Method for reducing structural damage to the surface of a single crystal aluminum nitride substrate and single crystal aluminum nitride substrate produced thereby

The heat treatment method in an autoclave effectively removes near-surface damage on single-crystal aluminum nitride substrates by sublimating the damaged areas, ensuring improved crystalline quality and uniform deposition for enhanced crystal growth.

JP7569850B2Active Publication Date: 2024-10-18FRAUNHOFER GESELLSCHAFT ZUR FORDERUNG DER ANGEWANDTEN FORSCHUNG EV
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2022520166
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-10-01
Filing Date
2020-09-30
Publication Date
2024-10-18
Estimated Expiration
2040-09-30

AI Technical Summary

Technical Problem

Existing methods struggle to effectively remove near-surface structural damage on single-crystal aluminum nitride substrates, particularly at the edges, which affects the quality of subsequent material deposition and limits the achievable crystal diameter during growth processes.

Method used

A heat treatment method in an autoclave at high temperatures (2000-2350°C) and controlled oxygen partial pressure (10⁻⁴ mbar) is used to sublimate and remove damaged areas on the substrate surface, utilizing a temperature gradient and inert gas atmosphere to ensure uniform and controlled material removal.

Benefits of technology

The method achieves a substantially damage-free surface, allowing for improved crystalline quality and uniform material deposition, thereby enhancing the diameter of high-quality crystal growth regions and preventing unwanted surface layer formation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007569850000001
    Figure 0007569850000001
  • Figure 0007569850000002
    Figure 0007569850000002
  • Figure 0007569850000003
    Figure 0007569850000003
Patent Text Reader

Abstract

The present invention relates to a method for reducing structural damage to the surface of a single-crystal aluminum nitride substrate. According to this method, damaged areas of the aluminum nitride substrate are sublimated and removed by heat-treating the substrate in an autoclave crucible. This method is used to prepare the surface of single-crystal aluminum nitride (AlN), and a particular object of the present invention is to eliminate, or at least significantly reduce, near-surface structural damage to the single-crystal material caused by mechanical processing. The present invention also relates to aluminum nitride substrates so treated.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for reducing structural damage at the surface of a single crystal aluminum nitride substrate, by heat treating the substrate in a crucible in an autoclave, thereby sublimating and removing the aluminum nitride in damaged areas of the substrate surface. The method is used for the surface treatment of single crystal aluminum nitride (AlN), and in particular the method is aimed at removing, or at least substantially removing, structural damage near the surface of the single crystal material caused by mechanical treatment. The present invention relates to the aluminum nitride substrate thus treated. [Background technology]

[0002] The production of substrate wafers, e.g. wafers or seed plates, from grown single crystals involves several processing steps, usually mechanical processing steps. These include circular or flat grinding, sawing, edge rounding, lapping and polishing. When these mechanical steps are terminated by a polishing step, damage near the surface of the single crystal material is often observed.

[0003] A distinction is made between potentially damaging regions close to the surface: a polished layer with a thickness of 0.1-1 μm directly on the surface, then a sublayer 1-100 μm from the surface, a deformation layer 1-200 μm from the surface, and finally the substrate, which shows no visible effects.

[0004] Such surface damage can also affect areas below the visible surface (subsurface damage), and surface treatments are now known to remove these. These include chemical etching (see Non-Patent Document 1, Non-Patent Document 2) and / or the so-called "chemical mechanical polishing step" (CMP) (Patent Document 1). However, damage to the edge of the wafer, for example after edge rounding, cannot be addressed by the usual CMP process.

[0005] It has been found that for single crystals produced by the PVT method, such as the semiconductors aluminum nitride (AlN) and silicon carbide (SiC), the quality of the surface treatment of the seed face directly influences the dislocation density of the material deposited on it during growth. Removal or reduction of near-surface damage can directly improve the dislocation density at the phase boundary between the seed crystal and the newly grown crystalline material, and also reduce the dislocation density in the volume of the new single crystal.

[0006] When these wafers are used as seed plates for growth processes (e.g. for crystal growth but also epitaxy processes such as MOVPE for layer deposition), in particular near-surface damage present at the wafer rim or at the wafer edge is intentionally accepted, as during the growth process new material with poor crystalline quality is often deposited in this edge region. Therefore, attempts are made to geometrically shield the edge region from the growth flow with other materials and, if necessary, to appropriately adjust the thermal boundary conditions in this region, preventing or reducing the deposition of material.

