Air introduction / exit member, temperature control pot mold, preform temperature control method, and blow molding device
The preform temperature adjustment device addresses the issues of slow cooling and uneven thickness in blow molding by using a hollow rod with a flow path adjustment member to enhance air flow velocity and temperature uniformity, resulting in transparent and uniformly thick containers.
Patent Information
- Application Number
- JP2020195044
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-01-31
- Filing Date
- 2020-11-25
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2040-01-31
AI Technical Summary
Conventional blow molding devices face challenges in finely adjusting the radial gap between the hollow rod and preform, leading to slow air flow rates and reduced cooling efficiency, resulting in non-transparent containers and uneven thickness due to temperature inconsistencies.
A preform temperature adjustment device with a hollow rod and flow path adjustment member that forms a first air flow path between the preform and the hollow rod, allowing for precise control of the air flow passage area to enhance cooling efficiency and uniform temperature distribution.
The device shortens molding cycle time, ensures transparency of the finished container, and eliminates uneven thickness by improving air flow velocity and temperature uniformity.
Smart Images

Figure 0007566596000002 
Figure 0007566596000003 
Figure 0007566596000004
Abstract
Description
[Technical field]
[0001] The present invention relates to a preform temperature adjustment device and method for a hot parison type blow molding machine. Specifically, the present invention relates to a preform temperature adjustment device and method that can perform an appropriate temperature adjustment process in a short time even for a preform that has been released from a mold at a high temperature after a short injection molding time. [Background technology]
[0002] Conventionally, there has been known a blow molding apparatus equipped with an injection molding section for injection molding a preform, a temperature adjustment section for adjusting the temperature of the preform molded in the injection molding section, and a blow molding section for blow molding the preform whose temperature has been adjusted in the temperature adjustment section (see, for example, Patent Document 1). This type of blow molding apparatus is obtained by adding a temperature adjustment section to a conventional blow molding apparatus mainly equipped with only an injection molding section and a blow molding section (see, for example, Patent Document 2). Since a preform just molded in the injection molding section does not have a temperature distribution suitable for blow molding, a temperature adjustment section capable of more actively adjusting the temperature of the preform is provided between the injection molding section and the blow molding section, making it possible to adjust the temperature of the preform to a temperature suitable for blow molding. Note that this temperature adjustment section uses a heating pot type (heating block) or a heating rod to heat the preform without contact and adjust the temperature.
[0003] There is also a temperature control method that can quickly and locally cool only the bottom of a preform to successfully mold a container with a thick bottom. Specifically, a blow molding device has been proposed for manufacturing a container that has a bottom having a desired thickness and a body having a wall part stretched to a uniform thin wall when blow molding is performed by inserting a preform into a cavity of a temperature control pod mold, and by bringing the outer peripheral surface of the bottom of the preform and the lower part of the body part connected to the bottom into close contact with a cooling pot and a cooling rod arranged below the temperature control pod mold to ensure cooling, and by raising the temperature of the body part except for the lower part of the body part connected to the bottom to a predetermined temperature by a heating block arranged above the temperature control pod mold (see, for example, Patent Document 3).
[0004] Also, a blow molding apparatus has been proposed in which the preform is cooled not only in the injection molding section but also in a temperature control section, thereby shortening the injection molding time (specifically, the cooling time) that determines the molding cycle time (for example, see Patent Document 4).Moreover, in recent years, a device has been devised in which a hollow rod is inserted into a preform housed in a temperature control pod mold, and cooling air is circulated through the gap between the outer periphery of the hollow rod and the inner periphery of the preform to cool the entire preform, thereby shortening the molding cycle time and making the container transparent. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Japanese Patent Application Publication No. 06-315973 [Patent Document 2] International Publication No. 2017 / 098673 [Patent Document 3] International Publication No. 2013 / 012067 [Patent Document 4] Japanese Patent Application Publication No. 05-185493 Summary of the Invention [Problem to be solved by the invention]
[0006] However, in the above conventional example, it is difficult to finely adjust the radial dimension of the gap between the outer periphery of the hollow rod and the inner periphery of the preform, and the cross-sectional area of the gap must be relatively large, which tends to reduce the air flow rate and result in insufficient cooling efficiency. As a result, when a thermoplastic resin that is easily crystallized in the temperature range during blow molding is used as the material for the preform, there is a problem that the resulting finished container is not transparent and is prone to whitening or clouding.
[0007] In addition, even if there is a temperature deviation in the circumferential direction of the preform coming from the injection molding section, it is difficult to eliminate this by short-term processing in the temperature adjustment section, and there is a problem that thickness deviation occurs in the body of the container obtained by blow molding the preform in the blow molding section subsequent to the temperature adjustment section.
[0008] The present invention aims to provide a preform temperature adjustment device in a blow molding machine that can shorten the molding cycle time and eliminate uneven thickness while making the container transparent, and a straightening member used therein. [Means for solving the problem]
[0009] The preform temperature adjustment device of the present invention is characterized in that, in order to adjust the temperature of an injection-molded, bottomed preform (1), a hollow rod member (18) is inserted into the preform (1) held by a holding member (50) and a first air flow passage (21a) is formed between the preform (1) and the hollow rod member (18), in the preform temperature adjustment device (20), a flow path adjustment member (19) is fitted onto the outer periphery of the hollow rod member (18) and attached, thereby at least partially adjusting the cross-sectional area of the first air flow passage (21a).
