Gas container manufacturing method
The use of a honeycomb-shaped housing member with thermally conductive partition walls and dual adhesive layers addresses temperature unevenness and stabilizes storage material pellets, enhancing gas storage and release performance in gas containers.
Patent Information
- Application Number
- JP2022044382
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-03-18
- Publication Date
- 2024-10-16
- Estimated Expiration
- 2042-03-18
AI Technical Summary
Conventional gas containers face issues with temperature unevenness in the internal space, leading to reduced mechanical strength and inadequate storage and release performance of gases due to deformation and difficulty in uniformly accommodating and fixing storage material pellets.
A honeycomb-shaped housing member with partition walls made of thermally conductive material is used, along with two adhesive layers of different viscosities to stabilize and uniformly distribute storage material pellets, ensuring proper adhesion and integration within the gas container.
The solution enhances the storage and release performance of gases by stabilizing the storage material within the gas container, allowing for a sufficient amount to be accommodated and held, thereby improving the overall gas handling capabilities.
Smart Images

Figure 0007567840000001 
Figure 0007567840000002 
Figure 0007567840000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a gas container for storing and releasing a gas, such as hydrogen gas. [Background technology]
[0002] In recent years, technologies have been proposed for using hydrogen gas, natural gas, and the like as fuel for vehicles and various devices. Gas containers for storing and releasing these gases have also been actively studied (for example, Patent Document 1).
[0003] The gas container introduced in Patent Document 1 contains a hydrogen storage alloy, which is a type of storage material, in its internal space. The storage material physically or chemically absorbs and releases the gas to be stored (hereinafter, referred to as the filled gas, as necessary). These storage materials can increase the amount of gas that can be stored in the internal space.
[0004] On the other hand, the storage material undergoes a temperature change when absorbing and releasing the fill gas.
[0005] For example, if the storage material is a hydrogen storage alloy, a change in temperature will cause a change in the volume of the storage material, as described in Patent Document 1. In such a case, if the amount and speed of temperature change of the storage material, i.e., the amount and speed of volume change of the storage material, become excessive, there is a risk that the mechanical strength of the gas container will decrease, such as deformation.
[0006] Furthermore, since the absorption and release of the fill gas by a general storage material is accompanied by a temperature change, the absorption and release of the fill gas by the storage material occurs when the temperature of the storage material changes. Therefore, in order to smoothly absorb and release the fill gas into and from the storage material, it is considered essential to make the temperature of the storage material uniform throughout the entire internal space.
[0007] In the internal space of the gas container disclosed in Patent Document 1, a heat transfer pipe, which is a passage for a heat exchange medium, and fin portions extending from the heat transfer pipe are arranged. According to this gas container, the temperature of the gas storage material in the internal space is controlled by circulating a heat exchange medium through the heat medium pipe. [Prior art documents] [Patent documents]
[0008] [Patent Document 1] Japanese Patent Application Publication No. 6-281097 Summary of the Invention [Problem to be solved by the invention]
[0009] As described above, in the gas container introduced in the above-mentioned Patent Document 1, the temperature of the gas storage material in the internal space is controlled by circulating a heat exchange medium through a heat medium pipe. However, even this type of gas container cannot be said to be excellent in terms of the storage and release performance of the filled gas.
[0010] In order to improve the storage and release performance of the filled gas in the gas container, the inventors of the present invention have investigated the reason why sufficient storage and release performance of the filled gas cannot be obtained in the conventional gas container as introduced in Patent Document 1. As a result of intensive research, the inventors have come up with the idea that in the conventional gas container, temperature unevenness still occurs in the internal space, and this causes the amount and speed of occlusion and release of the filled gas to reach a plateau in the storage material in the conventional gas container.
[0011] The inventors of the present invention have further conducted extensive research and have arrived at the idea of arranging a honeycomb-shaped storage member in the internal space in order to eliminate or reduce the temperature unevenness in the internal space. The storage member has a number of sub-spaces defined by partition walls made of a thermally conductive material, and the storage material is stored and held in the sub-spaces.
[0012] The partition walls of the storage member are made of a thermally conductive material and function as a heat exchanger. The storage member is thermally homogenized by the partition walls, and the storage material contained and held in the sub-spaces defined by the partition walls is also thermally homogenized. It is believed that a gas container having a honeycomb-shaped storage member can thereby achieve improved performance in storing and releasing the filled gas.
[0013] However, the process for manufacturing this type of gas container is very complicated, and it is also difficult to store and hold a sufficient amount of storage material in each of the sub-spaces of the container member in this type of gas container.
[0014] That is, the honeycomb-shaped storage member has many sub-spaces, each of which has a relatively small diameter, and therefore, for example, when a powder of primary particles or secondary particles formed by agglomeration of the primary particles is used as the storage material, it is necessary to directly fill each of the many relatively small sub-spaces with the powder of the storage material. However, the process of filling the sub-spaces with powdered storage material is very complicated, and filling the sub-spaces with a sufficient amount of powdered storage material is itself very difficult. Furthermore, this manufacturing method is prone to problems such as uneven filling of the amount of storage material in each sub-space. Furthermore, powdered storage material is difficult to handle.
[0015] For this reason, the inventor of the present application aimed to prepare storage material pellets in advance by solidifying the storage material powder into the same shape as the sub-spaces, instead of the above-mentioned storage material powder, and insert the storage material pellets into each sub-space. In this case, the handling of the storage material is improved, so it is believed that the manufacturing process of the gas container can be simplified compared to the case where the storage material powder is directly filled, and the amount of storage material filled in each sub-space can be increased and the variation in the amount filled can be reduced.
[0016] However, when actually manufacturing this type of gas container, the storage material pellets rub against the partition wall when they are inserted into the sub-space, causing the surface of the storage material pellets to be scraped off, resulting in a problem that the total amount of storage material contained and held in the internal space of the gas container falls short of the planned amount.
[0017] Furthermore, when this type of gas container is used as a fuel container for an automobile, if the storage material pellets are not stably fixed to the partition wall that defines the sub-space, the storage material pellets and the partition wall will rub against each other due to vibrations during driving, causing the surface of the storage material pellets to be scraped off. In this case, if the storage material falls off the storage material pellets and leaks out of the gas container, the total amount of storage material contained and held in the internal space of the gas container will not reach the planned amount.
[0018] For this reason, simply using storage material pellets makes it difficult to store and retain a sufficient amount of storage material in the internal space of the gas container, and in this case too, it is difficult to improve the storage and release performance of the filled gas in the gas container.