[0007] Both methods have significant drawbacks in the growth process. If low-quality material is allowed to deposit, the edge region limits the crystal diameter that can be achieved with good-quality material. The low-quality material may grow parasitically into the good-quality region, further reducing the diameter of the good-quality region. The geometrical cover of the damaged rim region has the same drawback of reducing the diameter of the good-quality region. In particular, measures must be taken to prevent polycrystals from being deposited on the cover itself, by a suitable combination of the choice of cover material and appropriate thermal boundary conditions during growth. Depending on the growth material and the required growth conditions, this is often impossible or, if achieved, requires a very large effort.

[0008] Furthermore, attempts to remove near-surface damage by chemical etching, for example with aqueous potassium hydroxide or molten solutions, may be associated with other specific challenges: for example, surface contamination from the chemicals used may be difficult to remove and may result in surface morphologies that are unfavorable for use in growth processes, due to selective etching attack of dislocations or other lattice defects.

[0009] In particular, for the optimization of nucleation in the PVT growth of SiC semiconductors, a damage removal step, temperature gradient inversion (T(nucleus)>T(source)) has been proposed to remove surface damage and surface contamination of the polished nuclei at the beginning of the growth step and at the same time avoid material precipitation during the heating process at low temperatures (Non-Patent Document 3). However, this method is difficult to use for the growth of silicon carbide (SiC) and does not replace mechanical polishing after the sawing step of SiC, because the surface is easily graphitized due to the non-stoichiometric sublimation of silicon carbide (SiC) and the significant removal of important materials, which results in the silicon carbide (SiC) surface being unusable as a nucleation surface. [Prior art documents] [Non-patent literature]

[0010] [Non-Patent Document 1] "Defects in SiC substrates and epitaxial layers affecting semiconductor device performance" Muller S., Sumakeris J., Brady M., Glass R., Hobgood H., Jenny J., Carter C. (2004) [Non-Patent Document 2] The European Physical Journal Applied Physics, 27(1-3), 29-35. doi:10.1051 / epjap:2004085 [Non-Patent Document 3] MM Anikin et al., Proc. ICSCRM-95, Kyoto, Japan, 1996, page 33 and Temperature gradient controlled Sic crystal growth, M. Anikin, R. Madar, Materials Science and Engineering B46 (1997) 278-286 [Patent documents]

[0011] [Patent Document 1] US2010 / 0062601 Summary of the Invention

[0012] The problem to be solved by the present invention is to provide a method for surface treatment of a single crystal aluminum nitride substrate, with the aim of achieving a surface that is as free or as little damaged as possible in the areas close to the surface of the aluminum nitride substrate, thereby achieving as complete a treatment as possible in the entire surface area.

[0013] This problem is solved by a method for the surface treatment of a single-crystal aluminum nitride substrate having the features of claim 1 and by a single-crystal aluminum nitride substrate produced thereby having the features of claim 12. Further dependent claims indicate advantageous configurations.

[0014] According to this invention, a method for treating the surface of a single crystal aluminum nitride substrate is proposed, in which the substrate is heat-treated in a crucible in an autoclave to sublimate and remove aluminum nitride from damaged areas of the surface. The heat treatment is carried out at a temperature of at least 2000°C and an oxygen partial pressure of at most 10 -4 The reaction is carried out under an atmosphere of 10 ... mbar.

[0015] Unlike silicon carbide, aluminum nitride sublimation is essentially stoichiometric, so that heat treatment of the aluminum nitride semiconductor of the present invention can be performed without the problems associated with silicon carbide, i.e., longer treatment times or greater material removal do not result in the formation of undesirable surface layers due to non-stoichiometric rearrangement reactions.

[0016] The temperature of the heat treatment is selected to produce a sufficiently high partial pressure of aluminum at the substrate interface so that the damaged material can be removed by sublimation from the substrate surface.

[0017] The absolute temperature within the autoclave, the temperature gradient at the substrate surface and the atmospheric pressure within the autoclave can be adjusted to provide a sufficiently high and simultaneously controlled removal rate.

