Thin films for solar concentrators
A multilayer thin film with chromophore-infused PVB layers enhances light confinement and transmission efficiency, addressing photon leakage issues and enabling LSCs for building integration.
Patent Information
- Application Number
- JP2021571370
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-05-31
- Filing Date
- 2020-05-29
- Publication Date
- 2024-09-24
- Estimated Expiration
- 2040-05-29
AI Technical Summary
Existing luminescent solar concentrators (LSCs) face performance losses due to photon leakage mechanisms, such as reflection, absorption, reabsorption, and refractive escape, and the use of plastic matrices limits their application in the building sector due to flammability and low thermal stability.
A multilayer thin film with a chromophore-infused first layer and a second transparent layer, made of polyvinyl butyral (PVB), promotes total internal reflection and structural integrity, allowing for efficient light confinement and integration with glass surfaces.
The multilayer thin film enhances light confinement and transmission efficiency, enabling LSCs to be used in building applications while maintaining structural strength and safety.
Smart Images

Figure 0007555361000002 
Figure 0007555361000001 
Figure 0007555361000006
Abstract
Description
[Technical field]
[0001] The present invention relates to thin films designed to make luminescent solar concentrators, and more particularly to multilayer luminescent thin films for solar concentrators. [Background technology]
[0002] Luminescent solar concentrators (hereafter referred to as LSCs) are photovoltaic devices based on sheets or thin films functionalized with transparent photoluminescent and / or colored substances (hereafter referred to as chromophores), which are able to capture and reintroduce a portion of the incident solar radiation. A portion of the radiation emitted by the chromophores remains trapped inside the thin film / sheet due to the phenomenon of total internal reflection.
[0003] If the solar concentrator has a sufficiently smooth air interface, the portion of the fluorescent light trapped inside the sheet or thin film will experience multiple reflection processes from one interface to another and reach its boundary. On the lateral surfaces of the concentrator, there are photovoltaic cells that convert a portion of the luminescent radiation trapped inside the sheet / thin film into an electric current. This electric current can be advantageously used to power external users (illumination systems, charging systems, shading or integrated lighting systems, etc.), can be stored in a storage system, or can be introduced into the power grid.
[0004] Compared to flat photovoltaic systems and conventional concentrated photovoltaic systems (hereafter referred to as CPV), LSC devices have many and important advantages. The main advantages are: a) A significant reduction in the amount of semiconductor material used. b) Use of direct and diffuse solar radiation components: Solar radiation is converted with the same efficiency regardless of the position and orientation of the panel and regardless of the inclination of the capture surface (i.e. horizontal, vertical and / or oblique tilt), with the resulting advantage of being able to use the LSC device both on sides that are directly exposed to the sun (i.e., facing south) and on sides that are only exposed to the diffuse component (i.e., facing north). c) Good heat dissipation due to the large area of the collector panel placed in contact with the outside environment, which allows the photovoltaic receivers bonded to the edge of the sheet to function under reduced temperature conditions, which gives them a high conversion efficiency (the effectiveness of real commercial semiconductors decreases with increasing operating temperature). d) Absence of a solar tracking system: this feature, which makes LSC photovoltaic panels unique in comparison with conventional CPV panels, on the one hand significantly increases the architectural integration of the device and, on the other hand, considerably reduces costs, weight and maintenance activities. e) The possibility of identifying chromophores that allow a high degree of overlap between their own emission spectrum and the spectral response curve of the photovoltaic cell: this allows the cell to operate while maximizing the conversion efficiency and minimizing its overheating and any damage.
[0005] However, the performance of an LSC device depends on different leakage mechanisms, the first of which is related to sunlight that does not reach the luminescent chromophores due to the reflection of a portion of the photons at the surface of the sheet, the second loss mechanism can be attributed to the chromophore system and in particular to the following phenomena: i) The chromophores are characterized by a particular spectral region in which they have a high absorption coefficient and within which the luminous radiation is not absorbed and passes through to the opposite surface of the sheet. ii) A portion of the absorbed photons is not re-emitted by the chromophore and is dissipated in the form of heat. iii) The light re-emitted by the chromophores is refracted by the matrix within which, instead of being internally reflected, the chromophores are dispersed through a so-called "escape cone". iv) Re-absorption of photons emitted by a first portion of the chromophore present inside the luminescent film by a second portion of the chromophore: This phenomenon occurs due to a possible partial overlap of the emission and absorption bands of the luminescent substances.
