Meltblown nonwoven fabrics and air filters

The nonwoven fabric with specific additive ratios addresses the trade-off between efficiency and pressure loss, ensuring stable processing and high performance by optimizing elongation and strength properties.

JP7567447B2Active Publication Date: 2024-10-16TOYOBO MC CORP
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2020212709
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-12-22
Publication Date
2024-10-16
Estimated Expiration
2040-12-22

AI Technical Summary

Technical Problem

Conventional melt-blown nonwoven fabrics face a trade-off between high collection efficiency and low pressure loss, with fine fibers leading to increased pressure loss and decreased surface area, while coarse fibers reduce efficiency but increase elongation, causing poor workability and dimensional instability during processing.

Method used

A melt-blown nonwoven fabric containing 0.01 to 3 parts by weight of a hindered amine additive and 0.025 to 0.25 parts by weight of a fatty acid metal salt per 100 parts of resin, achieving an elongation at break divided by basis weight of 0.5 to 4.0 and breaking strength divided by basis weight of 0.2 to 1.0, enhancing dimensional stability and processability.

Benefits of technology

The fabric exhibits excellent dimensional stability and improved workability during processing, maintaining high collection efficiency and low pressure loss, with enhanced thermal stability and reduced charge loss.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

To provide a melt-blown nonwoven fabric excellent in dimensional stability.SOLUTION: Relative to 100 pts. weight of resin to form nonwoven fabric, a melt-blown nonwoven fabric contains 0.01 pts. weight to 3 pts. weight of a hindered amine-based additive and 0.025 pts. weight to 0.25 pts. weight of a fatty acid metal salt, and has a value obtained by dividing fracture elongation [%] in a tension test by basis weight [g / m2] of 0.5 to 4.0.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a meltblown nonwoven fabric having excellent dimensional stability during processing. [Background technology]

[0002] Conventionally, air filters are used to remove pollen, dust, etc. from gas, and nonwoven fabrics are often used as the filter material of the air filters. Among them, the melt-blowing method, which is one of the manufacturing methods of the nonwoven fabrics, is widely used for manufacturing filter materials for air filter products, battery separators, etc. The melt-blowing method is generally a method in which a thermoplastic polymer extruded from a spinneret is thinned into a fibrous form by spraying hot air, and the self-fusion property of the obtained fibers is utilized to form a fiber web.

[0003] The meltblowing method has the advantage that it does not require complicated steps compared to other nonwoven fabric manufacturing methods such as the spunbonding method, and also that it is easy to obtain fine fibers with single fiber diameters of several tens of μm to several μm or less.

[0004] The performance required for an air filter is high collection efficiency that can collect a large amount of microscopic dust, and low pressure loss that has little resistance when gas passes through the inside of the air filter. In order to obtain a filter medium with high collection efficiency, it is suitable for the single fibers constituting the nonwoven fabric to be fine, but on the other hand, when the single fibers are made finer, the nonwoven fabric becomes easily crushed, and there is a problem that the pressure loss increases due to the increase in fiber density of the nonwoven fabric.

[0005] In addition, in order to obtain a filter medium with low pressure loss, it is suitable for the single fibers constituting the nonwoven fabric to have a large fineness, but on the other hand, when the single fibers are made large in fineness, the fiber surface area in the nonwoven fabric is reduced, and there is a problem that the collection efficiency is reduced. Thus, in the performance required for air filters in the conventional technology, high collection efficiency and low pressure loss are in a contradictory relationship.

