Fiberglass textile structure having parylene coating

Parylene coating via chemical vapor deposition addresses the inadequacies of organic polymer coatings on glass fibers, enhancing durability and alkali resistance for glass fiber reinforcements in alkaline materials.

JP7561193B2Active Publication Date: 2024-10-03SAINT GOBAIN ADFORS
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2022537131
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-12-16
Filing Date
2020-12-14
Publication Date
2024-10-03
Estimated Expiration
2040-12-14

AI Technical Summary

Technical Problem

Existing glass fiber reinforcements for alkaline materials like cement and concrete are inadequate due to insufficient protection from organic polymer coatings, leading to increased costs and reduced fire resistance, especially when using alkali-resistant glass fibers.

Method used

Applying a parylene coating via chemical vapor deposition to glass fiber textiles, providing a durable and effective barrier against alkaline environments, which can be enhanced with additional organic layers.

Benefits of technology

The parylene coating significantly enhances the durability and alkali resistance of glass fibers, maintaining mechanical properties and reducing deterioration in alkaline conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007561193000001
    Figure 0007561193000001
  • Figure 0007561193000002
    Figure 0007561193000002
  • Figure 0007561193000003
    Figure 0007561193000003
Patent Text Reader

Abstract

The present invention relates to a fiberglass textile structure characterized by a parylene (poly(para-xylylene)) coating having a thickness of 5 μm to 30 μm, preferably 6 μm to 25 μm, in particular 7 μm to 20 μm. The present invention also relates to a method for consolidating a solid material, which method comprises introducing the textile structure provided with the parylene coating into a liquid base material, preferably a base material comprising water and a hydraulic binder, and curing the base material.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a fiberglass textile structure coated on its surface with a parylene coating several microns thick, and the use of such a textile structure to reinforce materials, preferably materials containing alkaline hydraulic binders. [Background technology]

[0002] Textiles used to reinforce hydraulic binder-based materials, in particular materials based on plaster or cementitious materials such as mortar or concrete, are generally based on organic polymers, steel or glass fibres.

[0003] Steel is the oldest and most widely used reinforcing material, allowing very significant reinforcement, especially in structural applications (see for example US Pat. No. 3,120,257 or WO 95 / 13440).

[0004] The polymers are generally used in the form of dispersed short fibers or in the form of textiles impregnated with resin (see, for example, WO 2017 / 117045).

[0005] Glass fibres are used in particular for the reinforcement of cementitious materials, especially façade mortar in external thermal insulation composite systems (ETICS), in the manufacture of cement boards or for the reinforcement of prefabricated concrete. Glass fibres are generally used in the form of non-woven webs bound with organic binders or in the form of grids.

[0006] Fiberglass has the advantages over steel of being light and flexible, and therefore easy to wind, transport and handle, as well as good resistance to acid corrosion.

[0007] If glass fibers are to be used in alkaline materials such as cement, mortar, and concrete, alkali-resistant glass fibers (AR glass) must be used, which are significantly more expensive than regular glass (E or C glass).

[0008] It is known to protect reinforcing fibers made from normal E or C glass with organic coatings based on thermoplastic or thermosetting polymers, in particular based on SBR (styrene-butadiene rubber) elastomers, styrene-acrylic latex, acrylic latex or based on PVC, but the protection provided by these polymers is generally insufficient in effectiveness and durability, and perfect persistence of the coating is required and difficult to obtain. These drawbacks and imperfections limit the use of glass fibers in demanding applications. Alkali-resistant protective layers, for example based on organic polymers, have the drawback of significantly increasing the cost of glass fiber-based reinforced products and degrading their fire resistance. Summary of the Invention [Problem to be solved by the invention]

[0009] The invention is based on the idea of ​​protecting glass fiber textile reinforcements by a specific type of organic polymer that is not deposited by liquid route, but by a method similar to chemical vapor deposition. This deposition method allows very good coverage of textile structures, even down to the smallest details. The deposited layer perfectly conforms to the irregularities of the surface, and as a result offers the underlying glass a better protection than a normal polymer deposition.

