation. The resulting formulation is calcined at a temperature of up to 2,100°F, resulting in a 5m 2 / g~1000m 2 A metal-impregnated Sr-alumina spinel with a surface area of 1.0 μm / g is obtained.
[0058] 8. The reverse water gas shift (RWGS) catalyst of embodiment 3, wherein the catalyst comprises the following components: a) 10 m 2 / g~1000m 2 %. A Mg-alumina spinel according to embodiment 2, having a surface area of 10 m / g, impregnated with up to 35 wt. % of a Ba salt. 2 / g~1000m 2 A Ba-alumina spinel according to embodiment 2 having a surface area of 10 m / g, the Ba-alumina spinel being mixed with up to 35 wt.% of CaCO3, MgCO3, SrCO3, CaO, MgO or SrO. 2 / g~1000m 2 d) 10m / g of Ba-alumina spinel according to embodiment 2, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce. 2 / g~1000m 23. A Ba-alumina spinel according to embodiment 2, having a surface area of at least 10 m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce; 2 / g. e) 10m 2 / g~1000m 2 The Ba-alumina spinel according to embodiment 2, having a surface area of 1 / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher order mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce, and natural or artificial layered solids comprising 5-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation. The resulting formulation is calcined at a temperature of up to 2,100°F, resulting in a 5m 2 / g~1000m 2 A metal-impregnated Ba-alumina spinel with a surface area of 1000 nm / g is obtained.
[0059] 9. The reverse water gas shift (RWGS) catalyst of embodiment 3, wherein the catalyst comprises the following components: a) 10 m 2 / g~1000m 2 %. A Mg-alumina spinel according to embodiment 2, having a surface area of 10 m / g, impregnated with up to 35 wt. % of a Li salt. 2 / g~1000m 2 The Li-alumina spinel according to embodiment 2, having a surface area of 10 m / g, wherein the Li-alumina spinel is mixed with up to 35 wt.% of CaCO3, MgCO3, SrCO3, CaO, MgO or SrO. 2 / g~1000m 2d) 10m Li-alumina spinel according to embodiment 2, having a surface area of 10m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce. 2 / g~1000m 2 3. The Li-alumina spinel of embodiment 2 having a surface area of at least 10 m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce; 2 / g. e) 10m 2 / g~1000m 2 The Li-alumina spinel according to embodiment 2, having a surface area of 1 / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher order mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce, and natural or artificial layered solids comprising 5-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation. The resulting formulation is calcined at a temperature of up to 2,100°F, resulting in a 5m 2 / g~1000m 2 A metal-impregnated Li-alumina spinel with a surface area of 1000 nm / g is obtained.
[0060] 10. The reverse water gas shift (RWGS) catalyst of embodiment 3, wherein the catalyst comprises the following components: a) 10 m 2 / g~1000m 2 %. The Mg-alumina spinel according to embodiment 2, having a surface area of 10 m / g, impregnated with up to 35 wt. % of a Rb salt. 2 / g~1000m 2The Rb-alumina spinel according to embodiment 2, having a surface area of 10 m / g, wherein the Rb-alumina spinel is mixed with up to 35 wt.% of CaCO3, MgCO3, SrCO3, CaO, MgO or SrO. 2 / g~1000m 2 d) 10m Rb-alumina spinel according to embodiment 2, having a surface area of 10m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce. 2 / g~1000m 2 3. The Rb-alumina spinel of embodiment 2 having a surface area of at least 10 m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce; 2 / g. e) 10m 2 / g~1000m 2 The Rb-alumina spinel according to embodiment 2, having a surface area of 1 / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher order mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce, and natural or artificial layered solids comprising 5-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation. The resulting formulation is calcined at a temperature of up to 2,100°F, resulting in a 5m 2 / g~1000m 2 A metal-impregnated Rb-alumina spinel having a surface area of 1000 nm / g is obtained.
[0061] 11. The reverse water gas shift (RWGS) catalyst of embodiment 3, wherein the catalyst comprises the following components: a) 10 m2 / g~1000m 2 %. A Mg-alumina spinel according to embodiment 2, having a surface area of 10 m / g, impregnated with up to 35 wt. % of a Cs salt. 2 / g~1000m 2 A Cs-alumina spinel according to embodiment 2 having a surface area of 10 m / g, the Cs-alumina spinel being mixed with up to 35 wt.% of CaCO3, MgCO3, SrCO3, CaO, MgO or SrO. 2 / g~1000m 2 d) 10m / g of Ni-alumina spinel according to embodiment 2, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce. 2 / g~1000m 2 3. A Cs-alumina spinel according to embodiment 2, having a surface area of at least 10 m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce; 2 / g. e) 10m 2 / g~1000m 2 The Cs-alumina spinel according to embodiment 2, having a surface area of 1 / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher order mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce, and natural or artificial layered solids comprising 5-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation. The resulting formulation is calcined at a temperature of up to 2,100°F, resulting in a 5m 2 / g~1000m 2A metal-impregnated Cs-alumina spinel with a surface area of 1000 nm / g is obtained.
