Material molding device and material molding method

The material molding apparatus and method use radiation to monitor and adjust molding conditions in real time, addressing the challenge of internal flaws in composite materials, enhancing productivity and quality by preventing defects.

JP7562445B2Active Publication Date: 2024-10-07MITSUBISHI HEAVY IND LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2021029488
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-02-26
Publication Date
2024-10-07
Estimated Expiration
2041-02-26

AI Technical Summary

Technical Problem

Existing methods for integral molding of composite materials fail to directly detect internal flaws such as voids and porosity, requiring time-consuming trial and error to establish optimal molding conditions, and are sensitive to material storage conditions, leading to reduced productivity.

Method used

A material molding apparatus and method that uses radiation to directly and in real time monitor internal flaws by irradiating the material with radiation, detecting the transmitted radiation, and adjusting molding conditions based on the detection results to prevent or eliminate flaws.

Benefits of technology

Enables direct and real-time detection of internal flaws, allowing for immediate adjustments to molding conditions to prevent or eliminate voids, porosity, and other defects, thereby improving productivity and quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007562445000001
    Figure 0007562445000001
  • Figure 0007562445000002
    Figure 0007562445000002
  • Figure 0007562445000003
    Figure 0007562445000003
Patent Text Reader

Abstract

To provide a material formation device that can monitor flaws generated in a material being formed, directly and in real time.SOLUTION: The present invention includes: an irradiation unit 11 for irradiating a material 21 with radiation; a detection unit 12 for detecting radiation that passed through the material 21 being formed; and a control unit 40. The control unit 40 monitors flows in the material 21 on the basis of information from the detection unit 12 when the material 21 is being formed. The irradiation unit 11, the detection unit 12, and the material 21 being formed are set relatively movable along a predetermined direction of the material 21 being formed and around a predetermined direction.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a material forming apparatus and a method for forming a material. [Background technology]

[0002] In recent years, with the expanding need for composite materials, the one-piece molding of parts with complex shapes has been studied. However, in one-piece molding, internal defects such as voids and porosity occur frequently. For this reason, it takes time and money to find optimal molding conditions (e.g., pressure conditions and temperature conditions), and it is not possible to quickly develop high-quality parts. Furthermore, depending on the material, the allowable range of molding conditions that are less likely to cause internal flaws is narrow, and molding conditions must be modified depending on the storage period and conditions of the material, resulting in a diversification of molding conditions and reduced productivity.

[0003] For example, Patent Document 1 discloses a control method for resin molding (RTM), in which the ratio of the resin flow permeability coefficient between both gaps in a mold and the other central part is determined in advance by simulation, and the amount of pressure reduction for resin injection when this ratio exceeds a predetermined allowable range is set in advance as reference data for multiple cases, and the pressure and temperature are corrected by comparing the actual flow pattern with the preset reference data. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2003-039479 A Summary of the Invention [Problem to be solved by the invention]

[0005] However, the control method described in Patent Document 1 only compares the ratio of permeability coefficients obtained in advance by simulation, and does not directly detect the presence or absence of internal flaws.

[0006] The present disclosure has been made in consideration of the above circumstances, and aims to provide a material molding device and a material molding method that can directly and in real time monitor defects that occur inside a material during molding. [Means for solving the problem]

[0007] In order to solve the above problems, the material molding apparatus and material molding method of the present disclosure employ the following measures. That is, a material molding apparatus according to one aspect of the present disclosure includes an irradiation unit that irradiates a material with radiation, a detection unit that detects radiation that has passed through the material during molding, and a control unit, and the control unit monitors internal defects of the material based on information from the detection unit while the material is being molded.