[0006] The third leakage mechanism originates from the transparent matrix and includes the following potential limitations: i) the material of the sheet is not completely transparent over the entire range of wavelengths of light emitted by the chromophores and this creates light absorption and therefore a loss in performance. ii) Imperfections in the surface finish can introduce refractions at the exterior of the luminescent sheet / thin film, thereby reducing the luminous intensity perceived by the photovoltaic cell.
[0007] A fourth loss mechanism is linked to photovoltaic cells, which in fact have a spectral response that depends on the wavelength of the incident photons and are not able to convert the entire emission spectrum in an optimal manner.
[0008] The use of chromophores with a large Stokes shift (difference in wavelength between the peak of the absorption spectrum and the peak of the emission spectrum) allows for a dramatic reduction in chromophore self-absorption, the second leakage mechanism, while absorption by the inert matrix can be reduced by using materials with high transparency.
[0009] The most well-known and most widely tested method for producing LSC sheets consists of dispersing chromophores in a transparent matrix of plastic material, in particular polymethylmethacrylate (PMMA) or polycarbonate (PC). Although the use of plastic material has the advantages of reduced weight (relative to glass) and relatively large versatility and relatively low production costs, it is not particularly suitable for use in the building sector, the relatively large degree of flammability, the emission of fumes in case of combustion and the relatively low resistance to scratches constituting aspects that significantly limit the applicability of LSC systems in the building sector.
[0010] On the other hand, the inclusion of chromophores inside a glassy matrix is extremely difficult, since chromophore complexes are usually characterized by components of organic nature and these usually degrade irreversibly at temperatures above 150-200° C., while the temperatures for processing glass are much higher.
[0011] An example of a luminescent solar concentrator is described in US 2015 / 194555, where a single layer thin film functionalized with chromophores is inserted between two sheets of glass or plastic material. Confinement of fluorescent radiation is facilitated due to the difference in refractive index between the outer surface of the outer sheet and air. Summary of the Invention [Problem to be solved by the invention]
[0012] The object of the present invention is to provide a thin film for luminescent solar concentrators that is easy and cheap to manufacture, and which can be used in the architectural sector without the above-mentioned drawbacks. [Means for solving the problem]
[0013] The above object is fully achieved by the thin film for luminescent solar concentrators according to the invention, as characterized in the appended claims.
[0014] The invention will now be described, by way of non-limiting example, with reference to the accompanying drawings in which: [Brief description of the drawings]
[0015] [Figure 1] 1 shows a graph of the spectral power density of a solar source (S) in comparison with the absorption spectrum (A) and emission spectrum (E) of a chromophore used in a luminescent solar concentrator (LSC). [Diagram 2] 1 shows a luminescent solar concentrator (LSC) made in accordance with the present invention. [Diagram 3] 3 shows a multi-layer thin film fabricated in accordance with the present invention and used in the luminescent solar concentrator (LSC) of FIG. 2. [Figure 4] Referring to FIG. 2, the optical path of a light ray emitted by a color center is shown diagrammatically. [Diagram 5] FIG. 3 is a perspective view of the luminescent solar concentrator (LSC) of FIG. 2. [Figure 6] 1 shows a graph of the refractive index increase measured in a sample of PVB (polyvinyl butyral) mixed with a chromophore based on a perylene compound. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0016] With reference to FIG. 3, reference number 1 indicates as a whole a plastic thin film designed for producing a luminescent solar concentrator.
[0017] The thin film 1 comprises a first plastic layer (thin film) 19 mixed with chromophores dispersed therein and covered on both sides or faces by a respective transparent second layer (thin film) 18 which in the illustrated example is thicker than the first layer 19.