[0062] 12. The reverse water gas shift (RWGS) catalyst of embodiment 3, wherein the catalyst comprises the following components: a) 10 m 2 / g~1000m 2 % Fe salt. 2 / g~1000m 2 The Fe-alumina spinel according to embodiment 2, having a surface area of 10 m / g, wherein the Fe-alumina spinel is mixed with up to 35 wt.% of CaCO3, MgCO3, SrCO3, CaO, MgO or SrO. 2 / g~1000m 2 d) 10m / g of Fe-alumina spinel impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce. 2 / g~1000m 2 The Fe-alumina spinel according to embodiment 2, having a surface area of at least 10 m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce; 2 / g. e) 10m 2 / g~1000m 2The Fe-alumina spinel according to embodiment 2 having a surface area of 1 / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher order mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce, and natural or artificial layered solids comprising 5-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation. The resulting formulation is calcined at a temperature of up to 2,100°F, resulting in a 5m 2 / g~1000m 2 A metal-impregnated Fe-alumina spinel with a surface area of 1000 nm / g is obtained.
[0063] 13. The reverse water gas shift (RWGS) catalyst of embodiment 3, wherein the catalyst comprises the following components: a) 10 m 2 / g~1000m 2 %. The Mg-alumina spinel according to embodiment 2, having a surface area of 10 m / g, impregnated with up to 35 wt. % Co salt. 2 / g~1000m 2 A Ni-alumina spinel according to embodiment 2 having a surface area of 10 m / g, the Ni-alumina spinel being mixed with up to 35 wt.% of CaCO3, MgCO3, SrCO3, CaO, MgO or SrO. 2 / g~1000m 2 d) 10m / g of Ni-alumina spinel according to embodiment 2, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce. 2 / g~1000m 23. A Co-alumina spinel according to embodiment 2 having a surface area of at least 10 m / g, impregnated with up to 35% of a first, second, third or higher mixture of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce; 2 / g. e) 10m 2 / g~1000m 2 The Co-alumina spinel according to embodiment 2, having a surface area of 1 / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher order mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce, and natural or artificial layered solids comprising 5-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation. The resulting formulation is calcined at a temperature of up to 2,100°F, resulting in a 5m 2 / g~1000m 2 A metal-impregnated Co-alumina spinel having a surface area of 1000 nm / g is obtained.
[0064] 14. The reverse water gas shift (RWGS) catalyst of embodiment 3, wherein the catalyst comprises the following components: a) 10 m 2 / g~1000m 2 % Ni salt. 2 / g~1000m 2 A Ni-alumina spinel according to embodiment 2 having a surface area of 10 m / g, the Ni-alumina spinel being mixed with up to 35 wt.% of CaCO3, MgCO3, SrCO3, CaO, MgO or SrO. 2 / g~1000m 2d) 10m / g of Ni-alumina spinel according to embodiment 2, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce. 2 / g~1000m 2 3. The Ni-alumina spinel of embodiment 2 having a surface area of at least 10 m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce; 2 / g. e) 10m 2 / g~1000m 2 The Ni-alumina spinel according to embodiment 2, having a surface area of 1 / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher order mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce, and natural or artificial layered solids comprising 5-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation. The resulting formulation is calcined at a temperature of up to 2,100°F, resulting in a 5m 2 / g~1000m 2 A metal-impregnated Ni-alumina spinel with a surface area of 1 / g is obtained.
[0065] 15. The reverse water gas shift (RWGS) catalyst of embodiment 3, wherein the catalyst comprises the following components: a) 10 m 2 / g~1000m 2 %. A Mg-alumina spinel according to embodiment 2, having a surface area of 10 m / g, impregnated with up to 35 wt. % of a Cu salt. 2 / g~1000m 2A Cu-alumina spinel according to embodiment 2 having a surface area of 100 μm / g, the Cu-alumina spinel being mixed with up to 35 wt. % of CaCO3, MgCO3, SrCO3, CaO, MgO or SrO. 2 / g~1000m 2 d) 10m Cu-alumina spinel according to embodiment 2, having a surface area of 1000 μm / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce. 2 / g~1000m 2 A Cu-alumina spinel according to embodiment 2 having a surface area of at least 10 m 2 e) Cu-alumina spinel impregnated with up to 35% mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce as different metal spinels with a mean particle size of 10m / g. 2 / g~1000m 2 The Cu-alumina spinel according to embodiment 2, having a surface area of 1 / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher order mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce, and natural or artificial layered solids comprising 5-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation. The resulting formulation is calcined at a temperature of up to 2,100°F, resulting in a 5m 2 / g~1000m 2 A metal-impregnated Cu-alumina spinel with a surface area of 1000 μm / g is obtained.
[0066] 16. The reverse water gas shift (RWGS) catalyst of embodiment 3, wherein the catalyst comprises the following components: a) 10 m 2 / g~1000m 2 %. A Mg-alumina spinel according to embodiment 2, impregnated with up to 35 wt. % of a Zn salt, having a surface area of 10 m 2 / g~1000m 2 Zn-alumina spinel according to embodiment 2, having a surface area of 10 m / g, mixed with up to 35% by weight of CaCO3, MgCO3, SrCO3, CaO, MgO or SrO. 2 / g~1000m 2 Zn-alumina spinel according to embodiment 2, having a surface area of 10 m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce. 2 / g~1000m 2 Zn-alumina spinel according to embodiment 2 having a surface area of at least 10 m 2 e) Zn-alumina spinel impregnated with up to 35% mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce as different metal spinels with a mean particle size of 10m / g. 2 / g~1000m 2 Zn-alumina spinel according to embodiment 2 having a surface area of 1 / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher order mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce, and natural or artificial layered solids comprising 5-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation. The resulting formulation is calcined at a temperature of up to 2,100°F, resulting in a 5m 2 / g~1000m 2A metal-impregnated Zn-alumina spinel having a surface area of 1000 nm / g is obtained.