[0006] As a method for solving the above problems, attempts have been made to simultaneously satisfy high collection efficiency and low pressure loss by making nonwoven fabric into an electret and utilizing electrostatic action in addition to physical action (see Patent Documents 1, 2, and 3). Furthermore, a heat-resistant electret material has been proposed by adding a hindered amine-based additive to the fibers that make up the nonwoven fabric (see Patent Document 4). [Prior art documents] [Patent documents]

[0007] [Patent Document 1] Japanese Patent Application Publication No. 61-289177 [Patent Document 2] U.S. Patent No. 6,119,691 [Patent Document 3] JP 2003-3367 A [Patent Document 4] Japanese Patent Publication No. 63-280408 Summary of the Invention [Problem to be solved by the invention]

[0008] As described above, the collection performance is improved by making the nonwoven fabric into an electret, and the thermal stability is further improved by adding a hindered amine-based additive, but it has been found that the elongation of the nonwoven fabric increases, causing the following problems: When manufacturing a nonwoven fabric as a filter medium, tension is applied to the nonwoven fabric in various steps such as molding or functionality-imparting processing, and the nonwoven fabric is wound up into a roll or laminated with a reinforcing material. If the elongation of the nonwoven fabric increases, problems occur in that the width becomes wider or the processability becomes very poor when force is applied to the nonwoven fabric as described above.

[0009] In view of the above problems, the present invention has an object to provide a melt-blown nonwoven fabric having excellent dimensional stability and good processability, and an air filter using the same. [Means for solving the problem]

[0010] As a result of intensive research conducted by the present inventors in order to solve the above problems, they have completed the present invention having the following configuration. 1. When the resin forming the nonwoven fabric is taken as 100 parts by weight, the nonwoven fabric contains 0.01 to 3 parts by weight of a hindered amine additive and 0.025 to 0.25 parts by weight of a fatty acid metal salt, and the breaking elongation [%] in a tensile test is expressed as the basis weight [g / m 2 ] is 0.5 to 4.0. 2. The breaking strength in the tensile test [N / 50mm] is calculated based on the basis weight [g / m 2 2. The melt-blown nonwoven fabric according to claim 1, wherein the value obtained by dividing the 3. The melt-blown nonwoven fabric according to 1 or 2, which is electret. 4. An air filter comprising the melt-blown nonwoven fabric according to any one of 1 to 3. Effect of the Invention

[0011] According to the above-mentioned configuration of the present invention, since the value of breaking elongation divided by basis weight in a tensile test is 0.5 to 4.0, it is possible to provide a nonwoven fabric for filters having excellent dimensional stability during processing. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] The melt-blown nonwoven fabric of the present invention contains 0.01 to 3 parts by weight of a hindered amine additive and 0.025 to 0.25 parts by weight of a fatty acid metal salt, when the resin forming the nonwoven fabric is taken as 100 parts by weight. It has been found that by containing 0.01 to 3 parts by weight of a hindered amine additive and 0.025 to 0.25 parts by weight of a fatty acid metal salt, the dimensional stability is excellent and the processability is high, as shown in the examples described later.

[0013] The content of the hindered amine additive is 0.01 to 3 parts by weight relative to 100 parts by weight of the resin constituting the nonwoven fabric, and from the viewpoints of processability, charge retention effect, and uniformity as a material, it is preferably 0.7 to 1.5 parts by weight. Specific examples of the hindered amine stabilizer include poly[{(6-(1,1,3,3-tetramethylbutyl)imino-1,3,5-triazine-2,4-diyl}{(2,2,6,6-tetramethyl-4-piperidyl)imino}hexamethylene{(2,2,6,6-tetramethyl-4-piperidyl)imino}], dimethyl succinate-1-(2-hydroxyethyl)-4-hydroxy-2,2,6,6-tetramethylpiperidine polycondensate, and bis(1,2,2,6,6-pentamethyl-4-piperidyl)-2-(3,5-di-t-butyl-4-hydroxybenzyl)-2-n-butylmalonate.

[0014] The content of the fatty acid metal salt is 0.025 to 0.25 parts by weight, and preferably 0.03 to 0.1 parts by weight, relative to 100 parts by weight of the resin constituting the nonwoven fabric. Specific examples of the fatty acid in the fatty acid metal salt include stearic acid, lauric acid, myristic acid, palmitic acid, etc., and examples of the metal element include magnesium, sodium, potassium, aluminum, zinc, etc.

