A textured thin film obtained from an additive overlay process that provides complete and uniform coverage of non-smooth surfaces

A textured thin film using microparticle liquid feedstock maintains surface texture and provides abrasion resistance on non-smooth surfaces, addressing the limitations of existing coatings and environmental hazards.

JP7570811B2Active Publication Date: 2024-10-22PRAXAIR ST TECHNOLOGY INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2019568366
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2018-06-08
Filing Date
2018-06-11
Publication Date
2024-10-22
Estimated Expiration
2038-06-11

AI Technical Summary

Technical Problem

Existing coating processes fail to provide sufficient abrasion resistance while preserving the underlying surface texture or profile of non-smooth surfaces, and some methods, like hard chrome plating, are environmentally hazardous.

Method used

A textured thin film is applied using a particulate liquid feedstock with microparticles of 5 micrometers or less, delivered by an additive overlaying device, to create a continuous, uniform coating that conforms to the substrate's pattern, maintaining the texture and providing abrasion resistance.

Benefits of technology

The coating maintains the underlying texture and provides excellent wear and corrosion resistance without altering the surface profile, even on complex geometries, with a thickness of 25 micrometers or less, and hardness comparable to hard chrome plating.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007570811000001
    Figure 0007570811000001
  • Figure 0007570811000002
    Figure 0007570811000002
  • Figure 0007570811000003
    Figure 0007570811000003
Patent Text Reader

Abstract

The present invention relates to a textured thin film that can be applied over a non-smooth surface to improve the surface's hardness, corrosion resistance, and wear resistance properties while maintaining the underlying profile of the non-smooth surface. Using an additive overlay process, a textured thin film can be produced on a non-smooth surface so as to fully preserve the surface texture or profile of the underlying surface without substantially altering or degrading the underlying surface texture or profile of the non-smooth surface. The textured thin film provides uniform and complete coverage of the non-smooth surface and maintains the surface profile. [Selected Figure] Figure 1a
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a continuous, textured, thin film applied over a non-smooth surface for use in a variety of applications, where the film substantially retains the surface texture of the underlying non-smooth surface that it overlies. [Background technology]

[0002] Many coated substrate surfaces require coatings that maintain or do not significantly degrade the underlying surface texture or pattern of the substrate surface. It should be understood that the terms "texture", "surface texture" and "pattern" are intended to have the same meaning throughout as used herein. As used throughout, the term "substrate" refers to any non-smooth surface that is characterized by a certain random or non-random surface pattern or textured profile. Substrates include any suitable type of material, such as metal and alloy surfaces.

[0003] One example of a substrate is an embossing roll having a feature of recesses or grooves and / or raised protrusions to generate a certain pattern or surface texture. Another example of a substrate is a work roll having a predefined surface texture. For example, a work roll for use with metals or metal alloys (e.g., steel, titanium, copper, brass, and aluminum) having a certain surface texture may be required to produce rolled workpieces and other products. As used herein, "workpiece" and "product" refer to any type of material that the coated substrate may come into contact with as part of the rolling process or end use (e.g., heat treatment, annealing, etc.), including, for example, strip, slab, or other rolled sheet metal, and other sheet products. Textured work rolls for hot and cold rolling mills to operate have certain benefits, including allowing a significant reduction in the thickness of the workpiece material passing through the work roll.

[0004] Additionally, the surface texture of the work rolls is desirable because it can act to capture lubricant at the roll bite that would otherwise be starved of lubricant (due to the extreme temperatures associated with hot rolling), which then expels the lubricant to the roll / slab interface, thereby substantially minimizing material transfer due to adhesion between the roll surface and the slab surface, and minimizing debris and smudge entrainment on the slab surface as it enters the cold rolling stand.

[0005] Furthermore, the work rolls of large cold rolling and temper mills used in the production of sheet steel must have a well-defined textured surface, which is imparted to the sheet steel as it passes through the rolls. When the sheet is then formed into a required profile, for example a car body shell, the surface texture of the sheet plays a very important role, firstly in the oil lubrication required during pressing of the sheet, and then in the painting of the metal shell. It is known in the art that certain qualities of surface roughness and surface lubricity are required in the pressing of sheet steel for the automotive industry and other applications.