[0019] The present invention has been made in consideration of the above circumstances, and has an object to provide a technique capable of improving the storage and release performance of a filled gas in a gas container. [Means for solving the problem]
[0020] A first aspect of the method for producing a gas container according to the present invention that solves the above problems is as follows: A container body having an internal space; a cap connecting the outside of the container body with the internal space; a honeycomb-shaped container member disposed in the internal space and including a plurality of sub-spaces partitioned by partition walls made of a thermally conductive material; a storage material that is accommodated and held in the sub-space and that absorbs and releases a fill gas, comprising: a step of inserting and fixing a storage material pellet, which is formed by solidifying the powder of the storage material and has the same shape as the sub-space, into the sub-space of the containing member; The assembling step includes: an adhesive layer forming step of forming a first adhesive layer on one of the outer peripheral surface of the storage material pellet and the sub-space side surface of the partition wall, and forming a second adhesive layer having a lower viscosity than the first adhesive layer on the other; and an inserting step of inserting the storage material pellet into the sub-space after the adhesive layer forming step.
[0021] A second aspect of the method for producing a gas container according to the present invention, which solves the above problems, is as follows: A container body having an internal space; a cap connecting the outside of the container body with the internal space; a honeycomb-shaped container member disposed in the internal space and including a plurality of sub-spaces partitioned by partition walls made of a thermally conductive material; a storage material that is accommodated and held in the sub-space and that absorbs and releases a fill gas, comprising: a step of inserting and fixing a storage material pellet, which is formed by solidifying the storage material powder and has the same shape as the sub-space, into the sub-space of the storage member; The assembling step includes: an adhesive layer forming step of forming a first adhesive layer on one of an outer peripheral surface of the storage material pellet and a side surface of the sub-space of the partition wall, and a second adhesive layer having a lower viscosity than the first adhesive layer and positioned further forward in the insertion direction than the first adhesive layer; and an inserting step of inserting the storage material pellet into the sub-space after the adhesive layer forming step. Effect of the Invention
[0022] According to the present invention, it is possible to improve the performance of storing and releasing the filled gas in a gas container. [Brief description of the drawings]
[0023] [Figure 1] FIG. 2 is an explanatory diagram for explaining a schematic diagram of the gas container according to the first embodiment. [Diagram 2]1 is an explanatory diagram illustrating a schematic axial cross section of a gas container according to a first embodiment. [Diagram 3] FIG. 2 is an explanatory diagram for explaining a schematic exploded view of a main part of the gas container according to the first embodiment. [Figure 4] FIG. 2 is an explanatory diagram for explaining a typical example of a container member in the gas container according to the first embodiment. [Diagram 5] FIG. 2 is an explanatory view illustrating a schematic diagram of an adhesive layer forming step in the manufacturing method of Example 1. [Figure 6] 4 is an explanatory diagram illustrating a schematic diagram of an insertion step in the manufacturing method according to the first embodiment. FIG. [Figure 7] 4 is an explanatory diagram illustrating a schematic diagram of an insertion step in the manufacturing method according to the first embodiment. FIG. [Figure 8] 4 is an explanatory diagram illustrating a schematic diagram of an insertion step in the manufacturing method according to the first embodiment. FIG. [Figure 9] 11 is an explanatory view showing a schematic diagram of an adhesive layer forming step in the manufacturing method of Example 2. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0024] The method for manufacturing a gas container according to the present invention is a method for manufacturing a gas container having the above-mentioned honeycomb-shaped container member, and includes an assembly step of inserting and fixing storage material pellets in the sub-space of the container member.
[0025] In the manufacturing method of the gas container according to the first aspect of the present invention, the assembling step includes two steps: an adhesive layer forming step (1-1) below, and an insertion step (1-2) below. (1-1) an adhesive layer forming step of forming a first adhesive layer on one of the outer peripheral surface of the storage material pellet and the side surface of the sub-space in the partition wall, and forming a second adhesive layer having a lower viscosity than the first adhesive layer on the other; (1-2) An inserting step of inserting a storage material pellet into the sub-space after the above-mentioned (1-1) adhesive layer forming step.
[0026] In the method for producing a gas container according to the second aspect of the present invention, the assembly step includes two steps: an adhesive layer forming step (2-1) below, and an insertion step (2-2) below. (2-1) an adhesive layer forming step of forming a first adhesive layer on one of the outer peripheral surface of the storage material pellet and the side surface of the sub-space in the partition wall, and a second adhesive layer having a lower viscosity than the first adhesive and located further forward in the insertion direction than the first adhesive layer; (2-2) An inserting step of inserting a storage material pellet into the sub-space after the above-mentioned (2-1) adhesive layer forming step.
[0027] Hereinafter, as necessary, the manufacturing method of the gas container according to the first aspect of the present invention may be referred to as the first manufacturing method, and the manufacturing method of the gas container according to the second aspect of the present invention may be referred to as the second manufacturing method. Also, the outer peripheral surface of the storage material pellet may be referred to as the pellet outer peripheral surface, and the sub-space side surface of the partition wall may be referred to as the partition inner peripheral surface.
[0028] As described above, the first production method of the present invention has (1-1) the adhesive layer forming step, and the second production method of the present invention has (2-1) the adhesive layer forming step.
[0029] In both the (1-1) adhesive layer forming step and the (2-1) adhesive layer forming step, a first adhesive layer and a second adhesive layer are formed. The first adhesive layer and the second adhesive layer are adhesive layers that function to bond the outer peripheral surface of the pellet to the inner peripheral surface of the compartment, so that in the gas container obtained through the assembly process, the containing member and the storage material are bonded and integrated.
[0030] In order to bond the storage material to the storage member and stably hold it in the storage member, it is considered best not to make the gap between the outer circumferential surface of the pellet and the inner circumferential surface of the compartment too large. In this case, it is necessary to fill the narrow gap with adhesive.
[0031] However, because the adhesive has a relatively high viscosity, it has a relatively large frictional resistance with the outer peripheral surface of the pellet and / or the inner peripheral surface of the compartment, making it difficult to spread the adhesive evenly. For this reason, it is not easy to spread the adhesive evenly in the narrow gap between the outer peripheral surface of the pellet and the inner peripheral surface of the compartment.
[0032] If the adhesive does not reach the gap between the outer peripheral surface of the pellet and the inner peripheral surface of the compartment, air may be trapped inside the cured adhesive layer (referred to as the cured adhesive layer). In this case, the adhesive area between the cured adhesive layer and the mating material (i.e., the outer peripheral surface of the pellet and / or the inner peripheral surface of the compartment) may decrease, or the strength of the cured adhesive layer itself may decrease.
[0033] Therefore, there is a problem that it is difficult to stably bond the storage material to the containing member by simply bonding the outer peripheral surface of the pellet and the inner peripheral surface of the compartment by a normal method.
[0034] In the first and second manufacturing methods of the present invention, two types of adhesive layers with different viscosities, i.e., a first adhesive layer and a second adhesive layer with a lower viscosity than the first adhesive layer, are used as the adhesive layer for adhering the storage material to the housing member. As a result, according to the first and second manufacturing methods, it is possible to stably bond and integrate the storage material with the storage member.
[0035] Specifically, in the first manufacturing method, in (1-1) an adhesive layer forming step, a first adhesive layer is formed on one of the outer peripheral surface of the pellet and the inner peripheral surface of the compartment, and a second adhesive layer is formed on the other, and then in (1-2) an insertion step, a storage material pellet is inserted into the sub-space.