[0008] In addition, a method for molding a material according to one aspect of the present disclosure includes a step of irradiating a material with radiation in an irradiation unit, a step of detecting the radiation irradiated from the irradiation unit and transmitted through the material in a detection unit, and a step of monitoring for internal defects in the material based on information from the detection unit while the material is being molded. Effect of the Invention

[0009] According to the present disclosure, defects occurring within the material being molded can be directly monitored in real time. [Brief description of the drawings]

[0010] [Figure 1] 1 is a schematic configuration diagram of a material molding device according to an embodiment of the present disclosure. FIG. [Diagram 2] 2 is a cross-sectional view taken along line II-II shown in FIG. [Diagram 3] FIG. 13 is a schematic diagram of a material molding device according to another example. [Figure 4] 11A and 11B are diagrams showing changes in the heat generation range of a heater accompanying movements of an irradiation unit and a detection unit. [Diagram 5] 11A and 11B are diagrams illustrating movements of an irradiation unit and a detection unit accompanying detection of a heater. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, a material molding device and a material molding method according to an embodiment of the present disclosure will be described with reference to the drawings.

[0012] Fig. 1 shows a schematic diagram of a material molding apparatus 1 in which a material 21 being molded is placed. Fig. 2 shows a cross-sectional view taken along line II-II in Fig. 1.

[0013] As shown in FIG. 1, a material molding apparatus 1 is an apparatus used, for example, when molding a composite material in an autoclave. The material molding apparatus 1 includes an irradiation unit 11, a detection unit 12, a control unit 40, an autoclave (container) 31, and a heater (heating unit) .

[0014] Moreover, a material 21 is contained inside the autoclave 31. The material 21 may be, for example, a composite material. In this case, the material 21 is sealed in a vacuum bag 32. Moreover, the material 21 together with the vacuum bag 32 is placed on a jig 36. It should be noted that the "material" referred to here means the state before molding is completed, and is to be distinguished from the state after molding is completed.

[0015] One end of a suction nozzle 33 is connected to the vacuum bag 32. The other end of the suction nozzle 33 is connected to a vacuum pump 34. This allows the inside of the vacuum bag 32 to be evacuated.

[0016] The irradiation unit 11 is a device capable of irradiating radiation such as X-rays, etc. The irradiation unit 11 irradiates radiation toward the material 21 being molded. The detection unit 12 is a device that detects the radiation irradiated from the irradiation unit 11 . 1 and 2, the irradiation unit 11 and the detection unit 12 are disposed at positions facing each other across the material 21 being molded. With this arrangement, the detection unit 12 detects radiation that has passed through the material 21 being molded.

[0017] The control unit 40 performs image processing on information related to the amount of radiation detected by the detection unit 12 to image a cross section of the material 21 being molded. The imaged cross section is visually confirmed by an operator or automatically recognized by the control unit 40. This makes it possible to directly monitor in real time any flaws that have occurred inside the material 21 being molded (hereinafter referred to as "internal flaws"). When an internal flaw is detected, the molding conditions can be changed to ones that are less likely to cause internal flaws or ones that will eliminate internal flaws. Examples of molding conditions that can be changed will be described later. The internal defects include, for example, voids, porosity, cracks, and peeling.

[0018] Here, the control unit 40 is composed of, for example, a central processing unit (CPU), a random access memory (RAM), a read only memory (ROM), and a computer-readable storage medium. A series of processes for realizing various functions is, for example, stored in a storage medium in the form of a program, and the various functions are realized by the CPU reading this program into a RAM or the like and executing information processing and arithmetic operations. In addition, the program may be pre-installed in a ROM or other storage medium, provided in a state stored in a computer-readable storage medium, or distributed via wired or wireless communication means. The computer-readable storage medium includes a magnetic disk, a magneto-optical disk, a CD-ROM, a DVD-ROM, a semiconductor memory, and the like.

[0019] The autoclave 31 is a pressure-resistant vessel that contains the material 21 . The irradiation unit 11 and the detection unit 12 are located outside the autoclave 31. That is, the inside (layer) of the material 21 being molded is monitored from outside the autoclave 31 by the irradiation unit 11, the detection unit 12, and the control unit 40. For this reason, the furnace wall of the autoclave 31 is preferably made of a material that is easily permeable to radiation. Examples of materials that are easily permeable to radiation include aluminum alloys and reinforced plastics.

