Powder coating manufacturing method and manufacturing equipment
The method of static electricity-assisted induction heating and high-speed hot air blasting addresses the inefficiencies of conventional powder coating by rapidly raising the temperature to the baking point, ensuring uniform heating and compact equipment design.
Patent Information
- Application Number
- JP2020125293
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-07-22
- Publication Date
- 2024-10-03
- Estimated Expiration
- 2040-07-22
AI Technical Summary
Conventional powder coating methods require long baking times due to slow temperature increase, leading to potential defects and increased equipment scale, especially when using thermosetting powders, and infrared irradiation may cause uneven heating.
A method involving static electricity for powder adhesion, followed by induction heating for temporary welding and high-speed hot air blasting to rapidly raise the temperature to the baking point, combined with a jet heating device for uniform heating.
This method allows for rapid and uniform temperature increase, reducing baking line length and preventing defects, while maintaining coating quality and compacting equipment scale.
Smart Images

Figure 0007560971000001 
Figure 0007560971000002 
Figure 0007560971000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method and equipment for producing powder-coated articles. [Background technology]
[0002] In recent years, from the perspective of environmental protection, the release of organic solvents into the atmosphere has become a major problem, and within the paint industry, there are growing expectations for powder coatings as an alternative to conventional organic solvent-based coatings, as they are environmentally friendly because they do not require exhaust or wastewater treatment and can be recovered and reused. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2005-218998 A Summary of the Invention [Problem to be solved by the invention]
[0004] If the powder coating is thermosetting, it hardens through a cross-linking reaction when heat is applied, so after the powder coating has been applied to the substrate, it must be placed in an atmosphere of a certain temperature for a certain period of time to melt and harden, i.e., baked. For this purpose, a hot air circulating drying oven, in which extremely slow hot air is circulated inside the oven, as described in Patent Document 1, is used. Since the baking temperature is relatively high, it takes time to heat up. Therefore, if multiple powder-coated objects are passed through a drying oven in succession, the oven length becomes longer, and the scale of the manufacturing equipment becomes larger. Also, if the temperature rise speed of the powder paint is slow, melting and hardening may occur partially, which may cause coating defects. In response to this problem, it has been proposed to install an infrared ray irradiation furnace before the drying furnace and quickly raise the temperature of the powdered material to the baking temperature by irradiating it with infrared rays. However, if there are any shaded areas that are not hit by the infrared rays, those areas will not be heated enough.
[0005] The present invention has been made in response to the above-mentioned problems in the conventional art, and has as its object to provide a new and useful method for producing powder-coated objects which incorporates a heating method capable of quickly and evenly raising the temperature of a powder-coated object to which a powder paint has been applied up to the baking temperature. Another object of the present invention is to provide a production facility for the above-mentioned production method. [Means for solving the problem]
[0006] The present invention has been made to achieve the above-mentioned object, and the invention [1] is a method for manufacturing a powder coated product, comprising a powder adhesion step in which powder paint is adhered to an object to be coated by utilizing static electricity, a temporary welding step in which, after the powder adhesion step, induction heating is applied to melt the boundary side with the object to temporarily weld the powder paint, a heating step in which, after the temporary welding step, a bundle of hot air is blown at high speed to raise the temperature to a baking temperature, and a baking step in which, after the heating step, the powder paint is baked to form a powder coated product, wherein the temporarily welded powder paint is capable of withstanding the impact of the bundle of hot air blown at high speed in the heating step and is prevented from flying out.
[0007] The invention [2] is a method for producing a powder coated article as described in [1], characterized in that the thickness of the article to be coated is 0.5 mm or more.
[0008] The invention [3] is a method for manufacturing a powder-coated article as described in [1] or [2], characterized in that in the temporary bonding process, the surface of the powder paint applied to the article to be coated is heated to a temperature of 55°C or higher and lower than 80°C.
[0009] The invention [4] is a method for producing a powder coated article described in any one of [1] to [3], characterized in that in the heating process, hot air having a temperature higher than the baking temperature is blown so that the wind speed in the vicinity of the powder paint applied to the article is 5 m / sec or more.