[0036] As a result, the first adhesive layer (or the second adhesive layer) formed on the outer peripheral surface of the pellet and the second adhesive layer (or the first adhesive layer) formed on the inner peripheral surface of the compartment are pressed against each other, and the low-viscosity second adhesive layer deforms relative to the high-viscosity first adhesive layer at the interface between the first adhesive layer and the second adhesive layer.
[0037] Therefore, the second adhesive layer functions as a filler between the outer peripheral surface of the pellet and the inner peripheral surface of the compartment, and the first adhesive layer functions as a pressing material for spreading the second adhesive layer. Furthermore, the second adhesive layer also functions as a lubricant for the first adhesive layer, and the first adhesive layer also functions as a filler.
[0038] In this way, in the first manufacturing method of the present invention, the first adhesive layer and the second adhesive layer can be filled without any gaps between the outer peripheral surface of the pellet and the inner peripheral surface of the compartment. As a result, the storage material can be stably bonded and integrated with the containing member, and a sufficient amount of storage material can be stored and held in the internal space of the gas container, improving the storage and release performance of the filled gas in the gas container.
[0039] On the other hand, in the second manufacturing method of the present invention, in the (2-1) adhesive layer forming step, a first adhesive layer and a second adhesive layer are formed on one of the outer peripheral surface of the pellet and the inner peripheral surface of the compartment, and the second adhesive layer is formed further forward in the insertion direction than the first adhesive layer, and then in the (2-2) insertion step, the storage material pellet is inserted into the sub-space.
[0040] In the second manufacturing method, both the first adhesive layer and the second adhesive layer are formed on the same side of the outer peripheral surface of the pellet and the inner peripheral surface of the compartment, but the second adhesive layer having a lower viscosity is formed further forward in the insertion direction than the first adhesive layer having a higher viscosity. The forward side in the insertion direction may be rephrased as the forward side in the direction in which the storage material pellet advances in the insertion process.
[0041] As described above, by forming the low-viscosity second adhesive layer further forward in the insertion direction than the high-viscosity first adhesive layer, when the storage material pellet is inserted, the first adhesive at the rear of the insertion direction presses the second adhesive at the front of the insertion direction in the insertion direction. Therefore, in the second manufacturing method, similarly to the first manufacturing method, the second adhesive layer functions as a filler filled between the outer peripheral surface of the pellet and the inner peripheral surface of the compartment, and the first adhesive layer functions as a pressing material for spreading the second adhesive layer. In addition, the second adhesive layer also functions as a lubricant for the first adhesive layer, and the first adhesive layer also functions as a filler.
[0042] As a result, the second manufacturing method of the present invention also makes it possible to fill the space between the outer peripheral surface of the pellet and the inner peripheral surface of the compartment with the first adhesive layer and the second adhesive layer without any gaps, thereby making it possible to stably adhere and integrate the storage material to the storage member. Therefore, like the first manufacturing method, the second manufacturing method of the present invention makes it possible to store and retain a sufficient amount of storage material in the internal space of the gas container, thereby improving the storage and release performance of the filled gas in the gas container.
[0043] Hereinafter, the first and second manufacturing methods of the present invention will be described for each step and component. In addition, matters common to the first and second manufacturing methods may be simply described as the manufacturing method of the present invention. Furthermore, the gas container manufactured by the manufacturing method of the present invention may be referred to as the gas container of the present invention.
[0044] Unless otherwise specified, the numerical range "x to y" described in this specification includes the lower limit x and the upper limit y. These upper and lower limit values, as well as the numerical values listed in the examples, can be arbitrarily combined to form a new numerical range. Furthermore, any numerical value selected from any of the above numerical ranges can be used as the upper and lower limit numerical values of the new numerical range.
[0045] The manufacturing method of the present invention is a method for manufacturing a gas container having a container body, a mouthpiece, a housing member and a storage material. First, the gas container of the present invention manufactured by the manufacturing method of the present invention will be described below.
[0046] [Gas bottle] There are no particular limitations on the type of fill gas contained in the gas container of the present invention, and no particular limitations on the pressure of the fill gas within the gas container, but the gas container of the present invention is particularly suitable for realizing a so-called pressure-resistant container in which a fuel gas such as hydrogen gas or natural gas is filled at high pressure.
[0047] Among the components of the gas container of the present invention, the container body has an internal space for containing the target filled gas. As a material for such a container body, it is preferable to select a material having so-called gas barrier properties that makes it difficult for the filled gas to permeate.
[0048] Specifically, the material of the container body may be appropriately selected depending on the type of filled gas, the environment in which the gas container is installed, and the like.
[0049] For example, if the filled gas is hydrogen gas, it is preferable to use polyethylene resin, polypropylene resin, etc. as the material for the container body. It is also preferable to coat the inside of the container body with a material with excellent gas barrier properties, such as ethylene-vinyl alcohol copolymer (EVOH). In cases where the gas container of the present invention is intended to be installed in a house or the like and the mass of the gas container can be somewhat large, a metal material such as aluminum or stainless steel may be selected as the material for the container body.
[0050] The shape of the container body is not particularly limited, but it is preferable that the container body has a shape such as a cylindrical shape or a regular polygonal tubular shape in which the internal pressure caused by the filled gas is uniformly dispersed.
[0051] The container body may be integrally formed with the nozzle, or may be formed separately from the nozzle. For example, the container body may be insert-molded using a preformed nozzle as an insert, or the nozzle may be inserted into a preformed container body to integrate the two. In order to prevent leakage of the filled gas to the outside of the container body, it is preferable to interpose a seal member such as an O-ring between the mouthpiece and the container body.
[0052] The material of the base is not particularly limited, but since the base is required to have a certain degree of rigidity, it is preferable to select a metal material such as aluminum, an aluminum alloy, or stainless steel as the material for the base.
[0053] The cap connects the outside of the container body with an internal space provided in the container body, and functions as an inlet / outlet for the fill gas.
[0054] At least one nozzle is required for one container body, but a plurality of nozzles may be provided for one container body. For example, when the container body is cylindrical, the nozzles may be integrated with both axial ends of the container body. In this case, both of the two nozzles may be used as an inlet / outlet for the filler gas, or one of the nozzles may be plugged.Also, as in the embodiment described later, one of the nozzles may be used as an inlet / outlet for the filler gas, and the other may be used as a heat exchanger through which a heat exchange medium flows. Of course, the gas container of the present invention may have a heat exchanger separate from the base.
[0055] When the gas container of the present invention is used as a pressure-resistant container, it is preferable that the outside of the container body is covered with a reinforcing layer.
[0056] The reinforcing layer may be made of high-strength fibers impregnated with resin (so-called FRP), similar to general pressure-resistant containers. Examples of the high-strength fibers include carbon fibers, glass fibers, and aramid fibers, and examples of the resin impregnated in the high-strength fibers include thermosetting resins such as epoxy resins, unsaturated polyester resins, and vinyl ester resins.
