EUV transmitting film, its use and exposure method

A temporary protective layer on EUV-transmissive membranes, removable by EUV exposure, addresses the issue of reduced transmittance in existing pellicle membranes by preventing film formation, ensuring high EUV transmittance.

JP7554368B2Active Publication Date: 2024-09-19NGK CORP
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023562760
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-09-15
Publication Date
2024-09-19
Estimated Expiration
2042-09-15

AI Technical Summary

Technical Problem

Existing EUV-transmissive pellicle membranes suffer from reduced transmittance due to natural oxide films and side reaction films forming on the surface of high-EUV-transmittance core materials, and protective layers further decrease transmittance while being difficult to remove.

Method used

A temporary protective layer made of amorphous carbon, Cu, or organic resist is applied to the EUV-transmissive membrane, which can be removed by EUV exposure, preventing the formation of natural oxide and side reaction films, and ensuring high EUV transmittance during exposure.

Benefits of technology

The EUV-transmissive film maintains high transmittance by eliminating absorption caused by protective layers and preventing film formation, achieving up to 95% transmittance during exposure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007554368000002
    Figure 0007554368000002
  • Figure 0007554368000001
    Figure 0007554368000001
  • Figure 0007554368000003
    Figure 0007554368000003
Patent Text Reader

Abstract

Provided is an EUV-transmissive film in which EUV absorption by a protective layer causing a decrease in EUV transmittance can be suppressed, thereby enabling exhibition of high EUV transmittance at the time of exposure. The EUV-transmissive film comprises: a main layer (12) formed of a single layer or a composite layer including two or more layers and having an EUV transmittance of 85% or higher at a wavelength of 13.5 nm; and a protective layer (14) covering at least one side of the main layer and containing, as a major component, at least one selected from the group consisting of amorphous carbon, Cu, Al, and organic resist.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an EUV transmitting film, a method for using the same, and an exposure method. [Background technology]

[0002] The miniaturization of semiconductor manufacturing processes is progressing year by year, and various improvements are being made to each process. In particular, in the photolithography process, EUV (extreme ultraviolet) light with a wavelength of 13.5 nm has begun to be used instead of the 193 nm wavelength of the conventional ArF exposure. As a result, the wavelength suddenly became 1 / 10 or less, and its optical characteristics became completely different. However, since there is no material with high transmittance for EUV light, there is still no practical pellicle, which is a film that prevents particle adhesion on photomasks (reticles). For this reason, device manufacturers are currently manufacturing semiconductor devices without being able to use pellicles.

[0003] Therefore, pellicle membranes have been developed, and it is considered desirable to use Si, Be, Y, Zr, etc., which have high EUV transmittance, as the core material of the pellicle membrane. Patent Document 1 (Japanese Patent No. 6858817) discloses a pellicle membrane including a core layer containing a material that is substantially transparent to EUV radiation, such as (poly)Si, and a cap layer containing a material that absorbs IR radiation.

[0004] In addition, Patent Document 2 (JP 2020-98227 A) discloses a pellicle film stretched over one end surface of a pellicle frame, the pellicle film having a main layer of single crystal Si and graphene on one or both sides of the main layer. It is said that the main layer having graphene can prevent the pellicle film from being damaged during pellicle fabrication and exhibit sufficient mechanical strength. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] Patent No. 6858817 [Patent Document 2] JP 2020-98227 A Summary of the Invention

[0006] Incidentally, the core material with high EUV transmittance used in the pellicle film forms a natural oxide film of several nm on its surface in the atmosphere, and this oxide film absorbs EUV, reducing the EUV transmittance of the pellicle film. In particular, Be is a material with high EUV transmittance, but it is said that a natural oxide film of 2 to 3 nm is formed on its surface, and the transmittance loss due to this oxide film is large at 6 to 9%. In addition, since the process of producing the pellicle film may involve treatment using gases other than the atmosphere, such as fluorine or chlorine, or acid or alkaline solutions, a side reaction film may form on the surface of the core material, which may reduce the EUV transmittance. Therefore, it is desirable to form a protective layer on the surface of the core material to suppress the formation of these films.

