Process for removing iron and phosphate ions from chlorinated hydrocarbon waste streams - Patents.com
The process addresses the challenge of disposing of waste streams from chlorinated hydrocarbon production by converting iron and phosphate compounds into insoluble precipitates, achieving low ion concentrations and compliance with environmental regulations.
Patent Information
- Application Number
- JP2023094495
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2018-02-07
- Filing Date
- 2023-06-08
- Publication Date
- 2024-09-20
- Estimated Expiration
- 2039-01-31
AI Technical Summary
Existing processes for producing chlorinated hydrocarbons like HCC-240fa and HCC-250fb generate waste streams containing high concentrations of iron and phosphate ions, which are difficult to dispose of due to environmental regulations, and require thermal oxidation, leading to the release of hydrogen chloride and other harmful substances.
A process that involves thermal oxidation of the waste stream to convert iron and phosphate compounds into insoluble precipitates like FePO4, Fe(OH)3, and Ca3(PO4)2, followed by exposure to a base to form a precipitate, which is then separated, reducing the iron and phosphate concentrations to very low levels.
The process effectively reduces iron and phosphate ions in the waste stream to less than 500 ppm or less than 10 ppm, meeting environmental discharge standards and minimizing the harmful substances in the treated stream.
Abstract
Description
[Background technology]
[0001] 1. Field of disclosure
[0002] The present disclosure relates to a process for the removal, and in one embodiment, simultaneous removal, of iron and phosphate ions from chlorinated hydrocarbon waste streams.
[0003] 2. Description of Related Technology
[0004] Some commercial processes for producing chlorinated hydrocarbons such as 1,1,1,3,3-pentachloropropane (HCC-240fa) and / or 1,1,1,3-tetrachloropropane (HCC-250fb) typically use iron powder and catalysts such as tributyl phosphate (TBP) and / or triethyl phosphate (TEP). Exemplary processes for producing HCC-240fa and HCC-250fb are detailed in U.S. Patent Nos. 8,722,946 and 8,907,147, the disclosures of which are incorporated herein by reference.
[0005] In one exemplary process for producing HCC-240fa, carbon tetrachloride is reacted with vinyl chloride to form HCC-240fa according to the following reaction (1): CCl4+CH2=CHCl→CCl3-CH2-CHCl2(HCC-240fa) (1)
[0006] In one exemplary process for producing HCC-250fb, carbon tetrachloride is reacted with ethylene to form HCC-250fb according to the following reaction (2): CCl4+CH2=CH2→CCl3-CH2-CH2Cl(HCC-250fb) (2)
[0007] In each of the above reactions (1) and (2), iron powder and TBP or TEP can be used to generate the reaction catalyst, i.e., TBP-FeCl2 or TEP-FeCl2 complexes in situ.
[0008] In each of the aforementioned processes, the catalyst must be periodically purged to remove high boiling organic impurities formed during the reaction and to maintain catalytic activity. However, catalyst removal produces streams containing at least one of chlorinated hydrocarbons, TBP and / or TEP, iron, FeCl2 and / or FeCl3, TBP-FeCl2 and / or TBP-FeCl3 complexes, and TEP-FeCl2 and / or TEP-FeCl3 complexes.
[0009] The aforementioned catalyst removal streams are considered waste streams, and the chlorinated hydrocarbons and phosphorus-containing organic compounds in the waste streams are typically destroyed by thermal oxidation or incineration.
[0010] In addition, after incineration, high concentrations of hydrogen chloride (HCl), FeCl3 and Waste water streams containing iron and / or phosphate ions (FeCl2, FeCl3, FeCl4, and H3PO4 are generated and typically treated with ferric chloride to comply with applicable environmental regulations. 3+ and / or PO4 3- ) must be removed from the waste water stream before the stream is discharged. Summary of the Invention
[0011] The present disclosure provides a process for the simultaneous removal of iron and phosphate ions from a chlorinated hydrocarbon waste stream, such as a waste stream derived from a process for producing 1,1,1,3,3-pentachloropropane (HCC-240fa) and / or 1,1,1,3-tetrachloropropane (HCC-250fb), containing at least one of chlorinated hydrocarbons, tributyl phosphate (TBP) and / or triethyl phosphate (TEP), iron, FeCl2 and / or FeCl3, TBP-FeCl2 and / or TBP-FeCl3 complexes, and TEP-FeCl2 and / or TEP-FeCl3 complexes, which is subjected to thermal oxidation to produce a second aqueous waste stream containing at least one of hydrogen chloride (HCl), FeCl3 and / or FeCl2, H3PO4, and water. The second waste stream is exposed to a base to produce a precipitate comprising at least one insoluble compound selected from the group consisting of FePO4, Fe(OH)3, and Ca3(PO4)2, and the precipitate is separated from the second waste stream to produce a liquid phase comprising trace amounts of iron and phosphate ions.
