Battery
By using a breathable porous body closure on the battery case, the deformation problem caused by battery expansion in the vacuum environment is solved, and the stability and efficient manufacturing of the battery in the vacuum environment are achieved.
Patent Information
- Application Number
- JP2023121151
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-07-25
- Publication Date
- 2025-02-06
AI Technical Summary
When a solid lithium-ion battery is used in a vacuum environment, the gas in the container expands and causes the container to deform.
A porous body with breathability is used as the closure member, and the battery case is closed through the opening of the closure member and internal gas is allowed to be discharged.
Effectively prevent the battery case from deforming in a vacuum environment, while maintaining the stability and manufacturing efficiency of the internal structure.
Smart Images

Figure 2025017853000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a battery. [Background technology]
[0002] 2. Description of the Related Art Conventionally, a battery including a laminate cell and a metal case that houses the laminate cell has been known.
[0003] For example, a solid-state lithium-ion battery has been disclosed that includes a laminate as a power generating element, a first container that houses the laminate, a terminal connected to the laminate and drawn out of the first container, and a second container that houses the first container. The laminate includes a positive electrode layer, a negative electrode layer, and a solid electrolyte layer. The first container is made of a first film and a second film. The second container has a metal body and a metal lid. The lid has a hole through which the terminal passes. The lid is fixed airtightly to the body by welding, adhesive, or the like. The gap between the terminal and the hole is filled with a filler material (see Patent Document 1 below). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Patent Publication No. 2022-81801 Summary of the Invention [Problem to be solved by the invention]
[0005] When an attempt is made to use a solid-state lithium-ion battery such as that described in Patent Document 1 in a vacuum environment, the gas in the second container may expand, causing the second container to deform.
[0006] The present invention provides a battery capable of suppressing deformation of the casing when the battery is used in a vacuum environment. [Means for solving the problem]
[0007] The present invention [1] includes a battery comprising: a laminated cell having leads; a housing having an opening through which the leads pass and containing the laminated cell; and a sealing body made of a porous body having air permeability and sealing the opening of the housing.
[0008] According to this configuration, the sealing body that seals the opening of the housing is made of a porous body having air permeability.
[0009] Therefore, when the battery is used in a vacuum environment, the gas inside the casing passes through the sealing member and is discharged to the outside of the casing.
[0010] As a result, when the battery is used in a vacuum environment, deformation of the casing due to expansion of gas inside the casing can be suppressed.
[0011] The present invention [2] includes the battery of the above [1], wherein the laminate cell comprises a cell having a positive electrode layer, a negative electrode layer, and a solid electrolyte layer disposed between the positive electrode layer and the negative electrode layer, a current collector laminated on the cell, a laminate film covering the laminate of the cell and the current collector, and the lead connected to the current collector, at least a portion of which is exposed from the laminate film.
[0012] The present invention [3] includes the battery according to the above [1] or [2], in which the casing is made of metal and the sealing body is made of the insulating porous body.
[0013] With this configuration, the rigidity of the housing makes it possible to suppress expansion of the laminate cell, while the sealing body insulates the leads from the housing.
[0014] The present invention [4] includes the battery of any one of the above [1] to [3], wherein the sealing body has a slit through which the lead passes and is bonded to the inner surface of the opening.
[0015] With this configuration, the battery can be manufactured through a simple process of housing the laminate cell in the casing, inserting the seal into the opening of the casing while passing the leads through the slits, and then adhering the seal to the inner surface of the opening.
[0016] Therefore, the manufacturing efficiency of the battery can be improved. Effect of the Invention
[0017] According to the battery of the present invention, deformation of the casing can be suppressed when the battery is used in a vacuum environment. [Brief description of the drawings]
[0018] [Figure 1] Fig. 1A is a perspective view of a battery according to one embodiment of the present invention, and Fig. 1B is an exploded view of the battery shown in Fig. 1A. [Diagram 2] Fig. 2A is a plan view of the laminate cell shown in Fig. 1B, and Fig. 2B is a cross-sectional view taken along line AA of the laminate cell shown in Fig. 2A. [Diagram 3] Figure 3A is a cross-sectional view showing the layer structure of the cell shown in Figure 2B, and Figure 3B is an enlarged view of the laminate cell shown in Figure 2B. [Figure 4] Fig. 4A is a plan view of the positive electrode current collector shown in Fig. 3B, and Fig. 4B is a cross-sectional view taken along line BB of the positive electrode current collector shown in Fig. 4A. [Diagram 5] FIG. 5 is a cross-sectional view of the laminate cell shown in FIG. 2A taken along line CC. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] 1.Battery 1A and 1B, the battery 1 includes a laminate cell 10, a housing 11, and a sealing body 12. The battery 1 is an all-solid-state battery that uses a solid electrolyte as the electrolyte.