[0067] 17. The reverse water gas shift (RWGS) catalyst of embodiment 3, wherein the catalyst comprises the following components: a) 10 m 2 / g~1000m 2 % of La salt. 2 / g~1000m 2 The La-alumina spinel according to embodiment 2, having a surface area of 10 m / g, wherein the La-alumina spinel is mixed with up to 35 wt.% of CaCO3, MgCO3, SrCO3, CaO, MgO or SrO. 2 / g~1000m 2 d) 10m La-alumina spinel according to embodiment 2, having a surface area of 10m / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce. 2 / g~1000m 2 The La-alumina spinel according to embodiment 2 has a surface area of at least 10 m 2 e) La-alumina spinel impregnated with up to 35% mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce as different metal spinels with a mean particle size of 10m / g. 2 / g~1000m 2The La-alumina spinel according to embodiment 2, having a surface area of 1 / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher order mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce, and natural or artificial layered solids comprising 5-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation. The resulting formulation is calcined at a temperature of up to 2,100°F, resulting in a 5m 2 / g~1000m 2 A metal-impregnated La-alumina spinel with a surface area of 1000 nm / g is obtained.
[0068] 18. The reverse water gas shift (RWGS) catalyst of embodiment 3, wherein the catalyst comprises the following components: a) 10 m 2 / g~1000m 2 % of Ce salt. 2 / g~1000m 2 A Ce-alumina spinel according to embodiment 2 having a surface area of 10 m / g, the Ce-alumina spinel being mixed with up to 35 wt.% of CaCO3, MgCO3, SrCO3, CaO, MgO or SrO. 2 / g~1000m 2 d) 10m 20m 30m 40m 50m 60m 70m 80m 90m 10m 11m 12m 13m 14m 15m 16m 17m 18m 19m 20m 21m 22m 23m 24m 25m 26m 27m 28m 29m 30m 31m 32m 33m 34m 35m 36m 37m 38m 39m 40m 41m 42m 43m 44m 45m 46m 47m 48m 49m 50m 51m 52m 53m 54m 55m 56m 57m 58m 59m 60m 61m 62m 63m 2 / g~1000m 2 A Ce-alumina spinel according to embodiment 2 having a surface area of at least 10 m 2e) Ce-alumina spinel impregnated with up to 35% mixture of primary, secondary, tertiary or higher mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce as different metal spinels with a mean particle size of 10m / g. 2 / g~1000m 2 Zn-alumina spinel according to embodiment 2 having a surface area of 1 / g, impregnated with up to 35% of a mixture of primary, secondary, tertiary or higher order mixtures of salts including, but not limited to, Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La and Ce, and natural or artificial layered solids comprising 5-10% of the catalyst formulation, 20-30% of the catalyst formulation, 40-50% of the catalyst formulation, 50-60% of the catalyst formulation, 60-70% of the catalyst formulation, 70-80% of the catalyst formulation. The resulting formulation is calcined at a temperature of up to 2,100°F, resulting in a 5m 2 / g~1000m 2 A metal-impregnated Ce-alumina spinel with a surface area of 1000 nm / g is obtained.
[0069] 19. In the embodiments 5 to 18, the present invention is directed to a CO2 hydrogenation catalyst formulation that focuses on impregnating a specific metal into a metal-alumina spinel synthesized from the same metal, but also includes various permutations of other metals in the embodiment 3 on other metal-spinels in the embodiment 2 (e.g., Ni on Mg-aluminate, Ni on Ba-aluminate, etc.).
[0070] 20. This embodiment comprises a reverse water gas shift (RWGS) catalyst (Type C) employing one of the metal-alumina spinels according to embodiment 2 by a) impregnating with up to 35% by weight of two metal salts (e.g., nitrates, acetates, carbonates, etc.) or metal hydroxides selected from the group consisting of Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce, the metal salts or metal hydroxides not chemically bound to the spinel, and b) calcining the metal-alumina spinel impregnated with two or more metals at a temperature of up to 2,100° F., thereby synthesizing a solid solution of the two metals on the metal-alumina spinel.
[0071] 21. The reverse water gas shift (RWGS) catalyst according to embodiment 20, wherein the catalyst comprises: a) 10m 2 / g~1000m 2 A reverse water gas shift (RWGS) catalyst produced by a process comprising: b) synthesizing a Mg-alumina spinel according to embodiment 2 having a surface area of 100 nm / g, b) impregnating the spinel with a mixture of Ni and Mg up to 35% by weight, c) calcining the Ni and Mg impregnated Mg-alumina spinel at a temperature up to 2,100° F., and d) thereby producing a solid solution of the two metals having a composition of Ni2Mg. Ni and Mg form a solid solution at 2,100° F. because both Ni and Mg crystallize in a face-centered cubic structure and have similar electronegativity and valence.
[0072] 22. The reverse water gas shift (RWGS) catalyst according to embodiment 20, wherein the catalyst comprises: a) 10m 2 / g~1000m 2A reverse water gas shift (RWGS) catalyst produced by a process comprising: b) synthesizing a Mg-alumina spinel according to embodiment 2 having a surface area of 100 nm / g, b) impregnating the spinel with a mixture of Ni and Cu up to 35% by weight, c) calcining the Ni and Mg impregnated Mg-alumina spinel at a temperature up to 2,100° F., and d) thereby producing a solid solution of the two metals having a composition of NiCu. Ni and Cu form a solid solution at 2,100° F. because both Ni and Cu crystallize in a face-centered cubic structure and have similar atomic radii, electronegativities and valencies.