[0018] The film 1 according to the invention is preferably a multilayer film, as referred to below, designed as described in more detail below for producing layered glass.
[0019] The first layer 19 has a thickness of 1 μm to 150 μm.
[0020] Each second layer 18 has a thickness between 160 μm and 3200 μm. Preferably, each second layer 18 has a thickness substantially less than 1600 μm in such a way that the total thickness of the multilayer thin film 1 is substantially less than 3200 μm. Preferably, the two second layers 18 have the same thickness.
[0021] The first layer 19 is preferably made from PVB (polyvinyl butyral).
[0022] The second layer 18 is also preferably made from PVB (polyvinyl butyral).
[0023] Advantageously, layers 18 and 19 are made of the same material, and the presence of chromophores in the first layer modifies the refractive index of the material, thus promoting confinement by total internal reflection. In a variant embodiment not shown, the first layer 19 is bonded on only one of its two sides to a respective second transparent plastic covering layer 18. In this case, the second layer 18 preferably has a thickness substantially less than 3600 μm.
[0024] In a further variant embodiment not shown, the thin film 1 can comprise a number n of layers greater than three, again with an optically active intermediate layer (layer 19) having a thickness between 1 and 150 μm.
[0025] In all the above mentioned cases (i.e. structures with three or more layers, symmetrical or not, or two-layer or multi-layer structures), the total thickness of the thin film 1 is such that it is possible to include the latter as an intermediate layer in a layered glass and to use it in particular in architectural work, for example to manufacture windows or covering panels.
[0026] Thus, as shown in Figures 2 to 5, the thin film 1 can be interposed in the form of a thin film between two sheets of glass 2 in order to optimize the bond, so as to increase the structural strength and to prevent the dispersion of glass fragments in case of breakage. At the same time, the layered glass provided with the thin film 1 according to the invention can be associated with a LSC device of known type, including a set of bypass diodes 4 (optional), an electrical connector 5 and a photovoltaic cell 6.
[0027] In fact, the film 1 is a luminescent plastic film, characterized by the presence of chromophores capable of absorbing a portion of the solar radiation and of intercalating it isotropically.
[0028] The process leading to the layered glass is a lamination process which can occur by using heated rollers or in an autoclave at temperatures between 120° C. and 150° C., compatible with non-degradation of the chromophore system.
[0029] The PVB from which layer 18 (or single layer 18) is made is cut from a roll, while the PVB from which layer 19 is made comes from a specific process which will be described below.
[0030] First, it is noted that the inherent physical-chemical properties of PVB do not allow dissolving this material to incorporate chromophores inside it, so it is necessary to use a technique that involves dissolving the PVB in a solvent, mixing the chromophore powder, and subsequent redeposition of the additional PVB by evaporation of the solvent.
[0031] According to the first embodiment, the first layer 19 is made of a perylene chromophore, a naphthalene derivative (2-(2-ethylhexyl)-6,7-dimethoxy-1H-benzo[de]isocyanoline-1,3(2H)-dione), a rhodamine compound (C 28 H 31 The luminescent organic compounds preferably include one or more types or varieties of chromophores based on luminescent organic compounds selected from ClN2O3), 3-hydroxyflavone, 4-dicyanomethyl-6-dimethylaminostyryl-4H-pyran (DCM).
[0032] In this case, as described below, the first layer 19 has a density of 1.0 mg / cm 3 The present invention relates to a chromophore-based luminescent organic compound having a chromophore concentration of greater than 1000 nm.
[0033] According to a second embodiment, the first layer 19 comprises one or more types or varieties of chromophores based on lanthanide compounds, preferably selected from chromophores based on compounds of europium (Eu), yttrium (Y), lanthanum (La), gadolinium (Gd), erbium (Er), and terbium (Tb), neodymium (Nd), ytterbium (Yb).
[0034] In this case, as described below, the first layer 19 has a density of 2.0 mg / cm 3 The present invention includes chromophores based on lanthanide compounds having a chromophore concentration of greater than 1000 nm.