[0015] The melt-blown nonwoven fabric of the present invention has a breaking elongation [%] and a basis weight [g / m 2 The value obtained by dividing the breaking elongation by the basis weight is 0.5 to 4.0, and preferably 1.0 to 3.5. If the value obtained by dividing the breaking elongation by the basis weight exceeds 4.0, the nonwoven fabric will be cut in width during winding or lamination with a reinforcing material in the manufacturing process of a filter using the nonwoven fabric as a filter medium, making it difficult to handle. If the value is below 0.5, the nonwoven fabric will not be flexible and will break during pleating, which will be a problem. If the value is in the range of 0.5 to 4.0, the cut in width during processing will be small, and improvements in processability and workability can be expected.

[0016] Here, the breaking elongation is measured by pulling a nonwoven fabric sample using a tensile tester and measuring the elongation at the time the sample breaks (breaks). The breaking elongation (tensile elongation) is calculated by the following formula. Breaking elongation [%] = 100 × (L-L0) / L0 L0: length of sample before test, L: length of sample just before break

[0017] The melt-blown nonwoven fabric of the present invention further has a breaking strength [N / 50 mm] and a basis weight [g / m 2 [0.2 to 1.0] is preferably 0.3 to 0.7. When the value obtained by dividing the breaking strength by the basis weight is in the range of 0.2 to 1.0, improvements in processability and workability can be expected.

[0018] The breaking strength herein refers to the maximum strength when a nonwoven fabric sample is pulled to break using a tensile tester.

[0019] The raw material of the melt-blown nonwoven fabric of the present invention can be a thermoplastic resin capable of melt spinning. For example, polyolefin resins such as polyvinyl chloride, polyvinylidene chloride, acrylic, polypropylene, low-density polyethylene, high-density polyethylene, linear low-density polyethylene, copolymerized polypropylene (for example, a binary or multi-component copolymer of propylene with ethylene, butene, 1,4-methylpentene-1, etc.), polyethylene terephthalate, polybutylene terephthalate, polyester resins such as these low-melting polyesters copolymerized with isophthalic acid in addition to terephthalic acid as an acid component, polyamide resins such as nylon 6 and nylon 66, polystyrene (atactic polystyrene, syndiotactic polystyrene), polyurethane elastomers, polyester elastomers, polytetrafluoroethylene, and other thermoplastic resins can be used. In addition, functional resins can be used, such as those that are biodegradable using biodegradable resins such as lactic acid-based polyesters. In addition, copolymers containing these as the main component and blends of multiple polymers of these polymers can be used.

[0020] In addition to the hindered amine additive, the melt-blown nonwoven fabric of the present invention may contain additives such as nitrogen-containing hindered phenol, metal salt hindered phenol, phenol, sulfur, and phosphorus. Furthermore, the melt-blown nonwoven fabric of the present invention may contain various additives such as matting agents, lubricants, pigments, heat stabilizers, light resistance agents, ultraviolet absorbers, electrostatic agents, conductive agents, and heat storage materials within an appropriate range, as necessary. In addition, additives having various functions such as dust removal, deodorization, antibacterial, antifungal, antiviral, insect repellent, insecticide, pest repellent, harmful substance removal, fragrance, dehumidification, humidity control, moisture absorption (drying), moisture (humidity) permeation, adsorption of oil, etc., ion balance adjustment such as cation adsorption, and evaporation or sustained release of water and volatile drugs, etc. may be added.

[0021] The fiber form of the melt-blown nonwoven fabric may be a single-phase form consisting of a single polymer, or a composite form consisting of a plurality of types of the polymer (core-sheath type composite form, parallel type composite form, split fiber type composite form).

[0022] The cross-sectional shape of the fibers is not limited to a circular shape, but may be an ellipse, a diamond, a triangle, a T-shape, or the like, or may have a hollow portion, and any shape may be appropriately selected.