[0007] However, although a significant decrease in the EUV transmittance of the pellicle film can be prevented by attaching a reaction suppression protective layer to the surface of a core material such as Si or Be, such a protective layer also has a lower EUV transmittance than the pure core material, leading to a decrease in the EUV transmittance of the entire pellicle film. For example, Ru can be used as a protective layer for a Be core material. In a three-layer structure (Ru / Be / Ru) pellicle film in which Ru is provided to a thickness of 1 to 2 nm on the front and back surfaces of the Be core material, the Ru protective layer causes a loss in EUV transmittance of about 3 to 6%, significantly decreasing the performance of the pellicle film. Other examples of protective layers include nitrides such as Si3N4 and Be3N2, but the same decrease in EUV transmittance as above is an issue. In other words, an EUV-transmitting film is desired that can suppress or eliminate EUV absorption by the protective layer, which was a factor in the decrease in EUV transmittance in conventional pellicle films.

[0008] The present inventors have now discovered that by covering a main layer having a high EUV transmittance with a temporary protective layer that can be removed by EUV exposure, it is possible to eliminate EUV absorption by the protective layer, which has been a cause of reduced EUV transmittance, and thereby provide an EUV transmitting film that can exhibit high EUV transmittance upon exposure.

[0009] Therefore, an object of the present invention is to provide an EUV transmitting film that can eliminate EUV absorption by a protective layer, which has been a cause of reduced EUV transmittance, and thereby exhibit high EUV transmittance upon exposure.

[0010] According to the present invention, the following aspects are provided. [Aspect 1] A main layer having an EUV transmittance of 85% or more at a wavelength of 13.5 nm and composed of a single layer or a composite layer of two or more layers; a protective layer covering at least one surface of the main layer, the protective layer including at least one selected from the group consisting of amorphous carbon, Cu, Al, and an organic resist as a main component; EUV-transmitting membrane. [Aspect 2] 2. The EUV transmissive film of claim 1, wherein both sides of the main layer are covered with the protective layer. [Aspect 3] 3. The EUV transmitting film according to claim 1 or 2, wherein the main layer contains Be, Si, Y, or Zr as a main component. [Aspect 4] 4. The EUV transmitting film according to any one of aspects 1 to 3, wherein the protective layer has a thickness of 5 nm or less. [Aspect 5] 5. The EUV transmitting film according to any one of aspects 1 to 4, wherein the protective layer is made of amorphous carbon. [Aspect 6] A step of mounting the EUV transmitting film according to any one of aspects 1 to 5 in an EUV exposure device; irradiating the EUV transmitting film with EUV, thereby removing the protective layer; and a method for using the EUV transmitting film. [Aspect 7] A step of mounting the EUV transmitting film according to any one of aspects 1 to 5 in an EUV exposure device; irradiating the EUV transmitting film with EUV light, thereby removing the protective layer and exposing the main layer; a step of transmitting EUV light through the exposed main layer by EUV irradiation to perform pattern exposure on a photosensitive substrate in the EUV exposure device; An exposure method comprising: [Brief description of the drawings]

[0011] [Figure 1] 1 is a schematic cross-sectional view showing one embodiment of an EUV transmitting film according to the present invention. [Figure 2A] 1 is a process flow diagram showing the first half of the manufacturing procedure of the EUV transmitting films in Examples 1 to 3. [Figure 2B] 1 is a process flow diagram showing the latter half of the manufacturing procedure of the EUV transmitting films in Examples 1 to 3. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] EUV permeable membrane FIG. 1 shows a schematic cross-sectional view of an EUV transmitting film 10 according to an embodiment of the present invention. The EUV transmitting film 10 includes a main layer 12 and a protective layer 14 covering at least one side of the main layer 12. The main layer 12 has an EUV transmittance of 85% or more at a wavelength of 13.5 nm, and is composed of a single layer or a composite layer of two or more layers. The protective layer 14 contains at least one selected from the group consisting of amorphous carbon, Cu, Al, and an organic resist as a main component. In this way, by covering the main layer having a high EUV transmittance with a temporary protective layer that can be removed by EUV exposure, it is possible to eliminate EUV absorption by the protective layer, which has been a cause of a decrease in EUV transmittance, and thus it is possible to provide an EUV transmitting film that can exhibit a high EUV transmittance upon exposure.