[0010] The invention [5] is a manufacturing equipment for powder-coated objects for carrying out the method according to any one of [1] to [4], characterized in that a coating booth for carrying out the powder adhesion process, an induction heating device for carrying out the temporary fixing welding process, a jet ejection type heating device for carrying out the temperature increase process, and a heat equalizing furnace for carrying out the baking process are installed in a line, and the object to be coated is transported and subjected to each process in sequence.
[0011] The invention [6] is a manufacturing equipment for powder coated articles described in [5], in which an induction heating device induction heats an article to be coated with powder paint by passing it between opposing work coils, and is characterized in that, as a welding promotion mechanism, the manufacturing equipment is provided with a distance changing means that can change the distance between the work coil and the article to be coated and / or a spacing changing means that changes the vertical spacing between the multiple coil elements that make up the work coil. Effect of the Invention
[0012] The manufacturing method of the present invention incorporates a temperature raising method that can raise the temperature of the powder-adhered material to the baking temperature quickly and evenly, and in this manufacturing facility, the baking line installed downstream of the coating booth can be shortened. [Brief description of the drawings]
[0013] [Figure 1] 1 is a line configuration diagram of a manufacturing facility according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a configuration diagram of a pair of work coils of the induction heating device of FIG. [Diagram 3] FIG. 3 is a schematic diagram of the induction heating device of FIG. 2. [Figure 4] FIG. 3 is a schematic explanatory diagram of an induction heating device according to another embodiment different from that of FIG. 2. [Diagram 5] FIG. 2 is an image explanatory diagram of the jet ejection type heating device of FIG. 1. [Figure 6] FIG. 2 is a perspective view showing temperature measurement points of the powder deposit used in the examples. [Figure 7] 1 is a graph showing temperature rise of powdery deposits obtained in the examples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] Hereinafter, a method for producing a powder coated article according to an embodiment of the present invention will be described together with a production line implemented as a production facility. The coating object of the present invention is made of a conductive material, mainly metal, because induction heating is used. The thickness of the thin object is 0.5 to 4.0 mm, and the thickness of the thick object is more than that, but the thickness of the coating object of the present invention is 0.5 mm or more. In other words, the present invention is applicable to both thin and thick objects. Powder paints can be used without any particular restrictions as long as they have been used for powder coating in the past. Powder paints are solid powders whose main raw materials are polymer resins and pigments, and do not contain organic solvents. However, they are broadly divided into thermoplastic and thermosetting types, and thermosetting types include epoxy-based powder paints, polyester-based powder paints, epoxy-polyester-based powder paints, fluororesin-based powder paints, and acrylic-based powder paints. When using these types of powder paints, they are usually melted and hardened by baking after application, so currently, the present invention mainly assumes the use of these types.
[0015] Inside the manufacturing facility, the object to be coated (W) is transported by being hung from a jig or placed on a conveyer belt, and in the manufacturing facility 1 shown in Figure 1, it is hung from a jig in the attachment / detachment area and transported on the transport path (L). Note that when powder is attached, it becomes a powder-adhered object, when it is temporarily welded, it becomes a powder-welded object, and when baking is completed, it becomes a powder-coated object, but in the following description, the terms object to be coated (W1), powder-adhered object (W2), powder-welded object (W3), and powder-coated object (W4) are used depending on the situation.
[0016] Before the powder is applied, a series of processes is carried out to remove oil and foreign matter and make the surface easier for paint to adhere to, for example washing with hot water, degreasing (iron phosphate), water washing 1, 2, 3, draining, and cooling. These are conventional processing methods and equipment. The workpiece (W1) that has been pretreated is loaded into the painting booth 3 from the loading area.
[0017] In the coating booth 3, a powder deposition process is carried out in which powder paint is deposited on the workpiece (W1) using static electricity. In this embodiment, an electrostatic dry spraying method is adopted, in which powder paint is sprayed onto the surface of the workpiece (W1). According to this method, charged powder paint is sprayed from an electrostatic gun toward the workpiece (W1), and the powder paint adheres to the surface of the workpiece (W1) due to the attractive force between positive and negative ions. Another method that uses static electricity is frictional charging coating, and both of these methods can be adopted in the present invention.