[0010] The organic polymer used in the present invention is parylene, in particular parylene C, which is known per se but which, to the inventors' knowledge, has not previously been used for the chemical protection of glass fibres against alkaline environments. This polymer can be deposited directly on the glass fibres, with or without sizing, and can, if desired, be coated in places with an organic binder, for example in the case of a non-woven mat of glass fibres.

[0011] The protection provided by the parylene layer may of course be enhanced by depositing other organic layers, for example polymers, particularly elastomers, deposited above or below the parylene layer. [Means for solving the problem]

[0012] A first object of the present application is therefore a fiberglass textile structure provided with a Parylene (poly(para-xylylene)) coating having a thickness between 5 μm and 30 μm.

[0013] The present application further relates to a method for strengthening a solid material, said method comprising introducing a textile structure with a parylene coating into a liquid base material and curing the base material.

[0014] And, the present application relates to a reinforced solid product or material comprising a textile structure with a solid base material (matrix) and a parylene coating incorporated into the solid base material. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] In this application, the term "textile structure" refers to a set of textile glass fibers. Textile glass fibers, also called glass filaments or monofilaments, may simply be collected into rovings or multifilament yarns. These rovings or yarns may then be assembled into more complex structures by weaving, knitting, or sewing, or by bonding, for example, with a binder. Thus, the textile structures of the present invention include rovings and multifilament yarns, stitched or bonded nonwoven mats or webs, cloths (finely woven textiles), grids (openly woven or knitted textiles), or nonwoven products having a grid structure, often called laid scrims, formed from layers of yarns superimposed in at least two different directions.

[0016] The textile structure of the present invention is preferably selected from the group consisting of multifilament yarns, rovings, nonwoven mats bonded with organic binders, cloths, woven grids, knitted grids, and laid scrims. Naturally, the textile structure also encompasses combinations of two or more elements from this list, for example laminates of woven or knitted grids with nonwoven mats.

[0017] If the textile structure is a nonwoven mat, the textile glass fibers are preferably bound using an organic binder based on a thermosetting polymer. Examples of thermosetting polymer binders are binders obtained from melamine-formaldehyde resins, urea-formaldehyde resins or phenol-formaldehyde resins, or mixtures of these resins.

[0018] The parylene coating preferably has a thickness of 6 μm to 25 μm, in particular 7 μm to 20 μm.

[0019] The deposition of parylene coatings is carried out by a known method using a gas phase process called the "Gorham process" named after its inventor (Gorham WF, 1966 "A New, General Synthetic Method for the Preparation of Linear Poly(p-xylylene)," J. Polym. Sci. Part A-1 Vol.4, p.3027-3039). This deposition method comprises reacting a solid dimeric precursor of the formula: [2,2]paracyclophane, optionally chlorinated, with [ka] These include sublimation by heating to temperatures above 100°C, pyrolysis of the gaseous dimer at temperatures of about 500°C to 700°C resulting in the formation of reactive monomers, and deposition of the reactive monomers onto the object to be coated, which is maintained under vacuum (about 0.1 Torr (about 1.33 Pa)) and typically at ambient temperature.

[0020] This deposition may be carried out on the components of the textile structure (monofilaments, rovings, yarns) or on textile structures made from monofilaments, rovings or yarns.

[0021] Thus, in a woven grid type textile structure, the coating may coat each of the yarns of the grid individually, so that they are present at the yarn contact points, or the coating may be applied to the finished textile structure, coating the surface of the structure without being present at the contact points between the yarns or filaments.

[0022] To form an effective alkali-resistant barrier, the parylene coating preferably completely covers the entire surface of the textile structure so as to isolate the textile structure from the atmosphere.

[0023] The glass fibers of the textile structure of the present invention may in principle be made of any type of glass, for example A, E, C, T or AR glass.

[0024] In one preferred embodiment, the glass fibers are made from E, A, or C glass. These are the less expensive glasses that benefit most from the chemical barrier function of the parylene coating due to their high sensitivity to alkali. E glass is of particular interest because it is inexpensive but sensitive to alkali.