[0013] As mentioned above, a core material with high EUV transmittance may form a natural oxide film of several nm on its surface in the atmosphere. In addition, in the process of producing a pellicle film, a side reaction film may be formed on the surface of the core material because a gas other than the atmosphere, such as fluorine or chlorine, or an acid or alkaline solution may be used. The formation of such a film reduces the EUV transmittance of the pellicle film. Therefore, it is desirable to form a protective layer on the surface of the core material to suppress the formation of these films. However, attaching a reaction suppression protective layer to the surface of the core material leads to a decrease in the EUV transmittance of the pellicle film as a whole. These problems are successfully solved by the EUV transmitting film of the present invention. The mechanism by which the EUV transmitting film of the present invention can prevent the formation of a natural oxide film and the like while also preventing a decrease in EUV transmittance due to the protective layer is as follows. The EUV transmitting film of the present invention has a main layer with high EUV transmittance and a protective layer covering at least one side of the main layer, and this protective layer is a temporary protective layer that can be removed by EUV exposure. That is, while the pellicle film is produced, mounted on an EUV exposure device, and subjected to an exposure process, the above-mentioned natural oxide film and side reaction film are formed, but the EUV transmitting film of the present invention has a protective layer, which can prevent the formation of the above-mentioned films. Next, the exposure process is generally performed in a hydrogen atmosphere, in which there are many hydrogen radicals generated by EUV. Therefore, by forming the protective layer from a material that can be removed by hydrogen radicals, the protective film of the EUV transmitting film is removed in the exposure device, and a film of only the pure core material (main layer) is obtained, so that the pellicle film can exhibit high transmittance. By this mechanism, the EUV transmitting film of the present invention can prevent the formation of a natural oxide film and the like by the temporary protective layer, while preventing a decrease in EUV transmittance by the protective layer by removing the temporary protective layer during the exposure process. As a result, it is possible to exhibit high EUV transmittance during exposure.

[0014] The main layer 12 has an EUV transmittance of 85% or more at a wavelength of 13.5 nm, preferably 92% or more, more preferably 94% or more, and even more preferably 96% or more. In the exposure process, the protective layer 14 of the EUV transmission film 10 is removed and the main layer 12 remains. Therefore, the higher the EUV transmittance of the main layer 12, the more desirable it is. The upper limit value is not particularly limited and ideally is 100%, but typically it is 99% or less, and more typically 98% or less.

[0015] The main layer 12 may be a single layer or a composite layer of two or more layers. In any case, the main layer 12 preferably contains Be, Si, Y, or Zr as a main component. Here, the "main component" in the main layer 12 means a component that occupies 50 mol% or more, preferably 70 mol% or more, more preferably 80 mol% or more, and even more preferably 90 mol% or more of the main layer 12. However, the main layer 12 (especially a single layer or at least one layer constituting the composite layer) may consist only of Be, Si, Y, or Zr. Such a main layer 12 contributes to the realization of a high EUV transmittance while ensuring the basic functions (such as the function of preventing particle adhesion) as a pellicle film. From such a viewpoint, the thickness of the main layer 12 is preferably 10 to 70 nm, more preferably 15 to 50 nm, and even more preferably 20 to 35 nm.

[0016] As described above, the main layer 12 may be a composite layer of two or more layers. For example, when a protective layer of amorphous carbon is directly provided on the main layer which is a metallic beryllium layer, amorphous carbon and metallic beryllium may react to form beryllium carbide. Therefore, for example, the main layer 12 is configured as a composite layer such as a metallic beryllium layer / nitride beryllium layer (or nitride beryllium layer / metallic beryllium layer / nitride beryllium layer), and by providing a protective layer of amorphous carbon on the nitride beryllium layer, the reaction between amorphous carbon and metallic beryllium can be prevented, that is, the reaction between the main layer and the protective layer can be suppressed. In this specification, the term "nitride beryllium" means an inclusive composition that allows not only a stoichiometric composition such as Be3N2 but also a non-stoichiometric composition such as Be3N 2-x (where 0 < x < 2).

