Transfer sheet and method for producing the same
The transfer sheet with a moisture absorption prevention layer on the back surface addresses the issue of ink effectiveness in high humidity and temperature by maintaining stability through lamination or solid printing, ensuring prolonged effective performance.
Patent Information
- Application Number
- JP2020115050
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-07-02
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2040-07-02
AI Technical Summary
Conventional transfer paper with suppressor ink loses effectiveness in high temperature and high humidity environments due to moisture absorption, leading to weakened inhibitor performance.
A transfer sheet design featuring a moisture absorption prevention layer on the back surface of the base sheet, either through lamination with a resin film or solid printing with ink, to prevent moisture absorption into the suppression ink.
The transfer sheet maintains stable performance even during long-term storage under varying environmental conditions, extending the effective period by more than four times compared to designs without the moisture absorption prevention layer.
Smart Images

Figure 0007574554000002 
Figure 0007574554000001
Abstract
Description
[Technical field]
[0001] The present invention relates to a transfer sheet for forming a pattern or the like on the surface of a decorative sheet used for flooring materials, etc., and more specifically, to a transfer sheet having a suppressing ink specification that partially suppresses foaming in the transfer material and a moisture absorption prevention layer that prevents moisture absorption by the suppressing ink. And the manufacturing method of the transfer sheet Regarding. [Background technology]
[0002] 2. Description of the Related Art Transfer papers using suppressing ink are known in the art (see Patent Documents 1 and 2). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2005-22373 A [Patent Document 2] JP 2015-193249 A [Patent Document 3] Japanese Patent Application Publication No. 11-267407 Summary of the Invention [Problem to be solved by the invention]
[0004] However, conventional transfer paper using suppression ink had the problem that the suppression effect was weakened in the high temperature and humidity environments of summer. This is because the suppressor contained in the suppressor ink reacts with water molecules (see Patent Document 3). The present invention focuses on the above-mentioned points, and aims to provide a transfer sheet that can exhibit stable effects even when stored for a long period of time by providing a moisture absorption prevention layer on the back surface of a base sheet to prevent moisture absorption into the inhibiting ink. [Means for solving the problem]
[0005] A transfer sheet according to one embodiment of the present invention is a transfer sheet having a peelable pattern layer containing an inhibiting ink that inhibits foaming in the material to be transferred onto the surface of a base sheet, and is characterized in that a moisture absorption prevention layer is provided on the back surface of the base sheet to prevent moisture absorption into the pattern layer. The transfer sheet according to one aspect of the present invention is characterized in that a resin film is laminated on the back surface of the base sheet as the moisture absorption prevention layer.
[0006] In one aspect of the transfer sheet of the present invention, the moisture absorption prevention layer is solid-printed on the back surface of the base sheet using a solid ink. In one embodiment of the transfer sheet of the present invention, the coating amount of the solid ink is 0.5 g / m 2 More than 3.0g / m 2 The present invention is characterized in that: A transfer sheet according to one embodiment of the present invention is characterized in that the moisture absorption prevention layer is provided only on the back surface of the base sheet, out of three locations: the back surface of the base sheet, the space between the base sheet and the picture pattern layer, and the front surface of the picture pattern layer. Effect of the Invention
[0007] According to one aspect of the present invention, a transfer sheet capable of exhibiting stable effects even when stored for a long period of time can be provided. [Brief description of the drawings]
[0008] [Figure 1] FIG. 2 is a cross-sectional view of a transfer sheet according to the first embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] (Transfer sheet 10 according to the embodiment) In Figure 1, 10 is a transfer sheet 10 according to an embodiment, which is used to form a pattern or the like on the surface of a transfer material, which is a floor material (decorative material) for use in wet areas such as kitchens, washrooms, and toilets (not shown). The transfer sheet 10 is formed from the following layers: The following (1) to (3) will be discussed later. (1) Base sheet 20 (release paper) (2) 30 pattern layers (3) Moisture absorption prevention layer 40
[0010] (Base sheet 20) The base sheet 20 is, for example, a release paper. The base sheet 20 may be made of, in addition to "paper", an olefin resin, a polyester resin, or a laminate of paper and an olefin resin, or a laminate of paper and a polyester resin sheet. As the base sheet 20 according to this embodiment, a laminate in which paper and an olefin-based resin are laminated can be suitably used.
[0011] As the olefin resin, for example, one or a mixture of two or more types of various resins such as polypropylene resin, low density polyethylene resin, high density polyethylene resin, polymethylpentene resin, etc. can be used as a single layer or a laminated structure in which multiple layers are combined. To explain this with reference to the embodiment described later, the base sheet 20 is made of paper laminated with polypropylene resin on both sides. The print surface, which is the front surface of the base sheet 20, is glossy finished, but a matte finish may also be used. Further, the back surface of the base sheet 20 used has a matte finish, but a gloss finish may also be used.