[0023] The melt-blown nonwoven fabric of the present invention is preferably electretized by known techniques such as corona discharge method or water flow charging method, because it can obtain a filter medium or air filter with higher performance.When the electret nonwoven fabric that does not contain hindered amine additive comes into contact with water, it usually loses its charge.It has been found that the electret nonwoven fabric that contains hindered amine additive is difficult to lose charge even when it comes into contact with water.

[0024] The basis weight of the meltblown nonwoven fabric of the present invention is 5 to 100 g / m 2 is preferable, and more preferably 10 to 60 g / m 2The fiber diameter is 0.001 to 100 μm, preferably 0.005 to 20 μm, more preferably 0.01 to 10 μm, further preferably 0.02 to 5 μm, and particularly preferably 0.03 to 3 μm. If the fiber diameter exceeds 100 μm, it is difficult to obtain a practical collection efficiency as an air filter, and the efficiency is greatly reduced when the charge decays. If the fiber diameter is smaller than 0.001 μm, it is difficult to impart an electrostatic charge as an electret material.

[0025] The fibers of the meltblown nonwoven fabric of the present invention may be homogeneous and made of a single manufacturing method and material, or may be a mixture of two or more types of fibers differing in manufacturing method, material and fiber diameter.

[0026] The air filter of the present invention uses the melt-blown nonwoven fabric of the present invention, and may be subjected to, for example, shaping or attachment to a frame, etc. The air filter of the present invention may also be formed by combining the melt-blown nonwoven fabric of the present invention with other materials.

[0027] When the melt-blown nonwoven fabric of the present invention is used as a filter material to manufacture an air filter, it may be processed into a wavy shape. Examples of methods for processing into a wavy shape include repeated folding into peaks and valleys, which is generally called pleating, and wavy processing of the core in cardboard processing. By processing into a wavy shape in this way, the filtration area can be increased for a certain ventilation area, and the pressure loss is reduced as the speed of air passing through the air filter for a specific air volume decreases, improving breathability. In addition, the collection efficiency is improved and the life is extended, and the strength of the air filter itself is increased compared to when it is used as a single plate, which has the advantage of improving the handling when it is attached to an air conditioner or when it is replaced.

[0028] As described above, the present invention provides a melt-blown nonwoven fabric and an air filter which exhibit little loss of charge when heated, i.e., excellent thermal stability, and which also exhibits excellent dimensional stability during processing. EXAMPLES

[0029] The present invention will be described in detail below with reference to examples. However, the present invention is not limited to the following examples, and can be modified as appropriate within the scope of the above and below-mentioned aims. Such modified examples are also included in the technical scope of the present invention.

[0030] First, the property values ​​measured in the examples and comparative examples and the methods for measuring them are shown below.

[0031] (Melt flow index [g / 10min]) Measurement was performed according to JIS K6921-2:2018, Table 3, 1.1 Melt mass-flow rate (MFR).

[0032] (Average fiber diameter (μm)) Ten small samples were randomly taken from the melt-blown nonwoven fabric, and photographs were taken at 500 to 3000 times magnification using a scanning electron microscope. The fiber diameters of 10 fibers from each sample, a total of 100 fibers, were measured, and the average value was rounded off to the first decimal place to calculate the average value.

[0033] (G / m 2 )) In accordance with JIS L1906 (2000 edition) 5.2, three samples of melt-blown nonwoven fabric measuring 50 cm lengthwise and 50 cm widthwise were taken, and the weight of each sample was measured. The average value obtained was converted to a value per unit area and rounded off to the first decimal place.