[0017] The protective layer 14 is a layer for temporarily protecting the main layer 12. Therefore, the protective layer 14 may cover at least one side of the main layer 12, but it is preferable to cover both sides of the main layer 12 with the protective layer. The protective layer 14 contains at least one selected from the group consisting of amorphous carbon, Cu, Al, and an organic resist as a main component. Considering the high EUV transmittance, the small effect on the main layer 12 of the residue when the protective layer 14 is removed, and the ease of removal of the protective layer 14, it is preferable that the protective layer 14 contains amorphous carbon as a main component, and more preferably is composed of amorphous carbon. Amorphous carbon generally does not have a completely irregular atomic arrangement, and while it has a crystal structure microscopically (i.e., it has microcrystals), these microcrystals are irregularly arranged and often become amorphous as a whole. Among them, those containing many microcrystals with a three-dimensional four-coordinate structure like diamond are called DLC (Diamond-like Carbon), and those containing many fine particles with a planar three-coordinate structure like graphite are called GLC (Graphite-like Carbon). The protective layer 14 may be carbon having a completely irregular atomic arrangement, or may be carbon having irregular microcrystals. Furthermore, it may be amorphous carbon that is not completely dense and contains fine pores. Here, the "main component" in the protective layer 14 means a component whose weight occupies 50% by weight or more, preferably 60% by weight or more, more preferably 70% by weight or more, and even more preferably 80% by weight or more of the total weight of the protective layer 14. However, the protective layer 14 may be made of at least one selected from the group consisting of amorphous carbon, Cu, Al, and organic resist.

[0018] The thickness of the protective layer 14 is preferably 5 nm or less, and more preferably 3 nm or less. Although there is no particular lower limit to the thickness of the protective layer 14, it is typically 1 nm or more.

[0019] As described above, the main layer 12 may be a composite layer of two or more layers. For example, in addition to a metal layer such as a beryllium layer, the main layer 12 may be provided with a nitride layer such as a beryllium nitride layer on one or both of its sides. In this case, it is preferable that the main layer 12 has a nitrogen concentration gradient region in which the nitrogen concentration decreases as it approaches the metal layer such as the beryllium layer. That is, as described above, the composition of beryllium nitride can include non-stoichiometric compositions such as Be3N (where 0 < x < 2) from the stoichiometric composition such as Be3N2. The beryllium nitride constituting the beryllium nitride layer preferably has a gradient composition that approaches a beryllium-rich composition as it approaches the beryllium layer. By doing so, the adhesion between the nitride layer (i.e., the beryllium nitride layer) and the metal layer (i.e., the beryllium layer) constituting the main layer 12 can be improved, and the generation of stress caused by the difference in thermal expansion between the two layers can be alleviated. That is, it is possible to improve the adhesion between the two layers to suppress peeling, or to make it difficult to peel as a thermal expansion relaxation layer between the two layers when it absorbs EUV light and becomes high temperature. The thickness of the nitrogen concentration gradient region is preferably smaller than the thickness of the nitride layer. That is, it is not necessary for the entire thickness of the nitride layer to be the nitrogen concentration gradient region. For example, it is preferable that only a part of the thickness of the nitride, for example, 10 to 70% of the thickness of the nitride layer, is the nitrogen concentration gradient region, and more preferably 15 to 50% of the region is the nitrogen concentration gradient region. 2-x (In the formula, 0 < x < 2), the beryllium nitride constituting the beryllium nitride layer preferably has a gradient composition that approaches a beryllium-rich composition as it approaches the beryllium layer. By doing so, the adhesion between the nitride layer (i.e., the beryllium nitride layer) and the metal layer (i.e., the beryllium layer) constituting the main layer 12 can be improved, and the generation of stress caused by the difference in thermal expansion between the two layers can be alleviated. That is, it is possible to improve the adhesion between the two layers to suppress peeling, or to make it difficult to peel as a thermal expansion relaxation layer between the two layers when it absorbs EUV light and becomes high temperature. The thickness of the nitrogen concentration gradient region is preferably smaller than the thickness of the nitride layer. That is, it is not necessary for the entire thickness of the nitride layer to be the nitrogen concentration gradient region. For example, the nitride layer only a part of the thickness, for example, 10 to 70% of the thickness of the nitride layer, is preferably the nitrogen concentration gradient region, and more preferably 15 to 50% of the region is the nitrogen concentration gradient region.