[0010] Furthermore, the preform temperature adjustment method of the present invention is a method for adjusting the temperature of a preform, in which an injection-molded, bottomed preform (1) is held by a holding member (50) and temperature-adjusted in a temperature adjustment section (20), and is characterized by comprising the steps of: inserting a hollow rod member (18) to which a flow path adjustment member (19) is attached into the preform (1) to form a first air flow passage (21a) between the preform (1) and the flow path adjustment member (19); and inserting the hollow rod member (18), the flow path adjustment member (19), and the preform (1) into a cavity (17a) of a temperature control pot mold (17), and then circulating cooling air through the first air flow passage (21a).
[0011] The present invention also provides an apparatus for manufacturing resin molded containers, which is an apparatus for manufacturing resin molded containers (100) including an injection molding section (10) for injection molding a bottomed preform (1), a temperature adjustment section (20) for adjusting the temperature of the preform (1) molded in the injection molding section (10), and a blow molding section (30) for blow molding the preform (1) whose temperature has been adjusted in the temperature adjustment section (20), and which is characterized in that in the blow molding apparatus (100) in which a hollow rod member (18) is inserted into the preform (1) held by a holding member (50) to form a first air flow passage (21a) between the preform (1) and the hollow rod member (18), a flow path adjustment member (19) is fitted onto the outer periphery of the hollow rod member (18) and attached, thereby adjusting the area of the first air flow passage (21a) at least partially.
[0012] In addition, in the method for manufacturing a resin molded container of the present invention, an injection-molded, bottomed preform (1) is held by a holding member (50) and blow molded after being temperature-adjusted in a temperature adjustment section (20), and includes the steps of: forming a first air flow passage (21a) between the preform (2) and the flow passage adjustment member (19) by inserting a hollow rod member (18) having a flow passage adjustment member (19) attached thereto into the preform (1) during temperature adjustment in the temperature adjustment section (20); and circulating cooling air through the first air flow passage (21a) after inserting the hollow rod member (18), flow passage adjustment member (19), and preform (1) into a cavity of a temperature-adjusted pot mold (17). Effect of the Invention
[0013] The present invention can provide a preform temperature adjustment device and a temperature adjustment method that can shorten the molding cycle time and eliminate uneven thickness while making the finished container transparent. [Brief description of the drawings]
[0014] [Figure 1] 1 is a perspective view of a blow molding apparatus, which is an example of a resin molded container manufacturing apparatus to which a preform temperature adjustment device according to an embodiment of the present invention is applied; [Diagram 2] FIG. 2 is a perspective view of an example of a preform being injection molded in the injection molding section. [Diagram 3] 3 is a cross-sectional front view of the temperature adjustment unit. FIG. [Figure 4] FIG. 4 is an enlarged cross-sectional view of a main portion of FIG. [Diagram 5] FIG. 2 shows a front view of the hollow rod of the temperature adjustment unit. [Figure 6] 6(A) and (B) respectively show a front view of a first embodiment of a rectifying rod used in the temperature adjusting section and a cross-sectional view taken along line VIB-VIB in FIG. 6(A). [Figure 7]7(A) and (B) respectively show a partially sectional front view of a second embodiment of a rectifying rod and a sectional view taken along line VIIB-VIIB in FIG. 7(A). [Figure 8] 8(A) and (B) respectively show a partially sectional front view of a third embodiment of a straightening rod and a sectional view taken along line VIIIB-VIIIB in FIG. 8(A). [Figure 9] 9(A) and (B) respectively show a front cross-sectional view of the fourth embodiment of the flow straightening rod and a cross-sectional view taken along line IXB-IXB in FIG. 9(A). [Figure 10] 9 is used in a temperature adjustment section, the cross-sectional view corresponding to FIG. 4. FIG. [Figure 11] 11(A) to (C) respectively show a front cross-sectional view of the fifth embodiment of the rectifying rod, and cross-sectional views taken along lines XIB-XIB and XIC-XIC in FIG. 11(A). [Figure 12] Figures 12(A) to (C) respectively show a front cross-sectional view of the sixth embodiment of the straightening rod, a cross-sectional view along line XIIA-XIIA in Figure 12(B), the front cross-sectional view, and a cross-sectional view along line XIIC-XIIC in Figure 12(B). [Figure 13] Figures 13(A) and (B) are respectively a front cross-sectional view of an example of a hollow rod to which the straightening rod shown in Figure 12 is applied, a cross-sectional view along line XIIIA-XIIIA in Figure 13(B), and the front cross-sectional view. [Figure 14] 16 shows a cross-sectional view corresponding to FIG. 4 when the flow straightening rods and hollow rods shown in FIG. 12, FIG. 13 and FIG. 15 are used in a temperature adjusting section. [Figure 15] Figures 15(A) to (C) respectively show a front cross-sectional view of the seventh embodiment of the straightening rod, a cross-sectional view along line XVA-XVA in Figure 15(B), the front cross-sectional view, and a cross-sectional view along line XVIC-XVIC in Figure 15(B). [Figure 16] Figures 16(A) and (B) are respectively a front cross-sectional view of another example of a hollow rod to which the straightening rod shown in Figure 15 can be applied, a cross-sectional view along line XVIA-XVIA in Figure 16(B), and the front cross-sectional view. [Figure 17]17(A) to (C) show a perspective view, a front view, and a plan view, respectively, of the finished container removed after blow molding the preform. [Figure 18] FIG. 7 is a cross-sectional view of the rectifying rod shown in FIG. 6. [Figure 19] 19(A) and (B) are diagrams showing first and second experimental data indicating the uneven thickness state of a completed container, respectively. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] Hereinafter, preferred embodiments of the present invention will be described with reference to the drawings. (First embodiment) FIG. 1 shows an oblique view of a blow molding apparatus, which is an example of a manufacturing apparatus for resin molded containers to which a preform temperature adjustment device according to one embodiment of the present invention is applied; FIG. 2 shows an oblique view of a preform injection molded in the injection molding section; FIG. 3 shows a cross-sectional view of the temperature adjustment section as viewed from the front; and FIG. 4 shows an enlarged cross-sectional view of a key portion of FIG. 3.
