Semiconductor device manufacturing method

The method addresses reliability and yield issues in semiconductor device manufacturing by forming protective films and using CMP to maintain insulating film thickness, enhancing the reliability and yield of three-dimensional memory structures.

JP7551433B2Active Publication Date: 2024-09-17KIOXIA CORP
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2020168325
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-05
Publication Date
2024-09-17
Estimated Expiration
2040-10-05

AI Technical Summary

Technical Problem

Existing methods for manufacturing semiconductor devices face challenges in ensuring the reliability and yield of the devices due to issues such as particle generation, roll-off regions, and defocusing during photolithography processes, particularly in the formation of three-dimensional memory structures.

Method used

A method involving the formation of a multilayer film with alternating first and second films, followed by partial removal to create laminates and recesses, and the application of protective films to cover the edges, along with chemical mechanical polishing (CMP) to maintain a sufficient insulating film thickness, thereby preventing roll-off regions and defocusing.

Benefits of technology

The method enhances the reliability and yield of semiconductor devices by suppressing particle generation, roll-off formation, and defocusing, resulting in a highly reliable semiconductor device with improved manufacturing consistency.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

To provide a semiconductor device with high reliability.SOLUTION: A manufacturing method for a semiconductor device includes the steps of: forming a multilayer film by stacking first films and second films alternately on a surface of a semiconductor substrate; forming a plurality of laminate bodies and a concave part between one of the laminate bodies and another one of the laminate bodies by removing the multilayer film partially and exposing an end part of the surface; forming a first insulating film filling the concave part; forming a first protection film on the laminate bodies, the first insulating film, and the end part; forming a second insulating film overlapping with at least a part of the other one of the laminate bodies and the end part on the first protection film; and removing partially the second insulating film along a thickness direction using chemical mechanical polishing.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] An embodiment of the present invention relates to a method for manufacturing a semiconductor device. [Background technology]

[0002] 2. Description of the Related Art In a known method for manufacturing a semiconductor device such as a three-dimensional memory, a semiconductor device is manufactured by bonding a first semiconductor substrate having memory cells to a second semiconductor substrate having peripheral circuits. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] US Patent Application Publication No. 2017 / 0077122 [Patent Document 2] U.S. Pat. No. 1,052,9233 Summary of the Invention [Problem to be solved by the invention]

[0004] One of the problems to be solved by the present invention is to provide a semiconductor device having high reliability. [Means for solving the problem]

[0005] A manufacturing method of a semiconductor device according to an embodiment includes the steps of forming a multilayer film by alternately stacking first and second films on a surface of a semiconductor substrate, partially removing the multilayer film to form a plurality of laminates and a recess between one of the plurality of laminates and another of the plurality of laminates, and exposing an edge of the surface, forming a first insulating film that fills the recess, forming a first protective film on the plurality of laminates, the first insulating film, and the edge, forming a second insulating film on the first protective film that overlaps at least a portion of the other one of the plurality of laminates and the edge, and partially removing the second insulating film along a thickness direction using chemical mechanical polishing. [Brief description of the drawings]