[0020] (1) Laminated cell As shown in FIGS. 2A and 2B, the laminate cell 10 includes a plurality of cells 2, a plurality of current collectors 3, a positive electrode lead 4 as an example of a lead, a negative electrode lead 5 as an example of a lead, and a laminate film 6.
[0021] (1-1) Cell In this embodiment, the cell 2 has a sheet shape. When viewed from the thickness direction of the cell 2, the cell 2 has a substantially rectangular shape. The shape of the cell 2 is not limited. The cell 2 may have a plate shape or a film shape. Also, the cell 2 may have a substantially circular shape when viewed from the thickness direction of the cell 2.
[0022] The thickness of the cell 2 is, for example, 100 μm or more, preferably 200 μm or more, and for example, 1000 μm or less, preferably 800 μm or less.
[0023] As shown in FIG. 3A, the cell 2 has a positive electrode layer 21, a negative electrode layer 22, and a solid electrolyte layer 23. The cell 2 does not have a current collector. The cell 2 is composed of the positive electrode layer 21, the negative electrode layer 22, and the solid electrolyte layer 23. The cell 2 is a bare cell independent of the current collector 3. The cell 2 may be integrated with the current collector 3.
[0024] (1-1-1) Positive electrode layer The positive electrode layer 21 is disposed away from the negative electrode layer 22 in the thickness direction of the cell 2. The positive electrode layer 21 is disposed on the opposite side of the solid electrolyte layer 23 to the negative electrode layer 22 in the thickness direction of the cell 2. The positive electrode layer 21 is in contact with the solid electrolyte layer 23 but is not in contact with the negative electrode layer 22.
[0025] The positive electrode layer 21 is made of a powder containing a positive electrode active material. In this embodiment, the positive electrode layer 21 does not contain a resin such as a binder. In this embodiment, the positive electrode layer 21 is made of a mixture of a powder of the positive electrode active material and a powder of a solid electrolyte. The positive electrode layer 21 does not have to contain a solid electrolyte. The positive electrode layer 21 may be made of only the positive electrode active material.
[0026] The positive electrode active material may be, for example, a lithium-containing oxide. The lithium-containing oxide may, for example, be a lithium-nickel composite oxide (LiNi X M 1-X O2), lithium cobalt oxide (LiCoO2), lithium nickel oxide (LiNiO2), lithium nickel cobalt aluminum oxide (LiNi 0.8 Co 0.15 Al 0.05 O2, NCA-based layered oxide), lithium manganate (spinel-type lithium manganate (LiMn2O4)), and Li-excess composite oxide (Li2MnO3-LiMO2).
[0027] The positive electrode active material is not limited to lithium-containing oxides as long as it is capable of inserting and extracting lithium ions. Examples of the positive electrode active material include olivine compounds (LiMPO4) and sulfur-containing compounds (Li2S).
[0028] In the above chemical formula, M represents a transition metal.
[0029] As the positive electrode active material, from the viewpoint of easily obtaining a high capacity, a lithium-containing oxide containing at least one selected from the group consisting of Co, Ni, and Mn is preferably used.
[0030] In addition, from the viewpoint of improving rate characteristics, the surface of the positive electrode active material may be covered with a coating material.
[0031] Coating materials include, for example, Li4Ti5O 12 , LiTaO3, Li4NbO3, LiAlO2, Li2ZrO3, Li2WO4, Li2TiO3, Li2B4O7, Li3PO4, Li2MoO4, LiBO2, alumina (Al2O3), and carbon (C).
[0032] The positive electrode active materials can be used alone or in combination of two or more kinds.
[0033] The solid electrolyte exhibits lithium ion conductivity. Examples of the solid electrolyte include an organic solid electrolyte and an inorganic solid electrolyte.
[0034] Inorganic solid electrolytes include, for example, sulfides, oxides, nitrides, and hydrides.