[0016] As shown in FIG. 1, the blow molding apparatus 100 includes an injection molding section 10, a temperature adjustment section 20, a blow molding section 30, and an ejection section 40, and is an apparatus for injection molding a preform 1 in the injection molding section 10, and then finally blow molding the preform 1 in the blow molding section 30 to produce a container 101 (see FIGS. 1 and 14).
[0017] The injection molding section 10, the temperature adjustment section 20, the blow molding section 30, and the removal section 40 are arranged in such an arrangement as to form the four sides of a square when viewed from above. Above these, a rotating disk (not shown) is provided with a neck mold 50 (see FIG. 3) for holding the neck portion 3 (see FIG. 2) of the preform 1 molded in the injection molding section 10. This rotating disk has four sets of neck molds 50 arranged in such an arrangement as to form the four sides of a square when viewed from above. As a result, the rotating disk rotates 90 degrees counterclockwise around a vertical axis on the injection molding section 10, the temperature adjustment section 20, the blow molding section 30, and the removal section 40, so that each process is performed on the preform 1 held by the neck mold 50.
[0018] The injection molding section 10 includes an injection core mold 11, an injection cavity mold 12, and an injection device (not shown), and is provided to injection mold the preform 1. The injection core mold 11 and the injection cavity mold 12 are provided with a cooling circuit (not shown), and a cooling medium of about 5 to 20°C is flowed through them. The preform 1 is made of a thermoplastic synthetic resin, and is formed with a bottom (hollow bottom) having a neck portion 3 on the open side and a storage portion (main body portion) 2 on the closed side, as shown in Fig. 2. The storage portion 2 is composed of a body portion 2a connected to the neck portion 3 on the open side, and a bottom portion 2b located on the closed side and connected to the body portion 2a. The preform 1 is blow molded to become a finished container 102 such as a PET bottle (see Figs. 1 and 14), and has a shape such that the container 102 after blow molding has been shrunk in the vertical and horizontal directions in Fig. 14 to make it thicker.
[0019] In the injection molding section 10, a thermoplastic synthetic resin material (for example, a polyester resin such as PET (polyethylene terephthalate)) is heated at a high temperature to melt it, and the melted material is injected (filled) between the molding space (cavity) defined by the injection core mold 11, the injection cavity mold 12, and the neck mold 50 by an injection device (not shown). The material of the part of the injected material close to the cavity surface is cooled to a temperature lower than the melting point (for example, about 255 ° C. in the case of PET), for example, about 20 ° C., and solidified to form a surface layer (suitably called an external layer, outer layer, or skin layer) in the storage section 2, and the preform 1 is molded. At this time, the internal layer (suitably called an internal layer or core layer) of the storage section 2 of the preform 1 is kept at a temperature below the melting point of the molding material and above the glass transition point temperature (for example, 150 to 200 ° C.), and the storage section 2 is adjusted so that it has a heat amount (retained heat) that can be stretched in the blow molding section 30. In this embodiment, the molding cycle time, that is, the molding time of the preform 1, is shortened compared to the conventional method. Specifically, of the injection time (filling time) and cooling time related to the injection molding time of the preform, the cooling time is set to be significantly shorter than that of the conventional method. For example, the cooling time is set to 2 / 3 or less of the injection time, preferably 1 / 2 or less, and more preferably 1 / 3 or less.
[0020] The preform 1, which has solidified to a certain extent after being injection molded in the injection molding section 10, is lifted upward together with the rotating plate while still held by the neck mold 50, and is pulled out (released) from the injection cavity mold 12 and the injection core mold 11. As shown in FIG. 1, the rotating plate rotates 90 degrees counterclockwise, and is transported to the temperature adjustment section 20.
[0021] The temperature adjustment section 20 is disposed next to the injection molding section 10, and as shown in Figures 3 and 4, is equipped with a cylindrical air nozzle 16 at the top and a temperature adjustment pot mold 17 at the bottom. The lower end of the air nozzle 16 abuts airtightly against the neck portion 3 of the preform 1. The temperature adjustment pot mold 17 is composed of multiple steps (temperature adjustment blocks) in the vertical direction so that the temperature of the preform 1 can be adjusted in the vertical direction. Temperature adjustment media (cooling media) of different temperatures (for example, a predetermined temperature in the range of 10°C to 90°C) can be circulated in each step. The internal structure of the cylindrical air nozzle 16 will now be described.