[0006] Many coating processes have been adopted, but they do not provide suitable wear life. One example is the hard chrome plating process, which is widely used today. However, the main drawback of the hard chrome plating process is that it uses hexavalent chromium. Due to the carcinogenic properties of hexavalent chromium, the unauthorized use of Cr(VI) compounds will be prohibited in the European Union from September 2017 by the Regulation on Registration, Evaluation, Authorization and Restriction of Chemicals (REACH).

[0007] As an alternative, electrical discharge coating (EDC) has been explored to create a texture on the underlying surface while depositing a coating on the workpiece surface. EDC is a surface alloying / coating process to create a hard, wear-resistant layer with an electrical discharge textured surface on a metal substrate. Compacted and / or sintered metal carbide electrodes have been used during electrical discharge texturing to improve roll wear resistance by surface alloying. During the EDC process, current flows through the electrode, causing ionization of the dielectric in the spark gap. During ionization, temperatures in excess of 8000K can be generated, at which point localized melting and vaporization of the electrode and workpiece surface occurs to create the coating surface. The product tends to exhibit unacceptably low levels of tungsten carbide adhesion to the workpiece surface, resulting in poor wear resistance.

[0008] Furthermore, other current coating processes generally cannot preserve the surface texture or profile of the underlying non-smooth surface. Today, when a coating is applied to a non-smooth surface, which may be produced by, for example, texturing, embossing, engraving, etching or knurling, the uneven surface is lost when a thick protective coating is applied over it.

[0009] In view of the shortcomings of current coating processes, there remains a need for improved coatings and processes for their manufacture that can coat non-smooth substrate surfaces to a sufficient film mass to provide protective abrasion resistance and not substantially degrade the surface texture or profile of the underlying non-smooth surface, thereby substantially preserving the surface texture or profile of the underlying surface. Summary of the Invention

[0010] In one aspect, a textured thin film is provided that includes a substrate that includes a non-smooth surface characterized by a pattern having a predetermined number of peaks and valleys. The textured thin film extends continuously along the entire non-smooth surface. The textured thin film is obtained from a liquid feedstock of particulates that is delivered by an additive overlaying device. The particulates have an effective diameter of about 5 micrometers or less. The textured thin coating has a minimum and maximum thickness of about 25 micrometers or less, such that the ratio of the minimum thickness to the maximum thickness is in the range of about 0.6 to about 1.0, thereby producing a film texture that substantially matches the pattern of the non-smooth surface.

[0011] In a second aspect, a textured thin film is provided that includes a substrate that includes a non-smooth surface characterized by a pattern. The pattern is characterized by a contour profile defined by a predetermined number of peaks and valleys. The textured thin film extends continuously along the entire non-smooth surface to produce (i) coated peaks, each of which matches the contour profile of a corresponding peak of the non-smooth surface, and (ii) coated valleys, each of which matches the contour profile of a corresponding valley of the non-smooth surface. The textured thin film is obtained from liquid feed particulates that are delivered by an additive overlay device. The textured thin film has a minimum and maximum thickness of about 25 micrometers or less, such that the ratio of the minimum thickness to the maximum thickness is in the range of about 0.6 to about 1.0.

[0012] In a third aspect, a method for producing a substrate that is completely coated along an outer surface of a substrate without substantially changing or degrading the texture profile of the outer surface of the substrate, the method comprising the steps of: providing an outer surface to a substrate, the outer surface having a pattern characterized as being non-smooth as defined by the texture profile; providing an additional overlay apparatus, the additional overlay apparatus comprising a combustion chamber and a nozzle; generating a hot gas effluent; supplying a liquid source of particulate to the hot gas effluent, the particulate having a size in the range of 0.1 to 5 micrometers; generating a molten particulate effluent; and directing the molten particulate effluent onto the non-smooth texture profile to produce a textured film that substantially conforms to the pattern of the non-smooth surface. [Brief description of the drawings]