[0057] The reinforcing layer may be formed by a general method, for example, by winding high-strength fibers impregnated with a resin material around the container body to form a helical layer or a hoop layer, and then heating and curing the resin material. Alternatively, the helical layer or the hoop layer made of resin and high-strength fibers may be formed into a sheet shape, which is attached to the container body, and then the resin material may be heated and cured.
[0058] The containing member is disposed in the internal space of the container body.
[0059] The storage member has a honeycomb shape in which a plurality of sub-spaces are arranged, each of which is partitioned by a partition wall. The shape of each sub-space is not particularly limited, but for the convenience of storing and holding the storage material in the sub-space, it is preferable that the sub-space has a columnar shape extending in the extension direction of the nozzle, i.e., the flow direction of the filled gas.
[0060] Each sub-space may have the same shape or different shapes, but taking into consideration the rigidity of the partition walls that define the sub-spaces, it is preferable that the flow path cross-section of each sub-space be a regular polygonal shape such as a regular hexagon or a regular octagon. The flow passage cross section of each sub-space may or may not be constant over the entire axial length of the sub-space, but taking into account pressure loss of the fill gas, it is preferably constant over at least 50% of the axial length of the sub-space, more preferably constant over at least 75% of the axial length, and especially preferred over the entire axial length of the sub-space.
[0061] The partition walls that partition the subspaces may have any shape that corresponds to the shape of the subspaces. As described above, the partition wall is made of a heat-conductive material and functions as a heat exchanger. In this specification, the heat-conductive material means a material having a higher thermal conductivity than air at room temperature of 25° C., and specific examples of the material include various metals, alloys, ceramics, etc., such as stainless steel, aluminum, alumina, and silicon carbide.
[0062] The partition wall may be manufactured by integrating plate-shaped materials by welding or bonding, or may be manufactured by extruding and firing a ceramic raw material slurry.
[0063] In the gas container of the present invention, at least one of the partition walls preferably has a communication port that communicates two adjacent sub-spaces, whereby the two adjacent sub-spaces communicate with each other through the communication port and the fill gas can flow between the two sub-spaces through the communication port.
[0064] In the gas container of the present invention, all of the partition walls may have connecting ports, or only some of the partition walls may have connecting ports, but in order to homogenize the concentration of the filled gas throughout the entire internal space, it is preferable that most of the partition walls have connecting ports. The size of the communication opening is not particularly limited, and the communication opening may be covered with a ventilation material such as mesh.
[0065] The sub-spaces accommodate and hold a storage material. In the gas container of the present invention, the storage material may be accommodated and held in all of the sub-spaces, or the storage material may be accommodated and held only in some of the sub-spaces, with no storage material being accommodated and held in the remaining parts. In this specification, the sub-space that accommodates and holds the storage material will be referred to as a storage section, and the sub-space that does not accommodate and hold the storage material will be referred to as a hollow section, as necessary.
[0066] In order to make the concentration of the filled gas uniform throughout the entire internal space, it is preferable that the gas container of the present invention has a sub-space, i.e., a hollow portion, in which no storage material is contained and which functions as a flow path for the filled gas.
[0067] There are no particular limitations on the ratio of the hollow portion to the storage portion, the ratio of the cross-sectional areas of the flow paths, etc., but there is an optimal range for these ratios in order to store and release a sufficient amount of the fill gas and to ensure a sufficient flow path for the fill gas.
[0068] Specifically, when the average cross-sectional area of the flow passage of the storage portion is taken as 100%, the average cross-sectional area of the flow passage of the cavity portion is preferably within a range of 10 to 500%, a range of 20 to 200%, or a range of 50 to 150%.
[0069] The ratio (number ratio) of the cavities to the storage portions is preferably within a range of 1:50 to 1:1, 1:15 to 1:2, or 1:7 to 1:3.
[0070] In addition, when the sum of the flow path cross-sectional areas of the storage portions is taken as 100%, the sum of the flow path cross-sectional areas of the hollow portions is preferably within a range of 2 to 50%, 7 to 30%, or 15 to 23%.
[0071] The storage material is contained and held in the sub-space and stores and releases the fill gas. Such a storage material may be appropriately selected according to the type of fill gas to be stored in the gas container of the present invention.
[0072] For example, when the filling gas is hydrogen, examples of the storage material include porous carbon materials such as carbon nanotubes, porous metal complexes (so-called MOFs), zeolites, hydrogen storage alloys, metal hydrides, and the like.
[0073] In the gas container of the present invention, each storage material is contained and held in the sub-space in the form of a storage material pellet obtained by solidifying powder of the storage material.
[0074] More specifically, the storage material pellets are formed into pellets by crosslinking powder of the storage material with a crosslinking agent or binding with a binder. The storage material powder is a general term for the primary particles and secondary particles of the storage material.
[0075] The shape of the storage material pellet is the same as the shape of the sub-space that contains and holds the storage material pellet. In this specification, the term "same shape" includes "approximately the same shape." Specifically, the volume of the storage material pellet is allowed to be within a range of 90% to 100% of the volume of the sub-space. It is more preferable that the volume of the storage material pellet is 95% or more of the volume of the sub-space. The production method of the present invention will now be described.
[0076] [Manufacturing method] The manufacturing method of the present invention is a method for manufacturing the above-mentioned gas container of the present invention, and includes an assembly step of inserting and fixing the above-mentioned storage material pellets into the sub-space of the containing member. As described above, the assembly step differs between the first manufacturing method and the second manufacturing method, but they are similar in that the first adhesive layer and the second adhesive layer are formed. In this specification, the first adhesive layer and the second adhesive layer will first be described.
[0077] The first adhesive layer and the second adhesive layer are two types of adhesive layers with different viscosities. Therefore, the type of adhesive constituting the first adhesive layer (referred to as the first adhesive), the type of adhesive constituting the second adhesive layer (referred to as the second adhesive), and the combination of the first adhesive and the second adhesive are not particularly limited, as long as the first adhesive layer has a higher viscosity than the second adhesive layer.
[0078] In other words, the first adhesive and the second adhesive may be appropriately selected depending on the required adhesive strength and the environment in which the gas container is used. The adhesive in the present invention refers to a composition that can change from a fluid state to a solid state and can adhere to at least the outer peripheral surface of the pellet and the inner peripheral surface of the compartment when changing from a fluid state to a solid state.
[0079] For example, the first adhesive and the second adhesive may be in a fluid state during the insertion process, i.e., when the storage material pellet is inserted into the sub-space. After the insertion process, the first adhesive and the second adhesive may change from a fluid state to a solid state by hardening through a chemical reaction or evaporation of a solvent, etc., and may be fixed to the outer peripheral surface of the pellet and the inner peripheral surface of the compartment. The term "fluid state" as used here refers to a state that is capable of flowing, and is a concept that includes liquid, gel, sol, slurry, etc.
[0080] Specific examples of the first adhesive and the second adhesive include a reactive adhesive, a solvent adhesive, an emulsion adhesive, a hot melt adhesive, and a synthetic rubber adhesive.