[0022] Reference numeral 18 denotes a hollow rod inserted into the preform 1, and as shown in Figures 3 to 5, a sleeve (hollow piece) 18a is fitted and fixed to the lower end, and the hollow rod 18 is arranged concentrically with the cylindrical air nozzle 16 and fixed to a fixed portion 18b at the upper part. As shown in Figure 5, the hollow rod 18 has a cooling air outlet hole 18c at the upper end, a circumferential groove 18d below, and an air flow passage 21b inside. The sleeve 18a is provided when the axial length of the preform 1 is large, and is not necessarily required when the length of the preform 1 is short.
[0023] 19A is a first embodiment of a cylindrical flow path adjustment rod (hereinafter, referred to as a flow straightening rod), and as shown in Figures 4 and 6, the outer periphery 19a has a true circular cross section (see Figure 6(B)), and is a truncated cone shape whose outer diameter gradually decreases from the top to the bottom, and has an engaged portion (screw hole) 19b provided at the upper end, and a relatively large curved surface provided on the outer periphery of the lower end 19c to facilitate the flow of cooling air described later. The inclination angle of this truncated cone is determined according to the inclination angle of the inner periphery of the preform 1, and in this case is, for example, 0.34 degrees with respect to the axis.
[0024] As shown in Figures 3 and 4, this rectifying rod 19A is attached by commonly fitting it to the lower end of the hollow rod 18 and the outer periphery of the sleeve 18a, and is firmly fixed by engaging an engaging member (screw) 24 (see Figure 4) with the circumferential groove 18d via the engaged portion (screw hole) 19b at the upper end of the rectifying rod 19A. Therefore, since the rectifying rod 19A can be easily attached and detached to the hollow rod 18 by a screw fastening method or the like, various different types of rectifying rods can be easily and interchangeably attached to the same hollow rod 18. In other words, there is no need to prepare different types of hollow rods themselves, and costs and labor can be reduced. Thus, the air nozzle 16, hollow rod 18 and rectifying rod 19A form an integrated structure (hereinafter, this integrated structure will be simply referred to as an air inlet / outlet member), and are raised and lowered as an integrated structure by a drive device (not shown).
[0025] As described later, when the preform 1 supported by the neck mold 50 is inserted into the pot cavity 17a (see FIG. 4) of the temperature-controlled pot mold 17 and the air inlet / outlet member is lowered to contact the neck portion 3, the cooling air (compressed air) flowing in from the cooling air inlet 16a (see FIG. 3) flows from the inner periphery of the air nozzle 16 to the outer periphery of the rectifying rod 19A and the inner periphery of the preform 1, forming a first air flow passage 21a with a ring-shaped cross section between the outer periphery of the rectifying rod 19A and the inner periphery of the preform 1, and the cooled air that moves radially inward at the lower end of the rectifying rod 19A flows upward from the lower end opening of the sleeve 18a to the inside of the sleeve 18a and the inside of the hollow rod 18, forming a second air flow passage 21b. The cooled air is discharged to the outside from the air outlet 16b through the upper cooling air outlet hole 18c (see FIG. 3). In some cases, the air may flow in from the second air flow passage 21b and flow out through the first air flow passage 21a. In addition, the space formed in the first air flow passage 21a, particularly between the straightening rod 19A and the inner circumference of the preform 1, is called a ring-shaped gap 22 (see FIG. 4). The radial dimension of this ring-shaped gap 22 is smaller than the radial dimension formed between the upstream hollow rod 18 and the air nozzle 16, and is set to, for example, 0.5 to 1.5 mm, preferably 0.5 mm to 1.0 mm. Therefore, the air flow passing through the ring-shaped gap 22 is narrowed and flows at a higher speed than the upstream side. In other words, by using the flow path adjustment rod, the cooling air can be made faster and more straight in the ring-shaped gap 22 than in the upstream area.
[0026] Next, the operation of the preform temperature adjustment device of the present invention will be described. 3 and 4, the preform 1 supported by the neck mold 50 is transported from the injection molding section 10 and inserted into the cavity 17a of the temperature control pot mold 17. Before and after this, the air inlet / outlet member is lowered, and the hollow rod 18 and the straightening rod 19 are inserted into the preform 1. At this time, the neck mold 50 is centered with respect to a centering ring 60 attached onto the temperature control pot mold 17 .
[0027] As described above, the first air flow passage 21a (ring-shaped gap 22) into which the cooling air flows and the second air flow passage 21b through which the air used to cool the preform 1 flows are formed.
[0028] 3, for example, cooling air at room temperature (for example, 10°C to 20°C) passes through the first air flow passage 21a, i.e., the ring-shaped gap 22, from the air inlet 16a at a relatively high speed, thereby providing a large cooling effect to the main body 2 (body 2a and bottom 2b) of the preform 1, and lowering the temperature of the preform 1 to an appropriate temperature suitable for the next blowing process. Before cooling the preform 1 by circulating the cooling air through it, compressed air may be separately introduced into the preform 1 to bring the preform 1 into close contact with the cavity 17a of the temperature control pot mold 17. This allows the preform 1 to be cooled from the inside and the temperature to be reliably controlled from the outside, improving the cooling effect as well as the efficiency of removing temperature deviations and uniform temperature. After cooling, the air smoothly changes its flow direction radially inward at the lower end of the first air flow passage 21a, i.e., at the lower end 19c of the straightening rod, and then rises through the second air flow passage 21b inside the sleeve 18a and is discharged to the outside through the air outlet 16b.