[0018] Both coating methods have been widely adopted, and the coating booth 3 in which the electrostatic dry spraying method is performed is also of a conventional configuration. First, the powder paint is applied to the entire workpiece (W1) in the main spray section, and then fine adjustments are made in the sub-spray section to ensure that the powder paint is applied evenly. The amount of adhesion is adjusted so that the thickness of the final coating film is about 30 to 150 μm, which is conventional for powder coating.
[0019] When the workpiece (W1) leaves the coating booth 3, the powder paint has adhered to the surface of the workpiece (W1) to form a powder-adhered object (W2). This powder-adhered object (W2) is sent to an induction heating device 5. In the induction heating device 5, high-frequency induction heating is applied to melt the boundary between the workpiece (W1) and the attached powder paint, thereby carrying out a temporary welding process to temporarily weld the powder paint to the workpiece (W1). Specifically, it is configured with the device described in JP 2005-259575 A. As shown in Fig. 2 and Fig. 3, a pair of work coils 5a, 5a are erected in parallel while being connected by a flexible tube 5b through which a copper wire is passed, and the powder deposit (W2) passes between the pair of work coils 5a, 5a.
[0020] In the high-frequency induction heating method, the workpiece (W1) is heated, and the powder paint adhering to it receives heat from the workpiece (W1) and becomes heated, with the melting of the powder paint starting from the boundary side with the workpiece (W1). In the present invention, this mechanism is utilized to melt only the boundary side with the substrate (W1) rather than the entire powder paint, and the molten part acts as an adhesive to weld the powder paint to the substrate (W1) and temporarily secure it. The strength of the temporary welding need only be such that the powder paint is not blown off by the impact of the high-velocity hot air in the next heating process, in which a beam of hot air is blown at high speed to quickly raise the temperature to the baking temperature, and the purpose can be sufficiently achieved even with thick substrates if it is temporarily secured.
[0021] Although it is possible to perform the baking process using only high-frequency induction heating, if the workpiece (W1) is thick and has various shapes and sizes, baking the workpiece all at once is likely to result in uneven heating. On the other hand, changing the work coil for each product type is not realistic in terms of cost and work. In contrast, the present invention is used in the preliminary stage of temperature rise as described above, and is therefore fully capable of handling thick objects in this stage as described above.
[0022] In the induction heating device 5, the holding member 5c of the work coil 5a can be moved in the opening and closing direction by a ball screw mechanism 5d connected to the opening and closing motor, and the opening and closing motor and the ball screw mechanism 5d can be moved together by driving the center movement motor 5e, so that the distance between the work coil 5a and the powder deposit (W2) can be changed and the high frequency output can be changed, and the temporary welding state can be optimized according to the shape and size of the workpiece (W1) within the application range of these changing means. In other words, these changing means are used as a welding promotion mechanism.
[0023] For powder paints currently available on the market, the completion of the temporary welding process is when the surface of the powder paint applied to the workpiece (W1) reaches a temperature of 55°C or higher and below 80°C. Completion can be determined by time management based on temperature measurements using a non-contact thermometer or pre-accumulated temperature rise data.
[0024] The induction heating device 5 may be another example described in JP 2012-138175 A. This device not only allows the high-frequency output to be changed, but also, as shown in Fig. 4, the work coil 5a is composed of multiple coil elements 5f, 5f ..., which are held by holding members 5g, 5g ..., and the holding members 5g, 5g ... can be moved in the vertical direction to change the vertical spacing between the coil elements 5f, 5f ... by rotating the arm member 5h, and by using this changing means, the temporary welding state can be optimized according to the shape and size of the workpiece (W1) within the applicable range of this means. It is technically possible to use a structure in which this is also used in conjunction with a distance changing means, and a combination of both change means may be used, but this is not necessarily required for the purpose of temporary welding.