[0006] [Figure 1] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Diagram 2] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Diagram 3] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 4] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Diagram 5] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 6] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 7] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 8] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 9] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 10] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 11] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 12] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 13] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 14] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 15] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 16] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 17] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 18] 3A to 3C are schematic cross-sectional views for explaining an example of a manufacturing method of the semiconductor device according to the first embodiment. [Figure 19] FIG. 2 is a schematic diagram showing an example of the structure of a semiconductor device manufactured without forming a protective film 11 and a protective film 14. [Figure 20] 6A to 6C are diagrams for explaining an example of a manufacturing method of the semiconductor device according to the second embodiment. [Figure 21] 6A to 6C are diagrams for explaining an example of a manufacturing method of the semiconductor device according to the second embodiment. [Figure 22] 6A to 6C are diagrams for explaining an example of a manufacturing method of the semiconductor device according to the second embodiment. [Figure 23] 6A to 6C are diagrams for explaining an example of a manufacturing method of the semiconductor device according to the second embodiment. [Figure 24] 6A to 6C are diagrams for explaining an example of a manufacturing method of the semiconductor device according to the second embodiment. [Diagram 25] 6A to 6C are diagrams for explaining an example of a manufacturing method of the semiconductor device according to the second embodiment. [Figure 26] 6A to 6C are diagrams for explaining an example of a manufacturing method of the semiconductor device according to the second embodiment. [Figure 27] 13A to 13C are diagrams for explaining an example of a manufacturing method of the semiconductor device according to the third embodiment. [Figure 28] 13A to 13C are diagrams for explaining an example of a manufacturing method of the semiconductor device according to the third embodiment. [Figure 29] 13A to 13C are diagrams for explaining an example of a manufacturing method of the semiconductor device according to the third embodiment. [Diagram 30] 13A to 13C are diagrams for explaining an example of a manufacturing method of the semiconductor device according to the third embodiment. [Diagram 31] 13A to 13C are diagrams for explaining an example of a manufacturing method of the semiconductor device according to the fourth embodiment. [Diagram 32] 13A to 13C are diagrams for explaining an example of a manufacturing method of the semiconductor device according to the fourth embodiment. [Diagram 33] FIG. 2 is a schematic diagram showing a structural example of a semiconductor device in which a semiconductor substrate 1, which is manufactured without forming a protective film 11 and a protective film 14, is bonded to a semiconductor substrate 23. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0007] Hereinafter, the embodiments will be described with reference to the drawings. The relationship between the thickness and planar dimensions of each component, the thickness ratio of each component, etc. shown in the drawings may differ from the actual product. In addition, in the embodiments, substantially the same components are given the same reference numerals and the description will be omitted as appropriate.

[0008] (First embodiment) 1 to 18 are schematic cross-sectional views for explaining an example of a manufacturing method for a semiconductor device according to the first embodiment, and show a part of an XZ cross section including an X axis of a semiconductor substrate 1 and a Z axis orthogonal to the X axis and orthogonal to a Y axis orthogonal to the X axis.

[0009] 1, a multilayer film 2 is formed on a surface 1a of a semiconductor substrate 1, and a protective film 3 is formed on the multilayer film 2. Note that another layer may be provided between the surface 1a and the multilayer film 2.

[0010] An example of the semiconductor substrate 1 includes a silicon wafer. An example of the multilayer film 2 is formed by alternately stacking a first film, such as a silicon oxide film having a thickness of 25 nm, and a second film, such as a silicon nitride film having a thickness of 25 nm. The second film is a sacrificial layer. The sacrificial layer is a region in which a conductive layer will be formed later. The number of layers of the first film and the second film is not particularly limited.

[0011] The protective film 3 is provided to protect the multilayer film 2 against, for example, etching. An example of the protective film 3 includes a silicon nitride film having a thickness of 100 nm.

[0012] 2, the multilayer film 2 and the protective film 3 are partially removed to form a plurality of stacked bodies 2a and a recess 2b provided between one of the plurality of stacked bodies 2a and another one of the plurality of stacked bodies 2a and adjacent to the stacked body 2a. The stacked body 2a is a region where memory cells of the three-dimensional memory are formed.

[0013] By partially removing the multilayer film 2, a staircase region A for forming contacts between a conductive layer to be formed later and other wiring is formed in the laminate 2a. The staircase region A is formed, for example, by forming a resist mask on the multilayer film 2 and alternately switching between a process of partially removing the first film and the second film by anisotropic etching and a process of shrinking the resist mask by isotropic etching. At this time, the multilayer film 2 is also removed in a region B between a pair of staircase regions A. A peripheral circuit for a three-dimensional memory may be formed in region B.

[0014] The formation of the laminate 2a and the recess 2b is performed together with the multilayer edge cut, which exposes the edge of the surface 1a of the semiconductor substrate 1 by partially removing the multilayer film 2, as shown in FIG. 2. The multilayer edge cut exposes the edge of the surface 1a of the semiconductor substrate 1 by partially removing the multilayer film 2 from the multilayer edge cut end X on the top surface of the laminate 2a on the most end side toward the edge of the surface 1a of the semiconductor substrate 1. This makes it possible to suppress the generation of particles at the edge of the surface 1a. The width of the laminate 2a on the most end side may be shorter than the width of the other laminates 2a. The length from the edge of the semiconductor substrate 1 to the multilayer edge cut end X is not particularly limited, but is, for example, 1.5 mm or more and 3.0 mm or less. The laminate 2a on the most end side may be provided in plurality along the periphery of the surface 1a.