[0029] According to this, when comparing the conventional case where no straightening rods are provided with the case where the straightening rods 19A are provided as in the present invention, the radial dimension of the ring-shaped gap 22 of the present invention is finely adjusted smaller by the amount of the straightening rods 19A provided, compared to the former case where no straightening rods are provided. Therefore, the flow velocity of the cooling air passing through the first air flow passage 21a increases by that amount, improving the cooling efficiency of the preform.
[0030] Even when the cross-sectional area of the ring-shaped gap in the conventional example is relatively large, it is possible to increase the flow rate of the cooling air by increasing the air pressure or the amount of air supplied, but this results in a problem of increased air consumption.
[0031] Second embodiment FIG. 7 shows a second embodiment of the flow straightening rod, that is, a flow straightening rod 19B. The flow straightening rod 19B has a notch 19d extending in the axial direction at least at one location in the circumferential direction of the outer periphery.
[0032] As a result of carrying out an experiment using the flow straightening rod 19B having the notch 19d (see Figs. 16(A) and (B)), it was observed that the thickness of the container 101 at the portion corresponding to the notch 19d of the preform storage portion 2 tends to be larger than the thickness of the non-corresponding portion. This will be described in detail later.
[0033] Third embodiment FIG. 8 shows a straightening rod 19C which is a third embodiment of the straightening rod. The rectifying rod 19C has two axially extending notches 19d1 and 19d2 at circumferential positions on the outer periphery, which are diametrically opposed to each other. Therefore, the wall thickness of the container 101 at two locations corresponding to the two notches 19d1 and 12d2d of the preform storage portion 2 is greater than the wall thickness of the non-corresponding portions. Of course, the notches 19d may be provided at three or more locations in the circumferential direction of the outer periphery.
[0034] (Fourth embodiment) FIG. 9 shows a flow straightening rod 19D which is a fourth embodiment of the flow straightening rod. This straightening rod 19D has a large diameter portion 19e at the upper end, a small diameter portion 19f at the axially lower portion, and a generally tapered portion 19g connecting these. FIG. 10 shows the state in which this straightening rod 19D is attached to the hollow rod 18 and the sleeve 18a, and further inserted into the cavity 17a of the temperature control pod mold 17 together with a preform 1B, which is different from the preform 1A held by the neck mold 50. In this figure, the same parts as those in FIG. 4 are given the same reference numerals and their explanation will be omitted. As seen from this figure, the second preform 1B has a substantially tapered inner diameter portion 1c connecting the large inner diameter portion 1a at the neck portion 3A and the smaller inner diameter portion 1b below.
[0035] Therefore, the large diameter portion 19e, the tapered portion 19g and the small diameter portion 19f of the straightening rod 19D are in contact with the three inner diameter portions 1a, 1c and 1b of the preform 1B in order with approximately uniform gap dimensions, thereby providing a first air flow passage 21a with a uniform cross-sectional area along the flow of cooling air, and a uniform cooling effect can be imparted along the axial direction of the preform 1B.
[0036] Fifth embodiment FIG. 11 shows a flow rod 19E which is a fifth embodiment of the flow rod. 9, but further has a notch 19h extending in the axial direction at one circumferential position on the outer periphery. Of course, the notch 19h may be provided at two or more circumferential positions on the outer periphery.
[0037] Therefore, according to this, the same effects as those of the notches 19d (19d1 and 19d2) of the third and fourth embodiments (FIGS. 7 and 8) are achieved. In each of the above embodiments, the cross-sectional shape of the straightening rod 19 is basically circular, but is not limited to this and may be elliptical or polygonal, and one or more notches may be further provided in these ellipses or polygons. In addition, in each of the above-described embodiments, the cutouts 19d, 19h are linear, but the cutouts are not limited to this and may take various forms such as curved or uneven.
[0038] Sixth embodiment 12(A) to (C) show a flow straightening rod 19F which is a sixth embodiment of the flow straightening rod. The rectifying rod 19F is provided at its upper end with a polygonal (for example, regular octagonal) engaging recess 19i. The polygonal engaging recess 19i has a plurality (eight) of substantially rectangular inner surfaces.
[0039] Fig. 13 shows a hollow rod 18X for mounting the rectifying rod 19F. In the embodiment shown in Fig. 4 and Fig. 10, a sleeve 18a, which is a separate member, is mounted on the lower end of the hollow rod 18, but this hollow rod 18X has a sleeve portion 18e integrally formed at the lower end, and an engagement protrusion 18f consisting of a polygonal prism portion is formed at a height position in the middle. This prism portion has a plurality (eight pieces) of substantially rectangular outer surface portions. Therefore, as shown in Fig. 14, the rectifying rod 19F is fitted into the sleeve portion 18e of the hollow rod 18X from below in the figure (the side toward the open end through which the compressed air flows in and out), and the polygonal engagement recess 19i is engaged with the polygonal engagement protrusion 18f of the hollow rod 18X in a direction determined based on polygonal engagement. More specifically, multiple inner surfaces of the engagement recess 19i come into contact with multiple outer surfaces of the prismatic portion of the polygonal engagement protrusion 18f, and the rectifying rod 19F is engaged with the hollow rod 18X in a state oriented (positioned) at a predetermined angular position in the circumferential direction. Furthermore, the lower end of the rectifying rod 19F is supported by a locking member (retaining ring) 23 (see FIG. 14) attached to the locking ring engagement recess 18g at the lower end of the sleeve portion 18e, and is locked to the hollow rod 18X.