[0020] The autoclave 31 is configured so that a pressurized inert gas (e.g., nitrogen) can be supplied and discharged. This allows the pressure inside the autoclave 31 (i.e., the pressure applied to the material 21) to be adjusted as desired. The pressure is determined and adjusted by the control unit 40.

[0021] Each heater 35 has a hot wire and a power source. The hot wire portion of the heater 35 that generates heat is provided inside the autoclave 31. This allows the atmospheric temperature around the material 21 to be adjusted as desired. The temperature is determined and adjusted by the control unit 40. In addition, the output of the heater 35 according to the temperature is determined and adjusted by the control unit 40. The temperature is acquired by, for example, a thermometer (not shown) such as a thermocouple. The acquired temperature is, for example, the internal temperature of the autoclave 31, the surface temperature of the jig 36, etc.

[0022] In the material molding device 1 configured as above, the irradiation unit 11, the detection unit 12, and the material 21 being molded are relatively movable along and around a predetermined direction of the material 21. This makes it possible to detect internal flaws in the entire material 21 being molded.

[0023] As a configuration for relatively moving the irradiation unit 11 and the detection unit 12, and the material 21 being molded, for example, there are the following.

[0024] First, as shown in Fig. 1 and Fig. 2, the jig 36 on which the material 21 is placed is configured to be able to travel in a predetermined direction (left and right direction in Fig. 1) on rails 37. Also, the irradiation unit 11 and the detection unit 12 are configured not to move in the predetermined direction. As a result, the irradiation unit 11 and the detection unit 12 and the material 21 being molded move relatively along the predetermined direction of the material 21. Note that the jig 36 does not necessarily need to be moved in the predetermined direction by traveling on the rails 37, and may be moved in the predetermined direction by, for example, a linear slider or a conveyor. As shown in Fig. 2, the irradiation unit 11 and the detection unit 12 are configured to rotate around the material 21, the jig 36, and the rail 37 in a predetermined direction. At this time, the irradiation unit 11 and the detection unit 12 maintain a positional relationship in which they face each other. The material 21 is also configured not to rotate in the predetermined direction. As a result, the irradiation unit 11, the detection unit 12, and the material 21 being molded move relatively around the predetermined direction of the material 21.

[0025] Here, instead of a configuration in which irradiation unit 11 and detection unit 12 are rotated around a predetermined direction, a configuration in which material 21, jig 36 and rail 37 are rotated around a predetermined direction may be used as shown in FIG.

[0026] Furthermore, instead of a configuration in which the jig 36 on which the material 21 is placed is moved along a predetermined direction, as shown in FIG. 4, the irradiation unit 11 and the detection unit 12 may be configured to be moved along a predetermined direction. In this case, it is preferable to configure the heater 35 so that the heat generation range can be moved in accordance with the movement of the irradiation unit 11 and the detection unit 12. The heat generation range can be moved, for example, by moving the position of the contact point between the heat wire and the power source. This makes it possible to heat an appropriate position in accordance with the movement of the irradiation unit 11 and the detection unit 12.

[0027] 5, when the control unit 40 detects that a member other than the material 21 (for example, a heavy metal such as the heat ray of the heater 35) has entered the radiation irradiated from the irradiation unit 11, the irradiation unit 11 and the detection unit 12 are moved so as to change the irradiation angle of the radiation. This makes it possible to prevent, for example, the heat ray of the heater 35 from appearing in the tomographic image, thereby improving the accuracy of detecting internal flaws.

[0028] As a result of monitoring the inside of the material 21 using the material molding device 1 as described above, if any internal flaws are detected in the material 21, the molding conditions are changed as described above. The "molding conditions" referred to here are, for example, the pressure and atmospheric temperature inside the autoclave 31.