[0012] In one form thereof, the invention provides a process for removing iron and phosphate ions from a waste stream comprising: providing a waste stream containing at least one of hydrogen chloride (HCl), FeCl3, FeCl2, H3PO4, and water; exposing the waste stream to a base to produce a precipitate comprising at least one insoluble compound selected from the group consisting of FePO4, Fe(OH)3, and Ca3(PO4)2; and separating the precipitate from the waste stream.
[0013] The waste stream after the separation step can be a liquid phase comprising CaCl2 and at least one of less than 500 ppm iron ions and less than 500 ppm phosphate ions. Alternatively, the waste stream after the separation step can be a liquid phase comprising CaCl2 and at least one of less than 10 ppm iron ions and less than 10 ppm phosphate ions.
[0014] The process may further include the additional steps of evaporating liquid from the waste stream after the separating step and recovering solid CaCl.
[0015] The base may be selected from the group consisting of potassium hydroxide (KOH), sodium hydroxide (NaOH), calcium oxide (CaO), calcium hydroxide (Ca(OH)2), and combinations thereof. You can choose.
[0016] The pH of the waste stream after the exposing step can be from 1 to 8. The molar ratio of iron ions to phosphate ions in the second waste stream after the separating step can be from 1 to 10. Alternatively, the molar ratio of iron ions to phosphate ions in the waste stream after the separating step can be from 1 to 2.
[0017] The step of separating can include separating the precipitate from the waste stream by at least one method selected from the group consisting of filtration, sedimentation, flocculation, centrifugation, and combinations thereof.
[0018] In another aspect, the disclosure provides a process for removing iron and phosphate ions from a waste stream, the process comprising the steps of providing a first waste stream containing organic matter, the first waste stream containing at least one of chlorinated hydrocarbons, tributyl phosphate (TBP) and / or triethyl phosphate (TEP), iron, FeCl2 and / or FeCl3, TBP-FeCl2 complexes and / or TBP-FeCl3 complexes, and TEP-FeCl2 complexes and / or TEP-FeCl3 complexes; and subjecting the first waste stream to thermal oxidation to produce a second waste stream containing at least one of hydrogen chloride (HCl), FeCl3, FeCl2, H3PO4, and water. exposing the second waste stream to a base to produce a precipitate comprising at least one insoluble compound selected from the group consisting of FePO4, Fe(OH)3, and Ca3(PO4)2, and separating the precipitate from the second waste stream.
[0019] The second waste stream after the separation step can be a liquid phase comprising CaCl2 and at least one of less than 500 ppm iron ions and less than 500 ppm phosphate ions. Alternatively, the second waste stream after the separation step can be a liquid phase comprising CaCl2 and at least one of less than 10 ppm iron ions and less than 10 ppm phosphate ions.
[0020] The process may further include the additional steps of evaporating liquid from the second waste stream after the separating step and recovering solid CaCl.
[0021] The base may be selected from the group consisting of potassium hydroxide (KOH), sodium hydroxide (NaOH), calcium oxide (CaO), calcium hydroxide (Ca(OH)2), and combinations thereof.
[0022] The second waste stream after the subjecting step may comprise a total concentration of FeCl3 and FeCl2 of less than 20 wt.%, the second waste stream may comprise a total concentration of H3PO4 of less than 20 wt.%, and / or the second waste stream comprises less than 40 wt.% HCl.
[0023] The molar ratio of iron ions to phosphate ions in the second waste stream after the separation step may be from 1-10, or may be from 1-2.