[0073] Catalyst Performance Embodiments Most of the improved CO2 hydrogenation catalysts described above in the embodiments of the catalyst composition meet the commercial quality and performance specifications summarized in Table 1.
[0074] 1. Low Cost Ingredients -Catalysts are primarily formulated using low-cost Group 1 elements (alkali metals) including Na, K, Li, Cs, Rb, Group 2 elements (alkaline earth metals): Mg, Ca, Sr, Ba, and Be, transition metals including Ni, Co, Fe, and Cu, and rare earth elements including Ce, Y, and La. The addition of small amounts of precious metals (Au, Ag, Pt, Pd, Ir, etc.) has not been found to improve the performance of these improved CO2 hydrogenation catalysts.
[0075] 2. Commercial Production -Substrates and catalysts are economically produced in multi-ton quantities using well-established commercial-scale production processes. Metal-alumina spinel substrates can be prepared a) by co-precipitation or b) by mixing appropriate molar amounts of metal precursors and alumina particles to form a slurry, drying the slurry and calcining the mixture at temperatures up to 2,600° F. Catalysts are prepared by impregnating the metals onto the metal-alumina spinel substrates followed by calcination at temperatures up to 2100° F.
[0076] 3. Physically robustThe disclosed catalyst has a hardness of 4 Mohs to 10 Mohs or equivalent on the Rockwell hardness scale. This high level of hardness eliminates potential problems such as catalyst breakage, cracking and wear.
[0077] 4. Chemically and physically stable - These a) metal-alumina spinels, b) metal-impregnated metal-alumina spinels, and c) solid solutions impregnated with metal-alumina spinels maintain their chemical and physical properties (such as not melting) at temperatures up to 2,100°F.
[0078] 5. Compatible with commercial catalytic reactors - Catalyst pellets, tablets or hollow tablets are easy to load into catalytic reactors (tubular or packed bed reactors). The pressure drop from top to bottom of the catalytic reactor is 0-50 psi, typically 0-25 psi. Activation of the catalyst (e.g. reduction with H2) can be performed in-situ if necessary.
[0079] 6. High CO 2 Conversion Efficiency - The CO2 to CO conversion efficiency of H2 / CO2 blends with a ratio higher than 3.0 / 1.0 is 2,000hr -1 ~1,000,000hr -1 and a temperature of 1,300° F. to 1,800° F., the ratio is 70% to 100%, preferably 75% to 100%, and more preferably 80% to 100%.
[0080] 7. High CO production selectivity The disclosed catalyst formulations have a CO selectivity of at least 90%. Some of the preferred catalyst formulations have a CO selectivity of greater than 99% with a methane selectivity of less than 1%, and in some cases as low as 0.1%.
[0081] 8. No coking or chemical changes -These improved catalyst formulations do not undergo coking or changes in chemical composition during operation.
[0082] 9. Long-term performance-Several of the improved CO2 hydrogenation catalysts have been tested for over 1,500 hours on stream, with the degradation of CO2 conversion found to be 0-0.50% per 1,000 hours. EXAMPLES
[0083] Example 1: Improved RWGS Catalyst Formulation A - A stream containing CO2 is produced by an industrial process or captured from ambient air. This CO2 stream is fed to a CO2 capture facility, which uses an adsorbent such as methyldiethanolamine (MDEA) in an adsorption tower to capture the CO2. Relatively pure CO2 is regenerated from the MDEA by heating.
[0084] Low carbon electricity from wind, solar, nuclear or other low carbon sources is available on-site at the carbon capture facility. High purity water is produced from locally available water. Low carbon H2 is produced from pure water by electrolysis.
[0085] The reaction uses low carbon electricity to split water into H2 and O2. The electrolyser in this example is a PEM electrolyser. The electrolyser produces two streams: H2 and O2.
[0086] The improved catalyst formulation A of this embodiment 2 (above) comprises: a) 10m 2 / g~1000m 2 3. synthesizing a metal-aluminate spinel having a surface area of 100 / g, the metal spinel comprising: a. Group 2 metals which are calcined with alumina, thereby forming Mg-aluminate, Ca-aluminate, Sr-aluminate, Ba-aluminate and Be-aluminate. b. Group 1 metals calcined with alumina, thereby forming Li-aluminate, Rb-aluminate and Cs-aluminate. c. Transition metals which are calcined with alumina, thereby forming Fe-aluminate, Co-aluminate, Ni-aluminate, Cu-aluminate, Zn-aluminate. d. Rare earth metals calcined with alumina, thereby forming La-aluminate, Ce-aluminate. The compound is produced by a method comprising the steps selected from the group consisting of:
[0087] The improved catalyst is used to convert the recovered CO2 and renewable H2 streams to synthesis gas. Example 1 provides the relationship between temperature and the % conversion of CO2 to CO for the improved CO2 hydrogenation catalyst. In this example, the H2 to CO2 ratio is 3.4 / 1.0, the pressure is 300 psig, and the space velocity is 20,000 hr -1 The CO2 conversion varies from 75% to 83.5% at 1,250 to 1,650°F, with a conversion loss of 0 to 0.5% after 1,000 hours on stream. The lifetime of these catalysts is excellent, as the catalysts showed little sintering in these relevant temperature ranges. The CO selectivity is greater than 99.5%, with CH4 selectivity ranging from 0 to 0.5%. The dotted line is a fitted curve showing that the relationship between CO2 conversion and temperature is close to a straight line.