[0035] According to a third embodiment, the first layer 19 comprises one or more types or varieties of luminescent crystals and / or nanocrystals based chromophores preferably selected from silicon (Si), cadmium selenide (CeSe), lead sulfide (PbS), lead selenide (PbSe), zinc selenide (ZeSe), copper indium sulfide (CuInS2), the composite system CdSe / CdS, the composite system PbS / CdS, copper based composite systems (Cu) and CdSe, manganese based composite systems (Mn) and ZeSe.
[0036] In this case, as described below, the first layer 19 has a density of 0.4 mg / cm3 The present invention includes luminescent crystal and / or nanocrystal based chromophores having a chromophore concentration of greater than 100 nm.
[0037] With reference to the above, it has indeed been found experimentally that the production of thin film layers 19 having a density of chromophores above a threshold value, depending on the type of molecules used, results in large variations in the refractive index of the material.
[0038] Figure 6 shows the increase in refractive index measured in PVB samples mixed with chromophores based on perylene compounds, and similar behavior was also found for chromophores based on naphthalene, lanthanide, and colloidal crystalline complexes.
[0039] As a result of this increase in refractive index, the luminous radiation re-emitted by the chromophore remains primarily confined inside the first layer 19, thereby experiencing total internal reflection at the interface with the transparent layer 18.
[0040] In practice, the first plastic layer 19 has a first refractive index and the second unmixed layer 18 has a second refractive index less than the first refractive index so as to promote confinement by total internal reflection of the luminous radiation inside the first layer 19.
[0041] Advantageously, total reflection occurs primarily inside layer 19 mixed with the chromophore due to the increase in refractive index promoted by the presence of the chromophore itself relative to layer 18 .
[0042] This effect, which is common to all the above mentioned chromophores, is significant only above a certain concentration of the chromophores.
[0043] The "threshold" concentration varies according to the type of chromophore used. i. In the case of organic chromophores, 1.1 mg / cm 3 A threshold concentration of the chromophore has been found. ii. In the case of lanthanide-based chromophores, 2.1 mg / cm3 A threshold concentration of the chromophore has been found. iii. In the case of colloidal nanocrystal-based chromophores, 0.5 mg / cm 3 A threshold concentration of 0.01 has been found.
[0044] According to a further embodiment, the first layer 19 may contain chromophores of one or more of the above mentioned types or kinds in coexistence with the above mentioned individual concentrations.
[0045] According to any of the techniques described above, the first layer 19 is prepared from a solution of PVB (polyvinyl butyral) dissolved and mixed with chromophores based on organic complexes and / or complexes based on the lanthanide series and / or complexes based on inorganic crystals / nanocrystals, as described above. The mixture is then coated on an inert substrate to form the first layer 19. Airbrush or It is deposited by roll printing and then peeled off from the inert substrate after drying.
[0046] Layer 19 is then bonded to one or more second layers 18 by roller lamination.
[0047] Alternatively, the mixture described above is deposited by roll printing directly onto the second layer 18 .
[0048] In the latter case, the set of layers 18 and 19 may optionally be joined after at least one further layer 18 by roller lamination.
[0049] airbrush The deposition technique using has the advantage of allowing the deposition of large surfaces using automated equipment that is widely designed and industrialized. Another aspect linked to this deposition technique is that it promotes the evaporation of the solvent due to the high surface / volume ratio. In fact, layers with a relatively large thickness require a much longer time to obtain solidification of the thin film due to the relatively slow process of diffusion of the solvent towards the surface and the subsequent evaporation.
[0050] However, the thickness of the layer (thin film) obtained by this deposition technique is very reduced and is generally less than 10 μm, regardless of the amount of solvent used. After deposition, the thin film produced does not have a thickness that allows it to be easily handled and requires an inert and transparent support substrate. Moreover, the very reduced thickness of the thin film that can be produced by this technique makes it less suitable to be used as such as an encapsulation material for layered glass. For this reason, the layer 19 thus obtained is bonded to (or formed directly on) one or more layers 18, as described above.