[0024] The step of separating can include separating the precipitate from the second waste stream by at least one method selected from the group consisting of filtration, sedimentation, flocculation, centrifugation, and combinations thereof. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0025] The present disclosure provides a process for the simultaneous removal of iron and phosphate ions from a chlorinated hydrocarbon waste stream, such as a waste stream derived from a process for producing 1,1,1,3,3-pentachloropropane (HCC-240fa) and / or 1,1,1,3-tetrachloropropane (HCC-250fb), containing at least one of chlorinated hydrocarbons, tributyl phosphate (TBP) and / or triethyl phosphate (TEP), iron, FeCl2 and / or FeCl3, TBP-FeCl2 and / or TBP-FeCl3 complexes, and TEP-FeCl2 and / or TEP-FeCl3 complexes, which is subjected to thermal oxidation to produce a second aqueous waste stream containing at least one of hydrogen chloride (HCl), FeCl3 and / or FeCl2, H3PO4, and water. The second waste stream is exposed to a base to produce a precipitate comprising at least one insoluble compound selected from the group consisting of FePO4, Fe(OH)3, and Ca3(PO4)2, and the precipitate is separated from the second waste stream to produce a liquid phase comprising trace amounts of iron and phosphate ions.
[0026] The waste stream, sometimes referred to herein as the first waste stream, in purging the catalyst from the reaction of the aforementioned process to remove high boiling organic impurities formed during the process and to maintain catalytic activity, is derived from a process for producing 1,1,1,3,3-pentachloropropane (HCC-240fa) and / or 1,1,1,3-tetrachloropropane (HCC-250fb).
[0027] This first waste stream is a mixture of chlorinated hydrocarbons, tributyl phosphate (TBP) and / or lysine. The composition contains at least one of triethyl phosphate (TEP), iron, FeCl2 and / or FeCl3, TBP-FeCl2 complexes and / or TBP-FeCl3 complexes, and TEP-FeCl2 complexes and / or TEP-FeCl3 complexes.
[0028] After the first waste stream is discharged from the HCC-240fa and / or HCC-250fb process, the components of the first waste stream including chlorinated hydrocarbons, TBP, TEP, iron, FeCl2, FeCl3, TBP-FeCl2 complexes, TBP-FeCl3 complexes, TEP-FeCl2 complexes, and TEP-FeCl3 complexes are sent to a waste treatment unit and destroyed by thermal oxidation, such as by incineration.
[0029] Flue gas from incineration may be cooled, for example, by adding water, typically to a temperature of 40°C to 70°C, such that most of the hydrogen chloride (HCl) remains in the flue gas, and, optionally, the flue gas itself may be recovered by other means, while certain amounts of HCl, iron oxides (FeO and / or FeO), and phosphorus pentoxide (PO / PO) are recovered. 10 ) is trapped in the water to form an aqueous stream containing the aforementioned components. In the aqueous stream, Fe2O3 and / or FeO react with HCl in the water to form FeCl3 and / or FeCl2, and P2O5 and / or PO 10 reacts with water to form H3PO4.
[0030] The aqueous stream produced after water addition, sometimes referred to herein as the second waste stream, contains relatively high concentrations of ferrous chloride (FeCl2) and / or ferric chloride (FeCl3), as well as hydrogen phosphate (H3PO4), and typically cannot be easily disposed of due to environmental regulations. The second waste stream may also contain hydrogen chloride (HCl).
[0031] In the second waste stream, the total concentration of ferrous chloride (FeCl2) and ferric chloride (FeCl3) may be, for example, as low as 0 wt%, 3 wt%, 5 wt%, or 7 wt%, or as high as 13 wt%, 15 wt%, 17 wt%, 20 wt%, or within any range defined between any two of the foregoing values, such as 0 wt% to 20 wt%, 3 wt% to 17 wt%, 5 wt% to 15 wt%, or 7 wt% to 13 wt%.
[0032] Also, in the second waste stream, the total concentration of hydrogen phosphate (H3PO4) may be, for example, as low as 0 wt%, 3 wt%, 5 wt%, or 7 wt%, or as high as 13 wt%, 15 wt%, 17 wt%, 20 wt%, or within any range defined between any two of the foregoing values, such as 0 wt%-20 wt%, 3 wt%-17 wt%, 5 wt%-15 wt%, or 7 wt%-13 wt%.
[0033] In the second waste stream, the concentration of HCl may be, for example, as low as 0 wt%, 1 wt%, 5 wt%, or as high as 10 wt%, 25 wt%, or 40 wt%, or within any range defined between any two of the foregoing values, such as 0 wt% to 40 wt%, 1 wt% to 25 wt%, or 5 wt% to 10 wt%.
[0034] The molar ratio of iron ions to phosphate ions in the second waste stream can be, for example, 1-10, 1-8, 3-7, or 1-2.