[0088] Example 1 - Typical relationship between temperature and % conversion of CO2 to CO for the modified RWGS catalyst. Figure 1 shows a typical relationship between temperature and % conversion of CO2 to CO for the modified RWGS catalyst. The X-axis is temperature in degrees Fahrenheit. The Y-axis is the molar % conversion of CO2 to CO. As seen at temperatures between 1200°F and 1750°F, the CO2 conversion is between 70-85%.
[0089] Example 2: Improved RWGS Catalyst Formulation B - This improved catalyst formulation B is described in embodiment #3 (above) as a metal on metal aluminate. This type B CO2 hydrogenation catalyst is prepared by impregnating one of the metal-alumina spinels described in embodiment 2 with: a) up to 35 wt. % of a metal salt (e.g., nitrate, acetate, carbonate, etc.) or metal hydroxide selected from the group consisting of Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce, which is not chemically bonded to the spinel; b) calcining the impregnated metal-coated metal-alumina spinel at a temperature up to 2,100° F., thereby producing a 5 mm 2 / g~1000m 2 The metal-impregnated metal-alumina spinels with surface areas of 0.1 μm / g were synthesized using the method described above.
[0090] In this example, the catalyst is MgO or Mg(OH)2 impregnated onto Mg-alumina spinel, which is reduced in-situ with H2 to produce Mg, MgO and Mg(OH)2 on the surface of the spinel.
[0091] The improved catalyst is used to convert the captured CO2 and renewable H2 streams to synthesis gas. In this example, the H2 to CO2 ratio is 3.4 / 1.0, the temperature is 1,650°F, the pressure is 300 psig, and the space velocity is 20,000 hr -1 CO2 conversion is 82% at 1,650°F with a conversion loss of 0-0.5% after 1,000 hours on stream. CO selectivity is greater than 99%.
[0092] Example 3. Improved RWGS Catalyst Formulation C - This improved RWGS catalyst C is described in embodiments 20-23 for the efficient conversion of CO2 and H2 to synthesis gas, and is 2 / g~1000m 2The catalyst is produced by a process comprising the steps of: a) synthesizing a Mg-aluminate spinel having a surface area of 10000000 / g; b) coating the spinel with up to 20% by weight of Mg, thereby providing a metal-coated spinel; c) impregnating the metal-coated spinel with a solution containing a water-soluble nickel salt and a rare earth metal nitrate or acetate; and d) calcining the impregnated metal-coated spinel at a temperature of up to 2,100°F, thereby synthesizing a catalyst that is an impregnated spinel containing up to 35% by weight of nickel and 0.1% to 5.0% by weight of a rare earth metal. The catalyst may contain 0.1 to 5 parts by weight of cerium, ruthenium, lanthanum, platinum or rhenium and 2% to 20% by weight of nickel per 100 parts by weight of the spinel support. As described in embodiment #21, the solid solution catalyst is Ni2Mg.
[0093] Another improved catalyst type C for efficient conversion of CO2 and H2 to synthesis gas is 2 / g~1000m 2 b) synthesizing a Mg-aluminate spinel having a surface area of 100000 / g, b) coating the spinel with up to 20 wt% Cu, thereby providing a metal-coated spinel, c) impregnating the metal-coated spinel with a solution containing a water-soluble Ni salt and a rare earth metal nitrate or acetate, and d) calcining the impregnated metal-coated spinel at a temperature of up to 2,100° F., thereby synthesizing a catalyst that is an impregnated spinel containing up to 20 wt% nickel and 0.1 wt% to 5.0 wt% rare earth metal. As described in embodiment #22, the solid solution catalyst is NiCu3.
[0094] The relationship between temperature and CO2 conversion efficiency (Example #1) is similar for catalyst #1 and catalyst #2. The difference is that catalyst #1 has a CH4 selectivity of 0-0.5% whereas catalyst #2 has a CH4 selectivity of up to 7.0% (depending on temperature and pressure). However, catalyst #2 is more efficient at higher space velocities.
[0095] References U.S. Patent 7,718,832 B1 05 / 2010 Schuetzle et al 8,388,987 B2 03 / 2013 Ikematsu et al 8,394,862 B1 03 / 2013 Schuetzle et al 8,741,001 B1 06 / 2014 Schuetzle et al 9,090,831 B2 07 / 2015 Schuetzle et al 9,476,002 B1 10 / 2016 Schuetzle et al 9,611,145 B1 04 / 2017 Schuetzle et al 9,631,147 B1 04 / 2017 Schuetzle et al 10,478,806 B1 11 / 2019 Schuetzle et al
[0096] U.S. Patent Application 2003 / 0113244 Al 06 / 2003 DuPont et al
[0097] Foreign Patent Documents GB 1995 / 2279583 A1 11 / 1995 Iwanani et al AU 2015 / 203898 B2 7 / 2015 Landau et al WO 2018 / 219992 A1 6 / 2018 Lizandara et al
