Power Cable

The cable design with specific coating layer compositions addresses UV and oxidation issues, enhancing durability and reducing maintenance needs by using an ultraviolet absorber and controlled calcium carbonate content in the coating layers.

JP7555779B2Active Publication Date: 2024-09-25KK TOSHIBA
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2020173274
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-14
Publication Date
2024-09-25
Estimated Expiration
2040-10-14

AI Technical Summary

Technical Problem

PVC power transmission cables used outdoors in solar power generation suffer from UV deterioration and oxidation, leading to insulation failure and high maintenance costs due to frequent replacements.

Method used

A power transmission cable design with a core and multiple coating layers, where the outermost layer contains an ultraviolet absorber and light stabilizer, and the innermost layer contains calcium carbonate, with a lower calcium carbonate content in the outermost layer to prevent oxidative deterioration and leaching, thereby enhancing durability.

Benefits of technology

The cable maintains insulation and extends the replacement cycle by preventing cracks and fissures, ensuring long-term durability even under direct sunlight exposure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007555779000001
    Figure 0007555779000001
  • Figure 0007555779000002
    Figure 0007555779000002
  • Figure 0007555779000003
    Figure 0007555779000003
Patent Text Reader

Abstract

To provide a power transmission cable having excellent durability.SOLUTION: According to an embodiment, a power transmission cable 1 has a core 3 having an insulated wire 2, and a plurality of coating layers 4 provided on an outer periphery of the core 3. Of the plurality of coating layers 4, an outermost coating layer 4b includes an ultraviolet absorber and a photostabilizer, and an innermost coating layer 4a includes calcium carbonate. The content of calcium carbonate of the outermost coating layer 4b is lower than the content of calcium carbonate of the innermost coating layer 4a.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] SUMMARY OF THE DISCLOSURE An embodiment of the present invention relates to a cable for transmitting electrical current. [Background technology]

[0002] Polyvinyl chloride (PVC) cables, which are used for power transmission in solar power generation and other applications, can develop cracks on their surface due to UV degradation and oxidation when laid outdoors, making it difficult to maintain their insulation. To prevent this, it is customary for general installed cables to be replaced every five years. However, solar panels are installed in places where maintenance is difficult, such as on roofs, so they cannot be easily replaced. For this reason, there is a demand for improved weather resistance of cables with a coating layer that includes PVC. There is also a demand for general installed cables to reduce risk by improving their durability and to reduce costs by extending the replacement cycle. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2019-179628 A [Patent Document 2] JP 2016-71984 A [Patent Document 3] JP 2006-54056 A [Patent Document 4] Japanese Patent Application Publication No. 7-11084 [Patent Document 5] Japanese Patent Application Publication No. 1-210339 [Patent Document 6] Japanese Utility Model Application Publication No. 4-8317 [Patent Document 7] Japanese Utility Model Application Publication No. 4-99614 Summary of the Invention [Problem to be solved by the invention]

[0004] The present invention has been made in consideration of the above circumstances, and has an object to provide a power transmission cable having excellent durability. [Means for solving the problem]

[0005] According to an embodiment, there is provided a power cable including a core including an insulated wire and a plurality of coating layers provided on the outer periphery of the core. Among the plurality of coating layers, an outermost coating layer includes an ultraviolet absorbing agent and a light stabilizer, and an innermost coating layer includes calcium carbonate. A content of 9% by weight or more but less than 16% by weight The calcium carbonate content of the outermost coating layer is less than the calcium carbonate content of the innermost coating layer. [Brief description of the drawings]

[0006] [Figure 1] FIG. 1 is a cross-sectional view illustrating an example of a power transmission cable according to an embodiment. [Diagram 2] FIG. 2 is a schematic diagram illustrating an example of an extrusion molding device used in manufacturing the power transmission cable according to the embodiment. [Diagram 3] 1 is a graph showing the relationship between the calcium carbonate content, the bending radius, and the number of bending times before breaking for the insulated wire of Experiment 1. [Figure 4] FIG. 2 is a schematic diagram showing a bending durability test method for an insulated wire. [Diagram 5] 13 is a graph showing the relationship between the plasticizer content, bending radius, and number of bending breaks in the insulated wire of Experiment 2. [Figure 6] FIG. 2 is a cross-sectional view illustrating a schematic diagram of an insulated electric wire used in Experiments 1 and 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0007] An example of the power transmission cable according to the embodiment is a solar cable, specifically a power transmission cable for photovoltaic power generation. The power transmission cable of the embodiment includes a core including an insulated wire, and a plurality of coating layers provided on the outer periphery of the core. The number of coating layers may be two or more. Of the plurality of coating layers, the outermost coating layer includes an ultraviolet absorber and a light stabilizer. The innermost coating layer includes calcium carbonate. The calcium carbonate content of the outermost coating layer is set to be less than the calcium carbonate content of the innermost coating layer. Hereinafter, the power transmission cable of the embodiment will be described with reference to FIG. 1. FIG. 1 is a cross-sectional view that typically shows a cross section obtained when the power transmission cable is cut in a direction intersecting with the longitudinal direction.