[0034] (processability) Activated carbon particles (particle size) on top of a general reinforcement material 200 ~ 400 μm) and then melt The blown nonwoven fabric was laminated and bonded to produce an activated carbon sheet. This sheet was then reciprocatingly pleated. The pleats are processed with a processing machine so that the pleats are 3.0 cm high, and the following criteria are met: Evaluated. ◯: The pleats are uniform and there are no problems with processing. △: The pleats are slightly uneven. ×: There is a problem with processing, such as uneven pleats or tears in the nonwoven fabric.

[0035] (Breaking strength, breaking elongation) According to 5.3.1 of JIS L1906 (2000 edition), tensile tests were carried out on three samples in both the longitudinal and transverse directions under the conditions of a sample size of 5cm x 20cm, grip interval of 15cm, and tensile speed of 20cm / min. The maximum strength when the sample was pulled until it broke was taken as the breaking strength [N / 50mm], the elongation at break was taken as the breaking elongation [%], and each was calculated based on the basis weight of the sheet [g / m 2 ] was divided by this to calculate the figure.

[0036] [Example 1] A meltblown nonwoven fabric (basis weight 20 g / m2) containing 1.0 part by weight of a hindered amine additive, Chimassorb 944 (manufactured by BASF), and 0.05 part by weight of magnesium stearate, for 100 parts by weight of polypropylene resin with a melt flow index of 1300. 2 The nonwoven fabric had a breaking strength per unit area of ​​0.7 and a breaking elongation per unit area of ​​2.0. The processability was rated as good. [Example 2] A meltblown nonwoven fabric (basis weight 45 g / m) containing 1.0 part by weight of a hindered amine additive, Chimassorb 944 (manufactured by BASF), and 0.05 part by weight of magnesium stearate, was prepared. 2 The nonwoven fabric had a breaking strength per unit area of ​​0.3 and a breaking elongation per unit area of ​​3.5. The processability was rated as good. [Comparative Example 1] A melt-blown nonwoven fabric (basis weight 20 g / m) containing 1.0 part by weight of a hindered amine additive, Chimassorb 944 (manufactured by BASF), for 100 parts by weight of polypropylene resin with a melt flow index of 1300. 2The nonwoven fabric had a breaking strength per unit area of ​​0.3 and a breaking elongation per unit area of ​​0.3. The processability was rated x. [Comparative Example 2] A meltblown nonwoven fabric (basis weight 20 g / m) containing 1.0 part by weight of a hindered amine additive, Chimassorb 944 (manufactured by BASF), and 0.01 part by weight of magnesium stearate, was prepared. 2 The nonwoven fabric had a breaking strength per unit area of ​​0.5 and a breaking elongation per unit area of ​​0.2. The processability was rated x.

[0037] It can be seen that the melt-blown nonwoven fabrics of Examples 1 and 2 are superior in processability to those of Comparative Examples 1 and 2. [Industrial Applicability]

[0038] The melt-blown nonwoven fabric of the present invention has heat resistance and excellent dimensional stability during processing, and can be suitably used as a filter material for air filters.

Claims

1. When the resin forming the nonwoven fabric is taken as 100 parts by weight, the nonwoven fabric contains 0.01 to 3 parts by weight of a hindered amine additive and 0.025 to 0.25 parts by weight of a fatty acid metal salt, and the breaking elongation [%] in a tensile test is expressed as the basis weight [g / m 2 ] is 0.5 to 4.

0.

2. The breaking strength [N / 50 mm] in the tensile test was calculated based on the basis weight [g / m 2 2. The melt-blown nonwoven fabric according to claim 1, wherein the value obtained by dividing the

3. The meltblown nonwoven fabric according to claim 1 or 2, which is electretized.

4. An air filter comprising the melt-blown nonwoven fabric according to any one of claims 1 to 3.

Citation Information

Patent Citations

  • Production of electret fibrous sheet

    JP1986289177A

  • Heat resistant electret material

    JP1988280408A

  • Electret fiber sheet

    JP2003003367A

  • Method for producing electret and electrification device

    JP2005029944A

  • Nonwoven webs and fibers having electret properties, methods for producing the same, and uses thereof