[0015] Next, as shown in Fig. 3, an insulating film 4 is formed on the multiple stacked bodies 2a, the recesses 2b, and the ends of the surface 1a. The insulating film 4 is a buried insulating film that fills the recesses 2b. An example of the insulating film 4 includes a silicon oxide film having a thickness of 3.3 µm.

[0016] By photolithography and etching, a region of the insulating film 4 on the protective film 3 is removed in the memory cell formation region C overlapping the stacked body 2a. At this time, in order to prevent generation of particles at the end of the surface 1a, edge cut of the insulating film 4 is simultaneously performed at the insulating film edge cut end Y that is closer to the end than the multilayer film edge cut end X, as shown in Fig. 4. At this time, in the region D between the multilayer film edge cut end X and the insulating film edge cut end Y, the insulating film 4 is removed even though the multilayer film 2 has been removed in the memory cell formation region C.

[0017] 5, an insulating film 5 is formed on the stack 2a, the insulating film 4, and the end of the surface 1a. The insulating film 5 is provided, for example, to thicken the insulating film on the protective film 3. An example of the insulating film 5 includes a silicon oxide film having a thickness of 500 nm.

[0018] 6, the insulating film 5 is partially removed in the thickness direction (Z-axis direction) by CMP until the region of the insulating film 5 on the stacked body 2a has a thickness of, for example, 200 nm, thereby planarizing the upper surface of the insulating film 5. However, the present invention is not limited to this, and the insulating film 5 may be partially removed until the upper surface of the protective film 3 is exposed.

[0019] 7, the region of the insulating film 5 on the stack 2a and the protective film 3 are removed to expose the upper surface of the stack 2a. The region of the insulating film 5 on the stack 2a and the protective film 3 can be removed by using, for example, dry etching.

[0020] 8, a protective film 11 is formed on the stacked body 2a, the insulating film 4 embedded in the recess 2b, and the insulating film 5 at the end of the surface 1a. The protective film 11 is provided to protect the stacked body 2a, the insulating film 4, and the insulating film 5 against processing using, for example, CMP. An example of the protective film 11 includes a 100 nm silicon nitride film.

[0021] 9, an insulating film 12 is formed on the protective film 11. The insulating film 12 overlaps the edge of the front surface 1a of the semiconductor substrate 1 and the stacked body 2a. An example of the insulating film 12 includes a silicon oxide film having a thickness of 3.0 μm.

[0022] Next, as shown in FIG. 10, a mask is formed on the surface of the protective film 11 from the region overlapping the end of the surface 1a to the region inside the multilayer film edge cut end X, and then an etching process is performed to remove the insulating film 12 on the protective film 11 while leaving the insulating film 12 on at least a portion of one of the laminates 2a and on the end of the surface 1a.

[0023] Next, as shown in FIG. 11, an insulating film 13 is formed on the protective film 11 and the insulating film 12, and a protective film 14 is formed that overlaps the end of the surface 1a on the end side from the multilayer film edge cut end X, but does not overlap the laminate 2a. An example of the insulating film 13 includes a silicon oxide film having a thickness of 100 nm. The protective film 14 is provided to protect the insulating film 12 and the insulating film 13 against processing using CMP, for example. An example of the protective film 14 includes a silicon nitride film having a thickness of 100 nm. Note that it is preferable that the height of a part of the upper surface of the protective film 14 with respect to the surface 1a of the semiconductor substrate 1 is the same as the height of a part of the upper surface of the protective film 11.

[0024] The protective film 14 is formed, for example, by forming a film such as a silicon nitride film on the entire surface of the insulating film 13, forming a resist film only on the edge of the surface 1a, and removing the center of the film by dry etching. At this time, the protective film 11 is not removed because it is covered by the insulating film 13. The protective film 14 can also be formed by a film forming device capable of forming a film only on the edge of the surface 1a, in which case the insulating film 13 may be omitted.

[0025] 12, an insulating film 15 is formed on the insulating film 13 and the protective film 14. The insulating film 15 is provided, for example, to thicken the insulating film on the protective film 11. An example of the insulating film 15 includes a silicon oxide film having a thickness of 200 nm.