[0008] The power transmission cable 1 of the embodiment includes a core 3 having one or more insulated wires 2, and a plurality of coating layers 4. Reference symbol D in Fig. 1 indicates the outer diameter of the cable 1. For example, in the case of a four-core 600V CV cable, the outer diameter of the cable 1 is 5.5 mm for the insulated wires. 2 In this case, the finished outer diameter of the cable can be 16 mm or more. A plurality of insulated electric wires 2 (for example, 4) are used in the cable 1 shown in FIG. 1. Each of the insulated electric wires 2 is formed of a plurality of linear conductors 5 and an insulator 6. The conductors 5 are formed, for example, from copper. The plurality of conductors 5 are adjacent to each other and are gathered together, and the cross section of the assembled outer shape is approximately circular. The assembly of conductors 5 is bundled together by covering the outer periphery with an insulator 6. The insulated electric wires 2 having the above structure are arranged so that the outer peripheries (insulators 6) are adjacent to each other, and these insulated electric wires 2 are bundled together by the intervening space 7 present in the gap between the outer periphery and the insulated electric wires 2 so that the cross section is circular, thereby forming the core 3. The intervening space 7 can be formed, for example, from an insulating material such as paper or resin. The outer periphery of the core 3 is covered with a coating layer 4 having a two-layer structure, for example. The coating layer 4 protects the core 3 and maintains the insulation of the cable 1. The coating layer 4a located on the inside is in contact with the outer peripheral surface of the core 3 and functions as the innermost coating layer 4a. The coating layer 4b located on the outside is in contact with the innermost coating layer 4a, forms the outer peripheral surface of the cable 1, and functions as the outermost coating layer 4b. There is a seam between the innermost coating layer 4a and the outermost coating layer 4b.

[0009] The innermost coating layer 4a and the outermost coating layer 4b are each formed of an insulating composition containing an insulating resin such as polyvinyl chloride (PVC). The composition contains additives in addition to the insulating resin. Examples of additives include plasticizers and calcium carbonate. The plasticizer provides flexibility to the coating layer. On the other hand, calcium carbonate is intended to increase the structural stability and impact resistance of the coating layer. The proportion of these additives in the coating layer is not small. Power cables, which are often used outdoors, can be affected by weather such as direct sunlight and rain. When a cable is used outdoors for a long period of time, the additives in the coating layer are leached or desorbed due to the effects of ultraviolet rays, heat, or moisture. As a result, the durability of the coating layer decreases, as described below.

[0010] Additives in the coating layer, such as plasticizers, undergo autoxidation starting from molecular chain scission due to thermal degradation or ultraviolet light. Oxidation causes a decrease in the mechanical strength of the coating layer, such as a decrease in elongation retention, fatigue strength, and toughness.

[0011] Furthermore, when the power transmission cable is used outdoors, the amount of plasticizer in the coating layer decreases due to the effects of moisture or heat, and the durability of the coating layer decreases.

[0012] On the other hand, calcium carbonate is originally difficult to dissolve in water, but as shown in the reaction formula (1) below, it reacts with water containing carbon dioxide to become calcium bicarbonate, which becomes highly soluble in water.

[0013] CaCO 3 + CO 2 + H 2 O → Ca(HCO 3 ) 2 (1) When calcium carbonate is dissolved from the coating layer by the above mechanism, the dissolved portion becomes hollow, forming many holes in the coating layer. The holes caused by calcium carbonate dissolution become the starting points for oxidation and cracks. The structure of the coating layer becomes weak due to dissolution, so the wear resistance or impact resistance of the coating layer decreases.