[0035] The sulfide may, for example, contain Li2S and another sulfide containing at least one element selected from the group consisting of Group 13 elements, Group 14 elements, and Group 15 elements of the periodic table.
[0036] Examples of Group 13, 14 and 15 elements of the periodic table include P, Si, Ge, As, Sb and Al, preferably P, Si and Ge, and more preferably P.
[0037] Specifically, sulfides include, for example, Li2S-SiS2, Li2S-P2S5, Li2S-GeS2, Li2S-B2S3, Li2S-Ga2S3, Li2S-Al2S3, Li2S-GeS2-P2S5, Li2S-Al2S3-P2S5, Li2S-P2S3, Li2S-P2S3-P2S5, LiX-Li2S-P2S5, LiX-Li2S-SiS2, and LiX-Li2S-B2S3 (X: I, Br, or Cl).
[0038] As the solid electrolyte, preferably, an inorganic solid electrolyte is used, more preferably, a sulfide is used. The solid electrolyte can be used alone or in combination of two or more kinds. The ratio of the positive electrode active material to the solid electrolyte is not limited.
[0039] The positive electrode layer 21 has a thickness of, for example, 50 μm or more, or preferably 100 μm or more. The positive electrode layer 21 has a thickness of, for example, 500 μm or less, or preferably 300 μm or less.
[0040] (1-1-2) Negative electrode layer The negative electrode layer 22 is disposed away from the positive electrode layer 21 in the thickness direction of the cell 2. The negative electrode layer 22 is disposed on the opposite side of the solid electrolyte layer 23 to the positive electrode layer 21 in the thickness direction of the cell 2. The negative electrode layer 22 is in contact with the solid electrolyte layer 23 but is not in contact with the positive electrode layer 21.
[0041] The negative electrode layer 22 is made of a powder containing a negative electrode active material. The negative electrode layer 22 does not contain a resin such as a binder. In this embodiment, the negative electrode layer 22 is made of a mixture of a powder of the negative electrode active material and a powder of a solid electrolyte. The negative electrode layer 22 does not have to contain a solid electrolyte. The negative electrode layer 22 may be made of only the negative electrode active material.
[0042] The negative electrode active material is not limited as long as it is a material capable of inserting and extracting lithium ions. Examples of the negative electrode active material include carbon materials, metals and alloys thereof, semimetals, and compounds of metals or semimetals.
[0043] Examples of carbon materials include graphite (natural graphite, artificial graphite), hard carbon, and amorphous carbon. Examples of metals and their alloys include lithium and its alloys. Examples of metalloids include silicon. Examples of metal or metalloid compounds include oxides, sulfides, nitrides, hydrates, and silicides (lithium silicides) of metals or metalloids. Examples of metal or metalloid oxides include titanium oxide and silicon oxide.
[0044] The negative electrode active material may be used alone or in combination of two or more thereof. For example, silicon oxide and a carbon material may be used in combination as the negative electrode active material.
[0045] Examples of the solid electrolyte contained in the negative electrode layer 22 include the above-mentioned solid electrolytes. Preferably, the solid electrolyte contained in the negative electrode layer 22 is the same as the solid electrolyte contained in the positive electrode layer 21. The ratio of the negative electrode active material to the solid electrolyte is not limited.
[0046] The thickness of the negative electrode layer 22 is approximately the same as the thickness of the positive electrode layer 21. The thickness of the negative electrode layer 22 is, for example, 50 μm or more, or preferably 100 μm or more. The thickness of the negative electrode layer 22 is, for example, 500 μm or less, or preferably 300 μm or less.
[0047] (1-1-3) Solid electrolyte layer The solid electrolyte layer 23 is disposed between the positive electrode layer 21 and the negative electrode layer 22 in the thickness direction of the cell 2. The solid electrolyte layer 23 is made of a powder of a solid electrolyte. The solid electrolyte layer 23 does not contain a resin such as a binder.
[0048] The solid electrolyte may be, for example, any of the solid electrolytes described above. Preferably, the solid electrolyte is the same as the solid electrolyte contained in the positive electrode layer 21.
[0049] The solid electrolyte layer 23 is thinner than the positive electrode layer 21 and the negative electrode layer 22. The solid electrolyte layer 23 has a thickness of, for example, 10 μm or more, or preferably 30 μm or more. The solid electrolyte layer 23 has a thickness of, for example, 300 μm or less, or preferably 100 μm or less.