[0029] For example, if voids are detected, the pressure conditions can be changed such that the pressure inside the autoclave 31 is reduced to expel the voids, and then the pressure is increased to crush the voids. Moreover, by slowing down the heating rate inside the autoclave 31, it is possible to achieve temperature conditions that make it difficult for voids to occur. By controlling the molding conditions as described above, it is possible to change the molding conditions to those which are less likely to cause voids or to those which eliminate voids.

[0030] The pressure and temperature are merely examples of molding conditions, and if there are other conditions that can be changed, they may also be changed.

[0031] [Variations] The above explanation takes as an example the material molding device 1 used in autoclave molding, but the basic configuration of the material molding device 1 (irradiation unit 11, detection unit 12, and control unit 40) can also be applied to molding methods that use pressure and heat, such as injection molding, oven molding (non-autoclave molding), RTM (Resin Transfer Molding), etc. In addition, the material is not limited to composite materials, and may be, for example, resin or ceramic.

[0032] For example, in the case of RTM, a mold is provided into which resin (melted by heating) as material 21 is injected. This mold is provided with multiple ports (supply ports) through which the resin is supplied. If voids are detected as a result of monitoring using tomographic images, the flow rate of the resin injected from each port can be adjusted to create a resin fluidity condition that eliminates the voids. In addition to the flow rate, the pressure and temperature of the injected resin may also be adjusted. Of course, the temperature of the resin can also be changed by heater 35.

[0033] Also, for example, in the case of injection molding, a mold is provided into which resin (melted by heating) or ceramic powder as material 21 is fed. This mold is provided with multiple gates (supply ports) through which the resin or ceramic powder is fed. If voids are detected as a result of monitoring using tomographic images, the flow rates of the resin or ceramic powder fed from each gate can be adjusted to achieve flow conditions for the resin or ceramic powder that eliminate the voids. In addition to the flow rates, the pressure or temperature of the resin or ceramic powder fed may also be adjusted.

[0034] In any of the above molding methods, internal defects in the material 21 can be directly monitored in real time by imaging the cross-section of the mold.

[0035] This embodiment provides the following advantages. The material molding device 1 includes an irradiation unit 11 that irradiates radiation onto the material 21, a detection unit 12 that detects radiation that has passed through the material being molded, and a control unit 40, and the control unit 40 monitors internal flaws in the material 21 based on information from the detection unit 12 while the material 21 is being molded, so that flaws (e.g., voids, porosity, etc.) that have occurred inside the material 21 being molded can be detected directly and in real time. This makes it possible to change, for example, based on the detection results, the molding conditions to those that are less likely to cause internal flaws or to those that will eliminate internal flaws. The molding conditions include, for example, pressure conditions, temperature conditions, and material flowability conditions.

[0036] In addition, the irradiation unit 11 and detection unit 12 and the material 21 being molded are capable of moving relatively along and around a specified direction of the material 21 being molded, so that internal flaws in all directions of the material 21 being molded can be detected.

[0037] Furthermore, since the heating section has a heat generating range that can be moved in a predetermined direction, it is possible to heat an appropriate position in accordance with the relative movement of the material during molding.

[0038] Furthermore, when the control unit detects a member other than the material 21 being molded, it changes the position of the irradiation unit 11 so as to change the irradiation angle of the radiation, so that even if the material 21 being molded and the heat rays of the heater 35 overlap on the irradiated radiation, for example, the radiation can be irradiated while avoiding them. This makes it possible to improve the accuracy of detecting internal defects.

[0039] Furthermore, the molding method of material 21 includes a step of irradiating radiation to the material by irradiation unit 11, a step of detecting the radiation irradiated from irradiation unit 11 and transmitted through the material by detection unit 12, and a step of monitoring internal defects in material 21 based on information from detection unit 12 during molding of the material, so that defects (e.g., voids, porosity, etc.) occurring inside material 21 during molding can be detected directly and in real time. This makes it possible to optimize molding conditions based on the detection results, and the material can be molded under molding conditions that are less likely to cause internal defects or that eliminate internal defects.