[0035] The second waste stream is then treated with or subjected to a base or a basic solution. The base can be an inorganic base, including at least one base, such as potassium hydroxide (KOH), sodium hydroxide (NaOH), calcium hydroxide (Ca(OH)2), or calcium oxide (CaO). The pH of the basic solution can be any pH above 7, and the pH of the second waste stream after treatment with the basic solution can be, for example, as low as 1, 2, or 3, or as high as 8, 9, or 10, or within any range defined between any two of the foregoing values, such as 1-10, 2-9, or 3-8. In one particular embodiment, the pH of the second waste stream after treatment with the basic solution is between 2.5 and 8.
[0036] An exemplary reaction illustrating the treatment of the second waste stream with a base is set forth below.
[0037] The following reactions (3)-(7) are illustrative when CaO is used as the base. CaO+H2O→Ca(OH)2(3) 2HCl+Ca(OH)2→CaCl2+2H2O (4) FeCl3+H3PO4→FePO4(s)+3HCl (5) 2FeCl3+3Ca(OH)2→2Fe(OH)3(s)+3CaCl2(6) 2H3PO4+3Ca(OH)2→Ca3(PO4)2(s)+6H2O (7)
[0038] When CaO is added to the second waste stream, it is converted to Ca(OH)2 by reacting with water as in reaction (3), and Ca(OH)2 reacts with HCl in the second waste stream to form soluble CaCl2 as in reaction (4), and the pH of the second waste stream increases. HCl is produced via thermal oxidation of chlorinated carbon. Most of the H3PO4 present in the second waste stream reacts with FeCl3 as in reaction (5) to produce water-insoluble solid FePO4 when the pH is adjusted to 2.5 or higher after an inorganic base is added. Excess FeCl3 reacts with Ca(OH)2 to form insoluble Fe(OH)3 as in reaction (6). A small amount of H3PO4 can react with Ca(OH)2 to produce Ca3(PO4)2 as in reaction (7), and the resulting Ca3(PO4)2 has some solubility in water.
[0039] The following reactions (8) to (11) are illustrative when KOH or NaOH is used as the base. HCl+KOH / NaOH→KCl / NaCl+H2O (8) FeCl3+H3PO4→FePO4(s)+3HCl (9) FeCl3+3KOH / NaOH→Fe(OH)3(s)+3KCl / NaCl (10) H3PO4+3K(OH) / NaOH→K3PO4 / Na3PO4+3H2O (11)
[0040] When KOH or NaOH is added to the second waste stream, the KOH or NaOH reacts with HCl in the second waste stream to form soluble KCl or NaCl, as in reaction (8), and the pH of the waste stream increases. Most of the H3PO4 present in the second waste stream reacts with FeCl3 to produce water-insoluble solid FePO4, as in reaction (9), once the pH is adjusted to 2.5 or higher after an inorganic base is added. Excess FeCl3 reacts with KOH or NaOH to form insoluble Fe(OH)3, as in reaction (10). Small amounts of H3PO4 can react with KOH or NaOH to produce K3PO4 / Na3PO4, as in reaction (11), resulting in water-soluble K3PO4 / Na3PO4.
[0041] In the present process, the residual phosphate ion concentration in the liquid phase of the second waste stream after KOH / NaOH is added and the produced solids are separated is higher than when CaO or Ca(OH)2 are used because the solubility of K3PO4 / Na3PO4 is much higher than Ca3(PO4)2.
[0042] The second waste stream may be treated with a base by discharging the second waste stream into a mixer where a base is added to adjust the pH of the second waste stream to the above levels. As a result of such a process, a solid precipitate forms in the liquid phase of the second waste stream, which precipitate includes iron phosphate (FePO4), iron hydroxide (FePO4), which are insoluble in water under weak acid or basic pH conditions. The second waste stream contains one or more of calcium phosphate (Ca3(PO4)2), and calcium phosphate (Fe(OH)3), and thus precipitates out of the second waste stream as a solid.
[0043] Optionally, fresh ferrous chloride (FeCl2) and / or ferric chloride (FeCl3) may be added during the aforementioned base treatment step as desired to adjust the molar ratio of iron ions to phosphorus ions in the second waste stream.
[0044] The solid precipitate of iron phosphate (FePO), iron hydroxide (Fe(OH)), and / or calcium phosphate (Ca(PO)) is then separated from the liquid of the second waste stream by filtration, physical and / or chemical precipitation, flocculation, centrifugation, or a combination of the aforementioned techniques.