[0018] In order to prevent undesirable oxidation of the aluminum nitride surface, the oxygen concentration in the autoclave is made as small as possible. From this point of view, the maximum oxygen partial pressure is set to 10 -4 mbar is chosen.

[0019] The heat treatment is desirably carried out at a temperature of 2000°C to 2350°C, preferably 2150°C to 2250°C.

[0020] In a further preferred embodiment, the heat treatment is carried out at a pressure of 1 mbar to 10 -4 mbar vacuum or from 1 mbar to 1.5×10 3 The reaction is carried out under an inert gas atmosphere of 1000 mbar, preferably selected from the group consisting of nitrogen, argon, helium or combinations thereof.

[0021] Furthermore, in the heat treatment, it is preferred that the temperature gradient perpendicular to the substrate surface is at least 5° C. / cm.

[0022] In a further preferred embodiment, the thermal gradient parallel to the substrate surface during the heat treatment is at most 1° C. / cm. If such a thermal gradient is maintained, laterally homogeneous material can be removed.

[0023] In a further preferred embodiment, the thermal gradient parallel to the substrate surface during the heat treatment is at least 1° C. / cm. This removes laterally inhomogeneous material, thereby improving the alignment of the crystal axes. <0001> The substrate normal can be tilted relative to

[0024] The nitrogen polarity plane of aluminum is <0001> Preferably, the substrate is specifically removed at an orientation of + / - 5° relative to the substrate.

[0025] Furthermore, carbon is preferably present in the autoclave atmosphere during heat treatment in the form of carbon-containing species, which prevents the formation of aluminum droplets on the aluminum nitride surface during cooling. This is preferably achieved by having the inner surface of the crucible, on which the aluminum nitride substrate is placed, contain or consist of tantalum carbide, which allows a carbon partial pressure to be generated during heat treatment.

[0026] The method of the present invention is suitable for pre-treating a substrate, in particular for removing damage caused by steps such as sawing, grinding, abrading or a combination thereof, thus providing a substantially damage-free surface.

[0027] As a further advantage, the method of the present invention can be used to remove subsurface damage to the substrate, as well as damage to the rim region and / or edge of the substrate.

[0028] In accordance with the present invention, a single crystal aluminum nitride substrate can be provided that is substantially free of damage at the surface or near surface regions.

[0029] The following figures and examples are intended to more fully illustrate the features of the present invention, without the present invention being limited to the specific embodiments shown therein. [Brief description of the drawings]

[0030] [Figure 1]Figure 1 is a schematic diagram showing the state of a wafer after round edge processing. [Diagram 2] FIG. 2 shows the edge-shielded wafer during the growth process. [Diagram 3] FIG. 3 shows the structure of the crucible used in the present invention. [Figure 4] X-ray topography images of mechanically and CMP polished AlN wafers, FIG. 4a shows one without heat treatment and FIG. 4b shows one with heat treatment. [Diagram 5] 1 shows an AFM image of an AlN wafer processed according to the present invention.

[0031] Figure 1 shows a wafer 1 that has been subjected to a mechanical edge rounding process. During this mechanical process, structural damage 2 has been caused to the rounded edge of the wafer. According to the prior art, such wafers are usually subjected to a growth step with the edge area shielded by a cover 3. This is shown in Figure 2.

[0032] 3 shows a crucible 11 used in the method of the invention, in which an aluminum nitrite wafer is placed on a holder 12. A suitable temperature profile then leads to partial sublimation of the aluminum nitrite wafer 13 at its surface.

[0033] FIG. 4a shows an X-ray topography image of a wafer mechanically processed according to the prior art, and FIG. 4b shows an X-ray topography image of a wafer processed according to the method of the present invention. From this figure, it can be seen that the wafer in FIG. 4a has a dark contrast at the rim of the wafer. This dark area is damage caused in the rim area by the mechanical processing. On the other hand, FIG. 4b shows a wafer thermally processed according to the method of the present invention. There is no structural damage at the rim of the wafer and no dark contrast is visible.