[0020] The EUV transmitting film 10 preferably has a main region for transmitting EUV in the form of a free-standing film. That is, it is preferable that the substrate (e.g., Si substrate) used in film formation remains as a border only at the outer edge of the EUV transmitting film 10, that is, the substrate (e.g., Si substrate) does not remain in the main region other than the outer edge, that is, the main region is preferably composed of only the main layer 12 and the protective layer 14. It is preferable that the protective layer 14 is completely removed in the exposure process. Note that, since the inside of the exposure device is usually depressurized to an ultra-high vacuum before processing is started, the oxygen partial pressure inside the exposure device is extremely low, and the main layer 12 exposed after the protective layer 14 is removed is almost never oxidized. There is a possibility that the surface of the main layer 12 is very slightly oxidized by a small amount of residual oxygen in the exposure device, but the oxidized portion can be reduced by EUV irradiation in a hydrogen atmosphere. Therefore, the EUV transmitting film 10 subjected to the exposure process can maintain a high EUV transmittance until it is taken out of the exposure device.

[0021] Manufacturing method The EUV transmitting film according to the present invention can be produced by forming a laminated film to be the EUV transmitting film on a Si substrate, and then removing unnecessary portions of the Si substrate by etching to form a free-standing film. Therefore, as described above, the main portion of the EUV transmitting film is in the form of a free-standing film with no Si substrate remaining.

[0022] (1) Preparation of Si substrate First, a Si substrate is prepared on which a laminated film is to be formed. After a laminated film consisting of a main layer 12 and a protective layer 14 is formed on the Si substrate, the main region (i.e., the region to be a free-standing film) other than the outer edge portion is removed by etching. Therefore, in order to perform etching efficiently and in a short time, it is desirable to thin the thickness of the Si substrate in the region to be a free-standing film in advance. Therefore, it is desirable to form a mask corresponding to an EUV transmission shape on the Si substrate using a normal semiconductor process, etch the Si substrate by wet etching, and thin the thickness of the main region of the Si substrate to a predetermined thickness. The Si substrate that has been subjected to wet etching is washed and dried to prepare a Si substrate having a cavity formed by wet etching. Note that the wet etching mask may be made of any material that is resistant to corrosion by a wet etching solution for Si, and for example, SiO2 is preferably used. Also, the wet etching solution is not particularly limited as long as it can etch Si. For example, TMAH (tetramethylammonium hydroxide) is preferable because it can perform very good anisotropic etching of Si when used under appropriate conditions.

[0023] (2) Formation of laminated film The laminated film may be formed by any film forming method. A preferred example of the film forming method is a sputtering method. When a three-layer structure of amorphous carbon / beryllium / amorphous carbon is formed, it is preferable that the beryllium film as the main layer 12 is formed by sputtering using a pure Be target, and the amorphous carbon film as the protective layer 14 is formed by sputtering using a graphite target. The methods for forming the beryllium and amorphous carbon films are not limited to these. The beryllium film and the amorphous carbon film may be formed in a single-chamber sputtering device as in the embodiment described later, or the beryllium film and the amorphous carbon film may be formed in separate chambers using a two-chamber sputtering device.

[0024] When the main layer 12 is made as a composite layer having a three-layer structure of beryllium nitride / beryllium / beryllium nitride, it is preferable that the beryllium film is made by sputtering using a pure Be target, and the beryllium nitride film is made by reactive sputtering. This reactive sputtering can be performed, for example, by introducing nitrogen gas into a chamber during sputtering using a pure Be target, so that beryllium and nitrogen react to generate beryllium nitride. As another method, beryllium nitride can be made by forming a beryllium film, and then irradiating it with nitrogen plasma to cause a nitriding reaction of beryllium to generate beryllium nitride. In any case, the synthesis method of beryllium nitride is not limited to these.