[0012] (Pattern layer 30) As shown in FIG. 1, the picture design layer 30 is provided on the printing surface, which is the front surface of the base sheet 20, and contains an inhibiting ink that inhibits foaming in the transfer material. The picture design layer 30 is formed from the following layers as shown in FIG. (1) Picture Ink Section 31 The picture ink section 31 is made up of color inks. (2) Foam-inhibiting ink section 32 The expansion inhibiting ink section 32 is formed between adjacent pattern ink sections 31 and is made of an inhibiting ink.
[0013] (Repression inks and printing inks) The inhibiting ink may contain any conventionally known foaming inhibitor, such as triazine compounds, triazole compounds such as benzotriazoles and aminotriazoles, trimellitic anhydride, maleic acid, fumaric acid, adipic acid, etc., and among these, triazole compounds are preferably used. More preferably, the compound is an aminotriazole.
[0014] The foam-inhibiting ink section 32 containing the inhibiting ink can be used as a binder resin by appropriately selecting resins such as vinyl resins such as vinyl chloride-vinyl acetate copolymers, acrylic resins, polyester resins, and urethane resins, either alone or as a composite such as a mixture or copolymer. Furthermore, the expansion-inhibiting ink portion 32 may contain an extender pigment for reducing tackiness, various stabilizers, and the like. As the extender pigment, for example, silica can be suitably used.
[0015] The picture pattern layer 30 can be provided with any pattern, such as a decorative pattern for decorating the surfaces of buildings such as houses and stores, interior and exterior materials for vehicles such as trains and automobiles, airplanes and ships, flooring, etc., designs, colors, wood grain patterns, cork patterns, stone patterns, tile patterns, joints, wood grain duct patterns, etc. Such a picture pattern layer 30 can be made using any conventionally known printing ink, and examples of printing ink pigments include, but are not limited to, isoindolinone yellow, polyazo red, phthalocyanine blue, carbon black, iron oxide, and titanium oxide.
[0016] As the binder resin used in the printing ink, various resins such as urethane resins, acrylic resins, polyester resins, vinyl resins, etc. can be appropriately selected and used alone or as a composite such as a mixture or copolymer. Furthermore, there is no problem if various additives such as hardeners, catalysts, stabilizers, initiators, etc. are added to the picture design layer 30 according to the selected binder resin. The expansion-inhibiting ink portion 32 and the picture pattern layer 30 as described above can be provided by appropriately selecting a conventionally known printing technique such as gravure printing, offset printing, gravure offset printing, screen printing, flexographic printing, ink jet printing, or the like.
[0017] (Moisture absorption prevention layer 40) As shown in FIG. 1, the moisture absorption prevention layer 40 is provided on the back surface of the base sheet 20 to prevent the picture pattern layer 30 from absorbing moisture. In other words, the moisture absorption prevention layer 40 is provided only on the back surface of the base sheet 20 out of three locations: the back surface of the base sheet 20, between the base sheet 20 and the picture pattern layer 30, and on the front surface of the picture pattern layer 30. The moisture absorption prevention layer 40 is of the following two types. The following (1) and (2) will be discussed later. (1) Lamination method (2) Solid printing method
[0018] (Lamination method) In the lamination method, a resin film is laminated on the back surface of the base sheet 20, and the resin film prevents moisture absorption into the picture pattern layer 30 through the base sheet 20. The resin film is, for example, laminated with PP resin. The resin film is not limited to olefin resin such as PP, but may be a polyester film such as PET. Although the thickness of the resin film is set to 15 μm, the thickness may be less than 15 μm as long as the back surface of the base sheet 20 is not exposed. The thickness of the resin film is 3 μm or more and 25 μm or less, and 15 μm is preferable.
[0019] (Lamination method) In the laminate method, the period during which the moisture absorption suppression effect is exerted is definitely extended compared to the case without the moisture absorption prevention layer 40, and the effective period can be extended by more than four times. In addition, in the case of the lamination method, the period during which the suppression effect was exhibited was also extended when the resin used in the resin film or its thickness was changed.
[0020] (Solid printing method) In the solid printing method, a solid printed layer is provided on the back surface of the base sheet 20 using a solid ink, and the solid printed layer formed by solid printing suppresses moisture absorption into the picture pattern layer 30 through the base sheet 20. Solid printing is done using an acrylic chloride vinyl acetate resin similar to ink, or colored ink (hereinafter simply referred to as "ink" or "ink for solid images"). Printing can be done under various conditions regarding the number of solid prints and the amount of coating. The amount of ink applied for solid printing is, for example, 0.5 g / m 2 More than 3.0g / m 2 Less than or equal to 0.5 g / m 2 More than 1.5g / m 2 The following is recommended: 0.5g / m 2 When the coating amount is less than this, the period during which the suppression effect is exerted is slightly longer than when there is no moisture absorption prevention layer 40, but this does not result in a significant improvement. Further, for example, gravure printing is used as the solid printing, but the solid printing is not limited to this, and printing methods such as flexographic printing, offset printing, and ink jet printing can also be used.