[0081] The viscosity of the first adhesive and the second adhesive can be adjusted by various methods. For example, the viscosity can be adjusted by appropriately setting the molecular weight of the resin components such as oligomers and polymers contained in the first adhesive and the second adhesive. In general, it is considered that a resin component with a low molecular weight has a lower viscosity than a resin component with a high molecular weight.
[0082] Alternatively, the viscosity of the adhesive can be adjusted by blending various fillers into the first adhesive or the second adhesive. Furthermore, it is possible to adjust the viscosity of the first adhesive and the second adhesive by appropriately setting the type and amount of the filler. Although it depends on the type and particle size of the filler, when a small-diameter filler is used, it is generally said that the viscosity of the adhesive increases as the amount of the filler is increased.
[0083] If the first adhesive or the second adhesive is a solvent-based adhesive or an emulsion-based adhesive, the viscosity of the adhesive can be adjusted by appropriately adjusting the mixing ratio of the solvent or dispersion medium (i.e., the solids concentration of the adhesive). The higher the solids concentration, the higher the viscosity of the adhesive. Furthermore, the viscosity of the first adhesive or the second adhesive can be adjusted by appropriately changing the mixing ratio of the base agent and the hardener or the type of the base agent and / or the hardener. In such cases, the composition of the first adhesive layer and the second adhesive layer will be substantially the same. The manufacturing method of the present invention will be described below by dividing it into a first manufacturing method and a second manufacturing method.
[0084] [First manufacturing method] As described above, the first production method includes the (1-1) adhesive layer forming step and the (1-2) insertion step. (1-1) Adhesive layer formation process (1-1) In the adhesive layer forming step, a first adhesive layer is formed on one of the outer peripheral surface of the pellet and the inner peripheral surface of the compartment, and a second adhesive layer is formed on the other. The first adhesive layer and the second adhesive layer are as described above.
[0085] The first adhesive layer and the second adhesive layer may be formed on either the outer peripheral surface of the pellet or the inner peripheral surface of the compartment. The first adhesive layer may be formed only on a portion of the outer peripheral surface of the pellet or the inner peripheral surface of the compartment in the circumferential direction, or may be formed over the entire circumferential direction.Similarly, the second adhesive layer may be formed only on a portion of the outer peripheral surface of the pellet or the inner peripheral surface of the compartment in the circumferential direction, or may be formed over the entire circumferential direction.
[0086] In order to firmly integrate the storage material pellet and the storage member, it is preferable that the first adhesive layer is formed around the entire circumferential surface of the pellet or the inner circumferential surface of the compartment, and similarly, it is preferable that the second adhesive layer is formed around the entire circumferential surface of the pellet or the inner circumferential surface of the compartment.
[0087] In order to easily perform the adhesive layer forming step, it is preferable to form the first adhesive layer only on a part of the axial direction of the outer peripheral surface of the pellet or the inner peripheral surface of the compartment, and the same is true for the second adhesive layer. Note that, in the adhesive layer forming step (1-1), it is more preferable to form the second adhesive layer further forward in the insertion direction than the first adhesive layer, as in the adhesive layer forming step (2-1) of the second production method described above.
[0088] The amount of the first adhesive layer and the amount of the second adhesive layer are not particularly limited, but since, as described above, the second adhesive layer functions as a filler filled between the outer peripheral surface of the pellet and the inner peripheral surface of the compartment, and the first adhesive layer functions as a pressing material for spreading the second adhesive layer, it is more preferable to make the amount of the first adhesive layer greater than the amount of the second adhesive layer.
[0089] The method of forming the first adhesive layer and the second adhesive layer is not particularly limited, and any method may be adopted. For example, the first adhesive layer may be formed by applying the first adhesive to the outer peripheral surface of the pellet or the inner peripheral surface of the compartment. Also, for example, if the first adhesive layer is made of a thermoplastic resin, the first adhesive, which has been molded in advance into a ring shape or the like along the outer peripheral surface of the pellet or the inner peripheral surface of the compartment, may be attached to the outer peripheral surface of the pellet or the inner peripheral surface of the compartment, and heated to form a fluid first adhesive layer. The same applies to the second adhesive layer.
[0090] (1-2) Insertion process The (1-2) inserting step is a step of inserting the storage material pellet into the sub-space after the above (1-1) adhesive layer forming step. The (1-2) inserting step may be performed after (1-1), more specifically, when the first adhesive layer and the second adhesive layer are not hardened and are in a fluid state. If the first adhesive layer and the second adhesive layer are made of a thermoplastic resin, the first adhesive layer and the second adhesive layer that have been hardened may be heated and softened before the (1-2) inserting step.
[0091] [Second manufacturing method] The second manufacturing method includes the above-mentioned (2-1) adhesive layer forming step and (2-2) insertion step, of which (2-2) insertion step is omitted since it can be performed in the same manner as (2-1) insertion step.
[0092] (2-1) Adhesive layer formation process (2-1) In the adhesive layer forming step, a first adhesive layer and a second adhesive layer are formed on one of the outer peripheral surface of the pellet and the inner peripheral surface of the compartment. Of these, the second adhesive layer is formed further forward in the insertion direction than the first adhesive layer. The first adhesive layer and the second adhesive layer are as described above.
[0093] On the other of the outer peripheral surface of the pellet and the inner peripheral surface of the compartment, i.e., the surface on which the first adhesive layer and the second adhesive layer are not formed, it is not necessary to form an adhesive layer, and in some cases, the second adhesive layer may be formed.
[0094] In the adhesive layer forming step (2-1), similarly to the adhesive layer forming step (1-1), the first adhesive layer may be formed only on a portion of the circumferential direction of the outer peripheral surface of the pellet or the inner peripheral surface of the compartment, or may be formed over the entire circumference in the circumferential direction. Similarly, the second adhesive layer may be formed only on a portion of the circumferential direction of the outer peripheral surface of the pellet or the inner peripheral surface of the compartment, or may be formed over the entire circumference in the circumferential direction. Furthermore, it is preferable that the first adhesive layer is formed over the entire circumferential direction of the outer peripheral surface of the pellet or the inner peripheral surface of the compartment, and similarly, it is preferable that the second adhesive layer is formed over the entire circumferential direction of the outer peripheral surface of the pellet or the inner peripheral surface of the compartment.
[0095] Here, in order to easily carry out the adhesive layer formation process, it is preferable to form the first adhesive layer and the second adhesive layer on the outer peripheral surface of the pellet, and it is particularly preferable to form them on the leading portion of the outer peripheral surface of the pellet in the insertion direction.
[0096] In the manufacturing method of the present invention, there is a preferred shape for the partition wall. Specifically, it is preferable to provide a ring-groove-shaped pool portion at an end of the partition wall that is located on the sub-space side and on the insertion start side in the insertion process. The pool portion can also be said to be recessed toward the outside in the radial direction of the sub-space and to be open toward the insertion start side and in the radial direction.