[0034] Figure 5 shows an AFM image of an aluminum nitride wafer of the present invention, which has a stepped surface, which can be directly used as a seed plate for the novel PVT growth process to form aluminum nitrite crystals. EXAMPLES

[0035] The wafer is placed with the surface to be treated facing up on a tantalum carbide ceramic plate at the bottom of a tungsten crucible (typical height: 3 cm). The diameter of the crucible here is determined by the diameter size of the wafer and is usually 1 cm larger than the diameter of the wafer. To improve the control of the removal of the AlN material from the wafer surface by sublimation, an AlN polymaterial (mass of the order of the mass of the wafer to be treated) with as little impurities of oxygen as possible (less than 200 ppm) is additionally added to the end of the above-mentioned tantalum carbide ceramic in order to generate an additional partial pressure of AlN species in the gas phase during the thermal treatment of the wafer surface. For the control of this process, the temperature of the crucible lid (control temperature) is usually determined pyrometrically and is set specifically for the various process steps. It should be noted that in the above-mentioned crucible configuration, the control temperature is 50-70 ° C lower than the temperature of the wafer surface to be heat treated.

[0036] In this configuration, the crucible is placed in an autoclave and subjected to the conditions of the next step (the designated temperature corresponds to the controlled temperature). 1. Before the heat treatment process and during the initial heat treatment process up to about 500-700°C, >5N nitrogen (720mbar) was fed several times to maintain the temperature at 1E ―2 The autoclave is repeatedly evacuated to a vacuum of 1000 psi (720 mbar) to remove as much residual oxygen as possible from the autoclave. Finally, the autoclave is filled with >5N nitrogen (720 mbar). 2. By heating (RF heating or resistance heating), increase the controlled temperature to 2100°C at a rate of 12-15°C / min. 3. By heating, increase the controlled temperature from 2100°C to 2200°C at a rate of 2.5-3.0°C / min. 4.2 Maintain the temperature at 200 °C for 5-25 min to remove a surface layer of typically 20-50 μm, so that the temperature gradient in the axial direction of the wafer surface, in the direction of the crucible lid, is about 20 °C / cm. This gradient is set by the shape of the crucible and by the appropriate choice of shape and material of the insulation surrounding the crucible in the autoclave. 5. Reduce heat to room temperature and lower control temperature. Cooling rate is typically 4-5°C / min.

Claims

1. A method for treating the surface of a single crystal aluminum nitride substrate, comprising the steps of: placing the substrate in a crucible in an autoclave for a heat treatment that results in sublimation and removal of aluminum nitride from the damaged areas of the surface; The heat treatment is performed at a temperature of 2000° C. to 2350° C. and an oxygen partial pressure of up to 10 -4 The reaction was carried out under an atmosphere of 1000 psi. The heat treatment is carried out under a vacuum of 1 mbar to 10 −4 mbar or under an inert gas atmosphere of 1 mbar to 1.5×10 3 mbar; During said heat treatment, the temperature gradient perpendicular to the substrate surface is at least 5° C. / cm; A method in which nitrogen polar faces of aluminum nitride are specifically removed from said substrate with an orientation of + / - 5° relative to the crystallographic axis <0001>.

2. The heat treatment is carried out at 2150°C to 2250°C. The method of claim 1

3. The inert gas is preferably selected from nitrogen, argon, helium or a combination thereof. The method according to claim 1 or 2.

4. During said heat treatment, a temperature gradient parallel to the substrate surface is at most 1° C. / cm to allow for laterally uniform material removal; 4. The method according to any one of claims 1 to 3.

5. During said heat treatment, a temperature gradient parallel to the substrate surface is at least 1° C. / cm to remove laterally inhomogeneous material and tilt the substrate normal relative to the crystal axis <0001>.

5. The method according to any one of claims 1 to 4.

6. Carbon was contained in the atmosphere.

6. The method according to any one of claims 1 to 5.

7. removing damage caused by pre-treatment of the substrate; 7. The method according to any one of claims 1 to 6.

8. removing damage below the surface of the substrate; 8. The method according to any one of claims 1 to 7.

9. Remove edge damage from the rim area and / or the rim area; 9. The method according to any one of claims 1 to 8.

10. A single crystal aluminum nitride substrate produced by the method according to any one of claims 1 to 9.

Citation Information

Patent Citations

  • Group iii nitride crystal and growing method thereof

    JP2006335608A

  • Seed formation growth method for preparing aluminum nitride single crystals

    JP2008535759A

  • Apparatus and method for producing compound semiconductor single crystal

    JP2013075789A

  • Methods for polishing aluminum nitride

    US20100062601A1