[0025] In the case of forming a nitrogen concentration gradient region in a composite layer having a three-layer structure of beryllium nitride / beryllium / beryllium nitride, when forming a beryllium nitride film and a metal beryllium film, nitrogen gas is introduced into the chamber and sputtering using a pure Be target is continued, while stopping the introduction of nitrogen gas halfway and switching to the formation of a metal beryllium film. In this way, a region in which the nitrogen concentration in the film to be formed decreases in the thickness direction is formed as the concentration of nitrogen gas in the chamber decreases. On the other hand, when switching from metal beryllium to beryllium nitride, the nitrogen concentration gradient region can be formed by continuing sputtering and starting the introduction of nitrogen gas halfway, in the opposite manner to the above. The thickness of the nitrogen concentration gradient region can be controlled by adjusting the time for changing the nitrogen gas concentration.

[0026] (3) Self-supporting film The unnecessary parts of the Si substrate on which the composite film is formed, except for the outer edge part to be left as a border, are removed by etching to make the composite film into a free-standing film. The Si etching may be performed by any method, but is preferably performed by etching using XeF2.

[0027] Method of use and exposure As described above, the exposure process is generally performed in a hydrogen atmosphere, and the atmosphere contains many hydrogen radicals generated by EUV. Therefore, the protective layer 14 in the EUV transmitting film 10 is removed by the hydrogen radicals, and a film of only the pure core material (main layer 12) is obtained, so that the main layer 12 can exhibit high transmittance as a pellicle film in the exposure process. Therefore, a preferred method of using the EUV transmitting film includes a step of mounting the EUV transmitting film in an EUV exposure device, and a step of irradiating the EUV transmitting film with EUV to thereby remove the protective layer. In addition, a preferred exposure method includes a step of mounting the EUV transmitting film in an EUV exposure device, a step of irradiating the EUV transmitting film with EUV to thereby remove the protective layer to expose the main layer, and a step of transmitting EUV through the main layer exposed by EUV irradiation to perform pattern exposure on a photosensitive substrate in the EUV exposure device. EXAMPLES

[0028] The present invention will now be further illustrated by the following examples.

[0029] Example 1 According to the procedure shown in FIGS. 2A and 2B, a composite free-standing film (EUV-transmitting film) having a three-layer structure of amorphous carbon / beryllium / amorphous carbon was fabricated as follows.

[0030] (1) Preparation of Si substrate A Si wafer 20 with a diameter of 8 inches (20.32 cm) was prepared (FIG. 2A(a)). A SiO2 film 22 was formed on both sides of the Si wafer 20 by thermal oxidation to a thickness of 50 nm (FIG. 2A(b)). Resist was applied to both sides of the Si wafer 20, and exposure and development were performed to form a resist hole of 110 mm x 145 mm on one side to form a resist mask 24 for SiO2 etching (FIG. 2A(c)). One side of the substrate was wet-etched with hydrofluoric acid to etch away the exposed part of the SiO2 film 22, producing a SiO2 mask 22a (FIG. 2A(d)). The resist mask 24 for SiO2 etching was removed by an ashing device (FIG. 2A(e)). After that, Si was wet-etched with TMAH liquid. The etching rate was measured in advance, and this etching was performed only for the etching time required to achieve the target Si substrate thickness of 50 μm (FIG. 2A(f)). Finally, the SiO2 film 22 formed on the surface that was not etched was removed and cleaned with hydrofluoric acid to prepare a Si substrate 28 (FIG. 2B(g)). The Si substrate may be diced with a laser 30 (FIG. 2B(h)) to obtain a desired shape (FIG. 2B(i)) if necessary. In this way, a 110 mm x 145 mm cavity 26 was provided in the center of the 8-inch (20.32 cm) Si wafer 20, and a Si substrate 28 with a Si thickness of 50 μm in the cavity 26 area was prepared.

[0031] (2) Formation of composite membrane A composite film having a three-layer structure of amorphous carbon / beryllium / amorphous carbon was formed on the Si substrate 28 with the cavity 26 obtained in (1) above as follows (FIG. 2B(i)). First, the Si substrate 28 was set in a multi-target sputtering device, and a graphite target and a pure Be target were attached. The chamber was evacuated, and sputtering was performed using the graphite target at an internal pressure of 0.3 Pa and only argon gas, and the sputtering was terminated when a 2 nm film of DLC (Diamond-like Carbon) was formed as amorphous carbon. Next, the chamber was evacuated again, and sputtering was performed using the pure Be target at an internal pressure of 0.5 Pa and only argon gas, and the sputtering was terminated when a 30 nm film of beryllium was formed. Thereafter, sputtering was performed using the graphite target in the same manner as in the first step, and the sputtering was terminated when a 2 nm film of amorphous carbon was formed. In this manner, a composite film of amorphous carbon (C) 2 nm / beryllium (Be) 30 nm / amorphous carbon (C) 2 nm was formed as the EUV transmitting film 10. That is, this EUV transmitting film 10 includes a main layer containing Be as a main component, and protective layers containing amorphous carbon as a main component on both sides of the main layer.