[0014] In order to improve the durability of the coating layer 4, the coating layer 4 is configured as follows. The outermost coating layer 4b contains an ultraviolet absorber and a light stabilizer. The innermost coating layer 4a contains calcium carbonate. The calcium carbonate content of the outermost coating layer 4b is less than that of the innermost coating layer 4a. The outermost coating layer 4b may or may not contain calcium carbonate.

[0015] When the power cable 1 is used outdoors, the outermost coating layer 4b is greatly affected by the exposure atmosphere, specifically, ultraviolet rays, heat, or moisture, but the ultraviolet absorber and light stabilizer can suppress the oxidation and deterioration of additives such as plasticizers. Therefore, the decrease in additives can be suppressed. In addition, by making the content of calcium carbonate in the outermost coating layer 4b less than the content of calcium carbonate in the innermost coating layer 4a, the amount of calcium carbonate eluted from the outermost coating layer 4b can be reduced. As a result, the mechanical strength, abrasion resistance, and impact resistance of the outermost coating layer 4b can be suppressed from decreasing, and therefore the destruction of the outermost coating layer 4b due to cracks, fissures, etc. can be prevented. As a result, the outermost coating layer 4b blocks the effects of ultraviolet rays, heat, and moisture on the innermost coating layer 4a, so that the innermost coating layer 4a does not undergo oxidation and leaching of the plasticizer, or degeneration and elution of the calcium carbonate. Therefore, the function of the coating layer 4 can be maintained for a long period of time, and the durability of the power cable 1 can be improved. Even if a power transmission cable is placed on the back side of a solar panel, in actual wiring, some of the cable will protrude and it will be unavoidable that the cable will be exposed to direct sunlight. The power transmission cable 1 of this embodiment can achieve high durability even under direct sunlight.

[0016] The coating layer will be described in further detail below.

[0017] In the above-mentioned FIG. 1, an example in which the coating layer is made up of two layers has been described, but the number of layers is not limited to two, and the coating layer may be made up of three or more layers.

[0018] Each layer constituting the coating layer is formed of an insulating composition containing an insulating resin such as PVC. The insulating resin is preferably the main component in each layer. Here, the main component is the component that is present in the largest amount among the components constituting each layer. It is more preferable that the insulating resin content in each layer is 50% by weight or more.

[0019] As described above, the outermost coating layer contains an ultraviolet absorber and a light stabilizer. The outermost coating layer may or may not contain calcium carbonate. On the other hand, the innermost coating layer may contain calcium carbonate and may or may not contain an ultraviolet absorber and a light stabilizer. When the innermost coating layer contains an ultraviolet absorber and a light stabilizer, the content of the ultraviolet absorber and the light stabilizer in the innermost coating layer can be less than the content of the ultraviolet absorber and the light stabilizer in the outermost coating layer. This is because the durability of the outermost coating layer is improved, so that the outermost coating layer can block the influence of ultraviolet rays, heat, and moisture on the innermost coating layer, and therefore even if the innermost coating layer does not contain an ultraviolet absorber and a light stabilizer, both the oxidation and leaching of the plasticizer and the denaturation and elution of calcium carbonate can be prevented.

[0020] The innermost coating layer may be free of ultraviolet absorbing agents and light stabilizers. The contents of the ultraviolet absorber and antioxidant in the outermost coating layer are preferably about 1% by weight and 0.15% by weight or more, respectively. The content of the light stabilizer in the outermost coating layer is preferably about 1% by weight.

[0021] Examples of the ultraviolet absorbing agent include benzotriazole-based ultraviolet absorbing agents and hydroxyphenyltriazine-based ultraviolet absorbing agents. Benzotriazole-based ultraviolet absorbing agents can suppress the occurrence of cracks in the coating layer. Hydroxyphenyltriazine-based ultraviolet absorbing agents are effective in stabilizing (deactivating) damage caused by light, water, or heat. Those containing benzotriazole-based ultraviolet absorbing agents are preferred. Those containing both benzotriazole-based ultraviolet absorbing agents and hydroxyphenyltriazine-based ultraviolet absorbing agents are even more preferred.

[0022] An example of a light stabilizer is HALS (hindered amine light stabilizer), which is a radical scavenger that prevents autoxidation.

[0023] A preferred combination is one containing HALS and a benzotriazole-based UV absorber, which can suppress crack expansion and moisture penetration into the interior.