[0026] 13, the insulating films 12, 13, and 15 are partially removed in the thickness direction (Z-axis direction) by using CMP until, for example, a part of the upper surface of the protective film 11 and a part of the upper surface of the protective film 14 are exposed. At this time, small dishing 16 may occur between the protective film 11 and the protective film 14 in the exposed portion of the upper surface of the insulating film 12.

[0027] Next, the protective film 11 and the protective film 14 on the laminate 2a are removed to expose the upper surface of the laminate 2a, as shown in Fig. 14. The protective film 11 and the protective film 14 are removed by using, for example, dry etching.

[0028] 15 is an enlarged view of a portion of the staircase region A and the memory cell formation region C. Next, as shown in FIG. 15, a memory hole 7 is formed penetrating a stack 2a of a first film 201 such as a silicon oxide film and a second film 202 such as a silicon nitride film, and a memory layer 8 is formed in the memory hole 7. The memory layer 8 includes a block insulating film 81, a charge storage film 82, a tunnel insulating film 83, a semiconductor layer 84, and a core insulating layer 85.

[0029] The block insulating film 81, the tunnel insulating film 83, and the core insulating layer 85 include, for example, silicon oxide. The charge storage film 82 includes, for example, silicon nitride. The semiconductor layer 84 includes, for example, polysilicon.

[0030] A block insulating film 81, a charge storage film 82, and a tunnel insulating film 83 are sequentially stacked on the side surface of the memory hole 7. A semiconductor layer 84 is formed so as to penetrate the stacked body 2a and have its side surface in contact with the tunnel insulating film 83. The semiconductor layer 84 is in contact with the front surface 1a of the semiconductor substrate 1, and is connected to a source line (not shown) via the semiconductor substrate 1. A core insulating layer 85 is provided inside the semiconductor layer 84. The core insulating layer 85 extends along the semiconductor layer 84.

[0031] 16 shows an enlarged view of a portion of the staircase region A and the memory cell formation region C. Next, as shown in FIG. 16, the second film 202 is removed to form a cavity, and a conductive layer 202a is formed in the cavity. The conductive layer 202a constitutes the word line of the memory cell. An example of the conductive layer 202a includes a metal layer.

[0032] 17 shows an enlarged view of a portion of the staircase region A and the memory cell formation region C. Next, as shown in Fig. 17, a contact layer 9 is formed. The contact layer 9 includes a contact plug connected to the conductive layer 202a in the staircase region A and a contact plug connected to the memory layer 8 in the memory cell formation region C. Furthermore, a bit line is provided on the upper part of the contact plug in the memory cell formation region C.

[0033] 18, the wiring layer 10 is formed on the contact layer 9. The step caused by the dishing 16 is flattened in the CMP process when the contact layer 9 and the wiring layer 10 are formed.

[0034] As described above, in the example manufacturing method of the semiconductor device of this embodiment, by forming protective film 11 and protective film 14 that overlap the end portion of surface 1a of semiconductor substrate 1, an insulating film of sufficient thickness can be formed on the end portion of surface 1a of semiconductor substrate 1.

[0035] 19 is a schematic diagram showing a structural example of a semiconductor device manufactured without forming protective film 11 and protective film 14. If protective film 11 and protective film 14 are not formed, the insulating film at the end of surface 1a of semiconductor substrate 1 is largely removed. In this case, if CMP is performed in the process of forming contact layer 9 and wiring layer 10, pressure is concentrated at multilayer film edge cut end X, and roll-off region E is formed. If roll-off region E is formed, defocus occurs during exposure in the photolithography process when contact layer 9 and wiring layer 10 are formed in the subsequent process, and the yield at the end of semiconductor substrate 1 decreases.

[0036] In contrast, in the method for manufacturing a semiconductor device according to the present embodiment, by forming the protective film 11 and the protective film 14, the insulating film 12 can be left outside the multilayer film edge cut end X. This makes it possible to suppress the formation of the roll-off region E in the subsequent CMP process and to suppress a decrease in yield due to defocus in the photolithography process. In addition, by forming the protective film 11, dishing in the CMP process can be suppressed. Therefore, a semiconductor device with high reliability can be provided.

[0037] Second embodiment 20 to 26 are diagrams for explaining an example of a manufacturing method of the semiconductor device according to the second embodiment. Note that, for the same parts as those in the first embodiment, the explanation of the first embodiment can be appropriately applied, and therefore the explanation will be omitted here.