[0025] The powder welded material (W3) coming out of the induction heating device 5 is sent to a tunnel-shaped furnace 7. A jet ejection type heating device 9 is arranged upstream of the furnace 7, and a heating process is first carried out, where the powder welded material (W3) is heated to a baking temperature. The jet-type heating device 9 transmits heat by colliding a jet of hot air with the object to be heated, and is also called a jet oven, and can transmit thermal energy to the surface of the object to be heated with a high thermal conductivity. Taking advantage of this feature, the present invention aims to quickly raise the temperature to the baking temperature. In this jet-type heating device 9, as shown in Fig. 5, a number of nozzles 9a, 9a, ... are arranged vertically and front to back, and the nozzle outlets of each nozzle are arranged opposite each other. The powder welded material (W3) passes between the left and right nozzle groups. Therefore, the powder welded material (W3) receives the impact of the high-speed hot air flux from both the left and right sides.
[0026] The baking temperature and baking time ranges are determined to realize the optimal baking state depending on the type of powder paint, so the temperature and wind speed of the high-velocity hot air are optimally set to quickly bring the powder welded material (W3) up to the baking temperature, taking into account the temporary welding state and the equipment capacity. It is recommended that the temperature be set to a temperature somewhat higher than the baking temperature of the powder paint, preferably about 20 to 50° C. higher, for example, about 200 to 250° C. The higher the temperature, the more heat can be applied to the powder deposit (W3), but if the temperature is too high, it will exceed the baking temperature and overheat, so an upper limit is set. It is recommended that the wind speed be set to 5m / sec or more near the powder welded material (W3) to make the jet spray effective. The faster the wind speed, the stronger the force of the hot air flux, but if it is too fast, the strength of the temporary weld may be defeated by the impact and the powder paint may fly out, so it is expected that the upper limit will be around 15m / sec.
[0027] The temporarily welded powder paint receives this high-velocity hot air flux from the surface side, and the entire surface, including the inside, is melted evenly and reaches the baking temperature. Then, the paint is transported to the downstream side of the furnace 7. The downstream side of the furnace 7 is of a hot air circulation type, and the air heated by the burner combustion in the uniform heating and circulation device 11 is blown into the furnace 7 by the blowing fan, circulates inside the furnace 7, and is collected outside the furnace 7 by the operation of the suction fan and is heated again. In the furnace 7, the wind flows at a very low speed, specifically, about 0.1 to 1 m / sec, and there is almost no wind. Baking of the powder paint proceeds by leaving it at this atmospheric temperature for a certain period of time, for example, about 20 minutes at 180°C.
[0028] According to the method of the present invention, the atmospheric temperature required for this baking is not used to raise the temperature to the baking temperature, but the induction heating device 5 and the jet ejection type heating device 9 are used to raise the temperature to the baking temperature in one go, making it possible to shorten the furnace length to about one-third compared to when the inside of the furnace 7 is maintained at the atmospheric temperature and these devices are also responsible for raising the temperature to the baking temperature of the powder paint. This reduction more than covers the additional installation of the induction heating device 5 and the jet ejection type heating device 9. Furthermore, the rapid heating process avoids the mixture of melting and hardening that is typical of powders, resulting in good coating quality.
[0029] Although the embodiments of the present invention have been described in detail above, the specific configuration is not limited to the above-described embodiments, and the invention also includes design changes that do not deviate from the spirit of the present invention. EXAMPLES
[0030] Using the induction heating device 5 (FIG. 2) according to the above embodiment and the jet ejection type heating device 9 installed in the furnace 7, a temporary fixing, welding and temperature rise test for the powdery attachment (W2) was carried out. The powder deposit (W2) was a steel pipe with a wall thickness of 2 mm, a diameter of 32 mm, and a length of 30 cm, as shown in Figure 6, to which an epoxy resin powder paint was applied so that the coating thickness was 100 μm. When all of the measurement positions (No. 1 to No. 4) in the induction heating device 5 reached 70°C or higher, the material was moved to the jet ejection heating device 9 (220°C, wind speed 12 m / sec) and heated to the baking temperature of 180°C. As shown in the temperature rise graph in Figure 7, it took about 5 minutes to put the material into the induction heating device 5, take it out, and then put it back into the jet ejection heating device 9 to finally raise the temperature to the baking temperature. After that, the material was baked at 180°C using the uniform heating and circulation device 11, and the baking was completed in 10 minutes. In other words, it took 15 minutes to complete baking of the powder adhesion (W2).