[0097] First, an embodiment in which a first adhesive layer and a second adhesive layer are formed on the outer peripheral surface of a storage material pellet and a pool portion is provided in a partition wall in the second production method of the present invention will be described.
[0098] The pool portion is located on the partition wall at the insertion start side in the insertion step, in other words, on the partition wall at the rear side in the insertion direction described above. Therefore, when inserting the storage material pellets into the sub-space in the second manufacturing method of this aspect, the storage material pellets first pass through the pool portion of the partition wall.
[0099] Since the pool portion is stepped as described above, the diameter of the sub-space, i.e., the distance between the opposing partition walls, is wider in the pool portion than in the forward portion in the insertion direction from the pool portion. Such a pool portion has a function of storing a part of the adhesive layer. Since the second adhesive layer is formed on the outer peripheral surface of the storage material pellet on the forward side in the insertion direction, the second adhesive layer is stored in the pool portion.
[0100] In the insertion step, the second adhesive layer stored in the pool is gradually pushed forward in the insertion direction by the first adhesive layer, so that according to this embodiment, the second adhesive layer can be uniformly supplied to the gap between the outer circumferential surface of the pellet and the inner circumferential surface of the compartment.
[0101] In the second manufacturing method of the present invention, an embodiment in which a first adhesive layer and a second adhesive layer are formed on the inner peripheral surface of the partition wall and the partition wall has a pool portion will be described.
[0102] In this embodiment, the second adhesive layer may be formed in the area including the pool portion on the inner peripheral surface of the partition wall in the adhesive layer forming step. In other words, in this embodiment, the first adhesive layer and the second adhesive layer may be already stored in the pool portion after the adhesive layer forming step.
[0103] In the second manufacturing method of this aspect as well, in the insertion step, the storage material pellet passes through the pool portion of the partition wall and presses the first adhesive layer on the insertion start side of the pool portion toward the leading side in the insertion direction. The first adhesive layer pressed toward the leading side in the insertion direction further presses the second adhesive layer on the leading side in the insertion direction toward the leading side in the insertion direction. Since the first adhesive layer has a higher viscosity than the second adhesive layer, it functions as a pressing material for spreading the second adhesive layer, and the second adhesive layer stored in the pool is gradually pushed out toward the front side in the insertion direction. Therefore, this embodiment also makes it possible to uniformly supply the second adhesive layer to the gap between the outer circumferential surface of the pellet and the inner circumferential surface of the compartment.
[0104] In this embodiment, the pool is covered by the first adhesive layer stored at the insertion start side of the pool, which prevents the second adhesive layer stored in the pool from leaking to the insertion start side, making it possible to supply a sufficient amount of the second adhesive layer to the gap between the outer circumferential surface of the pellet and the inner circumferential surface of the compartment.
[0105] In the first manufacturing method of the present invention, an embodiment will be described in which a first adhesive layer is formed on the outer peripheral surface of the storage material pellet and a second adhesive layer is formed on the inner peripheral surface of the partition wall, and a pool portion is provided in the partition wall.
[0106] In this embodiment as well, in the adhesive layer forming step, it is preferable to form a second adhesive layer in a region including the pool portion on the inner peripheral surface of the partition wall.
[0107] In the first manufacturing method of this aspect, the first adhesive layer formed on the outer peripheral surface of the storage material pellet passes through the pool portion of the partition wall during the insertion step and presses the second adhesive layer stored in the pool portion toward the front side in the insertion direction. Therefore, even in this aspect, the first adhesive layer functions as a pressing material for spreading the second adhesive layer, and the second adhesive layer stored in the pool portion is gradually pushed out toward the front side in the insertion direction. Therefore, even in this aspect, it is possible to uniformly supply the second adhesive layer to the gap between the outer peripheral surface of the pellet and the inner peripheral surface of the partition.
[0108] Furthermore, in this embodiment, the first adhesive layer also functions as a lid for the pool portion, and the leakage of the second adhesive layer stored in the pool portion to the insertion start side is inhibited, so that this embodiment also makes it possible to supply a sufficient amount of the second adhesive layer to the gap between the outer peripheral surface of the pellet and the inner peripheral surface of the compartment.
[0109] The method for producing a gas container according to the present invention will be described below with reference to specific examples.
[0110] Example 1 The gas container of the first embodiment is a pressure-resistant container that is mounted on a vehicle and is used to store and release hydrogen gas, which is a type of fill gas. The manufacturing method of the first embodiment is the first manufacturing method. FIG. 1 is a diagram for explaining the gas container of Example 1. FIG. 2 is a diagram for explaining an axial cross section of a main part of the gas container of Example 1. FIG. 3 is a diagram for explaining an exploded view of a main part of the gas container of Example 1. FIG. 4 is a diagram for explaining a housing member of the gas container of Example 1. FIG. 5 is a diagram for explaining an adhesive layer forming step in the manufacturing method of Example 1. FIG. 6 to FIG. 8 are diagrams for explaining an insertion step in the manufacturing method of Example 1. In the following description, the axial direction and the radial direction refer to the directions shown in the respective drawings.
[0111] [Gas bottle] As shown in FIGS. 1 to 3, the gas container 1 of the first embodiment includes a container body 10, a cap 20, a cap 30, a reinforcing layer 40, storage material pellets 50, a storage member 60, and a connecting portion .
[0112] The container body 10 is made of polyethylene resin and is a so-called resin liner that is generally cylindrical with both axial ends tapered in diameter. As shown in FIG. 2, an internal space 18 is formed inside the container body 10 which is substantially cylindrical.
[0113] The container body 10 is formed by welding together four divided bodies (a first divided body 11, a second divided body 12, a third divided body 13, and a fourth divided body 14). These four divided bodies can be said to be the container body 10 divided into four bodies in a direction perpendicular to the axial direction.
[0114] The first division body 11 and the second division body 12 have the same cylindrical shape, and the third division body 13 and the fourth division body 14 have the same dome shape. The split bodies are arranged in the axial direction in the order of third split body 13, first split body 11, second split body 12, and fourth split body 14.
[0115] Both axial ends of the container body 10 are open. One of the openings is referred to as a first opening 15, and the other is referred to as a second opening 16. The first opening 15 is provided in the third divided body 13, and the second opening 16 is provided in the fourth divided body 14. A metal base 20 (base 20, base 30) is attached to each of the first opening 15 and the second opening 16 via an O-ring.
[0116] The base 20 has an integral heat exchange passage 21 through which a heat exchange medium circulates. The base 30 is fitted with a valve and a gas supply pipe (not shown). The cap 30 functions as a filler gas inlet / outlet through which hydrogen gas, which is the filler gas, flows in and out via the gas supply pipe and the valve. Note that the cap 20 is substantially plugged and does not function as a filler gas inlet / outlet, but functions as a heat exchanger.
[0117] As shown in FIG. 1, the outer surface of the container body 10 is covered with a reinforcing layer 40 made of FPR.
[0118] As shown in FIG. 2, a storage member 60 is disposed in the internal space 18 of the container body 10.