[0098] Non-Patent Documents Alamer, A.: CO2conversion by reverse water gas shift reaction, Master’s Thesis, UCLA Chemical Engineering (2018). Artz, J., Muller, T.E., Thenert, K., Kleinekorte, J., Meys, R., Sternberg, A., Bardow, A, Leitner, W: Sustainable conversion of carbon dioxide: An integrated review of catalysis and life cycle assessment. Chemical Reviews, 118, 434-504 (2018). Bahmanpour, A.M., Heroguel, F., Kilic, M., Baranowski, C.J., Artiglia, L.: Cu-Al spinel as a highly active and catalyst for the reverse water gas shift reaction. ACS Catal., 9, 6243-6251 (2019). Bahmanpour, A.M, Signorile, M., Krocher, O.: Recent progress in syngas production via catalytic CO2hydrogenation reaction, Applied Catalysis B: Environmental, 295, 120319 (2021). Centi, G., Perathoner, S.: Opportunities and prospects in the chemical recycling of carbon dioxide to fuels. Catalysis Today, 148, 191-205 (2009). Chen, J. G., Catalytic reduction of CO2by H2for synthesis of CO, Catalysis Letters, 91 (3), 247-252 (2003). Chen, P., Zhao, G., Shi, X-R., Zhu, J., D-J., Lu, Y.: Nano-intermetallic InNi3C0.5 compound discovered as a superior catalyst for CO2re-utilization, iScience,17, 315-324 (2019). Chen, X., Chen, Y., Song, C., Ji, P., Wang, N., Wang, W., Cui, L.: Recent advances in supported metal catalysts and oxide catalysts for the reverse water-gas shift reaction, Front. Chem., 8, 1-21 (2020). Choi, S., Sang, B-I., Hong, J., Hong, J., Yoon, K.J., Son, J., Lee, J-H, Kim, B-K., Kim, H.: Catalytic behavior of metal catalysts in high temperature RWGS reaction: In-situ FT-IR experiments and first-principles calculations, Scientific Reports, 1-10 (2017). Daza, Y.A., Kuhn, J.N.: CO2conversion by reverse water gas shift catalysis: Comparison of catalysts, mechanisms, and their consequences for CO2conversion to liquid fuels, Royal Society of Chemistry Advances, 6, 49, 675-49,691 (2016). Debek, R., Motak, M., Galvez, M.E., Da Costa, P. and Grzybek, T.: Catalytic activity of hydrotalcite-derived catalysts in the dry reforming of methane: On the effect of Ce promotion and feed gas composition, Reaction Kinetics, Mechanisms and Catalysis, 121, 185-208 (2017). Figueras F.: Basicity, catalytic and adsorptive properties of hydrotalcites. In: Gil A., Korili S., Trujillano R., Vicente M. (eds), Pillared Clays and Related Catalysts. Springer, New York, N.Y. (2010) Fischer, N., Claeys, M., Van Steen, E., Niemantsverdriet, H., Vosloo, M.: Syngas convention - fuels and chemicals from synthesis gas: state of the art, 2, 1-200 (2016). Goncalves, R.V., Vono, L.R., Wojcieszak, R., Carlos, S.B., Heverton-Wender, S.B.D., Liane, E.T.N., Rossi, M., Selective hydrogenation of CO2into CO on a highly dispersed nickel catalyst obtained by magnetron sputtering deposition: A step towards liquid fuels, Applied Catalysis B: Environmental, 209, 240-246 (2017). Gumber, S., Gurumoorthy, A.V.P.: Methanol economy versus H2economy, in Methanol: Science and Engineering. Basile, A., Dalena, F., editors. Elsevier; Amsterdam, The Netherlands 661-674 (2018). He, Y., Yang, K.R., Yu, Z., Fishman, Z.S., Achola, L.A., Tobin, Z.M., Heinlein, J.A., Hu, Shu, Suib, S.L., Batista, V., Pfefferle, L.D: Catalytic manganese oxide nanostructures for the reverse water gas shift reaction, Nanoscale, 11, 16677-16688 (2019). Hepburn, C., Adlen, E., Beddington, J., Carter, E.A., Fuss, S., Dowell, N.M., Minx, J. C., Smith, P., Williams, C.K.: The technological and economic prospects for CO2utilization and removal, Nature, 575, 87-97 (2019). Ishito, N., Hara, K., Nakajima, K., Fukuoka, A.: Selective synthesis of carbon monoxide via formates in reverse water-gas shift reaction over alumina-supported gold catalyst, Journal of Energy Chemistry, 25, 306-310 (2016). Jatav, J., Jatav, R., Bhardwaj, S.K., Sahu, P.K., Kumar, K, Journal of Chemical and Pharmaceutical Research, 8, 678-696 (2016). Jiang, Z., Xiao, T., Kuznetsov, V.L., Edwards, P.P.: Turning carbon dioxide into fuel. Phil. Trans. R. Soc. A, 368, 3343-3364 (2010). Kharaji, A.G., Takassi, M.A., Shariati, A.: Activity and Stability of Fe-V2O5 / γ- Al2O3Nano-catalyst in the Reverse Water Gas Shift (RWGS) Reaction, 2012 International Conference on Environmental Science and Technology, Singapore, 30 (2012). Kharaji, A.G., Shariati, A., Ostadi, M.: Development of Ni-Mo / Al2O3catalyst for reverse water gas shift (RWGS) reaction, Journal of Nanoscience and Nanotechnology,14, 6841-6847 (2014). Kim, S.S., Lee, H.H., Hong, S.C.: The effect of the morphological characteristics of TiO2 supports on the reverse water-gas shift reaction over Pt / TiO2 catalysts, Applied Catalysis B: Environmental, 119-120, 100-108 (2012). Kim, D.H., Park, J.L., Park, E.J., Kim, Y.D., Uhm, S.: Dopant effect of barium zirconate-based perovskite-type catalysts for the intermediate-temperature reverse water gas shift reaction, ACS Catalysis, 4, 3117 (2014). Lin, J., Hu, C., Xu, X., Shao, M., Hu, Y., Ma, C.: Investigation of various metals on hydrotalcite-based Cu / Zn / Al catalysts in methanol