[0045] The liquid phase of the second waste stream after the aforementioned separation contains relatively large amounts of calcium chloride (CaCl2) and advantageously very small amounts of ferric and / or ferrous ions (Fe 3+ and / or Fe 2+ ), and phosphate ions (PO4 3- ).
[0046] The total amount of iron ions remaining in the liquid phase of the second waste stream, also referred to herein as residual iron, can be, for example, very little, i.e., less than 0.01 ppm, 0.1 ppm, 1 ppm, or more, i.e., less than 10 ppm, 50 ppm, or 500 ppm, or within any range defined between any two of the aforementioned values, such as 0.01-500 ppm, 0.1-50 ppm, or 1-10 ppm.
[0047] The amount of phosphate ions remaining in the liquid phase of the second waste stream, also referred to herein as phosphorus or residual phosphorus, can be, for example, very little, i.e., less than 0.01 ppm, 0.1 ppm, 1 ppm, or more, i.e., less than 10 ppm, 50 ppm, or 500 ppm, or within any range defined between any two of the foregoing values, such as 0.01-500 ppm, 0.1-50 ppm, or 1-10 ppm.
[0048] Optionally, water may be removed from the liquid phase of the treated second waste stream by evaporation, for example, to concentrate and recover CaCl as a by-product. EXAMPLES
[0049] Example 1 300 grams of an aqueous solution containing 4.0 wt% FeCl3 and 2.0 wt% H3PO4 (Fe / P molar ratio = 1.21) was added to a 500 mL glass beaker. With stirring, 30% NaOH solution was slowly added to the beaker to adjust the solution pH to 3.0. The mixture was then filtered, and the Fe and P ion concentrations in the filtrate measured by inductively coupled plasma mass spectrometry (ICP-MS) were 12.5 ppm and 18.6 ppm, respectively. Example 2
[0050] 300 grams of an aqueous solution containing 4.0 wt% FeCl3 and 2.0 wt% H3PO4 (Fe / P molar ratio = 1.21) was added to a 500 mL glass beaker. With stirring, 30% NaOH solution was slowly added to the beaker to adjust the solution pH to 4.0. The mixture was then filtered, and the Fe and P ion concentrations in the filtrate measured by inductively coupled plasma mass spectrometry (ICP-MS) were 1.1 ppm and 19.9 ppm, respectively. Example 3
[0051] 4.0 wt% FeCl3 and 2.0 wt% H3PO4 (Fe / P molar ratio = 1.2 300 grams of an aqueous solution containing 1) was added to a 500 mL glass beaker. With stirring, 30% NaOH solution was slowly added to the beaker to adjust the solution pH to 5.0. The mixture was then filtered, and the Fe and P ion concentrations in the filtrate measured by inductively coupled plasma mass spectrometry (ICP-MS) were 0.08 ppm and 29.0 ppm, respectively. Example 4
[0052] 300 grams of an aqueous solution containing 4.0 wt% FeCl3 and 2.0 wt% H3PO4 (Fe / P molar ratio = 1.21) was added to a 500 mL glass beaker. With stirring, 30% NaOH solution was slowly added to the beaker to adjust the solution pH to 7.0. The mixture was then filtered, and the Fe and P ion concentrations in the filtrate measured by inductively coupled plasma mass spectrometry (ICP-MS) were 0.15 ppm and 57.4 ppm, respectively. Example 5
[0053] 300 grams of an aqueous solution containing 4.0 wt% FeCl3 and 2.0 wt% H3PO4 (Fe / P molar ratio = 1.21) was added to a 500 mL glass beaker. With stirring, 30% NaOH solution was slowly added to the beaker to adjust the solution pH to 8.0. The mixture was then filtered, and the Fe and P ion concentrations in the filtrate measured by inductively coupled plasma mass spectrometry (ICP-MS) were 0.23 ppm and 354.8 ppm, respectively. Example 6
[0054] 300 grams of an aqueous solution containing 4.0 wt% FeCl3 and 2.0 wt% H3PO4 (Fe / P molar ratio = 1.21) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 3.2. The mixture was then filtered, and the Fe and P ion concentrations in the filtrate measured by inductively coupled plasma mass spectrometry (ICP-MS) were 0.05 ppm and 0.74 ppm, respectively. Example 7
[0055] 300 grams of an aqueous solution containing 4.0 wt% FeCl3 and 2.0 wt% H3PO4 (Fe / P molar ratio = 1.21) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 5.3. The mixture was then filtered, and the Fe and P ion concentrations in the filtrate measured by inductively coupled plasma mass spectrometry (ICP-MS) were 0.02 ppm and 0.27 ppm, respectively. Example 8
[0056] 300 grams of an aqueous solution containing 4.0 wt% FeCl3 and 2.0 wt% H3PO4 (Fe / P molar ratio = 1.21) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 5.9. The mixture was then filtered, and the Fe and P ion concentrations in the filtrate measured by inductively coupled plasma mass spectrometry (ICP-MS) were 0.44 ppm and 1.1 ppm, respectively. Example 9