[0021] An area that is filled in with a color that is 100% ink concentration or a combination of two 100% colors is called a "solid" area, and "solid printing" refers to printing in the colors described above, where the print is completely covered with ink, with no gaps. Printing inks are composed of the four colors CMYK or DIC (spot colors) mixed to express specific colors, but the following colors are considered "solid colors." (1) C100% color (100% of CMYK single color) (2) C100% + M100% color (combination of CMYK100%) (3) 100% DIC color (100% special ink) (4) CMYK is all 100% multiplied (total solid)
[0022] (Solid printing method) In the solid printing method, the period during which the moisture absorption suppression effect is exerted is definitely extended compared to the case without the moisture absorption prevention layer 40, and the effective period can be extended by more than four times. In addition, in the solid printing method, when the amount of ink applied for solid printing is changed, for example, from 0.5 to 1.5 g / m 2 With this coating amount, the period during which the moisture absorption prevention effect was exhibited was longer than when there was no moisture absorption prevention layer 40. EXAMPLES
[0023] The transfer sheet according to the present invention will be described below with reference to Examples A to G and Comparative Examples A to D. Note that the present invention is not limited to the following Examples A to G.
[0024] Example A Example A was prepared using the materials and procedures set forth below. The base sheet was a paper laminated with polypropylene resin on both sides. The printing surface, which is the front surface of the base sheet, has a gloss finish, but a matte finish may also be used. The back surface of the base sheet used had a matte finish, but a gloss finish may also be used. The picture design layer is produced by picture printing. In Example A, a lamination method was adopted, and a laminate (PP resin, 15 μm thick) was laminated on the back surface as a moisture absorption prevention layer.
[0025] Example B Example B was the same as Example A, except that a lamination method was used, and a laminate (PET resin, 12 μm thick) was laminated on the back side as a moisture absorption prevention layer. Example C Example C is the same as Example A except that a laminate method is used and a laminate (PP resin, thickness 5 μm) is used on the back side as a moisture absorption prevention layer. Example D Example D is the same as Example A except that a laminate method is used and a laminate (PP resin, thickness 21 μm) is used on the back side as a moisture absorption prevention layer.
[0026] Example E In Example E, a solid printing method was used, and a moisture absorption prevention layer of 3 g / m was applied to the back side. 2 As the example, a target solid print was applied, and the rest was the same as in Example A. On the back surface of the base sheet, vinyl chloride and vinyl acetate, similar to the ink, are printed in a solid layer as a moisture absorption prevention layer. The standard number of lines for solid printing is 150, and the target dry coating amount is 3 g / m. 2 It is. Example F In Example F, a solid printing method was used, and a moisture absorption prevention layer of 1.5 g / m was applied to the back side. 2 As the example, a target solid print was applied, and the rest was the same as in Example A. Example G In Example F, a solid printing method was used, and a moisture absorption prevention layer of 0.5 g / m was applied to the back side. 2 As the example, a target solid print was applied, and the rest was the same as in Example A.
[0027] (Comparative example A) Comparative Example A was the same as Example A except that no moisture absorption barrier layer was provided, one-sided laminated paper was used, and a gloss finish was used. (Comparative example B) Comparative Example B uses a solid printing method and has a moisture absorption prevention layer of 0.4 g / m on the back.2 The same solid print as in Comparative Example A was used, and the same single-sided laminated paper as in Comparative Example A was used.
[0028] (Comparative example C) In Comparative Example C, the same solid printing method as in Comparative Example B was used, and a 0.1 g / m2 moisture absorption prevention layer was applied to the back surface. 2 The same solid print as in Comparative Example A was used, and the same single-sided laminated paper as in Comparative Example A was used. (Comparative example D) In Comparative Example D, the same solid printing method as in Comparative Example B was used, and a 30 g / m2 moisture absorption prevention layer was applied to the back side. 2 The same solid print as in Comparative Example A was used, and the same single-sided laminated paper as in Comparative Example A was used.
[0029] (Evaluation method and criteria) The transfer paper with the suppression ink used in the examples and comparative examples is stored in an environment of 40° C. and 90% humidity, and samples are taken out over time. The sample is thermally transferred onto a PVC foam layer using a transfer machine (I). Thereafter, the base paper (release paper) is peeled off, and the sol coat is applied evenly onto (I).