[0050] (1-2) Current collector As shown in FIG. 3B, the current collector 3 is stacked on the cell 2. Specifically, each of the multiple current collectors 3 is stacked alternately with each of the multiple cells 2. The multiple current collectors 3 include a positive electrode current collector 3A and a negative electrode current collector 3B. The positive electrode current collector 3A contacts the positive electrode layer 21 of the cell 2. The negative electrode current collector 3B contacts the negative electrode layer 22 of the cell 2.
[0051] Specifically, in this embodiment, the positive electrode current collector 3A, the first cell 2A, the negative electrode current collector 3B, the second cell 2B, and the positive electrode current collector 3A are stacked in this order from one side to the other side in the stacking direction of the cells 2 and the current collectors 3. In the stacking direction, one negative electrode current collector 3B is disposed between the negative electrode layer 22 of the first cell 2A and the negative electrode layer 22 of the second cell 2B. In other words, one current collector 3 is disposed between two cells 2 in the stacking direction.
[0052] As shown in FIGS. 4A and 4B, the current collector 3 has a conductor 31, an insulating member 32, and an adhesive layer 33.
[0053] (1-2-1) Conductors The conductor 31 is made of, for example, a metal and has a laminated portion 311 and a tab 312.
[0054] The laminated portion 311 extends in a first direction and a second direction. The first direction is perpendicular to the lamination direction. The second direction is perpendicular to both the first direction and the lamination direction. The laminated portion 311 has a sheet shape. The laminated portion 311 has one side S1 and the other side S2 in the thickness direction. In other words, the conductor 31 has one side S1 and the other side S2 in the thickness direction. The laminated portion 311 contacts the cell 2. When the current collector 3 is a positive electrode collector 3A, the laminated portion 311 contacts the positive electrode layer 21 of the cell 2. When the current collector 3 is a negative electrode collector 3B, the laminated portion 311 contacts the negative electrode layer 22 of the cell 2. The laminated portion 311 has a substantially rectangular shape when viewed from the lamination direction. The laminated portion 311 has a plurality of edges E1, E2, E3, and E4.
[0055] Edge E1 is disposed at one end of stacked portion 311 in the first direction. Edge E1 extends in the second direction. Edge E1 has a straight line shape. Edge E2 is disposed at the other end of stacked portion 311 in the first direction. Edge E2 extends in the second direction. Edge E2 has a straight line shape. Edge E3 is disposed at one end of stacked portion 311 in the second direction. Edge E3 extends in the first direction. Edge E3 has a straight line shape. Edge E4 is disposed at the other end of stacked portion 311 in the second direction. Edge E4 extends in the first direction. Edge E4 has a straight line shape.
[0056] The tab 312 is disposed on an edge of the laminated portion 311. In this embodiment, the tab 312 is disposed on an edge E3 on one side of the laminated portion 311 in the second direction. The tab 312 protrudes from the edge E3 of the laminated portion 311. The tab 312 may be a member separate from the laminated portion 311 and joined to the laminated portion 311. The tab 312 has a belt shape. The tab 312 does not contact the cell 2. When the current collector 3 is a positive electrode current collector 3A, the conductor 31 has a positive electrode tab 312A as the tab 312. When the current collector 3 is a negative electrode current collector 3B, the conductor 31 has a negative electrode tab 312B as the tab 312. In a state in which the cell 2, the positive electrode current collector 3A, and the negative electrode current collector 3B are stacked, the negative electrode tab 312B is disposed away from the positive electrode tab 312A. In a state in which the cell 2, the positive electrode current collector 3A, and the negative electrode current collector 3B are stacked, the negative electrode tab 312B does not overlap the positive electrode tab 312A in the stacking direction.
[0057] The thickness of the conductor 31 is, for example, 1 μm or more, preferably 5 μm or more, and for example, 100 μm or less, preferably 50 μm or less.
[0058] Examples of materials for the conductor 31 include copper (Cu), magnesium (Mg), stainless steel, titanium (Ti), iron (Fe), cobalt (Co), nickel (Ni), zinc (Zn), aluminum (Al), germanium (Ge), indium (In), lithium (Li), tin (Sn), and alloys thereof.