[0032] (3) Self-supporting film The Si substrate 28 with the composite film prepared in (2) above was set in the chamber of a XeF2 etcher capable of processing 8-inch (20.32 cm) substrates. The chamber was evacuated sufficiently. At this time, if moisture remains in the chamber, it reacts with the XeF2 gas to produce hydrofluoric acid, which can cause corrosion of the etcher or unexpected etching, so a sufficient vacuum was drawn. If necessary, the chamber was repeatedly evacuated and nitrogen gas was introduced to reduce the remaining moisture. Once a sufficient vacuum was achieved, the valve between the XeF2 raw material cylinder and the spare chamber was opened. As a result, XeF2 sublimated and XeF2 gas accumulated in the spare chamber as well. Once a sufficient amount of XeF2 gas had accumulated in the spare chamber, the valve between the spare chamber and the chamber was opened, and XeF2 gas was introduced into the chamber. The XeF2 gas decomposed into Xe and F, and the F reacted with Si to produce SiF4. Since the boiling point of SiF4 is -95°C, the generated SiF4 quickly evaporated, causing a reaction between the newly exposed Si substrate and F. When the Si etching progressed and the amount of F in the chamber decreased, the chamber was evacuated and XeF2 gas was introduced into the chamber again to perform etching. In this way, the vacuuming, introduction of XeF2 gas, and etching were repeated, and etching was continued until the Si substrate 28 corresponding to the portion to be made into a free-standing film disappeared. Etching was terminated when the unnecessary portion of the Si substrate disappeared. In this way, a composite free-standing film having a Si border 20 was obtained as an EUV-transmitting film 10 (FIG. 2B(j)).

[0033] Example 2 (comparison) A composite free-standing film having a three-layer structure of ruthenium / beryllium / ruthenium was produced in the same manner as in Example 1, except that the composite film was formed as follows.

[0034] (Formation of composite membrane) The Si substrate with the cavity formed obtained in (1) of Example 1 was placed in a multi-target sputtering device, and a pure ruthenium target and a pure Be target were attached. The chamber was evacuated, and sputtering was performed using the pure ruthenium target at an internal pressure of 0.3 Pa and only argon gas, and the sputtering was terminated when the time came for the ruthenium to be deposited to a thickness of 2 nm. Next, the chamber was evacuated again, and sputtering was performed using the pure Be target at an internal pressure of 0.5 Pa and only argon gas, and the sputtering was terminated when the time came for the beryllium to be deposited to a thickness of 30 nm. Thereafter, sputtering was performed using the pure ruthenium target in the same manner as in the first step, and the sputtering was terminated when the time came for the ruthenium to be deposited to a thickness of 2 nm. In this way, a composite film of ruthenium (Ru) 2 nm / beryllium (Be) 30 nm / ruthenium (Ru) 2 nm was formed as an EUV-transmitting film.

[0035] Example 3 (comparison) A composite free-standing film having a three-layer structure of crystalline carbon / beryllium / crystalline carbon was produced in the same manner as in Example 1, except that the composite film was formed as follows.