steam reforming, Chemical Engineering Technology, 44, 1121-1130 (2021). Lortie, M.: Reverse water gas shift reaction over supported Cu-Ni nanoparticle catalysts, Department of Chemical and Biological Engineering M.S. Thesis, University of Ottawa, Ottawa, Canada (2014). Lu, B., Kawamoto, K.: Preparation of mesoporous CeO2and monodispersed NiO particles on CeO2, and enhanced selectivity of NiO-CeO2for reverse water gas shift reaction, Materials Research Bulletin, 53, 70-78 (2014). National Academy of Sciences (NAS): Chemical Utilization of CO2into Chemicals and Fuels, Gaseous Carbon Waste Streams Utilization: Status and Research Needs, National Academies Press, Washington D.C. (2019). Pastor-Perez, L., Baibars, F., Le Sache, E., Arellano-Garcia, H., Gu, S., Reina, T.R.: CO2valorization via reverse water-gas shift reaction using advanced Cs doped Fe-Cu / Al2O3catalysts, Journal of CO2Utilization, 21, 423-428 (2017). Pastor-Perez, L., Shah, M., Le Sache, E., Ramierez-Reina, T.: Improving Fe / Al2O3catalysts for the reverse water-gas shift reaction: On the effect of Cs as activity / selectivity promoter, Catalysts, 6, 608-622 (2018). Pines, H., Haag, W.O.: Alumina, its intrinsic acidity and catalytic activity, J. Am. Chem. Soc., 82, 10, 2471-2483 (1960). Ranjbar, A., Aghamire, S.F., Irankhah, A.: Effect of MgAl2O4catalyst support synthesis method on the catalytic activity of nickel nano catalyst in reverse water gas shift reaction, Iranian Journal of Chemical Engineering,16, 58-69 (2019). Schuetzle, D., Tamblyn, G., Caldwell, M., Schuetzle, R.: Solar reforming of carbon dioxide to produce diesel fuel. U.S. Department of Energy report #DE-FE0002558 (2010). Schuetzle, D., Tamblyn, G., Caldwell, M., Hanbury, O., Schuetzle, R., Rodriquez, R., Johnson, A., Deichert, F., Jorgensen, R., Struble, D: Demonstration of a pilot integrated biorefinery for the efficient, direct conversion of biomass to diesel fuel. DOE Technical Report #DE-EE0002876, U.S. Department of Energy Bioenergy Technologies Office (DOE-BTO), Golden, CO, 1-261 (May 2015) (www.researchgate.net) Schuetzle, D.: Historical and predicted global climate changes and some potential accelerated climate moderation approaches, 2018 Global Climate Action Summit, San Francisco, CA, 1-42 (2020) (www.researchgate.net). Shukla, P.R. et al: Climate Change and Land: an IPCC special report on climate change, desertification, land degradation, sustainable land management, food security, and greenhouse gas fluxes in terrestrial ecosystems, 2019 Intergovernmental Panel on Climate Change (2019) (www.ipcc.ch) Sikander, U., Sufian, S., Salam, A.: A review of hydrotalcite based catalysts for hydrogen production systems, International Journal of Hydrogen Energy 42 (2017) Sun, F-M., Yan, C-F., Wang, Z-D., Guo, C-Q., Huang, S-L.: Ni / Ce on Zr-0 catalyst for high CO2conversion during reverse water gas shift reaction (RWGS), International Journal of H2Energy, 40 (46), 15985-15993 (2015) Tan, E.C.D., Schuetzle, D., Zhang, Y., Hanbury, O., Schuetzle, R.: Reduction of greenhouse gas and criteria pollutant emissions by direct conversion of associated flare gas to synthetic fuels at oil wellheads, International Journal of Energy and Environmental Engineering, 9, 305-321 (2018). Vogt, C., Monai, M., Kramer, G.J., Weckhuysen, B.M.: The renaissance of the Sabatier reaction and its applications on Earth and in space, Nature Catalysis, 2, 188-197 (2019). Wang, L., Zhang, S., Liu, Y., Reverse water gas shift reaction over Co-precipitated Ni-CeO2 catalysts, Journal of Rare Earths, 26,1, 66-70 (2008). Wang, Y., Liu, T., Lei, L., Chen, F.: High temperature solid oxide H2O / CO2co-electrolysis for syngas production, Fuel Processing Technology, 161 (2016). Wang, L., Liu, H., Chen, Y., Yang, S.: Reverse water-gas shift reaction over co-precipitated Co-CeO2 catalysts: Effect of Co content on selectivity and carbon formation, International Journal, 42, 6, 3682-3689 (2017). Yang, L., Pastor-Perez, L., Gua, S., Sepulveda-Escribanob, A, Reina, T.R.: Highly efficient Ni / CeO2-Al2O3catalysts for CO2upgrading via reverse water-gas shift: Effect of selected transition metal promoters, Applied Catalysis B: Environmental, 232, 464-471 (2018). Zhang, X., Zhu, X., Lin, L., Yao, S., Zhang, M., Liu, X., Wang, X., Li, Y.-W., Shi, C., Ma, D.: Highly dispersed copper over β Mo2C as an efficient and stable catalyst for the reverse water gas shift (RWGS) reaction, ACS Catalysis (2016). Zhang, L. et al: Active and stable MgAl2O4and Ni on MgAl2O4catalysts for RWGS reactions, Tsinghua University, Beijing (2021). Zhuang, Y.: Renewable syngas generation and biogas / landfill gas upgrade via thermocatalytic conversion of carbon dioxide, M.S. Thesis, University of Waterloo, Chemical Engineering (2017).