[0057] 300 grams of an aqueous solution containing 4.0 wt% FeCl3 and 2.0 wt% H3PO4 (Fe / P molar ratio = 1.21) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 7.7. The mixture was then filtered and the pH was measured by inductively coupled plasma mass spectrometry (ICP-MS). The P ion concentration in the filtrate was 0.47 ppm. Example 10
[0058] 300 grams of an aqueous solution containing 4.0 wt% FeCl3 and 2.0 wt% H3PO4 (Fe / P molar ratio = 1.21) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 9.3. The mixture was then filtered, and the Fe and P ion concentrations in the filtrate measured by inductively coupled plasma mass spectrometry (ICP-MS) were 0.01 ppm and 0.37 ppm, respectively. Example 11
[0059] 300 grams of an aqueous solution containing 8.35 wt% HCl, 1.55 wt% FeCl3, and 0.76 wt% H3PO4 (Fe / P molar ratio = 1.23) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 6.5. The mixture was then filtered, and the P ion concentration in the filtrate was measured by inductively coupled plasma mass spectrometry (ICP-MS) to be 0.59 ppm. Example 12
[0060] 200 grams of an aqueous solution containing 6.0 wt% HCl, 9.87 wt% FeCl3, and 3.76 wt% H3PO4 (Fe / P molar ratio = 1.59) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 5.8. The mixture was then filtered, and the P ion concentration in the filtrate was measured by inductively coupled plasma mass spectrometry (ICP-MS) to be 0.49 ppm. Visual observation showed that the mixture turned into a gel-like, non-flowable solid and was difficult to filter. Example 13
[0061] 200 grams of an aqueous solution containing 7.0 wt% HCl, 9.87 wt% FeCl3, and 3.76 wt% H3PO4 (Fe / P molar ratio = 1.59) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 6.1. The mixture was then filtered, and the P ion concentration in the filtrate was measured by inductively coupled plasma mass spectrometry (ICP-MS) to be 0.41 ppm. Visual observation showed that the mixture turned into a gel-like, non-flowable solid and was difficult to filter. Example 14
[0062] 200 grams of an aqueous solution containing 8.0 wt% HCl, 9.87 wt% FeCl3, and 3.76 wt% H3PO4 (Fe / P molar ratio = 1.59) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 5.7. The mixture was then filtered, and the P ion concentration in the filtrate was measured by inductively coupled plasma mass spectrometry (ICP-MS) to be 0.61 ppm. By visual observation, the mixture was flowable and filterable. Example 15
[0063] 200 grams of an aqueous solution containing 10.0 wt% HCl, 9.87 wt% FeCl3, and 3.76 wt% H3PO4 (Fe / P molar ratio = 1.59) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 5.8. The mixture was then filtered, and the P ion concentration in the filtrate was measured by inductively coupled plasma mass spectrometry (ICP-MS) to be 0.65 ppm. By visual observation, the mixture was flowable and filterable. Example 16
[0064] 200 grams of an aqueous solution containing 15.0 wt% HCl, 9.87 wt% FeCl3, and 3.76 wt% H3PO4 (Fe / P molar ratio = 1.59) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 4.4. The mixture was then filtered, and the P ion concentration in the filtrate was measured by inductively coupled plasma mass spectrometry (ICP-MS) to be 0.86 ppm. By visual observation, the mixture was flowable and filterable. (Example 17)
[0065] 200 grams of an aqueous solution containing 15.0 wt% HCl, 9.87 wt% FeCl3, and 3.76 wt% H3PO4 (Fe / P molar ratio = 1.59) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 6.2. The mixture was then filtered, and the P ion concentration in the filtrate was 1.9 ppm as measured by inductively coupled plasma mass spectrometry (ICP-MS). By visual observation, the mixture was flowable and filterable. (Example 18)
[0066] 200 grams of an aqueous solution containing 15.0 wt% HCl, 9.87 wt% FeCl3, and 3.76 wt% H3PO4 (Fe / P molar ratio = 1.59) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 8.0. The mixture was then filtered, and the P ion concentration in the filtrate was measured by inductively coupled plasma mass spectrometry (ICP-MS) to be 1.3 ppm. By visual observation, the mixture was flowable and filterable. (Example 19)