[0013] [Figure 1a] FIG. 1 illustrates a textured top surface of a substrate having a conventional thermal spray coating applied along the top surface, where the coating thickness is non-uniform along the peaks and valleys of the textured surface and the underlying texture is degraded. [Figure 1b] FIG. 1b shows the non-smooth upper surface of the same substrate as in FIG. 1a with a textured thin film having uniform coverage and thickness and extending continuously along the peaks and valleys, in accordance with the principles of the present invention, where the textured thin film is obtained from an additive overlay process. [Figure 2a] FIG. 1 illustrates another example of a textured top surface of a substrate having a conventional thermal spray coating applied along the top surface, the coating thickness being non-uniform along the peaks and valleys of the textured surface and degrading the underlying texture. [Figure 2b] FIG. 2b shows the non-smooth upper surface of the same substrate as in FIG. 2a with a textured thin film having uniform coverage and thickness and extending continuously along the peaks and valleys, in accordance with the principles of the present invention, where the textured thin film is obtained from an additive overlay process. [Diagram 3] FIG. 1 is a representative schematic diagram of a system for additive overlay processing. [Figure 4] 1 is a photomicrograph of a relatively thin film that has been textured to cover an entire non-smooth surface to substantially match the underlying pattern of a non-smooth substrate in accordance with the principles of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] The present invention recognizes that when thermal spray coatings are applied over non-smooth surfaces, which may be produced by texturing, embossing, engraving, etching or knurling, the fineness of the non-uniform surface (i.e., surface texture, profile or pattern) is lost or covered by conventional thermal spray coatings. The present invention provides a novel solution to overcome the inhibitions to non-smooth surfaces while maintaining the necessary wear resistance of the non-smooth surfaces. The additive overlay process with a carbide feedstock, preferably with particles ranging from about 0.1 to 5 micrometers in size, can overcome the shortcomings of conventional thermal spray coatings by producing a thin, textured, dense and wear-resistant film.

[0015] One aspect of the present invention focuses on a film that can generally produce the desired wear and corrosion resistance while substantially maintaining the resulting underlying texture or pattern of a non-smooth substrate surface. The textured thin film is characterized by the absence of chrome plating or EDC and is derived from a liquid feedstock of particulates about 5 micrometers or less in size delivered by an additive overlay device.

[0016] It should be understood that the present invention can be utilized with any type of substrate having a need to retain the surface texture or pattern of a non-smooth surface. A variety of non-smooth substrates can be utilized, such as embossing rolls, engraving rolls, etching rolls, knurling rolls, pinch rolls, calendar rolls, briquetting rolls, corrugating rolls, metering rolls, pulling rolls, godet rolls, and crimping rolls. In a preferred embodiment, the substrate can be a work roll, such as may be utilized in processes for rolling metal alloys (e.g., steel or aluminum alloys) or other non-metallic workpieces.

[0017] The present invention recognizes the anticipated drawbacks of utilizing dry powders to coat non-smooth textured surfaces. Specifically, FIG. 1a shows a dry powder-based coating 15 extending along a non-smooth surface 10. The non-smooth top surface 10 is shown in its entirety as having a representative non-smooth surface characterized by a pattern defined as a series of a predetermined number of peaks and valleys. The upper portion of the non-smooth top surface 10 is shown to be a textured surface as a somewhat contoured profile that is substantially wavy. It should be understood that the top surface 10 may have any other profile shape. For simplicity of representation, the non-smooth top surface 10 is not drawn to scale and the remainder of the non-smooth surface 10 has been purposely omitted. Other details of the non-smooth surface 10 have been purposely omitted to better clarify the principles of the present invention. The coated peaks are designated 11a, 12a, 13a, 14a, and the corresponding coated valleys are designated 11b, 12b, 13b, 14b. Each of the peaks 11a, 12a, 13a, 14a are shown as having equal heights and each of the valleys 11b, 12b, 13b, 14b are shown as having equal depths, however, it should be understood that the present invention contemplates any configuration of peaks and valleys.

[0018] The present invention recognizes that the dry powder-based coating 15 has a tendency to accumulate more in the valleys 11b, 12b, 13b, and 14b compared to the peaks 11a, 12a, 13a, and 14a as a result of the relatively large particle sizes that must be used to avoid agglomeration effects in the thermal spraying equipment. As a result, the underlying pattern of the non-smooth surface 10 is lost because the deposition of the relatively large sized molten powder particulates cannot be controlled to the degree necessary to obtain a substantially uniform coating along the peaks 11a, 12a, 13a, and 14a and the valleys 11b, 12b, 13b, and 14b. The dry powder-based coating 15 inhibits the local surface texture of the non-smooth surface 10, reducing the surface profile 10 by reducing or blunting the features of the valleys 11b, 12b, 13b, and 14b. Thus, the overall surface texture of the dry powder-based coating 15 is insufficient for certain end uses (e.g., embossing roll applications).