[0024] The calcium carbonate content of the outermost coating layer is preferably less than 9% by weight (including 0% by weight). This can enhance the effect of suppressing the formation of holes due to calcium carbonate elution from the outermost coating layer. The lower limit of the calcium carbonate content of the outermost coating layer is 0% by weight, that is, the outermost coating layer may not contain calcium carbonate.

[0025] On the other hand, the calcium carbonate content of the innermost coating layer can be about 9% by weight. This can further improve the structural stability and impact resistance of the coating layer. Furthermore, since the amount of resin can be reduced by increasing the amount of calcium carbonate, the cost can be reduced by increasing the amount of inexpensive clay containing calcium carbonate. The calcium carbonate content of the innermost coating layer can be 9% by weight or more, but the upper limit can be less than 16% by weight.

[0026] The coating layer may further contain at least one of a plasticizer, a stabilizer, a flame retardant, an antioxidant, or a pigment. Examples of the plasticizer include TOTM (trimellitic acid ester) and DINP (diisononyl phthalate). The type of plasticizer used may be one or more. When the outermost coating layer and / or the innermost coating layer contain a plasticizer, the plasticizer content in each layer may be 20% by weight or more and 40% by weight or less. This can improve the flexibility of the coating layer. The stabilizer is intended to prevent the decomposition of PVC. Examples of the stabilizer include ZnMg / Al-based stabilizers.

[0027] The thickness of the covering layer can be in the range of 1.5 mm to 3.5 mm inclusive, provided that the total thickness of all layers does not cause any problems in installation.

[0028] During manufacturing, the layers that make up the coating layer are in contact with each other but do not fuse together. This is because when each layer is molded one by one, a very thin film of moisture forms on the surface when it comes into contact with the outside air, and decomposition products during molding cover the surface. These films make the layers chemically separated even though they are physically observed as a single layer. This prevents cracks, fissures, or oxidation that occur in the outermost coating layer from reaching the inner coating layer that is in direct contact with it. It also prevents the inner coating layer from being affected by ultraviolet rays, heat, moisture, etc. As a result, it is possible to prevent oxidation and calcium carbonate elution in the inner coating layer, which can more than double the life of the power transmission cable.

[0029] The coating layer can be formed, for example, by extrusion molding. The innermost coating layer that is in direct contact with the core can be formed by normal extrusion molding. In the extrusion molding process, heating and melting, temperature maintenance, and then water cooling are performed. The water cooling process varies depending on the thickness of the power cable, but in some cases the length can be more than 30 m. After the surface of the innermost coating layer has cooled and the moisture has evaporated, a second extrusion molding is performed. On the surface of the innermost coating layer after the first molding, the residue of additives (e.g., stabilizer and plasticizer residues) and moisture generated during heating may be present randomly. Therefore, an interface that prevents the coatings from adhering to each other in the next molding may be formed. In this state, a second extrusion molding is performed. As a result, a coating layer in which the innermost coating layer and the outermost coating layer are not fused to each other is obtained. In the case of three layers, a third extrusion molding is performed after the surface of the layer formed by the second extrusion molding has cooled and the moisture has evaporated. In the case of four or more layers, the above steps are repeated.

[0030] An example of a method for forming a coating layer will be described with reference to FIG. 2. In the extrusion molding device 10 shown in FIG. 2, the plastic compound 16 put into the hopper 14 is melted and heated by the heater coil 13 in the cylinder 11. In the case of a composition containing PVC, it is heated to a high temperature of 180 to 240°C. The molten plastic 17 is extruded toward the die 15 by the screw 12 in the cylinder 11. Meanwhile, the core 18 on which the coating layer is formed is set on the reel in a linear shape according to the product standard. The core 18 unwound from the reel is pulled and passes through the die 15. At this time, the molten plastic 17 is filled into the die 15 from a cross (perpendicular) direction at a crosshead, and the core 18 is coated with the resin composition. The coated cable 19 is rapidly cooled near the die outlet, and then water-cooled, air-cooled, and dried, and then wound into a reel 20. The water-cooling, air-cooling, and drying processes are performed while the cable 19 is flowing, and the total length sometimes reaches several tens of meters. By repeating this series of steps (extrusion, water cooling, air cooling, and drying), the layers constituting the coating layer can be brought into a state in which they are in contact with each other but are not fused together.