[0040] The present embodiment described above can be understood, for example, as follows. That is, a material molding device (1) according to one embodiment of the present disclosure includes an irradiation unit (11) that irradiates a material (21) with radiation, a detection unit (12) that detects radiation that has passed through the material during molding, and a control unit (40), and the control unit monitors for internal defects in the material based on information from the detection unit while the material is being molded.

[0041] The material molding device according to this embodiment includes an irradiation unit that irradiates radiation onto the material, a detection unit that detects radiation that has passed through the material being molded, and a control unit, and the control unit monitors internal flaws in the material based on information from the detection unit while the material is being molded, so that flaws (e.g., voids, porosity, etc.) that have occurred inside the material being molded can be detected directly and in real time. This makes it possible to change the molding conditions to those that are less likely to cause internal flaws or to those that will eliminate internal flaws, for example, based on the detection results. The monitoring of internal defects is carried out, for example, by imaging cross sections caused by radiation.

[0042] In addition, in a material molding apparatus according to one aspect of the present disclosure, the irradiation unit, the detection unit, and the material being molded are capable of moving relatively along a predetermined direction of the material being molded and around the predetermined direction.

[0043] According to the material molding device of this embodiment, the irradiation unit, the detection unit, and the material being molded are capable of moving relatively along a specified direction of the material being molded and around the specified direction, so that internal defects can be detected for the entire material being molded.

[0044] In addition, a material molding device according to one embodiment of the present disclosure includes a container (31) that contains the material being molded and has an adjustable internal pressure, and the control unit controls the internal pressure of the container based on information from the detection unit.

[0045] The material molding device of this embodiment is equipped with a container that holds the material being molded and has an adjustable internal pressure, and the control unit controls the pressure inside the container based on information from the detection unit, making it possible to mold the material under pressure conditions that are less likely to cause internal scratches, or to mold the material under pressure conditions that will eliminate internal scratches in the material.

[0046] In addition, a material molding apparatus according to one embodiment of the present disclosure includes a mold to which the material is supplied through a plurality of supply ports, and the control unit controls at least one of the flow rate, pressure, and temperature of the material supplied from each of the supply ports based on information from the detection unit.

[0047] The material molding apparatus of this embodiment is equipped with a mold to which material is supplied through multiple supply ports, and the control unit controls at least one of the flow rate, pressure, and temperature of the material supplied from each supply port based on information from the detection unit, so that the material can be molded under material conditions that eliminate internal defects in the material.

[0048] In addition, a material molding apparatus according to one embodiment of the present disclosure includes a heating unit (35) that heats the ambient temperature surrounding the material being molded, and the control unit controls the output of the heating unit based on information from the detection unit.

[0049] The material molding device of this embodiment is equipped with a heating unit that heats the atmospheric temperature surrounding the material being molded, and the control unit controls the output of the heating unit based on information from the detection unit, so that the material can be molded under temperature conditions that are less likely to cause internal flaws, or can be molded under temperature conditions that will eliminate internal flaws.

[0050] In addition, in the material molding apparatus according to one aspect of the present disclosure, the heating section is configured so that the heat generation range is movable in a predetermined direction.

[0051] According to the material molding device of this embodiment, the heating section has a heat generation range that can be moved in a predetermined direction, so that appropriate positions can be heated in accordance with the relative movement of the material during molding.

[0052] In addition, in a material molding apparatus according to one aspect of the present disclosure, when a control unit detects a component other than the material being molded, the control unit changes the position of the irradiation unit so as to change the irradiation angle of the radiation.

[0053] According to the material molding device of this aspect, when the control unit detects a component other than the material being molded, it changes the position of the irradiation unit so that the irradiation angle of the radiation changes, so that even if the material being molded and an obstacle overlap on the irradiated radiation, the radiation can be irradiated while avoiding the obstacle, thereby improving the accuracy of detecting internal defects.