[0119] As shown in FIGS. 3 and 4, the storage member 60 has a honeycomb shape in which a plurality of sub-spaces 62 defined by partition walls 61 are arranged. 4, the subspaces 62 extend in the axial direction and are arranged in the radial direction, i.e., in a direction perpendicular to the axial direction. The subspaces 62 are of the same shape, and the radial cross section of each subspace 62 is a regular hexagon, and the radial cross section is constant in the axial direction. The partition wall 61 is made of SUS316L, a type of stainless steel, and has a plate shape. The thickness of the partition wall 61 is about 0.1 mm.
[0120] 2 and 3, the center of the containing member 60 is hollow, and a cylindrical connecting part 70 is integrated with the center. The connecting part 70 is made of the same material as the partition wall 61, and extends in the axial direction toward the base 20.
[0121] As shown in Fig. 4, each sub-space 62 contains a storage material pellet 50. The storage material is a porous carbon-based material, and the storage material pellet 50 is in the form of a pellet in which the storage material is cross-linked with a cross-linking agent. The shape of the storage material pellet 50 is approximately the same as the shape of the internal space 18.
[0122] The manufacturing method of the first embodiment will be described below.
[0123] [Manufacturing method] [Preparation process] First, the four divided bodies (first divided body 11, second divided body 12, third divided body 13, and fourth divided body 14) constituting the container body 10 were each injection molded. Of these, a base 20 was attached to the first opening 15 of the third split body 13 (see FIG. 3) together with an O-ring. Also, a base 20 was attached to the second opening 16 of the fourth split body 14 together with an O-ring. Moreover, the storage member 60 was manufactured by assembling the partition walls 61 into a honeycomb shape.
[0124] [Assembly process] In the assembly process, the storage material pellets 50 were inserted into the sub-spaces 62 of the storage member 60 and adhered to the partition walls 61 .
[0125] [Adhesive layer formation process] First, in the adhesive layer forming step of the assembling process, as shown in Fig. 5, a first adhesive was applied to a leading portion of the pellet outer circumferential surface 51 of the storage material pellet 50 in the insertion direction a to form a first adhesive layer 81. Also, a second adhesive was applied to a portion of the compartment inner circumferential surface 63 of the compartment wall 61 on the insertion start side, i.e., a trailing portion in the insertion direction a, to form a second adhesive layer 82.
[0126] Here, in Example 1, a ring-groove-shaped pool portion 65 is formed at an end portion located on the insertion start side of the compartment inner circumferential surface 63. In the adhesive layer forming step of Example 1, the second adhesive layer 82 is formed in an area including the pool portion 65 on the compartment inner circumferential surface 63.
[0127] The second adhesive has a lower viscosity than the first adhesive, and the second adhesive layer 82 has a lower viscosity than the first adhesive layer 81. The sum of the thickness of the first adhesive layer 81 and the thickness of the second adhesive layer 82 is slightly larger than the thickness of the gap between the pellet outer surface 51 and the compartment inner surface 63, in other words, the distance in the radial direction between the pellet outer surface 51 and the compartment inner surface 63.
[0128] [Insertion process] After the above-mentioned adhesive forming step, the storage material pellet 50 on which the first adhesive layer 81 was formed was inserted into the sub-space 62 of the containing member 60 on which the second adhesive layer 82 was formed.
[0129] 6, at this time, the first adhesive layer 81 abuts against the second adhesive layer 82 stored in the pool portion 65. Then, as the insertion of the storage material pellets 50 progresses, the second adhesive layer 82 is pressed by the first adhesive layer 81 and comes into pressure contact with the bottom surface 66 and inner circumferential surface 67 of the pool portion 65, and is also pressed by the reaction force against the bottom surface 66 and inner circumferential surface 67 of the pool portion 65 and comes into pressure contact with the first adhesive layer 81.
[0130] As described above, the viscosity of the first adhesive layer 81 is higher than that of the second adhesive layer 82, and the first adhesive layer 81 is less likely to deform than the second adhesive layer 82. Therefore, as shown in Fig. 7, the second adhesive layer 82 is pressed by the first adhesive layer 81 and deforms significantly, and is pushed out from the pool portion 65 toward the tip side in the insertion direction a. Then, as shown in Fig. 8, the second adhesive layer 82 fills the gap between the pellet outer peripheral surface 51 and the partition inner peripheral surface 63.
[0131] In other words, when the storage material pellet 50 is inserted into the sub-space 62, the first adhesive layer 81 and the second adhesive layer 82 are pressed together, and the second adhesive layer 82 is deformed relative to the first adhesive layer 81 at the interface between the first adhesive layer 81 and the second adhesive layer 82. Therefore, the second adhesive layer 82 functions as a filler that fills the gap between the pellet outer peripheral surface 51 and the compartment inner peripheral surface 63, and the first adhesive layer 81 functions as a pressing material for spreading the second adhesive layer 82. Furthermore, the second adhesive layer 82 also functions as a lubricant for the first adhesive layer 81, and the first adhesive layer 81 also functions as a filler.
[0132] 8, after the insertion step, the adhesive layer consisting of the first adhesive layer 81 and the second adhesive layer 82 was filled without any gaps in the gap between the pellet outer peripheral surface 51 and the compartment inner peripheral surface 63. As a result, an integrated product in which the storage material pellet 50 was assembled into the containing member 60 was obtained.
[0133] Thereafter, the containing member 60 fixed to the base 30 was inserted into the second split body 12 and the first split body 11, and the first split body 11, the second split body 12 and the fourth split body 14 were welded together to be integrated. Furthermore, the housing member 60 was fixed to the nozzle 20 while the connecting portion 70 integrated with the housing member 60 was brought into contact with the nozzle 20. Then, the integrated body of the first division body 11, the second division body 12, and the fourth division body 14 was welded to the third division body 13 to obtain the container body 10.
[0134] An FRP reinforcing layer 40 was formed on the surface of the container body 10 thus obtained, and the gas container 1 of Example 1 was obtained.
[0135] According to the manufacturing method of Example 1, it is possible to fill the space between the outer circumferential surface 51 of the storage material pellet 50 and the inner circumferential surface 63 of the partition wall 61 with the first adhesive layer 81 and the second adhesive layer 82 without leaving any gaps. As a result, the storage material pellets 50 can be stably bonded and integrated with the containing member 60, and furthermore, a sufficient amount of the storage material pellets 50 can be stored and held in the internal space 18 of the gas container 1, thereby improving the storage and release performance of the filled gas in the gas container 1.
[0136] For reference, the operation of the gas container 1 of the embodiment will be described below.
[0137] In the gas container 1 of the embodiment, a storage member 60 for storing and holding the storage material pellets 50 is disposed in the internal space 18 of the container body 10 .