[0031] The composition of the coating layer can be identified by, for example, Fourier transform infrared spectroscopy (FT-IR), gas chromatography-mass spectrometry (GC / MS), liquid chromatography-mass spectrometry (LC / MS), liquid chromatography-tandem mass spectrometry (LC-MS / MS), etc. Qualitative analysis of the components contained in the coating layer is possible with FT-IR. On the other hand, quantitative analysis of the components contained in the coating layer can be performed with GC / MS, LC / MS, or LC-MS / MS. LC-MS / MS allows for more detailed quantitative analysis than LC / MS, and is capable of identifying and quantifying components with longer molecular chains.

[0032] In order to confirm the relationship between the calcium carbonate content and the plasticizer content in the coating layer and the durability of the cable, the following experiment was carried out. 2 A stranded insulated electric wire with an outer diameter of 3.2 mm was used. A schematic structure of the stranded insulated electric wire is shown in Fig. 6. The insulated electric wire 40 is made of a plurality of conductors 41 and an insulator 42. The plurality of conductors 41 are arranged so that their outer circumferences are adjacent to each other. The insulator 42 fills the gaps between the conductors 41 and also covers the outer circumference of the conductors 41. (Experiment 1) Three types of PVC insulated wires 40 were prepared, each having an insulation 42 with a calcium carbonate content of 16 wt %, 9 wt %, and 20 wt %.

[0033] A bending durability test was performed on the obtained insulated wire 40. The test method is shown in FIG. 4. The tip of the insulated wire 40 was fixed to the base 30. The weight 31 was fixed near the other tip of the insulated wire 40. The weight 31 had a weight of 100 g. The insulated wire 40 was not bent in the state shown in FIG. 4 (1). Next, as shown in the operation (2), the part of the insulated wire 40 located between the base 30 and the weight 31 was bent 90 degrees to the left as viewed in FIG. 4 to conform to the outer peripheral surface shape of the bending cylinder 32 (bending to the left). After that, the bending was released and the wire was returned to the original state (1). After that, as shown in the operation (3), the part of the insulated wire 40 that had already been bent in the operation (2) was bent 90 degrees to the right as viewed in FIG. 4 to conform to the outer peripheral surface shape of the bending cylinder 32 (bending to the right). After that, the bending was released and the wire was returned to the original state (1). A series of bending operations from (1) to (2), returning to (1), performing (3), and returning to (1) was counted as one cycle, and the number of times the insulated wire 40 broke was counted. The bending speed was set to a value equivalent to 50 round-trip bending operations per minute. For each of the three types of insulated wires 40, the number of breaks was measured when the radius (bending radius) of the bending cylinder 32 was changed to three different values, and the results are shown in Figure 3. The horizontal axis of Figure 3 is the bending radius, which is the radius of the bending cylinder 32, and the vertical axis is the number of bends before breaking.

[0034] As is clear from Figure 3, the smaller the amount of calcium carbonate, the greater the number of times it takes to break, and the greater the durability. On the other hand, inexpensive clay containing calcium carbonate is expected to reduce costs. From the results of Figure 3, it is desirable for the calcium carbonate content of the coating layer to be in the range of 9% by weight or more and less than 16% by weight. (Experiment 2) Three types of PVC insulated wires 40 with different plasticizer contents in the insulators 42 were prepared.

[0035] The bending breakage test described in Experiment 1 was carried out on each of the PVC insulated wires 40. The number of breakages was measured when the radius (bending radius) of the bending cylinder 32 was changed to two different sizes, and the results are shown in Fig. 5. The horizontal axis of Fig. 5 represents the plasticizer content (wt%) in the insulator 42, and the vertical axis represents the number of bends to break.