[0040] According to this, for example, in FIG. 14, the gap size of the ring-shaped gap 22 varies slightly depending on the circumferential angle position, and therefore the degree of cooling (cooling strength) by the cooling air can be changed depending on the circumferential angle position. Specifically, the distribution of the degree of cooling can be adjusted by removing the rectifying rod 19F, rotating it by a predetermined angle (for example, 45 degrees), and reattaching it to the hollow rod 18X. That is, the position of the notch 19h of the rectifying rod 19F can be changed so as to face the high-temperature portion of the preform 1, thereby increasing the degree of cooling (cooling strength) of the high-temperature portion. The polygonal engagement recess 19i and the polygonal engagement protrusion 18f may be polygonal other than an octagon as long as it is a triangle or more.
[0041] Seventh embodiment 15(A) to (C) show a straightening rod 19G which is a seventh embodiment of the straightening rod. The rectifying rod 19G is provided with a plurality of (e.g., eight) engaging recesses 19j at equally spaced circumferential positions on the upper end of the rectifying rod 19G. Each engaging recess 19j is, for example, substantially rectangular or slit-shaped, and is formed so as to be recessed toward the outer diameter side on the inner circumferential surface of a substantially cylindrical recessed portion formed on the upper end of the rectifying rod 19G.
[0042] FIG. 16 shows a hollow rod 18Xa to which the rectifying rod 19G is attached. The hollow rod 18Xa also has a sleeve portion 18e integrally formed at its lower end, and a single engaging protrusion 18h consisting of a single protrusion (a substantially rectangular flat-plate-shaped protrusion) protruding in the radial direction at a midpoint in height. Therefore, the rectifying rod 19G is fitted into the sleeve portion 18e of the hollow rod 18Xa from below in the figure (the side toward the open end through which the compressed air flows in and out), and one of the engaging recesses 19j is oriented and engaged with the single engaging protrusion 18h of the hollow rod 18Xa. More specifically, the single engaging protrusion 18h is fitted into one of the multiple engaging recesses 19j, and the rectifying rod 19G is engaged with the hollow rod 18Xa in a oriented (positioned) state at a predetermined angular position in the circumferential direction. Furthermore, the lower end of the rectifying rod 19G is supported by a locking member (stop ring) 23 attached to a stop ring engagement recess 18g at the lower end of the sleeve portion 18e (see FIG. 14), and is locked to the hollow rod 18Xa.
[0043] According to this, for example, the gap size of the ring-shaped gap 22 varies slightly depending on the circumferential angle position, and therefore the degree of cooling (cooling strength) by the cooling air can be changed depending on the circumferential angle position. Specifically, the distribution of the degree of cooling can be adjusted by removing the rectifying rod 19G, rotating it, and engaging a different engaging recess 19j with the single engaging protrusion 18h of the hollow rod 18Xa. In other words, the position of the notch 19h of the rectifying rod 19G can be changed so as to face the high-temperature portion of the preform 1, thereby increasing the degree of cooling (cooling strength) of the high-temperature portion.
[0044] Fig. 14 is a schematic diagram of temperature adjustment unit 20 when hollow rod 18X and rectifying rod 19F (the same applies to hollow rod Xa and rectifying rod 19G) are mounted, and detailed explanation of the same parts as in Fig. 4 will be omitted. In Fig. 14, cavity 17a (see Fig. 4) of temperature adjustment pot mold 17 is composed of a single surface with no boundaries (slits or parting lines) between steps.
[0045] 12 and 13 are not limited to polygonal shapes, and may be various shapes of engaging portions having at least portions corresponding to the vertices of a polygon and capable of selectively engaging with each other. Also, the multiple engaging recesses 19j in Figs. 15 and 16 may be multiple engaging portions having various shapes, and the single engaging protrusion 18h may be two or more engaging protrusions that selectively engage with the multiple engaging portions. Also, in some cases, the engaging protrusions and engaging recesses of the rectifying rod and hollow rod may be arranged in reverse to those of the above embodiment.
[0046] (First Experimental Example) Next, a first experimental example is shown in FIG. 17 to FIG.
[0047] FIG. 17 shows a finished container 101 such as a PET bottle that has been blow molded in the blow molding section 30 and then removed after the preform 1 has been temperature-adjusted. In this case, the body 102 of the container 101 has a regular octagonal cross section and has eight sides 102a.
[0048] FIG. 18 is a schematic diagram showing the cross section of a flow straightening rod 19B used in this experiment, which has one notch 19d in the 90 degree direction.
[0049] 19(A) and (B) show the results of measuring the thickness t of container 101 obtained by blow molding preform 1 at positions every 45 degrees clockwise on container 101 (eight positions corresponding to the above octagon) for the following cases: when no notch is provided in straightening rod 19 in temperature adjustment section 20 during molding of container 102 (curve A, actual), when the above-mentioned single notch 19d is provided (curve B, dotted line), and when aluminum tape is applied to the outer periphery other than notch 19d to further reduce the air flow path area other than notch 19d (curve C, dashed dotted line) (this corresponds to the case where the dimension of notch 19d is further increased without applying aluminum tape).In FIG. 16, it can be seen that the radial distance from the center is the thickness (mm) of the body of container 101, and that the thickness t varies within the range of 0.6 to 1.4 mm. In this case, the 90 degree direction in which the cutout portion 19d of the flow straightening rod 19 in FIG. 15 is provided coincides with the 90 degree direction in FIG.