Claims
1. 1. A catalyst for producing synthesis gas, comprising: the catalyst comprises a chemical composition that does not contain a precious metal selected from the group of Rh, Pt, Au, Ag, Pd, or Ir; the catalyst has a hardness of 4 Mohs to 10 Mohs; the catalyst is chemically and physically stable at a temperature of 2,100° F. such that after being heat treated at 2,100° F., the BET surface area of the catalyst is 0-20% of its surface area prior to said treatment; The catalyst can be easily loaded into a catalytic reactor having an inlet-to-outlet pressure drop of 0-50 psi; The catalyst is CO 2 can be converted to CO, where CO 2 Conversion is between 70% and 100% at temperatures between 1,300°F and 1,800°F and pressures above 50 psi, and the catalyst does not coke during the conversion. 2 A catalyst where the conversion decreases by 0-1% per 1000 hours of operation.
2. The catalyst of claim 1 , wherein the catalyst comprises a metal-alumina spinel.
3. 3. The catalyst of claim 2, wherein the metal-alumina spinel is prepared by calcining a mixture of alumina and at least one element selected from the group consisting of at least one of the elements Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce.
4. 3. The catalyst of claim 2, wherein the metal-alumina spinel is impregnated with one or more metals selected from alkali metals, alkaline earth metals, transition metals and rare earth metals.
5. 5. The catalyst of claim 4, wherein one of the metals impregnated on the metal-alumina spinel is selected from the group of Ni, Co, Fe, Cu, La, Ce, Zr, Ti, La, Li, Cs, Rb, Mg, Ca, Sr, Ba, Be, and the catalyst is calcined at up to 2,100° F., thereby forming a solid solution on the metal-alumina spinel.
6. 5. The catalyst of claim 4, wherein the metal impregnation into the metal aluminate is 0.0 to 35 wt. % of a metal salt or metal hydroxide selected from the group consisting of Mg, Ca, Sr, Ba, Li, Rb, Cs, Fe, Co, Ni, Cu, Zn, La, and Ce, and the impregnated metal-coated metal-alumina spinel is calcined at a temperature up to 2,100° F., thereby synthesizing the metal-impregnated metal-alumina spinel catalyst.
7. The metal-alumina spinel impregnated with metal is 5 m 2 / g to 1000m 2 The catalyst of claim 4 having a surface area of 1 / g.
8. The catalyst of claim 1 , wherein the catalyst comprises hydrotalcite.
9. The catalyst of claim 1 , wherein the catalyst comprises a layered double hydroxide.
10. The catalyst is 5 m 2 / g to 1000m 2 9. The catalyst of claim 8 having a surface area of 1 / g.
11. The catalyst is 5 m 2 / g to 1000m 2 10. The catalyst of claim 9 having a surface area of 100 / g.
12. The catalyst is 5 m 2 / g to 1000m 2 3. The catalyst of claim 1 having a surface area of 1 / g.
13. The catalyst has the general composition ABO 3 wherein A is selected from the group consisting of Sr, Ca, Ba, Mg, Fe, La, Ca, Pb, or Bi, and B is selected from Al, Ti, Rb, Si, Fe, Yb, or Mn.
14. The catalyst has the general composition AB 2 O 4 wherein A is selected from the group consisting of Mg, Zn, Fe, Mn, Cu, Ni, Li, Cs, Rb, Mg, Ca, Sr, Ba, Be and Ti, and B is selected from the group consisting of aluminum, iron, chromium, cobalt and vanadium.
15. 15. The catalyst of claim 14, wherein the catalyst comprises a metal aluminate, where B is aluminum.
16. 1. A method for producing synthesis gas, comprising: reacting a feedstock comprising a mixture of hydrogen and carbon dioxide in a catalytic reactor containing a catalyst; the catalyst comprises a chemical composition that does not contain a precious metal selected from the group of Rh, Pt, Au, Ag, Pd, or Ir; the catalyst has a hardness of 4 Mohs to 10 Mohs; said catalyst is chemically and physically stable at a temperature of 2,100° F. such that after being heat treated at 2,100° F., the BET surface area of said catalyst is within the range of 0-5% of its surface area prior to said heat treatment; The catalyst can be easily loaded into a catalytic reactor having an inlet-to-outlet pressure drop of 0-50 psi; The catalyst is CO 2 can be converted to CO, where CO 2 Conversion is between 70% and 100% at temperatures between 1,300°F and 1,800°F and pressures above 50 psi, and the catalyst does not coke during the conversion. 2 Conversion rate decreases by 0-1% per 1000 hours of operation. The method wherein the catalytic reactor is operated at between 1,300° F. and 1,800° F. at a pressure of 50 psi to 450 psi, thereby producing a product stream comprising CO from the catalytic reactor.
17. The feedstock has a H 2 / CO 2 The method of claim 16 comprising a ratio.
18. 17. The method of claim 16, wherein the catalyst does not coke.
19. The method of claim 16, wherein the catalytic reactor is operated at a temperature of from 1300°F to 1800°F.
20. 17. The method of claim 16, further reacting the product stream to thereby produce at least one product selected from the list consisting of liquid fuels, methanol, propane, naphtha, and chemicals.
Citation Information
Patent Citations
Catalyst for producing synthetic gas from natural gas and carbon dioxide and method for producing the same
JP2011529394A
Supported perovskite-oxide composites for enhanced low temperature thermochemical conversion of co2 to co
US20200139351A1
Improved catalysts and processes for the direct production of liquid fuels from carbon dioxide and hydrogen
WO2021225567A1
Reverse water gas shift catalytic reactor systems
WO2021225643A1