[0059] (1-2-2) Insulating materials As shown in FIG. 4B, the insulating member 32 is laminated on one surface S1 of the conductor 31. As shown in FIG. 4A, the insulating member 32 is disposed on the laminated portion 311 of the conductor 31. The insulating member 32 is laminated on the peripheral portion of the laminated portion 311 of the conductor 31. The insulating member 32 has a substantially rectangular frame shape when viewed from the lamination direction. The insulating member 32 has a portion 32A extending along the edge E1 of the conductor 31, a portion 32B extending along the edge E2 of the conductor 31, a portion 32C extending along the edge E3 of the conductor 31, and a portion 32D extending along the edge E4 of the conductor 31. The insulating member 32 is not disposed on the tab 312 of the conductor 31.
[0060] When the cell 2, the positive electrode current collector 3A, and the negative electrode current collector 3B are stacked, the insulating member 32 is disposed around the cell 2. As shown in Fig. 3B, when the cell 2, the positive electrode current collector 3A, and the negative electrode current collector 3B are stacked, the insulating member 32 is disposed between the positive electrode current collector 3A and the negative electrode current collector 3B in the stacking direction. When the cell 2, the positive electrode current collector 3A, and the negative electrode current collector 3B are stacked, the insulating member 32 insulates the positive electrode current collector 3A from the negative electrode current collector 3B.
[0061] In the stacking direction, the thickness of the insulating member 32 is thinner than the thickness of the cell 2. When the current collector 3 does not have the adhesive layer 33, the thickness of the insulating member 32 may be the same as the thickness of the cell 2. The thickness of the insulating member 32 is, for example, 50 μm or more, preferably 75 μm or more, and for example, 500 μm or less, preferably 400 μm or less.
[0062] Examples of materials for the insulating member 32 include polyethylene terephthalate and polyimide.
[0063] (1-2-3) Adhesive layer As shown in Fig. 4B, the adhesive layer 33 is laminated on the other surface S2 of the conductor 31 at the peripheral portion of the conductor 31. The current collector 3 does not need to have the adhesive layer 33. As shown in Fig. 3B, in a state in which one cell 2 is laminated between two current collectors 3, the adhesive layer 33 of the current collector 3 arranged on the other side of the cell 2 in the stacking direction is adhered to the insulating member 32 of the current collector 3 arranged on one side of the cell 2 in the stacking direction.
[0064] The sum of the thickness of the adhesive layer 33 and the thickness of the insulating member 32 is not more than the thickness of the cell 2. The thickness of the adhesive layer 33 is, for example, 30 μm or more, preferably 50 μm or more, and for example, 300 μm or less, preferably 200 μm or less.
[0065] The adhesive layer 33 is preferably insulating. Examples of the material for the adhesive layer 33 include resins such as acrylic, polyimide, and silicone, and nonwoven fabrics impregnated with these resins.
[0066] (1-3) Positive and negative leads As shown in Fig. 2A, a portion of the positive electrode lead 4 is exposed from the laminate film 6. As shown in Fig. 5, the positive electrode lead 4 is joined to a positive electrode tab 312A within the laminate film 6. This allows the positive electrode lead 4 to be electrically connected to the positive electrode current collector 3A. The positive electrode lead 4 is not connected to the negative electrode current collector 3B.
[0067] As shown in Fig. 2A, a portion of the negative electrode lead 5 is exposed from the laminate film 6. The negative electrode lead 5 is joined to the negative electrode tab 312B (see Fig. 4A) within the laminate film 6. This allows the negative electrode lead 5 to be electrically connected to the negative electrode current collector 3B (see Fig. 2B). The negative electrode lead 5 is not connected to the positive electrode current collector 3A.
[0068] Each of the positive electrode lead 4 and the negative electrode lead 5 has, for example, a substantially rectangular flat plate shape. Examples of the material of the positive electrode lead 4 and the negative electrode lead 5 include pure metals and alloys. Examples of the pure metals include copper, nickel, aluminum, gold, and platinum. Examples of the alloys include alloys of the above-mentioned pure metals, stainless steel, and titanium. The positive electrode lead 4 and the negative electrode lead 5 may be plated. For example, the positive electrode lead 4 and the negative electrode lead 5 may be copper plates having a nickel plating layer and a gold plating layer.
[0069] (1-4) Laminate film 2A and 2B, the laminate film 6 covers the laminate of the cells 2 and the current collector 3. The laminate of the cells 2 and the current collector 3 is vacuum laminated. An example of the laminate film 6 is a metal laminate film in which a resin film is laminated on both sides of a metal foil.