[0038] First, similar to the example of the manufacturing method of the semiconductor device according to the first embodiment, the same steps as those shown in Fig. 1 to Fig. 7 are performed. Here, as an example, as shown in Fig. 20, the protective film 3 on the laminate 2a is left without being removed. In addition, the recess 2b, the staircase region A, and the region B are formed with a narrower width than those in the first embodiment. In addition, the interval F between adjacent protective films 3 is also formed narrower.

[0039] 21, an insulating film 12 is formed on the protective film 3, the insulating film 4, and the insulating film 5. An example of the insulating film 12 includes a silicon oxide film having a thickness of, for example, 2.9 μm.

[0040] 22, a protective film 14 is formed on the edge side of the multilayer film edge cut edge X so as to overlap the edge of the surface 1a but not overlap the laminate 2a. The protective film 14 is provided to protect a part of the insulating film 12 against processing using CMP, for example. An example of the protective film 14 includes a silicon nitride film having a thickness of 100 nm. Note that it is preferable that the height of a part of the upper surface of the protective film 14 with respect to the surface 1a of the semiconductor substrate 1 is the same as the height of a part of the upper surface of the protective film 3.

[0041] 23, an insulating film 15 is formed on the protective film 14 and the insulating film 12. An example of the insulating film 15 includes a silicon oxide film having a thickness of, for example, 300 nm.

[0042] 24, CMP is used to partially remove the insulating film 12 along the thickness direction (Z-axis direction) until, for example, the upper surfaces of the protective film 3 and the protective film 14 are exposed. At this time, dishing 17 occurs in the exposed portion of the insulating film 12 between the protective film 3 and the protective film 14, and dishing 18 also occurs in the exposed portion of the insulating film 12 between adjacent protective films 3. However, by narrowing the interval F between adjacent protective films 3, dishing 18 can be reduced.

[0043] Next, as shown in Fig. 25, the protective film 3 and the protective film 14 on the laminate 2a are removed to expose the upper surface of the laminate 2a. Thereafter, as shown in Fig. 26, the memory hole 7, the memory layer 8, the contact layer 9, and the wiring layer 10 are formed in the same manner as in the first embodiment. The steps caused by the dishing 17 and the dishing 18 are flattened in the CMP process when the contact layer 9 and the wiring layer 10 are formed in the same manner as in the first embodiment.

[0044] As described above, in the example manufacturing method of the semiconductor device of this embodiment, by forming a protective film 14 that overlaps the edge of the surface 1a of the semiconductor substrate 1, an insulating film of sufficient thickness can be formed on the edge of the surface 1a of the semiconductor substrate 1.

[0045] If the protective film 14 is not formed, the insulating film at the edge of the surface 1a of the semiconductor substrate 1 will be largely removed. In this case, if CMP is performed in the process of forming the contact layer 9 and the wiring layer 10, pressure will be concentrated at the multilayer film edge cut edge X, forming a roll-off region E. If the roll-off region E is formed, defocus will occur during exposure in the photolithography process when the contact layer 9 and the wiring layer 10 are formed in the subsequent process, and the yield at the edge of the semiconductor substrate 1 will decrease.

[0046] In contrast, in the semiconductor device manufacturing method of the present embodiment, by forming the protective film 14, it is possible to leave an insulating film of sufficient thickness outside the multilayer film edge cut end X. This makes it possible to suppress the formation of the roll-off region E in the subsequent CMP process and to suppress a decrease in yield due to defocus in the photolithography process. Therefore, it is possible to provide a semiconductor device with high reliability.

[0047] Furthermore, by making the interval F between adjacent stacked bodies 2a and protective films 3 sufficiently narrow, it is possible to form only protective film 14 without forming protective film 11, thereby achieving the same effect as the manufacturing method of the first embodiment with fewer steps compared to the manufacturing method of the first embodiment. Note that, in order to reduce the step caused by dishing 18 to a level that can be flattened when forming contact layer 9 and wiring layer 10, it is preferable that the interval F between adjacent protective films 3 is 500 μm or less.

[0048] This embodiment can be appropriately combined with other embodiments.

[0049] (Third embodiment) 27 to 30 are diagrams for explaining an example of a manufacturing method of a semiconductor device according to the third embodiment. Note that, for the same parts as those in the first embodiment, the explanation of the first embodiment can be appropriately applied, and therefore the explanation will be omitted here.