[0019] Instead, in accordance with the principles of the present invention, FIG. 1b shows a textured thin film 16 obtained from a liquid feedstock of solids sized 5 micrometers or less. The film 16 is provided by an additive overlay device. The textured thin film 16 is uniformly deposited to produce coated peaks 11a', 12a', 13a', and 14a', and coated valleys 11b', 12b', 13b', and 14b'. In addition, coverage of the peaks and valleys is substantially uniform and complete along the entire length of the non-smooth surface 10, such that the film 16 is characterized by a minimum to maximum thickness ratio of 0.6 to 1.0, preferably 0.7 to 1.0, and more preferably 0.8 to 1.0. FIG. 1b shows that the textured thin film 16 substantially conforms to the underlying pattern of the non-smooth surface 10. Specifically, the textured thin film 16 extends continuously along the entire non-smooth surface 10 to produce (i) coated peaks 11a', 12a', 13a', and 14a', each of which matches the contour profile of a corresponding peak of the non-smooth surface 10, and (ii) coated valleys 11b', 12b', 13b', and 14b', each of which matches the contour profile of a corresponding valley of the non-smooth surface 10. The film 16 extends continuously along the non-smooth surface 10. Ultimately, no valleys or peaks remain exposed. The film 16 exhibits a thickness of 25 micrometers or less, preferably 5 to 15 micrometers, and more preferably 5 to 10 micrometers.

[0020] The film can be made significantly thinner than conventional thermal spray coatings applied to contoured, non-smooth surfaces (e.g., FIG. 1a), yet the coating 16 can maintain or increase the wear resistance of the non-smooth surface 10. The film 16 of FIG. 1b is particularly advantageous when a particular application requires maximum surface coverage to produce maximum wear and corrosion resistance over complex shapes having textured patterns without altering or degrading the underlying textured pattern.

[0021] The benefits of the present invention may be used on other non-smooth surfaces. For example, FIG. 2b shows a non-smooth surface 20 having a substantially square wave pattern along its entire length. FIG. 2b shows a textured thin film 18 obtained from a liquid feedstock of solid particulates of 5 micrometers or less that are delivered by an additive overlay device. The textured thin film 18 is uniformly deposited to produce coated peaks 21a', 22a', 23a', and 24a', and coated valleys 21b', 22b', 23b', and 24b'. Additionally, coverage of the peaks and valleys is substantially uniform and complete along the entire length of the non-smooth surface 20, such that the film 18 is characterized by a ratio of minimum thickness to maximum thickness of 0.6 to 1.0, preferably 0.7 to 1.0, and more preferably 0.8 to 1.0.

[0022] FIG. 2b shows that the textured thin film 18 substantially conforms to the underlying pattern of the non-smooth surface 20 to maintain the underlying texture of the non-smooth surface 20. Specifically, the textured thin film 18 extends continuously along the entire non-smooth surface 20 to produce (i) coated peaks 21a', 22a', 23a', and 24a', each of which conforms to the contour profile of a corresponding peak of the non-smooth surface 20, and (ii) coated valleys 21b', 22b', 23b', and 24b', each of which conforms to the contour profile of a corresponding valley of the non-smooth surface 20. The film 18 extends continuously along the non-smooth surface 20. The end result is that no valleys or peaks are left exposed. The film 16 exhibits a thickness of 25 micrometers or less, preferably 5 to 15 micrometers, and more preferably 5 to 10 micrometers.

[0023] In contrast, Figure 2a shows that a dry powder-based coating 17 would not be expected to produce a uniform coverage along the textured surface 20. Similar to Figure 1b, more coating 17 will accumulate in the valleys than in the peaks, such that the thickness of coated valleys 21b, 22b, and 23b is greater than the thickness of coated peaks 21a, 22a, 23a, and 24a. The end result is that the coating will not be textured and will not substantially conform to the contours of the textured surface 20, thereby altering or degrading the underlying pattern of the textured surface 20.

[0024] In one aspect of the invention, the size (i.e., effective diameter) of the microparticles is 5 micrometers or less, preferably in the range of 0.1 to 3 micrometers, more preferably 0.5 to 2.5 micrometers. The coating thickness in a preferred embodiment may range from 5 to 25 micrometers. The combination of these attributes can result in a surface roughness (Ra) of the textured thin films 16 and 20 that is preferably less than about 1.5 micrometers.