[0070] (2) Housing As shown in FIG. 1B, the housing 11 houses the laminate cell 10. The housing 11 extends in the second direction. The housing 11 has a cylindrical shape. The shape of the housing 11 is not limited as long as it can house the laminate cell 10. The housing 11 suppresses the expansion of the laminate cell 10. The housing 11 is made of, for example, a metal. Examples of metals include aluminum and stainless steel.
[0071] The housing 11 has an opening 111. The opening 111 is located at one end of the housing 11 in the second direction. As shown in Fig. 1A, when the laminate cell 10 is housed in the housing 11, the positive electrode lead 4 and the negative electrode lead 5 extend through the opening 111 to the outside of the housing 11.
[0072] (3) Sealing body As shown in Fig. 1A, the sealing body 12 is located in the opening 111. The sealing body 12 is adhered to the inner surface of the opening 111. In this way, the sealing body 12 seals the opening 111 of the housing 11. The sealing body 12 is made of a porous body. The porous body has air permeability and is insulating. Examples of the porous body include a fluororubber sponge and a silicone sponge.
[0073] As shown in FIG. 1B, the sealing body 12 has two slits 121A and 121B. The slits 121A and 121B are aligned in a first direction. The slit 121B is located away from the slit 121A in the first direction. Each of the slits 121A and 121B extends in the first direction. As shown in FIG. 1A, the positive electrode lead 4 passes through the slit 121A. The negative electrode lead 5 passes through the slit 121B. The slits 121A and 121B may be connected to each other.
[0074] 2. Effects (1) In battery 1, sealing body 12 that seals opening 111 of housing 11 is made of a porous material that has air permeability.
[0075] Therefore, when the battery 1 is used in a vacuum environment, the gas inside the housing 11 passes through the sealing body 12 and is discharged to the outside of the housing 11 .
[0076] As a result, when the battery 1 is used in a vacuum environment, deformation of the casing 11 due to expansion of the gas inside the casing 11 can be suppressed.
[0077] (2) In battery 1, casing 11 is made of metal, and sealing body 12 is made of an insulating porous body.
[0078] Therefore, the expansion of the laminate cell 10 can be suppressed by the rigidity of the case 11, while the positive electrode lead 4 and the negative electrode lead 5 can be insulated from the case 11 by the sealing body 12.
[0079] (3) In battery 1, as shown in FIG. 1A, sealing body has slit 121A through which positive electrode lead 4 passes and slit 121B through which negative electrode lead 5 passes, and is adhered to the inner surface of opening 111.
[0080] Therefore, the battery 1 can be manufactured through a simple process of housing the laminate cell 10 in the housing 11, passing the positive electrode lead 4 through the slit 121A and the negative electrode lead 5 through the slit 121B, inserting the sealing body 12 into the opening 111 of the housing 11, and adhering the sealing body 12 to the inner surface of the opening 111.
[0081] Therefore, the manufacturing efficiency of the battery 1 can be improved. [Explanation of symbols]
[0082] 1 battery 2 Cell 21 Positive electrode layer 22 Negative electrode layer 23 Solid electrolyte layer 3 Current collector 4 Positive lead (example of lead) 5 Negative lead (example of lead) 6. Laminating film 10 Laminated Cell 11. Cabinet 111 Aperture 12 Sealing body 121A Slit 121B Slit
Claims
1. a laminate cell having leads; a housing having an opening through which the lead passes and housing the laminate cell; a sealing body made of a porous body having air permeability and sealing the opening of the housing; Equipped with a battery.
2. The laminate cell comprises: a cell having a positive electrode layer, a negative electrode layer, and a solid electrolyte layer disposed between the positive electrode layer and the negative electrode layer; A current collector laminated on the cell; a laminate film covering the stack of the cells and the current collector; the lead connected to the current collector and at least a portion of which is exposed from the laminate film; 10. The battery of claim 1 , comprising:
3. The housing is made of metal; The battery of claim 1 , wherein the sealing body is made from the insulating porous body.
4. The battery according to claim 1 , wherein the sealing body has a slit through which the lead passes and is adhered to an inner surface of the opening.
Citation Information
Patent Citations
Manufacturing method of secondary battery
JP2022081801A