[0050] 1 to 10 of the first embodiment are performed in the same manner as in the first embodiment. Next, as shown in Fig. 27, an insulating film 15 is formed on the insulating film 12 and the protective film 11. An example of the insulating film 15 includes a silicon oxide film having a thickness of, for example, 250 nm.

[0051] 28, the insulating film 12 and the insulating film 15 are partially removed in the thickness direction (Z-axis direction) by using CMP until, for example, a part of the upper surface of the protective film 11 is exposed. At this time, since a part of the insulating film 12 remains at the end of the surface 1a of the semiconductor substrate, the steep step existing on the end side of the multilayer film edge cut end X is mitigated.

[0052] Next, as shown in Fig. 29, the protective film 11 is partially removed to expose the upper surface of the stacked body 2a. The protective film 11 is removed by, for example, dry etching. Thereafter, as shown in Fig. 30, the memory hole 7, the memory layer 8, the contact layer 9, and the wiring layer 10 are formed in the same manner as in the first embodiment.

[0053] As described above, in the example manufacturing method of the semiconductor device of this embodiment, by forming the protective film 11 overlapping the edge of the surface 1a of the semiconductor substrate 1, an insulating film of sufficient thickness can be formed on the edge of the surface 1a of the semiconductor substrate 1.

[0054] If the protective film 11 is not formed, the insulating film at the edge of the surface 1a of the semiconductor substrate 1 will be largely removed. In this case, if CMP is performed in the process of forming the contact layer 9 and the wiring layer 10, pressure will be concentrated at the multilayer film edge cut edge X, forming a roll-off region E. If the roll-off region E is formed, defocus will occur during exposure in the photolithography process when the contact layer 9 and the wiring layer 10 are formed in the subsequent process, and the yield at the edge of the semiconductor substrate 1 will decrease.

[0055] In contrast, in the semiconductor device manufacturing method of the present embodiment, by forming the protective film 11, it is possible to leave the insulating film outside the multilayer film edge cut end X. This makes it possible to suppress the formation of the roll-off region E in the subsequent CMP process and to suppress a decrease in yield due to defocus in the photolithography process. Furthermore, by forming the protective film 11, it is possible to suppress dishing in the CMP process. Therefore, it is possible to provide a semiconductor device with high reliability.

[0056] Furthermore, by forming only the protective film 11 without forming the protective film 14, it is possible to achieve at least a part of the effects of the first embodiment with fewer steps than in the first embodiment.

[0057] This embodiment can be appropriately combined with other embodiments.

[0058] (Fourth embodiment) 31 and 32 are diagrams for explaining an example of a method for manufacturing the semiconductor device of the fourth embodiment. In the example of the method for manufacturing the semiconductor device of the fourth embodiment, as an example, a memory hole 7, a memory layer 8, a contact layer 9, and a wiring layer 10 are formed in a semiconductor substrate 1 through the steps shown in FIG. 1 to FIG. 18 of the first embodiment.

[0059] 31, a connection pad 19 that is connected to the wiring layer 10 is formed on the wiring layer 10. Without being limited to this, the semiconductor device may be manufactured using the manufacturing method of the second and third embodiments.

[0060] 32, a semiconductor substrate 23 is prepared, which includes an element 20 constituting a peripheral circuit such as a CMOS circuit, a wiring layer 21 provided on the element 20 and connected to the element 20, and a connection pad 22 provided on the wiring layer 21 and connected to the wiring layer 21. Thereafter, the semiconductor substrate 1 and the semiconductor substrate 23 are bonded together with the connection pad 19 facing the connection pad 22, thereby electrically connecting the memory layer 8 of the semiconductor substrate 1 and the element 20 of the semiconductor substrate 23.

[0061] In an example of a manufacturing method for a semiconductor device of this embodiment, a semiconductor substrate 1 manufactured using the manufacturing method of the first, second, or third embodiment is bonded to a semiconductor substrate 23 to manufacture a semiconductor device.