[0036] (Formation of composite membrane) The Si substrate with the cavity formed in (1) of Example 1 was placed in a chemical vapor deposition (CVD) apparatus, and crystalline carbon having a graphite crystal structure was deposited to a thickness of 2 nm using methane as the gas source. Next, the Si substrate with the crystalline carbon deposited was placed in a multi-target sputtering apparatus, and a graphite target and a pure Be target were attached. The chamber was evacuated, and sputtering was performed using a pure Be target at an internal pressure of 0.5 Pa and argon gas only, and the sputtering was terminated when a 30 nm film of beryllium was deposited. The graphite target was used to perform sputtering at an internal pressure of 0.3 Pa and argon gas only, and the sputtering was terminated when a 0.5 nm film of amorphous carbon was deposited. Thereafter, the sputtered Si substrate was placed in the vapor deposition apparatus again, and hydrogen cleaning was performed until the amorphous carbon was sufficiently removed, and crystalline carbon having a graphite crystal structure was deposited to a thickness of 2 nm using methane as the gas source in the same manner as in the first step. In this way, a composite film of crystalline carbon (C) 2 nm / beryllium (Be) 30 nm / crystalline carbon (C) 2 nm was formed as an EUV-transmitting film. The amorphous carbon film temporarily formed by sputtering was formed to suppress the oxidation of beryllium during the period from sputtering to chemical vapor deposition.

[0037] EUV transmittance The free-standing films as EUV-transmitting films prepared in Examples 1 to 3 were irradiated with EUV light at an output of 600 W in a hydrogen atmosphere of 20 Pa for 15 minutes, and the amount of EUV light transmitted was measured with a sensor. The EUV transmittance was calculated by comparing the obtained measurement value with the value measured with the sensor for the amount of EUV light directly without the EUV-transmitting film. As a result, the EUV transmittance of the composite free-standing film prepared in Example 1 was 95%. The EUV transmittance of the composite free-standing film prepared in Example 2, which is a comparative example, was 88%. The EUV transmittance of the composite free-standing film prepared in Example 3, which is a comparative example, was 90%. When the composite free-standing film in Example 3 was analyzed, it was confirmed that crystalline carbon remained in the protective layer. That is, in the composite free-standing film of crystalline carbon / beryllium / crystalline carbon in Example 3, it is considered that the crystalline carbon is difficult to remove in the exposure process and remains on the surface of the main layer of beryllium, thereby decreasing the EUV transmittance of the composite free-standing film. On the other hand, in the amorphous carbon / beryllium / amorphous carbon composite free-standing film of Example 1, the amorphous carbon is removed in the exposure process, leaving only the main layer of beryllium, which is thought to result in a high EUV transmittance of 95%.

Claims

1. a main layer having an EUV transmittance of 85% or more at a wavelength of 13.5 nm, the main layer being composed of a single layer or a composite layer of two or more layers and containing Be as a main component; a protective layer covering at least one surface of the main layer, the protective layer including at least one selected from the group consisting of amorphous carbon, Cu, Al, and an organic resist as a main component; An EUV transmitting film comprising:

2. An EUV transmitting film as described in claim 1, wherein Be accounts for 50 mol % or more of the main layer.

3. The EUV transmitting film according to claim 1 , wherein both sides of the main layer are covered with the protective layer.

4. The EUV transmitting film according to claim 1 , wherein the protective layer has a thickness of 5 nm or less.

5. The EUV transmitting film according to claim 1 or 2, wherein the protective layer is made of amorphous carbon.

6. A step of installing the EUV transmitting film according to claim 1 or 2 in an EUV exposure apparatus; irradiating the EUV transmitting film with EUV light, thereby removing the protective layer; A method of using the EUV transmitting film, comprising:

7. A step of installing the EUV transmitting film according to claim 1 or 2 in an EUV exposure apparatus; irradiating the EUV transmitting film with EUV light, thereby removing the protective layer and exposing the main layer; a step of transmitting EUV light through the exposed main layer by EUV irradiation to perform pattern exposure on a photosensitive substrate in the EUV exposure device;

8. 3. A method for using an EUV transmitting film, comprising the step of irradiating the EUV transmitting film according to claim 1 or 2 with EUV light, thereby removing the protective layer.

Citation Information

Patent Citations

  • Filter window, lithography projection apparatus, method of manufacturing filter window, method of manufacturing device and device manufactured by the method

    JP2005043895A

  • Films used in lithographic apparatus and lithographic apparatus containing such films

    JP2017522590A

  • Pellicle film for photo lithography and pellicle equipped with the same

    JP2020098227A

  • Film for use in a lithographic apparatus and a lithographic apparatus including such a film

    JP6858817B2

  • Pellicle with a wrinkle on a plane thereof, and Method for manufacturing the same

    KR1020200076258A