[0030] The sheet was foamed by placing it in an oven at 220° C. for 2 minutes (hereinafter referred to as the “evaluation sheet”) and evaluated by the following method. Evaluation of texture: Evaluated by sensory test. The evaluation was carried out by 10 examiners. The evaluation criteria were: 0 people...×, 1-6 people...△, 7-9 people...○, and 10 people...◎ for people who thought it was good. The accelerated test at 40°C and 90% humidity is equivalent to a week of storage at room temperature for two months. After 8 weeks, a grade of "◎" or "〇" was considered a pass. Anything other than that, "△" or "×", was considered a fail.
[0031] (Evaluation Results) The evaluation results of the wallpaper are as shown in Table 1 below. [Table 1]
[0032] (Examples A to G and Comparative Examples A to D) Of the total 11 evaluation sheets for Examples A to G and Comparative Examples A to D, only the seven evaluation sheets for Examples A to G were rated "pass" after eight weeks had elapsed. The remaining four evaluation sheets of Comparative Examples A to D were all rated "Fail" after eight weeks.
[0033] In addition, Comparative Example D was deemed "unacceptable" and "failed" due to a problem with production stability. 2 With the coating amount of , peeling occurred due to ink adhesion to the printed surface during winding, so evaluation was not possible. Of Comparative Examples A to D, it is presumed that the reason for this is that the moisture absorption prevention layer was not provided in Comparative Example A. 2 It can be inferred that the amount of coating was too small. 2 " It can be inferred that too little paint was applied.
[0034] Furthermore, of the seven evaluation sheets for Examples A to G, four evaluation sheets for Examples A to D were "passed" at the "10 week" point. The lamination method was adopted for all four evaluation sheets of Examples A to D. For this reason, it can be inferred that the lamination method allows for a longer storage period compared to the solid printing method. Of the four evaluation sheets for Examples A to D, the three evaluation sheets for Examples A, B, and D, excluding Example C, were rated "pass" at the time "12 weeks" had elapsed. Since the laminate of Example C (PP resin thickness 5 μm) is compared to the laminate of Example A (PP resin thickness 15 μm), the laminate of Example C (PET resin thickness 12 μm), and the laminate of Example D (PP resin thickness 21 μm), it can be inferred that a thicker resin thickness is advantageous in terms of extending the storage period.
[0035] Furthermore, when comparing Example A and Example B, the resins used are different between PP and PET, but as far as the evaluation results are concerned, it can be inferred that either resin is suitable for the lamination method. The amount of ink applied in the solid printing method is 0.5 g / m 2 " in Example E. 2 " can be assumed to be the upper limit. [Explanation of symbols]
[0036] 10 Transfer sheet 20 Base sheet 30 Pattern layer 31 Picture Ink Department 32 Foam-suppressing ink section 40 Moisture absorption prevention layer
Claims
1. A transfer sheet having a peelable picture pattern layer including an inhibiting ink for inhibiting foaming in a transfer material on the surface of a base sheet, A transfer sheet characterized in that a moisture absorption prevention layer is provided on the back surface of the base sheet to prevent moisture absorption into the picture pattern layer.
2. 2. The transfer sheet according to claim 1, wherein the moisture absorption prevention layer is a resin film.
3. 2. The transfer sheet according to claim 1, wherein the moisture absorption prevention layer is a solid print layer formed by applying an acrylic-vinyl-chloride-acetate resin or a color ink.
4. The coating amount of the acrylic chloride vinyl acetate resin or color ink is 0.5 g / m 2 3.0g / m or more 2 4. The transfer sheet according to claim 3, wherein the following is true:
5. A transfer sheet according to any one of claims 1 to 4, characterized in that the moisture absorption prevention layer is provided only on the back surface of the base sheet out of three locations: the back surface of the base sheet, the space between the base sheet and the picture pattern layer, and the front surface of the picture pattern layer.
6. A method for producing the transfer sheet according to any one of claims 1 to 5, comprising the steps of: A method for producing a transfer sheet, comprising laminating a resin film on the back surface of the base sheet as the moisture absorption prevention layer.
7. A method for producing the transfer sheet according to any one of claims 1 to 5, comprising the steps of: The method for producing a transfer sheet is characterized in that an acrylic-chloride-vinyl-acetate resin or a color ink is solid-printed on the back surface of the base sheet as the moisture absorption prevention layer.
Citation Information
Patent Citations
Transfer paper and manufacture of decorative board therewith
JP1983051180A
Transfer material for multistage press
JP1999034593A
Foaming inhibitor
JP1999267407A
Transfer sheet and ink composition used therefor
JP2005022373A
Method of manufacturing transfer material having excellent resistance to foil burr and transfer material
JP2009137219A