[0025] Surprisingly, the significant reduction in the amount of applied inventive films 16 and 18 of Figures 1b and 2b, respectively, compared to thermal spray coatings does not reduce the hardness, wear resistance, or corrosion resistance properties of the inventive films. By way of example, in one embodiment, the inventive films 16 and 18 of Figures 1b and 2b, respectively, have a microhardness (HV300) in the range of 900-1400, which is comparable to or better than a typical hard chrome plated surface, and have a minimal porosity of 0.5 vol% or less relative to the total volume of the inventive film deposited along a non-smooth surface.

[0026] The thin and textured films of the present invention can be provided with such properties by tungsten carbide-containing compositions, such as, for example, but not intended to be limiting, WC-CoCr, WC-Co, WC-Ni, or CrC-NiCr. The tungsten carbide-containing films extend along the non-smooth surface, preferably with carbide grain sizes in the range of 0.05 to 1 micron. The feedstock corresponding to the tungsten carbide composition can be obtained from sintered particulates or spray-dried sintered particulates, and the feedstock can include any suitable solvent, organic or inorganic, and in one preferred embodiment is an ethanol-based liquid. It is understood that the textured thin films may also have other compositions obtained from the feedstock suspension material that are suitable for providing wear resistance, corrosion resistance, and microhardness protection properties of the non-smooth surface of the substrate to withstand very aggressive environments.

[0027] In another embodiment, the film can be obtained from a liquid feedstock of nano-sized powder particles that are fully atomized to submicron particles. The submicron particles are deposited from an additive overlay device substantially continuously and preferably in a monolayer coating on each of the peaks and valleys of the non-smooth surface to produce a textured monolayer film that can be reduced in thickness along each of the peaks and valleys compared to those previously described herein. The monolayer coating reduces the amount of particulates that contact the non-smooth surface without unnecessary material waste. Furthermore, the nano-sized films 16 and 18 of Fig. 1b and Fig. 2b can improve the preservation of the pattern of the underlying non-smooth surface. Thus, the overall surface texture of the partially coated substrate remains substantially unchanged. The choice of a monolayer coating using nano-sized films or the stacking of multiple separate layers to produce a textured thin film may depend on the end application, such as the desired load capacity. As the load capacity increases, it may be necessary to stack multiple separate layers to produce a textured thin film.

[0028] The system and method for producing the film of the present invention uses an additive overlaying device having a combustion chamber that produces a hot gas effluent. Figure 3 shows an exemplary system and method in which a liquid feedstock with powder particulates is fed into the combustion chamber of the additive overlaying device to produce a stream of molten particulate effluent that can be directed onto a non-smooth surface. Particulates of the liquid feedstock having a size of 5 micrometers or less are fed into the hot gas, thereby producing an effluent that can be directed onto a non-smooth surface to conform to the pattern of the non-smooth surface. The size of the particulates is 5 micrometers or less, which allows the particulates to adhere such that the film has a thickness of 25 micrometers or less along the non-smooth substrate, thereby allowing the film to substantially conform to the underlying pattern of the substrate. EXAMPLES

[0029] The additive overlay device was used to produce textured thin films on non-smooth metal surfaces with textured profiles. An ethanol-based feedstock containing 20 wt% solids was prepared using fine particles (median particle size (d50) 2.35 micrometers) with a nominal composition of 86 wt% WC-10 wt% Co-4 wt% Cr. The liquid feedstock was fed from a pot into the additive overlay device at a pressure of 70 psi and a flow rate of 1 gallon / hour, and applied to the substrate at a spray distance of 4 inches using a combustible mixture fed into the combustion chamber of the additive overlay device.

[0030] The photomicrograph in FIG. 4 was obtained at 500x magnification and upon visual inspection shows that a dense film microstructure was achieved resulting in an as-deposited film thickness of less than 8 micrometers after four attempts. The photomicrograph shows that the film substantially conforms to the contours of the non-smooth metal surface. Visual observation determined that the entire metal surface was covered; no bare spots were detected.

[0031] While what are considered to be preferred embodiments of the invention have been shown and described, it will of course be understood that various modifications and changes in form or detail can be readily made without departing from the spirit and scope of the invention. For example, the additive overcoat and application methods described herein can be applied directly or indirectly to a non-smooth surface of a substrate. It should further be understood that in addition to a work roll, any type of substrate can be employed, such as, but not intended to be limiting, an embossing roll, an engraving roll, an etching roll, a knurling roll, a pinch roll, a calendar roll, a briquetting roll, a corrugating roll, a metering roll, a pulling roll, a godet roll, a crimping roll, and the like. It is therefore intended that the invention is not limited to the exact forms and details shown and described herein, nor is it intended to be limited to anything less than the full scope of the invention disclosed herein and claimed below.