[0067] 200 grams of an aqueous solution containing 20.0 wt% HCl, 9.87 wt% FeCl3, and 3.76 wt% H3PO4 (Fe / P molar ratio = 1.59) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 7.3. The mixture was then filtered, and the P ion concentration in the filtrate was 2.0 ppm as measured by inductively coupled plasma mass spectrometry (ICP-MS). By visual observation, the mixture was flowable and filterable. (Example 20)
[0068] 200 grams of an aqueous solution containing 15.0 wt% HCl, 9.87 wt% FeCl3, and 3.76 wt% H3PO4 (Fe / P molar ratio = 1.59) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 4.3. The mixture was then filtered, and the Fe and P ion concentrations in the filtrate measured by inductively coupled plasma mass spectrometry (ICP-MS) were 0.21 ppm and 0.12 ppm, respectively. Example 21
[0069] 200 grams of an aqueous solution containing 15.0 wt% HCl, 9.87 wt% FeCl3, and 3.76 wt% H3PO4 (Fe / P molar ratio = 1.59) was added to a 500 mL glass beaker. CaO powder was slowly added to the beaker while stirring to adjust the solution pH to 9.6. The mixture was then filtered, and the Fe and P ion concentrations in the filtrate measured by inductively coupled plasma mass spectrometry (ICP-MS) were 141 ppm and 4.0 ppm, respectively.
[0070] As used herein, the phrase "within any range defined between any two of the preceding values" means that any range extends beyond any two of the values recited preceding such phrase, regardless of whether those values are in the lower portion of the recitation or the higher portion of the recitation. For example, a pair of values may be selected from two lower values, two higher values, or a lower value and a higher value.
[0071] While the present disclosure has been described in terms of exemplary designs, the present disclosure can be further modified within the spirit and scope of the present disclosure, and this application is intended to cover such departures from the present disclosure as come within known or customary practice in the art to which the disclosure pertains. The present invention includes the following aspects. [1] 1. A process for removing iron and phosphate ions from a waste stream comprising: Hydrogen chloride (HCl), FeCl 3 , FeCl 2、H 3 PO 4 and providing a waste stream containing at least one of water; The waste stream is exposed to a base to form FePO 4 , Fe(OH) 3 , Ca 3 (PO 4 ) 2 forming a precipitate comprising at least one insoluble compound selected from the group consisting of: and separating said precipitate from said waste stream. [2] The waste stream after the separation step is 2 and, Fe ions less than 500 ppm, and and at least one of: less than 500 ppm phosphate ions. [3] The waste stream after the separation step is 2 and, Fe ions less than 10 ppm, and and at least one of the following: less than 10 ppm phosphate ions. [4] After the separating step, evaporating liquid from said waste stream; solid CaCl 2 and recovering the additional steps of: [5] The base may be potassium hydroxide (KOH), sodium hydroxide (NaOH), calcium oxide (CaO), calcium hydroxide (Ca(OH) 2 ), and combinations thereof. [6] The process of [1], wherein the pH of the second waste stream after the exposing step is 1 to 8. [7] The process according to [1], wherein the molar ratio of iron ions to phosphate ions in the second waste stream after the separation step is 1 to 10. [8] The process according to [1], wherein the molar ratio of iron ions to phosphate ions in the second waste stream after the separation step is 1 to 2. [9] 2. The process of claim 1, wherein the separating step comprises separating the precipitate from the waste stream by at least one method selected from the group consisting of filtration, sedimentation, flocculation, centrifugation, and combinations thereof.
[10] 1. A process for removing iron and phosphate ions from a waste stream comprising: Chlorinated hydrocarbons, tributyl phosphate (TBP) and / or triethyl phosphate (TEP), iron, FeCl 2 and / or FeCl 3 , TBP-FeCl 2 Complex and / or TBP-FeCl 3 Complexes, and TEP-FeCl 2 Complex and / or TEP-FeCl 3 providing a first waste stream containing organic matter, the first waste stream containing at least one of the complexes; The first waste stream is subjected to thermal oxidation to produce hydrogen chloride (HCl), FeCl 3 , FeCl 2、H 3 PO 4 and generating a second waste stream containing at least one of water. The second waste stream is exposed to a base to produce FePO 4 , Fe(OH) 3 , and Ca 3 (PO 4 ) 2 forming a precipitate comprising at least one insoluble compound selected from the group consisting of: and separating said precipitate from said second waste stream.