[0036] In Figure 5, the range of plasticizer content enclosed by the dotted line represents the range of excellent durability, with many flexions required before breaking. It can be seen that if the plasticizer content is greater or less than this range, the material breaks after a small number of flexions, and has poor durability. The same tendency is observed even when the bending radius is changed. Considering the results of Experiments 1 and 2, the composition of the innermost coating layer in the power cable of the embodiment may include 30% by weight of plasticizer, 1% by weight of ultraviolet absorber, 0.15% by weight of antioxidant, 1% by weight of light stabilizer, 50% by weight of PVC, and 9 to 15% by weight of calcium carbonate. The composition of the outermost coating layer may include 30% by weight of plasticizer, 1% by weight of ultraviolet absorber, 0.15% by weight of antioxidant, 1% by weight of light stabilizer, 50% by weight of PVC, and less calcium carbonate than the innermost coating layer. A power cable having an innermost coating layer and an outermost coating layer with the above composition can prevent the outermost coating layer from being damaged by cracks or fissures. As a result, the outermost coating layer blocks the effects of ultraviolet rays, heat, and moisture on the innermost coating layer, so that the innermost coating layer does not oxidize or leach out the plasticizer, or denature or dissolve the calcium carbonate. Therefore, the function of the coating layer can be maintained for a long period of time. Therefore, a solar cable, such as a power transmission cable for photovoltaic power generation, having a coating layer of the above composition can achieve excellent durability.

[0037] According to at least one embodiment described above, there is provided a power transmission cable having a plurality of coating layers, in which the outermost coating layer contains an ultraviolet absorber and a light stabilizer, and the calcium carbonate content of the outermost coating layer is less than the calcium carbonate content of the innermost coating layer. According to the power transmission cable of the embodiment, the outermost coating layer can be prevented from being broken due to cracks or fissures, and therefore the outermost coating layer can block the effects of the exposure environment (ultraviolet rays, heat, and moisture) on the innermost coating layer, thereby improving the durability of the coating layer. As a result, the power transmission cable of the embodiment has excellent durability when used outdoors, such as a power transmission cable such as a solar cable applied to photovoltaic power generation, or a general installation cable.

[0038] Although some embodiments of the present invention have been described, these embodiments are presented as examples and are not intended to limit the scope of the invention. These embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the spirit of the invention. These embodiments and their modifications are included in the scope and spirit of the invention, and are also included in the scope of the invention and its equivalents described in the claims. The invention as originally claimed in the present application is set forth below. [1] A core including an insulated wire; A power transmission cable comprising: A power transmission cable, wherein, among the multiple coating layers, an outermost coating layer contains an ultraviolet absorber and a light stabilizer, and an innermost coating layer contains calcium carbonate, and the calcium carbonate content of the outermost coating layer is less than the calcium carbonate content of the innermost coating layer. [2] The power transmission cable according to [1], wherein the innermost coating layer does not contain an ultraviolet absorber or a light stabilizer. [3] The power transmission cable according to [1] or [2], wherein the calcium carbonate content of the outermost coating layer is less than 9% by weight. [4] The power transmission cable according to any one of [1] to [3], wherein each of the plurality of coating layers contains polyvinyl chloride. [5] The power transmission cable according to any one of [1] to [4], wherein the multiple coating layers are not fused to each other. [Explanation of symbols]

[0039] 1...power transmission cable, 2...insulated wire, 3...core, 4...coating layer, 4a...innermost coating layer, 4b...outermost coating layer, 5...conductor, 6...insulator, 7...interposer, 10...extrusion molding device, 11...cylinder, 12...screw, 13...heater coil, 14...hopper, 15...die, 16...plastic compound, 17...molten plastic, 18...core, 19...cable, 20...reeled cable, 30...base, 31...weight, 32...bending cylinder, 40...stranded insulated wire, 41...conductor, 42...insulator.

Claims

1. a core including an insulated wire; A power transmission cable comprising: A power transmission cable, wherein, among the multiple coating layers, an outermost coating layer contains an ultraviolet absorber and a light stabilizer, and an innermost coating layer contains calcium carbonate in an amount of 9% by weight or more and less than 16% by weight, and the calcium carbonate content of the outermost coating layer is less than the calcium carbonate content of the innermost coating layer.

2. The power transmission cable of claim 1 , wherein the innermost coating layer does not contain an ultraviolet absorber and a light stabilizer.

3. 3. The power transmission cable according to claim 1, wherein the outermost coating layer has a calcium carbonate content of less than 9% by weight.

4. The power transmission cable according to claim 1 , wherein each of the plurality of coating layers contains polyvinyl chloride.

5. The power transmission cable according to any one of claims 1 to 4, wherein the plurality of coating layers are not fused to each other.

Citation Information

Patent Citations

  • Molding article made of vinyl chloride resin

    JP1989210339A

  • JP1992008317U

  • JP1992099614U

  • Stabilization of polyvinyl chloride

    JP1995011084A

  • Insulating wire / cable

    JP2001126547A