[0050] The experimental procedure was as follows: in temperature adjustment section 20, the temperature of preform 1 was adjusted using a straightening rod 19B having one notch 19d, and then preform 1 was blow molded in blow molding section 30 to obtain container 101, and the thickness of body 102 was measured at a point 116 mm above the bottom of container 101. First, looking at the measurement results in Fig. 16(A), in the 135-degree direction, when the cutout 19d is provided (curve B) and not provided (curve A), the former results in a thicker wall of the container body 102, and when aluminum tape is applied to areas other than the cutout 19d to reduce the air flow area (curve C), the wall thickness of the body 102 is even thicker, confirming the effect of providing the cutout 19d. Note that the reason the wall thickness is thicker in the 135-degree direction, which is shifted by 45 degrees, rather than in the 90-degree direction where the cutout 19d is provided, is thought to be that the container 101 was octagonal in shape, and this tendency is evident on the sides (or tops) adjacent by 45 degrees.
[0051] Next, FIG. 16(B) shows the results of an experiment similar to that shown in FIG. 16(A), except that the thickness of the body 102 was measured at a point 84 mm above the bottom of the container 102. According to this, when comparing the cases in which cutout 19d is provided (curve B) and not provided (curve A) in the 135 degree direction of container 101, and the case in which aluminum tape is applied to areas other than cutout 19d to reduce the air flow path area (curve C), a similar trend to that in Figure 16(A) was observed, but it can be seen that when aluminum tape is applied to areas other than cutout 19d (curve C), the thickness is even greater than in the case of Figure 16(A).
[0052] The reason for this result is considered to be as follows. That is, since the cross-sectional area of the portion corresponding to the notch 19d of the first air flow passage 21a (ring-shaped gap 22) is partially larger than the other portions, the flow resistance of the air at this portion is reduced, and more air flows in than in other portions, resulting in a relatively high cooling efficiency (cooling strength). In contrast, the other portions not corresponding to the notch 19d of the first air flow passage 21a have a small flow-path cross-sectional area, so the flow resistance is high and the amount of air flowing in is reduced, resulting in a relatively low cooling efficiency. Therefore, in the temperature adjustment section 20 consisting of the air nozzle 16 equipped with the straightening rod 19 with the notch 19d and the temperature adjustment pot mold 17, the preform 1 can be efficiently quenched to suppress clouding (haze, crystallization), and the local (vertical stripe-like) high-temperature portion of the storage section 2 of the preform 1 can be selectively cooled to actively eliminate temperature deviation.
[0053] This makes it possible to adjust the thickness deviation that was originally present in the storage section 2 of the preform 1 before it reached the temperature control device 20 to a uniform thickness in the finished container 101, or in some cases, it is even possible to deliberately impart thickness deviation.
[0054] In particular, in the case of so-called multiple-cavity production, in which multiple preforms 1 (six in Figure 1) are attached to and transported on one neck mold 50 in the blow molding apparatus 100, when there is a tendency for thickness unevenness to always occur in the container 101 due to, for example, the third preform out of the six in the injection molding section 10, the thickness unevenness of the container 101 can be eliminated by using a straightening rod 19B having the above-mentioned cutout 19d in the third temperature control pod mold 17 in the next temperature adjustment section 20.
[0055] (Second Experimental Example) Next, Table 1 below shows an experimental example of how the air flow rate for cooling the preform changed when the straightening rod was not installed (1) and when it was installed (2). The set pressure of the circulating air (cooling air, compressed air) was 0.6 MPa and 0.4 MPa when the straightening rod was not installed and when it was installed, respectively, and the circulating air entered from the neck side of the preform (IN) and exited from the bottom of the preform (OUT). The straightening rod used had no notches, as shown in Figures 6 and 9.
[0056] [Table 1]
[0057] In the above cases (1) and (2), the amount of circulating air supplied was adjusted so as to cool the container 102 to a temperature at which similar good transparency could be obtained without causing whitening or clouding. As a result, the amount of circulating air supplied (consumption) was reduced from 407 liters / minute in the case of (1) to 207 liters / minute in the case of (2). This shows that by providing the straightening rod, the amount of circulating air supplied can be significantly reduced, improving the cooling efficiency of the preform 1 and reducing the load on the device. [Explanation of symbols]
[0058] 1(1A, 1B)…Preform 2...Storage section (main body) 2a…Torso 2b…Bottom 3, 103…Neck section 10...Injection molding section 11…Injection core mold 12…Injection cavity mold 16…Air nozzle 16a…Air inlet 16b…Air outlet 17…Temperature-controlled pod type 17a…Temperature-controlled pod-type cavity 18, 18X, 18Xa... Hollow rod 18a…Sleeve 18b…Fixed part 18c…Air outlet hole 18d…peripheral groove 18e…Sleeve part 18f...Polygonal engagement convex part 18g…Engagement recess for retaining ring 18h...Single engagement protrusion 19A~19G...Flow path adjustment rod (flow straightening rod) 19a…Outer circumference 19b...Screw hole 19c...Lower end 19d, 19d1, 19d2...Notch 19e…Large diameter section 19f…Small diameter part 19g…Tapered section 19h…Notch 19i...Polygonal engagement recess 19j...Multiple engagement recesses 20...Temperature adjustment section 21a...first air flow passage 21b...Second air flow passage 22...Ring-shaped gap 23...Retaining ring 24…Screw 30…Blow molding section 40…Removal section 101...Container 102...Torso 102a...Side part
Claims
1. An air introduction / exhaust member for adjusting the temperature or cooling an injection-molded bottomed preform (1) in a state where the preform (1) is held by a holding member (50), The method includes at least an air nozzle (16) that is in airtight contact with the neck portion (3) of the preform (1), and a hollow rod (18) that is arranged concentrically with the air nozzle (16) and is inserted into the preform, A first air inlet / outlet (16a) is provided at the upper portion of the air nozzle (16), A second air inlet / outlet (18c) is provided at the upper portion of the hollow rod (18), A first air flow passage (21a) is formed between the air nozzle (16) and the hollow rod (18); A second air flow passage (21b) is formed inside the hollow rod (18). Air inlet and outlet parts.