Claims
1. 1. A process for removing iron and phosphate ions from a waste stream comprising: H 3 P.O. 4 , FeCl 3 and providing a waste stream containing water. The waste stream is treated with calcium oxide (CaO), calcium hydroxide (Ca(OH) 2 ), and combinations thereof to form FePO 4 , Fe(OH) 3 , and Ca 3 (P.O. 4 ) 2 forming a precipitate comprising: separating the precipitate from the waste stream; evaporating liquid from said waste stream; recovering the solid CaCl 2 .
2. The waste stream after the separation step is 2 and, Fe ions less than 500 ppm, and 2. The process of claim 1, wherein the liquid phase comprises at least one of: less than 500 ppm phosphate ions.
3. The waste stream after the separation step is 2 and, Fe ions less than 10 ppm, and 3. The process of claim 2, wherein the liquid phase comprises at least one of: less than 10 ppm phosphate ions.
4. 2. The process of claim 1, wherein the pH of the waste stream after the exposing step is from 1 to 8.
5. 2. The process of claim 1, wherein the molar ratio of iron ions to phosphate ions in the waste stream after the separation step is from 1 to 10.
6. 2. The process of claim 1, wherein the molar ratio of iron ions to phosphate ions in the waste stream after the separation step is from 1 to 2.
7. 2. The process of claim 1, wherein the separating step comprises separating the precipitate from the waste stream by at least one method selected from the group consisting of filtration, sedimentation, flocculation, centrifugation, and combinations thereof.
8. 1. A process for removing iron and phosphate ions from a waste stream comprising: Chlorinated hydrocarbons, tributyl phosphate (TBP) and / or triethyl phosphate (TEP), iron, FeCl 2 and / or FeCl 3 , TBP-FeCl 2 Complex and / or TBP-FeCl 3 Complexes, as well as TEP-FeCl 2 Complex and / or TEP-FeCl 3 providing a first waste stream containing organic matter, the first waste stream containing at least one of the complexes; The first waste stream is subjected to thermal oxidation to produce H 3 P.O. 4 , FeCl 3 and generating a second waste stream containing water. The second waste stream is treated with calcium oxide (CaO), calcium hydroxide (Ca(OH) 2 ), and combinations thereof to form FePO 4 , Fe(OH) 3 , and Ca 3 (P.O. 4 ) 2 forming a precipitate comprising: and separating said precipitate from said second waste stream.
9. The method of claim 1, wherein the second waste stream after the separation step comprises: Fe ions less than 500 ppm, and 9. The process of claim 8, wherein the liquid phase comprises at least one of: less than 500 ppm phosphate ions.
10. The method of claim 1, wherein the second waste stream after the separation step comprises: Fe ions less than 10 ppm, and 10. The process of claim 9, wherein the liquid phase comprises at least one of: less than 10 ppm phosphate ions.
11. After the separation step, evaporating liquid from the second waste stream; 9. The process of claim 8 further comprising the additional step of: recovering the solid CaCl2.
12. The process of claim 8, wherein after the exposing step, the second waste stream comprises a total concentration of FeCl 3 and FeCl 2 of less than 20% by weight.
13. The process of claim 8, wherein after the exposing step, the second waste stream comprises a total concentration of H 3 PO 4 of less than 20% by weight.
14. The process of claim 8, wherein after the exposing step, the second waste stream contains less than 40% HCl by weight.
15. The process of claim 8, wherein the molar ratio of iron ions to phosphate ions in the second waste stream after the separation step is 1 to 10.
16. The process of claim 8, wherein the molar ratio of iron ions to phosphate ions in the second waste stream after the separation step is 1 to 2.
17. The process of claim 8, wherein the separating step comprises separating the precipitate from the second waste stream by at least one method selected from the group consisting of filtration, sedimentation, flocculation, centrifugation, and combinations thereof.
Citation Information
Patent Citations
Treatment of waste chemical washing liquid
JP1986054284A
Waste water sludge treatment method
JP1998511601A
Method for recovering iron phosphate
JP2016172654A
Production of phosphate compounds from materials containing phosphorus and at least one of iron and aluminum
JP2016527162A