[0062] 33 is a schematic diagram showing a structural example of a semiconductor device in which a semiconductor substrate 23 is bonded to a semiconductor substrate 1 manufactured without forming the protective film 11 and the protective film 14. If the protective film 11 and the protective film 14 are not formed, the insulating film at the end of the surface 1a of the semiconductor substrate 1 is largely removed. In this case, if CMP is performed in the process of forming the contact layer 9 and the wiring layer 10, pressure is concentrated at the multilayer film edge cut end X, and a roll-off region E is formed. As a result, an unbonded region G is formed at the end of the semiconductor substrate 1. This causes a decrease in the reliability of the semiconductor device.

[0063] In contrast, in the example manufacturing method of the semiconductor device of this embodiment, the semiconductor substrate 1 and the semiconductor substrate 23 are bonded together in which the formation of the roll-off region E is suppressed, so that the unbonded region G can be reduced and the effective area in which a semiconductor product can be formed can be expanded.

[0064] Although some embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These novel embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included in the scope and spirit of the invention, and are included in the scope of the invention and its equivalents described in the claims. [Explanation of symbols]

[0065] 1...semiconductor substrate, 1a...surface, 2...multilayer film, 2a...laminate, 2b...recess, 3...protective film, 4...insulating film, 5...insulating film, 7...memory hole, 8...memory layer, 9...contact layer, 10...wiring layer, 11...protective film, 12...insulating film, 13...insulating film, 14...protective film, 15...insulating film, 16...dishing, 17...dishing, 18...dishing, 19...connection pad, 20...element, 21...wiring layer, 22...connection pad, 23...semiconductor substrate, 81...block insulating film, 82...charge storage film, 83...tunnel insulating film, 84...semiconductor layer, 85...core insulating layer, 201...first film, 202...second film, 202a...conductive layer.

Claims

1. forming a multilayer film by alternately stacking a first film and a second film on a surface of a semiconductor substrate; a step of partially removing the multilayer film to form a plurality of laminated bodies and recesses between the plurality of laminated bodies and to expose an end portion including a periphery of the semiconductor substrate on the surface; forming a first insulating film filling the recess; forming a second insulating film on the end portion and the plurality of stacked bodies; forming a second protective film on the second insulating film, the second protective film overlapping the end portion but not overlapping the plurality of stacked bodies; partially removing the second insulating film along a thickness direction by chemical mechanical polishing; A method for manufacturing a semiconductor device comprising the steps of:

2. forming a multilayer film by alternately stacking a first film and a second film on a surface of a semiconductor substrate; a step of partially removing the multilayer film to form a plurality of laminated bodies and recesses between the plurality of laminated bodies and to expose an end portion including a periphery of the semiconductor substrate on the surface; forming a first insulating film filling the recess; forming a first protective film on the plurality of stacked bodies, the first insulating film, and the end portion; forming a second insulating film on the first protective film so as to overlap at least a portion of another one of the plurality of stacked bodies and the end portion; forming a second protective film on the second insulating film, the second protective film overlapping the end portion but not overlapping the plurality of stacked bodies; partially removing the second insulating film along a thickness direction by chemical mechanical polishing; A method for manufacturing a semiconductor device comprising the steps of:

3. The method of claim 2 , wherein the first protective film comprises a silicon nitride film.

4. The method of claim 1 or 2, wherein the second protective film comprises a silicon nitride film.

5. the first film is a silicon oxide film, The method of claim 1 , wherein the second film is a silicon nitride film.

6. The method according to claim 1 , wherein each of the first and second insulating films comprises a silicon oxide film.

7. 7. The method of claim 6, further comprising forming a third insulating film over the second insulating film before partially removing the second insulating film using chemical mechanical polishing.

8. The method of claim 7 , wherein the third insulating film comprises a silicon oxide film.

9. forming a memory layer through one of the plurality of stacks; removing the second film to form a cavity, and forming a conductive layer in the cavity; The method of any one of claims 1 to 8, further comprising:

10. forming a first connection pad above the memory layer; a step of bonding the semiconductor substrate and a second semiconductor substrate having second connection pads such that the first and second connection pads face each other; The method of claim 9 further comprising:

Citation Information

Patent Citations

  • Semiconductor device, manufacturing method of semiconductor device, bonding method of semiconductor wafer and electronic apparatus

    JP2012174937A

  • Semiconductor substrate and manufacturing method of the same

    JP2013051354A

  • Semiconductor device

    JP2017059607A

  • Vehicle and method for detecting a parking space via a drone

    US10529233B1

  • Methods Of Manufacturing Semiconductor Devices

    US20120149185A1