2. The diameter of the hollow rod (18) at a portion inserted into the preform (1) is larger than the diameter of a portion not inserted into the preform (1) and is smaller than the diameter of the inner peripheral surface of the preform (1). The air inlet / outlet member according to claim 1 .
3. By replacing the hollow rod (18) with a hollow rod of a different outer shape, The present invention is characterized in that the cross-sectional area of an air flow passage (22) formed between the inner peripheral surface of the preform (1) and the outer peripheral surface of the hollow rod (18) is adjusted. The air inlet / outlet member according to claim 2 .
4. A cross section perpendicular to the axial direction of the hollow rod (18) at a portion inserted into the preform (1) is a circular cross section. The air inlet / outlet member according to claim 1 .
5. A cross section perpendicular to the axial direction of the hollow rod (18) at a portion inserted into the preform (1) is a circular cross section, and has a cross-sectional shape having a notch at at least one location in the circumferential direction. The air inlet / outlet member according to claim 1 .
6. A cross section perpendicular to the axial direction of the hollow rod (18) at a portion where the hollow rod (18) is inserted into the preform (1) has an elliptical or polygonal cross-sectional shape. The air inlet / outlet member according to claim 1 .
7. The hollow rod (18) has a cross-sectional shape in which the outer diameter of a portion corresponding to the neck portion (3) of the preform (1) is larger than the outer diameter of the other portions when viewed in the axial direction. The air inlet / outlet member according to claim 1 .
8. Cooling air for adjusting or cooling the temperature of the preform (1) flows into the first air flow passage (21a) and is discharged from the second air flow passage. The air inlet / outlet member according to claim 1 .
9. A temperature-controlled pot mold (17) used together with the air inlet / outlet member according to any one of claims 1 to 8, disposed below the holding member (50), and into which the preform (1) is inserted.
10. A method for adjusting the temperature of a preform, comprising holding an injection-molded bottomed preform (1) by a holding member (50) and adjusting the temperature in a temperature adjustment section (20), Inserting the preform (1) into a cavity (17a) of a temperature controlled pot mold (17); lowering the air nozzle (16) and the hollow rod (18); abutting the air nozzle (16) against the neck portion (3) of the preform (1) and inserting the hollow rod (18) into the preform (1); and after the lowering, a first air flow passage (21a) formed between the inner circumference of the air nozzle (16) and the outer circumference of the hollow rod (18) and a second air flow passage (21b) formed inside the hollow rod (18) are communicated through the inside of the preform (1). How to regulate the temperature of the preform.
11. the step of communicating the first air flow passage (21a) and the second air flow passage (21b) through the inside of the preform (1) and then circulating cooling air through the first air flow passage (21a), The method for adjusting the temperature of a preform according to claim 10.
12. The molding machine includes at least an injection molding section (10) for injection molding a bottomed preform (1), a temperature adjustment section (20) for adjusting the temperature of the preform (1) molded in the injection molding section (10), a blow molding section (30) for blow molding the preform (1) whose temperature has been adjusted in the temperature adjustment section (20), and a holding member (50) capable of holding a neck portion (3) of the preform (1) and transporting it intermittently to the blow molding section (30), The temperature adjustment unit (20) includes at least a temperature adjustment pot mold (17), an air nozzle (16), and a hollow rod (18), The temperature-controlled pot type (17) The preform (1) is inserted so that the preform (1) can be brought into close contact with the temperature-controlled cavity (17a) of the pot mold (17); The air nozzle (16) is capable of abutting against the neck portion (3) of the preform (1), and a first air flow passage (21 a) is formed between the air nozzle (16) and the hollow rod (18); The hollow rod (18) has a second air flow passage (21b) formed therein, When the air nozzle (16) and the hollow rod (18) are lowered, the first air flow passage (21a) and the second air flow passage (21b) communicate with each other through the inside of the preform (1). Blow molding equipment.
13. After the first air flow passage (21a) and the second air flow passage (21b) communicate with each other through the inside of the preform (1), cooling air can be circulated through the first air flow passage (21a).
13. The blow molding apparatus of claim 12.
Citation Information
Patent Citations
High speed biaxial orientation blow molding method
JP1993185493A
Molding apparatus
JP1994315973A
Cooling system, cooling method and cooling pin of molded article
JP2005067206A
Temperature control apparatus for preforms, temperature control method for preforms, resin container and method for producing resin container
WO2013012067A1
Injection mold for injection stretch blow molding machine, method for molding preform, preform, method for molding container, and container
WO2017098673A1