[0051] The roll printing deposition technique allows layers (thin films) to be produced with a thickness typically greater than 10 μm due to the reduced solvent content. The thickness of thin films produced by roll printing is less than 150 μm, typically less than 100 μm.
[0052] Also in this case, the thickness of the thin film is not such that it can be used directly for lamination of layered glass, and in this case the layer 19 thus obtained is bonded to (or formed directly on) one or more layers 18, as described above.
[0053] The technique described for producing the first layer 19 (active thin film) and its adhesion (or formation) on at least a second transparent layer 18 having a relatively large thickness allows a multilayer thin film 1 to be produced having a total thickness suitable for direct use as a thin film for producing layered glass.
[0054] In other words, the described invention is based on the use of plastic matrix multilayers, where only one layer (first layer 19) is mixed with chromophores, while at least one other layer (second layer 18) is optimized to ensure the structural, transparency and adhesion properties of glass. This solution allows the production of luminescent solar devices with exposed glass surfaces, which use a wide range of chromophore systems suitably dispersed in a plastic matrix as active material.
[0055] One of the advantages derived from the present invention is the improved efficiency of transmitting luminous radiation 11 (FIG. 4) due to the relatively effective confinement of the radiation within the first thin layer 19 .
[0056] Advantageously, the light 11 re-emitted by the chromophores and mainly trapped inside the first thin layer 19 is therefore transmitted in a clearly better manner than if the luminous radiation 10 were transmitted inside the entire thickness of the layered glass. The outer surface of the sheet of glass 2 may in fact be coated or covered with a thin layer of powder, which may thus adversely affect the correct transmission of the fluorescent radiation 10. On the other hand, according to the invention, the luminous radiation 11 remains trapped inside the first layer 19, the separation interface of which is always clear, clean and protected from dust or dirt. The edges of the multilayer thin film 1 and especially of the first layer 19 are therefore able to transmit the luminous radiation towards the photovoltaic cells 6 of the LSC device in an optimal and efficient manner.
[0057] More specifically, Figures 2, 4 and 5 show a multilayer thin film 1 containing within it a chromophore-rich region embedded between two sheets of glass 2. The multilayer thin film 1 performs the function of encapsulation as well as that of optically active material for luminescence purposes. The above-mentioned photovoltaic cells 6 are positioned on the boundary in the form of an array in order to convert the luminous radiation into electricity.
[0058] The border portions of the glass sheet 2 are advantageously covered by reflective strips 8 designed to prevent any elements for fixing the sheet from reducing the efficiency of transmitting luminous radiation towards the photovoltaic cell 6. The above-mentioned bypass diodes 4 and the above-mentioned electrical connectors 5 are mounted on a printed circuit 9 on top of which the photovoltaic cell 6 is housed.
[0059] The incident solar radiation 3 penetrates inside the multilayer thin film 1 and is partially absorbed. The remaining part 7 of the radiation absorbed by the chromophores is transmitted. The multilayer thin film 1 transmits a large part 11 of the fluorescent radiation inside the first layer 19. Due to the relatively large confinement effect introduced by the first layer 19, which has a high refractive index, the part of the luminous radiation 10 that is confined inside the sheet of glass 2 has a significantly smaller intensity than the part of the luminous radiation 11. This phenomenon makes it possible to illuminate the photovoltaic cell 6 in its central region, away from any recombination centers present in the peripheral regions of the cell 6. [Prior art documents] [Patent documents]
[0060] [Patent Document 1] US Patent Application Publication No. 2015 / 194555
Claims
1. A thin film for producing layered glass, comprising: a first plastic layer (19) made from PVB (polyvinyl butyral), having a first refractive index and having a chromophore additive dispersed therein; At least one second transparent plastic layer (18) having a second refractive index less than the first refractive index and a thickness greater than the first plastic layer (19), made from PVB (polyvinyl butyral) without additives, covering the first plastic layer; Including, the second transparent plastic layer is bonded to the first and / or second surface of the first plastic layer to promote confinement of luminous radiation inside the first plastic layer (19) by total internal reflection; the first plastic layer (19) being a thin film layer having the first refractive index increased by the presence of the chromophore; Thin film.