Claims

1. A textured thin film comprising: a substrate including a non-smooth surface characterized by a pattern, the pattern having a predetermined number of peaks and valleys; the textured thin film extends continuously along the entire non-smooth surface, the textured thin film comprising particulates having a particle size of 0.05 to 1 micrometer; The textured thin film has a minimum thickness and a maximum thickness of 25 micrometers or less, such that a ratio of minimum thickness to maximum thickness is in the range of 0.6 to 1.0, creating a film texture that substantially matches the pattern of the non-smooth surface.

2. 2. The textured thin film of claim 1, wherein the non-smooth surface is selected from the group consisting of a work roll, an embossing roll, an engraving roll, a knurling roll, a pinch roll, a calendar roll, a briquetting roll, a corrugating roll, and a godet roll.

3. The textured thin film of claim 1 , wherein the film has a thickness in the range of 5 to 25 micrometers.

4. 2. The textured thin film of claim 1, wherein the effective diameter of the microparticles is in the range of 0.05 to 1 micrometer.

5. 10. The textured thin film of claim 1, further comprising a surface roughness (Ra) of less than 1.5 micrometers.

6. 10. The textured thin film of claim 1 further comprising a microhardness (HV300) in the range of 900-1400.

7. 10. The textured thin film of claim 1, wherein the film comprises a composition selected from the group consisting of WC-CoCr, WC-Co, WC-Ni, and CrC-NiCr.

8. The textured thin film of claim 1 , wherein the pattern has a contour profile defined in a wave-like manner.

9. The textured thin film of claim 1 , wherein the pattern is sinusoidal or trapezoidal.

10. 2. The textured thin film of claim 1, wherein the non-smooth surface of the substrate has the pattern sufficiently preserved by the textured thin film extending continuously along the entire non-smooth surface.

11. A textured thin film comprising: a substrate including a non-smooth surface characterized by a pattern, the pattern characterized by a contour profile defined by a predetermined number of peaks and valleys; the textured thin film extends continuously along the entire non-smooth surface to produce (i) coated peaks, each of which matches the contour profile of a corresponding peak of the non-smooth surface, and (ii) coated valleys, each of which matches the contour profile of a corresponding valley of the non-smooth surface; the textured thin film comprises particulates; The textured thin film has a minimum thickness and a maximum thickness of 25 micrometers or less, such that the ratio of the minimum thickness to the maximum thickness is in the range of 0.6 to 1.

0.

12. 12. The textured thin film of claim 11, wherein the particulates have an effective diameter of 0.05 to 1 micrometer.

13. 12. The textured thin film of claim 11, wherein the particulates are nano-sized to produce a monolayer film.

14. 1. A method for producing a substrate having complete coverage along an exterior surface of the substrate without substantially altering or degrading a texture profile of the exterior surface of the substrate, the method comprising: providing the substrate with an exterior surface, the exterior surface having a pattern characterized as being non-smooth as defined by the texture profile; providing an additive deposition apparatus, the additive deposition apparatus comprising a combustion chamber and a nozzle; generating a hot gas effluent; supplying a liquid feedstock containing particulates suspended within the liquid to the hot gas effluent, the particulates having a size in the range of 0.1 to 5 micrometers; generating a molten particulate effluent; and directing the molten particulate effluent onto the non-smooth textured profile to produce a textured film that substantially conforms to the pattern of the non-smooth surface.

15. The method of claim 14 further comprising impinging the molten particulate effluent onto the substrate so as to extend continuously along the substrate.

16. 15. The method of claim 14, further comprising accumulating the molten particulate effluent on the substrate to a thickness of 25 micrometers or less.

17. 15. The method of claim 14, wherein the substrate is selected from the group consisting of a work roll, an embossing roll, an engraving roll, a knurling roll, a pinch roll, a calendar roll, a briquetting roll, a corrugating roll, and a godet roll.

18. 15. The method of claim 14, further comprising directing the molten particulate effluent onto the non-smooth texture profile such that the molten particulate effluent impacts the substrate at an angle less than 90 degrees relative to the surface of the substrate.

Citation Information

Patent Citations

  • Continuous casting roll having little heat inlet

    JP2000301302A