[0054] In addition, a method for molding a material according to one aspect of the present disclosure includes a step of irradiating a material with radiation in an irradiation unit, a step of detecting the radiation irradiated from the irradiation unit and transmitted through the material in a detection unit, and a step of monitoring for internal defects in the material based on information from the detection unit while the material is being molded.

[0055] The material molding method according to this embodiment includes a step of irradiating the material with radiation by an irradiation unit, a step of detecting the radiation irradiated from the irradiation unit and transmitted through the material by a detection unit, and a step of monitoring internal defects in the material based on information from the detection unit while the material is being molded, so that defects (e.g., voids, porosity, etc.) that occur inside the material during molding can be detected directly and in real time. This makes it possible to optimize molding conditions based on the detection results, and the material can be molded under molding conditions that are less likely to cause internal defects or that eliminate internal defects. [Explanation of symbols]

[0056] 1 Material forming equipment 11 Irradiation unit 12 Detection section 21 Material 31 Autoclave (container) 32 Vacuum Bag 33 Suction nozzle 34 Vacuum Pump 35 Heater (heating part) 36 Jig 37 Rail 40 Control section

Claims

1. an irradiation unit that irradiates radiation onto a material; a detection unit that detects radiation transmitted through the material being molded; A control unit; Equipped with The control unit is During molding of the material, monitoring for internal flaws in the material based on information from the detection unit; When a member other than the material being molded is detected, the position of the irradiation unit is changed so that the irradiation angle of the radiation changes. Material forming equipment.

2. An irradiation unit that irradiates a material with radiation; a detection unit that detects radiation transmitted through the material being molded; a container for containing the material being molded and having an adjustable internal pressure; A control unit; Equipped with The control unit is monitoring for internal flaws in the material based on information from the detection unit during molding of the material; The pressure inside the container is controlled based on the information from the detection unit. Material forming equipment.

3. The irradiation unit, the detection unit, and the material being molded are relatively movable along a predetermined direction of the material being molded and around the predetermined direction. The material forming apparatus according to claim 1 .

4. The irradiation unit, the detection unit, and the material being molded are movable relatively along a predetermined direction of the material being molded and around the predetermined direction.

3. The material forming apparatus according to claim 2.

5. A container is provided for containing the material being molded and the internal pressure of the container is adjustable; The control unit controls the pressure inside the container based on the information from the detection unit.

4. The material molding device according to claim 1 or 3.

6. a mold into which the material is supplied through a plurality of supply ports; The control unit controls at least one of a flow rate, a pressure, and a temperature of the material supplied from each of the supply ports based on information from the detection unit.

4. The material molding device according to claim 1 or 3.

7. A heating unit is provided for heating the ambient temperature of the material during molding, The control unit controls an output of the heating unit based on information from the detection unit.

7. A material molding apparatus according to claim 1.

8. The heating section has a heat generating range that can be moved in a predetermined direction.

8. The material forming apparatus according to claim 7.

9. A step of irradiating radiation onto a material in an irradiation unit; detecting radiation irradiated from the irradiation unit and transmitted through the material with a detection unit; monitoring for internal flaws in the material based on information from the detector during molding of the material; changing an irradiation angle of radiation when a member other than the material being molded is detected; Includes How the material is molded.

10. A step of irradiating a material with radiation by an irradiation unit; detecting radiation irradiated from the irradiation unit and transmitted through the material with a detection unit; monitoring for internal flaws in the material based on information from the detector during molding of the material; controlling the pressure inside a container that contains the material being molded based on information from the detection unit; Includes How the material is molded.

Citation Information

Patent Citations

  • Production of refractory product

    JP1985181642A

  • Method and apparatus for monitoring cure of resin

    JP1994344366A

  • Method for observing directly inside of coal-packed bed under carbonization

    JP2000131247A

  • Observation of resin behavior in resin sealing process for semiconductor device by using resin sealing unit and its control method

    JP2000200796A

  • Method for controlling rtm resin fluidity and device therefor

    JP2003039479A