2. The first plastic layer (19) has a thickness of 1 μm to 150 μm. The thin film of claim 1.
3. The second transparent plastic layer (18) has a thickness of 160 μm to 3200 μm. The thin film according to claim 1 or 2.
4. the first plastic layer (19) is covered on both the first side and the second side by the respective second transparent plastic layer (18); The thin film according to any one of claims 1 to 3.
5. The two second transparent plastic layers (18) have the same thickness; The thin film according to claim 4.
6. The first plastic layer (19) is made of a perylene chromophore, a naphthalene derivative (2-(2-ethylhexyl)-6,7-dimethoxy-1H-benzo[de]isochinoline-1,3(2H)-dione), a rhodamine compound (C 28 H 31 ClN 2 O 3 ), 3-hydroxyflavone, and 4-dicyanomethyl-6-dimethylaminostyryl-4H-pyran (DCM), The thin film according to any one of claims 1 to 5.
7. The first plastic layer (19) has a thickness of 1.0 mg / cm 3 luminescent organic compound-based chromophores having a concentration of greater than The thin film according to claim 6.
8. the first plastic layer (19) comprises one or more types of chromophores based on lanthanide compounds selected from chromophores based on compounds of europium (Eu), yttrium (Y), lanthanum (La), gadolinium (Gd), erbium (Er), terbium (Tb), neodymium (Nd) and ytterbium (Yb); The thin film according to any one of claims 1 to 7.
9. The first plastic layer (19) has a thickness of 2.0 mg / cm 3 and a lanthanide compound-based chromophore having a concentration of greater than 1000 nm. The thin film according to claim 8.
10. The first plastic layer (19) may be made of any of a variety of materials, including silicon (Si), cadmium selenide (CdSe), lead sulfide (PbS), lead selenide (PbSe), zinc selenide (ZnSe), copper indium sulfide (CuInS 2 ), comprising one or more types of chromophores based on luminescent crystals and / or nanocrystals selected from among the composite systems CdSe / CdS, the composite systems PbS / CdS, composite systems based on copper (Cu) and CdSe, composite systems based on manganese (Mn) and ZnSe, The thin film according to any one of claims 1 to 9.
11. The first plastic layer (19) has a thickness of 0.4 mg / cm 3 luminescent crystals and / or nanocrystal-based chromophores having a concentration of greater than The thin film of claim 10.
12. The first plastic layer (19) and the second transparent plastic layer (18) are bonded together by roller lamination. A thin film according to any one of claims 1 to 11.
13. said first plastic layer (19) being made from a mixture comprising a solution of dissolved PVB (Polyvinyl Butyral) and chromophores based on organic compounds and / or compounds based on the Lanthanide series and / or compounds based on inorganic crystals and / or nanocrystals; The first plastic layer (19) is obtained by depositing the mixture by airbrush or roll printing, A thin film according to any one of claims 1 to 12.
14. said first plastic layer (19) being made from a mixture comprising a solution of dissolved PVB (Polyvinyl Butyral) and chromophores based on organic compounds and / or compounds based on the Lanthanide series and / or compounds based on inorganic crystals and / or nanocrystals; The second transparent plastic layer (18) is obtained by depositing the mixture by airbrush or roll printing. A thin film according to any one of claims 1 to 11.
15. At least two sheets of glass (2); A multilayer film (1) according to any one of claims 1 to 14, interposed between said at least two sheets; Including, Layered glass.
Citation Information
Patent Citations
Efficient solar energy fluorescence condenser
CN103236462A
Solar modules with improved efficiency through the use of spectral concentrators.
JP2010531067A
Alignment method between resin film and substrate
JP2013105752A
Wavelength conversion material as enclosure for solar module system for improving photovoltaic collection efficiency
JP2013123037A
Solar cell module and photovoltaic power generation apparatus
JP2013175513A