[0025] If the textile structure is formed from glass fibres held together by a binder or coated with a binder (e.g. non-woven mats, cloths, woven or knitted grids, laid scrims), the glass fibres advantageously represent 30-95% by weight, preferably 35-90% by weight, in particular 40-85% by weight of the weight of the textile structure before deposition of the parylene coating. A further portion to reach 100% is formed, for example, by organic binders or fibres other than glass fibres, for example carbon fibres, natural fibres or metal fibres.

[0026] When the textile structure is formed by unbonded glass fibers or glass fibers coated with an organic binder (rovings, spun yarns), the glass fibers typically represent 98-100% of the weight of the textile structure before deposition of the parylene coating.

[0027] The total surface mass of the textile structure to be covered with the parylene coating is advantageously between 30 and 600, preferably between 40 and 500, in particular between 50 and 400.

[0028] The parylene coating advantageously represents between 5 and 200%, preferably between 8 and 160% and better still between 10 and 150% of the weight of the textile structure before deposition of the parylene coating.

[0029] The parylene used to form the alkali-resistant protective coating is preferably Parylene C (poly(2-chloro-paraxylylene)).

[0030] As is known, Parylene C has lower gas permeability and better acid resistance than Parylene N (non-chlorinated), and forms films with better mechanical strength and better abrasion resistance. Furthermore, the deposition performance of Parylene C is higher than that of Parylene N.

[0031] The textile structure of the present invention with a parylene coating may be further coated with an organic polymer coating. Such coatings are usually formed by elastomers, typically styrene-butadiene rubber, styrene acrylic, acrylic, or PVC. This additional coating enhances the alkali resistance of the textile structure of the present invention. In the case of laid scrims, it further ensures the cohesion of the structure formed by the overlapping layers of yarn.

[0032] The textile structure of the present invention can be used as a mechanical reinforcement for solid materials. Due to its good alkali resistance, the textile structure of the present invention is particularly suitable for the reinforcement of materials based on hydraulic binders. By "hydraulic binder" is meant an inorganic material that, when mixed with water, forms a liquid or paste that hardens due to the reaction of the binder with the water.

[0033] The hydraulic binder is in particular selected from the group consisting of portland cement, lime, high alumina cement, slag cement, sulfo-aluminous cement, and alkali-activated cement or plaster.

[0034] The method for reinforcing a solid material of the present invention includes introducing a textile structure with the parylene coating described above into a liquid base material and curing the base material.

[0035] The base material preferably comprises water and a hydraulic binder. It advantageously has a basic pH of more than 8, preferably more than 9, in particular more than 10.

[0036] The reinforced solid product or material obtained by the above method comprises a textile structure comprising a solid base material and a parylene coating embedded in the solid base material.

[0037] Examples of solid products or materials reinforced with the textile structure of the present invention include facade mortars, screeds, cement boards, concrete, prefabricated elements made from cement or concrete, and grouts of external insulation systems (EIS). EXAMPLES

[0038] Example 1 A coating of Parylene C with a uniform thickness of approximately 10 μm is applied to the E-glass fibres with a basis weight of 50 g / m2 bonded with 25% organic binder based on urea-formaldehyde resin. 2 The nonwoven mat is then deposited.

[0039] This nonwoven mat is then subjected to an ageing test in an alkaline environment as defined in ETAG 004 (Technical Guide for External Facade Thermal Insulation Systems), which test is carried out as follows:

[0040] Twenty rectangular specimens with dimensions 300 mm x 50 mm are cut from the nonwoven mat with the parylene coating. For half of the samples, the length direction (300 mm) is parallel to the machine direction, and for the other half of the samples, the length direction is perpendicular to the machine direction.

[0041] All 20 samples were diluted with 1 g / l NaOH, 4 g / l KOH, and 0.5 g / l Ca(OH). 2 , for 28 days at a temperature of 23°C.

[0042] After 28 days of immersion, the samples are rinsed in an acid solution (5 mL of 35% diluted HCl) for 5 minutes and then placed in three water baths of 4 liters each for 5 minutes in sequence.

[0043] The samples are then dried for 48 hours at a temperature of 23° C. (±2° C.) and a relative humidity of 50% (±5%).

[0044] The mechanical resistance to tension is then determined using an MTS Insider bench operating at a tension speed of 100 mm / min.