[0031] On the other hand, when the temperature of the powder-attached object (W2) was raised to 180° C. by the uniform heating and circulation device 11 and baking was continued thereafter, the time required was 30 minutes. In other words, the time required to complete baking for the powder-attached object (W2) was 30 minutes. In other words, according to the method of the present invention, the time until baking can be significantly shortened, so that the furnace length in a manufacturing facility in which multiple powder deposits (W2) are baked in succession can be shortened, thereby making the scale of the manufacturing facility more compact. Furthermore, in the method of the present invention, even if the powder paint is subjected to an impact during the heating process, the powder paint is prevented from flying out, and the mixture of hardened and molten paint is suppressed, so that the coating film of the powder-coated product (W4) is made denser, thereby improving the quality. [Explanation of symbols]
[0032] 1... Manufacturing equipment 3... Paint booth 5... Induction heating device 5a... Work coil 5b... Tube 5c... Holding member 5d... Ball screw mechanism 5e... Center movement motor 5f... Coil element 5g... Holding member 5h... Arm member 7... Furnace 9... Jet ejection type heating device 9a... Nozzle 11... Heating uniformity and circulation device W1…Object to be coated W2…Powder deposit W3…Powder deposit W4…Powder coated object
Claims
1. The method includes a powder adhesion step in which powder paint is adhered to the substrate by utilizing static electricity, a temporary welding step in which induction heating is applied after the powder adhesion step to melt the boundary side with the substrate to temporarily weld the powder paint, a temperature increase step in which a bundle of hot air is blown at high speed to raise the temperature to a baking temperature after the temporary welding step, and a baking step in which the powder paint is baked to produce a powder coated product after the temperature increase step. In the heating step, hot air having a temperature higher than the baking temperature is blown onto the powder coating material applied to the workpiece at a wind speed of 5 m / sec or more in the vicinity of the powder coating material applied to the workpiece, A method for manufacturing powder coated articles, characterized in that the powder paint that has been temporarily welded is capable of withstanding the impact of a hot air flux being blown at high speed during the temperature raising process, thereby preventing it from flying out.
2. In the method for producing a powder coated article according to claim 1, A manufacturing method characterized in that the thickness of the substrate is 0.5 mm or more.
3. In the method for producing a powder coated article according to claim 1 or 2, This manufacturing method is characterized in that in the temporary welding process, the surface of the powder paint applied to the substrate is heated to a temperature of 55°C or higher and lower than 80°C.
4. A manufacturing facility for powder-coated objects for carrying out the method according to any one of claims 1 to 3, comprising: The painting booth for the powder application process, the induction heating device for the temporary fixing and welding process, the jet ejection heating device for the temperature increase process, and the soaking furnace for the baking process are all installed in a line. A manufacturing facility characterized in that the workpieces are transported and subjected to each process in sequence.
5. In the manufacturing equipment for powder coated products according to claim 4, The induction heating device inductively heats the workpiece with the powder coating by passing it between opposing work coils. A manufacturing equipment characterized in that, as a welding promotion mechanism, it is equipped with a distance changing means that can change the distance between the work coil and the workpiece, and / or a spacing changing means that changes the vertical spacing between multiple coil elements that constitute the work coil.
Citation Information
Patent Citations
Electrostatic powder coating
JP1978056236A
Heating furnace in continuous powder electrostatic coating line
JP1986146366A
Baking method for powder painted metallic sheet
JP1991249975A
Method and furnace for baking coated metallic plate
JP1991284375A
Powder coating method and powder coating apparatus
JP2005218998A