[0138] The storage member 60 has a honeycomb structure with partition walls 61 running throughout, and the storage material pellets 50 are stored in sub-spaces 62 formed between the partition walls 61. The partition walls 61 are made of a heat conductive material and function as a heat exchanger. Due to the presence of such partition walls 61, the internal space 18 is thermally uniform throughout, and the temperature of the storage material pellets 50 stored in the internal space 18 is also uniform.
[0139] Furthermore, the partition wall 61 is in contact with the base 20 via the connecting portion 70 and is thermally connected to the base 20. Since the base 20 is integrally provided with the heat exchange flow path 21 through which the heat exchange medium circulates, the partition wall 61 indirectly exchanges heat with the heat exchange medium.
[0140] As a result, the temperature of the internal space 18 is efficiently and quickly regulated, and the temperature of the storage material pellets 50 in the internal space 18 is also efficiently and quickly regulated. Therefore, in the gas container 1 of the embodiment, the storage gas is smoothly absorbed into the storage material pellets 50 and the storage gas is smoothly released from the storage material pellets 50 in the internal space 18.
[0141] In the gas container 1, when the filler gas is supplied to the internal space 18 of the container body 10 through the valve and nozzle 30 (not shown), the filler gas flows into each sub-space 62 of the container member 60 through the axial end face 69 (see Figure 2) of the container member 60 arranged in the internal space 18.
[0142] The filler gas that has flowed into the sub-space 62 flows from the nozzle 30 side to the nozzle 20 side while being gradually occluded by the storage material pellets 50 contained and held in the sub-space 62. In this way, the gas container 1 of the first embodiment stores the filler gas.
[0143] Example 2 The manufacturing method of Example 2 is a second manufacturing method, and is generally the same as the manufacturing method of Example 1, except for the positions of the first adhesive layer and the second adhesive layer. The gas container of Example 2 is generally the same as the gas container of Example 1. Therefore, the manufacturing method of Example 2 will be described below, focusing on the differences from Example 1. FIG. 9 is an explanatory diagram that illustrates the adhesive layer forming step in the manufacturing method of Example 2.
[0144] [Manufacturing method] [Adhesive layer formation process] In the adhesive layer forming step in the manufacturing method of Example 2, a first adhesive layer 81 and a second adhesive layer 82 were formed on the leading portion in the insertion direction a of the outer circumferential surface 51 of the storage material pellet 50, as shown in Fig. 9. Furthermore, of these, the second adhesive layer 82 was disposed further forward in the insertion direction a than the first adhesive layer 81.
[0145] In the manufacturing method of Example 2, the thickness of the first adhesive layer 81 and the thickness of the second adhesive layer 82 are each slightly larger than the thickness of the gap between the outer circumferential surface 51 of the pellet and the inner circumferential surface 63 of the compartment.
[0146] [Insertion process] After the above-mentioned adhesive forming step, the storage material pellet 50 on which the first adhesive layer 81 and the second adhesive layer 82 were formed was inserted into the sub-space 62 of the containing member 60.
[0147] At this time, the second adhesive layer 82 located at the front side in the insertion direction a is first stored in the pool portion 65, and then the first adhesive layer 81 located behind the second adhesive layer 82 in the insertion direction a advances toward the pool portion 65. Therefore, in the manufacturing method of Example 2 as well, similar to the manufacturing method of Example 1, the second adhesive layer 82 is pressed by the first adhesive layer 81 to be pressed against the bottom surface 66 and inner circumferential surface 67 of the pool portion 65, and is also pressed against the bottom surface 66 and inner circumferential surface 67 of the pool portion 65 by the reaction force to be pressed against the first adhesive layer 81.
[0148] At this time, the second adhesive layer 82 is pressed against the first adhesive layer 81 and significantly deformed, and is pushed out from the pool portion 65 toward the front side in the insertion direction a, filling the gap between the pellet outer surface 51 and the partition inner surface 63. Thus, in the manufacturing method of Example 2, as in the manufacturing method of Example 1, the adhesive layer consisting of the first adhesive layer 81 and the second adhesive layer 82 was filled without any gaps into the gap between the pellet outer peripheral surface 51 and the compartment inner peripheral surface 63. As a result, a sufficient amount of storage material pellets 50 can be stored and held in the internal space 18 of the gas container 1, and the storage and release performance of the filled gas in the gas container 1 can be improved.
[0149] The present invention is not limited to the above-described embodiment, and various modifications can be made without departing from the spirit of the present invention. [Explanation of symbols]
[0150] 1: Gas container 10: Container body 18: Internal space 20: Base 50: Storage pellet 51: Outer surface of storage pellet 60: Storage member 61: Partition wall 62: Subspace 63: Side of subspace at partition wall 65: Pool portion 81: First adhesive layer 82: Second adhesive layer
Claims
1. A container body having an internal space; a cap connecting the outside of the container body with the internal space; a honeycomb-shaped container member disposed in the internal space and including a plurality of sub-spaces partitioned by partition walls made of a thermally conductive material; a storage material that is accommodated and held in the sub-space and that absorbs and releases a fill gas, comprising: a step of inserting and fixing a storage material pellet, which is formed by solidifying the storage material powder and has the same shape as the sub-space, into the sub-space of the storage member; The assembling step includes: an adhesive layer forming step of forming a first adhesive layer on one of an outer peripheral surface of the storage material pellet and the sub-space side surface of the partition wall, and forming a second adhesive layer having a lower viscosity than the first adhesive layer on the other of the outer peripheral surface and the sub-space side surface of the partition wall; an inserting step of inserting the storage material pellet into the sub-space after the adhesive layer forming step.
2. A container body having an internal space; a cap connecting the outside of the container body with the internal space; a honeycomb-shaped container member disposed in the internal space and including a plurality of sub-spaces partitioned by partition walls made of a thermally conductive material; a storage material that is accommodated and held in the sub-space and that absorbs and releases a fill gas, comprising: a step of inserting and fixing a storage material pellet, which is formed by solidifying the storage material powder and has the same shape as the sub-space, into the sub-space of the storage member; The assembling step includes: an adhesive layer forming step of forming a first adhesive layer on one of an outer peripheral surface of the storage material pellet and a side surface of the sub-space of the partition wall, and a second adhesive layer having a lower viscosity than the first adhesive layer and positioned further forward in the insertion direction than the first adhesive layer; an inserting step of inserting the storage material pellet into the sub-space after the adhesive layer forming step.
3. 3. The method for manufacturing a gas container according to claim 1, further comprising providing a ring-shaped pool portion at an end portion of the partition wall that is located on the sub-space side and on an insertion start side in the inserting step.
4. A method for manufacturing a gas container as described in claim 3, which cites claim 1, wherein the first adhesive layer is formed on the outer peripheral surface of the storage material pellet, and the second adhesive layer is formed on the sub-space side surface of the partition wall in an area including the pool portion.
Citation Information
Patent Citations
Hydrogen storage metal storage tank
JP1994281097A
High pressure hydrogen storage tank
JP2004307949A
Manufacturing method for hydrogen storage tank, and hydrogen storage tank
JP2009002370A
Storage canister
JP2012132562A
Fuel tank
US20170066320A1