[0045] Table 1 shows the tensile breaking strength (BST expressed in N / 5 cm) of samples cut parallel to the machine direction and samples cut perpendicular to the machine direction before and after exposure to the aging test, compared to samples of the same nonwoven mat that underwent the same treatment but were not pre-coated with Parylene. The values ​​shown in the table are the average (± standard deviation) calculated from 10 samples. [Table 1]

[0046] It can be seen that the aging of the nonwoven mat after exposure to alkaline conditions is greatly delayed by the presence of the parylene coating.

[0047] Example 2 A 10 μm thick layer of parylene is deposited on a spun yarn of E-glass that has a count of 68 tex before parylene deposition and 100 tex after parylene deposition.

[0048] Ten samples of this yarn are subjected to the "Distortion in cement" test described in standard EN 14649:2005 (Precast concrete products - test method for strength retention of glass fibers in cement and concrete; SIC-TEST).

[0049] Table 2 below shows the change in tenacity (expressed in cN / tex) and modulus (expressed in GPa) during testing of yarns coated with parylene compared to the same yarns (68 tex) that were not coated with parylene. [Table 2]

[0050] The deposition of the parylene protective layer allowed the yarn to retain approximately 90% of its elastic modulus, compared to only 21% for the control yarn without the parylene deposition. Similarly, tenacity was significantly less degraded in the presence of parylene compared to its absence.

[0051] A layer of Parylene C coating reinforcing yarns made from E-glass thus provides an effective protection for the glass yarns from chemical attack by the alkaline components of the cementitious material.

Claims

1. A textile structure made from glass fibres, characterised in that it is provided with a Parylene (poly(para-xylylene)) coating having a thickness of 5 μm to 30 μm, preferably 6 μm to 25 μm, in particular 7 μm to 20 μm.

2. 2. The textile structure according to claim 1, characterized in that the glass fibres are A, E or C glass fibres, preferably E glass fibres.

3. 3. The textile structure according to claim 1 or 2, characterized in that it is made of glass fibres held together by a binder or glass fibres coated with a binder, and that the glass fibres represent 30-95 wt.-%, preferably 35-90 wt.-%, in particular 40-85 wt.-% of the weight of the textile structure before deposition of the Parylene coating.

4. 4. The textile structure according to claim 1, wherein the parylene is Parylene C (poly(2-chloro-paraxylylene)).

5. 5. The textile structure according to claim 1 , characterized in that the parylene coating represents 5 to 200%, preferably 8 to 160%, and even better 10 to 150% of the weight of the textile structure before deposition of the parylene coating.

6. 6. The textile structure according to claim 1, characterized in that it is selected from the group consisting of multifilament yarns, rovings, nonwoven mats bound with organic binders, cloths, woven grids, knitted grids, and laid scrims.

7. 7. The textile structure according to claim 1, characterized in that the parylene coating completely covers the entire surface of the textile structure so as to isolate the textile structure from the atmosphere.

8. 8. A method for strengthening a solid material, comprising introducing a textile structure provided with a parylene coating according to any one of claims 1 to 7 into a liquid base material, preferably a base material comprising water and a hydraulic binder, and curing said base material.

9. 9. The method according to claim 8, characterized in that the liquid base material has a basic pH of more than 8, preferably more than 9, in particular more than 10.

10. 10. A reinforced solid product or material comprising a solid base material and a textile structure comprising a parylene coating according to any one of claims 1 to 7 embedded in said solid base material.

11. 11. Reinforced solid product or material according to claim 10, characterized in that it is selected from the group consisting of facade mortars, screeds, cement boards, concrete, prefabricated elements made from cement or concrete, and grouts of external insulation systems (EIS).

Citation Information

Patent Citations

  • Hydrophilization method of glass and glass fiber

    JP1983176143A

  • Fuel feed control device for internal combustion engine

    JP1993071381A

  • Film-forming apparatus, film-forming method, and method for manufacturing inkjet head

    JP2010001546A

  • Barrier laminate

    JP2020163742A

  • Thermoplastic composite material comprising a reinforcing component and a poly(phenylene) polymer and process to make said thermoplastic composite material

    US20160115300A1